Tipping paper adhesion testing method and cigarette production method and system
By combining different additives and varnish on the loading paper and testing the adhesion of cigarette packs or cigarette strips under simulated production conditions, the problem of inaccurate detection of the adhesion of the loading paper in the prior art is solved, and cigarette production is realized The optimization of temperature and time during the process improves product quality.
Patent Information
- Application Number
- CN202411012519.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-26
- Publication Date
- 2024-11-08
AI Technical Summary
The existing bonding and loading paper adhesion testing methods cannot accurately detect the adhesion between cigarette branches and cigarette boxes in packaging molded cigarettes, and cannot fully reflect the actual production situation, affecting the quality of cigarette products.
By printing different additives and varnish on the loading paper, the temperature conditions during normal production and fault repair are simulated, packaged into cigarette bags or cigarette strips, and heated in a beauty container to observe the adhesion between the cigarette stick and the tin foil. , adjust the temperature and time conditions, and intuitively judge the anti-adhesion.
The adhesion of the loading paper is achieved directly, accurately and comprehensively tested, and the temperature and time setting of the heating links in the production process is guided, so as to reduce the adhesion phenomenon in finished cigarettes and improve production quality.
Smart Images

Figure CN118902168A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of tipping paper detection, and in particular to a tipping paper adhesion testing method and a cigarette production method and system. Background Art
[0002] Tipping paper is an important component of cigarettes, and plays the role of connecting the filter rod with the cigarette. In recent years, with consumers' pursuit of differentiation and personalization of cigarette products, various cigarette companies have begun to give tipping paper more functions, such as more gorgeous appearance, more flavors, etc. Therefore, manufacturers need to use new production processes, printing methods, printing materials, additives, etc. to produce new categories of cigarettes. This will also bring about a variety of quality problems such as adhesion, which will seriously affect product quality and consumer experience. Therefore, it is very necessary to test the anti-adhesion properties of tipping paper, but there is currently no standard for anti-adhesion testing in the industry.
[0003] A Chinese patent with the patent number CN113984654A discloses a method for testing the anti-adhesion performance of cigarette tipping paper, comprising the following steps: preparing tipping paper to be tested, wherein the tipping paper to be tested comprises a front side provided with a printing layer, and a back side opposite to the front side; sample preparation: cutting the tipping paper to be tested into strip samples, and placing them in a constant temperature and humidity environment for balance; then stacking N strip samples to obtain a sample; N is a natural number greater than or equal to 2; testing: clamping the two ends of the sample in the length direction respectively, stretching the sample at a constant stretching speed, and recording the tensile strength of the sample when it is stretched to break, the greater the tensile strength, the worse the anti-adhesion performance. The detection method of this application is easy to operate, but the result is inaccurate. The reason for the adhesion of the tipping paper is that the packaged cigarettes are sealed by the carton and the packaging film. During the heating and plastic sealing, a certain amount of water vapor will be generated in the carton and the packaging film due to the volatilization of tobacco, tobacco materials, etc., and the packaging film will hinder the volatilization of water vapor, causing the additives and printing varnish on the surface of the tipping paper to melt to a certain extent, resulting in adhesion. The detection method in this patent cannot truly reflect the actual situation, and the packaged cigarettes may not only stick to each other, but also stick to the tin foil inside the cigarette box. This patent cannot be detected.
[0004] In the actual production process, a certain link in the production process fails. During its maintenance, the equipment in the heating link continues to work, resulting in an increase in the heating time of the cigarette, thereby increasing the possibility of melting the additives and printing varnish on the surface of the tipping paper, that is, increasing the possibility of adhesion of the tipping paper. However, the existing tipping paper adhesion test does not take this possibility into consideration, and it is impossible to comprehensively and accurately detect the adhesion of the tipping paper, which is not conducive to subsequent research and development and production. Summary of the invention
[0005] To solve at least one aspect of the above problems, the present invention provides a method for testing the adhesion of tipping paper and a method and system for producing cigarettes. The equipment and temperature conditions during normal production, as well as the maintenance time conditions when a failure occurs, are used as the testing equipment and conditions for the adhesion of tipping paper. This helps to directly, accurately and comprehensively test the adhesion of tipping paper corresponding to different combinations of additives, varnishes and tipping papers, thereby helping to guide the production of subsequent cigarettes.
