Heat-resistant chocolate product with freeze-dried composite skeleton as well as preparation method and application of heat-resistant chocolate product
The heat-resistant chocolate products that form a lyophilized composite skeleton by hydrogel and water-soluble ingredients solve the problems of harsh storage and transportation conditions and high sugar content of existing chocolate products, and achieve heat resistance and low energy consumption at room temperature effect.
Patent Information
- Application Number
- CN202410964503.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-18
- Publication Date
- 2024-11-08
AI Technical Summary
The existing chocolate products have harsh storage and transportation conditions, need cold chain transportation, and have high sugar content, which leads to high energy consumption and health risks, and lacks non-sugar-sustaining chocolate products that are heat-resistant and have low sugar content.
The heat-resistant chocolate product is used to form a lyophilized composite skeleton by dispersing the chocolate in the cavity of the lyophilized composite skeleton, and the heat-resistant lyophilized composite skeleton is formed by dispersing the chocolate in the cavity of the lyophilized composite skeleton, and the hydrogel and inulin are used to form a heat-resistant lyophilized composite skeleton. The chocolate does not melt at 120°C and reduces overall calories.
The heat resistance performance of storage and transportation at room temperature is achieved, the energy consumption of chocolate products is reduced, and the calories is not increased, and the good shape and food safety is maintained.
Smart Images

Figure BDA0004951345510000021 
Figure BDA0004951345510000022 
Figure BDA0004951345510000081
Abstract
Description
Technical Field
[0001] The present invention relates to the field of food technology, and in particular to a heat-resistant chocolate product with a freeze-dried composite skeleton, a preparation method and an application thereof. Background Art
[0002] Chocolate is a popular classic snack. Classic chocolate is known for its sweet and smooth taste, but there are two pain points. First, the bitter taste of pure cocoa ingredients requires the addition of a lot of sucrose or sugar alcohol to adjust the taste. Excessive intake of sucrose can easily lead to obesity, and excessive intake of sugar alcohol can easily lead to diarrhea. Second, the storage and transportation conditions are relatively harsh. The national standard "GB / T19343 Chocolate and Chocolate Products, Cocoa Butter Substitute Chocolate and Cocoa Butter Substitute Chocolate Products" recommends storage conditions: temperature ≤25℃, relative humidity ≤65%. Cold chain is required for transportation in summer, and storage and transportation consumes a lot of energy and has high costs.
[0003] Patent CN115777820A provides a low-sugar, high-fiber dark chocolate. This product uses sugar alcohols to replace sucrose to provide sweetness, and dietary fiber is added to achieve high fiber. However, the chocolate has a low melting point (about 32-36°C), requires cold chain transportation, and the use of a large amount of sugar alcohols is not good for consumer health. Patent CN116508870A provides a freeze-dried chocolate. This product is made by mixing, emulsifying, homogenizing, and freeze-drying oils and water-soluble components, but its structural skeleton is mainly sugar alcohols or sugars. Excessive consumption of sugars can easily lead to obesity and excessive consumption of sugar alcohols can easily lead to diarrhea, which does not meet consumer demand. Patent CN107594047A provides a heat-resistant chocolate product composition. The composition is made by mixing ethyl cellulose oil gel with chocolate. Its melting point is between 30 and 40°C, and its heat resistance is average. It still needs cold chain transportation in summer; and after the introduction of non-cocoa vegetable oil exceeding 5%, the product does not meet the definition of chocolate in "GB 9678.2 National Food Safety Standard Chocolate, Cocoa Butter Replacement Chocolate and Its Products". Patent CN 115997834A provides a freeze-dried chocolate, the melting point of which is ≥65°C, which is mainly achieved by reducing the fat content of chocolate and adding special chocolate powder (ZL 201910303370.5), wherein the fat content is ≤25%, but the special chocolate powder contains sucrose, lactose, glucose and other sugars, and its structural skeleton is sugar, with a high sugar content, which does not meet the needs of modern consumers. Patent CN102150728A provides a heat-resistant chocolate-type food with a cottony texture, in which a flowable chocolate-type component is mixed with anionic microbial polysaccharides to prepare gel particles, in which the microbial polysaccharides are evenly distributed, forming a chocolate-type food with a little chewiness and high heat resistance. It can be seen that the prior art lacks a heat-resistant and low-sugar non-sugar substitute chocolate product. Summary of the invention
[0004] In order to solve the above technical problems, the present invention provides a heat-resistant chocolate product with a composite skeleton formed by freeze-drying a hydrogel and a water-soluble component, which can meet the requirements of storage, transportation and carrying at room temperature and has low overall calories.
