Light-emitting device and preparation method

By forming nanopore gallium nitride columns in the target area of ​​the buffer layer of the light emitting device, the problem of porous structure is solved, the stress relaxation effect and light extraction efficiency are improved, and the preparation of high-quality gallium nitride indium material is achieved. .

CN118919624AActive Publication Date: 2024-11-08XIAMEN UNIV +1

Patent Information

Application Number
CN202410977433.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-19
Publication Date
2024-11-08
Estimated Expiration
2044-07-19

AI Technical Summary

Technical Problem

The porous and relaxation degree of porous structures in existing light emitting devices is uneven, resulting in stress mismatch and reduced indium content, making it difficult to obtain high-quality gallium nitride epitaxial materials.

Method used

GaN columns embedded in array form are used to form gallium nitride columns in the target area of ​​the buffer layer, with nanopores on the gallium nitride columns, and nanopores are formed in combination with local ion implantation and electrochemical etching processes, and porous is embedded in the target area only. Structure, reduce the unevenness of porosity in large areas.

Benefits of technology

The gallium nitride column of nanopores reduces lattice mismatch stress, improves stress relaxation effect, incorporates more indium into the luminescent structure layer, reduces unevenness of stress relaxation degree, and provides support through the buffer layer to form an air gap. To improve light extraction efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118919624A_ABST
    Figure CN118919624A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of semiconductor photoelectric devices, and discloses a light-emitting device and a preparation method thereof.The light-emitting device comprises a substrate layer, a buffer layer, a porous structure and a light-emitting structure layer, the buffer layer is located on the surface of one side of the substrate layer, and the buffer layer is provided with a target area; the porous structure is embedded in the target area, the porous structure comprises a gallium nitride column, and the gallium nitride column is provided with nanopores; the light-emitting structure layer is located on the surface of the side, away from the substrate layer, of the gallium nitride column and comprises a first doped semiconductor layer, a light-emitting layer and a second doped semiconductor layer, the first doped semiconductor layer is located on the surface of the side, away from the substrate layer, of the gallium nitride column, and the light-emitting layer is located between the first doped semiconductor layer and the second doped semiconductor layer; the conductivity type of the first doped semiconductor layer is opposite to the conductivity type of the second doped semiconductor layer. According to the invention, the condition of non-uniform aperture caused by large-area porosity is reduced, and the condition of non-uniform stress relaxation degree is further reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of semiconductor optoelectronic devices, and in particular to a light-emitting device and a preparation method thereof. Background Art

[0002] In recent years, third-generation semiconductor materials represented by silicon carbide and gallium nitride have been widely used in optoelectronic devices. Among them, gallium nitride materials have been widely used in the field of light-emitting devices due to their advantages such as wide bandgap, good stability, strong radiation resistance and high temperature resistance.

[0003] For optoelectronic semiconductor devices, changing the indium content in the gallium nitride-based ternary alloy material can change the band gap width of the material and thus regulate the wavelength of light emission. In order to achieve red light wavelength, the indium content of the semiconductor needs to be increased. However, increasing the indium content of the semiconductor will affect the in-plane lattice constant of the semiconductor and cause a large lattice mismatch between indium nitride and gallium nitride in the semiconductor material. The lattice mismatch strain also causes a reduction in the indium content through the composition pull effect, making it difficult to obtain high-quality gallium nitride indium.

[0004] In order to obtain high-quality and high-indium-content gallium nitride indium epitaxial materials, the existing technical solution is to etch one or more planar layer structures in the device into porous layers, and use the porous layers to achieve stress relaxation to reduce lattice mismatch strain. However, large-area porous structures face the problem of uneven porosity due to differences in contact time with the electrolyte used in electrochemical etching, which also leads to uneven relaxation. Summary of the invention

[0005] In view of this, the present invention provides a light-emitting device and a preparation method thereof, so as to solve the problems of uneven porosity and uneven relaxation of the porous structure in the existing light-emitting device.

