Inrush current for bubble elimination in electroplating systems

By using the surging cathode electrolyte liquid and weir portion design in semiconductor electroplating, the problem of bubbles on the surface of the electroplating bath is solved, and more efficient bubble removal and plating quality improvement is achieved.

CN118900940APending Publication Date: 2024-11-05APPLIED MATERIALS INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202280092875.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-01-26
Filing Date
2022-10-13
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

During the semiconductor electroplating process, bubbles form on the surface of the electroplating bath that hinders the electroplating operation, leads to equipment failure and high-cost waste substrates. The prior art is difficult to effectively remove bubbles, affecting the plating quality and efficiency.

Method used

By passing the surging cathode electrolyte liquid through the plating chamber after the electroplating operation, air bubbles are extracted and transported out of the container, combined with the design of the weir and level sensor, the flow is controlled to limit the formation and removal of the bubbles.

Benefits of technology

It effectively reduces the number of bubbles during the electroplating process, shortens the bubble removal time, reduces equipment damage and cost, and improves plating uniformity and output.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118900940A_ABST
    Figure CN118900940A_ABST
Patent Text Reader

Abstract

An example method of semiconductor processing may include performing an electroplating operation on a semiconductor substrate in an electroplating bath in a vessel of an electroplating system. The method may include removing the semiconductor substrate from the electroplating bath. The method may include closing a valve associated with a first drain path from the electroplating system. The method may include increasing flow to a second drain path from the electroplating system. The second drain channel may be associated with a drain channel from the vessel of the electroplating system.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] CROSS-REFERENCE TO RELATED APPLICATIONS

[0002] This application claims the benefit of and priority to U.S. Non-Provisional Application No. 63 / 303,154, filed on January 26, 2022, entitled “SURGING FLOW FOR BUBBLE CLEARING IN ELECTROPLATING SYSTEMS,” the contents of which are incorporated herein by reference in their entirety for all purposes. Technical Field

[0003] The present technology relates to electroplating operations in semiconductor processing. In particular, the present technology relates to systems and methods for performing bubble removal and elimination for electroplating systems.

[0004] background

[0005] Integrated circuits can be manufactured by a process of forming alternating patterned layers of material on a substrate surface. After formation, etching, and other processing on the substrate, metal or other conductive materials are often deposited or formed to provide electrical connections between components. Because this metallization can be performed after many manufacturing operations, problems caused during metallization can result in expensive scrapped substrates or wafers.

[0006] Electroplating is performed in a plating chamber where the device side of the wafer is in a liquid electrolyte bath and electrical contacts on a contact ring contact a conductive layer on the wafer surface. Current is passed through the electrolyte and the conductive layer. Metal ions in the electrolyte plate out onto the wafer, forming a metal layer on the wafer. Air or other bubbles along the surface of the plating bath fluid may interfere with electroplating at locations where the bubbles interrupt contact between the fluid and the substrate surface. During the electroplating process, bubbles may form along the surface of the plating bath from any number of sources.

[0007] Therefore, there is a need for improved systems and methods that can be used to produce high quality devices and structures and protect both the substrate and the electroplating bath. The present technology can address these and other needs.

[0008] Overview

[0009] An example method of semiconductor processing may include performing an electroplating operation on a semiconductor substrate in an electroplating bath in a vessel of an electroplating system. The method may include removing the semiconductor substrate from the electroplating bath. The method may include closing a valve associated with a first drain from the electroplating system. The method may include increasing flow to a second drain from the electroplating system. The second drain may be associated with a drain channel from the vessel of the electroplating system.

[0010] In some embodiments, the container may include a weir portion, surrounding the container, and increasing the flow to the second discharge channel may increase the flow through the weir portion to the discharge channel, the discharge channel leading to the second discharge channel. The weir portion may define a plurality of notches extending from the upper surface of the weir portion. The container may include an upper cup, defining a plurality of channels, the plurality of channels passing through the upper surface of the upper cup. One or more holes may couple each of the plurality of channels in a space in the container, the space being in contact with the membrane fluid. The cathode electrolyte may flow in the space. The space may contact the first surface of the membrane. The method may include flowing the anode electrolyte to contact the second surface of the membrane, the second surface of the membrane being opposite to the first surface of the membrane. The first discharge channel may be associated with one or more outlets of the space in the container. The central channel may be defined to pass through the upper cup. The cathode electrolyte may flow into the container via the upper cup. When performing an electroplating operation, the cathode electrolyte flow may extend into each of the plurality of channels and flow through the weir portion surrounding the container. The electroplating system may include a reflux pump, the fluid being coupled to the second discharge channel. The electroplating system may include a level sensor disposed in the discharge channel. The level sensor may be communicatively coupled to the return pump. The return pump may be operable to increase the flow rate from the second drain in response to a signal from the level sensor indicative of increasing catholyte level in the drain passage.

