Transistor structure with multiple vertical thin bodies

By adopting a single convex structure and vertical thin body design in the transistor, the problems of high standby current and increased leakage current path in the prior art are solved, and a vertical thin body transistor structure with low standby current and high conduction current is realized. Increased current ratio.

CN118899339APending Publication Date: 2024-11-05INVENTION & COLLABORATION LABORATORY INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410550375.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2024-05-03
Filing Date
2024-05-06
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

The prior art is difficult to achieve a fin field effect transistor with low standby current under technology less than 20 nanometers, and as the size decreases, the leakage current path increases, making it difficult to control the effective channel length and gate-induced drain leakage current.

Method used

Using a vertical thin-body transistor structure with a single convex structure, by forming a trench and a vertical thin body on the single convex structure, the combination of the gate dielectric layer and the conductive layer can reduce the standby current and increase the conduction current to form multiple Conductive channels to increase the current ratio.

Benefits of technology

Effectively reduce the standby current by 10 to 100 times and improve the on-current, which significantly improves the performance of the transistor, especially the ratio of conduction current in the on-state to the off-state current ratio.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118899339A_ABST
    Figure CN118899339A_ABST
Patent Text Reader

Abstract

The invention discloses a transistor structure. The transistor structure is provided. The transistor structure includes a body, a gate structure, a source region and a drain region. The body has a single convex structure, where the single convex structure is made of a first semiconductor material, and a trench is formed in the single convex structure. The gate structure is provided with a gate conductive layer and a gate dielectric layer, the gate conductive layer stretches across the upper portion of the single convex structure, and a part of the gate conductive layer is filled in the groove. The source region is in contact with a first end of the single convex structure. The drain region is in contact with the second end of the single convex structure. The ratio of the turn-on current to the turn-off current of the transistor structure is not less than 106. Therefore, compared with the prior art, the transistor structure not only can effectively reduce the leakage current path of the transistor in the closed state, but also greatly increases the conduction current of the transistor in the on state.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a transistor structure, and in particular to a transistor structure having a plurality of vertical thin bodies, wherein the transistor structure having the plurality of vertical thin bodies can not only effectively reduce the leakage current path of the transistor in a closed state, but also greatly increase the conduction current of the transistor in a conducting state. Background Art

[0002] The single-chip integration of silicon integrated circuits has achieved more than 50 billion transistors on a single die in 2021, which is called the transition from the Very Large Scale Integration (VLSI) era (more than millions of transistors on a single die) to the Gigabit-Scale Integration (GSI) era (more than billions of transistors on a single die). This achievement of higher integration of transistors on a single die has greatly enabled more powerful microsystems, significantly improved the performance, power, area, and cost (PPAC) of microsystems, and created many powerful chips, such as central processing units (CPUs), graphic processing units (GPUs), field programmable gate arrays (FPGAs), systems on a chip (SOCs), static random-access memory (SRAMs), dynamic random access memory (DRAMs), etc., where these powerful chips can enhance system capabilities and continuously support Moore's Law to lay the foundation for creating exponential economic growth.

[0003] Since giant scale integrated circuits generate such high productivity to develop new applications, thus stimulating rapid growth in economic scale, there is a strong demand for integrating more transistors in one die. Therefore, it is expected that the semiconductor industry will do its best to move towards the TSI (Tera-Scale Integration) era, that is, integrating more than trillions of transistors on one die. Therefore, how to significantly improve transistors to meet this TSI challenge requires the invention and engineering improvements of some transistor structures that have fundamental changes in performance, power consumption, area and cost. For example, if 1 trillion transistors are indeed integrated on a die, and each transistor is set to have a standby current Ioff (or called shutdown current Ioff) of about 0.5 picoamperes (pA), then the standby current Ioff of 1 trillion transistors will be close to 0.5 amperes.

[0004] However, it is difficult for the most advanced transistors using technology less than 20 nanometers (nm) to achieve a standby current Ioff of 0.5 pA. Even if various transistor structures (such as Fin Field-Effect Transistor (FinFET) or three-gate transistor designs) are used, the standby current Ioff of some transistor structures is still as high as 5 to 10 pA. Therefore, how to continuously reduce the size of transistors and reduce their standby current Ioff (for example, below 1 pA) is a key challenge for the semiconductor industry.

[0005] Figure 1 is a schematic diagram illustrating a fin field effect transistor (FinFET) having an active region formed into a fin structure in the prior art. Figure 1As shown, the gate structure 5 of the fin field effect transistor is formed above the fin structure or a three-dimensional convex silicon surface, and the gate structure 5 includes some conductive materials (such as metal, polysilicon, or polysiliconide (polyside), etc.) on an insulator or dielectric layer (such as oxide, oxide / nitride, or some high-k materials, etc.). Taking an N-type metal-oxide-semiconductor (MOS) transistor as an example, the source region 11 and the drain region 12 of the fin field effect transistor are formed by implanting high-concentration n-type (n+) dopants into a p-type substrate (or p-well) through ion implantation plus thermal annealing technology, thereby forming two separated heavily doped n+ / p junctions (n+ / p junctions) in the p-type substrate (or p-well). In addition, in order to reduce impact ionization and hot carrier injection in front of the heavily doped n+ / p junction, n- lightly doped-drains (LDD) 13 are usually formed in front of the source region 11 and the drain region 12 by ion implantation plus thermal annealing technology. Figure 1 As shown, such ion implantation plus thermal annealing technique often results in the lightly doped drain 13 penetrating into the portion of the active region below the gate structure 5. Therefore, the length of the effective channel 14 between the lightly doped drains 13 is inevitably shortened.

[0006] On the other hand, the progress of process technology is continuously and rapidly shrinking the geometric size of the N-type metal oxide semiconductor transistor in horizontal and vertical directions (for example, the minimum feature size called Lamda (λ) has been reduced from 28 nanometers (nm) to 5nm or 3nm). However, due to the shrinking geometric size of the fin field effect transistor (FinFET), the following problems are caused or made worse:

[0007] (1) As the length of the gate structure 5 decreases, it becomes increasingly difficult to reduce the standby current Ioff. Figure 2 The fin structure is formed in the fin structure, rather than only along the surface of the fin structure. Figure 3 Is to describe the evaluation and simulation Figure 2 The schematic diagram of the leakage current path is shown in Figure 3 (a) is the structure of a 3D fin field effect transistor simulated by Technology Computer-Aided Design (TCAD). Figure 3 (b) corresponds to Figure 3 (a) is a cross-sectional view of the structure of the 3D FinFET as shown in the red dashed rectangle 18, and Figure 3 (c) is the current distribution of the 3D fin field effect transistor when it is in the off state (that is, the standby current Ioff) (see "Impact of Current Flow Shape in Tapered (Versus Rectangular) FinFET on Threshold Voltage Variation Induced by Work-Function Variation", IEEE TRANSACTIONS ON ELECTRON DEVICES, VOL. 61, NO. 6, JUNE 2014).

[0008] (2) Because the dimensions in both the horizontal and vertical directions must be reduced simultaneously, it is increasingly difficult to perfectly align the junction edge of the lightly doped drain 13 (or the edge of the source region 11 / drain region 12) with the edge of the gate structure 5 using only the conventional self-alignment method formed by the gate, spacer, and ion implantation. In addition, the thermal annealing technique used to eliminate the damage caused by the ion implantation must rely on high temperature processing techniques (e.g., rapid thermal annealing methods using various energy sources or other thermal processes). One problem derived from this is that although the gate-induced drain leakage (GIDL) current should be minimized to reduce the leakage current, the generation of the gate-induced drain leakage current is difficult to control. Another problem derived from this is that because the length of the effective channel 14 is difficult to control, the short channel effect (SCE) is difficult to minimize. In addition, the relative position between the edge of the source region 11 / drain region 12 and the edge of the gate structure 5 is also difficult to adjust to control the gate-induced drain leakage (GIDL) current.

[0009] (3) In addition, since the ion implantation for forming the lightly doped drain 13 (or the n+ / p junction in an N-type metal oxide semiconductor transistor or the p+ / n junction in a P-type metal oxide semiconductor transistor) is similar to bombardment so as to inject ions directly from the top of the silicon surface downward into the substrate, it is difficult to create a uniform material interface with low defects from the source region 11 and the drain region 12 to the effective channel 14 and the substrate-body region (because the distribution of the doping concentration in the vertical direction is non-uniform, for example, in the vertical direction is from the top surface with a higher doping concentration to the junction with a lower doping concentration).

[0010] (4) In addition, when the size in the horizontal direction is reduced to 7nm, 5nm or 3nm, the height of the fin structure of the N-type metal oxide semiconductor transistor (for example, 40 to 100nm) is much larger than the width of the fin structure of the N-type metal oxide semiconductor transistor (for example, 3 to 10nm), thereby making the fin structure of the N-type metal oxide semiconductor transistor very fragile or even collapsed in the subsequent process (for example, forming the source region 11 / drain region 12, or the gate structure 5, etc.).

[0011] Therefore, the present invention discloses a new 3D transistor structure to solve the above-mentioned disadvantages of the FinFET. For example, the new 3D transistor structure can reduce the standby current Ioff by 10 to 100 times. Summary of the invention

[0012] An embodiment of the present invention provides a transistor structure. The transistor structure includes a body, a gate structure, a source region and a drain region. The body has a single convex structure, wherein the single convex structure is made of a first semiconductor material and a groove is formed in the single convex structure. The gate structure has a gate conductive layer and a gate dielectric layer, wherein the gate conductive layer spans over the single convex structure and a portion of the gate conductive layer fills the groove. The source region contacts the first end of the single convex structure. The drain region contacts the second end of the single convex structure. The ratio of the on-current (Ion) to the off-current (Ioff) of the transistor structure is not less than 10 6 .

[0013] In one embodiment of the present invention, the on-current / off-current ratio of the transistor structure is about 1 to 10×10 6 .

[0014] In one embodiment of the present invention, the single convex structure includes a first outer side wall and a second outer side wall covered by the gate conductive layer, and the single convex structure also includes a first inner side wall and a second inner side wall located in the groove, and the length of the first inner side wall or the second inner side wall is shorter than the length of the first outer side wall or the second outer side wall.

[0015] In one embodiment of the present invention, the bottom surface and sidewalls of the trench are covered by the gate dielectric layer, and the bottom of the gate conductive layer outside the single convex structure is lower than the bottom of a portion of the gate conductive layer.

[0016] In one embodiment of the present invention, the single convex structure includes two vertical thin bodies, the gate dielectric layer is disposed between the gate conductive layer and the two vertical thin bodies, and the width of one of the two vertical thin bodies is no greater than 3 nanometers.

