Blade pre-forged piece and molded line design method thereof

By dividing the blade preforged line into multiple control sections and remodeling, the problems of uneven deformation and metallurgical defects in preforged design in the prior art are solved, and better dimensional accuracy and uniform organization are achieved.

CN118905123AActive Publication Date: 2024-11-08AECC AVIATION POWER CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411243226.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-05
Publication Date
2024-11-08
Estimated Expiration
2044-09-05

AI Technical Summary

Technical Problem

In the prior art, in the design process of preforming parts, the underpressure method results in large metal flow resistance, large size deformation, and low mold life; the elliptical method causes large deformation of various parts to vary greatly, affecting grains. Uniformity, prone to metallurgical defects such as longitudinal light and dark stripes and cracks.

Method used

By designing the blade preforged line into multiple control sections, each section takes the two sides and the middle three points to calculate the offset, re-model it, and form a closed preforged line, reasonably allocate the metal volume, and ensure deformation during final forging. The degree is consistent, and the CNC machine tool is used for forging.

Benefits of technology

A more uniform tissue structure is achieved, the heat transfer between preforms and molds is slowed down, and the initial forging temperature is maintained, and better dimensional accuracy, surface quality and uniform tissue are obtained.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118905123A_ABST
    Figure CN118905123A_ABST
Patent Text Reader

Abstract

The invention discloses a blade pre-forged piece and a molded line design method thereof, and belongs to the technical field of machining, an A0 cross section and an N cross section are selected from cross sections of pre-forged piece molded line design, and a group of theoretical molded lines in a plurality of cross sections from the A0 cross section to the N cross section are formed for pre-forged piece design; the front edge circle center and the rear edge circle center of the theoretical molded line are connected, tangent circles of the upper curve and the lower curve of the theoretical molded line are made at each n equal part of the X-axis distance L with the bisector as the circle center, and the centers of all the tangent circles are sequentially connected from the front edge circle center through a spline line to produce the mean camber line of the theoretical molded line; making a tangent circle of the theoretical molded line by taking an intersection point of the center line of the X-axial distance L and the mean camber line as a circle center, and making tangent circles of the theoretical molded line on two sides of the center line of the X-axial distance L; and a closed pre-forged piece molded line is obtained according to the deformation amount of blade forming. The method is used for designing the blade part pre-forged piece, the deformation degree is consistent during blade finish forging by reasonably distributing the metal volume, and a more uniform structure is obtained.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of mechanical processing, and in particular relates to a blade pre-forging and a profile design method thereof. Background Art

[0002] For blades with wide chord, thin wall and large curvature, the underpressure method or ellipse method is usually used in the pre-forging design process. The underpressure method is to use the theoretical profile of the blade to offset in the direction of thickness thickening. The offset is calculated by multiplying the size of the thickest part of the theoretical line by the required deformation degree. The ellipse method is similar to the underpressure method. The short diameter of the ellipse is calculated by multiplying the thickest part of the theoretical profile by the required deformation degree. The structure can be an ellipse or two connected ellipses with a curve transition.

[0003] The above methods have the following shortcomings: the pre-forging profile designed by the underpressure method is completely consistent with the theoretical profile, resulting in large metal flow resistance during forming, large dimensional deformation, and short die life; the deformation degree of each part of the pre-forging profile designed by the elliptical method varies greatly, affecting the uniformity of the grains. During the deformation process, the metal is first bent and then formed, resulting in large residual stress, and the blades are prone to metallurgical defects such as longitudinal light and dark stripes and cracks.

[0004] In summary, the design method of the pre-forging profile of the pre-forging in the prior art has the problem of causing large dimensional deformation and large residual stress of the pre-forging. Summary of the invention

[0005] The object of the present invention is to provide a blade pre-forging and a profile design method thereof, which are used for designing blade pre-forgings, and by reasonably distributing the metal volume, the deformation degree of the blade during final forging is made consistent, thereby obtaining a more uniform structure.

