Solid oxide fuel cell and method for manufacturing solid oxide fuel cell
By adopting an open cathode structure and module end plate joint design in solid oxide fuel cells, the sealing problem caused by the recess of the power generation module is solved, the airtightness and conductivity are ensured, and the power generation performance is improved.
Patent Information
- Application Number
- CN202280093893.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2022-03-22
- Publication Date
- 2024-11-05
AI Technical Summary
In a solid oxide fuel cell, when multiple power generation modules are laminated, the central power generation portion may be depressed, making it difficult to guarantee the sealing properties between adjacent modules.
The solid oxide fuel cell design is adopted with an open cathode structure, in which the module end plate of the power generation module is bonded along the outer peripheral edge, forming a joint portion in the lamination direction, ensuring sealing and conductivity, and performing through welding or the like Join to avoid loading on internal components.
It effectively ensures the airtightness and conductivity between power generation modules, improves power generation performance, and enhances the contact effect between modules without affecting internal components.
Smart Images

Figure CN118901155A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a solid oxide fuel cell and a method for manufacturing the solid oxide fuel cell. Background Art
[0002] In fuel cells that operate at high temperatures, such as solid oxide fuel cells (SOFCs), there is a problem that the power generation unit deforms during operation. For example, in an SOFC composed of multiple stacked power generation modules, the power generation unit in the center is recessed, and there is a possibility that the sealing between adjacent power generation modules cannot be ensured.
[0003] JP2014-93168A discloses a fuel cell stack formed by stacking a plurality of power generation modules, wherein the power generation module is formed by stacking a plurality of single cells. In the fuel cell stack, the sealing portion formed on the frame at the periphery of the single cell is arranged in a zigzag shape along the stacking direction, so that the periphery of the single cell is bent, so that the periphery of the single cell follows the deformation of the center of the single cell in the stacking direction. Thus, the sealing is ensured. Summary of the invention
[0004] In the fuel cell stack described in JP2014-93168A, the sealing portion is configured in a serrated shape, so the rigidity of the periphery of the single cell is low, and even if the periphery of the power generation module is pressed to seal between the power generation modules, it cannot receive sufficient reaction force. Therefore, according to the technology described in JP2014-93168A, it is still possible that the sealing between adjacent power generation modules cannot be ensured.
[0005] The present invention has been made in view of the above-mentioned problems, and an object of the present invention is to provide a solid oxide fuel cell in which the sealing properties between power generation modules are ensured.
[0006] According to one aspect of the present invention, a solid oxide fuel cell having an open cathode structure is provided. The solid oxide fuel cell is composed of a plurality of stacked power generation modules, each of which is a stacked plurality of single cell units, and each power generation module is provided with a module end plate that seals at least the cathode reaction surface at one end in the stacking direction. In addition, the module end plate is provided with a joint portion along the outer periphery for joining adjacent power generation modules in the stacking direction. BRIEF DESCRIPTION OF THE DRAWINGS
[0007] Figure 1 It is an exploded perspective view of a solid oxide fuel cell according to a first embodiment of the present invention.
[0008] Figure 2 This is an exploded perspective view of the power generation module.
[0009] Figure 3 This is an exploded perspective view of a single battery unit.
[0010] Figure 4 It is a perspective view of a single battery unit.
[0011] Figure 5 It is a side view of two adjacent power generation modules.
[0012] Figure 6 This is a top perspective view of a power generation module in a solid oxide fuel cell according to a second embodiment.
[0013] Figure 7 It is a bottom-up stereoscopic view of the power generation module.
[0014] Figure 8 It is a diagram for explaining the engagement of ribs of two adjacent power generation modules.
[0015] Fig. 9 This is a top perspective view of a power generation module in a solid oxide fuel cell according to a modified example of the second embodiment.
[0016] Fig.10 This is a top perspective view of a power generation module in a solid oxide fuel cell according to a third embodiment.
[0017] Fig.11 It is a schematic side view of the vicinity of a joining portion between adjacent power generation modules in a solid oxide fuel cell according to a fourth embodiment. DETAILED DESCRIPTION
[0018] Hereinafter, embodiments of the present invention will be described with reference to the drawings and the like.
[0019] [First embodiment]
[0020] Figure 1 1 is an exploded perspective view of a solid oxide fuel cell (SOFC) 100 (hereinafter also referred to as a "fuel cell stack") according to the present embodiment. The solid oxide fuel cell 100 according to the present embodiment is mainly mounted on a vehicle or the like, but is not limited thereto.
