Preparation method and application of phosphogypsum leachate fluorine removal agent

By using the fluorine-depleting agent generated by the reaction of phosphogypsum and ammonium carbonate in the phosphogypsum leachate, combined with cerium sulfate and exciter, the problems of efficient fluorine removal and phosphorus recycling in the phosphogypsum leachate are solved, and the phosphorus loss rate is reduced and fluorosilicate scaling, achieving efficient fluorine removal effect.

CN118908390AActive Publication Date: 2024-11-08YIDU XINGFA CHEMICAL CO LTD

Patent Information

Application Number
CN202410860763.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-28
Publication Date
2024-11-08
Estimated Expiration
2044-06-28

AI Technical Summary

Technical Problem

High concentrations of fluorine, silicon, potassium and sodium elements in phosphogypsum leachate lead to scaling of potassium fluorosilicate and sodium fluorosilicate. The prior art uses calcium precipitation alone to remove fluorine under acidic conditions and has a high phosphorus loss rate. It is difficult to achieve effective recycling and utilization of resources.

Method used

The reaction of phosphogypsum and ammonium carbonate is used to form calcium carbonate residue, and mix it with phosphorus tailings, cerium sulfate and pH regulator and wet grind it. The exciter and propyl methacrylate 3-sulfonate are added to prepare fluorine removal agent. Combined with flocculant, the sedimentation treatment is carried out to reduce the fluorine content and recover the phosphorus element.

Benefits of technology

It realizes the efficient fluorine removal performance of fluorine remover, low phosphorus loss rate, slows down fluorosilicate scaling in the membrane system, improves the phosphorus recycling rate, and reduces the amount of sludge.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a preparation method and application of an ardealite leachate fluorine removal agent, and belongs to the technical field of wastewater treatment. The fluorine removal agent is prepared by the following steps: reacting phosphogypsum with ammonium carbonate to obtain calcium carbonate residues, mixing the calcium carbonate residues, phosphate tailings, cerous sulfate and a pH regulator, carrying out wet grinding, filtering, adding an exciting agent and 3-sulfonic acid propyl potassium methacrylate into filter residues, and calcining to obtain the fluorine removal agent. The defluorinating agent is used for defluorinating the phosphogypsum leachate. The fluorine removal agent disclosed by the invention is low in silicon and fluorine dissolution rate, stable in structure, more in surface pores, more in adsorption sites and capable of effectively removing fluorine ions in the ardealite leachate, the phosphorus loss rate in the ardealite leachate is low, the sludge amount is small, and the effect of relieving fluosilicate scaling of a membrane treatment system is remarkable.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of wastewater treatment, and in particular to a preparation method and application of a phosphogypsum leachate defluorinating agent. Background Art

[0002] Phosphogypsum leachate is acidic wastewater containing pollutants such as phosphorus and fluorine generated during the storage of phosphogypsum. This type of wastewater has a low pH value and complex composition. Once it seeps into the ground or into surrounding waters, it will pollute groundwater and surface water, destroy the water ecological balance, and even threaten the drinking water safety of surrounding residents. Therefore, phosphogypsum leachate needs to be treated.

[0003] At present, the treatment of phosphogypsum leachate is mainly carried out by low-cost calcium salt precipitation method. This method requires the leachate to be adjusted to a higher pH value, and phosphorus and fluorine are precipitated in the form of calcium salts. A large amount of sludge will be generated during the precipitation process. This method not only causes a waste of phosphorus and fluorine resources, but also the disposal of fluorine-containing sludge is a problem. Membrane separation technology can avoid the generation of a large amount of sludge. At the same time, clean water can be used as production water, and concentrated water can be reused in phosphoric acid production, realizing the recycling of phosphorus and fluorine resources. However, due to the high concentration of fluorine, silicon, potassium, and sodium elements in the phosphogypsum leachate, potassium fluorosilicate and sodium fluorosilicate scale are easily formed at low temperatures. Potassium fluorosilicate and sodium fluorosilicate adhere to the concentrated water pipeline and the surface of the reverse osmosis membrane, making the reverse osmosis membrane frequently cleaned and the operating efficiency low. In order to solve the problem of potassium fluorosilicate and sodium fluorosilicate scaling, the use of special antiscalants to inhibit fluorosilicate scaling has a certain effect, but in actual operation, the water quality of phosphogypsum leachate fluctuates greatly, and the problem of fluorosilicate scaling is still serious.

