Method and device for visualizing flow track of polishing solution
By adding developing particles and fluorescent dye to the polishing liquid, the flow characteristics of the polishing liquid are collected using dual-emission ultraviolet laser technology, the problem of difficult collection of the polishing liquid flow trajectory is solved, and more accurate interface data acquisition is achieved, and chemical machinery is promoted. Optimization of polishing technology.
Patent Information
- Application Number
- CN202411060909.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-02
- Publication Date
- 2024-11-08
AI Technical Summary
During the chemical mechanical polishing process, due to the complex movement trajectory of the polishing head and the opaque polishing liquid, it is difficult to collect in-situ data. The existing model is based on a simplified system and the simulation data is limited, making it difficult to fully characterize the flow characteristics of the interface polishing liquid.
Add developing particles and two fluorescent dyes to the polishing liquid, use the dual-emission ultraviolet laser pulser and the camera to acquire the first and second polishing indicators of the interface position, and derive the liquid film thickness and interface contact state, and realize it through the transparent parts to be polished In-situ data collection.
It improves the accuracy of parameter acquisition during chemical mechanical polishing, facilitates subsequent interface status research, and promotes the optimization of polishing technology.
Smart Images

Figure CN118905949A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of polishing liquid flow trajectory, and more specifically, relates to a polishing liquid flow trajectory visualization method and device. Background Art
[0002] In the process of chemical mechanical polishing (CMP), the polishing head has a complex motion trajectory, and the polishing pad, wafer and polishing liquid are opaque, which makes it extremely difficult to collect in-situ data during the CMP process. In most cases, the data collected during the chemical mechanical polishing process are mostly result data, or collected from non-in-situ, which is not conducive to studying the flow trajectory characteristics of the polishing liquid at the interface.
[0003] In the prior art, some mechanistic models have been developed to explain the chemical mechanical polishing phenomenon, but these models have only limited empirical data. Moreover, in most cases, the CMP data are obtained from overly simplified systems, and the fluid characteristics of the polishing liquid at the interface during the chemical mechanical polishing process have not been fully characterized.
[0004] Most scholars believe that simulation is a feasible alternative method for the study of CMP process. In the past, the numerical model of CMP process was based on contact mechanics, fluid dynamics or partial contact and non-contact fluid dynamics methods.
[0005] For example, many scholars have studied the effects of grooveless pads and circular radial pad grooves on the velocity distribution of the polishing liquid, as well as the effects of polishing head pressure, polishing liquid film thickness and polishing liquid velocity distribution on polishing performance. The main focus of scholars is to effectively understand the interaction between "wafer-polishing liquid-polishing pad" during the CMP process through simulation. However, since many parameters in the CMP process change all the time and belong to microscopic processes (such as the alternation of old and new polishing liquids, changes in the position of the active area with the swing of the polishing head, changes in temperature during the action process, and consumption of polishing pad thickness, etc.), CMP simulation has many difficulties in realizing the actual working conditions of CMP, and it is difficult to directly characterize the CMP process. Therefore, the data collected from the simulation platform has certain limitations, which affects the subsequent research progress of wafer polishing. Summary of the invention
[0006] The purpose of the present invention is to provide a method and device for visualizing the flow trajectory of a polishing liquid, which can collect the first polishing index and the second polishing index in situ during the chemical mechanical polishing process, ensure the accuracy of parameter collection, and facilitate subsequent research on the interface state.
[0007] To achieve the above object, the technical solution adopted by the present invention is: to provide a method for visualizing the flow trajectory of a polishing liquid, comprising the following steps: S100: putting the developer particles and two fluorescent dyes into the polishing liquid respectively, installing the transparent workpiece to be polished on the rotating spindle of the polishing equipment, starting the polishing equipment, and spraying the polishing liquid onto the polishing pad; S200: using a double-emission ultraviolet laser pulser to sequentially irradiate the interface position of the transparent workpiece to be polished twice, and using a double-emission ultraviolet fluorescence technology and a camera to collect the first polishing index of the interface position twice; S300: turning off the dual-emission ultraviolet laser pulser, applying the developing particle tracing technology and using a camera to collect the second polishing index of the interface position; S400: Derivation of the liquid film thickness of the polishing liquid according to the first polishing index obtained twice; S500: Obtaining an interface contact state and an interface friction coefficient according to the first polishing index and the second polishing index obtained twice.