[0017] In one embodiment of the present invention, the transistor structure further comprises a first recess and a second recess. The first recess is used to accommodate the source region. The second recess is used to accommodate the drain region. The sidewalls of the first recess and the sidewalls of the second recess are surrounded by a shallow trench isolation (STI) region, the edge of the source region contacts the two vertical thin bodies, and the edge of the drain region contacts the two vertical thin bodies.

[0018] In one embodiment of the present invention, the source region includes a lightly doped drain (LDD) region, a heavily doped region and a metal region. The lightly doped drain region contacts the two vertical thin bodies. The heavily doped region extends laterally from the lightly doped drain region. The metal region contacts the top surface and sidewalls of the heavily doped region.

[0019] One embodiment of the present invention provides a transistor structure. The transistor structure includes a body, a gate structure, a source region and a drain region. The body has a single convex structure with an original surface, wherein the body is made of a semiconductor material and the single convex structure has multiple conductive channels. The source region is in contact with the first end of the single convex structure. The drain region is in contact with the second end of the single convex structure. The gate structure has a gate conductive layer, wherein the gate conductive layer spans over the single convex structure, the first portion of the gate conductive layer is located in the single convex structure and below the original surface, and the second portion of the gate conductive layer is located above the original surface. The subthreshold slope (SS) of the transistor structure is not greater than 74.

[0020] In one embodiment of the present invention, the subthreshold slope of the transistor is between 71 and 74.

[0021] In one embodiment of the present invention, the length of the second portion of the gate conductive layer is greater than the length of the first portion of the gate conductive layer, and a groove is formed in the single convex structure and located between the first end of the single convex structure and the second end of the single convex structure.

[0022] In one embodiment of the present invention, the single convex structure includes two upwardly extending thin bodies, each thin body includes two conductive channels along the side walls of each thin body, and a trench filled with the first portion of the gate conductive layer is located between the two upwardly extending thin bodies.

[0023] In one embodiment of the present invention, the transistor structure further includes a gate dielectric layer spanning over the convex structure, wherein a first portion of the gate conductive layer is surrounded by the gate dielectric layer in the trench, and the gate conductive layer is surrounded by the gate dielectric layer along the four side walls and bottom of the trench.

[0024] In one embodiment of the present invention, the semiconductor material of the body is directly below the bottom of the trench, and the gate dielectric layer along the bottom of the trench is in direct contact with the semiconductor material of the body.

[0025] In an embodiment of the present invention, the transistor structure further includes a spacer sandwiching the sidewall of the single convex structure, and a shallow trench isolation region surrounding the spacer.

[0026] One embodiment of the present invention provides a transistor structure. The transistor structure includes a semiconductor body, a gate conductive layer, a gate dielectric layer, a source region and a drain region. The semiconductor body has a single convex structure. The gate dielectric layer spans over the single convex structure, and the single convex structure includes at least 4 conductor-oxide-semiconductor interfaces extending upward. The source region contacts the first end of the single convex structure. The drain region contacts the second end of the single convex structure. The on-state current (Ion) of the transistor structure is not less than 90uA.

[0027] In one embodiment of the present invention, an off current (Ioff) of the transistor structure is no greater than 90 pA.

[0028] In one embodiment of the present invention, the single convex structure includes two upwardly extending thin bodies, each of the upwardly extending thin bodies includes two upwardly extending conductor-oxide-semiconductor interfaces, and a groove is formed in the single convex structure to separate the two upwardly extending thin bodies.

[0029] In one embodiment of the present invention, the at least four upwardly extending conductor-oxide-semiconductor interfaces are horizontally displaced from each other, and there is no shallow trench isolation region between the two upwardly extending thin bodies.

[0030] In one embodiment of the present invention, the threshold voltage (Vth) of the transistor structure is between 330mv and 360mv.

[0031] In one embodiment of the present invention, the transistor structure further includes a spacer layer, wherein the spacer layer is adjacent to the gate conductive layer and spans across the top surface and sidewalls of the single convex structure. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] Figure 1is a schematic diagram illustrating a finfield-effect transistor (FinFET) having an active region formed as a fin structure in the prior art.

[0033] Figure 2 is a schematic diagram illustrating a higher leakage current path formed within a fin structure.

[0034] Figure 3 It is a diagram illustrating the structure of a 3D FinFET under Technology Computer-Aided Design (TCAD) simulation, a cross-sectional view of the structure of the 3D FinFET, and a schematic diagram of current distribution of the 3D FinFET in an off state.

[0035] Figure 4A It is a flow chart of a method for manufacturing a vertical thinbody field-effect transistor (VTBFET) disclosed in one embodiment of the present invention.

[0036] Figure 4B , Figure 4C , Figure 4D , Figure 4E Yes Description Figure 4A Schematic diagram of .

[0037] Figure 5 is a schematic diagram illustrating growing a pad oxide layer, depositing a pad nitride layer, and forming a trench.

[0038] Figure 6 is a schematic diagram illustrating depositing an oxide spacer layer on a p-type well and then depositing a nitride spacer layer on the oxide spacer layer.

[0039] Figure 7 is a schematic diagram illustrating the formation of shallow trench isolation regions and the deposition of a nitride layer.

[0040] Figure 8 It is a schematic diagram illustrating that the gate region spans across the active region and the shallow trench isolation region.

[0041] Fig. 9 is a schematic diagram illustrating the removal of the lithography mask.

[0042] Fig.10 1 is a schematic diagram for explaining the formation of a carbon silicon oxide spacer-2 layer and the formation of a recess (or a groove) based on the carbon silicon oxide spacer-2 layer.

[0043] Fig.11 is a schematic diagram illustrating forming a dielectric layer to fill a recess to form a central electrode, and then forming a nitride cap layer over the central electrode.

[0044] Fig.12 is a schematic diagram illustrating etching back the exposed shallow trench isolation region to form the vertical convex structure in the defined gate region.

[0045] Fig.13 is a schematic diagram illustrating the use of etching to remove the nitride cap and carbon silicon oxide spacer-2 layer near the center pole correlation region.

[0046] Fig.14 It is a schematic diagram for explaining the removal of the liner oxide layer near the center pole related area and the oxide spacer layer covering the convex structure, and etching the shallow trench isolation area corresponding to the center pole related area.

[0047] Fig.15 is a schematic diagram illustrating that the center pole is removed to expose the groove-2.

[0048] Fig.16 is a schematic diagram illustrating forming a gate dielectric layer and depositing a gate conductive material in a gate region.

[0049] Fig.17 is a schematic diagram illustrating deposition of a cap layer and etching of shallow trench isolation regions.

[0050] Fig.18 It is a schematic diagram for explaining etching away the pad nitride layer and the pad oxide layer, etching back a portion of the shallow trench isolation region, and forming an oxide spacer-2 layer and a nitride spacer-2 layer on the edge of the gate region.

[0051] Fig.19 is a schematic diagram illustrating etching away some exposed silicon to form shallow trenches for source and drain regions of the vertical thin body field effect transistor, growing an oxide-3 layer using a thermal oxidation process, and depositing nitride thereon using a chemical vapor deposition technique and etching back the nitride.

[0052] Fig. 20 is a schematic diagram illustrating depositing a tungsten layer and then depositing a titanium nitride layer over the tungsten layer.

[0053] Fig.21 is a schematic diagram illustrating etching away the oxide-3V layer to expose the silicon sidewall, then forming an n-type lightly doped drain, an n+ doped source and an n+ doped drain, and then depositing a titanium nitride layer and a tungsten layer.

[0054] Fig. 22 is a schematic diagram illustrating that a bonding pad is formed on an n+ doped source and an n+ doped drain.

[0055] Fig.23 is a schematic diagram illustrating a simulation result of a computer-aided design of a conventional fin field effect transistor and a vertical thin-body field effect transistor regarding on-state current.

[0056] Fig.24 is a schematic diagram illustrating a simulation result of a computer-aided design of the off current of a conventional fin field effect transistor and a vertical thin-body field effect transistor.

[0057] Fig.25 is a schematic diagram illustrating the structural difference between the conventional fin field effect transistor and the vertical thin-body field effect transistor.

[0058] Fig.26A and Fig.26B It is a flow chart of a method for manufacturing a novel vertical thin body field effect transistor (NuVTBFET) disclosed in another embodiment of the present invention.

[0059] Fig. 27 , Fig.28 , Fig.29 , Fig.30 , Fig.31 is a schematic diagram illustrating definition of a gate region on a fin structure.

[0060] Fig.32 and Fig.33 is a schematic diagram illustrating the formation of a source region and a drain region.

[0061] Fig.34 , Fig.35 , Fig.36 , Fig.37 is a schematic diagram illustrating forming a gate structure in the gate region. Fig.38 and Fig.39 Schematic diagram illustrating that a novel vertical thin body field effect transistor (NuVTBFET) has three vertical gate conductive portions connecting a top portion of a work function metal and a tungsten layer.

[0062] The reference numerals are described as follows:

[0063] 5. Gate structure

[0064] 11 Source

[0065] 12 Drain region

[0066] 13 n-lightly doped drain

[0067] 14 Valid channels

[0068] 16 Dashed rectangular area

[0069] 18 Red dotted rectangle

[0070] 200 Semiconductor substrate

[0071] 202 p-type well

[0072] 204 Pad Oxide Layer

[0073] 206 pad nitride layer

[0074] 304 Oxidation Spacer

[0075] 306 Nitrided spacer

[0076] 402 Shallow Trench Isolation Area

[0077] 802, 15062, 1904 Nitride layer

[0078] 902 Micro-Shadow Mask

[0079] 904, 1202 Depression

[0080] 1102 Carbon Silicon Oxide Spacer - 2 Layers

[0081] 1302, 2702 center pole

[0082] 1402 Nitride Cap Layer

[0083] 1501 Groove-2

[0084] 1502 Gate dielectric layer

[0085] 1504 Gate Conductive Material

[0086] 15042 Top gate conductive part 1506 cap layer 15064 Hard mask oxide layer

[0087] 1802 Oxide Spacer - 2 layers 1804 Nitride Spacer - 2 layers 1902 Shallow Groove

[0088] 1002 Oxide-3 layers

[0089] 10022 Oxide-3V layer

[0090] 10024, 3302 Oxide-3B layer

[0091] 1906, 2014, 2806, 3304, 3706 Tungsten layer

[0092] 1908, 2012, 3301 Titanium nitride layer

[0093] 2002 Silicon Sidewall

[0094] 2004, 2006, 3308 n-type lightly doped drain

[0095] 2008, 3306 n+ doped source

[0096] 2010 N+ doped drain

[0097] 2102, 2104, 2106, 2108 Conductor-Oxide-Semiconductor Structures 2202 Joint pad

