Protective film module packaging body and protective film module accommodating body
By using a combination of sealant layer and substrate layer in the protective film assembly packaging body, the air release amount of volatile organic components is reduced, the pollution problem in the protective film assembly packaging body and storage body is solved, and the stability of the components is improved and performance.
Patent Information
- Application Number
- CN202380028794.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-22
- Filing Date
- 2023-03-20
- Publication Date
- 2024-11-05
AI Technical Summary
The pollution problems caused by the release and adhesion of volatile organic components produced by the protective film assembly packaging body affect the quality and performance of the component.
A protective film assembly package is designed, including a sealant layer and a base material layer, the sealant layer has a thickness of less than 40 μm and an ethylene-vinyl alcohol copolymer, and a breaking strength of more than 5N and less than 50N, for reducing volatile organics. The amount of air release of the components.
The volatile organic components gas release amount in the protective film assembly packaging body and the storage body is effectively reduced, and the quality and performance stability of the assembly are improved.
Smart Images

Figure CN118901043A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a pellicle assembly package and a pellicle assembly container. Background Art
[0002] In the technology (photolithography) of applying a photosensitive material to the surface of an object such as an electronic component, a printed circuit board, a display panel, etc. and exposing it to a pattern to form a pattern, a transparent substrate with a pattern formed on one side called a mask is used. In these manufacturing processes, light is irradiated to the photosensitive layer through a mask (also called an exposure original plate, a photomask) to perform patterning. At this time, if there is foreign matter attached to the mask, the light will be absorbed by the foreign matter, or the light will be reflected and bent on the surface of the foreign matter. As a result, the pattern formed is deformed or the edges become rough, resulting in problems such as the size, quality and appearance of the patterned surface being damaged. In order to eliminate such problems, a method is adopted in which a protective film assembly having a protective film that transmits light is installed on the surface of the mask to suppress the adhesion of foreign matter.
[0003] In recent years, as electronic components have become more advanced in performance and their circuit widths have become smaller, pellicles are more susceptible to the effects of minute amounts of outgassing and fine particles than before. In order to reduce the amount of volatile organic gas generated by the outgassing adhering to the surface of the component, Japanese Patent Application Laid-Open No. 2007-12793 discloses a solution in which a container containing a pellicle assembly contains a polycarbonate resin and conductive carbon black in order to reduce the amount of volatile organic gas generated by the container. Summary of the invention
[0004] Problems to be solved by the invention
[0005] The inventors of the present invention have conducted in-depth research and have newly discovered that the outgassing of volatile organic components generated by the packaging body of the protective film assembly will adhere to the packaged protective film assembly. This is different from the outgassing of volatile components originating from the material constituting the protective film assembly itself, and is generated separately as outgassing from the protective film assembly, which becomes one of the factors of contamination of the protective film assembly.
[0006] An object of one embodiment of the present disclosure is to provide a pellicle package in which the amount of outgassing from the pellicle due to adhesion of outgassing of volatile organic components generated from the pellicle package is reduced.
[0007] Another embodiment of the present disclosure aims to provide a pellicle housing in which the amount of outgassing from the pellicle due to adhesion of outgassing of volatile organic components generated from the pellicle packaging body is reduced.
[0008] Solutions to Solve Problems
[0009] Specific means for solving the above-mentioned problems include the following.
[0010] <1> A pellicle package having a total outgassing amount of volatile organic components of 90 ppm or less under heating conditions of 100°C for 30 minutes.
[0011] <2> The pellicle package according to <1> above, comprising at least two layers: a sealant layer and a base material layer.
[0012] <3> The pellicle package according to <2> above, wherein the sealant layer has a thickness of 40 μm or less.
[0013] <4> The pellicle package according to <2> or <3>, further comprising an adhesive layer between the sealant layer and the base layer.
[0014] <5> The pellicle package according to any one of <2> to <4>, wherein the sealant layer comprises an ethylene-vinyl alcohol copolymer.
[0015] <6> The pellicle package according to any one of <1> to <5>, wherein the rupture strength is 5N or more and 50N or less.
[0016] <7> The pellicle assembly package according to any one of <1> to <6>, which is a package for a pellicle assembly having an adhesive for an original plate, wherein the adhesive for an original plate comprises a styrene butadiene-based adhesive.
