Mining method for spraying thin-layer material by utilizing supercritical carbon dioxide
By stirring the fine spray materials for minerals in a supercritical carbon dioxide environment, the problem of uneven dispersion of polymers is solved, the material performance is improved, and the reuse of carbon dioxide and the expansion of resources are realized. It is suitable for the support and protection of the mining environment. .
Patent Information
- Application Number
- CN202410960827.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-17
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2044-07-17
AI Technical Summary
The polymer dispersion in existing mineral thin spray materials is uneven, which affects its performance, especially the support and protection effects in the mining environment.
The supercritical carbon dioxide spray thin layer material method is used to fully stir the solid phase material and liquid phase material in the supercritical carbon dioxide environment through an explosion-proof mixer, and the dual properties of the gas phase and liquid phase promote the uniform dispersion of the polymer to prepare the properties Better spray materials for mines and spray them directly to the tunnels and slopes through spray guns.
It improves the dispersion of polymers, improves the bonding and sealing properties, realizes the reuse of carbon dioxide and the expansion of resources, and is suitable for underground construction, reducing coal dust, fire protection, support and other aspects.
Smart Images

Figure CN118909472A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of mine spraying materials, and in particular to a method for spraying a thin layer of mine material using supercritical carbon dioxide. Background Art
[0002] Supercritical carbon dioxide technology Due to its low toxicity, volatility and environmental friendliness, supercritical carbon dioxide has been widely used in chemical, pharmaceutical, material science and other fields.
[0003] Mining thin-spraying materials usually refer to special materials used for mine support and gas prevention, fire prevention, dust prevention, strengthening of tunnels and slopes and other engineering construction. These materials are usually sprayed on the surface of mine tunnels and slopes to improve their stability and reduce coal dust, fire prevention, support and other functions. These materials have the characteristics of strong adhesion, wear resistance, impact resistance, etc., and can meet special support requirements in mining environments. However, the performance of mining thin-spraying materials is closely related to the uniformity of polymer dispersion. At present, there is still a technical problem of uneven polymer dispersion in mining thin-spraying materials in the existing technology.
[0004] This shows that the prior art needs to be further improved. Summary of the invention
[0005] The purpose of the present invention is to provide a method for spraying a thin layer of material for mining using supercritical carbon dioxide. Since supercritical carbon dioxide has gas phase and liquid phase properties and has high diffusivity and permeability, its properties are fully utilized to promote the dispersion of polymers and prepare mining thin spraying materials with better performance. The equipment can be directly used underground, and the prepared mining thin spraying materials can be directly sprayed onto the required tunnels and slopes. Gas recovery can also be achieved to reuse carbon dioxide.
[0006] In order to achieve the above object, the present invention adopts the following technical solutions:
[0007] A method for spraying a thin layer of material using supercritical carbon dioxide for mining, comprising the following steps:
[0008] Step 1: Prepare the required equipment
[0009] The device comprises an explosion-proof mixer, the input end of the explosion-proof mixer is respectively connected to a carbon dioxide storage tank and a liquid material storage tank, and the output end of the explosion-proof mixer is connected to a spray gun;
[0010] Step 2: prepare solid phase materials and place them in the explosion-proof mixer, wherein the solid phase materials include cement and light calcium carbonate, and fully mix and stir the solid phase materials in the explosion-proof mixer to make the two mixed evenly;
[0011] Prepare a liquid material, the liquid material comprising a polymer, an additive and water, and place the liquid material in the liquid material storage tank;
[0012] Step 3, heating the explosion-proof mixer and keeping stirring;
[0013] Step 4: providing gaseous carbon dioxide through a carbon dioxide storage tank, and converting the gaseous carbon dioxide into supercritical carbon dioxide in an explosion-proof mixer by temperature control and pressurization;
[0014] Step 5: Input the liquid phase material into the explosion-proof mixer. In the explosion-proof mixer, the liquid phase material and the solid phase material are fully stirred and mixed under the supercritical carbon dioxide environment to prepare a slurry of the thin-shot material for mining;
[0015] Step 6: The mining thin-shot material slurry in the explosion-proof mixer is sprayed out through a spray gun.
[0016] In the above-mentioned method for spraying a thin layer of material using supercritical carbon dioxide for mining, in step one, a carbon dioxide explosion-proof delivery booster pump is connected between the carbon dioxide storage tank and the explosion-proof mixer, a liquid material explosion-proof delivery booster pump is connected between the liquid material storage tank and the explosion-proof mixer; and a thin spray material explosion-proof delivery pump is connected between the explosion-proof mixer and the spray gun.