[0011] Some embodiments of the present technology may include a method of semiconductor processing. The method may include performing an electroplating operation on a semiconductor substrate in a plating bath in a container of an electroplating system. The method may include removing the semiconductor substrate from the plating bath. The method may include diverting flow to a first exhaust channel from the electroplating system. The method may include increasing flow to a second exhaust channel from the electroplating system. The second exhaust channel may be associated with an exhaust passage from the container of the electroplating system. Increasing flow to the second exhaust channel may occur for a first period of time. The method may include, after the first period of time, reducing flow to the second exhaust channel from the electroplating system.

[0012] In some embodiments, the method may include increasing the flow to the first discharge channel when the flow to the second discharge channel is reduced after the first period of time. The container may include a weir portion surrounding the container. Increasing the flow to the second discharge channel may increase the flow through the weir portion into the discharge channel, which leads to the second discharge channel. The weir portion may define a plurality of notches extending from the upper surface of the weir portion. The container may include an upper cup defining a plurality of channels, the plurality of channels passing through the upper surface of the upper cup. One or more holes may couple each of the plurality of channels to a space in the container that is in contact with the membrane fluid. The central channel may be defined through the upper cup. The cathode electrolyte may flow into the container via the upper cup. When performing an electroplating operation, the cathode electrolyte flow may extend into each of the plurality of channels and flow through the weir portion. When the flow to the second discharge channel is increased, the height of the cathode electrolyte in the discharge channel may increase by less than or about 2 cm. The first period of time may be less than or about 30 seconds.

[0013] Some embodiments of the present technology may include a method of semiconductor processing. The method may include performing an electroplating operation on a semiconductor substrate in a plating bath in a container of an electroplating system. The container may include a weir portion surrounding the container. The method may include removing the semiconductor substrate from the plating bath. The method may include providing a first flow, the first flow passing through the electroplating system via a central channel through the container. The method may include providing a second flow, the second flow passing through the electroplating system via an auxiliary channel through the container and radially outward from the central channel. The first flow and the second flow may flow to a discharge channel from a container of the electroplating system. The flow flowing to the discharge channel may flow through the weir portion into the discharge channel. The discharge channel may lead to a discharge channel. In some embodiments, the weir portion may define a plurality of recesses extending from an upper surface of the weir portion. When the flow to the second discharge channel is increased, the height of the cathode electrolyte in the discharge channel increases by less than or approximately 2 cm.

[0014] This technology can provide several advantages over conventional technologies. For example, the present technology can reduce or limit bubbles along the meniscus of the electroplating bath during the electroplating process. In addition, the system can also eliminate bubbles with minimal time loss between subsequent electroplating operations, and also limit the modification parts or costs associated with the improved elimination capabilities. These and other embodiments and many of their advantages and features are described in more detail in conjunction with the following description and the accompanying drawings.

[0015] BRIEF DESCRIPTION OF THE DRAWINGS

[0016] A further understanding of the nature and advantages of the disclosed embodiments may be realized by reference to the remaining portions of the specification and the accompanying drawings.

[0017] Figure 1 A schematic diagram of an electroplating processing system according to some embodiments of the present technology is shown.

[0018] Figure 2 A cross-sectional view of a portion of an electroplating processing system is shown in accordance with some embodiments of the present technology.

[0019] Figure 3 An example of operation of a method of operating an electroplating system according to some embodiments of the present technology is shown.

[0020] Figure 4 A cross-sectional view of a portion of an electroplating processing system is shown in accordance with some embodiments of the present technology.

[0021] Figure 5 A perspective view of a slotted weir is shown in accordance with some embodiments of the present technology.

[0022] Figure 6 Example operations of a method of operating an electroplating system according to some embodiments of the present technology are illustrated.

[0023] Several drawings are included for illustrative purposes. It will be understood that the drawings are for illustrative purposes and are not to be considered to be to scale unless specifically noted that the drawings are to scale. Additionally, the drawings are provided as illustrations to aid understanding and may not include all aspects or information compared to actual representations and may include exaggerated material for illustrative purposes.

[0024] In the drawings, similar parts and / or features may have the same reference numerals. Furthermore, parts of the same kind may be distinguished by appending a letter after the reference numeral that distinguishes the similar parts and / or features. If only the preceding reference numeral is used in the specification, the description applies to any similar part and / or feature having the same preceding reference numeral, regardless of the suffix letter.

[0025] Specific description

[0026] Several operations in semiconductor manufacturing and processing are performed to create a large number of feature arrangements on a substrate. As semiconductor layers are formed, vias, trenches, and other pathways are created in the structure. These features can then be filled with conductive or metallic materials to provide layer-to-layer conductivity through the device.