[0004] At present, the problem of fluorosilicate scaling can be solved by coagulation and precipitation, but this method requires the leachate to be adjusted to alkalinity to effectively reduce the fluorine and silicon content. Commonly used defluorinators and desiliconizers need to be used under alkaline conditions. After the leachate is adjusted to alkalinity using caustic soda, a large amount of flocculent sludge will be produced, and mud and water separation is difficult. Lime treatment is used, and the removal of a small amount of fluoride ions is limited. Adding too much will cause the loss of phosphorus. In addition, limestone mining is restricted. Industrial high-calcium solid waste is used as a substitute for limestone, which can not only be used for defluorination and desiliconization, but also realize the resource utilization of industrial solid waste. Phosphorus tailings have been used as wastewater defluorinating agents as high-calcium industrial solid wastes. For example, in patent CN202310829549.0, calcined high-magnesium phosphorus tailings are used as defluorinating agents to effectively reduce the fluorine content in wastewater. However, the patent does not take into account that high-magnesium phosphorus tailings originally contain fluorine and silicon. If dissolved during use, it is unfavorable for the operation of the membrane system. There are originally a large amount of fluorine and silicon in phosphogypsum, and the use of phosphogypsum as a calcium source may also introduce harmful elements. When using phosphogypsum and phosphate tailings industrial solid waste to prepare defluoridation agents, the fixation of harmful elements in the defluoridation agents is a problem to be solved. In addition, under acidic conditions, the efficiency of removing fluoride using calcium precipitation alone is low, and it is also necessary to add additives to improve the defluoridation effect of calcium salts.

[0005] Therefore, there is an urgent need for an effective treatment method that can solidify the harmful components in phosphogypsum and phosphate tailings, reduce the leaching of harmful components, and at the same time improve the defluorination effect of the calcined products, reduce the fluorine content in the phosphogypsum leachate while reducing phosphorus loss, and slow down the fluorosilicate scaling of the membrane system. Summary of the invention

[0006] The purpose of the present invention is to provide a preparation method and application of a defluorinating agent for phosphogypsum leachate. The defluorinating agent has a low harmful substance dissolution rate and a high defluorination rate. When used for defluorination of phosphogypsum leachate, the phosphorus loss rate is low, and the effective removal of fluorine in the phosphogypsum leachate and the recovery and utilization of phosphorus can be achieved. In addition, the sludge settling performance is good and the sludge amount is small. The defluorinated phosphogypsum leachate wastewater entering the membrane system can effectively alleviate the fluorosilicate fouling problem.

[0007] In order to achieve the purpose of the invention, the present invention adopts the following technical solutions: A method for preparing a defluorinating agent, the method comprising the following steps: (1) reacting phosphogypsum and ammonium carbonate to obtain calcium carbonate slag and ammonium sulfate filtrate; (2) The calcium carbonate slag, phosphate tailings, cerium sulfate and pH adjuster obtained in step (1) are mixed and then wet-milled. After filtering, an activator and potassium 3-sulfonate propyl methacrylate are added to the residue, mixed evenly and then calcined to obtain a defluorinating agent. The filtrate is recycled as water for wet milling. Preferably, in step (1), the amount of ammonium carbonate used is 105% to 110% of the theoretical amount (theoretically, the molar ratio of calcium sulfate and ammonium carbonate in phosphogypsum is 1:1), the pH of the solution is adjusted to 8 to 9 with aqueous ammonia, the solid-liquid ratio of phosphogypsum and water is (1 to 1.1):1 (ammonium carbonate is dissolved by adding water, and ammonium carbonate reacts with calcium sulfate in phosphogypsum), the reaction temperature is 60 to 70°C, and the reaction time is 2.5 to 3 hours.