[0017] <8> A pellicle assembly container, comprising:
[0018] Protective film components,
[0019] a pellicle assembly container for accommodating the pellicle assembly, and
[0020] A pellicle package according to any one of <1> to <7> above, which packages the pellicle package container.
[0021] <9> The pellicle assembly container according to <8>, wherein the pellicle assembly includes an adhesive for an original plate,
[0022] The adhesive for the original plate is a styrene butadiene adhesive.
[0023] Effects of the Invention
[0024] According to one embodiment of the present disclosure, it is possible to provide a pellicle package in which the amount of outgassing from the pellicle is reduced due to the adhesion of outgassing of volatile organic components generated from the pellicle package.
[0025] According to another embodiment of the present disclosure, a pellicle housing can be provided in which the amount of outgassing from the pellicle due to adhesion of outgassing of volatile organic components generated from the pellicle packaging body is reduced. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 This is a schematic cross-sectional view showing an example of a pellicle assembly. DETAILED DESCRIPTION
[0027] In the present disclosure, a numerical range expressed using "to" means a range including the numerical values described before and after "to" as the minimum value and the maximum value, respectively.
[0028] In the numerical ranges recorded in stages in the present disclosure, the upper limit or lower limit recorded in one numerical range can be replaced by the upper limit or lower limit of the numerical range recorded in other stages. In addition, in the numerical ranges recorded in the present disclosure, the upper limit or lower limit recorded in one numerical range can be replaced by the value shown in the embodiment.
[0029] In the present disclosure, a combination of two or more preferred embodiments is a more preferred embodiment.
[0030] In the present disclosure, when there are a plurality of substances corresponding to each component, the amount of each component means the total amount of the plurality of substances unless otherwise specified.
[0031] In this specification, the term "process" includes not only an independent process but also a process that cannot be clearly distinguished from other processes as long as the intended purpose of the process can be achieved.
[0032] <Protective film module package>
[0033] The total amount of outgassing of volatile organic components in the pellicle package of the present disclosure under heating conditions of 100° C. for 30 minutes is 90 ppm or less.
[0034] According to the pellicle package of the present disclosure, the amount of outgassing from the pellicle caused by the adhesion of outgassing of volatile organic components generated from the pellicle package can be reduced.
[0035] The pellicle assembly packaging body refers to the packaging member that packages the pellicle assembly.
[0036] The volatile organic component refers to a component having a vapor pressure of 0.01 KPa or more at 25°C.
[0037] Examples of the volatile organic components include hydrocarbon compounds such as aromatic hydrocarbon compounds and aliphatic hydrocarbon compounds.
[0038] Outgassing refers to the gas generated by materials such as resin that make up the pellicle package.
[0039] The total amount of outgassing of volatile organic components from the pellicle package under heating conditions of 100°C for 30 minutes is 90 ppm or less, preferably 30 ppm or less, more preferably 15 ppm or less, further preferably 10 ppm or less, and particularly preferably 5 ppm or less. That is, the closer the total amount of outgassing of volatile organic components from the pellicle package under heating conditions of 100°C for 30 minutes is to 0 ppm, the better, and more preferably below the detection limit or 0 ppm.
[0040] When the total amount of outgassing of the volatile organic components in the pellicle package is within the above range, the amount of outgassing from the pellicle due to adhesion of outgassing of the volatile organic components generated in the pellicle package can be further reduced.
[0041] The outgassing amount of the above-mentioned volatile organic components is measured as follows.
[0042] Cut the protective film assembly package into 10 mg pieces and use them as test pieces. Place the test piece in a glass insert with two lids. Next, heat at 100°C for 30 minutes while injecting He gas as a carrier gas at 3.0 mL / min, and capture the volatilized volatile organic components with a -20°C cold trap. Use a gas chromatograph mass spectrometer (hereinafter also referred to as GCMS) to measure the amount of captured volatile organic components (converted to n-decane) as the amount of outgassing generated. The measurement conditions of GCMS are as follows.
[0043] Measurement device name: QP2010plus
[0044] Chromatographic column: DB-1 (inner diameter: 0.32 mm, length: 60 m, thickness: 1.00 μm)
[0045] Scanning range: 35~450m / Z
[0046] Ionization: 0.78kV
[0047] Measurement method: Calculate the amount of gas generated at 100°C for 30 minutes in terms of decane.
