Transparent mobile phone protection shell forming processing technology
Through adaptively adjusted CNC laser cutting and molding process, combined with multi-wavelength UV curing technology, the problem of low glue solidification efficiency is solved, and high-quality and diversified transparent mobile phone protective case molding is achieved, meeting market demand.
Patent Information
- Application Number
- CN202411115544.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-14
- Publication Date
- 2024-11-08
- Estimated Expiration
- Not applicable · inactive patent
Smart Images

Figure CN118906489A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of mobile phone accessory manufacturing, in particular to a transparent mobile phone protective shell forming process. Background Art
[0002] With the rapid development of the smartphone market, the demand for mobile phone cases is increasing. Mobile phone cases not only need to provide physical protection to prevent the phone from being damaged in a fall or collision, but also need to have a certain aesthetic appeal to meet consumers' pursuit of personalization and beauty. Therefore, the molding and processing technology of mobile phone cases has become the focus of attention in the industry.
[0003] Existing mobile phone protective case manufacturing technologies mainly include injection molding and compression molding. These methods can mass-produce mobile phone protective cases with certain standards, and meet the needs of various mobile phone models through different molds. In terms of material selection, polycarbonate (PC), polyethylene (PE), silicone, etc. are commonly used shell materials. They have certain elasticity and strength, can effectively absorb impact force, and protect mobile phones from damage.
[0004] However, the prior art has significant deficiencies in the operation process, especially in the solidification stage of the glue. In the traditional production process, it usually takes a long time to wait for the glue to solidify naturally after dripping the glue, which not only prolongs the production cycle, but also greatly reduces the efficiency of the entire production process. In addition, the fluidity of the glue before it is completely solidified may cause uneven distribution of the glue, affecting the quality and appearance of the final product. This method that relies on the natural solidification of glue is particularly insufficient when producing high-quality and highly consistent transparent mobile phone protective cases, especially when it is necessary to respond quickly to market changes and customer needs. Summary of the invention
[0005] In view of the deficiencies in the prior art, the present invention provides a transparent mobile phone protective case forming processing technology, which solves the problem that in the traditional process, it usually takes a long time to wait for the glue to solidify naturally after glue dripping, which not only prolongs the production cycle but also greatly reduces the efficiency of the entire production process.
[0006] To achieve the above objectives, the present invention is implemented through the following technical solutions: a transparent mobile phone protective shell forming process, comprising the following steps:
[0007] a) According to the preset mobile phone model size database, a CNC laser cutting machine with adaptive adjustment function is used to accurately cut the PET sheet, where the laser cutting machine automatically adjusts the laser power and cutting speed according to the thickness and material of the sheet;
[0008] b) Using a special AB crystal glue containing heat-sensitive color-changing particles, the glue is evenly dispensed along the contour of the PET sheet through an automatic glue dispensing system;
[0009] c) molding the PET sheet coated with glue under the pressure and temperature of the molding machine, wherein the molding machine is equipped with a temperature and pressure feedback system to adjust the molding conditions in real time to ensure molding quality;
[0010] d) Printing a pattern on the molded protective shell using a UV printer with multi-wavelength selectivity, the printer being able to select the most appropriate UV wavelength for curing according to the color requirements of the pattern;
[0011] e) The printed pattern undergoes a multi-stage UV curing process, gradually curing the ink at different wavelengths to improve the durability and UV resistance of the pattern.
[0012] Preferably, the CNC laser cutting machine with the adaptive adjustment function can automatically adjust the laser power between 100W and 200W and the cutting speed between 150mm / s and 250mm / s according to the real-time feedback of the cutting effect to adapt to PET sheets of different thicknesses and materials.
[0013] Preferably, the temperature and pressure feedback system of the molding machine can adjust the pressure between 4MPa and 6MPa and the temperature between 50°C and 70°C according to real-time data during the molding process to adapt to PET sheets of different thicknesses and materials.
[0014] Preferably, the laser power of the CNC laser cutting machine is set to 150W and the cutting speed is set to 200mm / s to ensure that the PET sheet does not produce thermal deformation during the cutting process.
[0015] Preferably, the mixing process of the AB crystal glue and the glitter agent is carried out in an environment where the temperature is controlled at 25° C., and a high-speed shear force agitator is used to stir at a speed of 5000 rpm for 10 minutes to ensure that the glitter is completely and evenly dispersed.