[0008] Preferably, in step (2), calcium carbonate slag and phosphorus tailings slag are mixed in a ratio of (0.5-1.5): (0.5-1.5), the amount of cerium sulfate added is 1%~5%, and the solid-liquid ratio of the mixture of wet-ground calcium carbonate slag and phosphorus tailings slag to water is (1~1.1):1.

[0009] Preferably, in step (2), the pH adjuster is one or more of sodium hydroxide, potassium hydroxide and ammonia water, and the amount of the pH adjuster added is 1% to 2%, ensuring that the pH value of the wet grinding slurry is greater than 7.

[0010] Preferably, in step (2), the activator is one or more of NaCl, K2SO4 and Na2CO3, and the amount used is 1% to 5%, and the amount of 3-sulfonate propyl methacrylate potassium added is 2% to 10%.

[0011] Preferably, in step (2), the calcination temperature is 900-1000° C. for 1.5-2.5 h.

[0012] A method for treating phosphogypsum leachate, the method adopts the defluorinating agent obtained by the preparation method.

[0013] Preferably, the method comprises the following steps: S1 adds the defluoridation agent into the phosphogypsum leachate; S2: After the reaction in step S1 is completed, a flocculant is added for sedimentation treatment to obtain a defluorinated pretreated phosphogypsum leachate; S3 introduces the defluorination pretreated phosphogypsum leachate obtained in step S2 into a membrane treatment system to complete the treatment of the phosphogypsum leachate.

[0014] More preferably, in step S1, the dosage of the defluorinating agent is 2-6 g / L, and the added amount is adjusted according to the fluorine content in the leachate and the pH of the leachate, and the pH value of the leachate after addition is controlled to be 3.5-4.5, and stirred for 0.5-1.5 hours.

[0015] More preferably, in step S1, the flocculant is polyacrylamide, the dosage of the flocculant is 2-6 mg / L, and the flocculation sedimentation time is 25-35 min.

[0016] Compared with the prior art, the present invention has the following beneficial effects: (1) The raw materials of the defluorination agent of the present invention are cheap and easily available, the preparation process is simple, the method of use is simple, and it is convenient for industrial production. The two solid wastes are effectively utilized to prepare the defluorination agent, thus realizing the resource utilization of solid wastes.

[0017] (2) The present invention adds cerium sulfate, which will generate cerium oxide after high-temperature calcination and distribute on the surface of the calcined product. Cerium oxide has good fluorine adsorption performance, so that the defluorination agent has both chemical precipitation and adsorption defluorination effects.

[0018] (3) Potassium 3-sulfonate propyl methacrylate chelates cerium and together with the activator promotes the formation of a eutectic between fluoride and silicate. The structure of the eutectic is stable, which reduces the dissolution rate of fluorine and silicon in the defluoridation agent.

[0019] (4) The activator and potassium 3-sulfonate propyl methacrylate can promote the formation of porous calcium oxide after calcination of phosphate tailings and calcium carbonate. In addition, potassium 3-sulfonate propyl methacrylate produces methane and hydroxyl radicals after high-temperature decomposition, which is conducive to the high-temperature self-crosslinking of calcium oxide, making the prepared defluorination agent more porous and more stable in structure, providing more adsorption sites for fluorine absorption. DETAILED DESCRIPTION

[0020] The following will be combined with the specific embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0021] Example 1 Treatment of phosphogypsum leachate wastewater: Water quality of phosphogypsum leachate: TP 5823ppm, CaO 1081ppm, Al2O3343ppm, Fe2O399.3ppm, F 640ppm, Si159ppm, pH 2.3.

