Preparation method and application of washable anti-swelling agent
By preparing water-resistant anti-swelling agents containing quaternary ammonium salts and hydroxyl groups, and adsorbing on the surface of bentonite by using static electricity and hydrogen bonding, the problems of poor temperature resistance and poor water-resistant performance of traditional anti-swelling agents at high temperatures are solved, and the problem of poor temperature resistance and poor water-resistant performance of traditional anti-swelling agents is achieved. Effective anti-swelling effect in deep wells, ultra-deep wells and deep sea oil and gas mining.
Patent Information
- Application Number
- CN202411399768.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-09
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2044-10-09
AI Technical Summary
Traditional clay anti-swelling agents have poor temperature resistance in high-temperature oil and gas mining and have poor water washing resistance, making it difficult to effectively prevent clay expansion and stabilize oil and gas reservoirs.
The Schiff base reaction of terephthaldehyde and N-methylethylenediamine is obtained by obtaining intermediate A, followed by ring-opening reaction with glycidol, and finally quaternized polymerization with dibromolelkanes to prepare a large amount of quaternary ammonium. The water-resistant anti-swelling agent of salt functional groups and hydroxyl groups is strongly adsorbed on the surface of bentonite by electrostatic and hydrogen bonding, improving anti-swelling properties and high temperature resistance.
The water-resistant anti-swelling agent maintains good structural stability at high temperatures, significantly improves the anti-swelling performance and water-washing rate, can effectively prevent clay expansion and stabilize oil and gas reservoirs, and is suitable for deep wells, ultra-deep wells and deep sea oil and gas mining.
Smart Images

Figure CN118894987A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of oilfield exploitation, and specifically relates to a preparation method and application of a water-washable anti-swelling agent. Background Art
[0002] In recent years, my country's oil and gas development has developed towards deep wells, ultra-deep wells, and deep sea areas. Shale in oil and gas reservoirs generally has problems such as wellbore instability. At the same time, clay minerals between layers will absorb water and swell, resulting in formation pore blockage, permeability reduction, and harm to oil and gas layers. This is of great significance to the protection of oil and gas reservoirs. During the water injection development stage, adding clay stabilizing agents such as anti-swelling agents to oil and gas reservoirs can effectively improve problems such as reservoir wellbore instability.
[0003] Current clay anti-swelling agent mainly contains inorganic salts, organic quaternary ammonium salts, polymers etc. Wherein organic quaternary ammonium salts have various types, less consumption, advantages such as anti-swelling efficiency is high, and have great research and development prospects. But there is the problem of poor temperature resistance in organic quaternary ammonium salt anti-swelling agent, which is unfavorable for its practical application in high-temperature oil and gas production. Publication number is that the invention patent of CN117720482A discloses a kind of multi-quaternary ammonium salt long-acting slow-release anti-swelling agent and preparation method thereof, with anhydrous piperazine, paraformaldehyde, 2-chloroethylamine, polyacid etc. as raw material, prepares a kind of multi-quaternary ammonium salt long-acting slow-release anti-swelling agent, can suppress clay expansion in a longer time and wider range, be preferably applied to the field of oilfield fracturing production increase technology. But this patent does not improve the problem that anti-swelling agent is poorly resistant to high temperature. Summary of the invention
[0004] The invention solves the problem that the traditional anti-swelling agent has poor temperature resistance and poor water washing resistance.
[0005] Technical solution: A method for preparing a water-resistant anti-swelling agent: Step (1): Add ethanol, terephthalaldehyde (CAS No. 623-27-8) and N-methylethylenediamine (CAS No. 109-81-9) into a flask equipped with a condenser reflux tube, stir to react, then distill under reduced pressure to remove ethanol, separate by column chromatography, and gradient elute with ethyl acetate and petroleum ether solution to obtain intermediate A.
[0006] Step (2): Add solvent, intermediate A and glycidol (CAS No. 556-52-5) into a flask equipped with a condenser reflux tube, stir to react, remove the solvent by distillation under reduced pressure, separate by column chromatography, and elute with ethyl acetate and petroleum ether solution in a gradient manner to obtain intermediate B.
[0007] Step (3): Add N,N-dimethylformamide, intermediate B and dibromoalkane into a reaction flask, stir for reaction, and then distill under reduced pressure, wash with acetone, and dry to obtain a water-resistant anti-swelling agent.