[0005] The first aspect of the present invention provides a heat-resistant chocolate product having a freeze-dried composite skeleton, which is made from the following raw materials in parts by weight:
[0006]
[0007] The hydrogel and the water-soluble component together constitute a freeze-dried composite skeleton, and chocolate is dispersed in the cavity of the freeze-dried composite skeleton; the water-soluble component includes inulin; and the heat-resistant chocolate product does not melt when placed at 120° C. for 12 hours.
[0008] Preferably, the heat-resistant chocolate product is made of the following raw materials in parts by weight:
[0009]
[0010] In some preferred embodiments of the present invention, the raw materials of the heat-resistant chocolate product do not include sugar and sugar substitutes, and the heat-resistant chocolate product has lower calories than chocolate of the same weight. The "sugar" described in the present invention refers to monosaccharides and disaccharides, including but not limited to white sugar, glucose, and lactose. The "sugar substitute" described in the present invention refers to sugar alcohols and high-intensity sweeteners, such as erythritol, mogroside, acesulfame potassium, sucralose, aspartame, neotame, saccharin sodium, steviol glycosides, etc.
[0011] In a preferred embodiment of the present invention, the heat-resistant chocolate product is made of the following raw materials in parts by weight: 17 parts of hydrogel, 24.9 parts of inulin, 58 parts of chocolate and 0.1 parts of soybean lecithin. In a preferred embodiment of the present invention, the heat-resistant chocolate product is made of the following raw materials in parts by weight: 5 parts of hydrogel, 58 parts of 100% dark chocolate, 36.9 parts of inulin, and 0.1 parts of lecithin. In a preferred embodiment of the present invention, the heat-resistant chocolate product is made of the following raw materials in parts by weight: 31 parts of hydrogel, 58 parts of 100% dark chocolate, 10.9 parts of inulin, and 0.1 parts of polyglycerol ricinoleate.
[0012] Preferably, the hydrogel is prepared according to the method of CN115918889A. Preferably, the hydrogel is a hydrogel formed by physically crosslinking polysaccharide gum and cellulose or its derivatives as raw materials; further preferably, the hydrogel is a hydrogel obtained by drying an aqueous solution of sodium carboxymethyl cellulose and pectin at 100°C to 120°C for 8h to 12h.
[0013] Preferably, in the present invention, the hydrogel is a gel dry particle with a particle size of 10 mesh or more; further preferably, the particle size of the hydrogel dry particle is 20-200 mesh.
[0014] Preferably, in the present invention, the water-soluble component further comprises one or more of water-soluble dietary fiber, fruit and vegetable powder, milk powder, medicinal and edible plant extracts, small molecule peptides, water-soluble vitamins, prebiotics and sodium hyaluronate.
[0015] In the preferred embodiment of the present invention, the chocolate is selected from one or more of cocoa butter, cocoa mass and cocoa liquor, and more preferably cocoa mass. In the preferred embodiment of the present invention, the chocolate may further include auxiliary materials such as phospholipids and polyglycerol ricinoleate.
[0016] Preferably, in the present invention, the emulsifier is selected from one or more of soybean lecithin, lecithin, polyglycerol ricinoleate, mono- and di-glycerol fatty acid esters, polyglycerol fatty acid esters, succinic acid monoglyceride, sucrose fatty acid esters, sodium octenyl succinate starch and acetylated mono- and di-glycerol fatty acid esters.