[0027] Electroplating operations may be performed to provide conductive material in through-holes and other features on a substrate. Electroplating utilizes an electrolyte bath containing ions of the conductive material to electrochemically deposit the conductive material on a substrate and in features defined on the substrate. The substrate upon which the metal is plated operates as a cathode. Electrical contacts such as rings or pins allow current to flow through the system. During electroplating, the substrate may be clamped to a head and immersed in an electroplating bath to form the metallization. Metal ions may be deposited from the bath onto the substrate.

[0028] In an electroplating system utilizing an inert anode, an additional source of metal ions may be used to supplement the catholyte solution. The metal ions may pass through the membrane and transfer from the anolyte solution to the catholyte. Both the catholyte and the anolyte may flow through opposite sides of the membrane. The membrane may be configured to allow metal ions to transfer from the anolyte to the catholyte and to limit the transfer of additives and other materials from the catholyte to the anolyte. The catholyte may then be circulated over the substrate surface during electroplating to allow the metal ions to precipitate on the substrate and form conductive structures.

[0029] Bubbles in the cathode electrolyte or plating bath may cause plating problems. When the substrate is immersed in the bath, bubbles trapped on the surface of the substrate may prevent the cathode electrolyte from contacting the surface at that location, which may hinder plating at that location and may cause defects or device failure. Eliminating bubbles from the meniscus of the bath surface can be challenging in many processing aspects. For example, when the substrate is removed from the bath, liquid falling back into the bath may cause bubbles to form on the surface. Similarly, subsequent cleaning operations may cause droplets to fall to the bath surface and form bubbles. Finally, air entrained in the cathode electrolyte may generate bubbles during the transfer process if it is not removed in advance. Although conventional techniques have tried to limit bubble formation on the surface, bubbles continue to be a challenge for electroplating operations.

[0030] The present technology overcomes these problems by surging cathode electrolyte liquid through the plating chamber after the plating operation, which can help extract bubbles from the surface of the liquid and convey them away from the plating vessel. As will be further described below, the elimination of bubbles from the plating bath according to some embodiments of the present technology can improve the plating operation by limiting or negating the competing forces that can retain bubbles in the vessel and limit the time between plating operations. After describing an example system that can incorporate embodiments of the present technology, the remainder of the disclosure will describe various aspects of the systems and processes of the present technology.

[0031] Figure 1A schematic diagram of an electroplating system 20 according to some embodiments of the present technology is depicted. This system may include one or more components as described below for processing substrates. It will be understood that the electroplating system 20 is included as an example of an electroplating system that can benefit from one or more aspects of the present technology. This figure can provide a general structure, as further described below. As shown, the electroplating system 20 may include a head 30 located above a container assembly 50. The container assembly 50 may be supported on a platform plate 24 and a relief plate, which is attached to a bracket 38 or other structure. A single electroplating system 20 may be used as a stand-alone unit, or multiple electroplating systems 20 may be provided in an array, with workpieces or substrates loaded into or removed from a processor by one or more robots. The head 30 may be supported on a lift / rotate unit 34, which is operable to raise or invert the head to load and unload workpieces into the head, and lower the head 30 to engage the container assembly 50 for processing.

[0032] Electrical control and power cables 40 connected to the lift / rotate unit 34 and the internal head assembly may be routed from the electroplating system 20 to a facility connection, or to a connection in an automated system of multiple processors. A rinse assembly 28 with a layered drain ring may be provided above the container assembly 50. A drain pipe 42 may connect the rinse assembly 28 to a facility drain when in use. An optional lift 36 may be provided below the container assembly 50 and may support the anode cup during anode replacement. Alternatively, the lift 36 may be used to support the anode cup on the remainder of the container assembly 50.

[0033] Flip to Figure 2 , which depicts a cross-sectional view of a portion of an electroplating processing system according to some embodiments of the present technology, and may depict further details of the electroplating system 20 described above. As shown, the container assembly 50 may include an anode cup 52, a lower membrane support 54, and an upper membrane support 56, which are fixed together using fasteners, bolts, or any other mechanism of mechanically coupling components. In the anode cup 52, the first or internal anode 70 may be located near the bottom of the internal anode electrolyte chamber, or near the bottom of the space formed between the internal anode and the back side of the internal membrane 85. The second or external anode 72 may be located near the bottom of the external anode electrolyte chamber, or near the bottom of the space surrounding the internal anode electrolyte chamber, and the external anode electrolyte chamber may also be formed between the external anode and the back side of the internal membrane 85. For example, the internal anode 70 may be a planar circular metal plate, and the external anode 72 may be a planar annular metal plate, and may include a platinum-coated titanium plate or any number of other materials according to embodiments of the present technology.

