Sludge deep conditioner composition and method for deep dehydration of sludge by using same
By using compositions of cell wall breakers, protein astringents and modified tannin flocculants, the problem of difficulty in dehydrating sludge is solved, efficient deep dehydration of sludge is achieved, and treatment costs are reduced.
Patent Information
- Application Number
- CN202411278107.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-12
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2044-09-12
AI Technical Summary
The existing sludge dewatering technology has the problems of high moisture content and difficulty in dehydration, especially due to the high organic content, fine particles and strong hydrophilicity in the sludge, the existing flocculants have poor effect in deep treatment.
Using a sludge depth conditioning agent composition, including cell wall breaker, protein astringent and modified tannin flocculants, a high-density cation charge and strong electrical neutralization adsorption capacity are formed through reasonable weight ratio and preparation method. flocculants for deep dehydration of sludge.
It realizes full release of water inside and outside the sludge, improves dehydration efficiency, reduces the amount of agent added, is suitable for deep conditioning of residual sludge, and reduces subsequent treatment costs.
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of sewage treatment, and in particular relates to a sludge deep conditioning agent composition and a method for deep dehydrating sludge by using the composition. Background Art
[0002] As the final product of water treatment, sludge has problems such as high water content and difficulty in dehydration. The water content of residual sludge generated by municipal sewage treatment plants is generally 95%~99%, and the volume is huge. Therefore, sludge reduction must first reduce the volume of sludge, and dehydration is an important link to reduce the subsequent treatment cost of sludge and improve the efficiency of sludge treatment. Due to the high organic matter content, fine particles, strong hydrophilicity and strong colloidal structure in sludge, sludge dehydration is difficult. The water contained in sludge can be roughly divided into free water, capillary water, bound water and intracellular water. Among them, free water accounts for about 70% of the total water, capillary water accounts for about 20% of the total water, and bound water and intracellular water account for about 10% of the total water. Free water can be easily removed by concentration or applying very small mechanical force, while capillary water and bound water need to be treated by adding strong chemical agents before they can be removed, and intracellular water must be released after cell wall rupture.
[0003] The key to using flocculants to condition sludge lies in the selection of flocculants. At present, there are two main types of flocculants used in water treatment: inorganic flocculants and organic flocculants. Inorganic flocculants are mainly polyaluminum and polyiron flocculants, which have good coagulation effects, a wide range of applications, strong electrical neutralization ability, and low unit price. However, they also have many problems, such as large dosage, toxic residual metals, certain corrosion to pipeline equipment, and impact on subsequent resource utilization of sludge. There are many types of organic polymer flocculants, which are usually used in small amounts, have fast floc formation speed, and have very excellent adsorption and bridging capabilities, but their electrical neutralization ability is weak and their ability to remove organic matter is poor, especially in the conditioning and dehydration of residual sludge, and cannot reach the level of deep treatment.
[0004] Therefore, how to obtain a sludge deep conditioner with good cell wall breaking effect, good flocculation performance and high floc density by rationally selecting raw materials and improving the preparation method and dosing method is an urgent problem to be solved by technical personnel in this field. Summary of the invention
[0005] In order to solve the above problems existing in the prior art, the present invention provides a sludge deep conditioner composition and a method for deep dehydration of sludge using the composition. The sludge deep conditioner composition of the present invention has a high degree of designability, and in the process of conditioning the excess sludge, the dosage of the agent is small and the dehydration effect is good. The molecular chain of the sludge deep conditioner composition of the present invention has a high density of cationic charges and a strong electrical neutralization adsorption capacity, and the flocculation effect is good, which can be applied to the conditioning of excess sludge. The method of the present invention can fully release the internal and external moisture of the sludge and improve the dehydration efficiency.
[0006] The technical solution adopted by the present invention is: The first aspect of the present invention provides a sludge deep conditioning agent composition, the raw material components comprising: Cell wall disrupting agent, 5-20 parts by weight; Protein astringent, 20-60 parts by weight; Modified tannin flocculant, 20-60 parts by weight.
