Reinforced coating structure and process method
By using a specific rust-preventive primer and a reinforcing coating process on classic car bodies, the problems of uneven coating and cracking were solved, achieving high-quality coating repair while reducing labor intensity and costs.
Patent Information
- Application Number
- CN202410948415.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-16
- Publication Date
- 2024-11-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Classic car body coatings are prone to mottled, cracked, and peeling during the restoration process. Existing technologies that increase the thickness of the paint coating result in uneven coating structure, making it prone to cracking, and are also labor-intensive and costly.
The anti-rust primer consists of components A and B. After applying putty, the coating is strengthened. Through manual spraying and condition adjustment, the coating and putty layer are fully reacted. Finally, the color paint is sprayed and finished to improve the coating quality and uniformity.
It improves the quality of classic car exterior coating repair, reduces rework, and lowers labor intensity and costs.
Smart Images

Figure CN118904685A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of classic car repair coating, and specifically relates to a reinforced coating structure and a process method. Background Art
[0002] Classic cars were hand-built from the 1950s to the 1980s by craftsmen who inherited the spirit of the carmaker, spending ten times the energy and effort that went into making ordinary cars. As time went by, the surface coating on classic cars became mottled, cracked, and peeled off. Therefore, repairing the exterior coating on classic cars has unique significance.
[0003] In the classic car restoration industry, the coating repair process is: polishing the body part or the whole car → cleaning the body base → spraying anti-rust primer → polishing → cleaning → applying putty → drying → polishing → cleaning → spraying color paint → low-temperature drying → modification. Because the surface of the putty is loose after drying, it has the advantages of easy polishing and good plasticity, but the loose state will cause the color paint to penetrate into the putty layer, and the coating will have "whitening" and loss of gloss and other paint film defects. The existing technical means to solve this technical problem is to increase the thickness of the color paint coating, but it will cause uneven thickness of the overall coating structure, resulting in poor mechanical properties of the coating, easy cracking of the coating, and time-consuming and labor-intensive rework. Summary of the invention
[0004] In view of the above problems, the present invention provides a reinforced coating structure and process method, which specifically comprises spraying an antirust primer coating on the body of a classic car, applying putty after drying, drying, grinding, cleaning and applying a reinforced coating, adjusting the state so that the coating and the putty layer fully react, applying a color paint, drying, modifying and delivering the car, wherein the antirust primer material is composed of component A and component B, wherein component A is composed of 45-65% of pigment filler, 2.5-5% of curing agent, 0.1-0.3% of dispersant, 0.1-0. It is composed of 3% defoamer, 1-2% leveling agent and 3.5-6% co-solvent. Component B is composed of 20-40% modified epoxy resin, 1.5-5% additives and solvents. It is manually sprayed, with a construction solid content of 25%-35%, a construction viscosity of 25 seconds-30 seconds, a temperature of 22℃-25℃, a spray gun caliber of 1.5mm-2.5mm, and a film thickness of 15μm-25μm after drying of the anti-rust primer. It improves the quality of exterior coating repair of classic cars, reduces rework, saves costs, and reduces labor intensity.
[0005] The technical solution of the present invention is as follows: a reinforced coating structure and a process method, comprising the following steps:
[0006] S1 sprays a rust-proof primer coating on the body of the classic car;
[0007] After S2 is dried, apply putty;
[0008] S3 is dried, polished, cleaned and then coated with reinforcing paint;
[0009] S4 state adjustment to make the paint and the putty layer fully react;
[0010] S5: Apply color paint, dry, retouch and deliver the vehicle.
[0011] Furthermore, in step S1, the anti-rust primer material consists of component A and component B, wherein component A consists of 45-65% pigments and fillers, 2.5-5% curing agent, 0.1-0.3% dispersant, 0.1-0.3% defoaming agent, 1-2% leveling agent and 3.5-6% cosolvent, and component B consists of 20-40% modified epoxy resin, 1.5-5% additives and solvents.
[0012] Furthermore, step S1 is manual spraying, with a construction solid content of 25%-35%, a construction viscosity of 25 seconds-30 seconds, a temperature of 22°C-25°C, a spray gun caliber of 1.5mm-2.5mm, and a film thickness of 15μm-25μm after drying of the anti-rust primer.
[0013] Furthermore, in step S2, the putty material includes 25-35% resin, 55-65% talcum powder, 2-5% titanium dioxide, 6-10% bentonite, 9-13% additives, and 3.5-5% styrene.
[0014] Furthermore, step S2 is manual spraying or scraping, the material is mixed with a curing agent ratio of 3.5% by weight, the spraying should be 25-30 cm away from the surface, the repeated spraying interval is 2-5 minutes, the spray gun caliber is 2.5 mm, and the spraying pressure is 2-2.5 bar.