[0098] 2502, 2504, 2506, 2508 N+ zone

[0099] 2704 Amorphous Silicon Carbide Layer

[0100] 2706 Anti-penetration layer

[0101] 2802 Polysilicon layer

[0102] 2902, 3202 Carbon silicon oxide layer

[0103] 2904, 3204, 3310 Oxide layer

[0104] 3102, 3502 High-k dielectric layer

[0105] 3104 Pseudo gate conductive layer

[0106] 3106 Gate Covering Layer

[0107] 3504 Metal Pole

[0108] 3702 Hard Mask Oxide Layer

[0109] 3704 Pad

[0110] 3708, 3710 Work function metal A, B length

[0111] AA, BB cross-section

[0112] G1~G3 vertical gate conductive part Leff effective channel length OHS Original Horizontal Surface STI Shallow Trench Isolation Sright, Sleft, VTB vertical thin body

[0113] 10-50, 102-154, 2602-2624 steps DETAILED DESCRIPTION

[0114] Please refer to Figure 4A , Figure 4B , Figure 4C , Figure 4D , Figure 4E , Figure 5 , Figure 6 , Figure 7 , Figure 8 , Fig. 9 , Fig.10 , Fig.11 , Fig.12 , Fig.13 , Fig.14 , Fig.15 , Fig.16 , Fig.17 , Fig.18 , Fig.19 , Fig. 20 , Fig.21 , Fig. 22 ,in Figure 4A is a flow chart of a method for manufacturing a vertical thin body field-effect transistor (VTBFET) disclosed in one embodiment of the present invention, and Figure 4A The manufacturing method of the vertical thin-body field effect transistor can make the vertical thin-body field effect transistor have lower standby current, lower gate-induced drain leakage (GIDL) current and lower short channel effect (SCE), and can form a solid fence wall to clamp the active region or narrow convex structure of the vertical thin-body field effect transistor. In addition, the detailed steps of the manufacturing method of the vertical thin-body field effect transistor (taking an N-type metal-oxide-semiconductor (MOS) transistor as an example) are as follows:

[0115] Step 10: Start;

[0116] Step 20: On the basis of the semiconductor substrate 200, an active region is defined and a convex structure having a plurality of current conducting channels or a plurality of vertical thin bodies is formed;

[0117] Step 30: forming a gate region of the vertical thin-body field effect transistor;

[0118] Step 40: forming a source region and a drain region of the vertical thin-body field effect transistor;

[0119] Step 50: End.

[0120] Please refer to Figure 4B , Figure 4C , Figure 5 , Figure 6 , Figure 7 , Figure 8 , Fig. 9 , Fig.10 , Fig.11 , Fig.12 , Fig.13 , Fig.14 , Fig.15 Step 20 includes:

[0121] Step 102: Generate a pad oxide layer 204 and deposit a pad nitride layer 206;

[0122] Step 104: defining the active region by using a photolithographic mask technique, and removing a portion of the semiconductor material (eg, silicon) outside the active region to form the convex structure;

[0123] Step 106: depositing a nitride spacer 306 (or an oxide spacer 304 and a nitride spacer 306) to surround the active region, and etching back the nitride spacer 306 (or an oxide spacer 304 and a nitride spacer 306);

[0124] Step 108: Deposit an oxide layer and use chemical mechanical polishing (CMP).

[0125] Using CMP (Chemical Processing) technology to remove excess oxide layer to form shallow trench isolation (STI) region 402;

[0126] Step 110: depositing a thin nitride layer 802;

[0127] Step 112: using a lithography mask 902 to define a gate region spanning the active region and above the shallow trench isolation region 402, and etching away the nitride layer 802 and the pad nitride layer 206 corresponding to the gate region;

[0128] Step 114: Remove the lithography mask 902, wherein a central pole correlation region is defined in the active region.

[0129] (central pole related area);

[0130] Step 116: depositing a carbon silicon oxide (SiCOH) layer (or a combination of an oxide layer / nitride layer) to form a carbon silicon oxide spacer-2 layer 1102;

[0131] Step 118: Based on the carbon silicon oxide spacer-2 layer 1102 and the nitride layer 802, a depression (or groove) 1202 is formed in the convex structure by using anisotropic etching technique;

[0132] Step 120: forming a dielectric layer (e.g., thermal oxide) as a center pole 1302 to fill the recess 1202; Step 122: depositing a nitride-3 layer and etching back the nitride-3 layer to form a nitride cap layer 1402; Step 124: etching back the exposed shallow trench isolation region 402 to establish the convex structure in the gate region;

[0133] Step 126: removing the nitride layer 802, the nitride spacer layer 306, the nitride cap layer 1402 and the carbon silicon oxide spacer-2 layer 1102 near the center pole related area;

[0134] Step 128: Remove the oxide spacer layer 304, the center pole 1302 and the liner oxide layer 204 near the center pole related area.

[0135] Please refer to Figure 4D , Fig.16 , Fig.17 , Fig.18 Step 30 comprises:

[0136] Step 130: forming a gate dielectric layer 1502 in the gate region;

[0137] Step 132: depositing a gate conductive material 1504 in the gate region, and then etching back the gate conductive material 1504;

[0138] Step 134: forming a cap layer 1506 and polishing the cap layer 1506 by the chemical mechanical polishing technique; Step 136: etching back the shallow trench isolation region 402;

[0139] Step 138: Etch away the pad nitride layer 206 and the pad oxide layer 204 to expose the original horizontal surface

[0140] (original horizontal surface)OHS;

[0141] Step 140: Form an oxide spacer-2 layer 1802 and a nitride spacer-2 layer 1804 on the edges of the gate conductive material 1504 and the cap layer 1506.

[0142] Please refer to Figure 4E , Fig.19 , Fig. 20 , Fig.21 , Fig. 22 Step 40 comprises:

[0143] Step 142: Etching away the exposed silicon;

[0144] Step 144: thermally grow oxide-3 layer 1002;

[0145] Step 146: forming a nitride layer 1904;

[0146] Step 148: forming a tungsten layer 1906;

[0147] Step 150: forming a titanium nitride (TiN) layer 1908;

[0148] Step 152: Etching away a portion of the oxide-3 layer 1002;

[0149] Step 154 ​​: forming n-type lightly doped drains (LDD) 2004 and 2006 , and then forming n+ doped source 2008 and n+ doped drain 2010 .

[0150] The detailed description of the above manufacturing method is as follows. Taking an N-type metal oxide semiconductor transistor as an example, it starts from a well-designed doped p-type well 202 mounted in a semiconductor substrate 200 (for example, in a p-type semiconductor substrate) (wherein in another embodiment of the present invention, it can start from the semiconductor substrate 200 instead of the p-type well 202), wherein in one embodiment of the present invention, the top surface of the p-type well 202 is about 500nm thick from the original horizontal surface OHS. In addition, for example, the semiconductor substrate 200 has a concentration close to 1x1016 dopant / cm3, but the actual doping concentration will be determined by the final mass production optimization.

[0151] In step 102, if Figure 5 As shown in FIG. 5( a ), a pad oxide layer 204 with a well-designed thickness is grown above the original horizontal surface OHS, and a pad nitride layer 206 with a well-designed thickness is deposited above the top surface of the pad oxide layer 204 .

[0152] In step 104, if Figure 5 As shown in (a), the active region of the vertical thin-body field effect transistor is defined by the anisotropic etching technology using the lithography mask technology, wherein the anisotropic etching technology removes part of the semiconductor material (e.g., silicon) outside the active region to form a trench (e.g., about 300 nanometers (nm) deep) to meet the needs of future shallow trench isolation regions 402, thereby also creating a convex structure of the active region. In addition, Figure 5 (b) is related to Figure 5 (a) The corresponding top view, where Figure 5 (a) is along Figure 5 (b) is a cross-sectional view taken along the X-direction cutting line.

[0153] In step 106, if Figure 6As shown in (a), an oxide spacer 304 is deposited at the edge of the active region, and then a nitride spacer 306 is deposited on the oxide spacer 304 (or the nitride spacer 306 is only deposited at the edge of the active region), and the anisotropic etching technology is used to etch back the oxide spacer 304 and the nitride spacer 306 so that the top surfaces of the oxide spacer 304 and the nitride spacer 306 are flush with the original horizontal surface OHS, wherein the oxide spacer 304 and the nitride spacer 306 are located outside the active region. Therefore, the key to step 106 is that the oxide spacer 304 and the nitride spacer 306 (or only the nitride spacer 306) form a solid fence wall (i.e., an isolation wall) to clamp the active region or the narrow convex structure, especially the sidewall of the convex structure. In addition, the strong fence wall can be a single layer (e.g., nitride spacer 306) or other composite layers (e.g., oxide spacer 304 and nitride spacer 306) to protect the narrow convex structure or the fin structure from collapsing during the formation of the source / drain or gate region of the vertical thin body field effect transistor.

[0154] In step 108, if Figure 7 As shown in (a), a thick oxide layer is deposited to completely fill the trench surrounding the active region, and the excess oxide layer is removed using the chemical mechanical polishing technique to form a shallow trench isolation region 402, wherein the top surface of the shallow trench isolation region 402 is flush with the top surface of the pad nitride layer 206. Similarly, the shallow trench isolation region 402 further surrounds or clamps the active region or the narrow convex structure, especially the sidewall of the convex structure, to protect the narrow convex structure from collapse during the formation of the source / drain or gate region of the vertical thin body field effect transistor.

[0155] In step 110, if Figure 7 As shown in (a), a nitride layer 802 is deposited on the pad nitride layer 206 and the shallow trench isolation region 402. In addition, Figure 7 (b) is related to Figure 7 (a) The corresponding top view, where Figure 7 (a) is along Figure 7 (b) is a cross-sectional view taken along the X-direction cutting line.

[0156] In step 112, if Figure 8 As shown in (a), a lithography mask 902 is used to define a gate region across the active region and above the shallow trench isolation region 402, thereby removing the nitride layer 802 and the liner nitride layer 206 corresponding to the gate region to form a recess 904. In addition, Figure 8 (b) is related to Figure 8 (a) The corresponding top view, where Figure 8 (a) is along Figure 8(b) is a cross-sectional view of the X-direction cutting line and Figure 8 (c) is along Figure 8 (b) is a cross-sectional view taken along the Y direction cutting line.

[0157] In step 114, if Fig. 9 As shown in (a), the lithography mask 902 is removed. In this way, a smooth edge of the gate region for the vertical thin-body field effect transistor is achieved, and the center pole related region is also defined in the active region, wherein the smooth edge is the edge of the nitride layer 802 and the liner nitride layer 206. In addition, Fig. 9 (b) is related to Fig. 9 (a) The corresponding top view, where Fig. 9 (a) is along Fig. 9 (b) is a cross-sectional view taken along the X-direction cutting line.