[0034] The inner and outer anolyte chambers may be filled with copper pellets, or may be fluidly coupled, for example, using tubes, pumps, valves, or other components, to a facility cabinet that may include copper pellets or some other material that may provide metal ions for electroplating operations in accordance with the present technology and may be used to electroplate copper or any other metal or material used in semiconductor processing. Figure 2 , the internal anode 70 can be electrically coupled to a first electrical conductor or connector 130, and the external anode 72 can be electrically coupled to a separate second electrical conductor or connector 132. Unlike many conventional designs, in some embodiments of the present technology, the electroplating system can have a central anode, and only a single external anode, but still achieve improved performance due to other design features. Having only two anodes instead of three or more anodes can simplify the design and control of the system, and can also reduce the overall cost and complexity of the system. It will be understood that a design including three or more anodes can also be selectively used, such as, for example, when utilizing a larger substrate.

[0035] The upper cup 76 may be contained in the upper cup housing 58 or the chamber body, or the upper cup housing 58 or the chamber body may surround the upper cup 76, and the upper cup 76 may be part of a container in which a substrate may be disposed to perform an electroplating operation. The upper cup housing 58 may be attached and sealed to the upper cup 76. The upper cup 76 may have a curved upper surface 124 and a central hole or opening that may form a central or internal container 120 in which the cathode electrolyte may flow. This container 120 may be defined by a generally cylindrical space in the diffuser 74 leading to a bell-shaped or trumpet-shaped space defined by the curved upper surface 124 of the upper cup 76. A set of concentric annular grooves may extend downward from the curved upper surface 124 of the upper cup 76. An external cathode electrolyte chamber 78, or space as further described below, may be formed in the bottom of the upper cup 76 and may be connected to the ring via an array of tubes or other channels.

[0036] The diffuser 74 may be positioned in the central opening of the upper cup 76 and may be surrounded by a diffuser shroud 82. A first or inner membrane 85 may be secured between the upper membrane support 56 and the lower membrane support 54 and may separate the inner anode electrolyte chamber from the container 120. The inner membrane support 88 may be provided in the form of radial spokes 114 located on the center of the upper membrane support 56, which may support the inner membrane 85 from above. This design allows the container 120 to remain substantially open, which may better allow high current to be provided from the inner anode to the workpiece when electroplating on the resistive film. The radial spokes may occupy or block less than about 5%, 10%, 15% or 20% of the cross-sectional area of ​​the container 120. Similarly, a second or outer membrane 86 may be secured between the upper membrane support and the lower membrane support and separate the outer anode electrolyte chamber from the outer cathode electrolyte chamber 78. The outer membrane support 89 may be provided in the form of radial legs 105 or 116 located on the upper membrane support 56, the outer membrane support 89 supporting the outer membrane from above.

[0037] A diffuser circumferential horizontal supply conduit 84 may be formed in the outer cylindrical wall of the upper cup 76, the diffuser circumferential horizontal supply conduit 84 being sealed by an O-ring or similar element between the outer wall of the upper cup 76 and the inner cylindrical wall of the upper cup housing 58. As shown in the figure, a radial supply conduit 80 may extend radially inward from the diffuser circumferential horizontal supply conduit 84 to an annular shroud surge chamber 87 that surrounds the upper end of the diffuser shroud 82. The radial supply conduit 80 may pass through the upper cup 76 between vertical tubes that connect annular grooves in the curved upper surface 124 of the upper cup 76 to the outer cathode electrolyte chamber 78. A current sampling assembly 200 may be included, which may include a sampling electrode and a containment electrolyte or thiefolyte, and in operation may help improve control of edge plating and improve plating uniformity.

[0038] During operation, the anolyte may be provided to the inner anolyte chamber via a more central inlet through the bottom of the structure. The anolyte may be provided to the outer anolyte chamber via a radially outer inlet through the bottom of the structure. The anolyte may flow out of the inner anolyte chamber via the circulation groove 162, and the anolyte may flow out of the outer anolyte chamber via the circulation groove 160. In addition, the cathode electrolyte may flow upward in the container 120 and flow radially outward. This flow may continue to overflow the weir 68, which may extend around the container and may transport the cathode electrolyte to the discharge channel 122. The cathode electrolyte may flow out of the discharge channel 122 to a recirculating reflux portion. The cathode electrolyte level indicator 140 may monitor the cathode electrolyte level in the discharge channel 122 and / or the upper cup 76. The indicator 140 may be communicatively coupled to the reflux pump and may be ramped to a higher or lower speed as shown below to control the cathode electrolyte level. It will be understood that the designations anolyte and catholyte as used herein refer to the location of the electrolyte in the vessel, and not necessarily to any particular chemical composition of the electrolyte.

