Welding process of tellurium-copper alloy material

By performing V-shaped bevel treatment and argon protection welding on tellurium copper alloy material, the problem of unqualified welding quality is solved, high-quality welding effect is achieved, the requirements of tensile strength and elongation are met, and it is suitable for actual processing needs. .

CN118905392APending Publication Date: 2024-11-08侯龙超
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411153591.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-21
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

Tellurium copper alloy material is difficult to complete in normal pressure welding, with slag and incomplete welding after welding, and the bevel cannot meet the production and processing needs.

Method used

V-shaped bevel welded parts are used to pickle, clean water rinse and low-temperature drying. Argon protective welding is used. The welding current is 120A and the gas flow is 8L/min to achieve argon protective melt welding.

Benefits of technology

It effectively solves the problem of unqualified welding quality of tellurium copper alloy material, meets the requirements of tensile strength and elongation, is easy to operate, and is suitable for actual processing needs.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention relates to a welding process of tellurium copper alloy materials, which comprises the following steps that tellurium copper alloy is cleaned before welding, a groove is V-shaped, and the angle of a slope surface is 45 + / -5 degrees; the welding process comprises the steps of acid pickling, clean water washing, low-temperature drying and groove preparation, and argon shield fusion welding is adopted. According to the welding process of the tellurium-copper alloy material, a groove of a weldment is in a V shape, argon shield welding is adopted, the argon flow is 8 L / min, the welding current is 120 A, and argon shield fusion welding is adopted. The mechanical properties of the welding tellurium-copper alloy material meet the conditions that the tensile strength Rm is larger than or equal to 180 MPa, and the ductility is larger than or equal to 25%. The welding technology is provided, and the actual machining requirement is met.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a welding process, in particular to a tellurium-copper alloy material welding process. Background Art

[0002] Gas shielded welding is arc welding that uses gas as the arc medium and protects the arc and welding area. There are two basic types of arcs: consumable arc and non-consumable arc. The consumable electrode melts during the welding process, and the electrode transfers the filler metal to the molten pool through the arc. There are several methods of consumable arc welding, such as tungsten inert gas shielded welding, plasma arc welding and carbon arc welding.

[0003] It is difficult to complete the welding of tellurium copper alloy materials under normal pressure. After the addition of tellurium, the copper alloy material has the property of resisting electric ablation. After normal welding, there will be post-weld slag and incomplete penetration, which will lead to unqualified welding quality. In addition, the groove during welding adopts X-type, which cannot meet the actual production and processing needs. Summary of the invention

[0004] The present invention aims to provide a welding technology to overcome the deficiencies of the prior art and effectively solve the welding problem of tellurium copper alloy materials. To achieve the above-mentioned purpose, the technical solution adopted by the present invention is: a welding process of tellurium copper alloy material, comprising the following steps: comprising the following steps: first, the workpiece to be welded is cleaned before welding, the oxide layer on the surface of the weldment is pickled, the groove of the weldment is V-shaped, and the angle of the groove surface is 45°±5°, and then pre-weld cleaning is performed, and the pre-weld cleaning includes: pickling - water rinsing - low-temperature drying - groove preparation.

[0005] The pre-welding cleaning includes: 1) the weldment needs to be pickled before welding, and the pickling concentration is 10% to 12% sulfuric acid solution; 2) rinse with clean water, using a large amount of deionized water to rinse the surface of the weldment until the pH of the solution after washing is 7; 3) after the weldment is washed, it is placed in a drying oven at 100°C for drying; 4) the weldment is made into a V-shaped groove, and the angle of the groove surface is 45°±5°.

[0006] The welding process of the tellurium copper alloy material is as follows: 1) during welding, argon gas protection welding is adopted; 2) the argon gas flow rate is 8L / min; 3) the welding current is 120A during welding. 4) argon gas protection melting welding is adopted. 5) the mechanical properties of the welded tellurium copper alloy material obtained by detection meet the following requirements: tensile strength R m ≥180MPa, elongation ≥25%.

[0007] Due to the application of the above technical solution, the present invention has the following advantages compared with the existing technology: The welding process of the tellurium-copper alloy material of the solution of the present invention is easy to operate, can perform melting welding on the tellurium-copper alloy material, and improves the quality of the welding material, thereby meeting the use requirements. DETAILED DESCRIPTION

[0008] The present invention is further described in detail below in conjunction with specific embodiments.

[0009] The welding process of a tellurium copper alloy material described in the present invention includes the following steps: first, the weld is cleaned before welding, the oxide layer on the surface of the weld is pickled, the groove of the weld is V-shaped, and the angle of the groove surface is 45°±5°, and then the weld is cleaned before welding, and the pre-weld cleaning includes: pickling - water rinsing - low-temperature drying - groove preparation. The welding process includes: 1) The weld needs to be pickled before welding, and the pickling concentration is 10% to 12% sulfuric acid solution; 2) rinse with water, use a large amount of deionized water to rinse the surface of the weld until the pH of the washed solution is 7; 3) After the weld is washed, place it in a drying oven at 100°C for drying; 4) The weld is made into a V-shaped groove, and the angle of the groove surface is 45°±5°

[0010] The welding process of a tellurium copper alloy material described in the present invention comprises the following steps: 1) argon gas protection welding is adopted during welding; 2) the argon gas flow rate is 8L / min; 3) the welding current is 120A during welding; 4) argon gas protection melting welding is adopted.

[0010] The obtained welded tellurium copper alloy material was tested for performance, and ten samples were taken to obtain the average value. The tensile test of metal materials refers to the standard GB / T228, and the mechanical properties of the welded tellurium copper alloy material obtained are as follows: tensile strength R m =220MPa, elongation =30%.

[0011] The welding process of the tellurium copper alloy material of the present invention is easy to operate. After the welding is processed in the early stage, a V-shaped groove is adopted, the tellurium copper alloy material can be melt-welded, and the quality of the welding material is improved, thereby meeting the actual processing requirements.

[0012] The above are only specific application examples of the present invention and do not constitute any limitation on the protection scope of the present invention. Any technical solution formed by equivalent transformation or equivalent replacement shall fall within the protection scope of the present invention.

Claims

1. A welding process for tellurium copper alloy material, characterized in that: The method comprises the following steps: firstly, cleaning the weldment before welding, pickling the surface oxide layer of the weldment, the groove of the weldment is V-shaped, and the angle of the groove surface is 45°±5°, and then cleaning before welding is performed, wherein the cleaning before welding comprises: pickling - water washing - low temperature drying - groove preparation, and argon gas protection melting welding is adopted.

2. The welding process of the tellurium copper alloy material according to claim 1, characterized in that: The pre-welding cleaning includes: 1) the weldment needs to be pickled before welding, and the pickling concentration is 10%~12% sulfuric acid solution; 2) rinse with clean water, using a large amount of deionized water to rinse the surface of the weldment until the pH of the solution after washing is 7; 3) after the weldment is washed, it is placed in a drying oven at 100°C for drying; 4) the weldment is made into a V-shaped groove, and the angle of the groove surface is 45°±5°.

3. The welding process of the tellurium copper alloy material according to claim 1, characterized in that: 1) During welding, argon gas protection welding is used; 2) The argon gas flow rate is 8L / min; 3) The welding current is 120A. 4) Argon gas protection melting welding is used.