Device and method for testing shear strength of straight section of FRP (Fiber Reinforced Plastic) stirrup

By designing the FRP stirrup shear tensile strength test device, the oblique cracks and stress states in concrete beams are simulated, and the FRP stirrup shear-tensile stress state testing problem in the existing technology is solved, and the FRP stirrup strength is achieved. accurate measurement and real simulation.

CN118913951APending Publication Date: 2024-11-08CSCEC-TAISEI CONSTR LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411321798.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-23
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The prior art lacks mechanical properties testing devices and methods for FRP stirrups under shear-tension stress state, making it difficult to accurately test their strength in concrete.

Method used

A test device for shear tensile strength of FRP stirrups linear segments is designed, including concrete test blocks, loading devices, FRP stirrups, inducing steel plates, steel cages and side limit devices. By simulating the oblique cracks and stress states in concrete beams, Longitudinal load and shear force are applied until the FRP stirrup breaks to measure its shear-tensile strength.

Benefits of technology

The mechanical properties of FRP stirrups under shear-tension stress are achieved, ensuring the accuracy and authenticity of the test results, reasonable force transmission path, easy access to materials and equipment, and easy processing, and simple testing methods.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118913951A_ABST
    Figure CN118913951A_ABST
Patent Text Reader

Abstract

The invention provides a device and method for testing the shear strength of an FRP stirrup linear segment, the device comprises a concrete test block, a loading device, an FRP stirrup, an induction steel plate, a reinforcement cage, a lateral confinement device and a roller, the loading device is connected to the concrete test block and is used for applying a longitudinal load to the two ends of the concrete test block; the FRP stirrups are embedded in the concrete test block, and a set included angle is formed between the plane where the FRP stirrups are located and the longitudinal load. The device and the method have the beneficial effects that the shearing-pulling force state of the FRP stirrup in the concrete is truly restored in the testing process, and the strength of the FRP stirrup in the state of simultaneously bearing the pulling force and the shearing force can be more accurately tested; the overall force transmission path is reasonable, and the whole process of generation, extension and widening of the oblique crack of the concrete beam of the building structure is truly simulated; the device is simple in overall structure and reasonable in stress mode, materials and equipment are common building materials which are easy to obtain and machine, and the device is easy to manufacture and use; the whole test method is simple and easy to control.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of building material testing, and in particular relates to a shear tensile strength testing device and a testing method for a straight segment of an FRP stirrup. Background Art

[0002] In recent years, fiber-reinforced polymer (FRP) bars have been increasingly used in buildings, bridges, underground engineering, marine engineering, tunnels, and civil engineering with special requirements. Fiber-reinforced polymer (FRP) bars have excellent properties such as corrosion resistance, light weight and high strength, electromagnetic insulation, good designability, and good fatigue performance. Using FRP stirrups to replace traditional steel bars can improve the stress performance and durability of concrete components. FRP stirrups have good application prospects in buildings in corrosive environments.

[0003] In the prior art, when concrete beams are subjected to shear, oblique cracks will be generated, so stirrups are required to pass through the oblique cracks to transmit force to enhance the shear performance of concrete beams. When FRP stirrups are used, the straight section of the FRP stirrups intersects with the oblique cracks at a certain angle, and at the intersection of the two, they are simultaneously subjected to tension parallel to the straight section of the FRP stirrups and shear perpendicular to the straight section of the FRP stirrups. This stress mode of being subjected to shear and tension at the same time is called shear-tension stress. Unlike steel bars, FRP is an anisotropic material with a lateral strength much lower than its longitudinal strength. When subjected to forces in two directions at the same time, its strength may decrease. The mechanical performance tests currently proposed for FRP bars focus on three aspects: the tensile strength and shear strength of linear FRP bars and the tensile strength of the curved section of the FRP stirrups. There is no mechanical performance test device and method for shear-tension stress of the straight section of the FRP stirrups. Summary of the invention

[0004] In order to solve the above technical problems, the present invention provides a shear-tension strength testing device and a testing method for a straight segment of an FRP stirrup, which realizes the testing of the mechanical properties of the FRP stirrup under a shear-tension stress state.

[0005] The technical solution adopted by the present invention is: a FRP stirrup straight segment shear strength test device, comprising:

[0006] Concrete test blocks;

[0007] A loading device, connected to the concrete test block, for applying a longitudinal load to both ends of the concrete test block;

[0008] The FRP stirrups are embedded in the concrete test block, and the plane where the FRP stirrups are located has a set angle with the longitudinal load.