[0008] In a possible implementation, in step S100, the developer particles are formed by silicon dioxide particles dyed with fluorescein isothiocyanate, and the diameter of the silicon dioxide particles is 0.5 micrometers to 1.5 micrometers.
[0009] In one possible implementation, in step S200, the dual-emitting ultraviolet laser pulser emits ultraviolet light of a first wavelength to the interface position of the transparent workpiece to be polished, the ultraviolet light of the first wavelength is used to stimulate the development of one of the fluorescent dyes, and the first polishing index under the action of the first wavelength ultraviolet light is collected by a camera; thereafter, the dual-emitting ultraviolet laser pulser emits ultraviolet light of a second wavelength to the interface position of the transparent workpiece to be polished, the ultraviolet light of the second wavelength is used to stimulate the development of another fluorescent dye, and the first polishing index under the action of the second wavelength ultraviolet light is collected by a camera.
[0010] In some embodiments, in step S200, the first polishing index includes the flow velocity and flow direction of the polishing liquid, the recirculation behavior of the old polishing liquid, and the circulation behavior of the new and old polishing liquids.
[0011] In some embodiments, in step S200, the second polishing index includes the moving speed of the developer particles and the retention phenomenon of the developer particles.
[0012] In a possible implementation, in step S400, the interface contact state includes a boundary lubrication state, a mixed lubrication state, and a fluid dynamic lubrication state.
[0013] In some embodiments, the moving speed of the developer particles in the boundary lubrication state is less than the moving speed of the developer particles in the mixed lubrication state and less than the moving speed of the developer particles in the hydrodynamic lubrication state.
[0014] In some embodiments, the thickness of the liquid film in the boundary lubrication state is less than the thickness of the liquid film in the mixed lubrication state and less than the thickness of the liquid film in the hydrodynamic lubrication state.
[0015] Compared with the prior art, the scheme shown in the embodiment of the present application can conveniently collect in-situ data of the "wafer-polishing liquid-polishing pad" interface during the chemical mechanical polishing process by adding developer particles and two fluorescent dyes to the polishing liquid. During the operation, a transparent workpiece to be polished is selected to facilitate the visualization of the characteristics of the interface position, so as to better collect polishing indicators, thereby promoting people to further optimize the chemical mechanical polishing technology.
[0016] The present invention also provides a polishing liquid flow trajectory visualization device, including a polishing pad, a polishing liquid dispenser, a transparent workpiece to be polished, a dual-emitting ultraviolet laser pulser and a camera. The transparent workpiece to be polished is connected to the rotating spindle of the polishing equipment through a telescopic rod. The dual-emitting ultraviolet laser pulser and the camera are respectively mounted above the transparent workpiece to be polished. The emitting end of the dual-emitting ultraviolet laser pulser is arranged toward the transparent workpiece to be polished and is used to emit ultraviolet rays to the transparent workpiece to be polished. The camera is arranged toward the transparent workpiece to be polished and is used to collect a first polishing index and a second polishing index at the interface position of the transparent workpiece to be polished.
[0017] Double-emitting ultraviolet laser pulser Double-emitting ultraviolet laser pulser In a possible implementation, the upper end of the telescopic rod is connected to the rotating main shaft through a reverse flange, and the lower end of the telescopic rod is connected to the transparent workpiece to be polished through a connecting piece, and the transparent workpiece to be polished is an acrylic material component, and the transmittance of the transparent workpiece to be polished is greater than 92%.
[0018] The above-mentioned device uses a dual-emission ultraviolet laser pulser to emit ultraviolet rays to the interface of the transparent workpiece to be polished, and uses a polishing liquid dispenser to spray polishing liquid to the interface. Then, the first polishing index and the second polishing index are collected with the help of a camera, and parameters such as liquid film thickness are derived. In-situ data collection can be conveniently performed. During the operation, a transparent workpiece to be polished is selected to facilitate the visualization of the characteristics of the interface position, so as to better collect polishing indicators, thereby promoting further optimization of chemical mechanical polishing technology. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0020] Figure 1A schematic diagram of the structure of a polishing liquid flow trajectory visualization device provided by an embodiment of the present invention; Figure 2 A schematic diagram of the structure of a transparent workpiece to be polished and a telescopic rod in a polishing liquid flow trajectory visualization device provided in an embodiment of the present invention; Figure 3 A contact state diagram of a transparent workpiece to be polished, a polishing liquid and a polishing pad in a method for visualizing a flow trajectory of a polishing liquid according to an embodiment of the present invention; Figure 4 It is a flow diagram of the overall flow trajectory of the polishing liquid and the developer particles in the polishing liquid flow trajectory visualization method according to an embodiment of the present invention.