[0021] like Figure 1 As shown, the fuel cell stack 100 is formed by stacking a plurality of power generation modules 10. Figure 1 In the figure, a structure formed by stacking five power generation modules 10 is referred to as a fuel cell stack 100, but the number of stacked power generation modules 10 is not limited thereto. In addition, although not shown, the fuel cell stack 100 includes end plates at both ends of the stacking direction of the power generation modules 10 and cover components that cover the entire stacked power generation modules 10.
[0022] Each power generation module 10 has a plurality of protrusions 11 extending from the outer periphery and protruding, and a manifold 12 is formed on the protrusion 11 as a hole for the fuel gas to flow in the stacking direction. In the present embodiment, two protrusions 11 are provided on one side of the power generation module 10 in the length direction (Japanese: long-hand direction), and one protrusion 11 is provided on the other side, but it is not necessarily limited to this. The fuel cell stack 100 stacks the power generation modules 10 in such a manner that the manifolds 12 of each power generation module 10 overlap. A manifold sealing member 121 is provided around the manifold 12 to seal the overlapping manifolds 12.
[0023] On the other hand, the cathode gas flowing in the stacking direction of the power generation modules 10 passes through a space formed between the recessed portion 13 corresponding to the convex portion 11 and a cover member covering the entire power generation module 10 .
[0024] Figure 2 is an exploded perspective view of the power generation module 10. Figure 2 As shown, the power generation module 10 is composed of a plurality of stacked single cell units 1. One side of each single cell unit 1 becomes a cathode reaction surface that reacts with the cathode gas (air), and the other side becomes an anode reaction surface that reacts with the anode gas (fuel gas). In this embodiment, the upper surface side of the single cell unit 1 is set as the anode reaction surface, and the lower surface side is set as the cathode reaction surface.
[0025] In addition, the power generation module 10 is provided with module end plates 2 at both ends of the stacking direction of the single battery cells 1. The module end plate 2 at one end of the stacking direction of the single battery cells 1 (the upper end of the power generation module 10) seals the cathode reaction surface of the one end of the stacking direction of the single battery cells 1 (the single battery cells 1 at the upper end in the stacking direction). The module end plate 2 at the other end of the stacking direction of the single battery cells 1 (the lower end of the power generation module 10) seals the anode reaction surface of the other end of the stacking direction of the single battery cells 1 (the single battery cells 1 at the lower end in the stacking direction).
[0026] The module end plate 2 is provided with a joint portion 21 along the outer periphery for joining the power generation modules 10 adjacent in the stacking direction. The module end plates 2 of the adjacent power generation modules 10 are joined to each other by the joint portion 21 at the outer periphery.
[0027] In addition, if Figure 2 As shown, a plurality of convex portions 14 that form the convex portion 11 of the power generation module 10 when stacked are provided from the outer periphery of each single battery unit 1 and the module end plate 2. A hole portion 15 is formed in the convex portion 14, and when a plurality of single battery units 1 are stacked, the hole portions 15 overlap to form the manifold 12 of the power generation module 10. An anode sealing member 151 is provided around the hole portion 15 to seal the overlapping hole portions 15.
[0028] Figure 3It is an exploded perspective view of the battery unit 1 .
[0029] like Figure 3 As shown, the single cell unit 1 includes a power generation single cell 3, a single cell frame 31 surrounding the outer periphery of the power generation single cell 3, a single cell sealing member 32, a channel flow path 4, a separator 5, an anode spacer 33, an anode sealing member 151, and a cathode spacer 35.
[0030] The power generation cell 3 is composed of a membrane electrode assembly in which an anode electrode is arranged on one side of a solid electrolyte layer and a cathode electrode is arranged on the other side. In this embodiment, the lower surface side of the power generation cell 3 is set as the anode electrode, and the upper surface side is set as the cathode electrode. Anode gas (fuel gas) and cathode gas (air) are supplied to the power generation cell 3, and the power generation cell 3 generates electricity based on the electrode reaction at the anode electrode and the cathode electrode. In addition, the power generation cell 3 can also be a structure including a support layer that supports the anode electrode and / or the cathode electrode.