[0017] In the above-mentioned method for spraying a thin layer of material using supercritical carbon dioxide for mining, in step one, the explosion-proof mixer includes an explosion-proof tank body, an agitator is arranged in the explosion-proof tank body, an explosion-proof motor is arranged on the outer wall of the explosion-proof tank body, the agitator is driven to rotate by the explosion-proof motor, and the outside of the explosion-proof tank body is connected to an explosion-proof mixer exhaust port, an explosion-proof mixer pressure relief valve, a heater, a pressure gauge and a temperature gauge.
[0018] In the above-mentioned method for spraying a thin layer of material using supercritical carbon dioxide for mining, in step 2, the polymer is a powder or a liquid, and the additives include a water reducing agent, a film-forming agent, a defoaming agent and cellulose.
[0019] In the above-mentioned method for spraying a thin layer of material using supercritical carbon dioxide for mining, in step 4, the temperature is 32-50° C. and the pressure is 7.4-20 MPa.
[0020] In the above-mentioned method for spraying a thin layer of material using supercritical carbon dioxide for mining, the polymer is a resin liquid, and in parts by weight, the polymer is 50 to 70 parts, the admixture is 5 to 10 parts, and water is 20 to 40 parts.
[0021] In the above-mentioned method for spraying a thin layer of material using supercritical carbon dioxide for mining, the weight ratio of the water reducing agent, film-forming agent, defoaming agent and cellulose in the admixture is 1-2:2-3:4-6:1-2.
[0022] In the above-mentioned method for spraying a thin layer of material using supercritical carbon dioxide for mining, the water reducer is a polycarboxylic acid water reducer, the film-forming agent is a polyurethane resin, the defoamer is an organosilicon defoamer, and the cellulose is wood cellulose.
[0023] Compared with the prior art, the present invention brings the following beneficial technical effects:
[0024] (1) The present invention utilizes supercritical carbon dioxide to prepare the thin spraying material for mining. Since supercritical carbon dioxide has the dual properties of gas phase and liquid phase, under supercritical conditions, the solubility of carbon dioxide is very strong, and it can quickly penetrate into the polymer system and evenly disperse the molecules in the polymer therein. In addition, supercritical carbon dioxide has both solubility in liquid state and diffusivity in gas state, and this dual property can further promote the dispersion of the polymer. Therefore, the polymer is more evenly dispersed, and the bonding performance and sealing performance are better.
[0025] (2) The present invention utilizes supercritical carbon dioxide to spray thin layer materials, which can expand the utilization of carbon dioxide resources.
[0026] (3) The device involved in the method of using supercritical carbon dioxide to spray thin layer materials of the present invention is suitable for underground, and can directly spray the mixed mining thin spraying material on the tunnel and slope surface through an explosion-proof delivery pump and a spray gun.
[0027] In summary, the method of the present invention is simple to operate, improves the dispersibility of the polymer, improves the performance of the thin-sprayed material for mining, realizes the fixation of carbon dioxide, and can also recycle carbon dioxide for repeated use. In addition, the device for preparing the thin-sprayed material for mining using supercritical carbon dioxide can be used underground, and the prepared thin-sprayed material for mining can be directly sprayed onto coal mine tunnels and slopes, thereby playing a role in reducing coal dust, fire prevention, and support. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] The present invention will be further described below in conjunction with the accompanying drawings:
[0029] Figure 1 A flow chart of a method for spraying a thin layer of material using supercritical carbon dioxide according to the present invention;
[0030] Figure 2 This is a schematic diagram of the device structure required for the present invention;
[0031] Figure 3 This is a schematic diagram of the explosion-proof mixer structure of the present invention;
[0032] In the figure:
[0033] 1-Carbon dioxide storage tank, 2-Carbon dioxide explosion-proof delivery booster pump, 3-Explosion-proof mixer, 4-Liquid material storage tank, 5-Liquid material explosion-proof delivery booster pump, 6-Explosion-proof gas recovery device, 7-Thin spray material explosion-proof delivery pump, 8-Spray gun, 9-Carbon dioxide storage tank outlet, 10-Carbon dioxide storage tank valve, 11-Carbon dioxide explosion-proof delivery booster pump inlet, 12-Carbon dioxide explosion-proof delivery booster pump outlet, 13-Liquid material storage tank outlet, 14-Liquid material storage tank valve, 15-Liquid material explosion-proof delivery booster pump inlet, 16-Liquid material explosion-proof delivery booster pump Discharge port, 17-explosion-proof gas recovery device air inlet, 18-explosion-proof mixer discharge valve, 19-thin spray material explosion-proof delivery pump feed port, 20-thin spray material explosion-proof delivery pump discharge port, 21-explosion-proof mixer liquid phase material feed port, 22-explosion-proof mixer carbon dioxide air inlet, 23-explosion-proof motor, 24-auger, 25-explosion-proof mixer discharge port, 26-explosion-proof mixer exhaust port, 27-explosion-proof mixer pressure relief valve, 28-heater, 29-pressure gauge, 30-temperature gauge, 31-carbon dioxide explosion-proof delivery booster pump outlet valve, 32-liquid phase material explosion-proof delivery booster pump discharge valve. DETAILED DESCRIPTION
[0034] The present invention proposes a method for spraying a thin layer of material using supercritical carbon dioxide for mining. In order to make the advantages and technical solutions of the present invention clearer and more specific, the present invention is further described below in conjunction with specific embodiments.