[0009] Furthermore, the concrete test block includes a cantilever portion and a test portion, the cantilever portion is arranged at both ends of the test portion in the longitudinal direction and protrudes to both sides of the test portion; the loading device abuts against the protruding portion of the cantilever portion; and the FRP stirrup passes through the transverse center of the test portion.

[0010] Furthermore, the plane where the FRP stirrups are located is a vertical plane, and the FRP stirrups include at least two straight line segments extending in the horizontal direction.

[0011] Furthermore, it also includes an induction steel plate for inducing the location where cracks are generated; the induction steel plate is buried in the test part, relatively arranged on both sides of the vertical plane, and perpendicular to the longitudinal load.

[0012] Furthermore, the center of the straight line segment and the induction steel plate are aligned with the lateral center of the test portion.

[0013] Furthermore, it also includes a steel cage, which is buried in the concrete test block, and is relatively arranged on both sides of the induction steel plate and surrounded by the outside of the FRP stirrups.

[0014] Furthermore, it also includes a side limit device, which includes a side limit roller, a side limit steel plate and a connecting piece; the side limit steel plate is arranged on both sides of the test part; the side limit roller is arranged between the side limit steel plate and the test part, and is arranged at intervals along the longitudinal direction of the test part; the connecting piece connects the two side limit steel plates.

[0015] Furthermore, it also includes rollers, which are arranged at the bottom of the concrete test block and spaced apart along the longitudinal direction of the concrete test block.

[0016] Furthermore, the loading device includes a force sensor and a jack, and the force sensor is arranged at a driving end of the jack.

[0017] A method for testing the shear tensile strength of a straight segment of an FRP stirrup, using any of the above-mentioned devices for testing the shear tensile strength of a straight segment of an FRP stirrup, comprises the following steps:

[0018] Make concrete test block molds;

[0019] Making a steel cage and placing the steel cage on both sides of the transverse center line of the concrete test block mold;

[0020] Placing FRP stirrups inside the steel cage so that the angle between the plane where the FRP stirrups are located and the longitudinal center line of the concrete test block mold is the same as the preset angle;

[0021] Temporarily fix the induction steel plate on both sides of the FRP stirrups;

[0022] Casting concrete test blocks and performing curing, and removing the concrete mold after the curing is completed;

[0023] Placing a roller on a horizontal surface, and placing the concrete test block on the roller;

[0024] Installing side limit devices on both sides of the test portion of the concrete test block;

[0025] Installing a loading device on the cantilever portion of the concrete test block so that the loading device abuts against a protruding portion of the cantilever portion;

[0026] The loading device is operated until the FRP stirrups break.

[0027] The advantages and positive effects of the present invention are:

[0028] (1) The FRP stirrup straight segment shear tensile strength test device and test method proposed in the present application, compared with the prior art which only performs tensile strength test or shear strength test, can truly restore the shear-tension state of the FRP stirrup in concrete during the test process, thereby being able to more accurately test the strength of the FRP stirrup under both tensile and shear states;

[0029] (2) The overall force transmission path is reasonable. During the test, the load is applied by a jack, and the load is transmitted to the test part through the cantilever part, and then to the FRP stirrups. The steel cage is buried in the concrete to ensure reliable load transmission.

[0030] (3) By setting up an induction steel plate and artificially applying load to generate cracks, the location where the cracks appear is specified, and the entire process of the generation, extension, and widening of oblique cracks in concrete beams of building structures is realistically simulated.

[0031] (4) By setting a lateral limit device, the lateral relative displacement of the concrete block after cracking is limited to ensure that the direction in which the crack opens and widens is perpendicular to the crack edge;

[0032] (5) The FRP stirrups form a set angle with the longitudinal centerline of the concrete specimen. The size of this angle is the same as the angle between the oblique crack in the concrete beam and the horizontal direction. Therefore, when using this device for testing, oblique cracks in concrete beams with different inclination angles can be simulated, so that the crack development pattern during the test is consistent with that of the actual building structure concrete beam, and the relative geometric relationship between the crack and the stirrups is consistent.

[0033] (6) The overall structure of the device is simple, the stress mode is reasonable, and the materials and equipment are common, easy to obtain, and easy to process building materials, which are easy to make and use; the overall test method is simple and easy to control. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] Figure 1 It is a structural schematic diagram of a specific implementation of the present invention;

[0035] Figure 2 is an exploded view of a device according to a specific embodiment of the present invention;

[0036] Figure 3 It is a schematic diagram of the stress state of FRP stirrups according to a specific embodiment of the present invention;

[0037] Figure 4 is a top view of a specific implementation of the present invention;

[0038] Figure 5 is a top cross-sectional view of a specific implementation of the present invention;

[0039] Figure 6 It is a left side cross-sectional view of a specific implementation of the present invention.