[0006] The present application is implemented by the following technical solution: A method for testing the adhesion of tipping paper, comprising the following steps:
[0007] Step 1: Divide several kinds of additives and several kinds of varnishes into several groups according to product requirements;
[0008] Step 2: printing the additives and varnishes in the groups onto multiple groups of tipping papers to be tested respectively, each group of tipping papers to be tested comprising a plurality of sheets of tipping papers to be tested;
[0009] Step 3: Rolling multiple groups of tipping papers to be tested into corresponding groups of cigarettes respectively, packing the cigarettes in the same group into corresponding multiple cigarette packs through a packaging machine, and wrapping each cigarette pack with a packaging film;
[0010] Step 4: randomly select at least one pack from each group of cigarette packs to be tested to form a cigarette pack group to be tested;
[0011] Step 5: Place the cigarette packs to be tested in the beauty device, heat them at the set temperature, and take them out after the set time to cool them naturally to room temperature;
[0012] Step 6: Open the outer packaging of each cigarette pack in the tested cigarette pack group and observe the adhesion between adjacent cigarettes and between cigarettes and tin foil;
[0013] Step 7: If there are adjacent cigarettes or cigarettes and tin foil stuck together in a cigarette pack, it is determined that the group of additives and varnish corresponding to the cigarette pack act on the tipping paper to be tested, and the anti-adhesion property under the set temperature and set time conditions is unqualified;
[0014] Step 8: If the adjacent cigarettes and the cigarettes and the tin foil in a cigarette pack are not stuck together, it is determined that the group of additives and varnish corresponding to the cigarette pack acts on the tipping paper to be tested, and the anti-sticking property under the set temperature and set time conditions is qualified;
[0015] Step 9: Adjust the set temperature and / or set time in step 5 as a new set temperature or set time, and return to step 4.
[0016] Preferably, the set duration ranges from 1 to 10 minutes.
[0017] More preferably, the set time lengths are 1 min, 3 min, 5 min and 10 min respectively.
[0018] Preferably, step 3 also includes packaging some cigarette packs in the same group into multiple cigarette rods through a packaging machine, and wrapping each cigarette rod with a packaging film; step 4 also includes randomly selecting at least one cigarette rod from each group of cigarette rods to be tested to form a cigarette rod group to be tested; and step 5 includes placing the cigarette pack group to be tested and the cigarette rod group to be tested in a beauty container.
[0019] Preferably, the set temperature ranges from 110 to 130°C.
[0020] Preferably, in step 4, the number of cigarette packs extracted from each group of cigarette packs to be tested is 3 to 5 packs.
[0021] The present application also provides a method for producing a cigarette, comprising the following steps:
[0022] Step 1: Determine the working temperature of the heating link in the production process according to the production requirements of the current brand of cigarettes;
[0023] Step 2: according to the test result of any one of the above-mentioned methods for testing the adhesion of the tipping paper, the type of additives, the type of varnish, the type of tipping paper of the current brand of cigarettes, and the working temperature determined in step 1, determine the maximum set time for the current brand of cigarettes to be non-adhesive at the working temperature;
[0024] Step 3: monitor the length of time the cigarette pack stays in the beauty device; when the length of time is greater than or equal to the set length of time in step 2, remove the cigarette pack; when the length of time is less than the set length of time in step 2, proceed to the next production process;
[0025] Step 4: Monitor the length of time the tobacco rod stays in the beauty device; when the length of time is greater than or equal to the set length of time in step 2, remove the tobacco rod; when the length of time is less than the set length of time in step 2, proceed to the next production process.
[0026] Preferably, when determining the maximum set time when the current production brand of cigarettes are not adhered in step 2, the set time of the cigarette pack in the beauty container and the set time of the cigarette rod in the beauty container are determined respectively; in step 3, the stay time of the current production cigarette pack in the beauty container is compared with the set time of the cigarette pack in the beauty container determined in step 2; in step 4, the stay time of the current production cigarette rod in the beauty container is compared with the set time of the cigarette rod in the beauty container determined in step 2.