[0016] Preferably, the diameter of the glue dropper of the automatic glue dropper is 0.5 mm, the glue drop spacing is 1 mm, the glue is dropped evenly along the contour of the PET sheet, and the glue drop amount per square centimeter is controlled at 0.05 ml.
[0017] Preferably, the holding time set by the molding machine during the molding process is 30 seconds to ensure that the glue is completely cured and forms the basic outline of the protective shell.
[0018] Preferably, the printing resolution of the UV printer is set to 1440dpi, and CMYK four-color ink is used to ensure the color accuracy and vividness of the pattern.
[0019] Preferably, after UV printing, a UV light source with a wavelength of 395 nm is used for irradiation for 30 seconds to ensure rapid curing of the printed ink and enhance the wear resistance and light resistance of the pattern.
[0020] Preferably, the step e) further includes plasma cleaning the molded protective shell before the UV printing step to improve the adhesion of the UV ink and the durability of the pattern, the plasma generator of the plasma cleaning treatment has an operating power of 200 W and a processing time of 60 seconds to ensure the cleanliness and activity of the surface of the protective shell.
[0021] The present invention provides a transparent mobile phone protective shell forming process, which has the following beneficial effects:
[0022] 1. The present invention provides two synthesis methods, namely, molding synthesis by a molding machine and manual pressing. This dual synthesis process improves the flexibility of production, so that high-quality transparent mobile phone protective shell molding can be achieved under different production conditions, meeting diverse market demands.
[0023] 2. The present invention uses an automatic glue dripping system to evenly drip glue along the contour of the PET sheet, ensuring the uniform distribution and bonding effect of the glue, which not only improves the structural strength of the protective shell, but also enhances the visual effect. The molding machine equipped with a temperature and pressure feedback system can monitor and adjust the pressure and temperature during the molding process in real time to ensure that the protective shell after molding is free of bubbles and defects, ensuring the molding accuracy and consistency of each protective shell, reducing the defective rate, and significantly improving the overall quality of the product. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 The present invention is a flow chart of the method. DETAILED DESCRIPTION
[0025] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0026] Embodiment 1:
[0027] Please refer to the attached Figure 1 The embodiment of the present invention provides a transparent mobile phone protective shell forming process, comprising the following steps:
[0028] a) According to the preset mobile phone model size database, a CNC laser cutting machine with adaptive adjustment function is used to accurately cut the PET sheet, where the laser cutting machine automatically adjusts the laser power and cutting speed according to the thickness and material of the sheet;
[0029] b) Using a special AB crystal glue containing heat-sensitive color-changing particles, the glue is evenly dispensed along the contour of the PET sheet through an automatic glue dispensing system;
[0030] c) molding the PET sheet coated with glue under the pressure and temperature of the molding machine, wherein the molding machine is equipped with a temperature and pressure feedback system to adjust the molding conditions in real time to ensure molding quality;
[0031] d) Printing a pattern on the molded protective shell using a UV printer with multi-wavelength selectivity, the printer being able to select the most appropriate UV wavelength for curing according to the color requirements of the pattern;
[0032] e) The printed pattern is subjected to a multi-stage UV curing process, which gradually cures the ink at different wavelengths to improve the durability and UV resistance of the pattern.
[0033] In one embodiment, material preparation and cutting
[0034] Step a: According to the preset mobile phone model size database, a CNC laser cutting machine with an adaptive adjustment function is used to accurately cut the PET sheet, wherein the laser cutting machine automatically adjusts the laser power and cutting speed according to the sheet thickness and material.
[0035] In a specific embodiment, a database containing the sizes of various mobile phone models is first established, and the specific size and shape of each model are recorded in the database. The CNC laser cutting machine is connected to the database, and the laser cutting parameters are automatically set by reading the size data in the database. The laser power can be automatically adjusted between 100W and 200W, and the cutting speed is between 150mm / s and 250mm / s. The real-time feedback system monitors the cutting effect and adjusts the laser power and speed in time to ensure that the PET sheet does not produce thermal deformation during the cutting process.
[0036] Through this adaptive adjustment function, PET sheets of different thicknesses and materials can be accurately cut, improving production consistency and efficiency while reducing material waste.
[0037] Glue treatment:
[0038] Step b: Use special AB crystal glue containing heat-sensitive color-changing particles to evenly dispense glue along the contour of the PET sheet through an automatic glue-drip system.