[0031] The cell frame 31 is a frame body for fixing the power generating cells 3, and is arranged to surround the outer periphery of the power generating cells 3. The cell frame 31 has a plurality of protrusions 311 extending and protruding from the outer periphery, and holes 312 are formed in the protrusions 311.
[0032] The cell sealing member 32 is disposed so as to surround the outer circumference of the power generating cell 3 , and seals the space between the power generating cell 3 and the cell frame 31 .
[0033] The channel flow path 4 is formed of a conductive material such as metal, and is respectively arranged between the two surfaces of the power generation cell 3 and the separator 5 discussed later. It is a member that forms an anode flow path on one side of the power generation cell 3 and a cathode flow path on the other side. The channel flow path 4 is formed into a so-called wave shape in which the concavities and convexities extending linearly in the width direction of the power generation cell 3 are repeatedly arranged in the length direction. As a result, a plurality of anode flow paths are divided and formed between one side of the power generation cell 3 and the separator 5, and a cathode flow path is divided and formed between the other side of the power generation cell 3 and the separator 5 (of the adjacent single cell unit 1). In this embodiment, an anode flow path is formed on the lower surface side of the power generation cell 3, and a cathode flow path is formed on the upper surface side.
[0034] The separator 5 is a conductive plate-shaped member, and one surface of the separator 5 is conductively bonded to the channel flow path 4. Thus, the separator 5 and the power generation cell 3 are electrically connected via the channel flow path 4. The other surface of the separator 5 is bonded to the channel flow path 4 of the adjacent battery unit 1.
[0035] In addition, the separator 5 has a plurality of protrusions 51 extending from the outer periphery at positions corresponding to the protrusions 311 of the cell frame 31, and holes 52 are formed at positions corresponding to the holes 312 of the cell frame 31 in the protrusions 51. The holes 52 of the separator 5 overlap with the holes 312 of the cell frame 31, thereby forming the holes 15 ( Figure 2 As described above, the anode sealing member 151 is provided around the hole 15 .
[0036] The anode separator 33 is a frame body stacked on the outer periphery of the separator 5 and is disposed between the cell frame 31 and the separator 5 to ensure the height of the anode flow path. The anode separator 33 is disposed so that its outer shape overlaps with the cell frame 31 and the separator 5 .
[0037] The cathode spacers 35 are disposed at both ends of the channel flow path 4 on the cathode side in the longitudinal direction, and ensure the height of the cathode flow path and seal both ends of the channel flow path 4 in the longitudinal direction.
[0038] Figure 4 It is a perspective view of the assembled single battery unit 1.
[0039] like Figure 4 As shown, the single cell 1 is provided with a hole 15 constituting a manifold 12 through which the fuel gas flows in the convex portion 14 , and the hole 15 between the single cell 1 is sealed by an anode sealing member 151 .
[0040] On the other hand, in the single battery unit 1, the cathode gas flowing in the stacking direction passes through the following space, which is formed between the recessed portion 16 corresponding to the convex portion 14 and the cover component covering the entire power generation module 10. When a plurality of single battery units 1 are stacked, the recessed portions 16 overlap, thereby forming the recessed portion 13 ( Figure 1 ) That is, the fuel cell stack 100 has an open cathode structure in which a flow path of cathode gas flowing along the stacking direction is formed not in the single cell unit 1 but by a cover component.
[0041] However, solid oxide fuel cells (SOFCs) operate at high temperatures. Therefore, in SOFCs formed by stacking a plurality of power generation modules, the power generation section in the center of the power generation module may be recessed during operation, and there is a possibility that the sealing between adjacent power generation modules cannot be ensured.
[0042] In contrast, in the solid oxide fuel cell 100 of the present embodiment, the power generation module 10 includes module end plates 2 at both ends in the stacking direction of the single cell units 1, and the outer peripheral edges of the module end plates 2 of adjacent power generation modules 10 are joined to each other by joints 21. Therefore, even if the center of the power generation module 10 is deformed, the sealing between the power generation modules 10 is ensured because the joints 21 are set at the portions that become the nodes of the deformation.
[0043] Hereinafter, the details of joining the module end plates 2 of adjacent power generation modules 10 will be described.
[0044] Figure 5 is a side view of two power generation modules 10 adjacent to each other in the stacking direction, and is viewed from Figure 1 The figure is viewed in the X direction. The power generation module on the upper side in the stacking direction is referred to as the power generation module 10A, and the power generation module on the lower side is referred to as the power generation module 10B.