[0006] To achieve the above object, the present invention provides the following technical solutions:

[0007] A blade pre-forging profile design method comprises the following steps:

[0008] Step 1, selecting the A0 section and the N section from the sections of the pre-forging profile design, and selecting the middle section between the A0 section and the N section according to the preset distance, to form a set of theoretical profiles in several sections from the A0 section to the N section for pre-forging design;

[0009] Step 2, connect the center of the leading edge circle of the theoretical profile and the trailing edge circle, make a tangent circle of the upper and lower curves of the theoretical profile with the bisector as the center at each n equal parts of the X-axial distance L, and use a spline to sequentially connect the centers of all tangent circles starting from the center of the leading edge to produce the middle arc line of the theoretical profile;

[0010] Step 3, make a tangent circle to the theoretical profile in step 1 with the intersection of the midline of the X-axis distance L and the mid-arc line in step 2 as the center, and make tangent circles to the theoretical profile on both sides of the midline of the X-axis distance L;

[0011] Step 4: According to the deformation of the blade, the diameters of the three circles in step 3 are enlarged at the centers to obtain three new circles. Arcs are drawn to be tangent to the upper and lower halves of the three new circles, and an arc is obtained, which is recorded as arc R. 上 , arc R 下 ;

[0012] Step 5: According to the arc R 上 , arc R 下 With the new circles at both ends in step 4, a closed pre-forging profile is obtained;

[0013] Step 6, repeat steps 2 to 5 to complete the theoretical profile operation of the remaining sections selected in step 1, and obtain a set of closed pre-forging profiles.

[0014] Preferably, in step 1, the distance from section A0 to section N is S; the intermediate section is the data of each S / m position increased from A0, and the sections closest to both sides of the data are selected to form a set of m+1 theoretical profiles from section A0 to section N for pre-forging design.

[0015] Furthermore, in step 1, the range of m is 2, 3, 4, 5, 6.

[0016] Preferably, in step 2, n is selected from an integer range not less than 9.

[0017] Preferably, in step 3, the tangent circle in step 2 is removed, the theoretical profile in step 1 and the center arc line in step 2 are retained, and a tangent circle to the theoretical profile is made with the intersection of the center line and the center arc line at the X-axis distance L as the center, with a diameter of ΦT0, and tangent circles to the theoretical profile are made at positions offset to the left and right by L / 3 from the center line, with diameters of ΦT1 and ΦT2, respectively.

[0018] Preferably, in step 4, the deformation amount of the blade molding ranges from 20% to 80%.

[0019] Furthermore, when the blade is made of TC4 titanium alloy material, the deformation amount of the blade forming is 50%.

[0020] Preferably, in step 5, the new circle of the front edge is moved from the arc R 上 , arc R 下 The left part of the arc is interrupted at the point of tangency and counted as R1. The new circle at the rear edge is connected to the arc R 上 , arc R 下 The right part of the arc is interrupted at the tangent point and counted as R2. In this way, the arcs R1 and R 上 , arc R2, arc R 下 Form a closed pre-forging profile.

[0021] Preferably, in step 6, three-dimensional modeling of the subsequent pre-forgings is performed based on the obtained set of closed pre-forging profiles.

[0022] A blade preforging adopts any one of the blade preforging profile design methods described above to obtain a set of closed preforging profiles for subsequent three-dimensional modeling of the preforging; a preforging mold is processed using a CNC machine tool based on the three-dimensional modeling of the preforging, and the preforging is forged using the mold.

[0023] Compared with the prior art, the present invention has the following beneficial technical effects:

[0024] The present invention provides a method for designing the profile of a blade pre-forging, which divides the overall blade profile into several control sections, takes two sides and three points in the middle of each control section to calculate their respective offsets, and then remodels the model, thereby avoiding the problems existing in the underpressure design method and the ellipse method used in the prior art. The present invention reasonably distributes the metal volume to make the degree of deformation of the blade consistent during final forging, thereby obtaining a more uniform structure. The pre-forging designed by this method is placed in the final forging die, and only the middle area of ​​the pre-forging fits the die, while the large areas of the front and rear edges are away from the die. On the one hand, the temperature loss caused by heat transfer between the pre-forging and the die is slowed down, and a higher initial forging temperature is maintained. On the other hand, the volume distribution and curvature direction of the pre-forging are conducive to the flow of metal. This design method can obtain better dimensional accuracy, surface quality and uniform structure. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 Select a schematic diagram for the theoretical profile;