[0007] Preferably, the cell wall disrupting agent is any one or more of potassium ferrate, potassium permanganate, and sodium percarbonate.
[0008] Preferably, the protein astringent is any one or more of aluminum sulfate, zinc carbonate, and sodium humate.
[0009] Preferably, the modified tannin flocculant is a product obtained by copolymerization of tannin with dimethyl diallyl ammonium chloride and N,N-methylenebisacrylamide.
[0010] The second aspect of the present invention provides a method for preparing the modified tannin flocculant, which is as follows: (a) adding 2-8 parts of tannin, 200-600 parts of dimethyldiallylammonium chloride, 1-3 parts of N,N-methylenebisacrylamide and 130-400 parts of distilled water, by mass, to obtain a monomer solution; Add 0.1-0.5 parts of chelating agent to the monomer solution, mix and dissolve thoroughly under stirring, and pass nitrogen to remove oxygen; (b) Slowly adding 0.03-0.5 parts by mass of an initiator to the solution system obtained in step (a) to initiate polymerization, and after the system temperature rises to 50-60° C., the temperature is maintained for 2-6 hours to obtain a modified tannin flocculant aqueous solution.
[0011] Preferably, in step (a), the dimethyldiallylammonium chloride is a dimethyldiallylammonium chloride aqueous solution with a mass percentage of 60%-65%.
[0012] Preferably, in step (a), the total solid content of tannin, dimethyldiallylammonium chloride and N,N-methylenebisacrylamide in the monomer solution is 35wt%-45wt%.
[0013] Preferably, in step (a), the chelating agent is a mixture of disodium ethylenediaminetetraacetate and diethylenetriaminepenta(methylenephosphonic acid) in a mass ratio of 2:(1-3); The initiator is any one or more of potassium persulfate, ammonium persulfate, ammonium cerium nitrate, and azobisisobutyramidine hydrochloride; The viscosity of the modified tannin flocculant aqueous solution is above 100,000 cps, and the solid content concentration is 40%. The third aspect of the present invention provides a method for deep dehydration of sludge using the sludge deep conditioning agent composition, comprising the following steps:
[0014] S1. Add the cell wall disrupting agent to the sludge to be treated and stir until fully mixed; the amount of the cell wall disrupting agent added is 0.5%-1% of the dry weight of the sludge; S2, adding a protein astringent to the sludge treated in step (S1), and stirring until fully mixed; the amount of the protein astringent added is 1%-5% of the dry weight of the sludge; S3, adding a modified tannin flocculant to the sludge treated in step (S2), and stirring until fully mixed; the dosage of the modified tannin flocculant is 1%-5% of the dry weight of the sludge; it should be noted that what is actually added here is an aqueous solution of the modified tannin flocculant, but the dosage of 1%-5% is calculated according to the solid phase addition amount of the modified tannin flocculant; S4. The sludge treated in step (S3) is allowed to stand in a conditioning tank for 10-15 minutes, and then subjected to filter pressing and dehydration, thereby completing deep dehydration of the sludge.
[0015] Preferably, the specific operating conditions of the filter pressing dehydration are: performing filter pressing treatment for 30-40 minutes at a pressure of 0.8-1.5 MPa, and completing the filter pressing; The filter press is a plate and frame filter press; The sludge to be treated is activated sludge or digested sludge with a moisture content of less than 95%.
