Polymer optical fiber and preparation method thereof

By adopting multi-layer core structure and modified polymer doping technology in polymer optical fibers, the precise regulation of the refractive index of the core layer is achieved, and the problem of insufficient radial refractive index regulation accuracy in the existing technology is solved, and the improvement of the improvement of the Communication bandwidth is simplified and production processes are reduced.

CN118897353APending Publication Date: 2024-11-05HUAWEI TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411284435.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-13
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

The existing polymer fibers have insufficient radial refractive index regulation accuracy, resulting in limited communication bandwidth, complex production processes and high material costs, making it difficult to meet the needs of future communication applications.

Method used

Polymer optical fibers with multi-layer core structures are used to adjust the refractive index of the core layer by doping modified polymers in the polymer matrix. The core layer and reflection are extruded layer by layer by layer by layer coextrusion die preparation method. The thickness and refractive index distribution of each layer are controlled to achieve a step-down refractive index distribution.

Benefits of technology

It improves the control accuracy of the refractive index of the core layer, reduces optical attenuation, enhances communication bandwidth, simplifies production processes, reduces material costs, and meets the needs of future communication applications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118897353A_ABST
    Figure CN118897353A_ABST
Patent Text Reader

Abstract

The embodiment of the invention relates to the technical field of polymer optical fibers, in particular to a polymer optical fiber and a preparation method thereof. In the embodiment of the invention, the fiber core comprises N fiber core layers which are sequentially arranged from inside to outside, N is an integer, and Ngt; 2; the Mth fiber core layer in the N fiber core layers sleeves the (M-1) th fiber core layer, and M is an integer and belongs to [2, N]; the refractive indexes of the N fiber core layers and the refractive indexes of the reflecting layers are decreased in a stepped mode in any radius direction of the polymer optical fiber from the central axis of the polymer optical fiber. The second fiber core layer to the Nth fiber core layer are polymer blends, and the raw materials of the polymer blends comprise a polymer matrix and a modified polymer; therefore, the refractive index of the polymer blend can be adjusted by adjusting the mass ratio of the polymer matrix to the modified polymer, so that the refractive index of each fiber core layer can easily reach the required theoretical refractive index, and the control precision of the refractive index of each fiber core layer is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of polymer optical fiber technology, and in particular to a polymer optical fiber and a method for preparing the same. Background Technology

[0002] Polymer optical fiber (POF), also known as plastic optical fiber or polymer fiber, is mainly composed of a transparent plastic core with a high refractive index and a transparent plastic reflective layer with a low refractive index.

[0003] Based on the refractive index distribution, polymer optical fibers can be divided into step-index polymer optical fibers (SI-POF) and graded-index polymer optical fibers (GI-POF). SI-POF inherently exhibits high modal dispersion, which limits the fiber communication bandwidth. Although GI-POF can meet the required communication bandwidth, it is difficult to achieve precise control over its radial refractive index. Summary of the Invention

[0004] To improve the adjustment accuracy of the radial refractive index of polymer optical fiber core, this application provides a polymer optical fiber and its preparation method, which can dope modified polymer in polymer matrix to adjust the refractive index of polymer matrix.

[0005] In a first aspect of this application, a polymer optical fiber is provided, the polymer optical fiber comprising a core and a reflective layer, the core comprising N core layers arranged sequentially from the inside out, where N is an integer and N>2; the Mth core layer of the N core layers is nested on the (M-1)th core layer, where M is an integer and M∈[2, N]; in any radial direction along the central axis of the polymer optical fiber, the refractive index of the N core layers and the refractive index of the reflective layer decrease in a stepwise manner; in the N core layers, the 2nd to the Nth core layers are polymer blends, the raw material composition of the polymer blends comprising a polymer matrix and a modified polymer, and the modified polymer is used to reduce the refractive index of the polymer matrix.

[0006] In the embodiments of this application, the second to Nth core layers are polymer blends, the raw material composition of which includes a polymer matrix and a modified polymer; therefore, the refractive index of the polymer blend can be adjusted by adjusting the mass ratio of the polymer matrix and the modified polymer, so that the refractive index of each core layer can easily reach the required theoretical refractive index, thereby improving the control accuracy of the refractive index of each core layer.

[0007] In some embodiments, N ≥ 6.

[0008] In some embodiments, the refractive index of the N-layer core and the refractive index of the reflective layer tend to have a square law distribution along any diameter direction of the polymer optical fiber.

[0009] In some embodiments, the material of the first fiber core layer is the polymer matrix, and the material of the reflective layer is the modified polymer, wherein the refractive index of the modified polymer is less than that of the polymer matrix.

[0010] In some embodiments, the polymer matrix is ​​polymethyl methacrylate; the modified polymer includes at least one of perfluoroethylene propylene, polytetrafluoroethylene, polychlorotrifluoroethylene, polyvinylidene fluoride, or polybutyl methacrylate.

[0011] In some embodiments, the theoretical thickness d1 of each fiber core layer satisfies the following formula:

[0012] d1 = floor{[(D÷2-10)÷N]}

[0013] The theoretical thickness d2 of the reflective layer satisfies the following formula:

[0014] d2=D÷2-N×d1

[0015] Where D represents the outer diameter of the polymer optical fiber, N is the number of core layers, and floor{} represents the floor function.