[0026] Figure 2 This is a schematic diagram of the arc in the calculation;

[0027] Figure 3 Schematic diagram for calculating closed curve;

[0028] Figure 4 This is a cross-sectional view of the pre-forging in the final forging die. DETAILED DESCRIPTION

[0029] In the following, only some exemplary embodiments are briefly described. As those skilled in the art will appreciate, the described embodiments may be modified in various ways without departing from the spirit or scope of the present invention. Therefore, the drawings and descriptions are considered to be exemplary and non-restrictive in nature.

[0030] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.

[0031] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.

[0032] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, an electrical connection, or a communication; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0033] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is lower in level than the second feature.

[0034] It should be understood that when used in this specification and the appended claims, the terms "include" and "comprises" indicate the presence of described features, integers, steps, operations, elements and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components and / or combinations thereof.

[0035] It should also be understood that the terms used in the present specification are only for the purpose of describing specific embodiments and are not intended to limit the present invention. As used in the present specification and the appended claims, unless the context clearly indicates otherwise, the singular forms "a", "an" and "the" are intended to include plural forms.

[0036] It should be further understood that the term "and / or" used in the present description and the appended claims refers to any and all possible combinations of one or more of the associated listed items, and includes these combinations.

[0037] Various structural schematic diagrams of the embodiments disclosed in the present invention are shown in the accompanying drawings. These figures are not drawn to scale, and some details are magnified and some details may be omitted for the purpose of clear expression. The shapes of various regions and layers shown in the figures and the relative sizes and positional relationships therebetween are only exemplary, and may deviate in practice due to manufacturing tolerances or technical limitations, and those skilled in the art may additionally design regions / layers with different shapes, sizes, and relative positions according to actual needs.

[0038] The embodiments of the present invention are described in detail below with reference to the accompanying drawings.

[0039] A blade preforging profile design method of the present invention comprises the following steps:

[0040] Step 1, select the A0 section and the N section from the sections of the pre-forging profile design, and select the middle section between the A0 section and the N section according to the preset distance to form a set of theoretical profiles in several sections from the A0 section to the N section for pre-forging design.

[0041] Step 2, connect the center of the leading edge circle and the trailing edge circle of the theoretical profile, make tangent circles of the upper and lower curves of the theoretical profile with the bisector as the center at each n equal parts of the X-axial distance L, and use splines to connect the centers of all tangent circles in sequence starting from the center of the leading edge to produce the center arc line of the theoretical profile.

[0042] Step 3, make a tangent circle to the theoretical profile in step 1 with the intersection of the midline of the X-axis distance L and the mid-arc line of step 2 as the center, and make tangent circles to the theoretical profile on both sides of the midline of the X-axis distance L.

[0043] Step 4: According to the deformation of the blade, the diameters of the three circles in step 3 are enlarged at the centers to obtain three new circles. Arcs are drawn to be tangent to the upper and lower halves of the three new circles, and an arc is obtained, which is recorded as arc R. 上 , arc R 下 .

[0044] Step 5: According to the arc R 上, arc R 下 With the new circles at both ends in step 4, a closed pre-forging profile is obtained.

[0045] Step 6, repeating steps 2 to 5 to complete the theoretical profile operation of the remaining sections selected in step 1, and obtaining a set of closed pre-forging profiles, and performing 3D modeling of the subsequent pre-forgings based on the obtained set of closed pre-forging profiles; after the 3D modeling, the 3D software can be programmed, and a physical mold can be processed by a CNC machine tool, and the mold can be used to produce pre-forgings that meet the deformation degree and reasonable metal distribution.

