By pretreatment, acidification and decolorization of soybean soap feet, the problem of dark color and low transparency of soybean acidic oil is solved, and soybean acidic oil with low acidity and low peroxide value is obtained. It is suitable for biodiesel production and improves the quality of raw materials .
Patent Information
- Application Number
- CN202410883241.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-03
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2044-07-03
AI Technical Summary
The existing soybean acidified oil has darker color and low transparency, which affects its application in biodiesel production, and has high acid value and peroxide value, affecting product quality.
After pretreatment and acidification of soybean soap feet, decolorization was used to use a modified adsorbent to obtain soybean acid oil with light color, high transparency, low acid value and low peroxide value. The pretreatment includes mixing soybean soap pins with sodium benzenesulfonate solution, adding concentrated sulfuric acid to the acidification treatment, and adsorbing with a modified adsorbent prepared by an aminosilane coupling agent and an amino acid-type surfactant.
The obtained soybean acidified oil has a light yellow appearance, an acidity of 35-41 mg/g, a peroxide value of 6.38-7.01 meq/kg, and a saponification value of 161-169 mg/g. It is suitable as a raw material for biodiesel and improves the quality of raw materials for biodiesel production.
Smart Images

Figure CN118909690A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of acidified oil, in particular to a preparation method and application of soybean acidified oil. Background Art
[0002] As a by-product of the vegetable oil processing industry chain, soybean acidified oil is produced during the soybean oil refining process. Specifically, soybean acidified oil is an oil resource extracted by acidifying the soap stock by-product formed during the soybean oil refining process. During the soybean oil refining process, the hydrated phospholipids, commonly known as "oil stock", will undergo a sulfuric acid-catalyzed acidification reaction step.
[0003] In current market applications, soybean acidified oil is mainly used to produce industrial-grade oleic acid or converted to stearic acid after hydrogenation. In both conversion pathways, whether to generate oleic acid or stearic acid, the soybean acidified oil must first be hydrolyzed to convert the neutral oil in it into a free fatty acid state, and then the soybean mixed fatty acids are obtained through a distillation process, and further processed into the desired end product on this basis.
[0004] The current soybean acidified oil is dark in color and not very transparent, which affects its use in subsequent processing, such as in biodiesel production.
[0005] In order to solve the technical problems of the prior art, the present application provides a preparation method and application of soybean acidified oil. Summary of the invention
[0006] In order to overcome the shortcomings of the prior art, the present application provides a method for preparing and applying soybean acidified oil, wherein the soap stock is pretreated, then acidolyzed, and finally decolorized to obtain an acidified oil with light color and high transparency. The acidified oil has low acid value, low peroxide value, and high saponification value, and can be used as biodiesel.
[0007] The technical solution adopted by this application to solve its technical problem is:
[0008] The first object of the present application is to provide a method for preparing soybean acidified oil, comprising the following steps:
[0009] (1) Pretreatment
[0010] The soybean soap stock and the sodium benzenesulfonate solution are fully mixed, then allowed to stand for separation, and the upper layer of the soap stock is collected;
[0011] (2) Acidification treatment
[0012] Heat the lower soap stock to 95-100℃, add concentrated sulfuric acid under stirring, and collect the upper oil layer after the reaction is completed;
[0013] (3) Decolorization
[0014] The upper oil layer and 0.05-0.08% by weight of the modified adsorbent of soybean soap stock are fully mixed and decolorized; after the decolorization, the mixture is filtered and allowed to stand for separation to obtain soybean acidified oil.
[0015] Preferably, in step (1), the mass concentration of the sodium benzenesulfonate solution is 0.1-0.5%; the amount of the sodium benzenesulfonate solution added is 0.1%-0.3% of the weight of the soybean soap stock.
[0016] Preferably, in step (1), the mixing is carried out at 50-60°C. In the present application, during the production process of soapstock, since it contains colloid-soluble hydrophilic impurities such as phospholipids, these impurities are prone to emulsification during hydration degumming. Emulsification will seriously affect the separation efficiency of oils and the quality of the final product. In the pretreatment, by fully mixing the soybean soapstock with the sodium benzenesulfonate solution, the surface charge of the dispersed phase particles of the soybean soapstock can be neutralized, the potential of the particles can be eliminated or reduced, and the hydration degree can be reduced, thereby reducing the emulsification phenomenon.