[0158] In step 116, if Fig.10 As shown in (a), the carbon silicon oxide layer (or the combination of the oxide layer / the nitride layer) is deposited in the central pole related area and etched back to form a carbon silicon oxide spacer-2 layer 1102 (wherein, for example, the width of the carbon silicon oxide spacer-2 layer 1102 may be 1-3 nm). Fig.10 As shown in (b), the carbon silicon oxide spacer-2 layer 1102 is located on the four surrounding edges within the central pole related area, and the carbon silicon oxide spacer-2 layer 1102 is used to protect the original silicon area below, wherein the original silicon area below the carbon silicon oxide spacer-2 layer 1102 serves as a surrounding ring of silicon (or surrounding Si ring) on ​​the central pole (SRS-CP) generated later.

[0159] In step 118, if Fig.10 As shown in (a), based on the carbon silicon oxide spacer-2 layer 1102 and the nitride layer 802, the anisotropic etching technology is used to etch the pad oxide layer 204 in the center pole related area and the semiconductor material of the semiconductor substrate 200 to form a depression (or groove) 1202 with a depth of about 50 to 80 nm (for example, 75 nm) in the exposed silicon area. That is, the carbon silicon oxide spacer-2 layer 1102 and the nitride layer 802 act as a mask so that the exposed pad oxide layer 204 in the center pole related area is removed and the exposed silicon is also removed about 75 nm deep to form a depression 1202 in the center pole related area. Therefore, the carbon silicon oxide spacer-2 layer 1102 acts like a rain cover to protect the silicon surrounding ring (SRS-CP) to be created. In addition, Fig.10 (b) is related to Fig.10(a) The corresponding top view, where Fig.10 (a) is along Fig.10 (b) is a cross-sectional view of the X-direction cutting line and Fig.10 (c) is along Fig.10 (b) is a cross-sectional view taken along the Y direction cutting line.

[0160] In step 120, if Fig.11 As shown in (a), the dielectric layer is formed (for example, by short-time growth of thermal oxide or chemical vapor deposition (CVD) deposition) as a central pole 1302 to fill the recess 1202, wherein the central pole 1302 is also called a central oxide pole or a column pole (CP).

[0161] In step 122, if Fig.11 As shown in (a), the nitride-3 layer is then deposited and etched back to form a nitride cap layer 1402 above the central pole 1302 to protect the central pole 1302. In addition, Fig.11 (b) is related to Fig.11 (a) The corresponding top view, where Fig.11 (a) is along Fig.11 (b) is a cross-sectional view of the X-direction cutting line and Fig.11 (c) is along Fig.11 (b) is a cross-sectional view taken along the Y direction cutting line.

[0162] In step 124, if Fig.12 As shown in (a), the exposed shallow trench isolation region 402 is etched back to a depth of about 50 to 80 nm to form a vertical convex structure in the defined gate region, wherein, for example, the shallow trench isolation region 402 in the defined gate region is etched down by about 75 nm (i.e., the height of the convex structure). In one embodiment of the present invention, the height of the convex structure is the same or substantially the same as the height of the center pole 1302 calculated from the original horizontal surface OHS of the p-type well 202 to the bottom of the center pole 1302. In addition, Fig.12 (b) is related to Fig.12 (a) The corresponding top view, where Fig.12 (a) is along Fig.12 (b) is a cross-sectional view taken along the Y direction cutting line.

[0163] In step 126, if Fig.13As shown in (a), etching is used to remove the nitride cap 1402 and the carbon silicon oxide spacer-2 layer 1102 near the central pole related area, the nitride layer 802, and the nitride spacer layer 306 covering the convex structure in the defined gate area. In this way, the previously defined central pole related area appears again. In addition, Fig.13 (b) is related to Fig.13 (a) The corresponding top view, where Fig.13 (a) is along Fig.13 (b) is a cross-sectional view of the X-direction cutting line and Fig.13 (c) is along Fig.13 (b) is a cross-sectional view taken along the Y direction cutting line.

[0164] In step 128, if Fig.14 As shown in (a), the liner oxide layer 204 near the center pole related area and the oxide spacer 304 covering the convex structure are removed by etching. The shallow trench isolation region 402 defined outside the gate region can also be etched a certain amount (for example, about 40 to 80 nm deep), so that the top surface of the shallow trench isolation region 402 defined outside the gate region is lower than the top surface of the liner nitride layer 206. Therefore, Fig.14 As shown in (c), the two outer sides of the single crystal silicon of the convex structure are exposed. More importantly, Fig.14 As shown in (b), there is the silicon surrounding ring (SRS-CP) on the central pole 1302. In addition, Fig.14 (b) is related to Fig.14 (a) The corresponding top view, where Fig.14 (a) is along Fig.14 (b) is a cross-sectional view of the X-direction cutting line and Fig.14 (c) is along Fig.14 (b) is a cross-sectional view taken along the Y direction cutting line.

[0165] Afterwards, if Fig.15 As shown in (a), the center pole 1302 is removed to expose the groove-2 1501. Fig.15 As shown in (c), in the convex structure, there are two vertical thin bodies Sright and Sleft for conducting current during the on-state of the vertical thin body field effect transistor, wherein the vertical thin body Sright has an outer side wall and an inner side wall adjacent to the trench-2 1501, and the vertical thin body Sleft is also the same. Fig.15 As shown in (c), in the groove-2 1501, the inner side wall of the vertical thin body Sright faces the inner side wall of the vertical thin body Sleft. In addition, Fig.15 (b) is related to Fig.15 (a) The corresponding top view, where Fig.15 (a) is along Fig.15(b) is a cross-sectional view of the X-direction cutting line and Fig.15 (c) is along Fig.15 (b) is a cross-sectional view taken along the Y direction cutting line.

[0166] In step 130, if Fig.16 As shown in (a), a gate dielectric layer (such as a high dielectric (high K) material or oxide) 1502 is then formed in the defined gate region.

[0167] In step 132, if Fig.16 As shown in (a), a gate conductive material (such as polysilicon, or a metal such as tungsten on a titanium nitride layer, or other metals with a suitable work function) 1504 is then deposited in the gate region, and the excess gate conductive material 1504 is removed using the chemical mechanical polishing technique, and then the gate conductive material 1504 is etched back / polished. Of course, in the presence of a gate last process, the previously formed gate conductive material 1504 can be removed and replaced with other suitable gate conductive materials. The portion of the gate conductive material 1504 in the trench-2 1501 can be referred to as a "conductive central pole", and the conductive central pole is surrounded by the gate dielectric layer 1502 in the trench-2 1501. In addition, Fig.16 (b) is related to Fig.16 (a) The corresponding top view, where Fig.16 (a) is along Fig.16 (b) is a cross-sectional view of the X-direction cutting line and Fig.16 (c) is along Fig.16 (b) is a cross-sectional view taken along the Y direction cutting line.

[0168] In step 134, if Fig.17 As shown in (a), a cap layer 1506 composed of a nitride layer 15062 and a hard mask oxide layer 15064 is then deposited in the gate region on the top surface of the gate conductive material 1504, wherein the cap layer 1506 is used to protect the gate conductive material 1504. Then, the cap layer 1506 is polished by the chemical mechanical polishing technique so that the top surface of the cap layer 1506 is flush with the top surface of the pad nitride layer 206.

[0169] In step 136, if Fig.17 As shown in (a), the shallow trench isolation region 402 is then etched (if there is a gate dielectric layer 1502 above the shallow trench isolation region 402, it is also etched together) to make the top surface of the shallow trench isolation region 402 flush with the top surface of the liner oxide layer 204. In addition, Fig.17 (b) is related to Fig.17(a) The corresponding top view, where Fig.17 (a) is along Fig.17 (a) is a cross-sectional view taken along the X-direction cutting line.

[0170] In step 138, if Fig.18 As shown in (a), the pad nitride layer 206 and the pad oxide layer 204 are etched away to expose the original horizontal surface OHS. In addition, a portion of the shallow trench isolation region 402 is etched back to make the top surface of the shallow trench isolation region 402 flush with the original horizontal surface OHS.

[0171] In step 140, if Fig.18 As shown in (a), an oxide-2 layer is then deposited on the edge of the gate material 1504 and the cap layer 506 to form an oxide spacer-2 layer 1802 and a nitride-2 layer is deposited to form a nitride spacer-2 layer 1804 on the edge of the gate material 1504 and the cap layer 506. In addition, Fig.18 (b) is related to Fig.18 (a) The corresponding top view, where Fig.18 (a) is along Fig.18 (b) is a cross-sectional view taken along the X-direction cutting line.

[0172] In step 142, if Fig.19 As shown in (a), some of the exposed silicon in the active region is then etched away to form shallow trenches 1902 (eg, about 50 nm to 60 nm deep) for the source and drain regions of the vertical thin-body field effect transistor.

[0173] In step 144, if Fig.19 As shown in (a), a thermal oxidation process called oxide-3 process is used to grow oxide-3 layer 1002 (including oxide-3V layer 10022 (assuming a sharp crystal direction (110)) penetrating the vertical sidewalls of the vertical thin body field effect transistor body and oxide-3B layer 10024 above the bottom of the shallow trench 1902. Since some sidewalls of the shallow trench 1902 have a vertical composite of oxide spacer-2 layer 1802 and nitride spacer-2 layer 1804, and those sidewalls of the shallow trench 1902 are further surrounded by shallow trench isolation region 402, the oxide-3 process should only grow very little oxide (that is, oxide-3 layer 1002) on these walls, so that the width of the source / drain region of the vertical thin body field effect transistor is practically unaffected by the thermal oxidation process. In addition, oxide-3V layer 10022 and oxide-3B layer 10024 appear Fig.19The thicknesses in (a) and subsequent figures are only for illustration of the present invention, and the geometry of the oxide-3V layer 10022 and the oxide-3B layer 10024 is not proportional to the size of the shallow trench isolation region 402 shown in those figures. For example, the thickness of the oxide-3V layer 10022 and the oxide-3B layer 10024 is about 20-30 nm, but the vertical height of the shallow trench isolation region 402 can be about 200-250 nm. Based on the oxide-3 process, the thickness of the oxide-3V layer 10022 can be very accurately controlled under precisely controlled thermal oxidation temperature, time and growth rate. Since the thermal oxidation process on a well-defined silicon surface results in 40% of the thickness of the oxide-3V layer 10022 being removed, the thickness of the silicon surface (110) exposed in the vertical wall of the body of the vertical thin body field effect transistor and the remaining 60% of the thickness of the oxide-3V layer 10022 are considered as additions to the vertical wall of the body of the vertical thin body field effect transistor. In addition, in one embodiment of the present invention, the edge of the oxide-3V layer 10022 can be aligned or substantially aligned with the edge of the gate region.