[0016] In some embodiments, the refractive index of the Mth fiber core layer satisfies the following formula:

[0017]

[0018] Where, n′ M n is used to represent the refractive index of the Mth core layer, n′1 is used to represent the refractive index of the first core layer, and D is used to represent the outer diameter of the polymer optical fiber.

[0019] In a second aspect of this application, a method for preparing polymer optical fibers as described in the first aspect is also provided. The method includes the following steps: feeding a polymer melt corresponding to the core layer or a polymer melt corresponding to the reflective layer into each of Q layered co-extrusion dies through each of N+1 melt feed dies; extruding the first to Nth core layers and reflective layers layer by layer using each layered co-extrusion die to obtain Q polymer optical fibers; wherein Q is an integer and Q is not less than N.

[0020] In some embodiments, before feeding the polymer melt corresponding to the core layer or the polymer melt corresponding to the reflective layer into each of the Q layered co-extrusion dies through each of the N+1 melt feed hoppers, the method further includes: determining the mass ratio of polymer matrix and modified polymer in the polymer melt corresponding to the 2nd to Nth core layers based on the Lorentz-Lorenz formula, the preset theoretical refractive index corresponding to each core layer, the refractive index of the polymer matrix, and the refractive index of the modified polymer.

[0021] In some embodiments, the Lorentz-Lorenz formula is expressed as follows:

[0022]

[0023] Where n′ is the refractive index of the polymer blend, n i Let be the refractive index of the i-th pure polymer component in the polymer blend. Let be the volume fraction of the i-th pure polymer component in the polymer blend.

[0024] It should be understood that the description in the Summary of the Invention section is not intended to limit the key or essential features of this disclosure, nor is it intended to restrict the scope of this disclosure. Other features of this disclosure will become readily apparent from the following description. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] To more clearly illustrate the technical solutions of the embodiments of the present invention, the following briefly introduces the drawings required for use in the embodiments of the present invention. Obviously, the drawings described below are only some embodiments of the present invention. Those skilled in the art can also derive other drawings based on these drawings without inventive effort.

[0026] Figure 1 This is a refractive index distribution diagram of existing GI-POF;

[0027] Figure 2 This is a schematic diagram of the propagation path of light in an existing GI-POF;

[0028] Figure 3 This is the refractive index distribution diagram of existing SI-POF;

[0029] Figure 4 This is a schematic diagram of the propagation path of light in an existing SI-POF;

[0030] Figure 5 These are schematic diagrams of the structure of polymer optical fibers provided in some embodiments of this application, and refractive index distribution diagrams of polymer optical fibers;

[0031] Figure 6 These are refractive index distribution diagrams of polymer optical fibers provided in some embodiments of this application;

[0032] Figure 7 These are refractive index fitting curves of polymer optical fibers provided in some embodiments of this application;

[0033] Figure 8 This is a schematic diagram of the path of light in a polymer optical fiber provided in some embodiments of this application;

[0034] Figure 9 This is a schematic diagram of the polymer optical fiber structure from one perspective, provided in some embodiments of this application;

[0035] Figure 10 These are refractive index distribution diagrams of polymer optical fibers provided in other embodiments of this application;

[0036] Figure 11 These are refractive index fitting curves for polymer optical fibers provided in other embodiments of this application;

[0037] Figure 12 These are schematic diagrams of polymer optical fiber production equipment provided in some embodiments of this application;

[0038] Figure 13 This is a schematic diagram of the structure of a layered co-extrusion die provided in some embodiments of this application;

[0039] Figure 14 This is a schematic diagram of the structure of a polymer feed tank provided in some embodiments of this application. DETAILED DESCRIPTION

[0040] The principles and spirit of this disclosure will be described below with reference to several exemplary embodiments illustrated in the accompanying drawings. It should be understood that these specific embodiments are described merely to enable those skilled in the art to better understand and implement this disclosure, and are not intended to limit the scope of this disclosure in any way. In the following description and claims, unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art.

[0041] As used herein, the term "comprising" and similar terms should be understood as open-ended inclusion, i.e., "including but not limited to". The term "based on" should be understood as "at least partially based on". The term "an embodiment" or "the embodiment" should be understood as "at least one embodiment". The terms "first", "second", etc., may refer to different or the same objects and are used only to distinguish the objects referred to, without implying a particular spatial order, temporal order, order of importance, etc., of the objects referred to.

[0042] Figure 1 These are refractive index profiles of existing graded-index polymer optical fibers (GI-POF) provided in some embodiments of this application. Please refer to... Figure 1 The GI-POF10 includes a fiber core 11 and a reflective layer 12. The refractive index at the axis O of the fiber core 11 is n'1, and the refractive index of the reflective layer 12 is n”. The refractive index of the fiber core 11 gradually decreases from the axis O along any radial direction of the GI-POF, and the refractive index of the GI-POF gradually decreases from the axis O along the radial direction of the GI-POF. Specifically, the refractive index of the fiber core 11 can be parabolically distributed from the axis O along the radial direction of the GI-POF. For example, Figure 2 A schematic diagram of the propagation path of higher-order mode light waves within GI-POF 10 is presented, such as... Figure 2 As shown, the propagation path of higher-order mode light waves in GI-POF 10 is approximately that of a sine wave.