[0022] (1) reacting phosphogypsum and ammonium carbonate to obtain calcium carbonate slag and ammonium sulfate filtrate, wherein the amount of ammonium carbonate used is 105% of the theoretical amount, the pH of the solution is adjusted to 8 with ammonia water, the solid-liquid ratio is 1:1, the reaction temperature is 60°C, and the reaction time is 2.5 h; (2) The calcium carbonate slag, phosphate tailings, cerium sulfate and pH adjuster obtained in step (1) are mixed, and then wet-milled at a liquid-to-solid ratio of 1:1. After filtering, an activator and 3-sulfonate propyl potassium methacrylate are added to the filter residue, mixed evenly, and calcined at 900° C. for 2 h to obtain a defluorinating agent, wherein the amount of cerium sulfate added is 1%, the pH adjuster is sodium hydroxide, the amount is 1%, the pH of the wet-milling slurry is 8, the activator is NaCl, the amount is 1%, and the amount of 3-sulfonate propyl potassium methacrylate added is 2%; (3) adding the defluorinating agent obtained in step (2) to the phosphogypsum leachate and stirring for 1 hour. The amount of defluorinating agent used is 4 g / L. The pH value of the leachate after the reaction is 4.1. (4) After the reaction in step (3) is completed, polyacrylamide is added for sedimentation treatment in an amount of 2 mg / L to obtain a defluorinated pretreated phosphogypsum leachate; (5) Introducing the defluorination pretreated phosphogypsum leachate obtained in step (4) into a membrane treatment system.

[0023] The defluorination pretreated phosphogypsum leachate obtained by this method has TP 4933ppm, CaO 1624ppm, Al2O35.5ppm, Fe2O33.5ppm, F 15.3ppm, Si 150ppm, fluorine removal rate reaches 97.6%, and phosphorus loss rate is 15.5%.

[0024] Example 2 Treatment of phosphogypsum leachate wastewater: Water quality of phosphogypsum leachate: TP 5823ppm, CaO 1081ppm, Al2O3343ppm, Fe2O399.3ppm, F 640ppm, Si 159ppm, pH 2.3.

[0025] The operation steps are the same as those in Example 1, except that in step (1), the amount of ammonium carbonate used is 110% of the theoretical amount, the pH of the solution is adjusted to 9 with ammonia water, the solid-liquid ratio is 1.1:1, the reaction temperature is 70°C, and the reaction time is 3 h; in step (2), the reaction calcination temperature is 1000°C, the amount of cerium sulfate added is 1%, the pH adjuster is sodium hydroxide, the amount is 1%, the pH of the wet grinding slurry is 8, the activator is K2SO4, the amount is 2%, and the amount of 3-sulfonate propyl methacrylate potassium added is 4%; in step (3), the amount of the defluorinating agent is 3.5 g / L, and the pH of the leachate after the reaction is 4.0; in step (4), the amount of polyacrylamide is 3 mg / L.

[0026] The defluorination pretreated phosphogypsum leachate obtained by this method has TP 5110ppm, CaO 1524ppm, Al2O33.4ppm, Fe2O36.5ppm, F 12.4ppm, Si 151ppm, fluorine removal rate reaches 98.1%, and phosphorus loss rate is 12.2%.

[0027] Example 3 Treatment of phosphogypsum leachate wastewater: Water quality of phosphogypsum leachate: TP 6718ppm, CaO 1843ppm, Al2O3446.8ppm, Fe2O385ppm, F 600ppm, Si 169ppm, pH 2.3.

[0028] The operation steps are the same as those in Example 1. In step (1), the amount of ammonium carbonate used is 108% of the theoretical amount, the solution pH is adjusted to 8 with ammonia water, the solid-liquid ratio is 1:1, the reaction temperature is 65°C, and the reaction time is 3 h. In step (2), the reaction calcination temperature is 950°C, the amount of cerium sulfate added is 3%, the pH adjuster is potassium hydroxide, the amount is 1%, the wet grinding slurry pH is 8, the activator is Na2CO3, the amount is 2%, and the amount of 3-sulfonate propyl methacrylate potassium added is 5%. In step (3), the amount of defluorination agent used is 4.2 g / L, and the pH of the leachate after the reaction is 3.95. In step (4), the amount of polyacrylamide used is 4 mg / L.

[0029] The defluorination pretreated phosphogypsum leachate obtained by this method has TP 5959ppm, CaO 2113ppm, Al2O32.2ppm, Fe2O31.2ppm, F 15.5ppm, Si 159ppm, fluorine removal rate reaches 97.4%, and phosphorus loss rate is 11.3%.