[0174] In step 146, if Fig.19 As shown in (a), a nitride is deposited on the top surface of the oxide-3B layer 10024 using the chemical vapor deposition technology, and the nitride is etched back to form a nitride layer 1904. In addition, Fig.19 (b) is related to Fig.19 (a) The corresponding top view, where Fig.19 (a) is along Fig.19 (b) is a cross-sectional view taken along the X-direction cutting line.

[0175] In step 148, if Fig. 20 As shown in (a), tungsten is deposited and etched back to form a tungsten layer 1906 on the top surface of the nitride layer 1904.

[0176] In step 150, if Fig. 20 As shown in (a), titanium nitride is then deposited (e.g., atomic layer deposition (ALD)) and etched back to form a titanium nitride layer 1908 above the top surface of the tungsten layer 1906. In addition, Fig. 20 (b) is related to Fig. 20 (a) The corresponding top view, where Fig. 20 (a) is along Fig. 20 (b) is a cross-sectional view taken along the X-direction cutting line.

[0177] In step 152, if Fig.21As shown in (a), a portion of the oxide-3V layer 10022 is then etched away using the top surface of the titanium nitride layer 1908 as a reference to expose the silicon sidewalls 2002 (having a crystal direction (110)).

[0178] In another embodiment of the present invention, Fig. 20 The step of forming the tungsten layer 1906 and the titanium nitride layer 1908 in the embodiment of the present invention can be omitted, and Fig.21 The portion of the oxide-3V layer 10022 that is etched may use the top surface of the nitride layer 1904 as a reference.

[0179] In step 154, if Fig.21 As shown in (a), a selective growth technique (e.g., selective epitaxy growth (SEG) technique) is then used to form n-type lightly doped drains 2004 and 2006, and then an n+ doped source 2008 and an n+ doped drain 2010 are formed. It is worth mentioning that when forming all the n-type lightly doped drains 2004, 2006, n+ doped source 2008 and n+ doped drain 2010 of the vertical thin-body field effect transistor, ion distribution is not required, and high-temperature thermal annealing is not required to eliminate the damage caused by heavy bombardment when forming the n+ doped source 2008 and the n+ doped drain 2010.

[0180] like Fig.21 As shown in (a), finally, a titanium nitride layer 2012 and a tungsten layer 2014 are deposited (for example, by atomic layer deposition) and the titanium nitride layer 2012 and the tungsten layer 2014 are etched back. In one embodiment of the present invention, Fig.21 As shown in (a), the bottom of the conductive center electrode is lower than the bottom of the oxide-3B layer 10024, and the heights of the n+ doped source 2008 and the n+ doped drain 2010 are approximately 40 to 60 nm.

[0181] In one embodiment of the present invention, the height of the convex structure (about 75 nm) is about 10 to 30 nm (for example, 20 nm) higher than the height of the n+ doped source 2008 and the n+ doped drain 2010 (or the height of the titanium nitride layer 2012 and the tungsten layer 2014). Therefore, the gap between the bottom of the gate region and the n+ doped source 2008 and the n+ doped drain 2010 (or the bottom of the titanium nitride layer 2012 and the tungsten layer 2014) is about 10 to 30 nm (for example, 20 nm). That is, the bottom of the gate region (gate dielectric layer 1502 or gate conductive material 1504) is lower than the bottom of the n+ doped source 2008 and the n+ doped drain 2010 (or the bottom of the titanium nitride layer 2012 and the tungsten layer 2014).

[0182] like Fig.21(c) Fig.21 (c) is a schematic diagram illustrating that the vertical thin-body field effect transistor has three vertical gate conductive portions G1 to G3, wherein the vertical gate conductive portions G1 to G3 are connected by the top gate conductive portion 15042 of the gate conductive material 1504. As described above, the four vertical sidewalls of the convex structure are covered by the gate dielectric layer 1502 and the gate conductive material 1504. In the vertical gate conductive portion G1, the gate conductive material 1504, the oxide (i.e., the gate dielectric layer 1502) and the semiconductor material (i.e., the p-type well 202) form a conductor-oxide-semiconductor structure 2102 along one outer sidewall of the convex structure, wherein the conductor-oxide-semiconductor structure 2102 is similar to a metal-oxide-semiconductor (MOS) structure. Similarly, in the vertical gate conductive portion G3, the gate conductive material 1504, the oxide (i.e., the gate dielectric layer 1502) and the semiconductor material (i.e., the p-type well 202) along the other outer sidewall of the convex structure form a conductor-oxide-semiconductor structure 2104. Similarly, in the vertical gate conductive portion G2 (or the conductive center pole), the gate conductive material 1504, the oxide (i.e., the gate dielectric layer 1502) and the semiconductor material (i.e., the p-type well 202) along the inner sidewall of the convex structure form another two conductor-oxide-semiconductor structures 2106 and 2108. Therefore, there are four conductor-oxide-semiconductor structures (or metal-oxide-semiconductor (MOS) structures) 2102, 2104, 2106 and 2108. According to the present invention, the uniqueness of the above embodiment is that the four conductor-oxide-semiconductor structures 2102, 2104, 2106 and 2108 share a source region and a drain region in the vertical thin-body field effect transistor. However, the present invention can be applied to the convex structure having multiple (e.g., 6 or 8) conductor-oxide-semiconductor structures (or metal-oxide-semiconductor (MOS) structures).

[0183] In another embodiment of the present invention, the material of the vertical gate conductive portion G2 may be different from or the same as the material of the vertical gate conductive portions G1, G3 (or the top gate conductive portion 15042).

[0184] In addition, if Fig.21 As shown in (a), due to the presence of the silicon surrounding ring in the convex structure, the length B of the gate conductive layer above the original horizontal surface OHS is longer than the length A of the conductive center pole. In addition, the lateral length of the outer side wall of the convex structure is greater than the lateral length of the inner side wall of the convex structure. In addition, Fig.21(b) is related to Fig.21 (a) The corresponding top view, where Fig.21 (a) is along Fig.21 (b) is a cross-sectional view of the X-direction cutting line and Fig.21 (c) is along Fig.21 (b) is a cross-sectional view taken along the Y direction cutting line.

[0185] In addition, if Fig. 22 As shown, when the bonding pad 2202 is formed on the n+ doped source 2008 and the n+ doped drain 2010, at least two sides (a side wall and a top) of the n+ doped drain 2010 (or the n+ doped source 2008) are in contact with the titanium nitride layer 2012 / tungsten layer 2014 and the bonding pad 2202. Therefore, the contact resistance of the n+ doped source 2008 and the n+ doped drain 2010 is also reduced accordingly.

[0186] Fig.23 1 is a schematic diagram illustrating a simulation result of a technology computer-aided design (TCAD) of an on-current Ion of a conventional fin field-effect transistor (Fin Field-Effect Transistor, FinFET) and the vertical thin-body field-effect transistor, wherein the conventional fin field-effect transistor ( Fig.23 The middle figure) has a fin width of 8nm, a fin height of 70nm, a gate dielectric layer of 1nm thickness, and the vertical thin-body field effect transistor ( Fig.23 ) has a 1.5 nm vertical thin body Sright, a 1.5 nm vertical thin body Sleft and a 1 nm thick gate dielectric layer covering the vertical thin bodies Sleft and Sright, wherein the central pole (not shown in FIG. Fig.23 ) exists between the vertical thin body Sleft and the vertical thin body Sright. When the work function of the central electrode and / or gate conductive material 1504 is adjusted by using appropriate gate metal materials, the current density of the vertical thin body field effect transistor in the on state (shown by the blue curve) is 7 times the current density of the conventional fin field effect transistor in the on state (shown by the brown dotted line), and the on current Ion of the vertical thin body field effect transistor is approximately 2 times the on current Ion of the conventional fin field effect transistor. It is worth noting that because of the vertical thin body Sleft and the vertical thin body Sright, there are multiple current conduction channels in the vertical thin body field effect transistor.

[0187] on the other hand, Fig.24FIG. 1 is a schematic diagram illustrating the simulation results of the Technology Computer-Aided Design (TCAD) of the off current Ioff of the conventional fin field effect transistor and the vertical thin body field effect transistor. Fig.24 As shown in the right figure of FIG, the current density of the conventional fin field effect transistor in the off state (marked by the brown dotted line) is 14 times the current density of the vertical thin body field effect transistor in the off state (marked by the blue curve), and the off current Ioff of the conventional fin field effect transistor is about 34 times the off current Ioff of the vertical thin body field effect transistor. Thus, compared with the conventional fin field effect transistor, the vertical thin body field effect transistor effectively increases the Ion / Ioff ratio by about 68 times.

[0188] In addition, because the width of the vertical thin body Sleft / vertical thin body Sright is about 1.5-3 nm (that is, the width of the silicon surrounding ring is about 1.5-3 nm), in another embodiment of the present invention, when the n-type lightly doped drains 2004, 2006 and the highly doped semiconductor region (n+ doped source 2008 and n+ doped drain 2010) are selectively grown at a predetermined temperature, the edge of the n-type lightly doped drain 2006 can move laterally to contact the gate dielectric layer 1502, and the same is true for the edge of the n-type lightly doped drain 2004. Therefore, in this embodiment, the effective channel length of the vertical thin body field effect transistor can be shorter than Fig.21 (a) shows the effective channel length (Leff) of the vertical thin-body field effect transistor.

[0189] Fig.25 is a schematic diagram illustrating the structural difference between the conventional fin field effect transistor and the vertical thin body field effect transistor. Fig.25As shown in (a), in the conventional fin field effect transistor, in order to increase the on-current Ion, there are usually two (or more) independent fin structures, and the two (or more) independent fin structures are separated by a shallow trench isolation region, wherein the shallow trench isolation region is located between the two independent fin structures. The gate region (gate dielectric layer and gate conductive layer) will span the two independent fin structures and the shallow trench isolation region therebetween. Then each end of the fin structure provides a seed crystal region for selective epitaxial growth of a lightly doped drain region and a highly doped semiconductor region. In this way, the two N+ regions 2502 and 2504 of the two fin structures are grown separately by selective epitaxial growth (SEG) technology, and because the two N+ regions 2502 and 2504 grown in the conventional fin field effect transistor are not restricted by the shallow trench isolation region, the N+ regions 2502 and 2504 will gradually expand like two independent mushrooms, and finally cause the N+ regions 2502 and 2504 to be connected together. Therefore, Fig.25 The body of the conventional fin field effect transistor in (a) includes two (or more) independent fin structures, each of which has a width of 6nm, the width of the shallow trench isolation region between the two independent fin structures may be 25nm, and the width of the shallow trench isolation region between the conventional fin field effect transistor and another conventional fin field effect transistor is also 25nm. Therefore, Fig.25 The pitch distance between the conventional FinFET and another conventional FinFET in (a) is 62 nm.