[0048] The specific method for making the outgassing amount of the above-mentioned volatile organic components fall within the above-mentioned range is not particularly limited, and examples thereof include a method of adjusting the material forming the pellicle assembly package, etc. For example, examples thereof include a method of making the pellicle assembly package a laminated body including at least two layers, namely a sealant layer and a substrate layer, and adjusting the material of the sealant layer and the thickness of the sealant layer, etc.
[0049] From the viewpoint of strength during use, the breaking strength of the pellicle package is preferably 5N to 50N, more preferably 7N to 45N, and even more preferably 10N to 40N.
[0050] The above-mentioned breaking strength is measured in accordance with JIS-K7127-5 (1999) (corresponding to ISO527-3: 1995). The breaking strength is measured by stretching both ends of the test piece type 5 of JIS-K7127 (dumbbell shape with a total length of 115 mm, a parallel part width of 6 mm, a distance between markings of 25 mm, and a grip width of 25 mm).
[0051] There is no particular limitation on the specific method for adjusting the breaking strength to fall within the above range, and examples thereof include a method of adjusting the material and thickness of the substrate layer.
[0052] The pellicle package preferably includes at least two layers, namely, a sealant layer and a base layer, and more preferably includes a sealant layer, an adhesive layer, and a base layer in this order.
[0053] In the case where the protective film component package is a laminated body comprising at least two layers, namely a sealant layer and a substrate layer, or in the case where the protective film component package is a laminated body comprising a sealant layer, an adhesive layer and a substrate layer in sequence, the outermost surface on the protective film component side may be the sealant layer, and the outermost surface on the peripheral surface side may be the substrate layer.
[0054] In the case where the pellicle assembly package is composed of at least two layers, namely a sealant layer and a substrate layer, or in the case where the pellicle assembly package is a laminated body that sequentially includes a sealant layer, an adhesive layer, and a substrate layer, it is believed that the outgassing of volatile organic components in the pellicle assembly package is likely to occur from the sealant layer. Therefore, if the outermost surface on the pellicle assembly side is the sealant layer, the adhesion of the outgassing of volatile organic components generated by the pellicle assembly package also becomes significant. In contrast, the pellicle assembly package of the present disclosure has the above-mentioned structure, so that the outgassing amount from the pellicle assembly caused by the adhesion of the outgassing of volatile organic components generated by the pellicle assembly package is easily maintained low.
[0055] (Sealing agent layer)
[0056] The sealant layer may be a single layer or a laminated body composed of two or more layers.
[0057] The material of the sealant layer is not particularly limited, and a composition containing a known resin can be used.
[0058] Examples of the resin include polyethylene (PE) (including high-density polyethylene (HDPE), medium-density polyethylene (MDPE), low-density polyethylene (LDPE), linear low-density polyethylene (LLDPE), etc.), polyolefin resins such as polypropylene (PP), polybutene, and polymethylpentene as homopolymers; copolymers of two or more selected from the group consisting of olefins such as ethylene, propylene, butene, and methylpentene; polyester resins such as polyethylene terephthalate (PET), polybutylene terephthalate (PBT), and polyethylene naphthalate; polyamide resins such as nylon-6, nylon-6,6, meta-xylene diamine-adipic acid polycondensate, and polymethylmethacrylimide; ethylene-vinyl alcohol copolymers; and the like. The resins may be used alone or in combination of two or more.
[0059] Among the above, the material for the sealant layer preferably includes at least one selected from the group consisting of polyester resins, polyamide resins and ethylene-vinyl alcohol copolymers, more preferably includes at least one selected from the group consisting of polyester resins and ethylene-vinyl alcohol copolymers, and further preferably includes ethylene-vinyl alcohol copolymers, from the viewpoint of further reducing the amount of outgassing from the protective film component caused by the adhesion of outgassing volatile organic components generated by the protective film component packaging body.
[0060] The thickness of the sealant layer (the total thickness in the case of a laminated structure consisting of two or more layers) is preferably 500 μm or less, more preferably 100 μm or less, further preferably 50 μm or less, and particularly preferably 40 μm or less.