[0035] It is understandable that the connection relationship described in this application refers to direct or indirect connection. For example, the connection between A and B can be either a direct connection between A and B or an indirect connection between A and B through one or more other electrical components. For example, A and C can be directly connected, and C and B can be directly connected, so that A and B are connected through C. It is also understandable that the "A connects B" described in this application can be a direct connection between A and B, or an indirect connection between A and B through one or more other electrical components.
[0036] The technical solution of the present application is further described in detail below in conjunction with the accompanying drawings.
[0037] Combination Figure 2 and Figure 3As shown, the device required for a method for spraying a thin layer of material using supercritical carbon dioxide for mining of the present invention includes a carbon dioxide storage tank 1, an explosion-proof mixer 3, a liquid material storage tank 4 and a spray gun 8, carbon dioxide is stored in the carbon dioxide storage tank 1, a carbon dioxide explosion-proof delivery booster pump 2 is arranged between the carbon dioxide storage tank 1 and the explosion-proof mixer 3, a carbon dioxide storage tank air outlet 9 and a carbon dioxide storage tank valve 10 are arranged on the carbon dioxide storage tank 1, the carbon dioxide explosion-proof delivery booster pump 2 is provided with a carbon dioxide explosion-proof delivery booster pump air inlet 11 and a carbon dioxide explosion-proof delivery booster pump air outlet 12, and a carbon dioxide explosion-proof delivery booster pump air outlet valve 31 is arranged between the carbon dioxide explosion-proof delivery booster pump 2 and the explosion-proof mixer 3.
[0038] A liquid-phase material explosion-proof conveying booster pump 5 is arranged between the liquid-phase material storage tank 4 and the explosion-proof mixer 3, and a liquid-phase material explosion-proof conveying booster pump inlet 15 and a liquid-phase material explosion-proof conveying booster pump outlet 16 are arranged on the liquid-phase material explosion-proof conveying booster pump 5. A liquid-phase material storage tank outlet 13 is arranged on the liquid-phase material storage tank 4, and a liquid-phase material storage tank valve 14 is arranged between the liquid-phase material storage tank 4 and the liquid-phase material explosion-proof conveying booster pump 5.
[0039] The explosion-proof mixer 3 is connected to an explosion-proof gas recovery device 6 , and the explosion-proof gas recovery device 6 is provided with an explosion-proof gas recovery device air inlet 17 .
[0040] The explosion-proof mixer 3 is connected to the spray gun 8 through the thin spray material explosion-proof delivery pump 7. The thin spray material explosion-proof delivery pump 7 is provided with a thin spray material explosion-proof delivery pump inlet 19 and a thin spray material explosion-proof delivery pump outlet 20. The explosion-proof mixer discharge valve 18 is provided on the pipeline connecting the thin spray material explosion-proof delivery pump 7 and the explosion-proof mixer 3.
[0041] Specifically, Figure 3 As shown, the specific structure of the explosion-proof mixer 3 includes an explosion-proof tank body, an augers 24 is arranged in the explosion-proof tank body, an explosion-proof motor 23 is arranged on the outer wall of the explosion-proof tank body, the augers are driven to rotate by the explosion-proof motor, and the outer side of the explosion-proof tank body is connected with an explosion-proof mixer exhaust port 26, an explosion-proof mixer pressure relief valve 27, a heater 28, a pressure gauge 29 and a temperature gauge 30. The explosion-proof tank body is also provided with an explosion-proof mixer liquid material feed port 21, an explosion-proof mixer carbon dioxide inlet port 22 and an explosion-proof mixer discharge port 25.