[0008] Preferably, in step (1), the molar ratio of terephthalaldehyde to N-methylethylenediamine is 1:(2-2.6).
[0009] Preferably, in step (1), the reaction is carried out at 70-80° C. for 8-12 h.
[0010] Preferably, in step (2), the solvent is methanol, ethanol or tetrahydrofuran.
[0011] Preferably, in step (2), the molar ratio of intermediate A to glycidol is 1:(2.4-3.8).
[0012] Preferably, in step (2), the reaction is carried out at 55-75° C. for 4-10 h.
[0013] Preferably, in step (3), the molar ratio of intermediate B to dibromoalkane is 1:(1-1.1).
[0014] Preferably, the structural formula of the dibromoalkane is , n is any integer from 2 to 6.
[0015] Preferably, in step (3), the reaction is carried out at 80-110° C. for 24-36 hours.
[0016] Preferably, the water-washable anti-swelling agent is used in oil field exploitation.
[0017] Technical effect: The present invention conducts a Schiff base reaction between terephthalaldehyde and N-methylethylenediamine to obtain an intermediate A, and the imino group thereof undergoes a ring-opening reaction with glycidol to obtain an intermediate B containing a tertiary amine group, and finally undergoes a quaternary ammonium polymerization reaction with dibromoalkanes such as 1,2-dibromoethane to obtain a water-resistant anti-swelling agent.
[0018] The main molecular chain of the water-resistant anti-swelling agent of the present invention contains a large amount of quaternary ammonium salt functional groups, and the side chain contains a large amount of hydroxyl groups, which form static electricity with the surface of bentonite silicate, and hydrogen bonds and the like interact with each other, and strong adsorption and interaction force occur between the two, and the interaction force is greater than the hydrogen bond force between the water molecules between the bentonite crystal layers and the bentonite, so that the anti-swelling agent can well squeeze out the water molecules between the bentonite crystal layers, which is conducive to improving the anti-swelling performance. In addition, the quaternary ammonium salt and the bentonite silicate have an electrostatic interaction, which reduces the ion exchange capacity of the bentonite, making the bentonite difficult to absorb hydrated cations and expand, thereby showing an excellent anti-swelling effect.
[0019] The main molecular chain of the water-resistant anti-swelling agent of the present invention contains a rigid benzene ring, has high structural stability, and is highly resistant to high temperatures, and can improve the high temperature resistance of the anti-swelling agent. After high temperature heat treatment at 120°C, the anti-swelling agent can maintain good structural stability and still have a good anti-swelling rate.
[0020] The anti-swelling agent of the present invention contains a large amount of quaternary ammonium salt and hydroxyl group, and has a strong adsorption effect and interaction force with bentonite through interactions such as static electricity and hydrogen bonds, so that the anti-swelling agent is firmly adsorbed on the surface of the bentonite and is difficult to fall off by water washing, thereby showing a higher water washing resistance rate, which is beneficial to improving the long-term anti-swelling performance of the anti-swelling agent. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 It is the reaction formula for preparing intermediate B.
[0022] Figure 2 This is the reaction formula for preparing water-resistant anti-swelling agent. DETAILED DESCRIPTION
[0023] The technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0024] Example 1 Step (1): Add 40 mL of ethanol, 30 mmol of terephthalaldehyde, and 60 mmol of N-methylethylenediamine to a flask equipped with a condenser reflux tube, heat to 75°C, stir and react for 12 hours, remove ethanol by vacuum distillation, separate by column chromatography, and gradient elute with ethyl acetate and petroleum ether solution to obtain intermediate A.
[0025] Step (2): Add 100 mL of ethanol, 30 mmol of intermediate A, and 108 mmol of glycidol to a flask equipped with a condenser reflux tube, heat to 75°C, stir and react for 4 h, remove ethanol by vacuum distillation, separate by column chromatography, and gradient elute with ethyl acetate and petroleum ether solution to obtain intermediate B.
[0026] Step (3): Add 50 mL of N,N-dimethylformamide, 50 mmol of intermediate B, and 50 mmol of 1,2-dibromoethane to a reaction bottle, heat to 80°C, stir and react for 36 hours, distill under reduced pressure, wash with acetone, and dry to obtain a water-resistant anti-swelling agent.