[0017] Preferably, in step (2), after adding concentrated sulfuric acid, when the pH of the lower water layer of the acidification reaction reaches 3-3.5, stop adding concentrated sulfuric acid and continue stirring for 2-3 hours; then add concentrated sulfuric acid until the oil phase and the water phase are clearly separated.
[0018] Preferably, the modified adsorbent is obtained by treating cellulose acetate with an aminosilane coupling agent and a surfactant.
[0019] Preferably, the aminosilane coupling agent is any one of 3-aminopropyldiethoxymethylsilane and γ-aminopropyltriethoxysilane.
[0020] Preferably, the surfactant is an amino acid surfactant, which is any one of sodium cocoyl glycinate and potassium cocoamide.
[0021] Preferably, the preparation method of the modified adsorbent comprises the following steps: fully mixing cellulose acetate, montmorillonite, aminosilane coupling agent, solvent, and sulfuric acid, and then performing a reflux reaction; after the reflux reaction is completed, adding a surfactant, and fully mixing to obtain a modified decolorant. In the present application, the modified decolorant contains montmorillonite and cellulose acetate, which have a large specific surface area and a porous structure, and can effectively adsorb pigments and odor substances in grease, thereby achieving a decolorization effect. Moreover, the aminosilane coupling agent in the modified decolorant can chemically combine with polar substances in grease, fix pigments and odor substances in grease by forming chemical bonds, and reduce the release of these substances. In addition, the surfactant component in the modified decolorant, such as an amino acid surfactant, can reduce the interfacial tension between grease and water, promote the dispersion of pigments and odor substances in grease, and help these substances contact and adsorb with the adsorbent. Through the decolorization treatment, the modified decolorant may also improve the oxidative stability of grease, reduce the oxidative deterioration of grease during storage and use, and extend the shelf life of grease.
[0022] More preferably, the weight ratio of the cellulose acetate, montmorillonite, aminosilane coupling agent and surfactant is 50:40:(30-40):(2-3).
[0023] The second purpose of the present application is to provide an application of soybean acidified oil, that is, to apply soybean acidified oil to the preparation of biodiesel.
[0024] The beneficial effects of the present invention are:
[0025] 1. The preparation method described in the present application effectively removes impurities and pigments in oils and reduces acidity through a series of steps such as pretreatment, acidification, and decolorization. The obtained soybean acidified oil has a light yellow appearance, an acidity of 35-41 mg / g, a peroxide value of 6.38-7.01 meq / kg, and a saponification value of 161-169 mg / g, showing the advantages of low acidity, low peroxide value and high saponification value.
[0026] 2. The soybean acidified oil prepared in the present application has low acidity and low peroxide value content, and is suitable as a raw material for biodiesel, thereby improving the quality of raw materials for biodiesel production. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] The present invention is further described below in conjunction with the accompanying drawings and embodiments.
[0028] Figure 1 The process flow chart of the preparation method described in this application. DETAILED DESCRIPTION
[0029] In order to facilitate the understanding of those skilled in the art, the present invention is further described below in conjunction with embodiments, and the contents mentioned in the implementation modes are not intended to limit the present invention.
[0030] As used herein, "and / or" includes the term of any and all combinations of one or more associated listed items. The terms used herein are only used to describe specific embodiments and are not intended to limit the present invention. As used herein, the singular forms "a", "an", "an" and "the" are also intended to include the plural forms, unless the context clearly indicates otherwise. It is further understood that "including", when used in this specification, specifies the stated features, integers, steps, operations, elements and / or compositions, but does not exclude the existence or addition of one or more other features, integers, steps, operations, elements, compositions and / or combinations thereof.
[0031] Unless otherwise defined, all terms (including technical and scientific terms) used herein have the same meaning as commonly understood by one of ordinary skill in the art to which the invention belongs. It is further understood that terms, such as defined in commonly used dictionaries, are interpreted in accordance with their meanings in the context of the relevant art and are not in an idealized or overly formal sense unless explicitly so defined herein.