[0043] For light waves of the same frequency, their propagation speed in a propagation medium is inversely proportional to the refractive index of the medium; that is, the higher the refractive index of the propagation medium, the slower the light wave propagates. When higher-order mode signals propagate in an optical fiber, they travel from regions with higher refractive index near the inner core to regions with lower refractive index near the outer core. Therefore, in regions with lower refractive index in the core, although the travel path of higher-order mode signals is longer, their propagation speed is greater; the greater propagation speed compensates for the longer propagation path. Compared to higher-order mode signals, lower-order mode signals propagate in regions closer to the fiber's central axis; their propagation path in the core is shorter, but their propagation speed is lower. Therefore, higher-order and lower-order mode signals entering the GI-POF 10 at the same time can arrive at the signal receiver at the same or similar times, which helps reduce the mode dispersion of the GI-POF 10, decrease signal broadening, and give the GI-POF 10 a higher communication bandwidth. Among them, higher-order mode signals are used to represent optical signals propagating near the interface between the fiber core and the reflector in the optical fiber; lower-order mode signals are used to represent optical signals propagating near the central axis of the optical fiber.

[0044] Figure 3 These are refractive index profiles of existing step-index polymer optical fibers (SI-POF) provided in some embodiments of this application. Please refer to... Figure 3SI-POF 20 comprises a core 21 and a reflective layer 22, wherein the refractive index of the core 21 is n'1, and the refractive index of the reflective layer 22 is n''. The refractive index of the core 21 remains constant radially from the axis of SI-POF 20. Due to the large numerical aperture of SI-POF 20 and its multimode nature, it exhibits high modal dispersion; higher-order modes (such as...) Figure 4 The L1 wave in SI-POF 20 has a longer path and takes longer to reach the end face of SI-POF 20, compared to lower-order modes (such as...). Figure 4 The significant time difference between the arrival times of L2 in the signal at the SI-POF 20 end face causes signal broadening, thus limiting the communication bandwidth of the SI-POF 20. A typical SI-POF can achieve a data transmission rate of 100Mbps × 100m.

[0045] Existing SI-POFs typically consist of only a core layer and a reflective layer. While it's possible to reduce the numerical aperture (NA) of an existing SI-POF by adjusting the refractive indices of the core layer to approximate those of the reflective layer, thereby increasing the data transmission rate, even with this reduction to 0.3, the data transmission rate still doesn't exceed 1 Gbps × 50 m, far from meeting the demands of future communication applications.

[0046] Specifically, the numerical aperture (NA) of polymer optical fiber is used to represent the coupling efficiency between the fiber and the light source, and NA can be calculated using the following formula:

[0047]

[0048] Where N1 is the refractive index of the fiber core material and N2 is the refractive index of the reflective layer material.

[0049] In future communication system applications, the requirements for data transmission rates are becoming increasingly stringent. This is particularly true in military equipment communication systems, next-generation automotive internet, smart home networks, lidar, video surveillance, and industrial automation control networks, where communication media are required to possess characteristics such as vibration resistance, electromagnetic interference resistance, high communication bandwidth, high optical coupling efficiency, and bend resistance. Specifically, communication bandwidth performance is required to be at least 3GHz × 50m for each channel. Among common wired communication media, polymer optical fibers (PIFs) are widely used due to their vibration resistance, electromagnetic interference resistance, high coupling efficiency, and bend resistance. However, the communication bandwidth of SI-POFs is only 100MHz × 100m. Although GI-POFs can meet the bandwidth requirements, their raw materials are perfluorinated or semi-fluorinated polymers, resulting in high material costs; furthermore, the production process involves preform drawing, which is complex and cannot achieve continuous production like extrusion. Additionally, adjusting the radial refractive index of the fiber preform is difficult, making precise refractive index adjustment challenging and prone to causing unstable refractive index distribution in the fiber.

[0050] Specifically, the methods for fabricating preforms include gel polymerization and centrifugal polymerization. Gel polymerization utilizes the gel effect, placing the peripheral methyl methacrylate monomers within a gel layer, resulting in faster polymerization and driving the dopant to aggregate radially inwards. Ultimately, the radial refractive index of the fiber preform exhibits a gradual gradient, with a high center and low ends. Centrifugal polymerization uses materials with different refractive indices and densities, subjected to varying centrifugal forces within the same apparatus, to form material layers at different locations, creating different refractive index gradients. However, neither of these methods makes it easy to adjust the radial refractive index distribution of the fiber preform.

[0051] Based on this, this application provides a polymer optical fiber and its fabrication method. The core of the polymer optical fiber includes N (N>2) core layers arranged sequentially from the inside out. Along any radial direction from the central axis of the polymer optical fiber, the refractive index of the N core layers and the refractive index of the reflective layer decrease in a stepwise manner. Among the N core layers, the second to Nth core layers are polymer blends. The raw material composition of the polymer blends includes a polymer matrix and a modified polymer. The modified polymer is used to reduce the refractive index of the polymer matrix. By controlling the mass ratio of the polymer matrix and the modified polymer, polymer blends with target refractive indices corresponding to each core layer can be obtained. Therefore, the refractive index of each core layer is easily controlled, and there is no need to dope with inert high-refractive-index materials, avoiding increased optical fiber attenuation. To facilitate the reader's understanding of this application, specific embodiments are described below.