[0015] Further, in step S3, manual spraying is specifically constructed with a solid content of 35%-45%, a construction viscosity of 25 seconds-30 seconds, a temperature of 22°C-25°C, a spray gun caliber of 1.5mm-2.5mm, a wet paint film thickness of 25μm-35μm, and the control method is a wet paint film thickness gauge.
[0016] Further, in step S3, the amount of coating added is enhanced according to the formula:
[0017]
[0018] Calculation, where h is the height of the absorbed liquid, σ is the surface tension, ρ is the liquid density, r is the pore radius, and θ is the angle between the liquid surface and the pore wall. If the calculated liquid absorption height is greater than the average height of the atomic putty pore, the atomic putty layer has fully absorbed the strengthening coating, otherwise it is necessary to adjust the material or process parameters.
[0019] Furthermore, the drying temperature is 20°C-80°C for 15 minutes to 5 hours.
[0020] The beneficial effects of the present invention are:
[0021] Improve the quality of classic car exterior coating repairs, reduce rework, save costs, and reduce labor intensity. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 This is a schematic diagram of the reinforced coating structure of the present invention.
[0023] Figure 2 The figure is a flow chart of the method of the present invention. DETAILED DESCRIPTION
[0024] It should be noted that in the description of the present invention, the terms "center", "up", "down", "left", "right", "vertical", "horizontal", "inside", "outside", "clockwise", "counterclockwise", etc. indicate directions or positional relationships based on the directions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction.
[0025] In the present invention, unless otherwise clearly specified and limited, the terms "set", "install", "connect", "connect" and the like should be understood in a broad sense. For example, "fixed" can be a fixed connection, a detachable connection, or an integral connection; the connection can be a mechanical connection or an electrical connection; the connection can be a direct connection or an indirect connection through an intermediate medium, and can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0026] The main process is: classic car body paint removal → body wipe clean → body spray anti-rust primer → drying → application of putty → drying → polishing → application of strengthening paint → state adjustment → application of color paint → drying → modification.
[0027] A reinforced coating structure and process method, specifically:
[0028] The S1 classic car body is sprayed with an anti-rust primer coating, and the anti-rust primer material is composed of component A and component B, wherein component A is composed of 45-65% pigment filler, 2.5-5% curing agent, 0.1-0.3% dispersant, 0.1-0.3% defoamer, 1-2% leveling agent and 3.5-6% cosolvent, and component B is composed of 20-40% modified epoxy resin, 1.5-5% additives and solvent. The above anti-rust primer materials are not limited to this, and other anti-rust primer materials can also be used to prepare related coatings.
[0029] Manual spraying, construction solid content 25%-35%, construction viscosity 25 seconds-30 seconds, temperature 22℃-25℃, spray gun caliber 1.5mm-2.5mm, film thickness of anti-rust primer after drying 15μm-25μm.
[0030] S2. Drying: Drying is carried out according to the material characteristics and the material drying temperature conditions.
[0031] S3, apply putty, the putty material includes 25-35% resin, 55-65% talcum powder, 2-5% titanium dioxide, 6-10% bentonite, 9-13% additives, 3.5-5% styrene. The above putty materials are not limited to this, other formula putty materials can also be used to prepare related coatings.
[0032] Manual spraying or scraping, the material is mixed with 3.5% curing agent (by weight ratio 100:3.5), and the mixture is stirred evenly to prevent the polymerization rate from being too low, which makes the product particularly sensitive to humidity. The spraying should be 25-30 cm away from the surface. The spraying can be repeated several times, with an interval of 2-5 minutes between repeated spraying. The spray gun caliber is 2.5mm, and the spraying pressure is 2-2.5bar.
[0033] S4, drying, 20 ℃, drying is completed in 3-5 hours, 40 ℃, drying is completed in 1 hour, 60 ℃, drying is completed in 30 minutes, 80 ℃, drying is completed in 15 minutes.
[0034] S5. Grinding: Grinding in a dry state.
[0035] S6. Wipe clean. The surface must be clean, dry and free of oil.
[0036] S7. Apply reinforcing coating. The reinforcing coating material is mainly composed of polyester-modified water-based acrylate. For specific material ratios, please refer to patent CN103387643B "Polyester-modified water-based acrylate and automotive water-based paint composition".
[0037] Manual spraying, construction solid content 35%-45%, construction viscosity 25 seconds-30 seconds, temperature 22℃-25℃, spray gun caliber 1.5mm-2.5mm, wet paint film thickness 25μm-35μm, control method is wet paint film thickness gauge.