[0027] Example 2 Step (1): Add 40 mL of ethanol, 30 mmol of terephthalaldehyde, and 60 mmol of N-methylethylenediamine to a flask equipped with a condenser reflux tube, heat to 80°C, stir and react for 8 hours, remove ethanol by vacuum distillation, separate by column chromatography, and gradient elute with ethyl acetate and petroleum ether solution to obtain intermediate A.
[0028] Step (2): Add 100 mL of methanol, 30 mmol of intermediate A, and 96 mmol of glycidol to a flask equipped with a condenser reflux tube, heat to 60°C, stir and react for 10 h, remove methanol by vacuum distillation, separate by column chromatography, and gradient elute with ethyl acetate and petroleum ether solution to obtain intermediate B.
[0029] Step (3): Add 50 mL of N,N-dimethylformamide, 50 mmol of intermediate B, and 55 mmol of 1,3-dibromopropane to a reaction bottle, heat to 110°C, stir and react for 24 hours, distill under reduced pressure, wash with acetone, and dry to obtain a water-resistant anti-swelling agent.
[0030] Example 3 Step (1): Add 50 mL of ethanol, 30 mmol of terephthalaldehyde, and 78 mmol of N-methylethylenediamine to a flask equipped with a condenser reflux tube, heat to 70°C, stir and react for 12 hours, remove ethanol by vacuum distillation, separate by column chromatography, and gradient elute with ethyl acetate and petroleum ether solution to obtain intermediate A.
[0031] Step (2): Add 80 mL of tetrahydrofuran, 30 mmol of intermediate A, and 72 mmol of glycidol to a flask equipped with a condenser reflux tube, heat to 55°C, stir and react for 10 h, remove tetrahydrofuran by vacuum distillation, separate by column chromatography, and elute with a gradient of ethyl acetate and petroleum ether solution to obtain intermediate B.
[0032] Step (3): Add 60 mL of N,N-dimethylformamide, 50 mmol of intermediate B, and 55 mmol of 1,4-dibromobutane to a reaction bottle, heat to 80°C, stir and react for 36 hours, distill under reduced pressure, wash with acetone, and dry to obtain a water-resistant anti-swelling agent.
[0033] Example 4 Step (1): Add 40 mL of ethanol, 30 mmol of terephthalaldehyde, and 72 mmol of N-methylethylenediamine to a flask equipped with a condenser reflux tube, heat to 75°C, stir and react for 12 hours, remove ethanol by vacuum distillation, separate by column chromatography, and gradient elute with ethyl acetate and petroleum ether solution to obtain intermediate A.
[0034] Step (2): Add 80 mL of ethanol, 30 mmol of intermediate A, and 72 mmol of glycidol to a flask equipped with a condenser reflux tube, heat to 75°C, stir and react for 8 h, remove ethanol by vacuum distillation, separate by column chromatography, and gradient elute with ethyl acetate and petroleum ether solution to obtain intermediate B.
[0035] Step (3): Add 60 mL of N,N-dimethylformamide, 50 mmol of intermediate B, and 50 mmol of 1,6-dibromohexane to a reaction bottle, heat to 100°C, stir and react for 24 hours, distill under reduced pressure, wash with acetone, and dry to obtain a water-resistant anti-swelling agent.
[0036] Comparative Example 1 Step (1): Add 20 mL of ethanol, 15 mL of water, and 50 mmol of N,N,N',N'-tetramethylethylenediamine ( ), 50mmol 1,2-dibromoethane, heated to 80℃, stirred for reaction for 36h, distilled under reduced pressure, washed with acetone, and dried to obtain a water-resistant anti-swelling agent.
[0037] Comparative Example 2 Step (1): Add 50 mL of ethanol, 30 mmol of terephthalaldehyde, and 60 mmol of N,N-dimethylethylenediamine ( ), heated to 70°C, stirred for 8h, distilled under reduced pressure to remove ethanol, separated by column chromatography, and eluted with ethyl acetate and petroleum ether solution in a gradient manner to obtain intermediate C. The structural formula is: .
[0038] Step (2): Add 50 mL of N,N-dimethylformamide, 50 mmol of intermediate C, and 50 mmol of 1,2-dibromoethane into a reaction bottle, heat to 80°C, stir and react for 36 hours, distill under reduced pressure, wash with acetone, and dry to obtain a water-resistant anti-swelling agent.