[0016] The inventors of the present application have found in long-term research that the modified tannin flocculant can combine the advantages of tannic acid and polydimethyldiallyl ammonium chloride. This is because: the phenolic hydroxyl group and hydroxyl group of tannin can combine with the hydrogen bonds and ionic bonds on the amino acid residues of proteins, and there are also more benzene ring structures. The benzene ring is hydrophobic and can form non-covalent bonds with proteins, which can change the protein from the original unfolded state to the folded state, and at the same time, cross-link between molecules to form a gel-like structure, so that the water in the intracellular tissue is squeezed out. Polydimethyldiallyl ammonium chloride is a pure cationic organic polymer. In addition to the bridging and sweeping functions of general polymer flocculants, it also has a strong ability to dissolve extracellular polymers and neutralize electricity. The micro-crosslinked modified flocculant formed by copolymerization of tannin and dimethyldiallyl ammonium chloride not only combines the advantages of the two types of substances, but also in the flocculation process, the micro-crosslinked molecular structure can make full use of the spatial extension advantage to adsorb suspended particles, and the formed flocs have high density and good sedimentation.
[0017] The present invention has the following beneficial effects: The present invention provides a sludge deep conditioner composition. By using a cell wall disruptor, a protein astringent, and a modified tannin flocculant as raw materials and performing appropriate weight proportioning, the sludge deep conditioner composition finally prepared can fully release the internal and external moisture of the sludge and improve the dehydration efficiency. The sludge conditioner composition of the present invention has a high degree of designability. In the process of conditioning the excess sludge, the dosage of the agent is small and the dehydration effect is good. The molecular chain of the sludge deep conditioner composition of the present invention has a high density of cationic charges and a strong electrical neutralization adsorption capacity, and the flocculation effect is good, and it can be applied to the conditioning of the excess sludge. DETAILED DESCRIPTION
[0018] To make the purpose, technical solution and advantages of the present invention clearer, the technical solution of the present invention will be described in detail below. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments of the present invention, all other implementation methods obtained by ordinary technicians in this field without creative work belong to the scope of protection of the present invention.
[0019] First, the present invention provides a sludge deep conditioning agent composition, the raw material components include: Cell wall disrupting agent, 5-20 parts by weight; Protein astringent, 20-60 parts by weight; Modified tannin flocculant, 20-60 parts by weight.
[0020] Preferably, the cell wall disrupting agent is any one or more of potassium ferrate, potassium permanganate, and sodium percarbonate.
[0021] Preferably, the protein astringent is any one or more of aluminum sulfate, zinc carbonate, and sodium humate.
[0022] Preferably, the modified tannin flocculant is a product obtained by copolymerization of tannin with dimethyl diallyl ammonium chloride and N,N-methylenebisacrylamide.
[0023] Furthermore, the present invention also provides a method for preparing the modified tannin flocculant, which is as follows: (a) adding 2-8 parts of tannin, 200-600 parts of dimethyldiallylammonium chloride, 1-3 parts of N,N-methylenebisacrylamide and 130-400 parts of distilled water, by mass, to obtain a monomer solution; Add 0.1-0.5 parts of chelating agent to the monomer solution, mix and dissolve thoroughly under stirring, and pass nitrogen to remove oxygen; (b) Slowly adding 0.03-0.5 parts by mass of an initiator to the solution system obtained in step (a) to initiate polymerization, and after the system temperature rises to 50-60° C., the temperature is maintained for 2-6 hours to obtain a modified tannin flocculant aqueous solution.
[0024] Preferably, in step (a), the dimethyldiallylammonium chloride is a dimethyldiallylammonium chloride aqueous solution with a mass percentage of 60%-65%.
[0025] Preferably, in step (a), the total solid content of tannin, dimethyldiallylammonium chloride and N,N-methylenebisacrylamide in the monomer solution is 35wt%-45wt%.
[0026] Preferably, in step (a), the chelating agent is a mixture of disodium ethylenediaminetetraacetate and diethylenetriaminepenta(methylenephosphonic acid) in a mass ratio of 2:(1-3); The initiator is any one or more of potassium persulfate, ammonium persulfate, ammonium cerium nitrate, and azobisisobutyramidine hydrochloride; The modified tannin flocculant aqueous solution has a viscosity of more than 100,000 cps and a solid content concentration of 40%.