[0052] This application provides a polymer optical fiber, which includes a core and a reflective layer. The core is the light-guiding region of the polymer optical fiber; the reflective layer, also called the cladding, is the material surrounding the core. The refractive index of the core is greater than that of the reflective layer. The core includes N core layers arranged sequentially from the inside out, where N is an integer and N>2. The Mth core layer of the N core layers is nested on the (M-1)th core layer, where M is an integer and M∈[2,N]. In any radial direction along the central axis of the polymer optical fiber, the refractive index of the N core layers and the refractive index of the reflective layer decrease in a stepwise manner. In the N core layers, the 2nd to Nth core layers are polymer blends. The raw material composition of the polymer blends includes a polymer matrix and a modified polymer, and the modified polymer is used to reduce the refractive index of the polymer matrix. The refractive index of each core layer is a constant value; that is, for each core layer, its refractive index does not change radially along the polymer optical fiber.

[0053] Specifically, in some embodiments, the first fiber core layer is cylindrical, and the second to Nth fiber core layers are annular, with the second to Nth fiber core layers sequentially nested on the first fiber core layer.

[0054] For example, Figure 5 The refractive index distribution diagrams of polymer optical fibers provided in some embodiments of this application are shown. For example... Figure 5 As shown, N=6, and the 6 core layers are core layer 1 (D1), core layer 2 (D2), core layer 3 (D3), core layer 4 (D4), core layer 5 (D5), and core layer 6 (D6). D7 is the reflective layer. D1 has the highest refractive index (n'1), and the reflective layer has the lowest refractive index (n"). Along any radius from the central axis of the polymer fiber, the refractive indices of the N core layers and the reflective layer decrease in a stepwise manner.

[0055] In some embodiments, N≥6. When N is less than 6, although the refractive index of polymer optical fiber decreases in a stepwise manner, the number of core layers is generally only 3 to 5, and the thickness of each core layer is too large, causing the refractive index between adjacent core layers to change rapidly. This prevents the refractive index distribution of the core from changing in an approximately gradual manner, which is not conducive to reducing the modal dispersion of polymer optical fiber.

[0056] In existing technologies, to increase the refractive index of the polymer matrix material, inert dopants with high refractive indices are typically used to dope the high-transmittance polymer matrix material. To ensure the core layer (i.e., the first fiber core layer) has the highest refractive index, the core layer material must be doped with the largest amount of inert dopants. Since the transmittance of inert dopants is lower than that of the polymer matrix, doping with a large amount of inert dopants increases the absorption loss of the core layer material, increases the loss in the main optical transmission region, and significantly increases the optical attenuation of the polymer fiber, which is detrimental to optical signal transmission. In the embodiments of this application, by doping the polymer matrix with modified polymers to reduce the refractive index of the polymer matrix, the optical attenuation problem of polymer fibers caused by the use of inert dopants can be avoided.

[0057] Specifically, in some embodiments, the first fiber core layer is cylindrical, and the second to Nth fiber core layers are annular, with the second to Nth fiber core layers sequentially nested on the first fiber core layer.

[0058] For example, Figure 5 Schematic diagrams of the polymer optical fiber provided in some embodiments of this application are shown, such as... Figure 5 As shown, the polymer optical fiber core comprises six core layers, namely D1, D2, D3, D4, D5, and D6, and the reflective layer of the polymer optical fiber is D7. The refractive index of the six core layers decreases in a stepwise manner from the axis of the polymer optical fiber along the radial direction of the polymer optical fiber.

[0059] In the embodiments of this application, the refractive index of the core layer decreases in a stepwise manner from the axis of the polymer fiber along the radial direction of the polymer fiber. The polymer fiber has at least 6 core layers. By increasing the number of core layers and reducing the thickness of each core layer, the refractive index distribution of the polymer fiber can tend to decrease gradually. Therefore, the higher-order modes carrying the optical signal will be continuously refracted in multiple core layers in the polymer fiber until the incident angle meets the numerical aperture, resulting in total internal reflection, returning to the polymer fiber, and then undergoing multiple refractions and one total internal reflection again. Since the propagation speed of light in materials with different refractive indices is inversely proportional to the refractive index of the material, although the higher-order modes travel a longer path in the fiber, they have a greater propagation speed as compensation, making the time when the higher-order modes finally arrive at the receiving end close to or almost equal to that of the lower-order modes, thereby reducing optical mode dispersion and thus reducing optical signal broadening.

[0060] The polymer optical fiber provided in this application embodiment can retain the advantages of the large core diameter of polymer optical fiber; at the same time, when connected to a light source, even if the polymer optical fiber and the light source are slightly deviated due to vibration, the optical signal can still be normally coupled into the polymer optical fiber.

[0061] In some embodiments, the material of the first core layer is a polymer matrix, the materials of the second to Nth core layers are polymer blends, and the raw material composition of the polymer blends includes a polymer matrix and a modified polymer, and the material of the reflective layer is a modified polymer; wherein, the refractive index of the modified polymer is lower than the refractive index of the polymer matrix; in the second to Nth core layers, the modified polymer is used to reduce the refractive index of the polymer matrix.