[0006] In a first aspect, the present invention provides a light emitting device, comprising:

[0007] substrate layer;

[0008] A buffer layer, the buffer layer is located on a surface of one side of the substrate layer, and the buffer layer has one or more target areas;

[0009] A porous structure, wherein the porous structure is embedded in the target area, the porous structure comprises gallium nitride columns arranged in an array, and the gallium nitride columns have nanopores;

[0010] A light-emitting structure layer, wherein the light-emitting structure layer is located on a side surface of the gallium nitride column away from the substrate layer, the light-emitting structure layer comprises a first doped semiconductor layer, a light-emitting layer and a second doped semiconductor layer, the first doped semiconductor layer is located on a side surface of the gallium nitride column away from the substrate layer, the light-emitting layer is located on a side surface of the first doped semiconductor away from the gallium nitride column, the second doped semiconductor layer is located on a side surface of the light-emitting layer away from the first doped semiconductor layer, and the conductivity type of the first doped semiconductor layer is opposite to the conductivity type of the second doped semiconductor layer.

[0011] Beneficial effects: The nanopores on the gallium nitride column can reduce the mismatch stress caused by the mismatch between the lattice constant of gallium nitride and the lattice constant of indium nitride; secondly, the nanopores in the gallium nitride column are conducive to stress relaxation, and due to the component pulling effect, more indium is incorporated into the light-emitting structure layer; thirdly, the porous structure is embedded only in the target area, which reduces the area of ​​the porous structure, thereby reducing the uneven pore size caused by large-area porosity, and further reducing the uneven degree of stress relaxation. At the same time, part of the buffer layer outside the target area can provide support between the buffer layer and the light-emitting structure layer, so that a greater degree of porosity can be achieved in the target area to form an air gap and achieve the effect of a reflector.

[0012] In an optional implementation, the depth of the gallium nitride column in the buffer layer is 0.1 μm-0.8 μm, the maximum width of the gallium nitride column is 5 μm-100 μm, and the distance between two adjacent gallium nitride columns is 1 μm-100 μm.

[0013] Beneficial effects: Avoid the failure of stress relaxation when the depth of the GaN column in the buffer layer is less than 0.1μm, and avoid the crystal damage caused by the formation of GaN when the depth of the GaN column in the buffer layer is greater than 0.8μm. The width of GaN must conform to the size of the light-emitting device, and the spacing between each GaN column must conform to the display spacing of the light-emitting device.

[0014] In an optional embodiment, the material of the light-emitting layer includes a mixture of gallium nitride, aluminum and indium.

[0015] By adding indium and aluminum elements into the light-emitting layer, gallium aluminum nitride and gallium indium nitride alloys can be formed. By changing the aluminum and indium components in the alloy, the wavelength range of light emission can be 200nm-1771nm, so that the spectral range corresponding to the band gap change of the gallium nitride-based semiconductor material can be from infrared light to ultraviolet light wave region, so as to be applied to multiple lighting fields with different wavelength requirements.

[0016] In an optional implementation, the light emitting structure layer is smaller than or equal to the area of ​​the target region.

[0017] The light emitting structure layer is smaller than or equal to the area of ​​the target region, that is, the light emitting structure layer is completely located on the indium gallium nitride column with nanopores. The nanopores on the indium gallium nitride can improve the scattering of light, thereby facilitating the improvement of the light extraction efficiency of the light emitting device.

[0018] In an optional embodiment, a non-porous layer is further included, wherein the non-porous layer is located between the gallium nitride column and the first doped semiconductor layer, and the material of the non-porous layer includes gallium nitride.

[0019] The non-porous layer is used to provide a smooth surface for the growth of the light-emitting structure layer, which is beneficial to ensuring the epitaxial crystallization quality of the light-emitting structure layer.

[0020] In an optional embodiment, a stress regulation layer is further included, wherein the stress regulation layer is located between the substrate and the buffer layer, the material of the stress regulation layer includes gallium nitride, and the thickness of the stress regulation layer is less than the thickness of the buffer layer.