[0017] The second aspect of the present invention provides a method for preparing a heat-resistant chocolate product having a freeze-dried composite skeleton according to the above technical solution, comprising the following steps:
[0018] S1, dissolving the water-soluble component and the hydrogel in water, and standing for more than 15 minutes to obtain an aqueous phase;
[0019] S2, adding the melted chocolate and the emulsifier into the water phase, stirring until no obvious particles are left, to obtain an oil-in-water chocolate emulsion;
[0020] S3, freeze-drying the oil-in-water chocolate emulsion composite liquid to obtain the heat-resistant chocolate product.
[0021] In the preferred embodiment of the present invention, the mass of water in step S1 is more than 10 times the mass of the hydrogel. In the preferred embodiment of the present invention, the standing time in step S1 is 15 min to 30 min.
[0022] In the preferred embodiment of the present invention, the melting temperature of the chocolate in step S2 is 40° C. to 55° C. In the preferred embodiment of the present invention, the stirring rate in step S2 is preferably greater than or equal to 200 rpm / min.
[0023] Preferably, in step S2, the freeze-drying conditions are: divided into three stages: pre-freezing, sublimation drying, and desorption drying:
[0024] Pre-freezing conditions are: temperature -40℃~-25℃, time 1~12h;
[0025] Sublimation drying conditions are: temperature -40℃~-25℃, time 8~72h, pressure 50~6000Pa;
[0026] The desorption drying conditions are: temperature 8-50°C, time 8-72h.
[0027] The third aspect of the present invention provides an application of the heat-resistant chocolate product described in the above technical solution or the heat-resistant chocolate product prepared by the method described in the above technical solution in preparing food. The food includes but is not limited to cakes, cold drinks, candies, beverages, bread, etc.
[0028] Compared with the prior art, the present invention has the following beneficial effects:
[0029] The present invention unexpectedly discovered that the heat-resistant chocolate product obtained by mixing the hydrogel with water-soluble ingredients such as inulin to form an aqueous phase, emulsifying the chocolate containing fat (oil phase) and the aqueous phase to form a chocolate emulsion, and freeze-drying the chocolate emulsion has extremely excellent heat resistance and will not melt after being placed at 120°C for 12 hours, effectively reducing the storage and transportation costs of chocolate products. Since the oil phase and the aqueous phase exist in the form of an oil-in-water emulsion under the action of an emulsifier, during the freeze-drying process, the water gradually sublimates, and the saturated hydrogel and the water-soluble ingredients are dehydrated and solidified, and finally form a composite structural skeleton with dense cavities (such as Figures 1-2 The comparison shown in the figure shows that the fat is dispersed in the gaps of the skeleton composed of hydrogel and water-soluble components. The melting point of the dry hydrogel and the solidified water-soluble components is much higher than that of the fat. Therefore, using the hydrogel and the water-soluble components as the structural skeleton of the freeze-dried chocolate can make the freeze-dried chocolate have super high heat resistance. Even if the fat melts at a high temperature, the melted fat only flows in the gaps of the structural skeleton composed of the hydrogel and the water-soluble components, causing the structure and density of the gaps in the structural skeleton to change. Even if a small amount of fat leaks, it will not cause the structural skeleton to collapse overall, and the freeze-dried chocolate can still maintain a good plastic state. Therefore, the freeze-dried chocolate has excellent tolerance to temperature.
[0030] The present invention shows that compared with chocolate products with a skeleton formed by freeze-drying hydrogel or inulin alone, heat-resistant chocolate products with a freeze-dried composite skeleton formed by hydrogel and water-soluble components including inulin have heat resistance far exceeding that of a single component, and the synergistic effect is obvious. The effect may be that after the hydrogel is dehydrated, a cavity is formed to form a macroscopic structure, and the water-soluble substance is precipitated on the cavity wall in a stacking manner to form a microscopic structure, and is compounded with the hydrogel structure to improve the strength of the structure, thereby showing an unexpected synergistic effect of enhancing heat resistance.