[0027] The present application also provides a cigarette production system, which adopts any of the above-mentioned cigarette production methods, including a first monitor, a second monitor, a first comparator, a second comparator, a first rejection device, a second rejection device and a controller; the first monitor is installed in the cigarette pack beautifier to monitor the length of time the cigarette pack stays in the cigarette pack beautifier; the second monitor is installed in the cigarette rod beautifier to monitor the length of time the cigarette rod stays in the cigarette rod beautifier; the first comparator stores the maximum set time when the current production brand of cigarettes is not adhered, determined according to any of the above-mentioned testing methods for the adhesion of the tipping paper, and the first comparator is communicated with the first monitor to compare the set time with the monitoring result in the first monitor; The second comparator stores the maximum set time when the current production brand of cigarettes is not sticky, determined according to any of the above-mentioned testing methods for the adhesion of the tipping paper. The second comparator is communicatively connected to the second monitor for comparing the set time and the monitoring results in the second monitor; the first rejection device is installed in the conveying device located behind the cigarette pack beautifier for rejecting unqualified cigarette packs; the second rejection device is installed in the conveying device located behind the cigarette rod beautifier for rejecting unqualified cigarette rods; the controller is communicatively connected to the first comparator, the second comparator, the first rejection device and the second rejection device for receiving the results of the first comparator and the second comparator, and controlling the operation of the first rejection device and the second rejection device respectively according to the results.
[0028] Preferably, the set time length stored in the first comparator is the maximum set time length of the cigarette pack in the beauty container when the current production brand of cigarettes is not stuck, determined according to any of the above-mentioned testing methods for the adhesion of the tipping paper; the set time length stored in the second comparator is the maximum set time length of the cigarette rod in the beauty container when the current production brand of cigarettes is not stuck, determined according to any of the above-mentioned testing methods for the adhesion of the tipping paper.
[0029] The method for testing the adhesion of tipping paper and the method and system for producing cigarettes of the present invention have the following beneficial effects:
[0030] The present application adopts the most direct and most realistic way to measure the adhesion of the tipping paper, that is, different kinds of additives, varnishes, and tipping papers to be tested are selected and combined according to product requirements, and the corresponding cigarette packs and / or cigarette rods are packaged by a packaging machine, and packaging films are wrapped on the outside of the cigarette packs and / or cigarette rods. The cigarette packs and / or cigarette rods to be tested are placed in a beauty container, and the temperature during normal production is used as the test temperature, and the maintenance time when the fault occurs is used as the test time. This helps to directly, accurately, and comprehensively test the adhesion of the tipping paper corresponding to different combinations of additives, varnishes, and tipping papers; the test results of the present application can guide actual production, that is, after determining the working temperature of the heating link in production according to production requirements, the maximum set time when there is no adhesion at the working temperature is determined according to the test results. When the residence time of the cigarette pack in the beauty container exceeds the set time, the cigarette pack is discarded, which helps to reduce the possibility of cigarette sticks in the finished cigarettes, thereby improving the production quality of cigarettes. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] In order to better understand the above and other purposes, features, advantages and functions of the present invention, reference may be made to the embodiments shown in the accompanying drawings. The same reference numerals in the accompanying drawings refer to the same components. It should be understood by those skilled in the art that the accompanying drawings are intended to schematically illustrate the preferred embodiments of the present invention and have no limiting effect on the scope of the present invention, and the components in the drawings are not drawn to scale.
[0032] Figure 1 A flow chart showing a method for testing the adhesion of tipping paper according to an embodiment of the present invention is shown;
[0033] FIG2 shows a flow chart of a cigarette production method according to an embodiment of the present invention;
[0034] FIG3 shows a structural block diagram of a cigarette production system according to an embodiment of the present invention. DETAILED DESCRIPTION
[0035] The following is a description of exemplary embodiments of the present disclosure in conjunction with the accompanying drawings, including various details of the embodiments of the present disclosure to facilitate understanding, which should be considered as merely exemplary. Therefore, it should be recognized by those of ordinary skill in the art that various changes and modifications may be made to the embodiments described herein without departing from the scope and spirit of the present disclosure. Similarly, for the sake of clarity and conciseness, descriptions of well-known functions and structures are omitted in the following description.