[0039] In a specific embodiment, AB crystal glue and glitter agent are mixed in a ratio of 10:1. In an environment of 25°C, a high-speed shear force agitator is used to stir at a speed of 5000rpm for 10 minutes to ensure that the glitter is completely and evenly dispersed. The automatic glue dispensing system includes a precisely controlled glue dispensing head with a diameter of 0.5mm, a glue dispensing spacing of 1mm, and a glue dispensing amount per square centimeter controlled at 0.05ml. The automatic glue dispensing machine uniformly dispenses glue along the edges and important positions of the PET sheet through a precise control system.
[0040] Through this uniform glue dripping process, the glue can be evenly distributed on the PET sheet, which not only improves the bonding effect of the glue, but also realizes the change of visual effect through heat-sensitive color-changing particles, enhancing the aesthetics and recognition of the product.
[0041] Compression Molding
[0042] Step c: The PET sheet coated with glue is molded under the pressure and temperature of the molding machine. The molding machine is equipped with a temperature and pressure feedback system to adjust the molding conditions in real time to ensure molding quality.
[0043] In a specific embodiment, a PET sheet coated with glue is placed in a molding machine. The pressure of the molding machine is set between 4MPa and 6MPa, the temperature is set between 50°C and 70°C, and the holding time is 30 seconds. The feedback system of the molding machine monitors the pressure and temperature in real time, obtains real-time data during the molding process through sensors, and automatically adjusts the pressure and temperature parameters to ensure that the protective shell after molding is free of bubbles and defects.
[0044] During the molding process, real-time adjustment of temperature and pressure ensures the molding accuracy of each protective case and reduces the defective rate. This process complements the aforementioned glue dripping process to ensure the quality and consistency of the final product.
[0045] UV printing
[0046] Step d: Use a UV printer with multi-wavelength selectivity to print a pattern on the molded protective shell. The printer can select the most suitable UV wavelength for curing according to the color requirements of the pattern.
[0047] In a specific embodiment, software is used for pattern design to ensure design accuracy. The printing resolution of the UV printer is set to 1440dpi, and CMYK four-color ink is used. During the printing process, the UV printer selects the most suitable UV wavelength for curing according to the color requirements of the pattern to ensure that the color of the pattern is bright and durable.
[0048] High-resolution UV printing and multi-wavelength selective curing technology ensure the color accuracy and durability of the pattern, while improving the aesthetic effect of the pattern. This step is closely related to the aforementioned compression molding, ensuring the unity of the protective case in terms of beauty and functionality.
[0049] UV curing
[0050] Step e: The printed pattern is subjected to a multi-stage UV curing treatment to gradually cure the ink at different wavelengths, thereby improving the durability and UV resistance of the pattern.
[0051] In a specific embodiment, after UV printing is completed, a UV light source with a wavelength of 395 nm is used for irradiation for 30 seconds to ensure rapid curing of the printed ink. Then, UV light sources with different wavelengths are gradually used for multi-stage curing, and the curing time and wavelength of each stage are adjusted according to the characteristics of the ink and the complexity of the pattern to ensure that the ink is completely cured and improve the wear resistance and UV resistance of the pattern.
[0052] The multi-stage UV curing process enhances the pattern's UV resistance and abrasion resistance, ensuring the case's aesthetics and functionality over long-term use. This step, combined with the aforementioned UV printing, further improves the quality of the pattern.
[0053] The CNC laser cutting machine with adaptive adjustment function can automatically adjust the laser power between 100W and 200W and the cutting speed between 150mm / s and 250mm / s according to the real-time feedback of the cutting effect to adapt to PET sheets of different thicknesses and materials.
[0054] The temperature and pressure feedback system of the molding machine can adjust the pressure between 4MPa and 6MPa and the temperature between 50℃ and 70℃ according to the real-time data during the molding process to adapt to PET sheets of different thicknesses and materials.
[0055] The laser power of the CNC laser cutting machine was set to 150 W and the cutting speed to 200 mm / s to ensure that the PET sheet did not produce thermal deformation during the cutting process.
[0056] The mixing process of AB crystal glue and glitter agent was carried out in an environment with a temperature controlled at 25°C, and a high-speed shear force agitator was used to stir at a speed of 5000rpm for 10 minutes to ensure that the glitter was completely and evenly dispersed.