[0021] Among them, the reference numerals in the figure are: 1. Polishing pad; 2. Polishing liquid dispenser; 3. Transparent workpiece to be polished; 4. Double-emitting ultraviolet laser pulser; 5. Camera; 6. Telescopic rod; 61. Reverse flange; 7. Polishing liquid. DETAILED DESCRIPTION
[0022] In order to make the technical problems, technical solutions and beneficial effects to be solved by the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.
[0023] It should be noted that when an element is referred to as being "disposed on" another element, it may be directly on another element or indirectly on another element. It should be understood that the orientation or positional relationship indicated by the terms "length", "width", "upper", "lower", "front", "back", "top", "bottom", "inside", "outside", etc. is based on the orientation or positional relationship shown in the accompanying drawings, which is only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation of the present invention. The terms "first" and "second" are only used for descriptive purposes and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "several" is two or more, unless otherwise clearly and specifically defined.
[0024] Please also read Figures 1 to 4 Now, the polishing liquid flow trajectory visualization method and device provided by the present invention are described. The polishing liquid flow trajectory visualization method comprises the following steps: S100: Put the developer particles and two fluorescent dyes into the polishing liquid respectively, install the transparent workpiece 3 to be polished on the rotating spindle of the polishing equipment, start the polishing equipment, and spray the polishing liquid onto the polishing pad 1; the developer particles are formed by silicon dioxide particles dyed with fluorescein isothiocyanate, and the diameter of the silicon dioxide particles is 0.5 microns-1.5 microns.
[0025] S200: using a double-emission ultraviolet laser pulser 4 to sequentially irradiate the interface position of the transparent workpiece to be polished 3 twice, and using a double-emission ultraviolet fluorescence technology and a camera 5 to collect the first polishing index of the interface position twice.
[0026] The dual-emission ultraviolet laser pulser 4 emits ultraviolet light of a first wavelength to the interface position of the transparent workpiece to be polished, and the ultraviolet light of the first wavelength is used to stimulate the development of one of the fluorescent dyes, and the first polishing index under the action of the first wavelength ultraviolet light is collected by the camera 5; then, the dual-emission ultraviolet laser pulser 4 emits ultraviolet light of a second wavelength to the interface position of the transparent workpiece to be polished, and the ultraviolet light of the second wavelength is used to stimulate the development of another fluorescent dye, and the first polishing index under the action of the second wavelength ultraviolet light is collected by the camera 5. The first polishing index includes the flow speed and flow direction of the polishing liquid, the recirculation behavior of the old polishing liquid, and the circulation behavior of the new and old polishing liquids.
[0027] S300: Turn off the dual-emission ultraviolet laser pulser 4, apply the developer particle tracing technology, and use the camera 5 to collect the second polishing index of the interface position; the second polishing index includes the moving speed of the developer particles and the retention phenomenon of the developer particles.
[0028] S400: Derivation of the liquid film thickness of the polishing liquid according to the first polishing indexes obtained twice.
[0029] S500: Obtaining an interface contact state and an interface friction coefficient according to the first polishing index and the second polishing index obtained twice.
[0030] The interface contact state includes boundary lubrication state, mixed lubrication state and hydrodynamic lubrication state. It should be noted that the moving speed of the developing particles in the boundary lubrication state is less than the moving speed of the developing particles in the mixed lubrication state and less than the moving speed of the developing particles in the hydrodynamic lubrication state.
[0031] The thickness of the liquid film in the boundary lubrication state is less than the thickness of the liquid film in the mixed lubrication state. The thickness of the liquid film in the hydrodynamic lubrication state is less than the thickness of the liquid film in the hydrodynamic lubrication state. Fluorescent dye. The method for visualizing the flow trajectory of the polishing liquid provided in this embodiment, compared with the prior art, can conveniently collect in-situ data of the "wafer-polishing liquid-polishing pad" interface during the chemical mechanical polishing process by adding developer particles and two fluorescent dyes to the polishing liquid. A transparent workpiece to be polished 3 is selected during the operation to facilitate visualization of the features of the interface position, so as to better collect polishing indicators, thereby promoting further optimization of the chemical mechanical polishing technology.