[0062] In the embodiments of this application, the refractive index of the polymer matrix is ​​adjusted by doping a modified polymer into the polymer matrix. The modified polymer needs to have the following characteristics: (1) the polymer matrix and the modified polymer have the same working wavelength window; (2) the refractive index of the modified polymer is lower than that of the polymer matrix; (3) in terms of physical properties, the modified polymer is compatible with the polymer matrix to form a polymer blend; (4) it does not chemically react with the polymer matrix in the molten state.

[0063] For example, in some embodiments, the polymer matrix is ​​polymethyl methacrylate (PMMA); in this case, the modified polymer needs to meet the following conditions: (1) it has the same working wavelength window as PMMA, that is, it has low absorption loss at working wavelengths of 520nm and 650nm; (2) its refractive index is lower than that of PMMA; (3) it is physically compatible with PMMA to form a polymer blend; (4) it does not chemically react with PMMA in the molten state.

[0064] Specifically, in some embodiments of this application, the modified polymer includes at least one of perfluoroethylene propylene, polytetrafluoroethylene, polychlorotrifluoroethylene, polyvinylidene fluoride, or polybutyl methacrylate.

[0065] In some embodiments, the outer diameter of the polymer optical fiber is 0.25 mm to 2.0 mm, and the thickness of the reflective layer is 10 μm to 20 μm.

[0066] Figure 6 The refractive index distribution diagrams of polymer optical fibers with 6 core layers provided in some embodiments of this application are presented. Figure 7 Showed Figure 6 The refractive index fitting curve of the polymer optical fiber. From Figure 6 and Figure 7 It is known that the refractive index distribution of polymer optical fibers with 6 core layers is close to a gradual change, which makes polymer optical fibers have lower bending loss.

[0067] In some embodiments, the theoretical thickness d1 of each fiber core layer satisfies the following formula:

[0068] d1 = floor{[(D÷2-10)÷N]}

[0069] Where d1 represents the theoretical thickness of the fiber core, D represents the outer diameter of the polymer fiber, N is the number of layers in the fiber core, and floor{} represents the floor function.

[0070] Specifically, in the above formula, rounding down means taking the integer less than the calculated result when the result is not an integer. [(D÷2-10)÷N] is used to represent the theoretical thickness of each fiber core layer obtained from the calculation.

[0071] At this point, the theoretical thickness d2 of the reflective layer satisfies the following formula:

[0072] d2=D÷2-N×d1

[0073] Where d2 represents the thickness of the reflective layer.

[0074] Specifically, in some implementations, the refractive index of the Mth fiber core layer is calculated using the following formula:

[0075]

[0076] Where n1 represents the refractive index of the first fiber core layer, M is an integer and M∈[1,N], n′ M The M-th core layer is used to represent the refractive index, and D is used to represent the outer diameter of the polymer optical fiber.

[0077] For example, in some embodiments, the theoretical outer diameter of the polymer optical fiber is 1000 μm, the number of core layers N is 6, the material of the first core layer (i.e., the polymer matrix) is PMMA, and the materials of the modified polymer and the reflective layer are both PVDF. The refractive index of PMMA is 1.492; the refractive index of PVDF is 1.42. Therefore:

[0078] The theoretical thickness of the fiber core layer is:

[0079] d1=floor{[(D÷2-10)÷N]}=floor{[(1000÷2-10)÷6=floor81.6667=81μm

[0080] The theoretical thickness of the reflective layer is:

[0081] d2=D÷2-N×d1=1000÷2-6×81=14μm

[0082] The refractive index of the Mth fiber core layer is:

[0083]

[0084] In this embodiment, the refractive index distribution of each core layer and reflective layer of the polymer optical fiber is shown in Table 1, where d represents the distance of the material of the core layer and reflective layer from the central axis.

[0085] Table 1

[0086]

[0087]

[0088] In this embodiment, the first to sixth core layers form the main space of the optical waveguide, while the reflective layer is used to increase the physical properties (such as flexibility, tensile strength, tensile yield strength, and breaking strength) and optical coupling capability of the polymer optical fiber. The refractive index difference between the reflective layer and the sixth core layer is the largest, which is beneficial for increasing the numerical aperture of the outermost layer, thereby facilitating the optical coupling of large-area signal sources.

[0089] In other embodiments, the theoretical outer diameter of the polymer optical fiber is 1000 μm, the number of core layers N is 9, the material of the first core layer (i.e., the polymer matrix) is PMMA, and the materials of the modified polymer and the reflective layer are both PVDF. Therefore:

[0090] The theoretical thickness of the fiber core layer is:

[0091] d1=floor{[(D÷2-10)÷N]}=floor{[(1000÷2-10)÷9=floor54.4444=54μm

[0092] The theoretical thickness of the reflective layer is:

[0093] d2=D÷2-N×d1=1000÷2-9×54=14μm

[0094] The refractive index of the Mth fiber core layer is:

[0095]

[0096] The refractive index distribution of the core and reflective layer of polymer optical fiber is shown in Table 2, where d represents the distance of the core and reflective layer materials from the central axis.