[0021] The stress regulation layer is used to regulate the lattice mismatch stress and thermal stress caused by the difference in thermal expansion coefficients generated in the subsequent preparation and growth process of the light-emitting device structure layer; the stress regulation layer is used to regulate the large thermal stress generated by the large difference in thermal expansion coefficients between the silicon substrate and the gallium nitride material during the large cooling process after the material preparation and growth are completed.

[0022] In a second aspect, the present invention provides a method for preparing a light emitting device, comprising the following steps:

[0023] providing a substrate layer;

[0024] Forming a buffer layer on one side surface of the substrate layer, wherein the buffer layer has one or more target areas;

[0025] forming a porous structure in the target region, wherein the porous structure includes gallium nitride pillars embedded in the target region in an array, and the gallium nitride pillars have nanopores;

[0026] A light-emitting structure layer is formed on a surface of the gallium nitride column on a side away from the substrate layer, and the light-emitting structure layer includes a first doped semiconductor layer, a light-emitting layer and a second doped semiconductor layer. The first doped semiconductor layer is located on a surface of the gallium nitride column on a side away from the substrate layer, the light-emitting layer is located on a surface of the first doped semiconductor on a side away from the gallium nitride column, and the second doped semiconductor layer is located on a surface of the light-emitting layer on a side away from the first doped semiconductor layer. The conductivity type of the first doped semiconductor layer is opposite to that of the second doped semiconductor layer.

[0027] Beneficial effects: In the light-emitting device prepared by the above method, the nanopores in the gallium nitride column can reduce the mismatch stress caused by the mismatch between the lattice constant of gallium nitride and the lattice constant of indium nitride; secondly, the nanopores in the gallium nitride column are conducive to stress relaxation, and due to the component pulling effect, more indium is incorporated into the light-emitting structure layer; thirdly, the porous structure is embedded only in the target area, which reduces the area of ​​the porous structure, thereby reducing the uneven pore size caused by large-area porosity, and further reducing the uneven degree of stress relaxation.

[0028] In an optional embodiment, forming a porous structure in a target area on the buffer layer comprises:

[0029] A dielectric layer is disposed on a surface of the buffer layer facing away from the substrate layer, wherein the dielectric layer has a preset pattern, and the preset pattern includes a hole array composed of a plurality of through holes;

[0030] Using the dielectric layer as a mask, ions are injected into the buffer layer through the through holes in the hole array to form gallium nitride pillars;

[0031] Performing a porosification treatment on the gallium nitride column to form nanopores;

[0032] Among them, the material of the buffer layer includes one or more of gallium nitride, indium nitride, and gallium indium nitride, and the ions include one or more of silicon ions, germanium ions, boron ions, tellurium ions, iodine ions, carbon ions, phosphorus ions, arsenic ions, sulfur ions, antimony ions, and tin ions.

[0033] In an optional embodiment, the gallium nitride column is formed by a local ion implantation process, the depth of the ion implantation is 0.1 μm-0.8 μm, and the implantation ion concentration of the local ion implantation process is 10 18 Magnitude.

[0034] In an optional embodiment, the gallium nitride column is made porous by electrochemical etching process;

[0035] The parameters of the electrochemical etching process include: the electrolyte used includes oxalic acid, hydrofluoric acid or nitric acid, the concentration of the electrolyte is 0.1M-0.3M, the etching voltage is 8V-15V, and the negative electrode used includes a platinum electrode or a gold electrode.

[0036] In an optional embodiment, the method further includes: after forming the light emitting structure layer, removing the mask to the first doped semiconductor layer, and forming an electrode on the light emitting structure layer after partially removing the mask. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] In order to more clearly illustrate the specific implementation methods of the present invention or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0038] Figure 1 is a schematic flow chart of a method for preparing a light-emitting device according to an embodiment of the present invention;

[0039] Figure 2 is a schematic structural diagram of a light emitting device according to an embodiment of the present invention;

[0040] Figure 3 is a schematic structural diagram of a substrate layer in the preparation of a light-emitting device according to an embodiment of the present invention;

[0041] Figure 4 It is a schematic structural diagram of a substrate layer and a stress regulating layer in the preparation of a light-emitting device according to an embodiment of the present invention;