[0030] Example 4 Treatment of phosphogypsum leachate wastewater: Water quality of phosphogypsum leachate: TP 6718ppm, CaO 1843ppm, Al2O3446.8ppm, Fe2O385ppm, F 600ppm, Si 169ppm, pH 2.3.

[0031] The operation steps are the same as those in Example 1, except that in step (1), the amount of ammonium carbonate used is 105% of the theoretical amount, the pH of the solution is adjusted to 8.5 with ammonia water, the solid-liquid ratio is 1.1:1, the reaction temperature is 65°C, and the reaction time is 3 h; in step (2), the calcination temperature is 1000°C, the amount of cerium sulfate added is 4%, the pH adjuster is potassium hydroxide, the amount is 1%, the pH of the wet grinding slurry is 8, the activator is Na2CO3, the amount is 3%, and the amount of 3-sulfonate propyl methacrylate potassium added is 8%; in step (3), the amount of the defluorinating agent used is 3.7 g / L, and the pH of the leachate after the reaction is 4.1; in step (4), the amount of polyacrylamide used is 5 mg / L.

[0032] The defluorination pretreated phosphogypsum leachate obtained by this method has TP 5896ppm, CaO 2132ppm, Al2O33.1ppm, Fe2O30.6ppm, F 13.7ppm, Si 155ppm, fluorine removal rate reaches 97.7%, and phosphorus loss rate is 12.2%.

[0033] Example 5 Water quality of phosphogypsum leachate: TP 6215ppm, CaO 1060ppm, Al2O3430ppm, Fe2O385ppm, F504ppm, Si 161ppm, pH 2.3.

[0034] The operation steps are the same as those in Example 1, except that in step (1), the amount of ammonium carbonate used is 110% of the theoretical amount, the pH of the solution is adjusted to 8.5 with ammonia water, the solid-liquid ratio is 1:1, the reaction temperature is 60°C, and the reaction time is 2.5 h; in step (2), the calcination temperature is 900°C, the amount of cerium sulfate added is 4%, the pH adjuster is ammonia water, the amount is 1.5%, the pH of the wet grinding slurry is 9, the activator is Na2CO3, the amount is 5%, and the amount of 3-sulfonate propyl methacrylate potassium added is 5%; in step (3), the amount of the defluorinating agent is 4.2 g / L, and the pH of the leachate after the reaction is 4.3; in step (4), the amount of polyacrylamide used is 6 mg / L.

[0035] The defluorination pretreated phosphogypsum leachate obtained by this method has TP 5112ppm, CaO 1624ppm, Al2O30.8ppm, Fe2O30.1ppm, F 9.8ppm, Si 150ppm, fluorine removal rate reaches 98.1%, and phosphorus loss rate is 17.7%.

[0036] Example 6 Water quality of phosphogypsum leachate: TP 6215ppm, CaO 1060ppm, Al2O3430ppm, Fe2O385ppm, F504ppm, Si 161ppm, pH 2.3.

[0037] The operation steps are the same as those in Example 1, except that in step (1), the amount of ammonium carbonate used is 105% of the theoretical amount, the pH of the solution is adjusted to 9 with ammonia water, the solid-liquid ratio is 1.1:1, the reaction temperature is 70°C, and the reaction time is 3 h; in step (2), the calcination temperature is 1000°C, the amount of cerium sulfate added is 3%, the pH adjuster is ammonia water, the amount is 1.5%, the pH of the wet grinding slurry is 9, the activator is NaCl, the amount is 3%, and the amount of 3-sulfonate propyl methacrylate potassium added is 6%; in step (3), the amount of the defluorinating agent used is 4 g / L, and the pH of the leachate after the reaction is 4.05; in step (4), the amount of polyacrylamide used is 3 mg / L.

[0038] The defluorination pretreated phosphogypsum leachate obtained by this method has TP 5212ppm, CaO 1576ppm, Al2O31.2ppm, Fe2O31.1ppm, F 10.5ppm, Si 148ppm, fluorine removal rate reaches 97.9%, and phosphorus loss rate is 16.1%.