[0045] like Figure 5 As shown, the module end plates 2 are disposed at both ends of the stacked battery cells 1 in the stacking direction, so as to seal the anode reaction surfaces and cathode reaction surfaces of the ends of the battery cells 1 in the stacking direction.
[0046] In addition, if Figure 5 As shown, the module end plate 2 is formed to be larger than the outer shape of the single battery unit 1 constituting the power generation module 10 in a plan view. The module end plate 2 is formed with a joint portion 21 along the outer peripheral edge of the module end plate 2 at a position offset in the outer peripheral direction relative to the single battery unit 1. In addition, the module end plate 2A that seals the anode reaction surface at the lower end of the power generation module 10A and the module end plate 2B that seals the cathode reaction surface at the upper end of the power generation module 10B are joined at the joint portion 21 with each other by conductive joining such as welding.
[0047] In this way, adjacent power generation modules 10 are joined to each other at the joint 21 along the peripheral portion of the module end plate 2. Therefore, even if the center of the power generation module 10 is deformed, the air tightness (sealing) between the power generation modules 10 is ensured because the joint 21 is formed at the portion that becomes the node of the deformation.
[0048] In addition, since the adjacent power generation modules 10 are joined by a conductive joint, the conductivity is ensured between the power generation modules 10. That is, the airtightness and the conductivity between the power generation modules 10 can be ensured at the same time.
[0049] Furthermore, the joint 21 for joining the adjacent power generation modules 10 is formed at a position offset in the outer peripheral direction relative to the single battery unit 1, so that when the adjacent power generation modules 10 are joined, no load is applied to the internal components of the power generation modules 10 (components constituting the single battery unit 1, etc.). Therefore, the load for joining can be applied to the joint 21 without considering the load on the internal components of the power generation module 10, and the power generation modules 10 can be brought into better contact with each other.
[0050] Furthermore, in the case where the fuel cell stack has a closed cathode structure in which the flow path of the cathode gas flowing in the stacking direction is sealed within the single cell unit, if the module end plate is used to seal both ends of the single cell unit in the stacking direction, it may be impossible to access the inside of the power generation module and the anode gas cannot be fully sealed. In contrast, in the present embodiment, an open cathode structure is used, so that even after the module end plate 2 is joined, the inside of the power generation module 10 can be accessed and the anode flow path can be sealed.
[0051] According to the solid oxide fuel cell 100 of the first embodiment described above, the following effects can be obtained.
[0052] The power generation module 10 of the solid oxide fuel cell 100 is provided with a module end plate 2 at both ends in the stacking direction of the single cell unit 1, and the module end plate 2 is provided with a joint portion 21 along the outer periphery for joining the power generation modules 10 adjacent in the stacking direction. In addition, the outer peripheries of the module end plates 2 of the power generation modules 10 adjacent in the stacking direction are joined to each other by the joint portion 21. Therefore, during the operation of the solid oxide fuel cell 100, even if the center of the power generation module 10 is deformed, the sealing (airtightness) between the power generation modules 10 is ensured because the joint portion 21 is set at the portion that becomes the node of the deformation.
[0053] Each power generation module 10 of the solid oxide fuel cell 100 is joined to a power generation module 10 adjacent in the stacking direction by a conductive joint at a joint portion 21 along the outer periphery of the power generation module 10. Thus, the sealing (airtightness) between the power generation modules 10 is ensured, and the conductivity between the power generation modules 10 is ensured. That is, the airtightness and the conductivity between the power generation modules 10 can be ensured at the same time.
[0054] The module end plate 2 of the solid oxide fuel cell 100 is formed to be larger than the outer shape of the single cell unit 1 constituting the power generation module 10 when viewed from above, and the joint portion 21 of the module end plate 2 is formed at a position offset in the peripheral direction relative to the single cell unit 1. Therefore, when the adjacent power generation modules 10 are joined, no load is applied to the internal components of the power generation module 10 (components constituting the single cell unit 1, etc.). Therefore, the load for joining can be applied to the joint portion 21 without considering the load on the internal components of the power generation module 10, and the power generation modules 10 can be brought into better contact with each other. Therefore, the power generation performance of the solid oxide fuel cell 100 is improved.