[0046] The present invention provides a method for designing the profile of a blade pre-forging. The method divides the entire blade profile into several control sections, takes the two sides and the middle three points of each control section to calculate the respective offsets, and then re-models the blade. This avoids the problem of the underpressure design method used in the prior art, which uses the thickness of the thickest part of the blade profile * the deformation, and the upper and lower surfaces are offset by a certain distance as a whole, resulting in large metal flow resistance and large dimensional deformation during forming. It also avoids the problem of large differences in deformation degrees of various parts of the elliptical method pre-forging profile, which affects the uniformity of the grains, the metal is first bent and then formed during the deformation process, the residual stress is large, and the blade is prone to metallurgical defects such as longitudinal light and dark stripes and cracks. The present invention reasonably distributes the metal volume to make the deformation degree of the blade consistent during final forging, thereby obtaining a more uniform structure. The blade profile is thick in the middle, followed by the leading edge, and the thinnest at the trailing edge. The pre-forged part designed using this method is placed in the final forging die, with only the middle area of ​​the pre-forging fitting into contact with the die, and large areas of the leading and trailing edges being away from the die. This, on the one hand, reduces the temperature loss caused by heat transfer between the pre-forging and the die, maintaining a relatively high initial forging temperature; on the other hand, the volume distribution and curvature direction of the pre-forging are conducive to the flow of metal. This design method can achieve better dimensional accuracy, surface quality, and uniform structure.

[0047] Example 1

[0048] The present invention provides a blade preforging profile design method, which is a design method for how blade parts are designed from a final theoretical profile to a preforging profile, so as to achieve reasonable volume distribution of the preforging and uniform deformation degree; the method is implemented by the following steps:

[0049] (1) Selection of theoretical profiles: The final blade body is controlled by a set of theoretical profiles from section A0 to section N, where the distance from section A0 to section N is S. The sections used for pre-forging profile design are first selected as section A0 and section N. The middle section is the data calculated from A0 for each additional S / m position (m can be 2, 3, 4, 5, 6), and the section closest to the data is selected. In this way, a set of m+1 theoretical profiles from section A0 to section N are selected for pre-forging design.

[0050] (2) Calculate the mid-arc line: Connect the center of the leading edge circle and the trailing edge circle of the theoretical profile. At an X-axis distance of L, make a tangent circle (n ≥ 9) of the upper and lower curves of the theoretical profile with the bisector as the center at each n equal parts of the distance L. Use a spline to connect the centers of all the tangent circles in sequence starting from the center of the leading edge to produce the mid-arc line of the theoretical profile.

[0051] (3) Define control points: Delete the auxiliary tangent circle, keep the theoretical profile line and the middle arc line, and make a tangent circle to the theoretical profile line with the intersection of the middle line of L and the middle arc line as the center, with a diameter of ΦT0. Perform the above operation at the position where the middle line is offset to the left and right by L / 3, with diameters of ΦT1 and ΦT2 respectively.

[0052] (4) Generate cross-section line: The deformation of the blade is X% (generally between 20% and 80% depending on the material properties). The diameter of the three circles is enlarged by 1 / (1-X%) times to obtain a new enlarged circle. Arc lines are drawn to be tangent to the upper and lower halves of the three new circles, and an upper and lower arc line is obtained, which is recorded as R. 上 , R down.

[0053] (5) Generate a closed line: Draw the new circle at the front edge from the 上 , R 下 The left part of the arc is interrupted at the point of tangency and counted as R1. The new circle at the rear edge is connected to R 上 , R 下 The right part of the arc is interrupted at the tangent point and counted as R2. In this way, the arcs R1 and R 上 , R2, R 下 Form a closed pre-forging profile.

[0054] (6) Repeat steps (2) to (5) to complete the theoretical profile operation of the remaining sections selected in (1), and obtain a set of closed preforging profiles for subsequent three-dimensional modeling of preforgings.

[0055] Example 2

[0056] Taking the 0th level stator blade of a certain machine as an example, the following steps are specifically included:

[0057] (1) Selection of theoretical profile: The blade body is finally controlled by a set of theoretical profiles from A0 to A24, and the distance from A0 to A24 is 109.2 mm. The sections used for pre-forging profile design are first selected as A0 and A24. The middle section is the data of each position increased by S / 4 = 27.3 mm from A0 (m is 4), and the section closest to the data is selected. In this way, a set of 4+1 theoretical profiles of A0, A3, A6, A12, and A24 sections are selected for pre-forging design.