[0039] Figure 3 Example operations of a method 300 for operating an electroplating system according to some embodiments of the present technology are illustrated. The method may be performed in a number of processing systems, including the electroplating system 20 described above, or any other electroplating system, and may include the components, assemblies, or subsystems described above. The method 300 may be performed to limit bubble formation along the surface or meniscus of the cathode electrolyte, and may improve electroplating uniformity across the wafer. The method 300 may include a number of optional operations that may or may not be particularly relevant to some embodiments of the methods of the present technology. The method 300 may be combined with Figure 4 The system shown in FIG. Figure 4 A cross-sectional view of a portion of an electroplating system 400 according to some embodiments of the present technology is depicted. The electroplating system 400 may schematically depict some components of the electroplating system 20 including the container assembly 50 described above, and some components of the electroplating system 20 may be included to help illustrate the operations performed, and are not intended to limit the present technology to the illustrated drawings. It will be understood that the electroplating system 400 may include any of the aforementioned components, as well as any number of other components commonly used in electroplating systems.

[0040] For example and as described in more detail above, the electroplating system 400 may include a container 405, which may contain a plating bath, such as a cathode electrolyte, and may be sized to accommodate a substrate or wafer for electroplating. The container may be defined by one or more of the components described above, such as including an upper cup 410 and a weir 415. The cathode electrolyte may flow upward through the central channel of the upper cup as shown, and may flow radially outward in the container. As described above, the cathode electrolyte may flow in multiple directions in the container. The flow may flow through the weir 415 and enter the exhaust channel 420. The exhaust channel 420 is formed in the chamber housing and extends around the container, such as the exterior of the upper cup 410 and the weir 415. In addition, the cathode electrolyte may flow through a channel formed through the upper cup from the upper surface of the upper cup, and through the hole 422 to the space 425, the hole 422 is formed from the channel through the bottom of the upper cup, and the space 425 is defined below the upper cup 410. Space 425 can be located between the upper cup and membrane 430, where the space can be located on a first surface of membrane 430. As shown, the cathode electrolyte can flow through the channels and holes into this space and can sweep along membrane 430 to receive metal ions from the anode electrolyte. The anode electrolyte can flow through space 435 along a second surface of membrane 430. The second surface is, for example, a surface opposite to the first surface and can allow the anode electrolyte to transfer metal ions through the membrane to the cathode electrolyte.

[0041] The cathode electrolyte can leave the system from several locations. For example, from the space 425, one or more first drains 427 can be coupled to this space and serve as an outlet, and the cathode electrolyte can be recovered from the space. For example, any number of drains can provide flow from the space 425 and can extend to a valve 440, which can control the flow from the first drain and can provide the cathode electrolyte to the bath 445, or some recovery system, which is used to replenish and / or re-transmit to the central channel and to the container via the upper cup. In addition, once the discharge channel 420 receives the cathode electrolyte, the cathode electrolyte can flow through the second drain 450 and be pumped back to the bath 445 of the cathode electrolyte, for example using a reflux pump 455. These flows can be controlled to a steady-state position to form a meniscus 460 at the top of the container and maintained by overflowing the weir. The substrate can then be transferred to a bath for electroplating.

[0042] As described above, the cathode electrolyte can circulate in the lower space below the upper cup and be in ionic communication with the anode electrolyte. The circulation of the cathode electrolyte in this space can help limit crystallization in the anode electrolyte. For example, in the case where the cathode electrolyte receives ions from the anode electrolyte without proper circulation, the anode electrolyte may become supersaturated near the membrane, which may cause crystals to form in the anode electrolyte and may reduce the ions available for electroplating on the wafer or substrate. Therefore, the cathode electrolyte can flow at a rate to ensure proper transport of metal ions. However, this flow may exert a force on the flow on the weir, which may cause vortices or ripples to form on the curved liquid surface, and may cause air to be trapped between the substrate and the cathode electrolyte, making electroplating at these locations challenging. In addition, this flow may cause bubbles to be trapped along the surface of the curved liquid surface, which may be trapped on the substrate again and limit electroplating at this location.

[0043] As described above, when the substrate is removed from the plating bath after the plating operation, the cathode electrolyte or electrolyte bath fluid may fall back into the container, causing bubbles to form along the surface. These bubbles should flow over the weir with the cathode plating solution and be removed from the plating bath without being entrained in the system. However, because the cathode electrolyte flows through the upper cup, the bubbles may be caught in vortices along the meniscus, and the flow over the weir may not be able to extract these bubbles from the system. The present technology can adjust the flow in the container to increase the flow over the weir, which can improve the removal of bubbles from the system. Increasing the inlet flow rate alone may not be enough to address the situation of bubble retention caused by the opposing flow through the upper cup. For example, if only a specific amount of inlet flow is increased, the flow through the upper cup may also increase, which may increase the force along the meniscus and may aggravate the flow characteristics and bubble retention. Therefore, the present technology can adjust the flow through the upper cup and increase the flow over the weir, which can help to extract bubbles from the surface and ensure a better meniscus for subsequent processing.

[0044] Method 300 may include operations that facilitate the removal of bubbles from an electroplating bath, and may be performed during or between wafer electroplating processes. For example, at selected operation 305, an electroplating operation may be performed on a semiconductor substrate immersed in an electroplating bath or cathode electrolyte. Once completed, the substrate may be removed or pumped out of the electroplating bath at operation 310. This operation and cleaning operations performed on the substrate may cause fluid droplets to fall back into the bath, and may cause bubble formation as described above. Method 300 may then adjust the cathode electrolyte flow by the system to improve bubble removal before a subsequent wafer is placed in the bath for electroplating.