[0036] As used herein, the term "including" and its variations mean open inclusion, i.e., "including but not limited to". Unless otherwise stated, the term "or" means "and / or". The term "based on" means "based at least in part on". The terms "an example embodiment" and "an embodiment" mean "at least one example embodiment". The term "another embodiment" means "at least one additional embodiment". The terms "first", "second", etc. may refer to different or the same objects. Other explicit and implicit definitions may also be included below.
[0037] In order to at least partially solve one or more of the above problems and other potential problems, the embodiments of the present disclosure provide a method for testing the adhesion of tipping paper, such as Figure 1 As shown, the following steps are included:
[0038] Step 1: Divide several kinds of additives and several kinds of varnishes into several groups according to product requirements;
[0039] Step 2: printing the additives and varnishes in the groups onto multiple groups of tipping papers to be tested respectively, each group of tipping papers to be tested comprising a plurality of sheets of tipping papers to be tested;
[0040] Step 3: rolling the multiple groups of tipping papers to be tested into corresponding multiple groups of cigarettes respectively, packaging the cigarettes in the same group into corresponding multiple cigarette packs through a packaging machine, and wrapping each cigarette pack with a packaging film; in some embodiments, this step also includes packaging some of the cigarette packs in the same group into multiple cigarette rods through a packaging machine, and wrapping each cigarette rod with a packaging film;
[0041] Step 4: randomly extract at least one pack from each group of cigarette packs to be tested to form a cigarette pack group to be tested. Preferably, the number of cigarette packs extracted from each group of cigarette packs to be tested is 3 to 5 packs. In some embodiments, this step further includes randomly extracting at least one cigarette rod from each group of cigarette rods to be tested to form a cigarette rod group to be tested.
[0042] Step 5: placing the cigarette pack group to be tested in the beauty device. In some embodiments, in this step, the cigarette pack group to be tested and the cigarette rod group to be tested are both placed in the beauty device, heated at a set temperature, and after staying for a set time, the cigarette packs are taken out and naturally cooled to room temperature; preferably, the set temperature ranges from 110 to 130°C, and the set time ranges from 1 to 10 minutes. More preferably, the set temperatures are 110°C, 120°C and 130°C, respectively, and the set time is 1 minute, 3 minutes, 5 minutes and 10 minutes, respectively;
[0043] Step 6: Open the outer packaging of each cigarette pack in the tested cigarette pack group and observe the adhesion between adjacent cigarettes and between cigarettes and tin foil;
[0044] Step 7: If there are adjacent cigarettes or cigarettes and tin foil stuck together in a cigarette pack, it is determined that the group of additives and varnish corresponding to the cigarette pack acts on the tipping paper to be tested, and the anti-adhesion performance under the set temperature and set time conditions is unqualified; preferably, when it is determined to be unqualified, the test of the group of cigarette packs at the set temperature is terminated, and the test is continued after updating other set temperatures;
[0045] Step 8: If the adjacent cigarettes and the cigarettes and the tin foil in a cigarette pack are not stuck together, it is determined that the group of additives and varnish corresponding to the cigarette pack acts on the tipping paper to be tested, and the anti-sticking property under the set temperature and set time conditions is qualified;
[0046] Step 9: Adjust the set temperature and / or set time in step 5 as the new set temperature or set time, and return to step 4; preferably, the test is performed in the order of gradually increasing the set temperature and gradually increasing the set time at the same temperature.
[0047] In a specific embodiment, as shown in Table 1, step 1: divide two groups of combinations to be tested according to product requirements, namely, sweetener and water-soluble varnish, sweetener and alcohol-soluble varnish;
[0048] Step 2: Print two combinations of sweetener and water-soluble varnish, and sweetener and alcohol-soluble varnish on two groups of tipping papers to be tested, respectively, each group of tipping papers to be tested includes a plurality of tipping papers to be tested;
[0049] Step 3: Roll the two groups of tipping papers to be tested into two corresponding groups of cigarettes respectively, pack the cigarettes in the same group into corresponding multiple cigarette packs through a packaging machine, and wrap each cigarette pack with a packaging film; pack some cigarette packs in the same group into multiple cigarette rods through a packaging machine, and wrap each cigarette rod with a packaging film;
[0050] Step 4: randomly select 3 packs from the two groups of cigarette packs to be tested to form a cigarette pack group to be tested, and randomly select 3 cigarette rods from the two groups of cigarette rods to be tested to form a cigarette rod group to be tested;
[0051] Step 5: Place the cigarette pack group and the cigarette rod group to be tested in a beauty device, and heat them at the set temperature and time in Table 1. After heating, take out the cigarette packs and cool them naturally to room temperature.