[0040] In the figure:

[0041] 1. FRP stirrups 11. Straight line segment 2. Induction steel plate

[0042] 3. Steel cage 31, transverse steel bars 32, steel cage stirrups

[0043] 4. Concrete test block 41, test part 42, cantilever part

[0044] 5. Side limit device 51, side limit roller 52, side limit steel plate

[0045] 53. Connector 6. Loading device 61. Jack

[0046] 62, force sensor 7, roller 8, leveling pad

[0047] 9. Horizontal cracks DETAILED DESCRIPTION

[0048] The embodiments of the present invention are described below with reference to the accompanying drawings.

[0049] like Figure 1-Figure 2 As shown, the present invention proposes a FRP stirrup straight segment shear strength testing device, comprising a concrete test block 4, a loading device 6 and an FRP stirrup 1: wherein the loading device 6 is connected to the concrete test block 4, and is used to apply a longitudinal load to both ends of the concrete test block 4; the FRP stirrup 1 is buried in the concrete test block 4, and the plane where the FRP stirrup 1 is located has a set angle with the longitudinal load.

[0050] When the FRP stirrups 1 are applied to a concrete beam, the oblique cracks generated in the concrete beam usually extend obliquely upward from the bottom of the concrete beam, forming a certain angle between the straight section 11 of the FRP stirrups 1; in order to simulate the actual stress state of the FRP stirrups 1 in concrete, it is necessary to make the angle between the cracks generated during the test and the straight section 11 of the FRP stirrups 1 the same as that under the actual stress state.

[0051] The device applies a longitudinal load to the concrete test block 4 through the loading device 6. Specifically, the longitudinal load is a tensile load applied along the longitudinal direction of the concrete test block 4, so that the concrete test block 4 can produce cracks extending along its transverse direction. In other words, the direction of the crack is limited by the above technical solution; then, the plane where the FRP stirrups 1 are located is inclined to the longitudinal direction of the concrete test block 4 and buried in the concrete test block 4, so that the angle between the straight segment 11 of the FRP stirrups 1 and the transverse crack 9 of the concrete test block 4 can be the same as the angle between the straight segment 11 of the FRP stirrups 1 and the oblique crack under the actual stress state.

[0052] At this time, the FRP stirrup 1 is subjected to a tensile force L along its length and a shear force T along the extension direction of the transverse crack 9, that is, the shear-tensile force it bears is the same as the shear-tensile force borne by the straight section 11 of the FRP stirrup 1 in the actual state. By testing the load size applied when the FRP stirrup 1 breaks, the shear-tensile strength of the FRP stirrup 1 in the actual use state can be obtained.

[0053] The above-mentioned set angle θ is the angle between the straight section 11 of the FRP stirrup 1 and the longitudinal axis of the concrete test block 4. By setting the set angle to different values, the change in the shear strength of the straight section 11 of the FRP stirrup 1 when the angle between the oblique crack of the concrete and the straight section 11 of the FRP stirrup 1 is different can be tested, thereby providing a basis for the arrangement and design of the FRP stirrup 1 in the concrete beam.

[0054] Furthermore, if Figure 1 As shown, the concrete test block 4 includes a cantilever portion 42 and a test portion 41. The cantilever portions 42 are arranged at both ends of the test portion 41 in the longitudinal direction and protrude to both sides of the test portion 41; the loading device 6 abuts against the protruding portion of the cantilever portion 42; during the test, the cantilever portions 42 at both ends of the concrete test block 4 are subjected to loads of the same magnitude and opposite directions, so the most likely location for the transverse crack 9 to appear is the transverse center of the test portion 41, and the FRP stirrup 1 is arranged to pass through the transverse center of the test portion 41, ensuring that the straight section 11 of the FRP stirrup 1 intersects with the transverse crack 9, and the angle between the two meets the test requirements.