[0190] However, if Fig.25 As shown in (b), in one embodiment of the present invention, as mentioned above, only one convex structure is formed based on the semiconductor substrate, and a groove is formed in the convex structure, so that there are two vertical thin bodies. However, there is no shallow trench isolation region between the two vertical thin bodies. Then the gate region (gate dielectric layer and gate conductive layer) will span the two vertical thin bodies and the groove between the two vertical thin bodies, wherein the portion of the gate conductive layer in the groove (that is, the central pole mentioned above) is surrounded by the gate dielectric layer, and in particular, the gate dielectric layer surrounds the central pole along the four side walls and bottom of the groove. The bottom of the groove is still the semiconductor material of the semiconductor substrate. Therefore, there is no shallow trench isolation region between the two vertical thin bodies.

[0191] like Fig.25 As shown in (b), even though there are two vertical thin bodies, due to the presence of the aforementioned silicon surrounding ring, one exposed end of the silicon surrounding ring only provides a seed crystal region for the selective epitaxial growth of the lightly doped drain region and the highly doped semiconductor region, rather than two separate seed crystal regions. Fig.25In the embodiment (b), the N+ region 2506 of the vertical thin-body field effect transistor is as follows: Fig.21 The described method is grown in a recess confined by a shallow trench isolation region by a selective epitaxial growth (SEG) technique. Fig.25 The body of the vertical thin body field effect transistor in (b) only includes a convex structure (or fin structure), and the convex structure has two vertical thin bodies extending upward, each of which has a width of about 1.5nm and a height of about 50-70nm. In each vertical thin body, there are two conductor-oxide-semiconductor structures or two conduction channels (located in the vertical thin body VTB (such as Fig.25 (b)). Fig.25 In the embodiment of (b), as described above, due to the lateral displacement caused by the thermal process, the lightly doped drain region of the source region / drain region contacts the two vertical thin bodies. The width of the shallow trench isolation region between the vertical thin body field effect transistor and another vertical thin body field effect transistor can be 12nm. Therefore, Fig.25 The distance between the vertical thin body field effect transistor and the another vertical thin body field effect transistor in (b) is 22 nm.

[0192] in addition, Fig.25 (c) corresponds to another embodiment of the present invention, wherein Fig.25 (c) and Fig.25 The main difference of (b) is that the N+ region 2508 is not grown in a depression limited by the shallow trench isolation region. Therefore, the N+ region 2508 can gradually expand like a mushroom. It is worth noting again that even though there are two vertical thin bodies in the convex structure, because of the presence of the silicon surrounding ring mentioned above, one exposed end of the silicon surrounding ring only provides a seed crystal region for the selective epitaxial growth of the lightly doped drain region and the highly doped semiconductor region, rather than two separate seed crystal regions.

[0193] In summary, there is a central pole in the convex structure in the vertical thin body field effect transistor, and the conductive central pole is surrounded by the gate dielectric layer 1502, so the conductive central pole in the convex structure can effectively suppress the leakage current path of the vertical thin body field effect transistor in the off state. However, the vertical thin body field effect transistor still has a plurality of vertical thin bodies (that is, vertical thin bodies Sright, Sleft) for conducting current during the on state. In addition, for example, the width of the vertical thin body Sright (or vertical thin body Sleft) can be about 1.5 to 2 nm. Because the conductive central pole is surrounded by the silicon surrounding ring, the conductive current of the vertical thin body field effect transistor in the on state will diverge and then converge in the conduction channel region extending from the drain region to the source region.

[0194] In addition, forming the solid fence wall (e.g. Figure 6 The oxide spacer 304 and the nitride spacer 306 shown in the figure are used to sandwich the active region or the narrow convex structure, especially the sidewall of the convex structure. The strong fence wall can be a single layer or other composite layers to protect the narrow convex structure from collapse during the formation of the source / drain region or the gate region of the vertical thin-body field effect transistor. In addition, the shallow trench isolation region 402 (such as Figure 7 As shown in the figure, the convex structure also surrounds or clamps the active region or the narrow convex structure (especially the sidewalls of the narrow convex structure) to protect the narrow convex structure from collapse during the formation of the source region / drain region or the gate region of the vertical thin-body field effect transistor. Therefore, even if the height of the convex structure of the vertical thin-body field effect transistor (e.g., 60 to 300 nm) is much larger than the width of the convex structure of the vertical thin-body field effect transistor (e.g., 3 to 7 nm), the convex structure protected by the solid fence wall is still unlikely to collapse in subsequent processes (e.g., forming the source region / drain region or the gate region, etc.).

[0195] Another advantage of the present invention is that, because the gate region (such as Fig.18 The thickness of the oxide spacer-2 layer 1802 and the nitride spacer-2 layer 1804 on the edge of the thermal oxidation process is controllable, and the oxide-3V layer 10022 and the oxide-3B layer 10024 (as shown in FIG. Fig.19 ) is also controllable, so the edge of the source region / the drain region can be aligned with the gate region (as shown in Fig.21 The edges of the source region / the drain region are aligned or substantially aligned, especially the source region / the drain region is formed by the selective epitaxial growth technology. Therefore, the relative position or distance between the edge of the source region / the drain region and the edge of the gate region is controllable and depends on the thickness of the spacer layer (oxide spacer-2 layer 1802 and nitride spacer-2 layer 1804) formed on the edge of the gate region and / or the thickness of the oxide layer (e.g. oxide-3V layer 10022). Therefore, the effective channel length Leff can be controlled, so that the problem of gate induced drain leakage (GIDL) current can be improved.

[0196] Please refer to the following Fig.26A and Fig.26B , Fig.26A and Fig.26B is a flow chart of a method for manufacturing a novel vertical thin-body field effect transistor (NuVTBFET) disclosed in another embodiment of the present invention, wherein Fig.26A , Fig.26BOnly the different processes between the novel vertical thin-body field effect transistor and the vertical thin-body field effect transistor (VTBFET) are shown. The detailed steps of the novel vertical thin-body field effect transistor (taking an N-type metal-oxide-semiconductor (MOS) field effect transistor as an example) (following the above step 118) are as follows:

[0197] Step 2602: Form a spin-on glass (SOG) and etch downward to produce a center electrode 2702 to fill the recess 1202 ( Fig. 27 );

[0198] Step 2604: Remove the SiCOH spacer-2 layer 1102 and etch down the shallow trench isolation region 402 in the gate region to align the top of the center pole 2702, and then create a dummy gate according to the damascene process by the following steps:

[0199] (dummy gate): forming a polysilicon spacer 2802, and depositing a titanium nitride (TiN) layer 2804 and a tungsten layer 2806 in the gate region ( Fig.28 );

[0200] Step 2606: remove the polysilicon layer 2802 and the pad oxide layer 204 below the polysilicon layer 2802 to expose the shallow trench isolation region 402. Then further etch the exposed shallow trench isolation region 402 to form a trench or a damascene spacer region, wherein the damascene spacer region will expose the original single convex silicon structure.

[0201] Si structure) sidewall;

[0202] Step 2608: In the trench or the damascene spacer region, a low-k spacer is formed by depositing a carbon-silicon oxide layer 2902, forming an oxide layer 2904 between the carbon-silicon oxide layers 2902, and then polishing the carbon-silicon oxide layer 2902 and the oxide layer 2904 using the chemical mechanical polishing (CMP) technique ( Fig.29 ). The low k

[0203] The spacer layer is a vertical spacer layer extending to the top of the pseudo gate, and the low-k spacer layer spans the top surface and sidewalls of the original single convex silicon structure; Step 2610: remove the pseudo gate (titanium nitride layer 2804 and tungsten layer 2806), etch the shallow trench isolation region 402 in the gate region, and remove the oxide spacer 304 and the nitride spacer 306 in the gate region to expose the sidewalls of the vertical thin silicon body of the gate region ( Fig.30 );

[0204] Step 2612: In the gate region, firstly, the center pole 2702 is etched and the pad oxide layer 204 is removed to expose the top of the vertical thin silicon body, a high-k dielectric layer 3102 is formed above the vertical thin silicon body in the gate region, and then a dummy gate conductive layer (e.g., polysilicon) 3104 is formed above the high-k dielectric layer 3102, and a gate capping layer (or hard mask) 3106 is formed above the dummy gate conductive layer 3104. Then, the amorphous silicon carbide layer 2704 is removed and the chemical mechanical polishing technology is used to polish and reduce the height of the pad nitride layer 206, the low-k spacer layer (carbon silicon oxide layer 2902 and oxide layer 2904) and the gate capping layer 3106 ( Fig.31 );

[0205] Step 2614: Remove the exposed pad nitride layer 206 (including the vertical nitride spacer 306) and the pad oxide layer 204 below the pad nitride layer 206 to expose the original semiconductor surface (OSS) or the original horizontal surface (OHS). Afterwards, another low-k spacer is formed next to the previous low-k spacer (for example, a carbon silicon oxide layer 3202 is deposited next to the carbon silicon oxide layer 2902, and then an oxide layer 3204 is formed). This dual low-k spacer structure helps to reduce the overlay capacitance ( Fig.32 );

[0206] Step 2616: Similar to the previous process of the vertical thin body field effect transistor (VTBFET), the source region and the drain region of the novel vertical thin body field effect transistor are formed ( Fig.33 );

[0207] Step 2618: In the gate-last process, the gate capping layer 3106, the dummy gate conductive layer 3104 (and the previous gate dielectric layer 3102 (if applicable)) are removed.

[0208] Then, in order to protect the vertical thin silicon body, the shallow trench isolation region 402 is deposited back into the gate region so that the shallow trench isolation region 402 is aligned with the top of the center pole 2702 ( Fig.34 );

[0209] Step 2620: First remove the center electrode 2702, and then form a high-k dielectric layer 3502 and a metal electrode 3504 ( Fig.35 );

[0210] Step 2622: Inside the gate region, etch back the shallow trench isolation region 402 and form a high-k dielectric layer 3502 to cover the vertical thin silicon bodies Sright, Sleft ( Fig.36 );

[0211] Step 2624: In the gate region, work function metals 3708 and 3710 are formed on the high-k dielectric layer 3502, and then a tungsten layer 3706 is formed on the work function metal 3708, and then a liner 3704 is formed on the tungsten layer 3706, and then a hard mask oxide layer 3702 is formed ( Fig.37 ).

