Ultraviolet light emitting diode

By using a composite structure of graphene layers sandwiching n-AlGaN layers in AlGaN-based ultraviolet light-emitting diodes, the lattice mismatch problem is solved, electron injection uniformity and radiative recombination efficiency are improved, and the luminous efficiency and heat dissipation performance of UV-LEDs are enhanced.

CN118919620APending Publication Date: 2024-11-08SUZHOU LABORATORY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410975593.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-19
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

In existing AlGaN-based ultraviolet light-emitting diodes, defects are numerous due to lattice mismatch and thermal expansion coefficient mismatch, which reduces crystal quality, electron concentration, conductivity, and current spreading capability, thus affecting luminous efficiency and uniformity.

Method used

A composite structure of graphene layers sandwiching n-AlGaN layers is adopted. Quasi-van der Waals epitaxial growth and dislocation filtering are used to reduce lattice mismatch, promote lateral current diffusion, and improve electron injection uniformity and radiative recombination efficiency.

Benefits of technology

It improves the luminous efficiency and luminous power of UV-LEDs, enhances heat dissipation performance, and extends device lifespan.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118919620A_ABST
    Figure CN118919620A_ABST
Patent Text Reader

Abstract

The invention discloses an ultraviolet light-emitting diode which sequentially comprises a substrate, a low-temperature AlN nucleating layer, a high-temperature AlN buffer layer, a non-doped AlGaN buffer layer, a composite n-type layer, a multi-quantum well active region, a p-type AlGaN layer, a p-type GaN ohmic contact layer, an n-type electrode arranged on the composite n-type layer and a p-type electrode arranged on the p-type GaN ohmic contact layer from bottom to top. Wherein the composite n-type layer is composed of a graphene layer, an n-AlGaN layer and a graphene layer. The composite layer formed by clamping the n-AlGaN layer with the two-dimensional graphene material with extremely high electron mobility is adopted as the n-type layer, lattice mismatch can be relieved, defects in the material are reduced, the crystal quality of the epitaxial layer is improved, rapid transverse expansion of electrons is facilitated, the electrons can be uniformly injected into a multi-quantum well active region, and the quantum efficiency is improved. And the photoelectric property of the ultraviolet light-emitting diode is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of manufacturing semiconductor optoelectronic materials and devices, and in particular to an ultraviolet light emitting diode. Background Art

[0002] AlGaN-based ultraviolet light emitting diodes (UV-LEDs) have the advantages of small size, high efficiency, long life, no pollution and easy integration, and have important applications in sterilization, medical diagnosis, high-density optical data storage and sensing. In order to gradually replace the toxic mercury lamp ultraviolet light source, it is necessary to develop UV-LEDs with higher luminous efficiency and higher luminous power. Figure 3 As shown, due to the lattice mismatch and thermal expansion coefficient mismatch between the AlGaN material and the substrate 201, the n-type AlGaN layer 205 and the multi-quantum well active region 206 in the AlGaN-based UV-LED prepared by the prior art, there are many defects in the AlGaN-based UV-LED, especially in the n-type AlGaN layer, and they extend to the multi-quantum well active region, reducing the crystal quality of the multi-quantum well active region material, thereby reducing the recombination efficiency of electrons and holes in the quantum well active region, affecting the luminous efficiency of the UV-LED. At the same time, the defects in the n-type AlGaN layer will also lead to an increase in the ionization energy of the n-type doped Si donor, making it difficult to activate the Si doped atoms in the n-type AlGaN layer, with a low electron concentration and low conductivity. In addition, defects will also reduce electron mobility, causing current congestion, making it impossible for electrons to be uniformly injected into the multi-quantum active region, reducing the luminous efficiency and uniformity of the UV-LED. Therefore, in order to obtain UV-LEDs with high luminous efficiency and high luminous power, it is urgent to improve the crystal quality, electron concentration, conductivity and current expansion capability of the n-AlGaN layer. Summary of the invention

[0003] Technical solution: To achieve the above purpose, the present invention adopts the following technical solution:

[0004] like Figure 1 and 2As shown, the present invention provides an ultraviolet light-emitting diode, comprising a substrate (101), a low-temperature AlN nucleation layer (102), a high-temperature AlN buffer layer (103), a non-doped AlGaN buffer layer (104), a lower graphene layer (1051), an n-AlGaN layer (1052), a composite n-type layer (105) composed of an upper graphene layer (1053), a multi-quantum well active region (106), a p-type AlGaN layer (107) and a p-type GaN ohmic contact layer (108), and an n-type electrode (109) arranged on the n-AlGaN layer (1052) and a p-type electrode (110) arranged on the p-type GaN ohmic contact layer (108); the lower graphene layer (1051), the n-type AlGaN layer (1052) and the upper graphene layer (1053) constitute a composite n-type layer (105).

[0005] Optionally, the thickness of the lower graphene layer (1051) is 0.3nm to 6nm; the thickness of the n-AlGaN layer (1052) is 200nm to 5000nm; and the thickness of the upper graphene layer (1053) is 0.3nm to 3nm.

[0006] Optionally, the substrate (101) is made of any material selected from the group consisting of silicon, sapphire, aluminum nitride, gallium nitride or silicon carbide in any crystal orientation.

[0007] Optionally, the low-temperature AlN nucleation layer (102) has a thickness of 5 nm to 20 nm; the high-temperature AlN buffer layer (103) has a thickness of 100 nm to 1000 nm; the non-doped AlGaN buffer layer (104) has a thickness of 50 nm to 5000 nm; the multi-quantum well active region (106) comprises a plurality of stacked multi-quantum well layer groups, wherein the multi-quantum well layer groups include Al x Ga 1-x N quantum well layer and Al y Ga 1-y N quantum barrier layers; the number K of the multi-quantum well layer groups satisfies: 5≤K≤20; the thickness of the p-type AlGaN layer (107) is 50nm-500nm; the thickness of the p-type GaN ohmic contact layer (108) is 20nm-200nm.

[0008] Optionally, the Al component in the non-doped AlGaN buffer layer (104) is 0.1 to 0.9; the Al component in the n-AlGaN layer (1052) is 0.1 to 0.8; the multi-quantum well active region (106) includes Al x Ga 1-x N quantum well layer and Al y Ga 1-yN quantum barrier layer, where 0 < x < y < 1; the Al component in the p-type AlGaN layer (107) is 0.1 to 0.8.

[0009] Optionally, the electron concentration in the composite n-type layer (105) is 1×10 18 cm -3 or higher; the hole concentration range in the p-type AlGaN layer (107) is 1×10 16 cm -3 ~5×10 19 cm -3 ; the hole concentration range in the p-type GaN ohmic contact layer (108) is 1×10 17 cm -3 ~1×10 20 cm -3 .

[0010] Beneficial effects:

[0011] (1) The present invention abandons the single n-AlGaN layer in the AlGaN-based UV-LED prepared by the prior art, but as shown in Figure 1 and Figure 2 , a composite n-type layer composed of graphene layers inserted above and below the n-AlGaN layer is adopted. The benefit of this is that on the one hand, the dislocations that have already formed in the underlying structure can be filtered, preventing their propagation to the multi-quantum well active region; on the other hand, due to the weak van der Waals force interaction along the graphene plane, group III nitrides such as AlGaN can grow on graphene in a quasi-van der Waals epitaxial manner, reducing the migration barrier of atoms and making atoms easier to diffuse, which can greatly alleviate the lattice mismatch problem and enable the subsequent epitaxially grown group III nitride thin film to have higher crystal quality.

[0012] (2) The electron mobility in graphene is less affected by temperature changes. It is known that the electron mobility in monolayer graphene can reach 15000 cm / (V·s) in the temperature range of 50 to 500 K, with super-strong conductivity. The present invention uses graphene layers to sandwich the n-AlGaN layer, and the upper graphene layer is in direct contact with the multi-quantum well active region. Therefore, the insertion of the graphene layer can promote the lateral diffusion of current, enable electrons to be uniformly injected into the active region, effectively alleviate the current congestion problem, increase the radiative recombination efficiency of electrons and holes in the active region, and thus improve the luminous efficiency and luminous power of the UV-LED.