[0055] The specific shape of the concrete test block 4 is not limited here, as long as the loading device 6 can be installed; in a specific embodiment, Figure 1 and Figure 2As shown, the concrete test block 4 is in the shape of an "I" as a whole, and the cantilever parts 42 are in the shape of parallel rectangles as a whole, which are symmetrically arranged at the two ends of the test part 41; the loading devices 6 are respectively arranged on both sides of the test part 41, and their two ends respectively abut against the protruding parts of the two cantilever parts 42. When in use, the same magnitude of longitudinal load is applied to the cantilever parts 42 simultaneously, so that tensile stress is generated inside the concrete test block 4, and then a transverse crack 9 is generated that develops laterally along the test part 41.

[0056] Furthermore, the plane where the FRP stirrup 1 is located is a vertical plane, and the FRP stirrup 1 includes at least two straight segments 11 extending in the horizontal direction. This design can better simulate the actual state of the straight segment 11 intersecting with the oblique crack when the FRP stirrup 1 is used in a concrete beam, and at the same time facilitate the observation of the entire process of the transverse crack 9 being generated, extended, widened, and broken from the top of the concrete test block 4. Specifically, the longitudinal direction of the concrete test block 4 is its length direction, and the transverse direction of the concrete test block is its width direction. This design can make the transverse crack 9 penetrate the thickness direction of the concrete test block 4, and the development direction of the transverse crack 9 is along the longitudinal direction of the concrete test block 4. Preferably, the straight segment 11 of the FRP stirrup 1 has a sufficient length so that it has sufficient gripping force with the concrete test block 4 to prevent the FRP stirrup 1 from falling out of the concrete test block 4.

[0057] In another specific embodiment, both ends of the straight section 11 of the FRP stirrup 1 in the length direction extend to the cantilever portion 42 of the concrete test block 4, so the connection portion between the cantilever portion 42 and the test portion 41 is set as an inclined surface to allow a sufficient concrete protective layer to be provided around the FRP stirrup 1 to avoid the formation of weak portions with insufficient gripping force.

[0058] Furthermore, the FRP stirrup straight segment shear strength testing device proposed in the present application also includes an induction steel plate 2 for inducing the location where cracks occur; the induction steel plate 2 is buried in the test part 41, relatively arranged on both sides of the vertical plane where the FRP stirrup 1 is located, and perpendicular to the longitudinal load.

[0059] Specifically, Figure 3 , Figure 4 As shown, the induction steel plates 2 are respectively arranged on the left and right sides of the FRP stirrups 1, and the two induction steel plates 2 are symmetrically arranged, which are buried in the concrete test block 4, and the three sides are flush with the surface of the concrete test block 4; therefore, the cross-sectional shape of the concrete test block 4 between the two induction steel plates 2 is the smallest, forming a weak part of the concrete test block 4. When the concrete test block 4 is subjected to a longitudinal load, this part is first damaged to form a transverse crack 9, and then the FRP stirrups 1 at this part are simultaneously subjected to tension and shear force under the action of concrete, and are in a shear-tension stress state.

[0060] Through the above technical scheme, it is achieved that the location where the transverse crack 9 of the concrete test block 4 is generated is further limited between the two induced steel plates 2, ensuring that the straight section 11 of the FRP stirrup 1 intersects with the transverse crack 9 at a set angle to meet the test requirements, more accurately simulate the actual state of the straight section 11 of the FRP stirrup 1 in the concrete beam, make the overall test process easier to control, and obtain more accurate test results.

[0061] Preferably, the distance between the two induction steel plates 2 is not less than 50 mm.

[0062] Furthermore, the center of the straight segment 11 of the FRP stirrup 1 and the induction steel plate 2 are aligned with the transverse center of the test portion 41, so that the position where the transverse crack 9 of the concrete test block 4 is generated coincides with the transverse center of the test portion 41. Since the longitudinal load applied by the loading device 6 is symmetrical about the transverse center of the test portion 41, the position where the concrete test block 4 itself is most likely to break under stress is the transverse center of the test portion 41. However, since the generation of cracks is based on comprehensive factors, by setting the induction steel plate 2 to be aligned with the transverse center of the test portion 41, the interference of other factors can be eliminated to the greatest extent, and it is easier to ensure the generation position of the transverse crack 9; and by setting the center of the straight segment 11 of the FRP stirrup 1 at this position, the concrete bonding stress on both sides of the center of the straight segment 11 of the FRP stirrup 1 is symmetrical, which is more consistent with the stress condition of the straight segment 11 of the FRP stirrup 1 in the actual state, which is conducive to improving the accuracy of the test results.

[0063] Furthermore, if Figure 5 , Figure 6 As shown, the FRP stirrup straight segment shear strength testing device proposed in the present application also includes a steel cage 3, which is buried in the concrete test block 4 and is relatively arranged on both sides of the induction steel plate 2 and surrounded by the outside of the FRP stirrup 1.