[0032] The exemplary invention described herein may appropriately lack any one or more element limitations that are not specifically disclosed herein. Therefore, the terms "comprise", "include", "contain", etc. should be understood broadly and non-restrictively. In addition, the terminology used herein is used as a description, not a limitation, and it is unintentional to use these terminology expressions that do not include any equivalent characteristics, but only describe some of their characteristics, but various modifications are possible within the scope of the present invention according to the rights. Therefore, although the present invention has been specifically disclosed by preferred embodiments and optional features, the modifications disclosed herein to embody the changes of the present invention may be recorded by those skilled in the art, and such modifications and changes will be considered to be within the scope of the present invention.
[0033] The raw materials or reagents used in the embodiments of the present invention and the comparative examples are all purchased from mainstream manufacturers in the market. Those without indicating the manufacturer or the concentration are all analytically pure raw materials or reagents that can be routinely obtained, as long as they can play the expected role, there is no particular restriction. The instruments and equipment such as the reactor and rotary evaporator used in the present embodiment are all purchased from major manufacturers in the market, as long as they can play the expected role, there is no particular restriction. If specific techniques or conditions are not indicated in the present embodiment, the techniques or conditions described in the literature in this area or according to the product specification are carried out.
[0034] The soybean soap stock of the present application is obtained by alkali refining, and the general composition varies with the process, operation and raw materials; in the soybean soap stock, the weight content of saponified matter is 30-45%, the weight content of neutral oil is 20-30%, the total fatty acid is 40-50%, and the rest is water, a small amount of fat and free alkali. Specifically, the soybean soap stock in the embodiment has a saponified matter weight content of 32%, a neutral oil weight content of 21%, a total fatty acid of 43%, water 2%, and a small amount of fat and free alkali.
[0035] Example 1
[0036] A method for preparing soybean acidified oil comprises the following steps:
[0037] (1) Pretreatment
[0038] The soybean soap stock and the sodium benzenesulfonate solution are fully mixed at 50° C., and then allowed to stand for separation to collect the upper soap stock; the mass concentration of the sodium benzenesulfonate solution is 0.1%; and the amount of the sodium benzenesulfonate solution added is 0.1% of the weight of the soybean soap stock.
[0039] (2) Acidification treatment
[0040] Heat the lower soap stock to 95°C, and add concentrated sulfuric acid under stirring. After adding concentrated sulfuric acid, when the pH of the lower water layer of the acidification reaction reaches 3-3.5, stop adding concentrated sulfuric acid and continue stirring for 2 hours. Then add concentrated sulfuric acid until the oil phase and the water phase are clearly separated.
[0041] When the oil phase and the water phase are clearly separated and the reaction is finished, the upper oil layer is collected;
[0042] (3) Decolorization
[0043] The upper oil layer and 0.05% by weight of the modified adsorbent of soybean soap stock are fully mixed, and decolorized at 50°C; after the decolorization, the mixture is filtered and allowed to stand for separation to obtain soybean acidified oil.
[0044] Specifically, the preparation method of the modified adsorbent comprises the following steps:
[0045] Cellulose acetate (substitution degree of 1.72-1.95), montmorillonite, aminosilane coupling agent (3-aminopropyldiethoxymethylsilane), and solvent (ethanol / water: 80 / 20, w / w) were mixed, and then concentrated sulfuric acid was added to adjust the pH to 5-6, stirred for 3 hours, and refluxed for 5 hours; after the reaction, a surfactant (sodium cocoyl glycinate) was added and fully mixed for 3 hours to obtain a modified adsorbent. The weight ratio of cellulose acetate, montmorillonite, aminosilane coupling agent, surfactant, and solvent is 50:40:30:2:1000.
[0046] Example 2
[0047] A method for preparing soybean acidified oil comprises the following steps:
[0048] (1) Pretreatment
[0049] The soybean soap stock and the sodium benzenesulfonate solution are fully mixed at 60° C., then allowed to stand for separation, and the upper layer of the soap stock is collected; the mass concentration of the sodium benzenesulfonate solution is 0.5%; and the amount of the sodium benzenesulfonate solution added is 0.3% of the weight of the soybean soap stock.