[0042] Figure 5 It is a schematic structural diagram of a substrate layer, a stress regulating layer, and a buffer layer in the preparation of a light-emitting device according to an embodiment of the present invention;

[0043] Figure 6 It is a schematic structural diagram of a substrate layer, a stress regulating layer, a buffer layer, and a dielectric layer in the preparation of a light-emitting device according to an embodiment of the present invention;

[0044] Figure 7 It is a schematic diagram of the structure of a substrate layer, a stress regulating layer, a buffer layer, a dielectric layer, and a gallium nitride column in the preparation of a light-emitting device according to an embodiment of the present invention;

[0045] Figure 8 It is a schematic structural diagram of a substrate layer, a stress regulating layer, a buffer layer, a dielectric layer, and a gallium nitride column with nanopores in the preparation of a light-emitting device according to an embodiment of the present invention;

[0046] Fig. 9 It is a schematic structural diagram of a substrate layer, a stress regulating layer, a buffer layer, a dielectric layer, a gallium nitride column with nanopores, and a non-porous layer in the preparation of a light-emitting device according to an embodiment of the present invention;

[0047] Fig.10 It is a schematic structural diagram of a substrate layer, a stress regulating layer, a buffer layer, a dielectric layer, a gallium nitride column with nanopores, a non-porous layer, and a first doped semiconductor layer in the preparation of a light-emitting device according to an embodiment of the present invention;

[0048] Fig.11It is a schematic structural diagram of a substrate layer, a stress regulating layer, a buffer layer, a dielectric layer, a gallium nitride column with nanopores, a non-porous layer, a first doped semiconductor layer, and a light-emitting layer in the preparation of a light-emitting device according to an embodiment of the present invention;

[0049] Fig.12 It is a schematic structural diagram of a substrate layer, a stress regulating layer, a buffer layer, a dielectric layer, a gallium nitride column with nanopores, a non-porous layer, a first doped semiconductor layer, a light-emitting layer, and a second doped semiconductor layer in the preparation of a light-emitting device according to an embodiment of the present invention;

[0050] Fig.13 It is a structural schematic diagram of a substrate layer, a stress regulating layer, a buffer layer, a portion of a dielectric layer, a gallium nitride column with nanopores, a non-porous layer, and a portion of a light-emitting structure layer in the preparation of a light-emitting device according to an embodiment of the present invention.

[0051] in,

[0052] 100, substrate layer;

[0053] 200, stress regulating layer;

[0054] 300, buffer layer;

[0055] 400, dielectric layer; 401, through hole;

[0056] 500, gallium nitride pillar; 501, nanopore;

[0057] 600, non-porous layer;

[0058] 700, a first doped semiconductor layer;

[0059] 800, luminous layer;

[0060] 900. A second doped semiconductor layer. DETAILED DESCRIPTION

[0061] The present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It is understood that the specific embodiments described herein are only used to explain the present invention, rather than to limit the present invention. It should also be noted that, for ease of description, only some structures related to the present invention are shown in the accompanying drawings, rather than all structures. In the following description, the description of known structures and technologies is omitted to avoid unnecessary confusion of the concept of the present invention. Various structural schematic diagrams according to embodiments of the present invention are shown in the accompanying drawings. These figures are not drawn to scale, and some details are magnified for the purpose of clear expression, and some details may be omitted. The shapes of various regions and layers shown in the figures and the relative sizes and positional relationships between them are only exemplary, and may be deviated due to manufacturing tolerances or technical limitations in practice, and those skilled in the art may additionally design regions / layers with different shapes, sizes, and relative positions according to actual needs. In the context of the present invention, when a layer / element is referred to as being "on" another layer / element, the layer / element may be directly on the other layer / element, or there may be an intermediate layer / element between them. In addition, if one layer / element is "on" another layer / element in one orientation, then when the orientation is reversed, the layer / element may be "below" the other layer / element.