[0027] Furthermore, the present invention also provides a method for deep dehydrating sludge using the sludge deep conditioner composition, comprising the following steps: S1. Add the cell wall disrupting agent to the sludge to be treated and stir until fully mixed; the amount of the cell wall disrupting agent added is 0.5%-1% of the dry weight of the sludge; S2, adding a protein astringent to the sludge treated in step (S1), and stirring until fully mixed; the amount of the protein astringent added is 1%-5% of the dry weight of the sludge; S3, adding a modified tannin flocculant to the sludge treated in step (S2), and stirring until fully mixed; the amount of the modified tannin flocculant added is 1%-5% of the dry weight of the sludge; S4. The sludge treated in step (S3) is allowed to stand in a conditioning tank for 10-15 minutes, and then subjected to filter pressing and dehydration, thereby completing deep dehydration of the sludge.
[0028] Preferably, the specific operating conditions of the filter pressing dehydration are: performing filter pressing treatment for 30-40 minutes at a pressure of 0.8-1.5 MPa, and completing the filter pressing; The filter press is a plate and frame filter press; The sludge to be treated is activated sludge or digested sludge with a moisture content of less than 95%.
[0029] In the following examples, 1 part by weight represents 1 g.
[0030] Example 1 This embodiment provides a sludge deep conditioning agent composition, the raw material components include: Potassium ferrate, 25 parts by weight; 100 parts by weight of first-grade sodium humate with an effective content of 70%; Modified tannin flocculant aqueous solution, 250 parts by weight.
[0031] The preparation method of the modified tannin flocculant is specifically as follows: (a) 3 parts by mass of tannin, 500 parts by mass of 65% aqueous dimethyldiallylammonium chloride solution, 1 part by mass of N,N-methylenebisacrylamide, and 318.5 parts by mass of distilled water were added to a reaction kettle to prepare a monomer solution having a solid content concentration of 40%, and then 0.2 parts by mass of disodium ethylenediaminetetraacetate and 0.1 parts by mass of diethylenetriaminepenta(methylenephosphonic acid) were added, the mixture was fully mixed and dissolved, and nitrogen was passed through the mixture under stirring to remove oxygen; (b) Slowly adding 0.1 parts of ammonium cerium nitrate and 0.2 parts of azobisisobutylamidine hydrochloride, by mass, to the solution system obtained in step (a) to initiate polymerization, and after the system temperature rises to 50° C., the temperature is maintained for 3 hours to obtain a modified tannin flocculant aqueous solution with a rotational viscosity of 11500 cps and a solid content concentration of 40%.
[0032] Furthermore, a method for deep dehydrating sludge using the sludge deep conditioner composition comprises the following steps: S1. Add 25g potassium ferrate to 100kg of sludge to be treated with a moisture content of 95% (residual sludge from Beijing Enterprises Water Group Yanjiao West Water Plant), and stir until fully mixed; S2. Add 100 g of first-grade sodium humate with an effective content of 70% to the sludge treated in step (S1), and stir until fully mixed; S3, adding 250 g of the modified tannin flocculant aqueous solution having a solid content concentration of 40% to the sludge treated in step (S2), and stirring until fully mixed; S4. The sludge treated in step (S3) was allowed to stand in the conditioning tank for 10 minutes, and then the concentrated sludge was extracted from the bottom of the tank and introduced into a plate and frame filter press for filter pressing and dehydration. The pressure was maintained at 1.5 MPa for 40 minutes. After the filter pressing was completed, the deep dehydration of the sludge to be treated was completed. The dehydration effect was tested, and the moisture content of the mud cake after dehydration was 53.26%.
[0033] Example 2 This embodiment provides a sludge deep conditioning agent composition, the raw material components include: Potassium permanganate, 25 parts by weight; 100 parts by weight of first-grade sodium humate with an effective content of 70%; Modified tannin flocculant aqueous solution, 250 parts by weight.