[0061] When the thickness of the sealant layer is equal to or smaller than the above range, the amount of outgassing from the pellicle due to adhesion of outgassing of volatile organic components generated from the pellicle package can be further reduced.
[0062] From the viewpoint of sealing performance, the thickness of the sealant layer (the total thickness in the case of a laminated structure composed of two or more layers) may be 3 μm or more, 5 μm or more, or 15 μm or more.
[0063] From the above viewpoints, the thickness of the sealant layer (the total thickness in the case of a laminated structure composed of two or more layers) may be 3 μm to 500 μm, or 3 μm to 40 μm.
[0064] The thickness of the sealant layer (the total thickness in the case of a laminated structure composed of two or more layers) may be 40 μm or more, 70 μm or more, or 90 μm or more.
[0065] As described above, when the pellicle assembly package is composed of at least two layers, namely a sealant layer and a substrate layer, it is considered that the outgassing of volatile organic components in the pellicle assembly package is likely to be generated from the sealant layer. Therefore, as the thickness of the sealant layer increases, the adhesion of the outgassing of volatile organic components generated by the pellicle assembly package is also likely to become significant. In contrast, the pellicle assembly package of the present disclosure has the above-mentioned structure, so that even if the thickness of the sealant layer is within the above-mentioned range, it is easy to maintain the outgassing amount from the pellicle assembly caused by the adhesion of the outgassing of volatile organic components generated by the pellicle assembly package at a low level.
[0066] (Base material layer)
[0067] The base material layer may be a single layer or a laminated body composed of two or more layers.
[0068] The material of the base material layer is not particularly limited, and a composition containing a known resin can be used.
[0069] Examples of the resin include polyethylene (including high-density polyethylene (HDPE), medium-density polyethylene (MDPE), low-density polyethylene (LDPE), and linear low-density polyethylene (LLDPE), ethylene-propylene copolymers, ethylene-butene copolymers, ethylene-hexene copolymers, ethylene-octene copolymers, polypropylene (PP), ethylene-vinyl acetate copolymers, ethylene-methyl methacrylate copolymers, and ionomer resins; polyester resins such as polyethylene terephthalate (PET), polybutylene terephthalate (PBT), and polyethylene naphthalate; nylon-6, nylon-6,6, and meta-xylene diols; Amine-adipic acid polycondensate, polymethyl methacrylimide and other amide resins; acrylic resins such as polymethyl methacrylate; styrene-acrylonitrile resins such as polystyrene, styrene-acrylonitrile copolymer, styrene-acrylonitrile-butadiene copolymer, polyacrylonitrile and other styrene-acrylonitrile resins; hydrophobic cellulose resins such as cellulose triacetate and cellulose diacetate; halogen-containing resins such as polyvinyl chloride, polyvinylidene chloride, polyvinylidene fluoride, Teflon (registered trademark); high hydrogen bond resins such as polyvinyl alcohol, ethylene-vinyl alcohol copolymer, cellulose derivatives; engineering plastic resins such as polycarbonate resin, polysulfone resin, polyethersulfone resin, polyetheretherketone resin, polyphenylene ether resin, polyoxymethylene resin, liquid crystal resin, etc. The resin may be used alone or in combination of two or more.
[0070] Among the above, the material for the substrate layer is preferably a material that is not easy to generate static electricity (preferably a resin that has been antistatically treated, more preferably a resin that includes either polyethylene terephthalate or polyethylene naphthalate), from the viewpoint of preventing dust and the like from adhering to the surface of the protective film component packaging body.
[0071] The thickness of the substrate layer (total thickness in the case of a laminated structure of two or more layers) is not particularly limited, and is, for example, preferably 0.1 μm to 500 μm, more preferably 1 μm to 100 μm, and further preferably 5 μm to 30 μm.
[0072] (Adhesive layer)
[0073] The pellicle package of the present disclosure may have an adhesive layer between the sealant layer and the base material layer as necessary.
[0074] The adhesive layer may be a single layer or a laminate composed of two or more layers.
[0075] The material of the adhesive layer is not particularly limited, and a composition containing a known resin can be used.
[0076] Examples of the resin include polyurethane resins, polyester resins, polyether resins, and mixtures thereof.