[0062] Gallium nitride materials have the advantages of wide bandgap, good stability, strong radiation resistance and high temperature resistance, and are widely used in the field of light-emitting devices. For gallium nitride light-emitting devices, the electronic band gap of the semiconductor material can be changed by changing the indium content in the gallium nitride light-emitting device, and thereby the emission wavelength of the gallium nitride light-emitting device can be changed. At present, the demand for red wavelength light-emitting devices is huge, and in order to achieve red wavelength light, it is necessary to further increase the indium content in gallium nitride light-emitting devices.

[0063] The technical solution adopted in the related art is to etch an entire or multiple planar layer structures in the device into a porous layer, and achieve stress relaxation by using the porous layer to achieve an increase in the indium content. However, large-area porous structures face the problem of uneven porosity due to differences in contact time with the electrolyte used in electrochemical etching, which also leads to uneven relaxation.

[0064] An embodiment of the present invention provides a method for preparing a light emitting device, comprising the following steps:

[0065] S11: Figure 3 As shown, a substrate layer 100 is provided.

[0066] The substrate layer 100 may be made of sapphire, silicon carbide, single crystal silicon, or glass.

[0067] S12: Figure 5As shown, a buffer layer 300 is formed on one side surface of the substrate layer 100 , and the buffer layer 300 has one or more target areas.

[0068] A buffer layer 300 is formed on the substrate by vapor phase epitaxial growth technology, molecular beam epitaxial growth technology or other commonly used epitaxial growth technology. The buffer layer 300 can be selected from one or more of gallium nitride, aluminum nitride, and indium nitride. The surface of the buffer layer 300 facing away from the substrate layer 100 is divided into one or more target areas.

[0069] S13: Figure 8 As shown, a porous structure is formed in the target region on the buffer layer 300 , and the porous structure includes gallium nitride pillars 500 embedded in the target region in an array form, and the gallium nitride pillars 500 have nanopores 501 .

[0070] Any gallium nitride column 500 is embedded in the buffer layer 300. The gallium nitride column 500 with nanopores 501 can be directly formed in the buffer layer 300 through an ion implantation process combined with an electrochemical etching process, or can be formed in the buffer layer 300 through a photolithography exposure process, a vapor deposition process combined with an electrochemical etching process.

[0071] S14: Fig.12 As shown, a light-emitting structure layer is formed on the surface of the side of the gallium nitride column 500 away from the substrate layer 100, and the light-emitting structure layer includes a first doped semiconductor layer 700, a light-emitting layer 800 and a second doped semiconductor layer 900. The first doped semiconductor layer 700 is located on the surface of the side of the gallium nitride column 500 away from the substrate layer 100, the light-emitting layer 800 is located on the surface of the first doped semiconductor away from the gallium nitride column 500, and the second doped semiconductor layer 900 is located on the surface of the side of the light-emitting layer 800 away from the first doped semiconductor layer 700. The conductivity type of the first doped semiconductor layer 700 is opposite to that of the second doped semiconductor layer 900.

[0072] When the first doped semiconductor layer 700 is N-type doped, the first doped semiconductor layer 700 may be N-type doped gallium nitride, or N-type doped gallium nitride indium, and the second doped semiconductor layer 900 is the opposite P-type conductivity type, and the second doped semiconductor layer 900 may be P-type doped gallium nitride, or P-type doped gallium nitride indium; when the first doped semiconductor layer 700 is P-type doped, the second doped semiconductor layer 900 is the opposite N-type doping. The material of the light emitting layer 800 includes a mixture formed by gallium nitride, aluminum element, and indium element.

[0073] In the light-emitting device prepared by the above method, the nanopores 501 in the gallium nitride column 500 can reduce the mismatch stress caused by the mismatch between the lattice constant of gallium nitride and the lattice constant of indium nitride; secondly, the nanopores 501 in the gallium nitride column 500 are conducive to stress relaxation, and due to the component pulling effect, more indium is incorporated into the light-emitting structure layer; thirdly, the porous structure is embedded only in the target area, which reduces the area of ​​the porous structure, thereby reducing the uneven pore size caused by large-area porosity, and further reducing the uneven degree of stress relaxation.