[0032] In this embodiment, the interface position refers to the direct action area of "wafer-polishing liquid-polishing pad". The transparent piece to be polished 3 is made of acrylic sheet and is used as a substitute for silicon wafer. The transparent piece to be polished 3 has similar polishing characteristics as semiconductor wafer. In addition, the transparent piece to be polished 3 also has high surface hardness and good wear resistance, and can repeatedly complete the CMP process without breaking the material.
[0033] On this basis, the acrylic transparent polishing piece 3 has a certain solvent resistance, can withstand relatively dilute inorganic acids, alkalis and aliphatic hydrocarbons, is insoluble in water, methanol, glycerol, etc., and can meet the process conditions of CMP. The most important point is that the light transmittance of the transparent polishing piece 3 is like glass, with a light transmittance of more than 92%, which is convenient for data collection of the area below it (that is, the area above the polishing pad 1).
[0034] In the above operation method, two fluorescent dyes are added to the polishing liquid respectively, and the two fluorescent dyes can be developed separately by emitting ultraviolet rays of different wavelengths through the dual-emission ultraviolet laser pulser 4, which is convenient for using the image presentation technology of the fluorescent dye to realize in-situ collection with the help of the camera 5. The dual-emission ultraviolet laser pulser 4 is used as a light source to irradiate the polishing liquid at the interface position, and the flow trajectory of the entire polishing liquid at the interface is visualized using the fluorescent dye online color imaging technology, thereby collecting the flow characteristics of the polishing liquid.
[0035] At the same time, the developer particles have a good tracing effect, and development can be achieved without the use of the dual-emission ultraviolet laser pulser 4 for irradiation, which makes it easy to use the camera 5 to collect the second polishing index and obtain the moving speed and retention phenomenon of the developer particles. The developer particles are small enough and have a large enough surface area, which is usually quantified by the Stokes number, which should be less than 0.1. Therefore, the developer particles can be captured by the surface tension of the polishing liquid (fluid) and can move with the fluid. Therefore, the behavior of the developer particles is considered to be a good estimate of the behavior of the fluid. Therefore, the flow trajectory characteristics of the polishing liquid collected in the above manner can visualize the flow trajectory of the polishing liquid at the interface, so that people can better understand the flow trajectory characteristics of the polishing liquid at the interface.
[0036] Finally, the liquid film thickness of the polishing liquid can be obtained by analyzing and deducing the two first polishing indicators. The interface contact state and friction coefficient at different positions can be obtained by analyzing and deducing the first polishing indicator and the second polishing indicator, which facilitates further understanding of the flow trajectory characteristics of the polishing liquid at the interface.
[0037] Therefore, the polishing liquid fluid characteristics at the interface are visualized by adding fluorescent dyes and developer particles, so as to better understand the polishing liquid fluid characteristics at the interface and collect corresponding parameters to promote further optimization of chemical mechanical polishing. The first polishing index and the second polishing index can be directly obtained by the above method, and the following indexes can also be derived, see Table 1: Table 1:
[0038] The present invention also provides a polishing liquid flow trajectory visualization device, comprising a polishing pad 1, a polishing liquid dispenser 2, a transparent workpiece to be polished 3, a dual-emitting ultraviolet laser pulser 4 and a camera 5. The transparent workpiece to be polished 3 is connected to a rotating spindle via a telescopic rod 6. The dual-emitting ultraviolet laser pulser 4 and the camera 5 are respectively mounted above the transparent workpiece to be polished 3. The emitting end of the dual-emitting ultraviolet laser pulser 4 is arranged toward the transparent workpiece to be polished 3 and is used to emit ultraviolet rays to the transparent workpiece to be polished 3. The camera 5 is arranged toward the transparent workpiece to be polished 3 and is used to collect a first polishing index and a second polishing index of the interface position of the transparent workpiece to be polished 3.