[0057] The glue dropper head diameter of the automatic glue dropper is 0.5mm, the glue drop spacing is 1mm, and the glue is dropped evenly along the contour of the PET sheet. The glue drop amount per square centimeter is controlled at 0.05ml.
[0058] The molding machine is set to hold for 30 seconds during the molding process to ensure that the glue is fully cured and forms the basic outline of the protective shell.
[0059] The printing resolution of the UV printer is set to 1440dpi, using CMYK four-color inks to ensure the color accuracy and vividness of the pattern.
[0060] After UV printing, a UV light source with a wavelength of 395nm is used to irradiate for 30 seconds to ensure the rapid curing of the printed ink and enhance the wear resistance and light resistance of the pattern.
[0061] e) further comprising plasma cleaning the molded protective shell before the UV printing step to improve the adhesion of the UV ink and the durability of the pattern, the plasma generator of the plasma cleaning treatment has an operating power of 200W and a processing time of 60 seconds to ensure the cleanliness and activity of the surface of the protective shell.
[0062] In a preferred embodiment:
[0063] Manual synthesis
[0064] Step f: Manually press the prepared sheet to the phone case to ensure a firm and smooth bond.
[0065] In a specific embodiment:
[0066] Cleaning: Before manual lamination, first clean the surface of the PET sheet and the phone case. Use a dust-free cloth and industrial-grade alcohol to wipe to ensure that there is no dust, grease or other impurities on the surface to ensure the bonding effect.
[0067] Alignment and positioning: Align the glued PET sheet with the phone case precisely. Use a dedicated alignment tool or jig to ensure there is no misalignment between the sheet and the phone case. During the alignment process, carefully check each corner to ensure a perfect fit.
[0068] Manual pressing: Use a manual pressing tool to press the aligned PET sheet and the phone case. The manual pressing tool can be a press with a flexible gasket, which applies uniform and appropriate pressure to make the sheet fit tightly with the phone case. During the pressing process, ensure that each part is subjected to uniform pressure to avoid bubbles and unevenness.
[0069] Auxiliary heating: During the lamination process, a hot air gun (hair dryer) can be used for auxiliary heating in low temperature mode, with the temperature controlled between 40°C and 50°C. The heating time is adjusted according to the characteristics of the glue, generally 30 seconds to 1 minute. Auxiliary heating can accelerate the curing of the glue and improve the bonding strength. This step is taken into account for the overall stability. In normal operation, the installation can be completed by manually pressing the sheet and the mobile phone.
[0070] Cooling and curing: After lamination, place the phone case in a room temperature environment for natural cooling for 5 to 10 minutes. This process ensures that the glue is fully cured and the bond is strong.
[0071] Contextual logic: Cleaning, alignment, pressing and auxiliary heating during the manual synthesis process ensure the perfect combination of the sheet and the phone case. The precise control of manual pressing complements the aforementioned automated glue dispensing and molding processes, further improving the quality and consistency of the final product.
[0072] Comparative Example 1:
[0073] Traditional mobile phone case adhesive method
[0074] Process flow:
[0075] Glue preparation: Prepare single-component glue according to the formula, usually including silicone, PU glue or other high-viscosity materials.
[0076] Glue dripping: Use a manual glue gun or a semi-automatic glue machine to drip liquid glue directly onto the designated position of the phone case, usually around the back and the middle part.
[0077] Dry naturally: Place the glued phone case in a well-ventilated place and let it dry naturally. It usually takes 24 hours or more to ensure that the glue is completely cured.
[0078] Glue Type:
[0079] One-component glue: Usually one-component liquid glue is used, such as silicone, PU glue, etc. These glues are easy to use, but the curing time is long, and bubbles may be generated during the curing process, affecting the bonding effect.
[0080] Drying time:
[0081] Glue takes a long time to dry, usually 24 hours or longer. This process depends on the ambient temperature and humidity. Higher temperatures and lower humidity can speed up the drying process, but it still takes several hours to more than a day.
[0082] Uneven distribution of glue may result in a weak bond, with bubbles or insufficient glue in some areas.
[0083] Bonding effect: After the glue solidifies, the bonding effect is relatively good, but after long-term use, the glue may age and lose its stickiness, affecting the service life of the mobile phone case.