[0039] Comparative Example 1 Treatment of phosphogypsum leachate wastewater: Water quality of phosphogypsum leachate: TP 5823ppm, CaO 1081ppm, Al2O3343ppm, Fe2O399.3ppm, F640ppm, Si 159ppm, pH 2.3.

[0040] The operation steps are the same as those in Example 1, except that cerium sulfate is not added in step (2).

[0041] The defluorination pretreated phosphogypsum leachate obtained by this method has TP 5033ppm, CaO 1724ppm, Al2O310.6ppm, Fe2O38.9ppm, Si 158ppm, F 40.8ppm, fluorine removal rate reaches 93.6%, and phosphorus loss rate is 13.6%.

[0042] Comparative Example 2 Treatment of phosphogypsum leachate wastewater: Water quality of phosphogypsum leachate: TP 6718ppm, CaO 1843ppm, Al2O3446.8ppm, Fe2O385ppm, F600ppm, Si 169ppm, pH 2.3.

[0043] (1) Phosphogypsum, phosphate tailings, pH adjuster and cerium sulfate were mixed evenly and wet-ground at a liquid-solid ratio of 1:1. After filtering, an activator and potassium 3-sulfonate propyl methacrylate were added to the filter residue and mixed evenly, and then calcined at 950°C for 2h. The amount of cerium sulfate added was 3%, the pH adjuster was potassium hydroxide, the amount was 1%, the pH of the wet-ground slurry was 8, the activator was Na2CO3, the amount was 2%, and the amount of potassium 3-sulfonate propyl methacrylate added was 5%; (2) adding the defluorinating agent obtained in step (1) to the phosphogypsum leachate and stirring for 1 hour. The amount of defluorinating agent used is 4.2 g / L. The pH value of the leachate after the reaction is 3.4. (3) After the reaction in step (2) is completed, polyacrylamide is added for sedimentation treatment in an amount of 4 mg / L to obtain a defluorinated pretreated phosphogypsum leachate; (4) Introducing the defluorinated pretreated phosphogypsum leachate obtained in step (3) into a membrane treatment system.

[0044] The defluorination pretreated phosphogypsum leachate obtained by this method has TP 6133ppm, CaO 2224ppm, Al2O3189ppm, Fe2O310.6ppm, F 200.8ppm, Si169ppm, fluorine removal rate reaches 66.5%, and phosphorus loss rate is 8.7%.

[0045] Comparative Example 3 Treatment of phosphogypsum leachate wastewater: Water quality of phosphogypsum leachate: TP 6718ppm, CaO 1843ppm, Al2O3446.8ppm, Fe2O385ppm, F600ppm, Si 169ppm, pH 2.3.

[0046] The operation steps and conditions are the same as those of Example 4, except that in step (2), no activator and potassium 3-sulfopropyl methacrylate are added.

[0047] The defluorination pretreated phosphogypsum leachate obtained by this method has TP 5833ppm, CaO 2232ppm, Al2O38.1ppm, Fe2O33.6ppm, F 33.6ppm, Si 179ppm, fluorine removal rate reaches 94.4%, and phosphorus loss rate is 13.2%.

[0048] Comparative Example 4 Treatment of phosphogypsum leachate wastewater: Water quality of phosphogypsum leachate: TP 6718ppm, CaO 1843ppm, Al2O3446.8ppm, Fe2O385ppm, F600ppm, Si 169ppm, pH 2.3.

[0049] The operation steps and conditions are the same as those of Example 4, except that potassium 3-sulfonate propyl methacrylate is not added in step (2).

[0050] The defluorination pretreated phosphogypsum leachate obtained by this method has TP 5913ppm, CaO 2132ppm, Al2O31.1ppm, Fe2O32.5ppm, F 28.6ppm, Si 172ppm, fluorine removal rate reaches 95.2%, and phosphorus loss rate is 12.0%. Comparative Example 5 Treatment of phosphogypsum leachate wastewater: Water quality of phosphogypsum leachate: TP 6718ppm, CaO 1843ppm, Al2O3446.8ppm, Fe2O385ppm, F600ppm, Si 169ppm, pH 2.3.