[0039] In a possible implementation, the upper end of the telescopic rod 6 is connected to the rotating main shaft through a reverse flange 61, and the lower end of the telescopic rod 6 is connected to the transparent part to be polished 3 through a connecting piece. The transparent part to be polished 3 is an acrylic material component, and the transmittance of the transparent part to be polished 3 is greater than 92%.
[0040] The above-mentioned device uses a dual-emission ultraviolet laser pulser 4 to emit ultraviolet rays to the interface of the transparent workpiece to be polished 3, and uses a polishing liquid dispenser 2 to spray polishing liquid to the interface. Then, the first polishing index and the second polishing index are collected with the help of a camera 5, and parameters such as liquid film thickness are derived. In-situ data collection can be conveniently performed. During the operation, a transparent workpiece to be polished 3 is selected to facilitate visualization of the characteristics of the interface position, so as to better collect polishing indicators, thereby promoting further optimization of chemical mechanical polishing technology.
[0041] Embodiment 1: S100: Put the developer particles and two fluorescent dyes into the polishing liquid respectively, install the transparent workpiece 3 to be polished on the rotating spindle of the polishing equipment, start the polishing equipment, and spray the polishing liquid onto the polishing pad 1; the developer particles are formed by dyeing silicon dioxide particles with fluorescein isothiocyanate, wherein the developer particles are formed by dyeing silicon dioxide particles with fluorescein isothiocyanate, and the diameter of the silicon dioxide particles is 1 micron.
[0042] S200: using a double-emission ultraviolet laser pulser 4 to sequentially irradiate the interface position of the transparent workpiece to be polished 3 twice, and using a double-emission ultraviolet fluorescence technology and a camera 5 to collect the first polishing index of the interface position twice.
[0043] The shooting parameter of the camera is 60 frames per second.
[0044] Among them, the dual-emitting ultraviolet laser pulser 4 emits ultraviolet light of the first wavelength to the interface position of the transparent workpiece to be polished 3, and the first wavelength ultraviolet light is used to stimulate the development of one of the fluorescent dyes, and the camera 5 is used to collect the first polishing index under the action of the first wavelength ultraviolet light; then, the dual-emitting ultraviolet laser pulser 4 emits ultraviolet light of the second wavelength to the interface position of the transparent workpiece to be polished 3, and the second wavelength ultraviolet light is used to stimulate the development of another fluorescent dye, and the camera 5 is used to collect the first polishing index under the action of the second wavelength ultraviolet light. The first polishing index includes the flow speed and flow direction of the polishing liquid, the recirculation behavior of the old polishing liquid, and the circulation behavior of the new and old polishing liquids. The liquid film thickness of the polishing liquid can be derived by obtaining the first polishing index twice, and the above method can visualize the overall flow trajectory of the polishing liquid at the interface position.
[0045] When collecting the second polishing index of the polishing liquid, since the developer particles are small enough and have a good tracing effect, the second polishing index such as the moving speed and retention phenomenon of the developer particles can be easily collected, and then the interface contact state and interface friction coefficient can be derived in combination with the first polishing index.
[0046] The developer particles have a sufficiently large surface area, which is usually quantified by the Stokes number, which should be less than 0.1. Therefore, the developer particles can be captured by the surface tension of the polishing liquid (fluid) and can move with the fluid. Therefore, the behavior of the developer particles is considered to be a good estimate of the behavior of the fluid. Therefore, the flow trajectory characteristics of the polishing liquid collected by the above method can visualize the flow trajectory of the polishing liquid at the interface, so that people can better understand the flow trajectory characteristics of the polishing liquid at the interface.
[0047] In the above operation, the first polishing index and the second polishing index of the polishing liquid can be directly collected, and the moving speed and moving direction parameters of the polishing liquid can be accurately obtained, and the moving speed and moving direction parameters of the developer particles can also be obtained. At the same time, the liquid film thickness, interface contact state, and interface friction coefficient parameters can be derived. The flow trajectory of the polishing liquid at the interface can be visualized through the collected first polishing index and second polishing index, so as to promote people to further optimize chemical mechanical polishing.