[0074] The method for preparing the light emitting device of this embodiment will be described in detail below. Figure 1 As shown, the following steps are included:

[0075] S1: Figure 3 As shown, sapphire is selected as the substrate layer 100.

[0076] S2: Figure 4 As shown, a low-temperature gallium nitride layer is formed on a sapphire substrate using a vapor phase epitaxial growth technique. Figure 5 As shown, a U (Undoped) type GaN (undoped GaN) layer with a thickness of 1μm-100μm is grown on the surface of the low-temperature GaN layer away from the sapphire substrate. There is a large lattice mismatch and thermal mismatch between the U-type GaN and the sapphire substrate. Using low-temperature GaN or AlN as a buffer layer can provide a better growth template for the subsequent epitaxy of nitrides, and improve the crystal quality of the GaN epitaxial layer to a certain extent.

[0077] S3: Figure 6 As shown, a silicon dioxide dielectric layer 400 is grown on the surface of the U-shaped gallium nitride layer away from the low-temperature gallium nitride layer. The silicon dioxide dielectric layer 400 has a preset pattern. The preset pattern includes a hole array composed of a plurality of through holes 401. Any through hole 401 can be a circular hole, a regular hexagonal hole, a square hole, an elliptical hole or other common through holes 401. The target area can be divided on the buffer layer 300 by the preset pattern; Figure 7 As shown, with the silicon dioxide dielectric layer 400 as a mask, a local ion implantation process is used to implant ions into the buffer layer 300 through the through hole 401 in the hole array to form a gallium nitride column 500. The implanted ions include one or more of silicon ions, germanium ions, boron ions, tellurium ions, iodine ions, carbon ions, phosphorus ions, arsenic ions, sulfur ions, antimony ions, and tin ions. The depth of the ion implantation is 100nm-800nm. The implanted ion concentration of the local ion implantation process is 10 18 The GaN column 500 is adapted to the shape of the corresponding through hole 401, and the GaN column 500 can be a cylinder, a hexagonal prism, a cuboid, an elliptical column or other prisms. Figure 8As shown, the gallium nitride column 500 is subjected to a porous treatment by an electrochemical etching process to form a gallium nitride column 500 having nanopores 501. The plurality of nanopores 501 are distributed in the gallium nitride column 500. Any nanopore 501 is a dendrite-shaped hole. In an alternative embodiment, the nanopore 501 may also be a circular hole, an elliptical hole or other common hole shapes. The specific conditions of the electrochemical etching process are: the electrolyte used includes oxalic acid, hydrofluoric acid or nitric acid, the concentration of the electrolyte is 0.1M-0.3M, M is mol / L, the etching voltage is 8V-15V, V is volts, and the negative electrode used includes a platinum electrode or a gold electrode.

[0078] S4: Fig. 9 As shown, a non-porous layer 600 is grown on the surface of the gallium nitride column 500 with nanopores 501 facing away from the substrate. The material of the non-porous layer 600 includes one or more of gallium nitride, indium nitride, and gallium indium nitride. Fig.10 As shown, N-type doped gallium nitride is grown on the surface of the non-porous layer 600 facing away from the substrate layer 100, as shown in FIG. Fig.11 As shown, a light emitting layer 800 is grown on the surface of the N-type doped gallium nitride away from the non-porous layer 600. The light emitting layer 800 may be one or more quantum wells, and the quantum wells are gallium nitride indium / gallium nitride quantum wells, such as Fig.12 As shown, a P-type doped gallium nitride layer is grown on the surface of the light emitting layer 800 which is away from the first doped semiconductor layer 700 .

[0079] S5: Fig.13 As shown, after the light-emitting structure layer is prepared, table etching is performed to remove the mask to the first doped semiconductor layer 700, and partially remove the P-type doped gallium nitride layer, the light-emitting layer 800 and the N-type doped gallium nitride layer, by etching silicon dioxide to the N-type gallium nitride layer, and preparing the electrode.