[0064] Specifically, Figure 4 , Figure 5As shown, two steel cages 3 are symmetrically arranged relative to the transverse center of the test part 41, and their function is to reinforce the concrete test block 4; preferably, the steel cage 3 includes transverse steel bars 31 and steel cage stirrups 32, wherein the transverse steel bars 31 are arranged along the transverse direction of the concrete test block 4, and the length of the transverse steel bars 31 can be set as needed, preferably, they are arranged from the position close to the induction steel plate 2 to the cantilever part 42 at intervals to enhance the bending performance of the cantilever part 42, to ensure that the cracks of the concrete test block 4 do not develop too large during the loading process, and to avoid the damage of the cantilever part 42. The steel cage stirrups 32 are arranged around the transverse steel bars 31 at intervals along the length direction of the transverse steel bars 31 to limit the development of the transverse cracks 9 of the concrete test block 4 and effectively transmit the tension in the concrete test block 4. The force transmission path during the loading process is: loading device 6-cantilever part 42-test part 41-FRP stirrups 1, wherein the concrete of the test part 41 and the steel cage 3 are subjected to force together.

[0065] Preferably, the steel cage 3 is arranged in the middle of the thickness direction of the concrete test block 4, and the distance between it and the surfaces of the concrete test block 4 meets the requirements for the thickness of the steel bar protective layer. At the same time, in order to ensure that the thickness of the concrete wrapped around the FRP stirrups 1 meets the test requirements, the net spacing between the FRP stirrups 1 and the steel cage 3 is not less than 35 mm.

[0066] Furthermore, the FRP stirrup straight segment shear strength testing device proposed in the present application also includes a side limit device 5, which includes a side limit roller 51, a side limit steel plate 52 and a connecting piece 53; the side limit steel plate 52 is arranged on both sides of the test portion 41; the side limit roller 51 is arranged between the side limit steel plate 52 and the test portion 41, and is arranged at intervals along the longitudinal direction of the test portion 41; the connecting piece 53 connects the two side limit steel plates 52.

[0067] like Figure 3 As shown, under the test state without applying lateral constraints, the concrete test block 4 produces transverse cracks 9 under the action of the longitudinal load, and then the transverse cracks 9 continue to extend and widen, so that the straight section 11 of the FRP stirrup 1 inside it is simultaneously subjected to the tensile force L and the shear force T. At this time, under the action of the longitudinal load, the transverse cracks 9 of the concrete test block 4 open along the longitudinal X direction, and at the same time, the concrete test blocks 4 on both sides of the transverse cracks 9 will also move laterally along the Y direction, but in the actual use state, the concrete beam will basically not move laterally after the oblique cracks appear. Therefore, the present application sets a lateral constraint device 5 to prevent the concrete test block 4 from such lateral movement, and ensures that the direction in which the crack opens and widens is perpendicular to the crack edge, so as to simulate the stress state of the FRP stirrup 1 under the actual state, so as to achieve the accuracy of the test results.

[0068] Specifically, the length direction of the side limit roller 51 is arranged along the height direction of the concrete test block 4, and is evenly spaced along the longitudinal direction of the test section 41. The distance between adjacent side limit rollers 51 is not limited here and can be selected according to needs; the length of the side limit steel plate 52 along the longitudinal direction of the test section 41 is preferably the same as the longitudinal length of the test section 41 to achieve a better limiting effect; the upper and lower ends of the side limit steel plate 52 are provided with connecting holes, and the connecting holes are exposed to the outside of the concrete test block 4, and the connecting members 53 are made of high-strength bolts, which pass through the connecting holes of the side limit steel plates 52 on both sides of the test section 41 respectively, and are fixed to the side limit steel plates 52 by nuts; by tightening the nuts, the side limit steel plates 52 can clamp the side limit rollers 51 to limit the lateral movement of the concrete test block 4; at the same time, the setting of the side limit rollers 51 can reduce the friction between the concrete test block 4 and will not affect the longitudinal movement of the concrete test block 4 to reduce the test error.

[0069] Since the side limit rollers 51 and the side limit steel plates 52 are arranged on both lateral sides of the test section 41 , the loading device 6 is also arranged on both lateral sides of the test section 41 . To avoid mutual interference between the two, the loading device 6 is preferably arranged on the outside of the side limit steel plates 52 .