[0045] The method 300 may include diverting flow through the first discharge channel at operation 315. Diverting the flow may be achieved in any number of ways and in a system including a valve, each discharge channel flows to a valve, such as the valve 440 previously described, and the flow from the first discharge channel may be reduced by at least partially closing the valve, and may include completely closing the valve in some embodiments. This may stop any opposing flow in the container and allow all flow to flow over the weir, which may reduce turbulent interference and allow all fluid to flow over the weir into the discharge channel in a more laminar manner. In addition, since the inlet flow may be maintained or increased in some embodiments, the flow to the discharge channel and the second discharge channel may be increased in operation 320. In some embodiments, the inlet flow may not be increased, and the increased flow may only come from the lack of an additional discharge path. This may control the amount of liquid level rise in the discharge channel, and may limit the time loss to return to steady-state operation.

[0046] For example, the increased second flow or flow over the weir may be performed for a first amount of time, after which the valve may return to a previous operating position or open, and flow from the first exhaust channel may be increased. This may cause the second flow, such as in the selected operation 325, to drop or decrease as the system returns to a previous level. By controlling the amount of additional flow over the weir, and ensuring that the amount of liquid in the exhaust channel is allowed to decrease appropriately, improved performance may be provided because the level in the exhaust channel may directly affect system operation. For example, when the flow over the weir is allowed to increase to remove bubbles, the level in the exhaust channel may rise from a first level 470a to a second level 470b, the first level 470a and the second level 470b may be relative and are only shown as examples, and are not necessarily specific levels. When the substrate is transferred to the bath, a large amount of cathode electrolyte fluid may be forced to flow over the weir and into the exhaust channel. If the liquid level in the drain channel is not allowed to decrease before transferring the succeeding wafer, splashing or overflowing onto the head or other system components may occur which may result in damage to the equipment.

[0047] As described above, a level sensor 475 may be disposed in the exhaust channel 420 and may monitor the level. This sensor may be communicatively coupled to the return pump 455, which may be ramped higher or lower to increase or decrease flow from the exhaust channel in response to a signal received from the level sensor, the signal indicating an increase or decrease in the cathode electrolyte level in the exhaust channel. However, simply ramping the pump to overcome the increase in flow may also be insufficient. For example, the size of the pump may not be able to overcome the change in liquid volume caused by the increased flow over the weir, which may cause the liquid level to rise. In addition, in the case of too high, the increased removal rate may cause the liquid level in the exhaust channel to drop too low, which may allow air to be entrained in the system. Therefore, in some embodiments, the inlet transfer rate may be maintained during the method 300, and a second period may occur before the subsequent wafer transfer, and during the second period, the liquid level in the exhaust channel may be reduced to a level similar to the previous first period. This can ensure uniform processing conditions between wafers and still provide for the removal of bubbles from the system.

[0048] The first period may start at any point in time after the electroplating operation has been completed, and may start when the substrate is just withdrawn from the container and the electroplating bath. Once all the flow or increased flow flows over the weir, the drain channel may flood after sufficient time, and the first period may thus be limited to eliminate bubbles and ensure that the drain channel is not overfilled. In order to limit the chance of the drain channel being flooded and limit yield losses during execution of the method, the first period may be maintained at less than or about 60 seconds, and may be maintained at less than or about 55 seconds, less than or about 50 seconds, less than or about 45 seconds, less than or about 40 seconds, less than or about 35 seconds, less than or about 30 seconds, less than or about 25 seconds, less than or about 20 seconds, less than or about 15 seconds, less than or about 10 seconds, less than or about 5 seconds, or less.

[0049] The second period of time may be any of these described periods of time, and may be the same, greater than, or less than the total amount of time of the first period of time. Thus, the entire process of increasing flow over the weir to remove bubbles and then returning the system to pre-treatment conditions after flow to the first discharge channel has been fully restored may be less than or about 2 minutes, and may be less than or about 90 seconds, less than or about 60 seconds, less than or about 50 seconds, less than or about 40 seconds, less than or about 30 seconds, less than or about 20 seconds, less than or about 10 seconds, or less. By controlling the timing and inlet flow of this method, as well as the pumping rate of the reflux pump, the liquid level in the discharge channel during the method may not rise by more than or about 5 cm, and may not rise by more than or about 4 cm, more than or about 3 cm, more than or about 2 cm, more than or about 1 cm, more than or about 9 mm, more than or about 8 mm, more than or about 7 mm, more than or about 6 mm, more than or about 5 mm, more than or about 4 mm, more than or about 3 mm, or less.