[0058] (2) Calculate the mid-arc line: Connect the center of the leading edge circle and the trailing edge circle of the theoretical profile. At an X-axis distance of L, make a tangent circle (n=16) of the upper and lower curves of the theoretical profile with the bisector as the center at every 16 equal parts of the distance L. Use a spline to connect the centers of all the tangent circles in sequence starting from the center of the leading edge to generate the mid-arc line of the theoretical profile.

[0059] (3) Define control points: Delete the auxiliary tangent circle, keep the theoretical profile line and the mid-arc line, and make a tangent circle to the theoretical profile line with the intersection of the mid-line of L and the mid-arc line as the center. The diameter is Φ4.55 mm. The mid-line of L / 2 is offset by L / 3 toward the leading and trailing edges to intersect with the mid-arc line. Repeat the above operation to obtain the leading and trailing edge diameters of Φ3.03 mm and Φ2.57 mm, respectively.

[0060] (4) Generate cross-section line: The blade is made of TC4 titanium alloy, and the required final forging deformation of the blade body is 50% (generally between 20% and 80% according to the material properties). The three circles with unchanged centers are enlarged by 1 / (1-50%)=2 times to obtain a new enlarged circle, and arc lines are drawn to be tangent to the upper and lower halves of the three circles of Φ3.03mm, Φ4.55mm and Φ2.57mm, respectively, to obtain an upper and lower arc line, recorded as R 上 , R down.

[0061] (5) Generate a closed line: Draw the new circle at the front edge from the 上 , R 下 The left part of the arc is interrupted at the point of tangency and counted as R1. The new circle at the rear edge is connected to R 上 , R 下 The right part of the arc is interrupted at the tangent point and counted as R2. In this way, the arcs R1 and R 上 , R2, R 下 Form a closed pre-forging profile.

[0062] (6) Repeat steps (2) to (5) to complete the theoretical profile operation of the remaining sections selected in (1), and obtain a set of closed preforging profiles for later three-dimensional modeling of preforgings.

[0063] The embodiment of the present invention provides a blade preforging, which adopts the above-mentioned blade preforging profile design method to obtain a set of closed preforging profiles for later three-dimensional modeling of the preforging; according to the three-dimensional modeling of the preforging, a final forging upper die and a final forging lower die of the preforging are processed by a numerically controlled machine tool, and the preforging designed by the method is placed in the final forging die, and the forging is seen in the original state of the die. Figure 4 Only the middle area of ​​the pre-forging is in contact with the die, and a large area of ​​the front and rear edges is away from the die. On the one hand, it slows down the temperature loss caused by heat transfer between the pre-forging and the die and maintains a higher initial forging temperature. On the other hand, the volume distribution and curvature direction of the pre-forging are conducive to the flow of metal. This design method can obtain better dimensional accuracy, surface quality and uniform structure.

[0064] The above shows and describes the basic principles and main features of the present invention and the advantages of the present invention. It is obvious to those skilled in the art that the present invention is not limited to the details of the above exemplary embodiments, and the present invention can be implemented in other specific forms without departing from the spirit or basic features of the present invention. Therefore, no matter from which point of view, the embodiments should be regarded as exemplary and non-restrictive. The scope of the present invention is defined by the attached claims rather than the above description, and it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims are included in the present invention. Any figure mark in the claims should not be regarded as limiting the claims involved.

[0065] In addition, it should be understood that although this specification is described in accordance with the implementation modes, not every implementation mode contains only one independent technical solution. This description of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment can also be appropriately combined to form other implementation modes that can be understood by those skilled in the art. The above content is only to illustrate the technical idea of ​​the present invention, and cannot be used to limit the protection scope of the present invention. Any changes made on the basis of the technical solution according to the technical idea proposed by the present invention shall fall within the protection scope of the claims of the present invention.