[0097] Table 1

[0098]

[0099]

[0100] For example, Figure 5-7 The refractive index distribution and refractive index fitting curve of polymer optical fiber with 6 core layers are presented. Figure 8Schematic diagrams illustrating the propagation paths of light waves in a polymer optical fiber with a six-core structure, provided in some embodiments of this application, are presented. Figure 8 It can be seen that the propagation path of light waves in polymer optical fibers with 6 core layers is close to a sine curve. Figure 9-11 A schematic diagram, refractive index distribution, and refractive index fitting curve of a polymer optical fiber with nine core layers are presented. Figure 5-7 and Figure 9-11 The refractive index distributions of two polymer optical fibers with different numbers of core layers show that, when the outer diameter of the polymer optical fiber remains constant, the more core layers there are and the smaller the thickness of each core layer, the closer the refractive index fitting curve of the polymer optical fiber is to a gradual distribution, which is more conducive to improving the modal dispersion of the polymer optical fiber.

[0101] In some embodiments, the refractive indices of the N core layers and the reflective layer tend to have a square-law distribution along any diameter direction of the polymer fiber. In this embodiment, when the refractive index of the polymer fiber has a square-law distribution along its diameter direction, the higher-order mode optical signal has higher speed compensation and a longer travel path in the effective core layer with a lower refractive index, allowing the lower-order mode signal and the higher-order mode signal to arrive at the end face of the polymer fiber at the same or similar time, thereby reducing the mode dispersion of the polymer fiber and improving the communication bandwidth.

[0102] This application also provides a method for preparing polymer optical fibers. The method is used to prepare the polymer optical fibers provided in the above embodiments. The method includes the following steps: feeding a polymer melt corresponding to a core layer or a polymer melt corresponding to a reflective layer into each of Q layered co-extrusion dies through each of N+1 melt feed barrels; extruding the first to Nth core layers and reflective layers layer by layer using each layered co-extrusion die to obtain Q polymer optical fibers; wherein Q is an integer and Q is not less than N.

[0103] In some embodiments, before feeding the polymer melt corresponding to a core layer or the polymer melt corresponding to a reflective layer into each of the Q layered co-extrusion dies through each of the N+1 melt feed hoppers, the method further includes: determining the mass ratio of polymer matrix and modified polymer in the polymer melt corresponding to the 2nd to Nth core layers based on the Lorentz-Lorenz formula, the preset theoretical refractive index corresponding to each core layer, the refractive index of the polymer matrix, and the refractive index of the modified polymer.

[0104] Specifically, in some embodiments, the Lorentz-Lorenz formula is expressed as follows:

[0105]

[0106] Where n′ is the refractive index of the polymer blend, n i Let be the refractive index of the i-th pure polymer component in the polymer blend. Let be the volume fraction of the i-th pure polymer component in the polymer blend.

[0107] For example, in some embodiments, the polymer matrix is ​​a polymer of one pure component, and the modified polymer is a polymer of another pure component. The expression for the Lorentz-Lorenz formula is as follows:

[0108]

[0109] in, and n1 and n2 are used to represent the volume fractions of the polymer matrix and modified polymer in the polymer blend, respectively, and are used to represent the refractive indices of the polymer matrix and modified polymer, respectively.

[0110] In some embodiments, the refractive index of the polymer blend can be initially calculated using the Lorentz-Lorenz formula to obtain the volume fractions of the polymer matrix and modified polymer in the polymer blend. Based on the calculated volume fractions of the polymer matrix and modified polymer, the polymer matrix and modified polymer are blended. The refractive index of the polymer blend film is tested using the ellipsometry method. The material ratio of the polymer matrix and modified polymer is optimized based on the tested refractive index and the actual required refractive index, so that the refractive index of the final polymer blend meets the actual refractive index required by each effective core layer material.

[0111] This application embodiment also provides a manufacturing apparatus for polymer optical fibers. This apparatus is used to manufacture the polymer optical fibers provided in the above embodiments. The apparatus includes: N+1 melt feed tanks, each melt feed tank being used to output a polymer melt corresponding to the material of each core layer or a polymer melt corresponding to the material of each reflective layer. The apparatus also includes: Q layered co-extrusion dies, each layered co-extrusion die including N+1 flow channels, each flow channel being connected to a melt feed tank, and each flow channel being used to extrude one of the core layers or the cladding layers; wherein Q is an integer, and Q is not less than N.

[0112] In some embodiments, the manufacturing equipment further includes: a feed inlet, a screw extruder, and a precision metering pump, wherein the feed inlet is used to input solid polymer particles corresponding to the material of each fiber core layer or the material of the reflective layer; the screw extruder is connected to the feed inlet and is used to convert the polymer particles input from the feed inlet into polymer melt; the precision metering pump is connected to the screw extruder and a flow channel of each layered co-extrusion die respectively, and the precision metering pump is used to input the polymer melt generated from the screw extruder into the flow channel of each layered co-extrusion die according to a preset output amount.

[0113] In the embodiments of this application, if the fiber extrusion equipment produces only a single fiber using conventional production methods, the flow rate of extruding one layer of polymer fiber material (each core layer or reflective layer material) through a single extruder is too high, resulting in a large thickness of each layer of polymer fiber material. If the number of core layers N is also large, the diameter of the polymer fiber preform extruded from the co-extrusion die will be too large, which is not conducive to thinning the polymer fiber preform to form a polymer fiber. At the same time, the interface between each two layers of polymer fiber material needs to be flat and smooth to reduce the linear scattering effect of the fiber and thus reduce fiber attenuation. Extruding one layer of polymer fiber material through a single extruder results in the prepared multi-step refractive index polymer fiber not having too many step changes, causing excessive refractive index changes between each core layer, making it impossible to achieve an approximately gradual change, and thus the modal dispersion of the polymer fiber cannot be well improved.