[0034] The preparation method of the modified tannin flocculant is specifically as follows: (a) 3 parts by mass of tannin, 500 parts by mass of 65% aqueous dimethyldiallylammonium chloride solution, 1 part by mass of N,N-methylenebisacrylamide, and 318.5 parts by mass of distilled water were added to a reaction kettle to prepare a monomer solution having a solid content concentration of 40%, and then 0.2 parts by mass of disodium ethylenediaminetetraacetate and 0.1 parts by mass of diethylenetriaminepenta(methylenephosphonic acid) were added, the mixture was fully mixed and dissolved, and nitrogen was passed through the mixture under stirring to remove oxygen; (b) Slowly adding 0.1 parts of ammonium cerium nitrate and 0.2 parts of azobisisobutylamidine hydrochloride, by mass, to the solution system obtained in step (a) to initiate polymerization, and after the system temperature rises to 50° C., the temperature is maintained for 3 hours to obtain a modified tannin flocculant aqueous solution with a rotational viscosity of 11500 cps and a solid content concentration of 40%.
[0035] Furthermore, a method for deep dehydrating sludge using the sludge deep conditioner composition comprises the following steps: S1. Add 25g potassium permanganate to 100kg of sludge to be treated with a moisture content of 95% (residual sludge from Beijing Enterprises Water Group Yanjiao West Water Plant), and stir until fully mixed; S2. Add 100 g of first-grade sodium humate with an effective content of 70% to the sludge treated in step (S1), and stir until fully mixed; S3, adding 250 g of the modified tannin flocculant aqueous solution having a solid content concentration of 40% to the sludge treated in step (S2), and stirring until fully mixed; S4. The sludge treated in step (S3) was allowed to stand in the conditioning tank for 10 minutes, and then the concentrated sludge was extracted from the bottom of the tank and introduced into a plate and frame filter press for filter pressing and dehydration. The pressure was maintained at 1.5 MPa for 40 minutes. After the filter pressing was completed, the deep dehydration of the sludge to be treated was completed. The dehydration effect was tested, and the moisture content of the mud cake after dehydration was 52.45%.
[0036] Example 3 This embodiment provides a sludge deep conditioning agent composition, the raw material components include: Potassium ferrate, 25 parts by weight; Aluminum sulfate, 75 parts by weight; Modified tannin flocculant aqueous solution, 250 parts by weight.
[0037] The preparation method of the modified tannin flocculant is specifically as follows: (a) 3 parts by mass of tannin, 500 parts by mass of 65% aqueous dimethyldiallylammonium chloride solution, 1 part by mass of N,N-methylenebisacrylamide, and 318.5 parts by mass of distilled water were added to a reaction kettle to prepare a monomer solution having a solid content concentration of 40%, and then 0.2 parts by mass of disodium ethylenediaminetetraacetate and 0.1 parts by mass of diethylenetriaminepenta(methylenephosphonic acid) were added, the mixture was fully mixed and dissolved, and nitrogen was passed through the mixture under stirring to remove oxygen; (b) Slowly adding 0.1 parts of ammonium cerium nitrate and 0.2 parts of azobisisobutylamidine hydrochloride, by mass, to the solution system obtained in step (a) to initiate polymerization, and after the system temperature rises to 50° C., the temperature is maintained for 3 hours to obtain a modified tannin flocculant aqueous solution with a rotational viscosity of 115,000 cps and a solid content concentration of 40%.
[0038] Furthermore, a method for deep dehydrating sludge using the sludge deep conditioner composition comprises the following steps: S1. Add 25g potassium ferrate to 100kg of sludge to be treated with a moisture content of 95% (residual sludge from Beijing Enterprises Water Group Yanjiao West Water Plant), and stir until fully mixed; S2. Add 75 g of aluminum sulfate to the sludge treated in step (S1) and stir until fully mixed; S3, adding 250 g of the modified tannin flocculant aqueous solution having a solid content concentration of 40% to the sludge treated in step (S2), and stirring until fully mixed; S4. The sludge treated in step (S3) was allowed to stand in the conditioning tank for 10 minutes, and then the concentrated sludge was extracted from the bottom of the tank and introduced into a plate and frame filter press for filter pressing and dehydration. The pressure was maintained at 1.5 MPa for 40 minutes. After the filter pressing was completed, the deep dehydration of the sludge to be treated was completed. The dehydration effect was tested, and the moisture content of the mud cake after dehydration was 54.62%.