[0052] Step 6: Open the outer packaging of each cigarette pack in the tested cigarette pack group, observe the adhesion between adjacent cigarettes and the adhesion between cigarettes and tin foil, and obtain the test results as shown in Table 1;
[0053] Step 7: If there are adjacent cigarettes or cigarettes and tin foil stuck together in a cigarette pack, it is determined that the group of additives and varnish corresponding to the cigarette pack acts on the tipping paper to be tested, and the anti-adhesion performance under the set temperature and set time conditions is unqualified; preferably, when it is determined to be unqualified, the test of the group of cigarette packs at the set temperature is terminated, and the test is continued after updating other set temperatures;
[0054] Step 8: If the adjacent cigarettes and the cigarettes and the tin foil in a cigarette pack are not stuck together, it is determined that the group of additives and varnish corresponding to the cigarette pack acts on the tipping paper to be tested, and the anti-sticking property under the set temperature and set time conditions is qualified;
[0055] Step 9: Adjust the set temperature and / or set time in step 5 as a new set temperature or set time, and return to step 4.
[0056]
[0057] The present application also provides a method for producing cigarettes, as shown in FIG2 , comprising the following steps:
[0058] Step 1: Determine the working temperature of the heating link in the production process according to the production requirements of the current brand of cigarettes;
[0059] Step 2: according to the test result of any one of the above-mentioned methods for testing the adhesion of the tipping paper, the type of additives, the type of varnish, the type of tipping paper of the current brand of cigarettes, and the working temperature determined in step 1, determine the maximum set time when the current brand of cigarettes is not adhered at the working temperature; preferably, determine the set time of the cigarette pack in the beauty container and the set time of the cigarette rod in the beauty container respectively;
[0060] Step 3: monitor the length of time the cigarette pack stays in the beauty device; when the length of time is greater than or equal to the set length of time the cigarette pack stays in the beauty device determined in step 2, remove the cigarette pack; when the length of time the cigarette pack stays in the beauty device determined in step 2 is less than the set length of time the cigarette pack stays in the beauty device determined in step 2, proceed to the next production process;
[0061] Step 4: Monitor the length of time the cigarette stick stays in the beauty device; when the length of time is greater than or equal to the set length of time the cigarette stick stays in the beauty device determined in step 2, remove the cigarette stick; when the length of time the cigarette stick stays in the beauty device determined in step 2, proceed to the next production process.
[0062] In a specific embodiment, the additive in the currently produced cigarettes is a sweetener, and the varnish is a water-soluble varnish. Step 1: according to the production requirements of the currently produced brand of cigarettes, the working temperature of the heating link in the production process is determined to be 120° C.;
[0063] Step 2: According to the test results in Table 1, the maximum setting time when the cigarette packs of the current production cigarettes are not adhered at 120°C is 3 minutes, and the maximum setting time when the cigarette rods of the current production cigarettes are not adhered at 120°C is 1 minute;
[0064] Step 3: Monitor the length of time the cigarette pack stays in the beauty device; if the length of time is greater than or equal to 3 minutes, remove the cigarette pack; if the length of time is less than 3 minutes, continue to the next production process;
[0065] Step 4: Monitor the length of time the tobacco rod stays in the beauty device; when the length of time is greater than or equal to 1 minute, remove the tobacco rod; when the length of time is less than 1 minute, proceed to the next production process.