Claims

1. A method for designing a profile of a blade preforging, characterized in that: The following steps are included: Step 1, selecting the A0 section and the N section from the sections of the pre-forging profile design, and selecting the middle section between the A0 section and the N section according to the preset distance, to form a set of theoretical profiles in several sections from the A0 section to the N section for pre-forging design; Step 2, connect the center of the leading edge circle of the theoretical profile and the trailing edge circle, make a tangent circle of the upper and lower curves of the theoretical profile with the bisector as the center at each n equal parts of the X-axial distance L, and use a spline to sequentially connect the centers of all tangent circles starting from the center of the leading edge to produce the middle arc line of the theoretical profile; Step 3, make a tangent circle to the theoretical profile in step 1 with the intersection of the midline of the X-axis distance L and the mid-arc line in step 2 as the center, and make tangent circles to the theoretical profile on both sides of the midline of the X-axis distance L; Step 4: According to the deformation of the blade, the diameters of the three circles in step 3 are enlarged at the centers to obtain three new circles. Arcs are drawn to be tangent to the upper and lower halves of the three new circles, and an arc is obtained, which is recorded as arc R. 上 , arc R 下 ; Step 5: According to the arc R 上 , arc R 下 With the new circles at both ends in step 4, a closed pre-forging profile is obtained; Step 6, repeat steps 2 to 5 to complete the theoretical profile operation of the remaining sections selected in step 1, and obtain a set of closed pre-forging profiles.

2. A blade preforging profile design method according to claim 1, characterized in that: In step 1, the distance from section A0 to section N is S; the middle section is the data calculated from A0 for each additional S / m position, and the sections closest to both sides of the data are selected to form a set of m+1 theoretical profiles from section A0 to section N for pre-forging design.

3. A blade preforging profile design method according to claim 2, characterized in that: In step 1, the range of m is 2, 3, 4, 5, 6.

4. A blade preforging profile design method according to claim 1, characterized in that: In step 2, n is selected from an integer not less than 9.

5. The method for designing a blade preforging profile according to claim 1, characterized in that: In step 3, remove the tangent circle in step 2, retain the theoretical profile in step 1 and the mid-arc in step 2, and make a tangent circle to the theoretical profile with a diameter of ΦT0 at the intersection of the midline and the mid-arc at an X-axis distance L as the center. Make tangent circles to the theoretical profile at positions offset to the left and right by L / 3 from the midline, with diameters of ΦT1 and ΦT2 respectively.

6. A blade preforging profile design method according to claim 1, characterized in that: In step 4, the deformation range of the blade molding is between 20% and 80%.

7. A blade preforging profile design method according to claim 6, characterized in that: When the blade is made of TC4 titanium alloy material, the deformation amount of the blade forming is 50%.

8. The method for designing a blade preforging profile according to claim 1, characterized in that: In step 5, the new circle at the front edge is aligned with the arc R. 上 , arc R 下 The left part of the arc is interrupted at the point of tangency and counted as R1. The new circle at the rear edge is connected to the arc R 上 , arc R 下 The right part of the arc is interrupted at the point of intersection and counted as R2. In this way, the arcs R1 and R 上 , arc R2, arc R 下 Form a closed pre-forging profile.

9. The method for designing a blade preforging profile according to claim 1, characterized in that: In step 6, three-dimensional modeling of the subsequent pre-forging is performed based on the obtained set of closed pre-forging profiles.

10. A blade preforging, characterized in that: A blade preforging profile design method as described in any one of claims 1 to 9 is used to obtain a set of closed preforging profiles for subsequent three-dimensional modeling of the preforgings; a preforging mold is processed using a CNC machine tool based on the three-dimensional modeling of the preforgings, and the preforgings are forged using the mold.

Citation Information

Patent Citations

  • Method for controlling forged blade extrusion molding residual stress

    CN110773699A

  • Blade precision forging forming method and blade

    CN115740351A

  • Blade finish forging forming die and design method

    CN115879221A

  • Method of making stamping of gas turbine engine blade from two-phase titanium alloy

    RU2818513C1

  • New moving blade modeling method for energy-saving transformation of axial flow fan with adjustable moving blades of power station

    WO2023040417A1