[0039] Example 4 This embodiment provides a sludge deep conditioning agent composition, the raw material components include: Potassium permanganate, 25 parts by weight; Aluminum sulfate, 75 parts by weight; Modified tannin flocculant aqueous solution, 250 parts by weight.
[0040] The preparation method of the modified tannin flocculant is specifically as follows: (a) 7 parts by mass of tannin, 600 parts by mass of 60% aqueous dimethyldiallylammonium chloride solution, 3 parts by mass of N,N-methylenebisacrylamide, and 315 parts by mass of distilled water were added to a reaction kettle to prepare a monomer solution with a solid content concentration of 40%, and then 0.1 parts by mass of disodium ethylenediaminetetraacetate and 0.2 parts by mass of diethylenetriaminepenta(methylenephosphonic acid) were added, the mixture was fully mixed and dissolved, and nitrogen was passed through the reaction kettle for deoxygenation under stirring; (b) Slowly adding 0.1 parts of ammonium cerium nitrate and 0.2 parts of azobisisobutylamidine hydrochloride, by mass, to the solution system obtained in step (a) to initiate polymerization, and after the system temperature rises to 60° C., the temperature is maintained for 6 hours to obtain a modified tannin flocculant aqueous solution with a rotational viscosity of 165,000 cps and a solid content concentration of 40%.
[0041] Furthermore, a method for deep dehydrating sludge using the sludge deep conditioner composition comprises the following steps: S1. Add 25g potassium permanganate to 100kg of sludge to be treated with a moisture content of 95% (residual sludge from Beijing Enterprises Water Group Yanjiao West Water Plant), and stir until fully mixed; S2. Add 75 g of aluminum sulfate to the sludge treated in step (S1) and stir until fully mixed; S3, adding 250 g of the modified tannin flocculant aqueous solution having a solid content concentration of 40% to the sludge treated in step (S2), and stirring until fully mixed; S4. The sludge treated in step (S3) was allowed to stand in the conditioning tank for 10 minutes, and then the concentrated sludge was extracted from the bottom of the tank and introduced into a plate and frame filter press for filter pressing and dehydration. The pressure was maintained at 1.5 MPa for 40 minutes. After the filter pressing was completed, the deep dehydration of the sludge to be treated was completed. The dehydration effect was tested, and the moisture content of the mud cake after dehydration was 51.25%.
[0042] Comparative Example 1 This comparative example provides a method for dehydrating sludge using a conventional inorganic sludge conditioner (a mixture of ferric chloride and lime), specifically: the amount of ferric chloride added is 6.12% of the dry weight of the sludge, and the amount of lime added is 24% of the dry weight of the sludge. After being treated with a plate and frame filter press at a pressure of about 1.5 MPa and a pressing time of 40 minutes, the moisture content of the mud cake is 58.56%.
[0043] Comparative Example 2 This comparative example provides a method for dehydrating sludge using potassium permanganate, sodium humate, and polydimethyldiallylammonium chloride, specifically: S1. Add 25g potassium ferrate to 100kg of sludge to be treated with a moisture content of 95% (residual sludge from Beijing Enterprises Water Group Yanjiao West Water Plant), and stir until fully mixed; S2. Add 75 g of aluminum sulfate to the sludge treated in step (S1) and stir until fully mixed; S3, adding 250 g of a polydimethyldiallylammonium chloride aqueous solution having a solid content concentration of 40% to the sludge treated in step (S2), and stirring until fully mixed; S4. The sludge treated in step (S3) was allowed to stand in the conditioning tank for 10 minutes, and then the concentrated sludge was extracted from the bottom of the tank and introduced into the same plate and frame filter press for filter pressing and dehydration. The pressure was maintained at 1.5 MPa for 40 minutes. After the filter pressing was completed, the deep dehydration of the sludge to be treated was completed. The dehydration effect was tested, and the moisture content of the mud cake after dehydration was 56.36%.