[0050] (2) Acidification treatment
[0051] Heat the lower soap stock to 100°C, and add concentrated sulfuric acid under stirring. After adding concentrated sulfuric acid, when the pH of the lower water layer of the acidification reaction reaches 3-3.5, stop adding concentrated sulfuric acid and continue stirring for 3 hours. Then add concentrated sulfuric acid until the oil phase and the water phase are obviously separated.
[0052] When the oil phase and the water phase are clearly separated and the reaction is finished, the upper oil layer is collected;
[0053] (3) Decolorization
[0054] The upper oil layer and 0.08% by weight of the modified adsorbent of soybean soap stock are fully mixed, and decolorized at 60° C. After the decolorization, the mixture is filtered and allowed to stand for separation to obtain soybean acidified oil.
[0055] Specifically, the preparation method of the modified adsorbent comprises the following steps:
[0056] Cellulose acetate (substitution degree of 1.72-1.95), montmorillonite, aminosilane coupling agent (γ-aminopropyltriethoxysilane), solvent (ethanol / water: 80 / 20, w / w) were mixed, sulfuric acid was added, pH was adjusted to 5-6, stirred for 3 hours, and refluxed for 6 hours; after the reaction, a surfactant (cocoamide potassium) was added and mixed for 4 hours to obtain a modified adsorbent. The weight ratio of cellulose acetate, montmorillonite, aminosilane coupling agent, surfactant, and solvent was 50:40:40:3:1000.
[0057] Example 3
[0058] A method for preparing soybean acidified oil comprises the following steps:
[0059] (1) Pretreatment
[0060] The soybean soap stock and the sodium benzenesulfonate solution are fully mixed at 55° C., then allowed to stand for separation, and the upper layer of the soap stock is collected; the mass concentration of the sodium benzenesulfonate solution is 0.4%; and the amount of the sodium benzenesulfonate solution added is 0.2% of the weight of the soybean soap stock.
[0061] (2) Acidification treatment
[0062] Heat the lower soap stock to 98°C, and add concentrated sulfuric acid under stirring. After adding concentrated sulfuric acid, when the pH of the lower water layer of the acidification reaction reaches 3-3.5, stop adding concentrated sulfuric acid and continue stirring for 2.5 hours. Then add concentrated sulfuric acid until the oil phase and the water phase are obviously separated.
[0063] When the oil phase and the water phase are clearly separated and the reaction is finished, the upper oil layer is collected;
[0064] (3) Decolorization
[0065] The upper oil layer and 0.07% by weight of the modified adsorbent of soybean soap stock are fully mixed, and decolorized at 55° C. After the decolorization, the mixture is filtered and allowed to stand for separation to obtain soybean acidified oil.
[0066] Specifically, the preparation method of the modified adsorbent comprises the following steps:
[0067] Cellulose acetate (substitution degree of 1.72-1.95), montmorillonite, aminosilane coupling agent (γ-aminopropyltriethoxysilane), solvent (ethanol / water: 80 / 20, w / w) are mixed, sulfuric acid is added, pH is adjusted to 5-6, stirred for 3 hours, and refluxed for 5-6 hours; after the reaction, a surfactant (cocoamide potassium) is added and mixed for 3.5 hours to obtain a modified adsorbent. The weight ratio of cellulose acetate, montmorillonite, aminosilane coupling agent, surfactant, and solvent is 50:40:35:2.5:1000.
[0068] Example 4
[0069] A method for preparing soybean acidified oil comprises the following steps:
[0070] (1) Pretreatment
[0071] The soybean soap stock and the sodium benzenesulfonate solution are fully mixed at 60° C., then allowed to stand for separation, and the upper layer of the soap stock is collected; the mass concentration of the sodium benzenesulfonate solution is 0.1%; and the amount of the sodium benzenesulfonate solution added is 0.3% of the weight of the soybean soap stock.