[0048] It should be noted that two types of fluorescent dyes need to be selected. The dual-emitting ultraviolet laser pulser 4 can emit ultraviolet rays of different wavelengths in different time periods to trigger the development of one of the fluorescent dyes. The camera 5 can be set to one or two. The camera 5 is used to record the fluorescence intensity of the corresponding fluorescent dyes under two different wavelengths, and then the first polishing index is collected. According to the 2004 document Measurements of slurry film thickness and wafer drag during CMP, after the light intensity ratio detected by the camera 5 is properly calibrated, the liquid film thickness of the polishing liquid can be derived. It is worth mentioning that the two fluorescent dyes used can be excited at different wavelengths, so the different fluorescence intensities of the other fluorescent dye in the polishing liquid can be recorded by the camera 5.
[0049] S300: Turn off the dual-emission ultraviolet laser pulser 4, apply the developing particle tracing technology, and use the camera 5 to collect the second polishing index of the interface position; S400: Derivation of the liquid film thickness of the polishing liquid according to the first polishing indexes obtained twice.
[0050] S500: Obtaining an interface contact state and an interface friction coefficient according to the first polishing index and the second polishing index obtained twice. Among them, the interface contact state includes boundary lubrication state, mixed lubrication state and fluid dynamic lubrication state.
[0051] It should be noted that the moving speed of the developer particles in the boundary lubrication state is less than the moving speed of the developer particles in the mixed lubrication state and less than the moving speed of the developer particles in the hydrodynamic lubrication state.
[0052] At the same time, the thickness of the liquid film in the boundary lubrication state is less than the thickness of the liquid film in the mixed lubrication state and less than the thickness of the liquid film in the hydrodynamic lubrication state.
[0053] The polishing index of the polishing liquid is obtained according to the flow trajectory characteristic analysis of the polishing liquid, and the polishing index includes the interface contact state and the interface friction coefficient of the polishing liquid. Among them, the interface contact state includes the boundary lubrication state, the mixed lubrication state and the fluid dynamic lubrication state. The moving speed of the developing particles in the boundary lubrication state is less than the moving speed of the developing particles in the mixed lubrication state. The moving speed of the developing particles in the fluid dynamic lubrication state is less than the moving speed of the developing particles in the fluid dynamic lubrication state. The liquid film thickness in the boundary lubrication state is less than the liquid film thickness in the mixed lubrication state. The liquid film thickness in the fluid dynamic lubrication state is less than the liquid film thickness in the mixed lubrication state.
[0054] Three test points 1, 2 and 3 are set on the periphery of the transparent workpiece 3 to be polished. The distances between the three test points and the center of the transparent workpiece 3 to be polished are equal. The distance between point 3 and the center of the transparent workpiece 3 to be polished is the largest, the distance between point 1 and the center of the transparent workpiece 3 to be polished is the smallest, and the distance between point 2 and the center of the transparent workpiece 3 to be polished is centered.
[0055] See also Figure 4 The polishing liquid flow trajectory characteristics at points 1, 2 and 3 captured by camera 5 are shown in the figure. The following conclusions can be drawn by analyzing the above flow trajectory characteristics.
[0056] Conclusion 1: Due to the rotation of the polishing pad 1 and the blocking effect of the edge of the transparent workpiece 3 to be polished, most of the new polishing liquid just sprayed onto the polishing pad 1 is pushed outward and thrown out of the transparent workpiece 3 to be polished.
[0057] Conclusion 2: There is a small amount of old polishing liquid (polishing liquid previously sprayed onto the polishing pad 1) recirculating at point 3.
[0058] Conclusion 3: The polishing liquid flows around the periphery of the transparent workpiece 3 to be polished, and multiple cycles are formed at point 2 and point 3, with a small and stable recycling area where new and old polishing liquids are mixed formed between the two.
[0059] Conclusion 4: The developer particles at point 1 stay on the polishing pad 1 more than once, and the moving speed of the developer particles is relatively low, that is, there is a retention phenomenon of the developer particles.
[0060] See also Figure 4 , combined with the above analysis results, we can obtain the following further findings.
[0061] For point 1, the presence of developer particle retention indicates that the interface state here may be boundary lubrication or mixed lubrication. Afterwards, since the film thickness of the polishing liquid here is moderate, it indicates that the interface here is in mixed lubrication.
[0062] For point 2, since the moving direction of the developer particles here is multi-directional or uncertain, it indicates that point 2 may be in a fluid lubrication state. At the same time, since the film thickness of the polishing liquid is the largest, it indicates that this position is in a fluid lubrication state. By analogy, the interface contact states at different positions can be obtained.