[0039] With reference to the SY / T 5971-2016 standard, the anti-swelling performance test was carried out: the water-resistant anti-swelling agent was added into distilled water to prepare anti-swelling agent solutions with different mass fractions.
[0040] 0.5 g of bentonite was added to a centrifuge tube, and 10 mL of anti-swelling agent solution was added. After mixing, the mixture was allowed to stand for 2 h, and then centrifuged in a centrifuge for 15 min. The volume V1 of the expanded bentonite was measured.
[0041] Add 0.5 g of bentonite into a centrifuge tube, add 10 mL of distilled water, mix well and let stand for 2 hours, then centrifuge in a centrifuge for 15 minutes, and measure the volume V2 of the expanded bentonite.
[0042] Add 0.5 g of bentonite into a centrifuge tube, add 10 mL of kerosene, mix well and let stand for 2 hours, then centrifuge in a centrifuge for 15 minutes, and measure the volume V0 of the bentonite after expansion.
[0043] Calculate the anti-swelling rate R. R = (V2-V1) / (V2-V0) × 100%.
[0044] The washable anti-swelling agent was placed in an oven, heated to 120°C, left for 72 hours, taken out and cooled; the anti-swelling performance test was then carried out according to the above method, and the anti-swelling rate was calculated.
[0045] The test results are shown in Table 1-3.
[0046] Table 1 Anti-swelling rate test when the mass fraction of anti-swelling agent solution is 0.5%
[0047] Table 2 Anti-swelling rate test when the mass fraction of anti-swelling agent solution is 1%
[0048] Table 3 Anti-swelling rate test when the mass fraction of anti-swelling agent solution is 1.5%
[0049] As shown in Table 1-3, the water-resistant anti-swelling agent prepared by Example 1-4 shows a very high anti-swelling rate at different mass fractions. This is because the main chain of the water-resistant anti-swelling agent contains a large amount of quaternary ammonium salt functional groups, and the side chain contains a large amount of hydroxyl groups, which form static electricity with the surface of bentonite silicate, hydrogen bonds and other interactions, and the two have strong adsorption and interaction forces, and their interaction forces are greater than the hydrogen bond forces between the water molecules between the bentonite crystal layers and the bentonite, so that the anti-swelling agent can well exclude the water molecules between the bentonite crystal layers, which is conducive to improving the anti-swelling performance. And the quaternary ammonium salt and the bentonite silicate have electrostatic interactions, which reduces the ion exchange capacity of the bentonite, making it difficult for the bentonite to absorb hydrated cations and expand, thereby showing excellent anti-swelling effect. At the same time, the main chain of the water-resistant anti-swelling agent contains a rigid benzene ring, has high structural stability, and is highly resistant to high temperatures, which can improve the high temperature resistance of the anti-swelling agent. After 120°C high temperature heat treatment, the anti-swelling agent can maintain good structural stability and still has a good anti-swelling rate.
[0050] Comparative Example 1: N,N,N',N'-tetramethylethylenediamine and 1,2-dibromoethane are used to carry out quaternization polymerization reaction. The main chain of the obtained water-resistant anti-swelling agent contains a large number of quaternary ammonium salt functional groups, but does not contain hydroxyl groups. The adsorption and interaction force with the surface of bentonite are low, resulting in an anti-swelling rate lower than that of the embodiments. In addition, the main chain of the anti-swelling agent does not contain a benzene ring structure, resulting in poor high temperature resistance of the anti-swelling agent. After high-temperature heat treatment at 120°C, the anti-swelling agent is easily thermally decomposed, and the anti-swelling rate decreases significantly.
[0051] In Comparative Example 2, the intermediate C obtained by the reaction of terephthalaldehyde and N,N-dimethylethylenediamine is subjected to a quaternary ammonium polymerization reaction with 1,2-dibromoethane. The obtained water-resistant anti-swelling agent does not contain hydroxyl groups, and has low adsorption and interaction forces with the surface of bentonite, resulting in an anti-swelling rate lower than that of the various embodiments. However, the molecular main chain of the water-resistant anti-swelling agent contains a rigid benzene ring, which can improve the high temperature resistance of the anti-swelling agent. After high-temperature heat treatment at 120°C, the anti-swelling agent can maintain good structural stability, and the anti-swelling rate decreases slightly.