[0077] The thickness of the adhesive layer is not particularly limited, but is preferably 1 μm or more, and more preferably 2 μm or more, from the viewpoint of adhesive strength, for example.
[0078] The thickness of the adhesive layer is not particularly limited, but is preferably 5 μm or less, more preferably 4 μm or less, from the viewpoint of shortening the curing reaction time when forming the adhesive layer and reducing the proportion of unreacted products and residual solvents during the curing reaction.
[0079] (Shape and properties of pellicle module packaging)
[0080] The shape of the pellicle package is not particularly limited.
[0081] Examples of the shape of the pellicle package include a sheet, a bag, a package, and a box.
[0082] The pellicle assembly package can be configured as needed to include a packaging member in a part of the package in which the total amount of outgassing of volatile organic components under heating conditions of 100°C for 30 minutes is greater than 90 ppm within the scope of obtaining the effects of the present disclosure. On the other hand, the proportion of the packaging member in the pellicle assembly package in which the total amount of outgassing is greater than 90 ppm is preferably 20% by mass or less of the entire pellicle assembly package, more preferably 10% by mass or less, and further preferably 5% by mass or less. The pellicle assembly package preferably does not include a packaging member in which the total amount of outgassing is greater than 90 ppm.
[0083] The volume of the pellicle assembly package is not particularly limited and can be appropriately set according to the size of the pellicle assembly and the packaging form. For example, the volume of the package is preferably 2000 cm3 ~70000cm 3 , more preferably 4000cm 3 ~30000cm 3 , more preferably 5000cm 3 ~10000cm 3 .
[0084] If the volume of the pellicle assembly package is within the above range, the balance between the volume of the pellicle assembly or pellicle assembly box packaged by the pellicle assembly package and the surface area of the pellicle assembly package is easily optimized. Therefore, the proportion of outgassing of volatile organic components generated by the pellicle assembly package becomes smaller, and the amount of outgassing from the pellicle assembly due to the adhesion of outgassing derived from the pellicle assembly package is also further reduced.
[0085] As one embodiment, the pellicle assembly package of the present disclosure may be a package for a pellicle assembly having an adhesive for an original plate containing a styrene-butadiene-based adhesive.
[0086] 《Protective film unit container》
[0087] The pellicle assembly housing of the present disclosure includes a pellicle assembly, a pellicle assembly container housing the pellicle assembly, and a pellicle assembly packaging of the present disclosure packaging the pellicle assembly container.
[0088] According to the pellicle housing of the present disclosure, the amount of outgassing from the pellicle due to adhesion of outgassing of volatile organic components generated from the pellicle packaging body can be reduced.
[0089] The pellicle assembly housing is a structure obtained by packaging a container that houses a pellicle assembly with the pellicle assembly packaging body of the present disclosure.
[0090] A known pellicle assembly can be used as the pellicle assembly. The pellicle assembly includes, for example, a pellicle membrane and a support frame that supports the pellicle membrane.
[0091] The shape of the pellicle container is not particularly limited, and examples thereof include a box shape.
[0092] Below, while referring to the attached Figure 1 A method of using a protective film assembly is described below. Figure 11 is a schematic cross-sectional view showing a protective film assembly 10. In the protective film assembly 10, the protective film 12 and the support frame 14 are bonded via a film adhesive layer 13. The support frame 14 is formed with a vent hole 16 and an original plate adhesive layer 15. Although not shown in the figure, a release sheet (such as a spacer) for protecting the original plate adhesive layer 15 may be further arranged on the surface of the original plate adhesive layer 15. The vent hole 16 may not be formed on the support frame 14, and the support frame 14 may be a structure formed by stacking a plurality of layers.
[0093] The protective film 12 is supported by a support frame 14 .
[0094] Examples of the material of protective film 12 include transparent materials such as quartz glass, fluorine-based resin, cellulose acetate, and carbon nanotubes.
[0095] The material of the support frame 14 includes an anodized aluminum frame, a titanium frame, a silicon frame, etc. The support frame 14 is preferably black from the viewpoints of preventing reflection of exposure light and facilitating inspection of the presence of attached foreign matter.
[0096] The film adhesive layer 13 bonds the support frame and the protective film.