[0044] Comparative Example 3 This comparative example provides a method for dehydrating sludge using potassium permanganate and the modified tannin flocculant aqueous solution, specifically: S1. Add 45g potassium permanganate to 100kg of sludge to be treated with a moisture content of 95% (residual sludge from Beijing Enterprises Water Group Yanjiao West Water Plant), and stir until fully mixed; S2, adding 300 g of the modified tannin flocculant aqueous solution having a solid content concentration of 40% to the sludge treated in step (S1), and stirring until fully mixed; S4. The sludge treated in step (S3) was allowed to stand in the conditioning tank for 10 minutes, and then the concentrated sludge was extracted from the bottom of the tank and introduced into the same plate and frame filter press for filter pressing and dehydration. The pressure was maintained at 1.5 MPa for 40 minutes. After the filter pressing was completed, the deep dehydration of the sludge to be treated was completed. The dehydration effect was tested, and the moisture content of the mud cake after dehydration was 57.53%.
[0045] Comparative Example 4 This comparative example provides a method for dehydrating sludge using aluminum sulfate and the modified tannin flocculant aqueous solution, specifically: S1. Add 100g of aluminum sulfate to 100kg of sludge to be treated with a moisture content of 95% (residual sludge from Yanjiao West Water Plant of Beijing Enterprises Water Group), and stir until fully mixed; S2, adding 300 g of the modified tannin flocculant aqueous solution having a solid content concentration of 40% to the sludge treated in step (S1), and stirring until fully mixed; S4. The sludge treated in step (S3) was allowed to stand in the conditioning tank for 10 minutes, and then the concentrated sludge was extracted from the bottom of the tank and introduced into the same plate and frame filter press for filter pressing and dehydration. The pressure was maintained at 1.5 MPa for 40 minutes. After the filter pressing was completed, the deep dehydration of the sludge to be treated was completed. The dehydration effect was tested, and the moisture content of the mud cake after dehydration was 58.17%.
[0046] Experimental example The dewatering effects of the different flocculants obtained in Examples 1-4 and Comparative Examples 1-4 were tested on the sludge, and the results are shown in Table 1.
[0047] Table 1- Comparison of sludge dewatering effects of different flocculants sample Example 1 Example 2 Example 3 Example 4 Comparative Example 1 Comparative Example 2 Comparative Example 3 Comparative Example 4 The proportion of the amount of additives to dry mud 3.9 3.9 4.0 4.0 30.12 4.0 3.3 4.4 Mud cake moisture content% 53.26 52.45 54.62 51.25 58.56 56.36 57.53 58.17 As can be seen from Table 1, the sludge deep conditioner composition of the present invention has a better sludge dehydration effect than similar products, can completely replace conventional inorganic sludge conditioners, greatly improve the calorific value of sludge, and help promote the resource utilization of sludge. Compared with conventional inorganic conditioners, the dosage of the agent accounts for more than 30% of the dry weight of the sludge. The dosage of the present invention is small, accounting for only about 4% of the weight of the dry sludge, which will greatly reduce the sludge disposal cost. The lack of any of the three components of the cell wall breaker, protein astringent, and modified tannin flocculant in the sludge deep conditioner composition of the present invention will affect the deep dehydration effect of the sludge (see Comparative Examples 2-4 for details), indicating that only under the joint action of the above three components can the dehydration effect of the conditioner composition of the present invention on the sludge be optimal.
Claims
1. A sludge deep conditioning agent composition, characterized in that: The raw material components include: Cell wall disrupting agent, 5-20 parts by weight; Protein astringent, 20-60 parts by weight; Modified tannin flocculant, 20-60 parts by weight.