[0212] In step 2602 (following step 118 above), if Fig. 27 As shown in (a), the spin-on glass (SOG) is formed and etched downward to form a central electrode 2702 (width 10 nm) to fill the recess 1202, wherein the active region is located above an anti-punch-through layer 2706, and the anti-punch-through layer 2706 is used to prevent breakdown between the drain and the body of the novel vertical thin-body field effect transistor. In addition, as Fig. 27 As shown in (a), the amorphous silicon carbide layer 2704 replaces the thin nitride layer 802. In addition, Fig. 27 (b) is related to Fig. 27 (a) The corresponding top view, where Fig. 27 (a) Included in Fig. 27 (b) shows two cross-sectional views ("AA" and "BB") taken at the locations shown.

[0213] Then, in step 2604, Fig.28 As shown in (a), the carbon silicon oxide spacer-2 layer 1102 is removed and the shallow trench isolation region 402 in the gate region is etched downward so that the shallow trench isolation region 402 is aligned with the top of the center pole 2702. Then, according to the damascene process, the pseudo gate is created. First, a polysilicon layer 2802 (thickness of 5nm) is deposited on both sides of the pad nitride layer 206, that is, a thin layer of intrinsic amorphous silicon / polycrystalline silicon is deposited in the gate region, and then the anisotropic etching technology is used to etch the intrinsic amorphous silicon / polycrystalline silicon to produce a polycrystalline silicon layer 2802. Then, a titanium nitride layer 2804 and a tungsten layer 2806 are deposited. Thereafter, the titanium nitride layer 2804 and the tungsten layer 2806 are polished using the chemical mechanical polishing technology until the polysilicon layer 2802 is aligned with the top of the amorphous silicon carbide layer 2704. In addition, Fig.28 (b) is related to Fig.28 (a) The corresponding top view, where Fig.28 (a) Included in Fig.28 (b) shows two cross-sectional views ("AA" and "BB") taken at the locations shown.

[0214] In step 2606, if Fig.29As shown in (a), the polysilicon layer 2802 and the pad oxide layer 204 thereunder are removed by the anisotropic etching technique to expose the shallow trench isolation region 402. Then, the exposed shallow trench isolation region 402 is further etched to form the trench or the inlaid spacer region between the titanium nitride layer 2804 and the pad nitride layer 206, wherein the inlaid spacer region will expose the sidewall of the original single convex Si structure.

[0215] In step 2608, if Fig.29 As shown in (a), in the trench or the inlaid spacer region, the low-k spacer is formed by depositing a carbon silicon oxide layer 2902, wherein the carbon silicon oxide layer 2902 is deposited on both edges of the trench, but the thickness of the carbon silicon oxide layer 2902 is not enough to cover the trench, so a cavity is left, and then an oxide layer 2904 is deposited to completely fill the cavity, wherein the carbon silicon oxide layer 2902 and the oxide layer 2904 form the inlaid spacer. Then, the carbon silicon oxide layer 2902 and the oxide layer 2904 are polished on top of the shallow trench isolation region 402, the pad nitride layer 206, the amorphous silicon carbide layer 2704, and the titanium nitride layer 2804 / tungsten layer 2806 using the chemical mechanical polishing (CMP) technology. In addition, the low-k spacer is a vertical spacer extending to the top of the pseudo gate, and the low-k spacer spans the top surface and sidewalls (or the outer sidewalls of the vertical thin silicon body) of the original single convex silicon structure. In addition, Fig.29 (b) is related to Fig.29 (a) The corresponding top view, where Fig.29 (a) Included in Fig.29 (b) shows two cross-sectional views ("AA" and "BB") taken at the locations shown.

[0216] In step 2610, if Fig.30 As shown in (a), the dummy gate (titanium nitride layer 2804 and tungsten layer 2806) is removed to expose the central pole 2702. Then, the shallow trench isolation region 402 in the gate region is etched, and the oxide spacer 304 and nitride spacer 306 in the gate region are removed to expose the sidewalls of the vertical thin silicon body. In addition, Fig.30 (a) is Fig.30 (b) The corresponding top view, where Fig.30 (a) Included in Fig.30 (b) shows two cross-sectional views ("AA" and "BB") taken at the locations shown.

[0217] In step 2612, if Fig.31As shown in (a), the center pole 2702 is first etched downward and the pad oxide layer 204 in the gate region is removed to expose the top of the vertical thin silicon body. Then, a high-k dielectric layer 3102 is formed above the vertical silicon thin body in the gate region, and then a dummy gate conductive layer (such as polysilicon) 3104 is formed above the high-k dielectric layer 3102, and a gate capping layer (or hard mask) 3106 is formed above the dummy gate conductive layer 3104. Then, the amorphous silicon carbide layer 2704 is removed and the chemical mechanical polishing technology is used to polish and reduce the height of the pad nitride layer 206, the low-k spacer layer (carbon silicon oxide layer 2902 and oxide layer 2904), the gate capping layer 3106, the nitride spacer layer 306 and the shallow trench isolation region 402. In addition, Fig.31 (b) is related to Fig.31 (a) The corresponding top view, where Fig.31 (a) Included in Fig.31 (b) shows two cross-sectional views ("AA" and "BB") taken at the locations shown.

[0218] In step 2614, if Fig.32 As shown in (a), the exposed pad nitride layer 206 (including the vertical nitride spacer 306) and the pad oxide layer 204 below the pad nitride layer 206 are removed to expose the original semiconductor surface (OSS) or the original horizontal surface (OHS). Thereafter, another low-k spacer is formed next to the previous low-k spacer (for example, a carbon silicon oxide layer 3202 is deposited next to the carbon silicon oxide layer 2902, and then an oxide layer 3204 is formed), wherein the structure of the dual low-k spacer helps to reduce the overlay capacitance. In addition, Fig.32 (b) is related to Fig.32 (a) Corresponding top view. Fig.32 (a), where Fig.32 (a) Included in Fig.32 (b) shows two cross-sectional views ("AA" and "BB") taken at the locations shown.

[0219] In step 2616, if Fig.33 As shown in (a), similar to the previous process of the vertical thin body field effect transistor (VTBFET), the source region and the drain region of the novel vertical thin body field effect transistor can be formed according to the above steps 142 to 154, so for the sake of simplicity, further description is omitted. In addition, Fig.33 (b) is related to Fig.33 (a) The corresponding top view, where Fig.33 (a) Included in Fig.33 (b) shows two cross-sectional views ("AA" and "BB") taken at the locations shown.

[0220] In step 2618, if Fig.34As shown in (a), in the gate-last process, the gate dielectric layer 3102, the gate conductive layer 3104 and the gate capping layer 3106 (and the previous gate dielectric layer 3102 (if applicable)) are removed. Then, in order to protect the vertical thin silicon body, the shallow trench isolation region 402 in the gate region is deposited back so that the shallow trench isolation region 402 is aligned with the top of the center pole 2702. In addition, Fig.34 (b) is related to Fig.34 (a) The corresponding top view, where Fig.34 (a) Included in Fig.34 (b) shows two cross-sectional views ("AA" and "BB") taken at the locations shown.

[0221] In step 2620, if Fig.35 As shown in (a), the center pole 2702 is first removed to leave a cavity, and then a high-k dielectric layer 3502 is formed on the four sidewalls of the cavity, and then a metal pole 3504 is formed on the high-k dielectric layer 3502 to fill the cavity. Then, the high-k dielectric layer 3502 and the metal pole 3504 are etched back to the top of the shallow trench isolation region 402. In addition, Fig.35 (b) is related to Fig.35 (a) The corresponding top view, where Fig.35 (a) Included in Fig.35 (b) shows two cross-sectional views ("AA" and "BB") taken at the locations shown.

[0222] In step 2622, if Fig.36 As shown in (a), the shallow trench isolation region 402 deposited back (as described in step 2618) in the gate region is first etched to expose the outermost side of the vertical thin silicon body Sright, Sleft, and then a high-k dielectric layer 3502 is further formed to cover the outermost side of the vertical thin silicon body Sright, Sleft. In addition, Fig.36 (b) is related to Fig.36 (a) The corresponding top view, where Fig.36 (a) Included in Fig.36 (b) shows two cross-sectional views ("AA" and "BB") taken at the locations shown.

[0223] In step 2624, if Fig.37 As shown in (a), in the gate region, work function metals 3708 and 3710 are formed on the high-k dielectric layer 3502, and then a tungsten layer 3706 is formed on the work function metal 3708, and then a liner 3704 is formed on the tungsten layer. In addition, Fig.37 (b) is related to Fig.37 (a) The corresponding top view, where Fig.37 (a) Included in Fig.37(b) shows two cross-sectional views ("AA" and "BB") taken at the positions shown in FIG. 1 . In one embodiment of the present invention, the lateral length B of the work function metal 3710 (gate conductive layer) above the metal pole 3504 is longer than the lateral length A of the metal pole 3504. In another embodiment of the present invention, the lateral length B of the work function metal 3710 above the metal pole 3504 is the same as or substantially the same as the lateral length A of the metal pole 3504.

[0224] Taking the process with a minimum feature size of 5nm (or technology node = 5nm) as an example, the new vertical thin-body field-effect transistor with multiple metal oxide semiconductor structures and multiple conduction channels has the following dimensions: the body width of the two vertical thin silicon bodies is 1.5nm, the gate dielectric thickness is about 1nm, the thickness of the center pole is about 3nm, so the starting thickness of the original single convex silicon structure is about 8nm.

[0225] Please refer to the following Fig.38 and Fig.38 After the gate structure of the novel vertical thin-body field effect transistor is completely formed, similar to Fig.39 ,similar Fig.21 (c) The novel vertical thin-body field effect transistor also has three vertical gate conductive portions G1 to G3, wherein the vertical gate conductive portions G1 to G3 connect the work function metal 3708 and the top portion of the tungsten layer 3706, and the functions of the vertical gate conductive portions G1 to G3 can be referred to Fig.21 (c) is described in detail, so it will not be repeated here. Therefore, there are four conductor-oxide-semiconductor structures or metal oxide semiconductor structures sharing a common source region and a common drain region. In this embodiment, the material of the top connection portion (that is, the combination of the work function metal 3708 and the tungsten layer 3706) is different from the material of the metal pole 3504. In addition, Fig.39 is another embodiment disclosed by the present invention, wherein Fig.38 and Fig.39 The difference is that Fig.39 As shown, Fig.38 The metal pole 3504 is replaced by a sandwich structure consisting of tungsten-work function metal-high-k dielectric layer. In addition, Fig.39 It also has three vertical gate conductive parts G1 to G3, and the functions of the vertical gate conductive parts G1 to G3 can also refer to Fig.21 (c) has already been described, so it will not be repeated here.