[0097] The material of the film adhesive layer 13 is not particularly limited, and examples thereof include fluoropolymers such as acrylic resin adhesives, epoxy resin adhesives, silicone resin adhesives, and fluorine-containing silicone adhesives.
[0098] The original plate adhesive layer 15 can be formed by applying a known adhesive and drying it.
[0099] The material of the original plate adhesive layer 15 (hereinafter also referred to as original plate adhesive) is not particularly limited, and examples thereof include acrylic, silicone, styrene butadiene, urethane, and olefin adhesives.
[0100] That is, in the pellicle housing of the present disclosure, the pellicle may include an adhesive for an original plate, and the adhesive for an original plate may be a styrene butadiene-based adhesive.
[0101] A styrene-butadiene adhesive can easily suppress the strain of the original plate, and therefore is preferably used as a material for the adhesive layer 15 for the original plate that bonds the support frame 14 and the original plate.
[0102] The styrene butadiene adhesive is more likely to be generated as outgassing from the pellicle assembly after outgassing of volatile organic components generated from the pellicle assembly package adheres to the pellicle assembly. The pellicle assembly package of the present disclosure has the above-mentioned structure, so that when the styrene butadiene adhesive is used as the material of the adhesive layer 15 for the original plate, the outgassing amount from the pellicle assembly caused by the adhesion of outgassing of volatile organic components generated from the pellicle assembly package can be reduced.
[0103] In the present disclosure, the term "adhesive" is a concept including adhesives and pressurizers.
[0104] In the present disclosure, the “adhesive layer” is a concept including an adhesive layer and a pressure-sensitive adhesive layer.
[0105] Examples of the material of the release sheet include polyethylene terephthalate films and polypropylene films.
[0106] Depending on the materials of pellicle membrane 12 and support frame 14 , support frame and pellicle membrane may be bonded together without interposing film adhesive layer 13 .
[0107] A known pellicle container can be used as the pellicle container.
[0108] Examples of the material of the pellicle container include resins such as polycarbonate, and conductive materials such as carbon nanotubes, conductive carbon black, and inorganic particles.
[0109] Preferred embodiments of the pellicle package in the pellicle housing of the present disclosure are the same as the preferred embodiments listed in the pellicle package of the present disclosure.
[0110] [Example]
[0111] Hereinafter, the present disclosure will be described in further detail using examples and the like, but the present invention is not limited to these examples.
[0112] <Experimental Example 1 to Example 3 and Comparative Example 1>
[0113] Pellicle package bodies having substrate layers and sealant layers of the materials and film thicknesses shown in the table were prepared. The total amount of outgassing of volatile organic components under heating conditions of 100°C for 30 minutes was measured for the pellicle package bodies obtained in each example by the above-mentioned measurement method (referred to as "total amount of outgassing of pellicle package bodies" in the table). The results are shown in Table 1. In addition, the values of breaking strength measured for the pellicle package bodies of each example by the above-mentioned measurement method were all within the range of 10N or more and 40N or less.
[0114] <Evaluation of the total amount of outgassing from pellicle modules>
[0115] (1) Preparation of various components as raw materials of mask adhesive
[0116] Thermoplastic elastomer (A)
[0117] Styrene-hydrogenated isoprene-styrene block copolymer (trade name "HYBRAR 7125" (manufactured by Kuraray Co., Ltd.), tanδ peak temperature: -5°C, styrene content: 20% by mass)
[0118] Tackifying resin (B)
[0119] Hydrogenated alicyclic petroleum resin: C9 hydrogenated petroleum resin (trade name "Alcon P-100" (manufactured by Arakawa Chemical Industries, Ltd.), softening point: 100±5°C, number average molecular weight (Mn): 610), rosin ester resin (trade name "PINECRYSTAL KE-311" (manufactured by Arakawa Chemical Industries, Ltd.), softening point: 100±5°C)
[0120] Softener
[0121] Polybutene (trade name: NISSAN POLYBUTENE 30N (manufactured by NOF Corporation))
[0122] ·wax
[0123] Polypropylene thermal decomposition type wax (trade name "HI-WAX NP055" (manufactured by Mitsui Chemicals, Inc.))