[0070] Furthermore, in order to facilitate the longitudinal movement of the concrete test blocks 4 on both sides of the transverse cracks 9, the FRP stirrup straight segment shear strength testing device proposed in the present application also includes a roller 7, which is arranged at the bottom of the concrete test block 4, and its length direction is arranged along the transverse direction of the concrete test block 4. Several rollers 7 are arranged at intervals along the longitudinal direction of the concrete test block 4 to reduce the friction when the concrete test block 4 is placed on the ground.

[0071] Preferably, a horizontal mat is also provided at the bottom of the roller 7, so that the concrete test block 4 is placed on a horizontal plane as a whole, so that the forces on various parts of the concrete test block are balanced, avoiding the influence of its own gravity on the test results, and ensuring the accuracy of the test results.

[0072] Further, the loading device 6 includes a force sensor 62 and a jack 61, and the force sensor 62 is arranged at the free end of the jack 61. Specifically, one end of the jack 61 abuts against the protruding part of the cantilever part 42 at one end of the test part 41, and the free end of the other end abuts against the force sensor 62; the other end of the force sensor 62 abuts against the protruding part of the cantilever part 42 at the other end of the test part 41, and the force sensor 62 and the jack 61 are fixed to the cantilever part 42 by abutting against the cantilever part 42, and transmit the longitudinal load to the cantilever part 42; preferably, the force sensor 62 and the jack 61 are arranged in the middle of the thickness direction of the concrete test block 4, so that the concrete test block 4 is subjected to balanced force in the thickness direction, and then the upper and lower parts of the straight section 11 of the FRP stirrup 1 are subjected to balanced force, which is conducive to ensuring the accuracy of the test results. The force sensor 62 can accurately identify the value of the longitudinal load applied by the jack 61. The force sensor 62 and the jack 61 are both electrically connected to the controller. The controller is preset with a loading program to control the jacks 61 on both sides to apply loads synchronously. During the loading process, the two force sensors 62 transmit the load values ​​to the controller. By observing the load values ​​displayed by the controller, it can be determined whether the loads applied by the two loading devices 6 are the same to ensure the accuracy of the test; at the same time, the controller stores the test data to facilitate the analysis of the test results.

[0073] In other specific embodiments, the loading device 6 can be selected as needed, and the shape of the concrete test block 4 is designed according to the loading device 6. For example, the loading device 6 can adopt a tensile test device, and the clamping mechanism of the tensile test device is clamped at both ends of the concrete test block 4, respectively, to simultaneously apply a tensile load to both ends of the concrete test block 4. In the loading process, the loading device 6 and the concrete test block 4 form a self-balancing structure, and there is no need to add a fixed structure, which is more convenient to use.

[0074] The second aspect of the present application further provides a method for testing the shear strength of a straight segment 11 of an FRP stirrup 1, using the above-mentioned FRP stirrup straight segment shear strength testing device, comprising the following steps:

[0075] (1) Making 4 concrete test block molds;

[0076] Specifically, in a specific embodiment, the mold of the concrete test block 4 is constructed into an "I" shape, and its shape and size are set according to the FRP stirrups 1 to be tested, so that the FRP stirrups 1 can be completely buried inside the concrete test block 4 and have a sufficient protective layer thickness.

[0077] Preferably, the concrete test block 4 mold is a standardized mold, which can be applied to the shear and tensile strength test of FRP stirrups 1 of the same specification to avoid the test error caused by the production of the concrete test block 4; at the same time, it can be used in a turnover manner to simplify the production process of the concrete test block 4.

[0078] Specifically, the concrete test block 4 mold includes four side plates and a bottom plate; during production, the concrete test block 4 mold is placed on a horizontal plane.

[0079] (2) making a steel cage 3 and placing the steel cage 3 on both sides of the transverse center line of the concrete test block 4 mold;

[0080] Specifically, the steel cage 3 extends from the transverse center line of the test part 41 of the concrete test block 4 to its cantilever part 42, and is located in the middle of the thickness direction of the concrete test block 4. The distance between it and each surface of the concrete test block 4 meets the requirements for the thickness of the steel bar protective layer; the steel cage 3 on both sides of the transverse center line of the concrete test block 4 mold is symmetrically arranged and temporarily fixed.