[0055] In addition, in the present embodiment, the power generation modules 10 are joined by welding, but the method is not limited thereto, and the joining may be done by brazing or the like, for example. Furthermore, the power generation modules 10 are preferably joined by a conductive joint, but the method is not necessarily limited thereto, and the power generation modules 10 may be joined by a non-conductive joint such as a glass or ceramic adhesive. When the power generation modules 10 are bent and deformed, the module end plates 2 of the adjacent power generation modules 10 contact each other at the outside of the joint 21, so that the conductivity between the power generation modules 10 can be ensured even with a non-conductive joint.
[0056] In addition, in the present embodiment, the module end plates 2 are provided at both ends of the stacking direction of the single cell unit 1, but the present invention is not necessarily limited to this. The module end plates 2 may be provided only on the cathode reaction surface side, which is one end of the stacking direction of the single cell unit 1. In this case, the anode reaction surface at the other end of the stacking direction of the single cell unit 1 in the adjacent power generation module 10 is joined to the joint portion 21 of the module end plate 2 that seals the cathode reaction surface. That is, one module end plate 2 is shared as an end plate that seals the cathode reaction surface and the anode reaction surface.
[0057] In addition, as in the present embodiment, the joint 21 of the module end plate 2 is preferably formed at a position offset in the peripheral direction relative to the single battery cell 1, but it is not necessarily limited to this. Even in the case where the joint 21 is formed at a position overlapping with the single battery cell 1, as long as the joint 21 is formed along the outer peripheral edge of the module end plate 2, the joint 21 is set at a portion that becomes a node of deformation, so that the sealing (airtightness) between the power generation modules 10 is also ensured.
[0058] [Second embodiment]
[0059] Reference Figure 6 to Figure 8 , a solid oxide fuel cell 100 according to a second embodiment is described. This embodiment is different from the first embodiment in that adjacent power generation modules 10 are rib-fitted to each other. Elements identical to those of the first embodiment are denoted by the same reference numerals, and description thereof is omitted.
[0060] Figure 6 is a three-dimensional view of the power generation module 10 viewed from the upper surface direction. Figure 7 This is a perspective view of the power generation module 10 as viewed from the bottom surface. Figure 6 and Figure 7 This is a diagram showing a state before a plurality of power generation modules 10 are joined together.
[0061] like Figure 6 and Figure 7 As shown, the power generation module 10 has a rib 17A protruding from the upper surface of the module end plate 2 at the upper end in the stacking direction of the single battery unit 1, and a rib 17B protruding from the lower surface of the module end plate 2 at the lower end in the stacking direction in a direction substantially perpendicular to the rib 17A.
[0062] In addition, in the power generation module 10, the upper surface of the module end plate 2 at the upper end in the stacking direction of the single battery unit 1 is formed with a fitting portion 18A as a groove into which the rib 17B is fitted, at a position corresponding to the rib 17B, and the rib 17B is formed protruding from the lower end of the power generation module 10 adjacent in the stacking direction (upward direction). On the other hand, in the lower surface of the module end plate 2 at the lower end in the stacking direction, the fitting portion 18B as a groove into which the rib 17A is fitted is formed at a position corresponding to 17A, and the rib 17A is formed protruding from the upper end of the power generation module 10 adjacent in the stacking direction (downward direction). As a result, when the power generation modules 10 are stacked, the rib 17A at the upper end of the power generation module 10 is fitted with the fitting portion 18B at the lower end, and the rib 17B at the lower end of the power generation module 10 is fitted with the fitting portion 18A at the upper end.
[0063] Figure 8 It is an enlarged view of a cross section of a rib fitting portion between adjacent power generation modules 10 .
[0064] like Figure 8 As shown, the rib 17A formed protruding from the upper end of the power generation module 10B of the power generation module 10A and the power generation module 10B adjacent in the stacking direction is engaged with the engaging portion 18B formed at the lower end of the power generation module 10A. Figure 8 This is a cross-sectional view of a portion where rib 17A of power generation module 10B is fitted with fitting portion 18B of power generation module 10A. Similarly, rib 17B formed protruding at the lower end of power generation module 10A is fitted with fitting portion 18B formed at the upper end of power generation module 10B.
[0065] In this way, adjacent power generation modules 10 are rib-fitted with each other, thereby suppressing displacement in the plane direction of the solid oxide fuel cell (fuel cell stack) 100. As a result, the vibration resistance of the solid oxide fuel cell (fuel cell stack) 100 is improved.