[0031] Compared with ordinary dark chocolate of the same quality, the heat-resistant chocolate product provided by the present invention has significantly reduced energy by more than 25%, and has the advantage of lower calories. On the one hand, the hydrogel and inulin that constitute the freeze-dried composite skeleton cannot be decomposed in the body and will not increase calories; on the other hand, the hydrogel and inulin that constitute the freeze-dried composite skeleton firmly lock the chocolate in a dense cavity, which helps to reduce the absorption and metabolic rate of chocolate in the body. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] Figure 1 is a cross-sectional view of the heat-resistant chocolate product of the present invention;
[0033] Figure 2 A cross-section of 100% dark chocolate. DETAILED DESCRIPTION
[0034] To make the purpose, technical scheme and advantages of the present invention clearer, the technical scheme in the embodiment of the present invention will be clearly and completely described below in conjunction with the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in the art without making creative work are within the scope of protection of the present invention. The experimental methods in the following examples that do not specify specific conditions are usually based on conventional conditions or according to the conditions recommended by the manufacturer. All raw materials that do not specify the synthesis method are purchased from the market.
[0035] Example 1
[0036] A heat-resistant chocolate product comprises, by weight, 17 parts of hydrogel, 58 parts of 100% dark chocolate, 24.9 parts of inulin, and 0.1 parts of soybean lecithin. The heat-resistant chocolate product is prepared by the following method:
[0037] (1) Preparation of hydrogel: by weight, 69 parts of sodium carboxymethyl cellulose and 1 part of pectin were dissolved in 1050 parts of water, dried at a drying temperature of 110° C. for 8 h, crushed and sieved, and a 100-140 mesh hydrogel was taken for later use;
[0038] (2) Preparation of aqueous phase: 17 parts of hydrogel particles, 24.9 parts of inulin, and 500 parts of water were mixed and gently stirred, and allowed to stand for 30 minutes;
[0039] (3) Emulsification: melt 58 parts of 100% dark chocolate and 0.1 parts of soybean lecithin at 50° C. in water and then slowly add them to the aqueous phase prepared in (2), stirring at 200 rpm for 1 hour until no obvious particles are present, to obtain a chocolate emulsion;
[0040] (4) Drying: The chocolate emulsion is poured into a mold and freeze-dried to obtain a heat-resistant chocolate product 1.
[0041] Among them, the freeze-drying conditions are divided into three stages: pre-freezing, sublimation drying, and desorption drying:
[0042] Prefreezing conditions are: temperature -40℃, time 4h;
[0043] Sublimation drying conditions are: temperature -40 °C, time 12 h, pressure 1000 Pa;
[0044] The desorption drying conditions are: temperature 15°C, time 12h.
[0045] Example 2
[0046] A heat-resistant chocolate product comprises, by weight, 5 parts of hydrogel, 58 parts of 100% dark chocolate, 36.9 parts of inulin, and 0.1 parts of lecithin. The heat-resistant chocolate product is prepared by the following method:
[0047] (1) Preparation of hydrogel: by weight, 69 parts of sodium carboxymethyl cellulose and 1 part of pectin were dissolved in 1050 parts of water, dried at a drying temperature of 110° C. for 8 h, crushed and sieved, and a 20-80 mesh hydrogel was taken for later use;
[0048] (2) Preparation of aqueous phase: 5 parts of hydrogel particles, 36.9 parts of inulin, and 300 parts of water were mixed and gently stirred, and allowed to stand for 30 minutes;
[0049] (3) Emulsification: melt 58 parts of 100% dark chocolate and 0.1 parts of lecithin at 50° C. and then slowly add them to the aqueous phase prepared in (2), stirring at 200 rpm for 1 hour until no obvious particles are present, to obtain a chocolate emulsion;
[0050] (4) Drying: The chocolate emulsion is poured into a mold and freeze-dried to obtain a heat-resistant chocolate product 2.