[0072] (2) Acidification treatment
[0073] Heat the lower layer of soap stock to 95°C, and add concentrated sulfuric acid under stirring. After adding concentrated sulfuric acid, when the pH of the lower water layer of the acidification reaction reaches 3-3.5, stop adding concentrated sulfuric acid and continue stirring for 3 hours; then add concentrated sulfuric acid until the oil phase and the water phase are clearly separated.
[0074] When the oil phase and the water phase are clearly separated and the reaction is finished, the upper oil layer is collected;
[0075] (3) Decolorization
[0076] The upper oil layer and 0.06% by weight of the modified adsorbent of soybean soap stock are fully mixed, and decolorized at 55° C. After the decolorization, the mixture is filtered and allowed to stand for separation to obtain soybean acidified oil.
[0077] Specifically, the preparation method of the modified adsorbent comprises the following steps:
[0078] Cellulose acetate (substitution degree of 1.72-1.95), montmorillonite, aminosilane coupling agent (3-aminopropyldiethoxymethylsilane), and solvent (ethanol / water: 80 / 20, w / w) were mixed, sulfuric acid was added, pH was adjusted to 5-6, stirred for 3 hours, and refluxed for 5 hours; after the reaction, surfactant (sodium cocoyl glycinate) was added and mixed for 4 hours to obtain a modified adsorbent. The weight ratio of cellulose acetate, montmorillonite, aminosilane coupling agent, surfactant, and solvent was 50:40:30:2:1000.
[0079] Example 5
[0080] A method for preparing soybean acidified oil comprises the following steps:
[0081] (1) Pretreatment
[0082] The soybean soap stock and the sodium benzenesulfonate solution are fully mixed at 60° C., then allowed to stand for separation, and the upper layer of the soap stock is collected; the mass concentration of the sodium benzenesulfonate solution is 0.5%; and the amount of the sodium benzenesulfonate solution added is 0.1% of the weight of the soybean soap stock.
[0083] (2) Acidification treatment
[0084] Heat the lower soap stock to 100°C, and add concentrated sulfuric acid under stirring. After adding concentrated sulfuric acid, when the pH of the lower water layer of the acidification reaction reaches 3-3.5, stop adding concentrated sulfuric acid and continue stirring for 2 hours; then add concentrated sulfuric acid until the oil phase and the water phase are clearly separated.
[0085] (3) Decolorization
[0086] The upper oil layer and 0.05-0.08% by weight of the modified adsorbent of soybean soap stock are fully mixed, and decolorized at 60°C; after decolorization, the mixture is filtered and allowed to stand for separation to obtain soybean acidified oil.
[0087] Specifically, the preparation method of the modified adsorbent comprises the following steps:
[0088] Cellulose acetate (substitution degree of 1.72-1.95), montmorillonite, aminosilane coupling agent (γ-aminopropyltriethoxysilane), and solvent (ethanol / water: 80 / 20, w / w) were mixed, and then sulfuric acid was added to adjust the pH to 5-6, stirred for 3 hours, and refluxed for 5 hours; after the reaction, a surfactant (cocoamide potassium) was added and fully mixed for 4 hours to obtain a modified adsorbent. The weight ratio of cellulose acetate, montmorillonite, aminosilane coupling agent, surfactant, and solvent is 50:40:35:3:1000.
[0089] Comparative Example 1
[0090] A method for preparing soybean acidified oil, without pretreatment, and other conditions are the same as those in Example 1;
[0091] Comparative Example 2
[0092] A method for preparing soybean acidified oil, without decolorization, and other conditions are the same as those in Example 1;
[0093] Comparative Example 3
[0094] A method for preparing soybean acidified oil, comprising: in step (3), fully mixing the upper oil layer and 0.05% by weight of montmorillonite from soybean soap stock, and decolorizing at 50°C; filtering and standing for separation after decolorization to obtain soybean acidified oil. Other conditions are the same as those in Example 1;
[0095] The acidified oils prepared in Examples 1-5 and Comparative Examples 1-3 were subjected to the following performance tests, wherein:
[0096] ① The acid value shall be determined in accordance with GB5530-1985;
[0097] ② The determination of peroxide value (POV) shall be carried out in accordance with GB5538-85;
[0098] ③Saponification value: measured in accordance with GB / T5534-2008;
[0099] ④Appearance inspection, observation with naked eyes.