[0066] In addition, Figure 6 and Figure 7 In the embodiment, a plurality of ribs 17B extending in the longitudinal direction of the power generation module 10 are formed on the lower surface of the module end plate 2 at the lower end in the stacking direction, and ribs 17A in a direction substantially perpendicular to the ribs 17B are formed on the upper surface of the module end plate 2 at the upper end in the stacking direction, but the present invention is not necessarily limited thereto. The position and number of the ribs 17 formed on the module end plate 2 can be arbitrarily determined. In addition, the fitting portion 18 can be provided at a position corresponding to the rib 17.
[0067] [Modification of the Second Embodiment]
[0068] Reference Fig. 9 , a solid oxide fuel cell 100 according to a modified example of the second embodiment will be described. Elements identical to those of other embodiments are denoted by the same reference numerals, and description thereof will be omitted.
[0069] Fig. 9 This is a perspective view of the power generation module 10 as viewed from the upper surface. Fig. 9 This is a diagram showing a state before a plurality of power generation modules 10 are joined together.
[0070] like Fig. 9 As shown, in this modified example, for the power generation module 10, the ribs 17 provided on the upper surface of the module end plate 2 at the upper end in the stacking direction of the single cell unit 1 are formed around the manifold 12 for the fuel gas to flow along the stacking direction. In addition, although not shown, on the lower surface of the module end plate 2 at the lower end in the stacking direction of the single cell unit 1, an engaging portion as a groove for the rib 17 to engage is formed at a position corresponding to the rib 17 of the power generation module 10 adjacent in the stacking direction (below). As a result, when the power generation modules 10 are stacked, the rib 17 at the upper end of the power generation module 10 is engaged with the engaging portion at the lower end of the power generation module 10 adjacent in the stacking direction. As a result, displacement of the solid oxide fuel cell (fuel cell stack) 100 in the plane direction is suppressed, and the vibration resistance of the solid oxide fuel cell (fuel cell stack) 100 is improved.
[0071] In addition, ribs 17 that fit into the fitting portion are formed around manifold 12, thereby preventing fuel gas from flowing in the planar direction between adjacent power generation modules 10. That is, the airtightness of manifold 12 is improved, and the power generation performance of solid oxide fuel cell 100 is improved.
[0072] [Third Embodiment]
[0073] Reference Fig.10 A solid oxide fuel cell 100 according to a third embodiment will be described. Elements identical to those of other embodiments are denoted by the same reference numerals, and description thereof will be omitted.
[0074] Fig.10 is a perspective view of the power generation module 10 as viewed from the upper surface direction. In addition, Fig.10 is a view of the state before the power generation modules 10 are joined to each other.
[0075] In this embodiment, the power generation module 10 is different from other embodiments in that it includes a high thermal conductivity layer 7.
[0076] As Fig.10 shown, the power generation module 10 has a high thermal conductivity layer 7 at the central portion above the module end plate 2 at the upper end in the stacking direction of the single cell units 1. The high thermal conductivity layer 7 is made of a material with a high thermal conductivity (Japanese: 熱伝導率の高い材料), for example, graphite, or metals such as silver, copper, aluminum, nickel, or ferritic stainless steel. Thereby, the thermal conductivity in the plane direction in the power generation portion of the power generation module 10 is increased, and the power generation performance of the solid oxide fuel cell 100 is improved.
[0077] In addition, as in this embodiment, the high thermal conductivity layer 7 is preferably provided at the central portion above the module end plate 2, but is not necessarily limited thereto, and may be provided at any position above the module end plate 2.
[0078] [Fourth Embodiment]
[0079] Refer to Fig.11 , and explain the solid oxide fuel cell 100 of the fourth embodiment. In addition, the same elements as those in other embodiments are denoted by the same reference numerals, and their explanations are omitted.
[0080] Fig.11 is a schematic side view of the vicinity of the joint portion 21 of adjacent power generation modules 10, and is a view for explaining the stacking process of the adjacent power generation modules 10 in the stacking direction. Fig.11 In (a) of Fig.11 , it is a view before the adjacent power generation modules 10 are stacked, in (b) it is a view when the adjacent power generation modules 10 are stacked, and in (c) it is a view when the stacking of the adjacent power generation modules 10 is completed. In addition, in Fig.11 , for convenience, the stacking process of two adjacent power generation modules 10 is shown, but each of the stacked multiple power generation modules 10 has the structure shown in
[0081] As Fig.11 shown in (a) of Fig.11As shown in (b), when the power generation modules 10 are stacked, the curved portions 23 of the module end plates 2 of the adjacent power generation modules 10 contact each other before the flat portions 22. The module end plates 2 of the adjacent power generation modules 10 are joined (welded) at the portions of the curved portions 23 that first contact each other when stacked. That is, the joint 21 is formed at the portions that first contact each other when stacked.