[0084] Performance Indicators Embodiment 1 Comparative Example 1 Accuracy ±0.1mm ±1mm Curing time Can be installed quickly Need to wait for the glue to solidify Glue uniformity Even distribution without bubbles Uneven, often with bubbles
[0085] Table 1
[0086] The embodiment of the present invention greatly improves the cutting accuracy and reduces the error by using a CNC laser cutting machine with an adaptive adjustment function. This is especially important for the high-end mobile phone case market. Consumers have extremely high requirements for accuracy. The automatic glue dripping system ensures the uniform distribution of glue, avoids the common problems of bubbles and unevenness in traditional methods, and improves the overall appearance and texture of the product. Combining the above indicators, the mobile phone case provided by the embodiment of the present invention has significantly improved its competitiveness in the market, meeting the stringent requirements of high-end consumers for product quality.
[0087] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A transparent mobile phone protective shell forming process, It is characterized in that The following steps are involved: a) According to the preset mobile phone model size database, a CNC laser cutting machine with adaptive adjustment function is used to accurately cut the PET sheet, where the laser cutting machine automatically adjusts the laser power and cutting speed according to the thickness and material of the sheet; b) Using a special AB crystal glue containing heat-sensitive color-changing particles, the glue is evenly dispensed along the contour of the PET sheet through an automatic glue dispensing system; c) molding the PET sheet coated with glue under the pressure and temperature of the molding machine, wherein the molding machine is equipped with a temperature and pressure feedback system to adjust the molding conditions in real time to ensure molding quality; d) Printing a pattern on the molded protective shell using a UV printer with multi-wavelength selectivity, the printer being able to select the most appropriate UV wavelength for curing according to the color requirements of the pattern; e) The printed pattern is subjected to a multi-stage UV curing process, which gradually cures the ink at different wavelengths to improve the durability and UV resistance of the pattern.
2. A transparent mobile phone protective shell forming process according to claim 1, It is characterized in that The CNC laser cutting machine with the adaptive adjustment function can automatically adjust the laser power between 100W and 200W and the cutting speed between 150mm / s and 250mm / s according to the real-time feedback of the cutting effect to adapt to PET sheets of different thicknesses and materials.
3. A transparent mobile phone protective shell forming process according to claim 1, It is characterized in that The temperature and pressure feedback system of the molding machine can adjust the pressure between 4MPa and 6MPa and the temperature between 50°C and 70°C according to real-time data during the molding process to adapt to PET sheets of different thicknesses and materials.
4. A transparent mobile phone protective shell forming process according to claim 1, It is characterized in that The laser power of the CNC laser cutting machine was set to 150 W and the cutting speed was set to 200 mm / s to ensure that the PET sheet did not produce thermal deformation during the cutting process.
5. A transparent mobile phone protective shell forming process according to claim 1, It is characterized in that The mixing process of the AB crystal glue and the glitter agent is carried out in an environment where the temperature is controlled at 25° C., and a high-speed shear force agitator is used to stir at a speed of 5000 rpm for 10 minutes to ensure that the glitter is completely and evenly dispersed.
6. A transparent mobile phone protective shell forming process according to claim 1, It is characterized in that The glue dropper of the automatic glue dropper has a diameter of 0.5 mm, a glue dropper spacing of 1 mm, and glue is dropped evenly along the contour of the PET sheet, and the glue dropper volume per square centimeter is controlled at 0.05 ml.
7. A transparent mobile phone protective shell forming process according to claim 1, It is characterized in that The holding time set by the molding machine during the molding process is 30 seconds to ensure that the glue is completely cured and forms the basic outline of the protective shell.
8. A transparent mobile phone protective shell forming process according to claim 1, It is characterized in that The printing resolution of the UV printer is set to 1440dpi, and CMYK four-color ink is used to ensure the color accuracy and vividness of the pattern.
9. A transparent mobile phone protective shell forming process according to claim 1, It is characterized in that After UV printing, a UV light source with a wavelength of 395 nm is used for irradiation for 30 seconds to ensure rapid curing of the printed ink and enhance the wear resistance and light resistance of the pattern.
10. A transparent mobile phone protective shell forming process according to claim 1, It is characterized in that The step e) further includes performing a plasma cleaning treatment on the molded protective shell before the UV printing step to improve the adhesion of the UV ink and the durability of the pattern, wherein the plasma generator of the plasma cleaning treatment has an operating power of 200 W and a processing time of 60 seconds to ensure the cleanliness and activity of the surface of the protective shell.