[0124] (2) Manufacturing of protective film components
[0125] 100 parts by mass of thermoplastic elastomer (A), 100 parts by mass of tackifier resin (B) and 200 parts by mass of softener are mixed in a total of 48 g to obtain a raw material mixture. The obtained raw material mixture is placed in Labo plastomill (manufactured by Toyo Seiki Seisaku-sho, Ltd., content: 60 mL) and sealed. Mix at 200°C and 100 rpm for 20 minutes to obtain a block-shaped mask adhesive. About 10 g of the mask adhesive is placed in a heating tank (tank temperature: 200°C) and melted. On the other hand, prepare Figure 1The anodized aluminum support frame 14 shown (external dimensions: 148.77 mm × 114.9 mm, frame height H: 2.5 mm, frame width W: 2 mm) is applied to one end face of the support frame 14 with a molten mask adhesive extruded from a needle connected to a heating tank to form an adhesive layer 15 for an original plate. The thickness of the adhesive layer 15 for an original plate formed is 0.6 mm. In addition, a spacer is arranged on the surface of the adhesive layer 15 for an original plate. The protective film 12 is attached to the other end face of the support frame 14 (i.e., the end face on the side where the adhesive layer 15 for an original plate is not formed) via a film adhesive layer 13 (fluoropolymer (AGC Corporation, CYTOP A type)), thereby obtaining a protective film assembly 10.
[0126] (Evaluation of total outgassing amount)
[0127] The pellicle of each example was prepared by placing it in a clean oven under an air atmosphere and heating it at a temperature within a range of 70° C. to 80° C. for 20 hours to perform a degassing treatment.
[0128] The protective membrane assembly was packaged using the protective membrane assembly packaging body of each example and stored at 23°C for 1 week. After the storage, the protective membrane assembly was taken out of the protective membrane assembly packaging body and placed in an oven. Then, the outgassing generated under heating conditions of 50°C for 4 hours was adsorbed on the powdered adsorbent material Tenax (trademark, manufactured by GL Science Co., Ltd.). After that, Tenax was set in the GCMS to measure the total amount (μg) (converted to n-decane) of outgassing of volatile organic components generated by the protective membrane assembly under heating conditions of 280°C for 10 minutes, and it was taken as the "total amount of outgassing of the protective membrane assembly (μg / protective membrane assembly)". The results are shown in Table 1.
[0129] In Table 1, polyethylene is marked as PE, and polyethylene terephthalate is marked as PET.
[0130] [Table 1]
[0131]
[0132] As shown in Table 1, it is found that the pellicle package of the example can reduce the amount of outgassing from the pellicle due to adhesion of outgassing of volatile organic components generated by the pellicle package, as compared with the pellicle package of the comparative example.
[0133] The entire disclosure of Japanese Patent Application No. 2022-045759 filed on March 22, 2022 is incorporated into this specification by reference.
[0134] All documents, patent applications, and technical standards described in this specification are incorporated herein by reference to the same extent as if each document, patent application, and technical standard was specifically and individually described as being incorporated by reference.
Claims
1. A pellicle package having a total outgassing amount of volatile organic components of 90 ppm or less under heating conditions of 100°C for 30 minutes. 2 . The pellicle package according to claim 1 , comprising at least two layers: a sealant layer and a base material layer. 3 . The pellicle package according to claim 2 , wherein the sealant layer has a thickness of 40 μm or less. 4 . The pellicle package according to claim 2 , further comprising an adhesive layer between the sealant layer and the base material layer. 5 . The pellicle package according to claim 2 , wherein the sealant layer comprises an ethylene-vinyl alcohol copolymer. 6 . The pellicle package according to claim 1 , wherein the rupture strength is 5 N or more and 50 N or less. 7 . The pellicle package according to claim 1 , which is a package for a pellicle having an adhesive for an original plate, wherein the adhesive for an original plate comprises a styrene butadiene-based adhesive.
8. A pellicle assembly container, comprising: Protective film components, a pellicle assembly container for accommodating the pellicle assembly, and A pellicle package according to any one of claims 1 to 4 that packages the pellicle package container.
9. The pellicle assembly container according to claim 8, wherein the pellicle assembly contains an adhesive for an original plate, The adhesive for the original plate is a styrene butadiene adhesive.