[0082] like Fig.11 As shown in (c) , when the stacking of the power generation modules 10 is completed, the module end plates 2 of the adjacent power generation modules 10 are in contact with each other at least at the joints 21 .
[0083] In this way, the power generation modules 10 are stacked after being bent so that the bending angle θ1 of the module end plate 2 at the upper end in the stacking direction is smaller than the bending angle θ2 of the module end plate 2 at the lower end in the stacking direction, so that the ends in the length direction are initially in contact when the power generation modules 10 are stacked. In addition, the module end plates 2 of adjacent power generation modules 10 are joined (welded) to each other at the initial contact portion, so that the adjacent power generation modules 10 are in contact at least at the ends of the module end plates 2. Therefore, the joining of the power generation modules 10 to each other is more reliably ensured, and the conductivity between the power generation modules 10 is improved. That is, the power generation performance of the solid oxide fuel cell 100 is improved.
[0084] As mentioned above, although the embodiment of the present invention has been described, the above embodiment merely shows a part of application examples of the present invention, and the protection scope of the present invention is not intended to be limited to the specific structure of the above embodiment.
[0085] The above-mentioned embodiments are described as separate embodiments, but they can be appropriately combined.
Claims
1. A solid oxide fuel cell having an open cathode structure, wherein: The solid oxide fuel cell is composed of a plurality of stacked power generation modules, and the power generation module is composed of a plurality of stacked single cell units. Each power generation module includes a module end plate that seals at least the cathode reaction surface that is one end in the stacking direction. The module end plate is provided with a joint portion along the outer periphery for joining the power generation modules adjacent to each other in the stacking direction.
2. The solid oxide fuel cell according to claim 1, wherein: Each power generation module is joined to a power generation module adjacent to the stacking direction at the joining portion by conductive bonding.
3. The solid oxide fuel cell according to claim 2, wherein: Each power generation module includes module end plates at both ends in the stacking direction, and outer peripheral edges of the module end plates of adjacent power generation modules are joined to each other by the joining portion.
4. The solid oxide fuel cell according to claim 3, wherein: The module end plate is formed to be larger than the outer shape of the single battery unit constituting the power generation module in a plan view. The joining portion of the module end plate is formed at a position offset in an outer peripheral direction with respect to the battery cell.
5. The solid oxide fuel cell according to claim 3, wherein: The module end plate of one of the adjacent power generation modules is protrudingly formed with ribs, The module end plate of the other power generation module is formed with an engaging portion that engages with the rib.
6. The solid oxide fuel cell according to claim 5, wherein: The power generation module has a manifold for allowing fuel gas to flow in the stacking direction. The ribs are formed around the manifold.
7. The solid oxide fuel cell according to any one of claims 1 to 6, wherein Each power generation module has a high thermal conductivity layer with a high thermal conductivity, and the high thermal conductivity layer is located between power generation modules adjacent to each other in the stacking direction.
8. A method for manufacturing a solid oxide fuel cell having an open cathode structure, wherein: A plurality of single battery cells are stacked, and a cathode reaction surface at least at one end in the stacking direction is sealed by a module end plate to form a power generation module. stacking a plurality of the power generation modules, The solid oxide fuel cell is constructed by joining each power generation module to a power generation module adjacent to the power generation module in the stacking direction at the outer peripheral edge of the module end plate.
9. The method for manufacturing a solid oxide fuel cell according to claim 8, wherein: A plurality of single battery cells are stacked, and both ends of the stacking direction are sealed using module end plates to form a power generation module. The end portions of the module end plates in the longitudinal direction are bent and formed. The solid oxide fuel cell is constructed by stacking a plurality of power generation modules having the module end plates formed by bending. The bending angle of the bending formation of the module end plate at the upper end in the stacking direction is smaller than the bending angle of the bending formation of the module end plate at the lower end in the stacking direction.