[0081] (3) Place the FRP stirrup 1 inside the steel cage 3 so that the angle between the plane where the FRP stirrup 1 is located and the longitudinal center line of the mold of the concrete test block 4 is the same as the preset angle θ;

[0082] Specifically, the FRP stirrup 1 is generally an enclosed rectangle, and its two longer straight segments 11 are used as test objects. Therefore, when placing the FRP stirrup 1, the plane where the FRP stirrup 1 is located is a vertical plane, and the straight segment 11 of the FRP stirrup 1 extends in the horizontal direction. At the same time, the angle between the vertical plane where the FRP stirrup 1 is located and the longitudinal center line of the mold of the concrete test block 4 is a preset angle θ. The center of the length of the straight segment 11 of the FRP stirrup 1 coincides with the transverse center line of the mold of the concrete test block 4.

[0083] (4) Temporarily fix the induction steel plate 2 on both sides of the FRP stirrup 1;

[0084] Specifically, the induction steel plate 2 is aligned with the transverse center line of the concrete test block 4 mold, and is symmetrically arranged on both sides of the FRP stirrups 1 relative to the longitudinal center line of the concrete test block 4 mold; preferably, the height of the induction steel plate 2 is the same as the height of the concrete test block 4 mold, its bottom end is placed on the bottom plate of the concrete test block 4 mold, and one side edge thereof is in contact with the side plate of the concrete test block 4 mold.

[0085] (5) pouring concrete test block 4 and curing it, and removing the concrete mold after the curing is completed;

[0086] (6) Place the roller 7 on a horizontal surface and place the concrete test block 4 on the roller 7;

[0087] Preferably, a leveling pad 8 is set on the ground, and a roller 7 is first placed on the leveling pad 8, with the length direction of the roller 7 being arranged along the transverse direction of the concrete test block 4, and a plurality of rollers 7 are evenly spaced; then the concrete test block 4 is placed on the roller 7;

[0088] (7) Install the side limit device 5 on both sides of the test portion 41 of the concrete test block 4;

[0089] Specifically, the side limit device 5 includes a side limit roller 51, a side limit steel plate 52 and a connecting member 53. In this embodiment, the connecting member 53 is a high-strength bolt. The upper and lower ends of the side limit steel plate 52 are provided with mounting holes that match the high-strength bolt. During installation, the side limit steel plate 52 is first fitted to the side of the test portion 41 of the concrete test block 4, and then the high-strength bolt is passed through the mounting hole to connect the side limit steel plates 52 on both sides. The nut is initially screwed on the high-strength bolt, but it is not locked at this time, so that a certain gap is maintained between the side limit steel plate 52 and the side of the test portion 41. Then the side limit roller 51 is inserted into the gap, and the nut is screwed so that the side limit steel plate 52 contacts the side limit roller 51 with the test portion 41 of the concrete test block 4, but it is not completely attached and is still in an adjustable state. Then the side limit roller 51 is adjusted so that it is perpendicular to the ground and the spacing is basically the same, and the nut is tightened to complete the installation of the side limit device 5.

[0090] (8) Install the loading device 6 on the cantilever portion 42 of the concrete test block 4 so that the loading device 6 abuts against the protruding portion of the cantilever portion 42;

[0091] Specifically, the loading device 6 includes a jack 61 and a force sensor 62. A cushion block is first set at the lower part of the position where the jack 61 and the force sensor 62 are to be installed, and then the jack 61 is placed on the cushion block, with its end opposite to the free end fitted to the cantilever portion 42 at one end of the testing portion 41. Then the jack 61 is fitted and placed on the free end of the jack 61, with the other end of the force sensor 62 facing the cantilever portion 42 at the other end of the testing portion 41. The jack 61 is operated to make the jack 61 and the force sensor 62 abut against the cantilever portion 42. After the cushion block is removed, the jack 61 and the force sensor 62 do not fall off due to the friction force, and the installation of the loading device 6 is completed.

[0092] (9) Operate the loading device 6 until the FRP stirrup 1 breaks.

[0093] Specifically, the jack 61 and the force sensor 62 are both electrically connected to the controller. The controller is preset with a loading program to control the jacks 61 on both sides to apply loads synchronously. During the loading process, the load values ​​of the two force sensors need to be monitored to ensure that the two are loaded synchronously so that the forces on both sides of the concrete test block 4 are balanced. The controller stores the growth and changes of the load values ​​applied during the test to facilitate the analysis of the test results.