[0013] (3) The high thermal conductivity of graphene is beneficial to improving the heat dissipation performance of the UV-LED, thereby extending the service life of the device. Description of the drawings

[0014] Figure 1A schematic diagram of the cross-sectional layer structure of a UV-LED provided by the present invention, wherein the numbers mean: a substrate 101, a low-temperature AlN nucleation layer 102, a high-temperature AlN buffer layer 103, a non-doped AlGaN buffer layer 104, a composite n-type layer 105 composed of a lower graphene layer 1051, an n-AlGaN layer 1052, and an upper graphene layer 1053, a multi-quantum well active region 106, a p-type AlGaN layer 107 and a p-type GaN ohmic contact layer 108, an n-type electrode 109, and a p-type electrode 110.

[0015] Figure 2 A schematic diagram of the three-dimensional structure of the composite n-type layer provided by the present invention, wherein the numbers mean: lower graphene layer 1051, n-AlGaN layer 1052, upper graphene layer 1053.

[0016] Figure 3 This is a schematic diagram of the cross-sectional layer structure of a UV-LED prepared using the prior art, in which the numbers mean: substrate 201, low-temperature AlN nucleation layer 202, high-temperature AlN buffer layer 203, undoped AlGaN buffer layer 204, n-type AlGaN layer 205, multi-quantum well active region 206, p-type AlGaN layer 207, p-type GaN ohmic contact layer 208, n-type electrode 209, and p-type electrode 210. DETAILED DESCRIPTION

[0017] In order to make the purpose, technical solutions and advantages of the present invention clearer, the embodiments of the present invention will be further described in detail below with reference to the accompanying drawings:

[0018] Figure 1 The figure shows a UV light emitting diode provided by the present invention, which comprises, from bottom to top, a c-plane sapphire substrate 101, a 10nm thick low-temperature AlN nucleation layer 102, an 800nm ​​thick high-temperature AlN buffer layer 103, a 1000nm thick non-doped Al 0.5 Ga 0.5 N buffer layer 104, 0.668 nm thick lower graphene layer 1051, thickness 600 nm, electron concentration 6×10 18 cm -3 Si-doped n-type Al 0.55 Ga 0.45 N layer 1052, 0.334nm thick upper graphene layer 1053, repeating period number 5, 2nm thick Al 0.5 Ga 0.5 N quantum well and 5nm thick Al 0.65 Ga 0.35 The multi-quantum well active region 106 of the N quantum barrier has a thickness of 100 nm and a hole concentration of 5×10 17 cm -3Mg-doped p-type Al 0.5 Ga 0.5 N layer 107, with a thickness of 150 nm and a hole concentration of 5×10 18 cm -3 A Mg-doped p-type GaN ohmic contact layer 108 , an n-type Ti / Au ohmic contact electrode 109 disposed on the composite n-type layer 105 , and a p-type Ni / Au ohmic contact electrode 110 disposed on the p-type GaN ohmic contact layer 108 .

[0019] Since the present invention provides a composite structure of a graphene material sandwiching an n-AlGaN layer as an n-type layer, group III nitrides such as AlGaN can be grown on the graphene material in a quasi-van der Waals epitaxial manner, which helps to reduce the migration barrier of Al atoms. Moreover, the insertion of the graphene layer can not only reduce the interaction force between the epitaxial layers distributed above and below it, and alleviate the lattice mismatch between the epitaxial layer and the substrate, but also filter the dislocations generated in the epitaxial layer below, prevent them from propagating to the multi-quantum well active area, and effectively release the stress generated in the epitaxial structure, thereby finally obtaining an AlGaN-based UV-LED with low dislocation density and high crystal quality. In addition, since the graphene material has an extremely high electron mobility, it can promote the lateral diffusion of current in the n-AlGaN layer, reduce current congestion, and evenly inject electrons into the multi-quantum well active area, increase the radiation recombination efficiency of electrons and holes, and improve the luminous efficiency and luminous power of the UV-LED.