[0051] The operation steps and conditions are the same as those in Example 4, except that no activator is added in step (2).

[0052] The defluorination pretreated phosphogypsum leachate obtained by this method has TP 5813ppm, CaO 2032ppm, Al2O33.1ppm, Fe2O33.5ppm, F 27.6ppm, Si 175ppm, fluorine removal rate reaches 95.4%, and phosphorus loss rate is 13.5%.

[0053] In Examples 1-6, the fluorine removal rate exceeded 97%, the phosphorus loss rate was below 18%, the fluorine content in the defluorinated filtrate was below 16 ppm, the defluorinating agent had a high efficiency in defluorination performance, the Al2O3 and Fe2O3 in the filtrate after defluorination in Examples 1-6 were both below 6 ppm, the defluorinating agent had excellent iron and aluminum removal performance, and the silicon content was reduced. After the defluorinated filtrate in Examples 1-6 entered the membrane system, the operation was stable, the fluorosilicate scaling problem was alleviated, and the cleaning frequency of the ultrafiltration and reverse osmosis membranes was extended from 3 days to 7 days. Compared with Example 1, the defluorination rate of the defluorinating agent obtained without adding cerium sulfate was lower than that of Example 1. This is because sulfuric acid The addition of cerium will result in cerium oxide existing on the surface of calcium oxide, unreacted calcium carbonate and other impurities. Cerium oxide has good fluorine adsorption performance, which improves the fluorine removal performance of the defluoridation agent. Compared with Example 3, Example 2 directly adopts phosphogypsum for calcination, and the fluorine removal rate of the defluoridation agent obtained is significantly lower than that of Example 3. This is because the temperature at which calcium sulfate in phosphogypsum is completely decomposed is greater than the temperature at which calcium carbonate is completely decomposed. When calcined at 900°C, the calcium sulfate in phosphogypsum is not completely decomposed, and the calcium oxide content in the obtained defluoridation agent is lower than that in Example 3, so the soluble calcium that reacts with fluoride ions for precipitation is insufficient. In addition, the rate at which calcium sulfate in phosphogypsum directly reacts with fluoride ions to convert into calcium fluoride is low. Compared with Example 4, the fluorine and silicon contents in the defluorination pretreated phosphogypsum leachate of Comparative Examples 3, 4, and 5 are higher than those in Example 4, which indicates that the activator and potassium 3-sulfonate propyl methacrylate can effectively improve the removal effect of the defluorinator on fluorine and silicon. Through the defluorinator leaching test, the addition of the activator and potassium 3-sulfonate propyl methacrylate can effectively reduce the leaching rate of fluorine and silicon in the defluorinator. This may be because the activator and potassium 3-sulfonate propyl methacrylate can jointly promote the formation of a eutectic between fluoride and silicate, and the eutectic has a stable structure, which reduces the fluorine and silicon dissolution rate of the defluorinator. In addition, the activator and potassium 3-sulfonate propyl methacrylate can promote the formation of porous calcium oxide after calcination of phosphate tailings and calcium carbonate. After high-temperature decomposition of potassium 3-sulfonate propyl methacrylate, methane and hydroxyl radicals are produced, which is beneficial to high-temperature self-crosslinking of calcium oxide, so that the prepared defluorinator has more pores and a stable structure, providing more adsorption sites for fluorine absorption, thereby improving the defluorination effect of the defluorinator.

[0054] The above embodiments and comparative examples show that the defluorinating agent has both chemical precipitation defluorinating and adsorption defluorinating properties, and the addition of an activator and potassium 3-sulfonate propyl methacrylate is beneficial to the fixation of harmful elements in the defluorinating agent and provides more fluorine adsorption sites, thereby achieving effective removal of fluorine from phosphogypsum leachate and recovery of phosphorus.