[0063] Based on the same inventive concept, an embodiment of the present application also provides a polishing liquid flow trajectory visualization device, including a polishing pad 1, a polishing liquid dispenser 2, a transparent workpiece to be polished 3, a dual-emitting ultraviolet laser pulser 4 and a camera 5. The transparent workpiece to be polished 3 is connected to the rotating spindle through a telescopic rod 6. The dual-emitting ultraviolet laser pulser 4 and the camera 5 are respectively mounted above the transparent workpiece to be polished 3. The emitting end of the dual-emitting ultraviolet laser pulser 4 is arranged toward the transparent workpiece to be polished 3 and is used to emit ultraviolet rays to the transparent workpiece to be polished 3. The camera 5 is arranged toward the transparent workpiece to be polished 3 and is used to collect the first polishing index and the second polishing index.
[0064] In this embodiment, the polishing liquid dispenser 2 contains a polishing liquid 7, and the polishing liquid 7 is mixed with developer particles. The developer particles are formed by dyeing silicon dioxide particles with fluorescein isothiocyanate, and the polishing liquid dispenser 2 is used to spray the polishing liquid 7 containing the developer particles onto the polishing pad 1, and the spraying position of the polishing liquid dispenser 2 is close to the transparent workpiece 3 to be polished.
[0065] The transparent workpiece to be polished 3 is connected to the rotating main shaft through a telescopic rod 6 , and the telescopic rod 6 can drive the transparent workpiece to be polished to perform lifting and lowering movements, thereby meeting the polishing start and stop requirements of the transparent workpiece to be polished 3 .
[0066] The dual-emission ultraviolet laser pulser 4 is used to emit ultraviolet rays of different wavelengths to the transparent workpiece 3 to be polished, so that the fluorescence intensity of the corresponding fluorescent dye in the polishing liquid 7 can be effectively collected by the camera 5. In addition, without the need for irradiation 4 by the dual-emission ultraviolet laser pulser, the camera can also collect the second polishing index such as the moving speed and retention phenomenon of the developer particles, and the liquid film thickness developer particles of the polishing liquid 7 can be derived according to the first polishing index. In addition, the interface contact state and interface friction state can be derived according to the first polishing index and the second polishing index.
[0067] The above-mentioned device can conveniently collect in-situ data of the "wafer-polishing liquid-polishing pad" interface during the chemical mechanical polishing process. The use of transparent workpieces to be polished during operation facilitates the visualization of the characteristics of the interface position, so as to better collect polishing indicators, thereby promoting further optimization of chemical mechanical polishing technology.
[0068] In a possible implementation, the upper end of the telescopic rod 6 is connected to the rotating main shaft through a reverse flange 61, and the lower end of the telescopic rod 6 is connected to the transparent part to be polished 3 through a connecting piece. The transparent part to be polished 3 is an acrylic material component, and the transmittance of the transparent part to be polished 3 is greater than 92%. In this embodiment, the fixed end (i.e., the upper end) of the telescopic rod 6 is connected to the rotating main shaft through the reverse flange 61, and can rotate circumferentially under the drive of the rotating main shaft. The extended end (i.e., the lower end) of the telescopic rod 6 is connected to the transparent workpiece to be polished 3 through a connecting piece, and can drive the transparent workpiece to be polished 3 to move up and down to achieve contact or separation between the transparent workpiece to be polished 3 and the polishing pad.
[0069] Specifically, the transparent acrylic piece to be polished 3 is solvent-resistant, resistant to relatively dilute inorganic acids, resistant to alkalis and resistant to aliphatic hydrocarbons, insoluble in water, methanol, glycerol, etc., and can meet the process conditions of CMP. In addition, the light transmittance of the transparent piece to be polished 3 is like glass, with a light transmittance of more than 92%, which is convenient for data collection of the area below it.
[0070] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. Visualization method of polishing liquid flow trajectory, It is characterized in that The following steps are involved: S100: putting developer particles and two fluorescent dyes into polishing liquid respectively, installing the transparent workpiece to be polished on the rotating spindle of the polishing device, starting the polishing device, and spraying the polishing liquid onto the polishing pad; S200: using a double-emission ultraviolet laser pulser to sequentially irradiate the interface position of the transparent workpiece to be polished twice, and using a double-emission ultraviolet fluorescence technology and a camera to collect the first polishing index of the interface position twice; S300: turning off the dual-emission ultraviolet laser pulser, applying the developing particle tracing technology and using a camera to collect the second polishing index of the interface position; S400: Derivation of the liquid film thickness of the polishing liquid according to the first polishing index obtained twice; S500: Obtaining an interface contact state and an interface friction coefficient according to the first polishing index and the second polishing index obtained twice.