[0051] Among them, the freeze-drying conditions are divided into three stages: pre-freezing, sublimation drying, and desorption drying:
[0052] Prefreezing conditions are: temperature -40℃, time 4h;
[0053] Sublimation drying conditions are: temperature -40 °C, time 12 h, pressure 1000 Pa;
[0054] The desorption drying conditions are: temperature 15°C, time 12h.
[0055] Example 3
[0056] A heat-resistant chocolate product comprises, by weight, 31 parts of hydrogel, 58 parts of 100% dark chocolate, 10.9 parts of inulin, and 0.1 parts of polyglycerol ricinoleate. The heat-resistant chocolate product is prepared by the following method:
[0057] (1) Preparation of hydrogel: by weight, 69 parts of sodium carboxymethyl cellulose and 1 part of pectin were dissolved in 1050 parts of water, dried at a drying temperature of 110° C. for 8 h, crushed and sieved, and a 40-100 mesh hydrogel was taken for later use;
[0058] (2) Preparation of aqueous phase: 31 parts of hydrogel particles, 10.9 parts of inulin, and 800 parts of water were mixed and gently stirred, and allowed to stand for 30 minutes;
[0059] (3) Emulsification: melt 58 parts of 100% dark chocolate and 0.1 parts of polyglycerol ricinoleate at 50° C. in water and then slowly add them into the aqueous phase prepared in (2), stirring at 200 rpm for 1 hour until no obvious particles are present, to obtain a chocolate emulsion;
[0060] (4) Drying: The chocolate emulsion is poured into a mold and freeze-dried to obtain a heat-resistant chocolate product 3.
[0061] Among them, the freeze-drying conditions are divided into three stages: pre-freezing, sublimation drying, and desorption drying:
[0062] Prefreezing conditions are: temperature -40℃, time 4h;
[0063] Sublimation drying conditions are: temperature -40 °C, time 12 h, pressure 1000 Pa;
[0064] The desorption drying conditions are: temperature 15°C, time 12h.
[0065] Comparative Example 1
[0066] The only difference from Example 1 is that inulin is not added, and the other steps and raw material amounts are the same. Comparative Sample 1 is obtained.
[0067] Comparative Example 2
[0068] The only difference from Example 1 is that no hydrogel is added and no hydrogel needs to be prepared, and the other steps and raw material amounts are the same. Comparative Sample 2 is obtained.
[0069] Comparative Example 3
[0070] The only difference from Example 1 is that inulin and hydrogel are not added, and hydrogel does not need to be prepared, and the other steps and raw material amounts are the same. Comparative Sample 3 is obtained.
[0071] Experimental example
[0072] 1. Sample evaluation:
[0073] a. Heat resistance test: Package the heat-resistant chocolate product 1, comparison samples 1 to 3, and 100% dark chocolate in aluminum foil bags, and place them at 40°C, 60°C, 80°C, 100°C, and 120°C for 12 hours, respectively, and observe the changes in the samples.
[0074] b. Caloric test: Measure the energy of implementation samples 1 to 3 and control sample 3. The calculation rules shall follow the "GB 28050 National Food Safety Standard General Rules for Nutrition Labeling of Prepackaged Foods".
[0075] 2. Results and analysis:
[0076] Table 1 Heat resistance test results
[0077]
[0078] Table 2 Energy test results
[0079] Sample name Energy / kJ / 100g Heat-resistant chocolate products1 1551 Heat-resistant chocolate products2 1570 Heat-resistant chocolate products3 1529 Control sample 3 2200
[0080] 3. Results Analysis
[0081] The heat resistance test results in Table 1 show that heat resistance: heat-resistant chocolate product 1 ≈ heat-resistant chocolate product 2 ≈ heat-resistant chocolate product 3 >> comparison sample 1 ≈ comparison sample 2 > comparison sample 3 ≈ ordinary chocolate. The heat resistance of comparison samples 1 and 2 is slightly better than that of ordinary chocolate and comparison sample 3, indicating that the heat resistance of chocolate can be improved by adding hydrogel or inulin alone through the same process; the heat resistance of comparison sample 3 is basically equivalent to that of ordinary chocolate, indicating that freeze-drying alone cannot effectively improve the heat resistance of chocolate. The heat resistance of implementation samples 1 to 3 is much stronger than that of comparison samples 1 and 2, indicating that the hydrogel and water-soluble components have obvious synergistic effects. Its effect may be that the hydrogel forms a macroscopic structure after dehydration to form a cavity, and the water-soluble substance precipitates on the cavity wall in a stacking manner to form a microscopic structure, and is compounded with the hydrogel structure to improve the structure strength, thereby showing an unexpected synergistic effect of enhancing heat resistance.