[0114] In the embodiments of this application, in the layered extrusion process, multiple screw-type melt feed barrels are used to extrude materials of different core layers. The extrusion screws need to be adapted to the power and material. Structurally, the more core layers, the better. The larger the number of core layers, the smaller the thickness of each core layer, and the less material is required for each core layer. Therefore, the material flow rate of the extrusion screw of a single melt feed barrel per unit time is much greater than the amount of material required for each layer of polymer optical fiber. This causes the material to deform the extrusion die during the extrusion of polymer optical fiber. If the volume of the extrusion die is increased, the cross-sectional area of ​​the initially drawn optical fiber will be too large, which is not conducive to the subsequent thinning and cooling of the optical fiber. Therefore, in order to make full use of the extrusion power of the current screw extruder, the embodiments of this application adopt a multi-fiber co-extrusion process. The production device is set to produce multiple optical fibers simultaneously, that is, the number of optical fibers produced simultaneously must be greater than or equal to the set effective core layer number. Each extrusion screw simultaneously extrudes material for the same core layer of multiple optical fibers, which not only solves the problem of excessive extrusion but also increases the yield of optical fibers. Taking the production of distributed structure polymer optical fiber with 6 effective core layers as an example, the production line should be equipped with at least 6 melt feed cylinders. Figure 12 The provided polymer production equipment is equipped with 7 melt feed cylinders.

[0115] like Figure 13 As shown, each melt feed barrel includes a feed inlet 131, a screw extruder 132, a precision metering pump 133, an exhaust device 134, a pressure sensor 135, an exhaust port 136, a discharge port 137, a first temperature sensor 138, and a second temperature sensor 139. The feed inlet 131 is connected to the screw extruder 132 and is used to feed solid polymer raw materials, such as polymer matrix plastic particles or modified polymer plastic particles, into the screw extruder 132. The screw extruder 132 is connected to the precision metering pump 133, which converts the input raw materials into polymer melt and feeds the polymer melt into the precision metering pump 133, thereby controlling the flow rate of the polymer melt discharged from the discharge port 137. The discharge port 137 is used to feed the polymer melt into a layered co-extrusion die. A first temperature sensor 138 is installed in the screw extruder 132 to detect the temperature of the polymer melt inside the screw extruder 131; a second temperature sensor 139 is installed in the precision metering pump 133 to detect the temperature of the polymer melt inside the precision metering pump 133. An exhaust device 134 is connected to the screw extruder 132 and is used to discharge the gas generated inside the screw extruder 132 through the exhaust port 136. A pressure sensor 135 is used to detect the pressure of the exhaust device 134.

[0116] In this embodiment, each melt feed hopper is equipped with an independent screw extruder. The polymer melt is extruded into the channel corresponding to the same core layer or unified reflective layer in each layered co-extrusion die through a precision metering pump, thereby transporting the polymer melt to the same core layer or reflective layer of the corresponding polymer optical fiber in the 7 optical fiber dies.

[0117] Figure 14 An exemplary diagram illustrating the structure of a layered co-extrusion die and the principle of layered co-extrusion is provided from one perspective. Figure 14 As shown, the feed ports of the layered co-extrusion die include a first feed port 611, a second feed port 612, a third feed port 613, a fourth feed port 614, a fifth feed port 615, a sixth feed port 616, and a seventh feed port 617 arranged sequentially along the fiber exit direction. The first to sixth feed ports are for the polymer melts corresponding to the first to sixth fiber core layers, respectively, while the seventh feed port is for the polymer melts corresponding to the reflective layer material. The first to sixth feed ports 611 are connected to the first layer flow channel 601, the second layer flow channel 602, the third layer flow channel 603, the fourth layer flow channel 604, the fifth layer flow channel 605, and the sixth layer flow channel 606, respectively. The polymer melts of each layer are fed into the respective flow channels from the first to the sixth feed ports 611 to 616. The feed flow rate of each flow channel is strictly controllable.

[0118] In some embodiments, a first inlet is used to input a polymer matrix in a molten state, and second to sixth inlets are used to input a melt blend of the polymer matrix and a modified polymer; a seventh inlet is used to input a modified polymer material in a molten state. Furthermore, the mass ratio of the polymer matrix to the modified polymer is different in the melt blends input through the second to sixth inlets; the mass percentage of the modified polymer in the melt blends increases sequentially from the second inlet to the sixth inlet.

[0119] The end of the die body furthest from the fiber outlet is a pressure-controlled air chamber 610. The fiber outlet direction represents the direction in which the polymer optical fiber is drawn after being extruded from the fiber outlet of the layered co-extrusion die.

[0120] After each layer of raw material enters the extrusion die, it will continue to move forward in the die and adhere to the next layer of feed, forming a structure in which the polymer ring of this layer adheres to the polymer ring of the next layer, until all the fiber core layers and reflective layers are adhered to each other in the die and extruded from the die.

[0121] In the embodiments of this application, after the P-th layer material advances a certain distance in the mold channel, it converges with the P+1-th layer material, and the P+1-th layer material covers the P-th layer material. By controlling the flow rate, temperature, and other parameters of the materials, as well as the structural design of the mold orifice, the interface between the two layers is made flat and smooth when the P+1-th layer material covers the P-th layer material, reducing the linear loss caused by the instability of the optical fiber structure. At the same time, the flow rate, temperature, pressure, and other parameters of the adjacent two layers can be adjusted according to the interface conditions, making the extrusion process real-time and controllable. Wherein, P∈[1,N].