2. The method for visualizing the flow trajectory of the polishing liquid according to claim 1, It is characterized in that In step S100 , the developer particles are formed by dyeing silicon dioxide particles with fluorescein isothiocyanate, and the diameter of the silicon dioxide particles is 0.5 micrometers to 1.5 micrometers.
3. The method for visualizing the flow trajectory of the polishing liquid according to claim 1, It is characterized in that In step S200, the dual-emission ultraviolet laser pulser emits ultraviolet light of a first wavelength to the interface position of the transparent workpiece to be polished, the ultraviolet light of the first wavelength is used to stimulate the development of one of the fluorescent dyes, and the camera is used to collect the first polishing index under the action of the first wavelength ultraviolet light; thereafter, the dual-emission ultraviolet laser pulser emits ultraviolet light of a second wavelength to the interface position of the transparent workpiece to be polished, the ultraviolet light of the second wavelength is used to stimulate the development of another fluorescent dye, and the camera is used to collect the first polishing index under the action of the second wavelength ultraviolet light.
4. The method for visualizing the flow trajectory of the polishing liquid according to claim 1, It is characterized in that In step S200, the first polishing index includes the flow speed and flow direction of the polishing liquid, the recirculation behavior of the old polishing liquid, and the circulation behavior of the new and old polishing liquids.
5. The method for visualizing the flow trajectory of the polishing liquid according to claim 4, It is characterized in that In step S200, the second polishing index includes the moving speed of the developer particles and the retention phenomenon of the developer particles.
6. The method for visualizing the flow trajectory of the polishing liquid according to claim 1, It is characterized in that In step S400, the interface contact state includes a boundary lubrication state, a mixed lubrication state and a hydrodynamic lubrication state.
7. The method for visualizing the flow trajectory of the polishing liquid according to claim 6, It is characterized in that The moving speed of the developer particles in the boundary lubrication state is less than the moving speed of the developer particles in the mixed lubrication state and less than the moving speed of the developer particles in the hydrodynamic lubrication state.
8. The method for visualizing the flow trajectory of the polishing liquid according to claim 6, It is characterized in that The thickness of the liquid film in the boundary lubrication state is less than the thickness of the liquid film in the mixed lubrication state and less than the thickness of the liquid film in the hydrodynamic lubrication state.
9. Polishing liquid flow trajectory visualization device, It is characterized in that The invention comprises a polishing pad, a polishing liquid dispenser, a transparent workpiece to be polished, a dual-emitting ultraviolet laser pulser and a camera. The transparent workpiece to be polished is connected to the rotating main shaft of the polishing device through a telescopic rod. The dual-emitting ultraviolet laser pulser and the camera are respectively mounted above the transparent workpiece to be polished. The emitting end of the dual-emitting ultraviolet laser pulser is arranged toward the transparent workpiece to be polished and is used to emit ultraviolet rays to the transparent workpiece to be polished. The camera is arranged toward the transparent workpiece to be polished and is used to collect a first polishing index and a second polishing index of an interface position of the transparent workpiece to be polished.
10. The polishing liquid flow trajectory visualization device according to claim 9, It is characterized in that The upper end of the telescopic rod is connected to the rotating main shaft through a reverse flange, and the lower end of the telescopic rod is connected to the transparent piece to be polished through a connecting piece. The transparent piece to be polished is an acrylic material component, and the light transmittance of the transparent piece to be polished is greater than 92%.
Citation Information
Patent Citations
A method for measuring wafer liquid film middle variant in CMP process
CN101266915A
Measuring apparatus of wafer lower fluid film intermediate variable in CMP process
CN101275825A
Laboratory table for real-timely observing nanoparticle movement
CN102346125A
Polishing liquid with luminous abrasive particles, and fluid mechanics research system and method
CN103497687A
Loose abrasive particle track detection method
CN107685288A
Cited By
Wafer monitoring method for chemical mechanical polishing, CMP equipment and computer storage medium
CN120038664A