[0050] In some embodiments, one or more components may also aid in removing air bubbles from the system. Figure 5 A perspective view of a slotted weir 500 is depicted in accordance with some embodiments of the present technology. The weir 500 may be used in place of any of the aforementioned weirs, including, for example, weir 68 and weir 415. The weir 500 may be castellated, and may have one or more grooves or notches 505 formed from the upper surface of the weir and extending at least partially through the outer edge of the weir. In some embodiments, this may improve the flow of liquid over the weir, and may improve bubble removal. Although weirs characterized by a uniform, planar outer profile may be used in embodiments of the present technology, slotted weirs may limit dry spots and increase flow at slotted locations. For example, on a planar weir, flow over the edge of the weir may be uneven, and flow at locations that do not pass over the edge of the weir may accumulate bubbles. However, the notches may reduce surface tension and increase surface flow at each notch location. This may further improve bubble removal by causing the flow rate to increase at each notch location, thereby pulling the flow over or through the weir. Therefore, in some embodiments, a slotted weir may be utilized to even further improve the removal of bubbles from the system.

[0051] Some embodiments of the present technology may further increase flow over the weir by passing the flow countercurrently through the upper cup so that both flows pass over the weir. Figure 6 Example operations of a method 600 for operating an electroplating system according to some embodiments of the present technology are illustrated. The method 600 may be performed in any of the aforementioned systems and may include any of the operations described with respect to the method 300. For example, the method 600 may optionally include performing an electroplating operation 605 and removing the substrate from the electroplating bath and container at an operation 610. In some embodiments, the method 600 may cause two flow paths to flow over the weir. For example, as previously described, at operation 615, a first flow may flow through the central channel of the upper cup and over the weir. Additionally, in some embodiments, a secondary pump 480 may be included in the system and may be used to cause a second flow at operation 620 to return the cathode electrolyte through the valve 440 and into the exhaust 427. The flow may then be forced upward through the holes and channels in the upper cup, such as along the flow path 485, which may increase the flow over the weir and may provide a uniformly directional flow through the chamber, which may improve the removal of bubbles from the system. Although illustrated as several operations, it will be appreciated that in some embodiments, the flow may be performed during the electroplating operation and a subsequent or second flow may be reverse flow after electroplating.

[0052] By allowing the flow to flow countercurrently through the first exhaust passage, flow through the membrane can be maintained during the bubble removal process, compared to the previous process, while ensuring that ion transfer through the membrane is not affected by the process. The process can be performed for any length of time, such as any of the time periods described above. By performing flow adjustments according to embodiments of the present technology, bubble removal can be improved compared to conventional systems, while limiting the impact on process throughput. In addition, the present technology can be easily retrofitted to existing systems, and in some embodiments, no component replacement or system reconfiguration is required.

[0053] In the foregoing description, for the purpose of illustration, many details have been presented to understand several embodiments of the present technology. However, it is obvious to those skilled in the art that some embodiments may be implemented without some of the details or with additional details. For example, other substrates that are conducive to the wet processing techniques described above may be used with the present technology.

[0054] Where several embodiments have been disclosed, those skilled in the art will appreciate that several modifications, alternative configurations, and equivalents may be used without departing from the spirit of the embodiments. In addition, some known processes and components are not described to avoid unnecessarily obscuring the present technology. Therefore, the above description should not be construed as limiting the scope of the present technology.

[0055] It will be understood that, unless the context clearly specifies otherwise, where a numerical range is provided, the smallest fraction of each intermediate value to the lower limit unit between the upper and lower limits of the range is also explicitly disclosed. Any narrower range between any stated value or unstated intermediate value in the stated range, and any other stated or intermediate value in the stated range are included. The upper and lower limits of these smaller ranges may be independently included or excluded in the range, and each range that includes either one, neither, or both limits in the smaller range is also included in this technology, but is still subject to any explicitly excluded limits in the stated range. Where the stated range includes one or two limits, the range that does not include either or both of these limits is also included. Where multiple values ​​are provided in a list, any range that includes or is based on any of these numerical values ​​is similarly specifically disclosed.

[0056] As used herein and in the appended claims, the singular forms "a," "an," and "the" include the plural forms unless the content clearly dictates otherwise. Thus, for example, reference to "a material" includes a plurality of such materials and reference to "the channel" includes one or more channels and equivalents thereof known to those skilled in the art, and so forth.

[0057] Furthermore, when used in this specification and the claims that follow, the words “comprise(s),” “comprising,” “contain(s),” “containing,” “include(s),” and “including” are intended to refer to the presence of stated features, integers, components, or operations, but they do not exclude the presence or addition of one or more other features, integers, components, operations, actions, or groups.

Claims

1. A method for semiconductor processing, the method comprising: performing an electroplating operation on a semiconductor substrate in an electroplating bath in a vessel of an electroplating system; removing the semiconductor substrate from the electroplating bath; closing a valve associated with a first exhaust from the electroplating system; and Flow is increased to a second drain from the electroplating system, wherein the second drain is associated with a drain passage from the vessel of the electroplating system.