[0038] According to the capillary principle, since there are many small and loose pores on the surface of the putty layer, which act as capillaries, the liquid polyester modified water-based acrylate reinforcing coating is an infiltrating liquid relative to the dry putty coating. Under the action of liquid infiltration, the polyester modified water-based acrylate will be absorbed along the putty pores. The amount of reinforcing coating absorbed can be estimated by the following formula to achieve quality expectations.
[0039] Pore absorption enhancing coating formula:
[0040]
[0041] h--absorbed liquid height
[0042] σ--Surface tension
[0043] ρ--Liquid density
[0044] r--hole radius
[0045] θ--the angle between the liquid surface and the pore wall
[0046] If the calculated liquid absorption height is greater than the average height of the putty pores, it means that the putty layer has fully absorbed the reinforced coating. Otherwise, the material or process parameters need to be adjusted.
[0047] S7. Adjust the state to enhance the full reaction between the paint and the putty layer.
[0048] S8. Apply color paint.
[0049] S9. Drying: Drying is carried out according to the material characteristics and the material drying temperature conditions.
[0050] S10, modification, elimination of paint film defects
[0051] S11. Delivery of vehicle.
[0052] The above is only a specific implementation of the present invention, but the protection scope of the present invention is not limited thereto. Any modification, equivalent replacement and improvement made by any person skilled in the art within the technical scope disclosed by the present invention and within the spirit and principle of the present invention shall be covered within the protection scope of the present invention. At the same time, the contents not described in detail in this specification belong to the prior art known to those skilled in the art.
[0053] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.
Claims
1. A reinforced coating structure and process method, characterized in that: The following steps are involved: S1 sprays a rust-proof primer coating on the body of the classic car; After S2 is dried, apply putty; S3 is dried, polished, cleaned and then coated with reinforcing paint; S4 state adjustment to make the paint and the putty layer fully react; S5: Apply color paint, dry, retouch and deliver the vehicle.
2. A reinforced coating structure and process method according to claim 1, characterized in that: In step S1, the anti-rust primer material consists of component A and component B, wherein component A consists of 45-65% of pigments and fillers, 2.5-5% of curing agent, 0.1-0.3% of dispersant, 0.1-0.3% of defoaming agent, 1-2% of leveling agent and 3.5-6% of cosolvent, and component B consists of 20-40% of modified epoxy resin, 1.5-5% of additives and solvents.
3. A reinforced coating structure and process method according to claim 2, characterized in that: Step S1 is manual spraying, with a construction solid content of 25%-35%, a construction viscosity of 25 seconds-30 seconds, a temperature of 22°C-25°C, a spray gun caliber of 1.5mm-2.5mm, and a film thickness of 15μm-25μm after the anti-rust primer is dried.
4. A reinforced coating structure and process method according to claim 1, characterized in that: In step S2, the putty material includes 25-35% resin, 55-65% talcum powder, 2-5% titanium dioxide, 6-10% bentonite, 9-13% additives, and 3.5-5% styrene.
5. A reinforced coating structure and process method according to claim 4, characterized in that: Step S2 is manual spraying or scraping. The material is mixed with a curing agent ratio of 3.5% by weight. The spraying distance should be 25-30 cm from the surface. The repeated spraying interval is 2-5 minutes. The spray gun caliber is 2.5 mm and the spraying pressure is 2-2.5 bar.
6. A reinforced coating structure and process method according to claim 1, characterized in that: In step S3, the reinforcing coating is manually sprayed, with a construction solid content of 35%-45%, a construction viscosity of 25 seconds-30 seconds, a temperature of 22°C-25°C, a spray gun caliber of 1.5mm-2.5mm, a wet paint film thickness of 25μm-35μm, and a control method of a wet paint film thickness gauge.
7. A reinforced coating structure and process method according to claim 6, characterized in that: In step S3, the amount of coating added is enhanced according to the formula: Calculation, where h is the height of the absorbed liquid, σ is the surface tension, ρ is the liquid density, r is the pore radius, and θ is the angle between the liquid surface and the pore wall. If the calculated liquid absorption height is greater than the average height of the atomic putty pore, the atomic putty layer has fully absorbed the strengthening coating, otherwise it is necessary to adjust the material or process parameters.
8. A reinforced coating structure and process according to any one of claims 1 to 7, characterized in that: The drying temperature is 20℃-80℃, and the drying time is 15 minutes to 5 hours.
Citation Information
Patent Citations
Superactive alloy polyester putty and preparation method thereof
CN102391708A
Polyester-modified aqueous acrylate and automobile aqueous paint composition
CN103387643A
Construction process for woodwork oil paint
CN107138375A
Technique for quickly repairing vehicle paint
CN107774548A
Novel painting line improving technique for auto parts
CN108465628A