[0042] Using the above device, combined with Figure 1 The present invention provides a method for spraying a thin layer of material using supercritical carbon dioxide for mining, which specifically includes the following steps:
[0043] Step 1: prepare solid phase materials and place them in an explosion-proof mixer. The solid phase materials include cement and light calcium carbonate. The solid phase materials in the explosion-proof mixer are fully mixed and stirred to make the two mixed evenly.
[0044] Prepare liquid phase materials, the liquid phase materials include polymer, additives and water, mix the liquid phase materials evenly and place them in a liquid phase material storage tank;
[0045] The above polymer is in powder or liquid form, specifically resin liquid, and according to weight, the polymer is 50-70 parts, the additive is 5-10 parts, and the water is 20-40 parts. The additive includes a water reducing agent, a film-forming agent, a defoaming agent and cellulose.
[0046] In the admixture, the weight ratio of water reducing agent, film-forming agent, defoaming agent and cellulose is 1-2:2-3:4-6:1-2.
[0047] More specifically, the water reducing agent is a polycarboxylic acid water reducing agent, the film forming agent is a polyurethane resin, the defoaming agent is an organosilicon defoaming agent, and the cellulose is wood cellulose.
[0048] Step 2, heating the explosion-proof mixer and keeping stirring;
[0049] Step 3: Provide gaseous carbon dioxide through a carbon dioxide storage tank, pass the carbon dioxide into an explosion-proof mixer, and convert the gaseous carbon dioxide into supercritical carbon dioxide by temperature control and pressurization; the temperature is 32-50°C and the pressure is 7.4-20MPa.
[0050] Step 4: inputting liquid phase material into the explosion-proof mixer. In the explosion-proof mixer, the liquid phase material and the solid phase material are fully stirred and mixed under the environment of supercritical carbon dioxide to prepare a slurry of thin spraying material for mining; supercritical carbon dioxide has both solubility in liquid state and diffusivity in gas state, and this dual property can further promote the dispersion of polymer;
[0051] Step 5: The mining thin-shot material slurry in the explosion-proof mixer is sprayed out through a spray gun.
[0052] The present invention will be further described below in conjunction with specific embodiments.
[0053] Embodiment 1:
[0054] Step 1: Weigh 100 parts of solid materials, cement and light calcium carbonate respectively, and weigh 70 parts of liquid materials, including 10 parts of polymer, 10 parts of admixture, and 20 parts of water. Among the admixtures, the weight ratio of water reducer, film former, defoamer, and cellulose is 1:3:4:2. Place the prepared solid materials in an explosion-proof mixer, mix and stir thoroughly; place the liquid materials in a polymer storage tank.
[0055] Step 2: starting the explosion-proof mixer and heating it;
[0056] Step 3: Open the valve of the carbon dioxide storage tank and the outlet valve of the carbon dioxide explosion-proof delivery booster pump, and fill the explosion-proof mixer with carbon dioxide through the carbon dioxide explosion-proof delivery booster pump to increase the pressure in the explosion-proof mixer, so that the gas phase carbon dioxide becomes a supercritical state.
[0057] Step 4: open the valve of the liquid material storage tank and the discharge valve 32 of the liquid material explosion-proof conveying booster pump, inject the liquid material into the explosion-proof mixer through the liquid material explosion-proof conveying booster pump, and fully mix and stir the solid material, liquid material and supercritical carbon dioxide in the explosion-proof mixer through the explosion-proof motor and agitator to form a slurry of thin spraying materials for mining.
[0058] Step 5: Close the valve of the liquid material storage tank, the discharge valve of the liquid material explosion-proof conveying booster pump, the valve of the carbon dioxide storage tank, and the outlet valve of the carbon dioxide explosion-proof conveying booster pump in sequence to stop the injection of carbon dioxide and polymer.
[0059] Step 6: Open the explosion-proof mixer pressure relief valve to complete the pressure relief in the explosion-proof mixer, and recover the exhausted carbon dioxide through the explosion-proof gas recovery device.
[0060] Step 7. After the pressure relief is completed, close the explosion-proof mixer pressure relief valve, open the explosion-proof mixer discharge valve, and use the auger to transport the mixed mining thin-spray material to the thin-spray material explosion-proof delivery pump, and spray the thin-spray material to the desired position through the thin-spray material explosion-proof delivery pump and the spray gun.