[0094] The FRP stirrup straight segment shear-tension strength test device and test method proposed in this application, compared with the prior art that only conducts tensile strength test or shear strength test, can truly restore the shear-tension state of FRP stirrups in concrete during the test process, so that the strength of FRP stirrups under tension and shear can be tested more accurately; the overall force transmission path is reasonable, FRP stirrups are buried in the concrete test block, and the concrete transmits force to the FRP stirrups, which can truly simulate the force of concrete on FRP stirrups in actual building structures. By setting an induction steel plate, artificially applying load to generate cracks, the whole process of the generation, extension and widening of oblique cracks in concrete beams of building structures is truly simulated. By setting a side limit device, the lateral relative displacement of the concrete block after cracking is limited to ensure that the direction of crack opening and widening is perpendicular to the crack edge; the FRP stirrups and the longitudinal center line of the concrete test block form a set angle, and the size of the angle is the same as the angle between the stirrups and the oblique cracks in the concrete beam, so that the crack development mode of the actual building structure concrete beam and the relative geometric relationship between the cracks and the stirrups are consistent during the test. The overall structure of the device is simple, the force mode is reasonable, and the materials and equipment are common, easy-to-obtain and easy-to-process building materials, which are easy to make and use.

[0095] The embodiments of the present invention are described in detail above, but the contents described are only preferred embodiments of the present invention and cannot be considered to limit the scope of implementation of the present invention. All equivalent changes and improvements made within the scope of the present invention should still fall within the scope of the patent coverage of the present invention.

Claims

1. A FRP stirrup straight segment shear strength test device, characterized in that: include: Concrete test blocks; A loading device, connected to the concrete test block, for applying a longitudinal load to both ends of the concrete test block; The FRP stirrups are embedded in the concrete test block, and the plane where the FRP stirrups are located has a set angle with the longitudinal load.

2. The FRP stirrup straight segment shear strength testing device according to claim 1, characterized in that: The concrete test block comprises a cantilever portion and a test portion, wherein the cantilever portion is arranged at both ends of the test portion in the longitudinal direction and protrudes toward both sides of the test portion; the loading device abuts against the protruding portion of the cantilever portion; and the FRP stirrup passes through the transverse center of the test portion.

3. The FRP stirrup straight segment shear strength testing device according to claim 1 or 2, characterized in that: The plane where the FRP stirrups are located is a vertical plane, and the FRP stirrups include at least two straight line segments extending in the horizontal direction.

4. The FRP stirrup straight segment shear strength testing device according to claim 3, characterized in that: It also includes an induction steel plate for inducing the location where cracks are generated; the induction steel plate is buried in the test part, relatively arranged on both sides of the vertical plane, and perpendicular to the longitudinal load.

5. The FRP stirrup straight segment shear strength testing device according to claim 4, characterized in that: The center of the straight line segment and the induction steel plate are aligned with the lateral center of the test portion.

6. The FRP stirrup straight segment shear strength testing device according to claim 4 or 5, characterized in that: It also includes a steel cage, which is buried in the concrete test block, arranged on both sides of the induction steel plate, and surrounded by the outside of the FRP stirrups.

7. The FRP stirrup straight segment shear strength testing device according to claim 4 or 5, characterized in that: It also includes a side limit device, which includes a side limit roller, a side limit steel plate and a connecting piece; the side limit steel plates are arranged on both sides of the test part; the side limit rollers are arranged between the side limit steel plates and the test part, and are arranged at intervals along the longitudinal direction of the test part; the connecting piece connects the two side limit steel plates.

8. The FRP stirrup straight segment shear strength testing device according to claim 1, 2, 4, or 5, characterized in that: It also includes rollers, which are arranged at the bottom of the concrete test block and spaced apart along the longitudinal direction of the concrete test block.

9. The FRP stirrup straight segment shear strength testing device according to claim 2, characterized in that: The loading device comprises a force sensor and a jack, and the force sensor is arranged at the driving end of the jack.

10. A method for testing the shear strength of a straight segment of FRP stirrups, characterized in that: The FRP stirrup straight segment shear strength test device as claimed in any one of claims 1 to 9 comprises the following steps: Make concrete test block molds; Making a steel cage and placing the steel cage on both sides of the transverse center line of the concrete test block mold; Placing FRP stirrups inside the steel cage so that the angle between the plane where the FRP stirrups are located and the longitudinal center line of the concrete test block mold is the same as the preset angle; Temporarily fixing the induction steel plate on both sides of the FRP stirrups; Casting concrete test blocks and performing curing, and removing the concrete mold after the curing is completed; Placing a roller on a horizontal surface, and placing the concrete test block on the roller; Installing side limit devices on both sides of the test portion of the concrete test block; Installing a loading device on the cantilever portion of the concrete test block so that the loading device abuts against a protruding portion of the cantilever portion; The loading device is operated until the FRP stirrups break.