[0226] In summary, in order to achieve the architectural advancement of the novel vertical thin-body field effect transistor to achieve the goals of power, efficiency and area reduction, Fig.372 are three cross-sectional views illustrating the novel vertical thin-body field effect transistor compared to a conventional tri-gate transistor / fin field effect transistor (FinFET). Fig.37 As shown in (a), the AA profile has three obvious differences:

[0227] (1) A conductive center electrode (metal electrode) is formed in a single convex Si fin body. The conductive center electrode can effectively suppress the leakage current path of the off state (Off state) of the novel vertical thin body field effect transistor. However, the novel vertical thin body field effect transistor still has two vertical thin bodies (vertical thin silicon bodies Sright and Sleft) for current conduction during the on state (ON state) of the novel vertical thin body field effect transistor. For example, the width of the vertical thin silicon bodies Sright and Sleft can be about 1.5 to 2 nm.

[0228] (2) forming a solid fence wall (e.g., a vertical oxide spacer layer and then a vertical nitride spacer layer) to clamp the active region or the narrow single convex silicon fin body, especially the sidewall of the single convex silicon fin body. The solid fence wall can be a single layer or other composite layers to protect the narrow single convex silicon fin body from collapse during the formation of the source / drain region or gate region of the novel vertical thin-body field effect transistor. In addition, a thick shallow trench isolation region further surrounds or clamps the active region or the narrow single convex silicon fin body.

[0229] (3) It has a raised shallow trench isolation (shallow trench isolation region 402) height. In addition, the source / drain region contact can be self-constructive by bonding the pad (titanium nitride layer 3301 and tungsten layer 3304) and the metal-semiconductor junction (titanium nitride layer 3301, tungsten layer 3304 and n+ doped source 3306 (or n+ doped drain)), which greatly reduces the burden of the erosive mask used to pattern the source / drain region contact holes.

[0230] (4) Underground insulator (oxide 3B layer 3302), which greatly suppresses junction leakage current and acts as an electrical barrier to noise and latch-up. Not only will transistor performance improve as cell width decreases, but cell height can also be scaled down because metal zero and latch-up design rules are relaxed by these architectural advantages.

[0231] Therefore, compared with the conventional Tri-Gate transistor / FinFET, the novel vertical thin-body field effect transistor has the following advantages:

[0232] (1) Better short channel effect (especially drain induced barrier lowering (DIBL)), so the gate width Lgate can be designed to be <10nm.

[0233] (2) The drain induces a lower channel barrier mainly because the vertical thin silicon body eliminates the junction leakage current path.

[0234] (3) Since the subsurface insulator ( Fig.37 (a) shows an oxide 3B layer 3302), so there is no latch-up between the N-type novel vertical thin-body field effect transistor and the P-type novel vertical thin-body field effect transistor, and the subsurface insulator can be used as an electrical blocking layer for noise.

[0235] (4) Generate compatible turn-on current by self-aligning source / drain region contacts and achieving huge source / drain contact resistance.

[0237] (5) Due to self-built contact ( Fig.37 (a) shows the titanium nitride layer 3301 and the tungsten layer 3304), which alleviates the mask bottleneck of the metal zero (M0) contact hole.

[0238] (6) Due to the subsurface gate ( Fig.37 (a) shows a metal pole 3504), which has less need for anti-penetration implantation.

[0239] In addition, the self-built technology of the new vertical thin-body field effect transistor is a key factor in alleviating the burden of the substantial increase in extreme ultraviolet (EUV) costs, and will accelerate the extension of Moore's Law with less investment. The unit area (gate pitch x fin pitch) of the new vertical thin-body field effect transistor is 34nm*22nm=748nm2, while the unit area of ​​the traditional N3 technology node Tri-Gate transistor / Fin field effect transistor (FinFET) is 45nm*26nm=1170nm2, compared with the traditional N3 technology node Tri-Gate transistor / Fin field effect transistor (FinFET) structure, the unit area of ​​the new vertical thin-body field effect transistor is reduced by about 36.1%.

[0240] In addition, logic transistor density scaling comes from reductions in two dimensions: cell width and cell height. Shrinking the transistors at the front end of the production line reduces the cell width, while shrinking the metal interconnects at the back end of the production line reduces the cell height. Compared to the N3 technology node, about 1.7 times the logic element density can be achieved through the design technology co-optimization (DTCO) technology in the new vertical thin-body field effect transistor. The gate length of the new vertical thin-body field effect transistor continues to shrink to 10 nanometers at a rate determined by Moore's Law, indicating that the technology node is moving towards 1.5 nanometers.

[0241] In addition, as shown in Table 1, the work function WF of the work function metal 3708 / 3710 can be adjusted to 4.2-4.3 so that the threshold voltage Vt of the novel vertical thin-body field effect transistor is about 330-360mv. By using appropriate gate metal materials to adjust the work function of the conductive center electrode and / or the gate conductive material, the current density of the on-state of the novel vertical thin-body field effect transistor can be 7 times that of the traditional fin field effect transistor (FinFET). Therefore, the novel vertical thin-body field effect transistor has a quantum enhancement function so that the ratio of the on-current (Ion) to the off-current (Ioff) of the novel vertical thin-body field effect transistor is not less than 106 (for example, 1-10×10 6 ) and the subthreshold slope (SS), that is, the slope of the drain current Id and the gate voltage Vg in the saturation region) of the novel vertical thin-body field effect transistor is not greater than 74 (e.g., 71-74). In addition, the on-current (Ion) of the novel vertical thin-body field effect transistor is not less than 90uA (e.g., 90-110uA), and the on-current (Ion) and off-current (Ioff) of the novel vertical thin-body field effect transistor are not greater than 90pA (e.g., 10-90pA).

[0242]

[0243] Table 1

[0244] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. A transistor structure, characterized in that Include: a body having a single convex structure, wherein the single convex structure is made of a first semiconductor material, and forming a groove in the single convex structure; a gate structure having a gate conductive layer and a gate dielectric layer, wherein the gate conductive layer spans over the single convex structure and a portion of the gate conductive layer fills the trench; a source region in contact with the first end of the single convex structure; and a drain region contacting the second end of the single convex structure; The ratio of the on-current to the off-current of the transistor structure is not less than 10 6 .

2. The transistor structure according to claim 1, characterized in that The on-current / off-current ratio of the transistor structure is about 1 to 10×10 6 .

3. The transistor structure according to claim 1, characterized in that The single convex structure includes a first outer sidewall and a second outer sidewall covered by the gate conductive layer. The single convex structure also includes a first inner sidewall and a second inner sidewall located in the groove, and the length of the first inner sidewall or the second inner sidewall is shorter than the length of the first outer sidewall or the second outer sidewall.

4. The transistor structure according to claim 1, characterized in that The bottom surface and sidewalls of the trench are covered by the gate dielectric layer, and the bottom of the gate conductive layer outside the single convex structure is lower than the bottom of a portion of the gate conductive layer.

5. The transistor structure according to claim 1, characterized in that The single convex structure includes two vertical thin bodies, the gate dielectric layer is arranged between the gate conductive layer and the two vertical thin bodies, and the width of one of the two vertical thin bodies is not greater than 3 nanometers.

6. The transistor structure according to claim 1, characterized in that Also includes: a first recess for accommodating the source region; a second recess for accommodating the drain region; and The sidewalls of the first recess and the second recess are surrounded by a shallow trench isolation region, the edge of the source region is in contact with the two vertical thin bodies, and the edge of the drain region is in contact with the two vertical thin bodies.

7. The transistor structure according to claim 6, characterized in that The source region comprises: a lightly doped drain region, contacting the two vertical thin bodies; a heavily doped region extending laterally from the lightly doped drain region; and A metal region contacts the top surface and sidewalls of the heavily doped region.

8. A transistor structure, characterized in that Include: a body having a single convex structure and having an original surface, wherein the body is made of a semiconductor material and the single convex structure has a plurality of conductive channels; a source region, contacting the first end of the single convex structure; a drain region contacting the second end of the single convex structure; and a gate structure having a gate conductive layer, wherein the gate conductive layer spans over the single convex structure, a first portion of the gate conductive layer is located within the single convex structure and below the original surface, and a second portion of the gate conductive layer is located above the original surface; The subthreshold slope of the transistor structure is no greater than 74.

9. The transistor structure according to claim 8, characterized in that The subthreshold slope of the transistor is between 71 and 74.

10. The transistor structure according to claim 8, characterized in that The length of the second portion of the gate conductive layer is greater than the length of the first portion of the gate conductive layer, and a trench is formed in the single convex structure and is located between the first end of the single convex structure and the second end of the single convex structure.

11. The transistor structure according to claim 10, characterized in that The single convex structure includes two thin bodies extending upward, each thin body includes two conductive channels along the sidewalls of each thin body, and a trench filled with the first portion of the gate conductive layer is located between the two thin bodies extending upward.

12. The transistor structure according to claim 11, characterized in that It also includes a gate dielectric layer spanning over the convex structure, wherein a first portion of the gate conductive layer is surrounded by the gate dielectric layer in the trench, and the gate conductive layer is surrounded by the gate dielectric layer along four sidewalls and the bottom of the trench.

13. The transistor structure according to claim 12, characterized in that Directly below the bottom of the trench is the semiconductor material of the body, and the gate dielectric layer along the bottom of the trench is in direct contact with the semiconductor material of the body.

14. The transistor structure according to claim 13, characterized in that The invention also comprises a separation wall for clamping the side wall of the single convex structure, and a shallow trench isolation region surrounding the separation wall.

15. A transistor structure, characterized in that Include: A semiconductor body having a single convex structure; a gate conductive layer and a gate dielectric layer, wherein the gate dielectric layer spans over the single convex structure, and the single convex structure comprises at least four conductor-oxide-semiconductor interfaces extending upward; a source region, contacting the first end of the single convex structure; and a drain region contacting the second end of the single convex structure; The on-state current of the transistor structure is not less than 90uA.

16. The transistor structure according to claim 15, characterized in that The off current of the transistor structure is no greater than 90 pA.

17. The transistor structure according to claim 16, characterized in that The single convex structure includes two thin bodies extending upwards, each of the thin bodies extending upwards includes two conductor-oxide-semiconductor interfaces extending upwards, and a groove is formed in the single convex structure to separate the two thin bodies extending upwards.

18. The transistor structure according to claim 17, characterized in that The at least four upwardly extending conductor-oxide-semiconductor interfaces are horizontally displaced from each other, and there is no shallow trench isolation region between the two upwardly extending thin bodies.

19. The transistor structure according to claim 15, characterized in that The threshold voltage of the transistor structure is between 330mv and 360mv.

20. The transistor structure according to claim 15, characterized in that Also includes: A spacer layer is adjacent to the gate conductive layer and spans across the top surface and sidewalls of the single convex structure.