[0052] Refer to SY / T 5971-2016 standard to test the water washability of the anti-swelling agent.
[0053] 0.5 g of bentonite was added to a centrifuge tube, and 10 mL of anti-swelling agent solution (mass fraction 1%) was added, mixed and allowed to stand for 2 h, and then centrifuged in a centrifuge for 15 min. The volume W0 of the bentonite after swelling was measured.
[0054] Remove the supernatant by centrifugation, add 10 mL of distilled water, mix well and let stand for 2 hours; then centrifuge for 15 minutes; repeat twice; measure the volume W3 of the expanded bentonite after three water washes. Calculate the water wash resistance N. N=W0 / W3×100%.
[0055] The test results are shown in Table 4.
[0056] Table 4 Water washability test of anti-swelling agent
[0057] As can be seen from Table 4, the water washing resistance of Examples 1-4 is significantly higher than that of Comparative Examples 1-2, mainly because the anti-swelling agent contains a large amount of quaternary ammonium salts and hydroxyl groups, which form electrostatic and hydrogen bond interactions with the surface of bentonite, and the two have strong adsorption and interaction forces, so that the anti-swelling agent is firmly adsorbed on the surface of bentonite and is difficult to fall off by water washing, thereby showing a higher water washing resistance, which is beneficial to improving the long-term anti-swelling performance of the anti-swelling agent.
[0058] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A method for preparing a water-resistant anti-swelling agent, characterized in that: The preparation method comprises the following steps: Step (1): Add ethanol, terephthalaldehyde and N-methylethylenediamine to a flask equipped with a condenser reflux tube, stir for reaction, distill under reduced pressure, and separate by column chromatography to obtain intermediate A; Step (2): Add a solvent, intermediate A, and glycidol into a flask equipped with a condenser reflux tube, stir for reaction, distill under reduced pressure, and separate by column chromatography to obtain intermediate B; Step (3): Add N,N-dimethylformamide, intermediate B and dibromoalkane into a reaction flask, stir for reaction, and then perform vacuum distillation, wash and dry to obtain a water-resistant anti-swelling agent.
2. The method for preparing the water-resistant anti-swelling agent according to claim 1, characterized in that: In the step (1), the molar ratio of terephthalaldehyde to N-methylethylenediamine is 1:(2-2.6).
3. The method for preparing the water-resistant anti-swelling agent according to claim 1, characterized in that: In the step (1), the reaction is carried out at 70-80° C. for 8-12 hours.
4. The method for preparing the water-resistant anti-swelling agent according to claim 1, characterized in that: In the step (2), the solvent is methanol, ethanol or tetrahydrofuran.
5. The method for preparing the water-resistant anti-swelling agent according to claim 1, characterized in that: In the step (2), the molar ratio of intermediate A to glycidol is 1:(2.4-3.8).
6. The method for preparing the water-resistant anti-swelling agent according to claim 1, characterized in that: In the step (2), the reaction is carried out at 55-75° C. for 4-10 hours.
7. The method for preparing the water-resistant anti-swelling agent according to claim 1, characterized in that: In the step (3), the molar ratio of the intermediate B to the dibromoalkane is 1:(1-1.1).
8. The method for preparing the water-resistant anti-swelling agent according to claim 7, characterized in that: The structural formula of the dibromoalkane is , n is any integer from 2 to 6.
9. The method for preparing the water-resistant anti-swelling agent according to claim 1, characterized in that: In the step (3), the reaction is carried out at 80-110° C. for 24-36 hours.
10. Use of the water-resistant anti-swelling agent obtained by the preparation method according to any one of claims 1 to 9 in oil field exploitation.
Citation Information
Patent Citations
Multi-quaternary ammonium salt long-acting slow-release anti-swelling agent and preparation method thereof
CN117720482A
Preparation method of high temperature clay stabilizer for oil fields
CN109054798A
Environment-friendly clay stabilizer
CN109554171A
Tetramine linear small-molecular compound, and preparation method and applications thereof
CN110498747A
Wetting reversal agent for pressure reduction and augmented injection of ultra-low permeability reservoir and preparation method thereof
CN111234795A
Cited By
A method for preparing antibacterial modified acrylic resin
CN119735982A
A method for preparing antibacterial modified acrylic resin
CN119735982B