2. The sludge deep conditioner composition according to claim 1, characterized in that: The cell wall disrupting agent is any one or more of potassium ferrate, potassium permanganate and sodium percarbonate.
3. The sludge deep conditioner composition according to claim 1, characterized in that: The protein astringent is any one or more of aluminum sulfate, zinc carbonate and sodium humate.
4. The sludge deep conditioner composition according to claim 1, characterized in that: The modified tannin flocculant is a product obtained by copolymerization of tannin, dimethyldiallylammonium chloride and N,N-methylenebisacrylamide.
5. The sludge deep conditioner composition according to claim 4, characterized in that: The preparation method of the modified tannin flocculant is specifically as follows: (a) adding 2-8 parts of tannin, 200-600 parts of dimethyldiallylammonium chloride, 1-3 parts of N,N-methylenebisacrylamide and 130-400 parts of distilled water, by mass, to obtain a monomer solution; Add 0.1-0.5 parts of chelating agent to the monomer solution, mix and dissolve thoroughly under stirring, and pass nitrogen to remove oxygen; (b) Slowly adding 0.03-0.5 parts by mass of an initiator to the solution system obtained in step (a) to initiate polymerization, and after the system temperature rises to 50-60° C., the temperature is maintained for 2-6 hours to obtain a modified tannin flocculant aqueous solution.
6. The sludge deep conditioner composition according to claim 5, characterized in that: In step (a), the dimethyldiallyl ammonium chloride is a dimethyldiallyl ammonium chloride aqueous solution with a mass percentage of 60%-65%.
7. The sludge deep conditioner composition according to claim 6, characterized in that: In step (a), the total solid content of tannin, dimethyldiallylammonium chloride and N,N-methylenebisacrylamide in the monomer solution is 35wt%-45wt%.
8. The sludge deep conditioner composition according to claim 6, characterized in that: In step (a), the chelating agent is a mixture of disodium ethylenediaminetetraacetate and diethylenetriaminepenta(methylenephosphonic acid) in a mass ratio of 2:(1-3); The initiator is any one or more of potassium persulfate, ammonium persulfate, ammonium cerium nitrate, and azobisisobutyramidine hydrochloride; The viscosity of the modified tannin flocculant aqueous solution is above 100,000 cps.
9. A method for deep dehydration using the sludge deep conditioner composition according to any one of claims 1 to 8, characterized in that: The following steps are involved: S1. Add the cell wall disrupting agent to the sludge to be treated and stir until fully mixed; The dosage of the cell wall disrupting agent is 0.5%-1% of the dry weight of the sludge; S2, adding a protein astringent to the sludge treated in step (S1), and stirring until fully mixed; the amount of the protein astringent added is 1%-5% of the dry weight of the sludge; S3, adding a modified tannin flocculant to the sludge treated in step (S2), and stirring until fully mixed; the dosage of the modified tannin flocculant is 1%-5% of the dry weight of the sludge; S4. The sludge treated in step (S3) is allowed to stand in a conditioning tank for 10-15 minutes, and then subjected to filter pressing and dehydration, thereby completing deep dehydration of the sludge.
10. The deep dehydration method according to claim 9, characterized in that: The specific operating conditions of the filter pressing dehydration are: the filter pressing treatment is carried out at a pressure of 0.8-1.5MPa for 30-40min, and the filter pressing is completed; The filter press is a plate and frame filter press; The sludge to be treated is activated sludge or digested sludge with a moisture content of less than 95%.
Citation Information
Patent Citations
Compound sludge conditioner for sludge dewatering
CN107686225A
Biological composite water treatment agent and preparation method and application thereof
CN110668582A
Method of enhancing sludge dewatering performance
CN110759629A
Method for enhancing dehydration performance of activated sludge by cationic starch grafted condensed tannin
CN111807674A
Cationic black wattle tannin flocculating agent and preparation method thereof
CN112441655A
Cited By
Sludge dehydration treatment method
CN121948808A