[0020] It should be noted that the use of a graphene layer in direct contact with the non-doped AlGaN buffer layer 104 and the multi-quantum well active region 106 can reduce the interaction force between the n-AlGaN layer 1052 and the non-doped AlGaN buffer layer 104 and the multi-quantum well active region 106, greatly reducing the lattice mismatch between heterogeneous materials, and at the same time filtering the dislocations generated below to prevent the dislocations from extending to the multi-quantum well active region 106, thereby enhancing the recombination efficiency of electrons and holes in the multi-quantum well active region 106, thereby improving the luminous efficiency and luminous power of the UV-LED.

[0021] It should be noted that graphene has high thermal conductivity, so by providing the lower graphene layer 1051 and the upper graphene layer 1053, it is beneficial to improve the heat dissipation performance of the UV-LED, thereby extending the service life of the device.

[0022] The above is an exemplary and specific description of the present invention in conjunction with the accompanying drawings. Obviously, the implementation of the present invention is not limited to the above-mentioned methods. As long as the methods, concepts and technical solutions of the present invention are used to make various non-substantial improvements; or the above methods, concepts and technical solutions of the present invention are directly applied to other occasions without improvement, they are all within the scope of protection of the present invention.

Claims

1. An ultraviolet light emitting diode, It is characterized in that The invention comprises a composite n-type layer (105) composed of a substrate (101), a low-temperature AlN nucleation layer (102), a high-temperature AlN buffer layer (103), a non-doped AlGaN buffer layer (104), a lower graphene layer (1051), an n-AlGaN layer (1052), and an upper graphene layer (1053), a multi-quantum well active region (106), a p-type AlGaN layer (107), and a p-type GaN ohmic contact layer (108), and an n-type electrode (109) arranged on the n-AlGaN layer (1052) and a p-type electrode (110) arranged on the p-type GaN ohmic contact layer (108); the lower graphene layer (1051), the n-type AlGaN layer (1052), and the upper graphene layer (1053) constitute the composite n-type layer (105).

2. The ultraviolet light emitting diode according to claim 1, It is characterized in that The thickness of the lower graphene layer (1051) is 0.3nm to 6nm; the thickness of the n-AlGaN layer (1052) is 200nm to 5000nm; and the thickness of the upper graphene layer (1053) is 0.3nm to 3nm.

3. The ultraviolet light emitting diode according to claim 1, It is characterized in that The substrate (101) is made of any one of silicon, sapphire, aluminum nitride, gallium nitride or silicon carbide in any crystal orientation.

4. The ultraviolet light emitting diode according to claim 1, It is characterized in that The thickness of the low-temperature AlN nucleation layer (102) is 5nm to 20nm; the thickness of the high-temperature AlN buffer layer (103) is 100nm to 1000nm; the thickness of the non-doped AlGaN buffer layer (104) is 50nm to 5000nm; the multi-quantum well active region (106) comprises a plurality of stacked multi-quantum well layer groups, wherein the multi-quantum well layer groups include Al x Ga 1-x N quantum well layer and Al y Ga 1-y N quantum barrier layers; the number K of the multi-quantum well layer groups satisfies: 5≤K≤20; the thickness of the p-type AlGaN layer (107) is 50nm-500nm; the thickness of the p-type GaN ohmic contact layer (108) is 20nm-200nm.

5. The ultraviolet light emitting diode according to claim 1, It is characterized in that The Al component in the undoped AlGaN buffer layer (104) is 0.1 to 0.9; the Al component in the n-AlGaN layer (1052) is 0.1 to 0.8; the multiple quantum well active region (106) includes Al x Ga 1-x N quantum well layers and Al y Ga 1-y N quantum barrier layers, where 0 < x < y < 1; the Al component in the p-type AlGaN layer (107) is 0.1 to 0.

8.

6. The ultraviolet light emitting diode according to claim 1, It is characterized in that The electron concentration in the composite n-type layer (105) is 1×10 18 cm -3 or more; the hole concentration in the p-type AlGaN layer (107) is in the range of 1×10 16 cm -3 ~5×10 19 cm -3 The hole concentration in the p-type GaN ohmic contact layer (108) is in the range of 1×10 17 cm -3 ~1×10 20 cm -3 .