[0082] The energy test in Table 2 shows that the energy of the chocolate with a composite structure of hydrogel and water-soluble ingredients is reduced by 29.5%, 28.6% and 30.5% respectively compared with ordinary dark chocolate, which is in line with the claim of energy reduction.
[0083] In summary, the chocolate product provided by the present invention has good heat resistance and lower energy than ordinary dark chocolate of the same quality.
[0084] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.
Claims
1. A heat-resistant chocolate product having a freeze-dried composite skeleton, characterized in that: Made from the following raw materials in parts by weight: Hydrogel 1 to 60 parts Water-soluble components 20 to 30 parts 50 to 80 servings of chocolate Emulsifier 0.01 to 1 part The hydrogel and the water-soluble component together constitute a freeze-dried composite skeleton, and the chocolate is dispersed in the cavity of the freeze-dried composite skeleton; The water-soluble component includes inulin; The heat-resistant chocolate product does not melt when placed at 120° C. for 12 hours.
2. The heat-resistant chocolate product according to claim 1, characterized in that: The hydrogel is a hydrogel formed by physically crosslinking polysaccharide gum and cellulose or its derivatives as raw materials; preferably, the hydrogel is a hydrogel obtained by drying an aqueous solution of sodium carboxymethyl cellulose and pectin at 100° C. to 120° C. for 8 h to 12 h.
3. The heat-resistant chocolate product according to claim 1 or 2, characterized in that: The hydrogel is a gel dry particle with a particle size of more than 10 meshes.
4. The heat-resistant chocolate product according to claim 1, characterized in that: The water-soluble components also include one or more of water-soluble dietary fiber, fruit and vegetable powder, milk powder, medicinal and edible plant extracts, small molecule peptides, water-soluble vitamins, prebiotics and sodium hyaluronate.
5. The heat-resistant chocolate product according to claim 1, characterized in that: The chocolate is selected from one or more of cocoa butter, cocoa mass and cocoa liquor.
6. A method for preparing a heat-resistant chocolate product having a freeze-dried composite skeleton according to any one of claims 1 to 5, comprising the following steps: S1, dissolving the water-soluble component and the hydrogel in water, and standing for more than 15 minutes to obtain an aqueous phase; S2, adding the melted chocolate and the emulsifier into the water phase, stirring until no obvious particles are left, to obtain an oil-in-water chocolate emulsion; S3, freeze-drying the oil-in-water chocolate emulsion composite liquid to obtain the heat-resistant chocolate product.
7. The preparation method according to claim 6, characterized in that: In step S1, the mass of water is more than 10 times the mass of the hydrogel.
8. The preparation method according to claim 6, characterized in that: In step S2, the melting temperature of the chocolate is 40°C to 55°C.
9. The preparation method according to claim 6, characterized in that: In step S2, the freeze drying is divided into three stages: pre-freezing, sublimation drying, and desorption drying: Pre-freezing conditions are: temperature -40℃~-25℃, time 1~12h; Sublimation drying conditions are: temperature -40℃~-25℃, time 8~72h, pressure 50~6000Pa; The desorption drying conditions are: temperature 8-50°C, time 8-72h.
10. Use of the heat-resistant chocolate product according to any one of claims 1 to 5 or the heat-resistant chocolate product prepared by the method according to any one of claims 6 to 9 in preparing food.