[0066] The present application also provides a cigarette production system, as shown in FIG3, using any of the above-mentioned cigarette production methods, including a first monitor, a second monitor, a first comparator, a second comparator, a first rejecting device, a second rejecting device and a controller;
[0067] The first monitor is installed in the cigarette pack beautifier, and is used to monitor the length of time the cigarette pack stays in the cigarette pack beautifier;
[0068] The second monitor is installed in the cigarette rod beauty device and is used to monitor the length of time the cigarette rod stays in the cigarette rod beauty device;
[0069] The first comparator stores the maximum set time when the cigarette of the current production brand is not adhered, determined according to any one of the above-mentioned methods for testing the adhesion of the tipping paper. Preferably, the set time stored in the first comparator is the maximum set time when the cigarette pack of the current production brand is not adhered, determined according to any one of the above-mentioned methods for testing the adhesion of the tipping paper. The first comparator is connected in communication with the first monitor for comparing the set time with the monitoring result of the first monitor;
[0070] The second comparator stores the maximum set time when the current brand of cigarettes is not sticking, determined according to any one of the above-mentioned methods for testing the stickiness of the tipping paper. Preferably, the set time stored in the second comparator is the maximum set time when the current brand of cigarettes is not sticking, determined according to any one of the above-mentioned methods for testing the stickiness of the tipping paper. The second comparator is in communication with the second monitor and is used to compare the set time with the monitoring result in the second monitor.
[0071] The first rejecting device is installed in the conveying device located behind the cigarette pack beauty device, and is used to reject unqualified cigarette packs;
[0072] The second rejecting device is installed in the conveying device located behind the tobacco rod beauty device, and is used to reject unqualified tobacco rods;
[0073] The controller is in communication connection with the first comparator, the second comparator, the first rejecting device and the second rejecting device, and is used for receiving the results of the first comparator and the second comparator, and controlling the operation of the first rejecting device and the second rejecting device respectively according to the results.
[0074] The embodiments of the present disclosure have been described above, and the above description is exemplary, not exhaustive, and is not limited to the disclosed embodiments. Many modifications and changes will be apparent to those of ordinary skill in the art without departing from the scope and spirit of the described embodiments. The selection of terms used herein is intended to best explain the principles of the embodiments, practical applications, or technical improvements in the market, or to enable other persons of ordinary skill in the art to understand the present invention.
Claims
1. A method for testing the adhesion of tipping paper, characterized in that: The following steps are involved: Step 1: Divide several kinds of additives and several kinds of varnishes into several groups according to product requirements; Step 2: printing the additives and varnishes in the groups onto multiple groups of tipping papers to be tested respectively, each group of tipping papers to be tested comprising a plurality of sheets of tipping papers to be tested; Step 3: Rolling multiple groups of tipping papers to be tested into corresponding groups of cigarettes respectively, packing the cigarettes in the same group into corresponding multiple cigarette packs through a packaging machine, and wrapping each cigarette pack with a packaging film; Step 4: randomly select at least one pack from each group of cigarette packs to be tested to form a cigarette pack group to be tested; Step 5: Place the cigarette packs to be tested in the beauty device, heat them at the set temperature, and take them out after the set time to cool them naturally to room temperature; Step 6: Open the outer packaging of each cigarette pack in the tested cigarette pack group and observe the adhesion between adjacent cigarettes and between cigarettes and tin foil; Step 7: If there are adjacent cigarettes or cigarettes and tin foil stuck together in a cigarette pack, it is determined that the group of additives and varnish corresponding to the cigarette pack act on the tipping paper to be tested, and the anti-adhesion property under the set temperature and set time conditions is unqualified; Step 8: If the adjacent cigarettes and the cigarettes and the tin foil in a cigarette pack are not stuck together, it is determined that the group of additives and varnish corresponding to the cigarette pack acts on the tipping paper to be tested, and the anti-sticking property under the set temperature and set time conditions is qualified; Step 9: Adjust the set temperature and / or set time in step 5 as a new set temperature or set time, and return to step 4.
2. A method for testing the adhesion of tipping paper according to claim 1, characterized in that: The setting time ranges from 1 to 10 minutes.
3. A method for testing the adhesion of tipping paper according to claim 2, characterized in that: The set time lengths are 1 minute, 3 minutes, 5 minutes and 10 minutes respectively.
4. A method for testing the adhesion of tipping paper according to claim 1, characterized in that: The step 3 also includes packaging some cigarette packs in the same group into multiple cigarette rods through a packaging machine, and wrapping each cigarette rod with a packaging film; the step 4 also includes randomly selecting at least one cigarette rod from each group of cigarette rods to be tested to form a cigarette rod group to be tested; and the step 5 includes placing the cigarette pack group to be tested and the cigarette rod group to be tested in a beauty container.