[0061] The explosion-proof mixer described in the present invention is a high-temperature and high-pressure explosion-proof mixer.
[0062] Parts not described in the present invention can be implemented by referring to the existing technology.
[0063] Those skilled in the art should recognize that the above embodiments are only used to illustrate the present application and are not intended to be limiting of the present application. As long as they are within the spirit and scope of the present application, appropriate changes and modifications to the above embodiments are within the scope of protection claimed in the present application.
Claims
1. A method for spraying a thin layer of material using supercritical carbon dioxide for mining, characterized in that: The following steps are involved: Step 1: Prepare the required equipment The device comprises an explosion-proof mixer, the input end of the explosion-proof mixer is respectively connected to a carbon dioxide storage tank and a liquid material storage tank, and the output end of the explosion-proof mixer is connected to a spray gun; Step 2: prepare solid phase materials and place them in the explosion-proof mixer, wherein the solid phase materials include cement and light calcium carbonate, and fully mix and stir the solid phase materials in the explosion-proof mixer to make the two mixed evenly; Prepare a liquid material, the liquid material comprising a polymer, an additive and water, and place the liquid material in the liquid material storage tank; Step 3, heating the explosion-proof mixer and keeping stirring; Step 4: providing gaseous carbon dioxide through a carbon dioxide storage tank, and converting the gaseous carbon dioxide into supercritical carbon dioxide in an explosion-proof mixer by temperature control and pressurization; Step 5: Input the liquid phase material into the explosion-proof mixer. In the explosion-proof mixer, the liquid phase material and the solid phase material are fully stirred and mixed under the supercritical carbon dioxide environment to prepare a slurry of the thin-shot material for mining; Step 6: The mining thin-shot material slurry in the explosion-proof mixer is sprayed out through a spray gun.
2. The method for spraying a thin layer of material using supercritical carbon dioxide for mining according to claim 1, characterized in that: In step one, a carbon dioxide explosion-proof delivery booster pump is connected between the carbon dioxide storage tank and the explosion-proof mixer, a liquid material explosion-proof delivery booster pump is connected between the liquid material storage tank and the explosion-proof mixer; and a thin spray material explosion-proof delivery pump is connected between the explosion-proof mixer and the spray gun.
3. The method for spraying a thin layer of material using supercritical carbon dioxide for mining according to claim 1, characterized in that: In step one, the explosion-proof mixer includes an explosion-proof tank body, an agitator is arranged inside the explosion-proof tank body, an explosion-proof motor is arranged on the outer wall of the explosion-proof tank body, the agitator is driven to rotate by the explosion-proof motor, and the outside of the explosion-proof tank body is connected with an explosion-proof mixer exhaust port, an explosion-proof mixer pressure relief valve, a heater, a pressure gauge and a temperature gauge.
4. The method for spraying a thin layer of material using supercritical carbon dioxide for mining according to claim 1, characterized in that: In step 2, the polymer is powder or liquid, and the additives include a water reducing agent, a film-forming agent, a defoaming agent and cellulose.
5. The method for spraying a thin layer of material using supercritical carbon dioxide for mining according to claim 1, characterized in that: In step 4, the temperature is 32-50° C. and the pressure is 7.4-20 MPa.
6. The method for spraying a thin layer of material using supercritical carbon dioxide for mining according to claim 4, characterized in that: The polymer is a resin liquid, and according to weight parts, the polymer is 50-70 parts, the additive is 5-10 parts, and the water is 20-40 parts.
7. The method for spraying a thin layer of material using supercritical carbon dioxide for mining according to claim 6, characterized in that: In the additive, the weight ratio of the water reducing agent, the film-forming agent, the defoaming agent and the cellulose is 1-2:2-3:4-6:1-2.
8. The method for spraying a thin layer of material using supercritical carbon dioxide for mining according to claim 7, characterized in that: The water reducing agent is a polycarboxylic acid water reducing agent, the film forming agent is a polyurethane resin, the defoaming agent is an organic silicon defoaming agent, and the cellulose is wood cellulose.
Citation Information
Patent Citations
High-toughness thin spraying material for rapid sealing reinforcement of underground coal mine and using method of high-toughness thin spraying material
CN113800870A
Preparation method of flexible early-strength thin spraying material for reinforcing, supporting and sealing mine roadway
CN116376334A
Anti-cracking and anti-freezing cement-based material as well as preparation method and application thereof
CN116553880A
Supercritical carbon dioxide automatic spraying system
CN117000458A
Supercritical carbon dioxide spraying equipment
CN118287279A