[0100] Table 1
[0101]
[0102] As can be seen from Table 1, the acidified oil described in the present application has a light yellow appearance, an acidity of 35-41 mg / g, a peroxide value of 6.38-7.01 meq / kg, and a saponification value of 161-169 mg / g, showing the advantages of low acidity, low peroxide value and high saponification value.
[0103] In Comparative Example 3, only conventional montmorillonite was used for decolorization. The appearance was dark yellow, the acidity was 68 mg / g, the peroxide value was 79.5 meq / kg, and the saponification value was 141 mg / g, showing the disadvantages of high acidity, significantly high peroxide value and low saponification value.
[0104] The above embodiments are preferred implementation schemes of the present invention. In addition, the present invention may also be implemented in other ways. Any obvious replacement without departing from the concept of the present invention is within the protection scope of the present invention.
Claims
1. A method for preparing soybean acidified oil, characterized in that: The following steps are involved: (1) Pretreatment The soybean soap stock and the sodium benzenesulfonate solution are fully mixed, then allowed to stand for separation, and the upper layer of the soap stock is collected; (2) Acidification treatment Heat the lower soap stock to 95-100℃, add concentrated sulfuric acid under stirring, and collect the upper oil layer after the reaction is completed; (3) Decolorization The upper oil layer and 0.05-0.08% by weight of the modified adsorbent of soybean soap stock are fully mixed and decolorized; after the decolorization, the oil is filtered and allowed to stand for separation to obtain soybean acidified oil.
2. The preparation method according to claim 1, characterized in that: In step (1), the mass concentration of the sodium benzenesulfonate solution is 0.1-0.5%; the amount of the sodium benzenesulfonate solution added is 0.1%-0.3% of the weight of the soybean soap stock.
3. The preparation method according to claim 1, characterized in that: In step (1), the mixing is carried out at 50-60°C.
4. The preparation method according to claim 1, characterized in that: In step (2), after adding concentrated sulfuric acid, when the pH of the lower water layer of the acidification reaction reaches 3-3.5, stop adding concentrated sulfuric acid and continue stirring for 2-3 hours; then continue to add concentrated sulfuric acid until the oil phase and the water phase are clearly separated.
5. The preparation method according to claim 1, characterized in that: In step (3), the modified adsorbent is obtained by treating cellulose acetate with an aminosilane coupling agent and a surfactant.
6. The preparation method according to claim 5, characterized in that: The aminosilane coupling agent is any one of 3-aminopropyldiethoxymethylsilane and γ-aminopropyltriethoxysilane.
7. The preparation method according to claim 5, characterized in that: The surfactant is an amino acid type surfactant.
8. The preparation method according to claim 5, characterized in that: The preparation method of the modified adsorbent comprises the following steps: fully mixing cellulose acetate, montmorillonite, aminosilane coupling agent, solvent and sulfuric acid, and then performing a reflux reaction; after the reflux reaction is completed, adding a surfactant and performing a full mixing to obtain a modified decolorizing agent.
9. The preparation method according to claim 5, characterized in that: The weight ratio of the cellulose acetate, montmorillonite, aminosilane coupling agent and surfactant is 50:40: (30-40):(2-3)。 10. An application of soybean acidified oil, characterized in that: The acidified oil prepared by the preparation method according to any one of claims 1 to 9 is applied to the preparation of biodiesel.
Citation Information
Patent Citations
Method for preparing acidic oil by using soapstock
CN109554230A
Preparation method of cottonseed oil stearic acid plant soap base
CN114106945A
Improvements in the Refining of Edible Oils
GB1198095A
Process for the removal of fatty acid from a hydrocarbon oxidate
GB1272111A
Method of cleaning recirculating zinc solutions of leaching from lignosulphonates
RU2718440C1
Cited By
Modified natural ester insulating oil special for power transformer and preparation method of modified natural ester insulating oil
CN119709287A
Production process for recovering acid oil and co-producing struvite by demulsifying and decomposing soapstock
CN121294075A
A production process of soapstock demulsification decomposition and recovery of acidified oil and coproduction of struvite
CN121294075B