2. A method for semiconductor processing as described in claim 1, wherein the container includes a weir portion surrounding the container, and wherein increasing the flow to the second exhaust channel increases the flow over the weir portion into the exhaust channel, the exhaust channel leading to the second exhaust channel.

3. A method of semiconductor processing as claimed in claim 2, wherein the dam portion defines a plurality of notches extending from an upper surface of the dam portion.

4. A method for semiconductor processing as described in claim 1, wherein the container includes an upper cup defining a plurality of channels, the plurality of channels passing through an upper surface of the upper cup, and one or more holes therein coupling each of the plurality of channels to a space in the container, the space being in contact with the membrane fluid.

5. The method of semiconductor processing as claimed in claim 4, wherein a cathode electrolyte flows in the space, and wherein the space contacts the first surface of the membrane.

6. The method of semiconductor processing according to claim 5, further comprising: An anode electrolyte is flowed to contact a second surface of the membrane, the second surface of the membrane being opposite the first surface of the membrane.

7. A method of semiconductor processing as claimed in claim 5, wherein the first exhaust channel is associated with one or more outlets of the space in the container.

8. A method for semiconductor processing as described in claim 5, wherein a central channel is defined through the upper cup, wherein the cathode electrolyte flows into the container via the upper cup, and wherein, when the electroplating operation is performed, the cathode electrolyte flow extends into each of the plurality of channels and flows through a weir surrounding the container.

9. The method of semiconductor processing as claimed in claim 1, wherein the electroplating system further comprises: a return pump fluidly coupled to the second exhaust passage; and A liquid level sensor is disposed in the discharge passage, wherein the liquid level sensor is communicatively coupled to the reflux pump.

10. A method of semiconductor processing as claimed in claim 9, wherein the reflux pump is operative to increase the flow rate from the second exhaust channel in response to a signal from the level sensor, the signal being indicative of increasing cathode electrolyte level in the exhaust channel.

11. A method of semiconductor processing, the method comprising: performing an electroplating operation on a semiconductor substrate in an electroplating bath in a vessel of an electroplating system; removing the semiconductor substrate from the electroplating bath; diverting flow to a first exhaust from the electroplating system; increasing flow to a second drain from the electroplating system, wherein the second drain is associated with a drain passage from the vessel of the electroplating system, wherein increasing flow to the second drain occurs for a first period of time; and After the first period of time, flow to the second exhaust from the electroplating system is reduced.

12. The method of semiconductor processing according to claim 11, further comprising: When the flow to the second exhaust passage is reduced after the first period, the flow to the first exhaust passage is increased.

13. A method of semiconductor processing as described in claim 11, wherein the container includes a weir portion surrounding the container, and wherein increasing the flow to the second exhaust channel increases the flow over the weir portion into the exhaust channel, the exhaust channel leading to the second exhaust channel.

14. The method of operating an electroplating system of claim 13, wherein the dam portion defines a plurality of notches extending from an upper surface of the dam portion.

15. A method for operating an electroplating system as described in claim 13, wherein the container includes an upper cup defining a plurality of channels, the plurality of channels passing through an upper surface of the upper cup, and one or more holes therein coupling each of the plurality of channels to a space in the container, the space being in contact with a membrane fluid.

16. A method for operating an electroplating system as described in claim 15, wherein a central channel is defined through the upper cup, wherein the cathode electrolyte flows into the container via the upper cup, and wherein, when the electroplating operation is performed, the cathode electrolyte flow extends into each of the plurality of channels and flows through the weir.

17. The method of semiconductor processing according to claim 11, wherein: When the flow to the second exhaust channel is increased, the height of the cathode electrolyte in the exhaust channel increases by less than or about 2 cm.

18. The method of semiconductor processing of claim 11, wherein the first period of time is less than or approximately 30 seconds.

19. A method of semiconductor processing, the method comprising: performing an electroplating operation on a semiconductor substrate in an electroplating bath in a vessel of an electroplating system, wherein the vessel includes a weir portion surrounding the vessel; removing the semiconductor substrate from the electroplating bath; providing a first flow through the electroplating system via a central passage through the vessel; and A second flow is provided, the second flow passing through the electroplating system via an auxiliary channel through the container and radially outward from the central channel, wherein the first flow and the second flow flow to a discharge channel from the container of the electroplating system, and wherein the flow flowing to the discharge channel flows over the weir into the discharge channel, and the discharge channel is accessible to a drain.

20. The method of semiconductor processing of claim 19, wherein the dam portion defines a plurality of notches extending from an upper surface of the dam portion, and wherein: When flow to the second exhaust channel is increased, the height of the cathode electrolyte in the exhaust channel increases by less than or about 2 cm.