[0122] The front of the mold is equipped with a pressure-controlled air chamber to provide pressure for the material flow channel. The gas used is typically dry air or an inert gas. Since each screw provides a small amount of polymer melt for its corresponding layer, insufficient material drive may cause the melt to remain in the mold for too long, leading to the following problems: 1. Material blockage and compression of the mold, causing mold damage; 2. Prolonged residence in the mold can cause excessively high temperatures, burning the material and increasing fiber attenuation; 3. When adjacent polymer melt layers are bonded in the layered co-extrusion mold, the interface may not be smooth enough, increasing fiber loss. The pressure chamber provides dry air or inert gas to each material channel for pressurization, propelling each layer forward in the mold. The pressure of each layer is independently controllable and equipped with a pressure sensor for real-time monitoring and adjustment, ensuring that the gas is used to propel the polymer melt forward in the mold without generating air bubbles within the melt.

[0123] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Under the concept of the present invention, the technical features in the above embodiments or different embodiments can also be combined, the steps can be implemented in any order, and there are many other variations in different aspects of the present invention as described above. For the sake of simplicity, they are not provided in detail. Although the present invention has been described in detail with reference to the above embodiments, ordinary technicians in this field should understand that they can still modify the technical solutions described in the above embodiments, or make equivalent replacements for some of the technical features therein. These modifications or replacements do not deviate the essence of the corresponding technical solutions from the scope of the technical solutions of the embodiments of the present invention.

Claims

1. A polymer optical fiber, comprising a core and a reflective layer, characterized in that: The fiber core comprises N fiber core layers arranged sequentially from the inside to the outside, where N is an integer and N>2; The Mth fiber core layer among the N fiber core layers is sleeved on the M-1th fiber core layer, where M is an integer and M∈[2,N]; In any radial direction of the polymer optical fiber from the central axis of the polymer optical fiber, the refractive index of the N core layers and the refractive index of the reflective layer decrease in a step-like manner; In the N core layers, the material of the second to Nth core layers is a polymer blend, the raw material composition of the polymer blend includes a polymer matrix and a modified polymer, and the modified polymer is used to reduce the refractive index of the polymer matrix.

2. The optical fiber according to claim 1, characterized in that N≥6.

3. The optical fiber according to claim 2, characterized in that, in any diameter direction along the polymer optical fiber, the refractive index of the N core layers and the refractive index of the reflective layer tend to be square-rate distributed.

4. The optical fiber according to claim 1, characterized in that The material of the first core layer is the polymer matrix, the material of the reflective layer is the modified polymer, and the refractive index of the modified polymer is smaller than the refractive index of the polymer matrix.

5. The optical fiber according to claim 1, characterized in that The polymer matrix is ​​polymethyl methacrylate; The modified polymer includes at least one of polyperfluoroethylene propylene, polytetrafluoroethylene, polychlorotrifluoroethylene, polyvinylidene fluoride or polybutyl methacrylate.

6. The optical fiber according to claim 1, characterized in that The theoretical thickness d1 of each core layer satisfies the following formula: d1=floor{[(D÷2-10)÷N]} The theoretical thickness d2 of the reflective layer satisfies the following formula: d2=D÷2-N×d1 Wherein, D is used to represent the outer diameter of the polymer optical fiber, N is the number of core layers, and floor{} is used to represent a floor rounding function.

7. The optical fiber according to any one of claims 1 to 6, characterized in that: The refractive index of the Mth core layer satisfies the following formula: Among them, n ′ M Used to represent the refractive index of the Mth core layer, n ′ 1 is used to represent the refractive index of the first core layer, d1 is used to represent the theoretical thickness of each core layer, and D is used to represent the outer diameter of the polymer optical fiber.

8. A method for preparing a polymer optical fiber according to any one of claims 1 to 7, characterized in that: The method comprises: Inputting a polymer melt corresponding to the core layer or a polymer melt corresponding to the reflective layer into each of the Q layered co-extrusion dies through each of the N+1 melt feeding barrels; Using each of the layered co-extrusion dies to extrude the first to Nth core layers and the reflection layer layer by layer to obtain Q polymer optical fibers; Wherein, Q is an integer, and Q is not less than N.

9. The method according to claim 8, characterized in that Before respectively inputting a polymer melt corresponding to the core layer or a polymer melt corresponding to the reflective layer into each of the Q layered co-extrusion dies through each of the N+1 melt feeding barrels, the method further comprises: Based on the Lorentz-Lorenz formula, the preset theoretical refractive index corresponding to each core layer, the refractive index of the polymer matrix and the refractive index of the modified polymer, the mass ratio of the polymer matrix and the modified polymer in the polymer melt corresponding to the 2nd to Nth core layers is determined.

10. The method according to claim 9, characterized in that The expression of the Lorentz-Lorenz formula is as follows: Among them, n ′ is the refractive index of the polymer blend, n i is the refractive index of the pure component i of the polymer in the polymer blend, is the volume fraction of the pure component of the ith polymer in the polymer blend.