Claims

1. A method for preparing a defluorinating agent, characterized in that: The method comprises the following steps: (1) reacting phosphogypsum and ammonium carbonate to obtain calcium carbonate slag and ammonium sulfate filtrate; (2) The calcium carbonate slag, phosphate tailings, cerium sulfate and pH adjuster obtained in step (1) are mixed and then wet-milled. After filtering, an activator and potassium 3-sulfonate propyl methacrylate are added to the residue, mixed evenly and then calcined to obtain a defluorinating agent. The filtrate is recycled as water for wet milling.

2. The method for preparing a defluorinating agent according to claim 1, characterized in that: In the step (1), the amount of ammonium carbonate used is 105% to 110% of the theoretical amount, the pH of the solution is adjusted to 8 to 9 with aqueous ammonia, the solid-liquid ratio of phosphogypsum and water is (1 to 1.1):1 (ammonium carbonate is dissolved by adding water, and ammonium carbonate reacts with calcium sulfate in the phosphogypsum), the reaction temperature is 60 to 70°C, and the reaction time is 2.5 to 3 hours.

3. The method for preparing a defluorinating agent according to claim 1, characterized in that: In the step (2), the calcium carbonate slag and the phosphorus tailings slag are mixed at a ratio of (0.5-1.5): (0.5-1.5), the amount of cerium sulfate added is 1%~5%, and the solid-liquid ratio of the mixture of the wet-ground calcium carbonate slag and the phosphorus tailings slag to water is (1~1.1):

1.

4. The method for preparing a defluorinating agent according to claim 1, characterized in that: In the step (2), the pH adjuster is one or more of sodium hydroxide, potassium hydroxide and ammonia water, and the amount of the pH adjuster added is 1% to 2% to ensure that the pH value of the wet grinding slurry is greater than 7.

5. The method for preparing a defluorinating agent according to claim 1, characterized in that: In the step (2), the activator is one or more of NaCl, K2SO4 and Na2CO3, and the amount used is 1% to 5%, and the amount of 3-sulfonate propyl methacrylate potassium added is 2% to 10%.

6. The method for preparing a defluorinating agent according to claim 1, characterized in that: In the step (2), the calcination temperature is 900-1000° C. for 1.5-2.5 hours.

7. A method for treating phosphogypsum leachate, characterized in that: The method adopts the defluorination agent obtained by the preparation method according to any one of claims 1 to 6.

8. The method for treating phosphogypsum leachate according to claim 7, characterized in that: The method comprises the following steps: S1 adds the defluoridation agent into the phosphogypsum leachate; S2: After the reaction in step S1 is completed, a flocculant is added for sedimentation treatment to obtain a defluorinated pretreated phosphogypsum leachate; S3 introduces the defluorination pretreated phosphogypsum leachate obtained in step S2 into a membrane treatment system to complete the treatment of the phosphogypsum leachate.

9. The method for treating phosphogypsum leachate according to claim 1, characterized in that: In step S1, the dosage of the defluoridating agent is 2-6 g / L, and the added amount is adjusted according to the fluorine content in the leachate and the pH value of the leachate. The pH value of the leachate after addition is controlled to be 3.5-4.5, and the mixture is stirred for 0.5-1.5 hours.

10. The method for treating phosphogypsum leachate according to claim 1, characterized in that: In step S1, the flocculant is polyacrylamide, the dosage of the flocculant is 2-6 mg / L, and the flocculation sedimentation time is 25-35 min.

Citation Information

Patent Citations

  • Preparation method of water body fluoride removal material

    CN102614849A

  • Method for preparing nanometer calcium carbonate slurry by using waste gypsum as calcium sources, products and application

    CN102674424A

  • Method of preparing fluorine adsorbent from waste bricks and application

    CN109482142A

  • Low-temperature vitrification harmless treatment method for overhaul slag, solid flux co-melted with overhaul slag, preparation method of solid flux, glass granules and application of glass granules

    CN110590153A

  • Aluminum-based compound fluorine removal agent and preparation method thereof

    CN113772762A

Cited By

  • Phosphogypsum leachate resourceful treatment system and method

    CN119263548A

  • Preparation method and application of aluminum-magnesium-based composite gel fluorine removal agent

    CN121372302A