5. A method for testing the adhesion of tipping paper according to claim 1, characterized in that: The set temperature ranges from 110 to 130°C.
6. A method for testing the adhesion of tipping paper according to claim 1, characterized in that: In step 4, the number of cigarette packs extracted from each group of cigarette packs to be tested is 3 to 5 packs.
7. A method for producing cigarettes, characterized in that: The following steps are involved: Step 1: Determine the working temperature of the heating link in the production process according to the production requirements of the current brand of cigarettes; Step 2: according to the test result of the method for testing the adhesion of tipping paper according to any one of claims 1 to 6, the type of additives, the type of varnish, the type of tipping paper of the current brand of cigarettes, and the working temperature determined in step 1, determine the maximum set time when the current brand of cigarettes is not adhered at the working temperature; Step 3: monitor the length of time the cigarette pack stays in the beauty device; when the length of time is greater than or equal to the set length of time in step 2, remove the cigarette pack; when the length of time is less than the set length of time in step 2, proceed to the next production process; Step 4: Monitor the length of time the tobacco rod stays in the beauty device; when the length of time is greater than or equal to the set length of time in step 2, remove the tobacco rod; when the length of time is less than the set length of time in step 2, proceed to the next production process.
8. The method for producing cigarettes according to claim 7, characterized in that: When determining the maximum set time when the current brand of cigarettes are not adhered in step 2, the set time of the cigarette pack in the beauty device and the set time of the cigarette rod in the beauty device are determined respectively; in step 3, the stay time of the current brand of cigarettes in the beauty device is compared with the set time of the cigarette pack in the beauty device determined in step 2; in step 4, the stay time of the current brand of cigarettes in the beauty device is compared with the set time of the cigarette rod in the beauty device determined in step 2.
9. A cigarette production system, using the cigarette production method according to any one of claims 7 or 8, characterized in that: It includes a first monitor, a second monitor, a first comparator, a second comparator, a first rejecting device, a second rejecting device and a controller; The first monitor is installed in the cigarette pack beautifier, and is used to monitor the length of time the cigarette pack stays in the cigarette pack beautifier; The second monitor is installed in the cigarette rod beauty device and is used to monitor the length of time the cigarette rod stays in the cigarette rod beauty device; The first comparator stores the maximum set time when the cigarette of the current production brand is not sticky, determined according to the method for testing the stickiness of the tipping paper according to any one of claims 1 to 6. The first comparator is connected in communication with the first monitor and is used to compare the set time with the monitoring result of the first monitor; The second comparator stores the maximum set time when the cigarettes of the current production brand are not stuck, determined by the method for testing the stickiness of the tipping paper according to any one of claims 1 to 6. The second comparator is connected in communication with the second monitor and is used to compare the set time with the monitoring result in the second monitor; The first rejecting device is installed in the conveying device located behind the cigarette pack beauty device, and is used to reject unqualified cigarette packs; The second rejecting device is installed in the conveying device located behind the tobacco rod beauty device, and is used to reject unqualified tobacco rods; The controller is in communication connection with the first comparator, the second comparator, the first rejecting device and the second rejecting device, and is used for receiving the results of the first comparator and the second comparator, and controlling the operation of the first rejecting device and the second rejecting device respectively according to the results.
10. A cigarette production system according to claim 9, characterized in that: The set time length stored in the first comparator is the maximum set time length of the cigarette pack in the beauty container when the current production brand of cigarettes is not stuck according to the test method for the adhesion of the tipping paper according to any one of claims 1 to 6; the set time length stored in the second comparator is the maximum set time length of the cigarette rod in the beauty container when the current production brand of cigarettes is not stuck according to the test method for the adhesion of the tipping paper according to any one of claims 1 to 6.
Citation Information
Patent Citations
Method for testing anti-adhesion performance of tipping paper for flavored cigarettes
CN113607639A
Method for detecting thermal adhesion performance of water-based ink
CN113899693A
Control method and device for cigarette packet small box beautifying device of carton packaging machine
CN114987857A
Disqualified cigarette packet detection device for cigarette packet beautifying device of packaging machine
CN219172882U