[0080] This embodiment also provides a light emitting device, such as Figure 2 and Fig.13As shown, it includes a substrate layer 100, a buffer layer 300, a porous structure and a light-emitting structure layer, the buffer layer 300 is located on one side surface of the substrate layer 100, and the buffer layer 300 has one or more target areas; the porous structure is embedded in the target area, the porous structure includes gallium nitride columns 500 arranged in an array form, and the gallium nitride columns 500 have nanopores 501; the light-emitting structure layer is located on the side surface of the gallium nitride columns 500 away from the substrate layer 100, the light-emitting structure layer includes a first doped semiconductor layer 700, a light-emitting layer 800 and a second doped semiconductor layer 900, the first doped semiconductor layer 700 is located on the side surface of the gallium nitride column 500 away from the substrate layer 100, the light-emitting layer 800 is located on the side surface of the first doped semiconductor away from the gallium nitride column 500, the second doped semiconductor layer 900 is located on the side surface of the light-emitting layer 800 away from the first doped semiconductor layer 700, and the conductivity type of the first doped semiconductor layer 700 is opposite to the conductivity type of the second doped semiconductor layer 900.

[0081] Specifically, the substrate layer 100 is a sapphire substrate, the buffer layer 300 is U-type gallium nitride, the first doped semiconductor layer 700 is N-type doped gallium nitride, and the second doped semiconductor layer 900 is P-type doped gallium nitride. In the above-mentioned light-emitting device, the nanopores 501 in the gallium nitride column 500 can reduce the mismatch stress caused by the mismatch between the lattice constant of gallium nitride and the lattice constant of indium nitride, and because the nanopores 501 enhance the scattering of light, it is beneficial to improve the light extraction efficiency of the light-emitting device; secondly, the nanopores 501 in the gallium nitride column 500 are conducive to stress relaxation, and due to the component pulling effect, more indium is incorporated into the light-emitting structure layer; thirdly, the porous structure is embedded only in the target area, which reduces the area of ​​the porous structure, thereby reducing the uneven pore size caused by large-area porosity, and further reducing the uneven degree of stress relaxation. At the same time, part of the buffer layer 300 outside the target area can provide support between the buffer layer 300 and the light-emitting structure layer, so that the target area can be more porous to form an air gap to achieve the effect of a reflector.

[0082] In one embodiment, the depth of the gallium nitride column 500 in the buffer layer 300 is 0.1 μm-0.8 μm, such as 0.1 μm, 0.5 μm, 0.7 μm, 0.8 μm, the maximum width of the gallium nitride column 500 is 5 μm-100 μm, such as 1 μm, 6 μm, 15 μm, 50 μm, 100 μm, and the spacing between two adjacent gallium nitride columns 500 is 1 μm-100 μm, such as 1 μm, 8 μm, 24 μm, 50 μm, 100 μm. The advantage of the depth selected by the gallium nitride column 500 is to avoid the gallium nitride column being less than 0.1 μm in the buffer layer, which leads to the failure of stress relaxation, and also avoid the gallium nitride column being formed when the depth of the buffer layer is greater than 0.8 μm. The width of the gallium nitride should meet the size of the light-emitting device, and the spacing between each gallium nitride column should meet the display spacing of the light-emitting device.

[0083] In one embodiment, the material of the light-emitting layer 800 includes a mixture of gallium nitride, aluminum, and indium. Indium and aluminum are doped into the light-emitting layer 800 to form gallium nitride aluminum and gallium nitride indium alloys. By changing the aluminum and indium components in the alloy, the wavelength range of light emission can be 200nm-1771nm, so that the spectral range corresponding to the band gap change of the gallium nitride-based semiconductor material can be from infrared light to ultraviolet light wave region, so as to be applied to multiple lighting fields with different wavelength requirements.

[0084] In one embodiment, the light emitting structure layer is smaller than or equal to the area of ​​the target region. The light emitting structure layer is smaller than or equal to the area of ​​the target region, that is, the light emitting structure layer is completely located on the gallium nitride indium column with nanoholes 501. The nanoholes 501 on the gallium nitride indium can improve the scattering of light, thereby facilitating the improvement of the light extraction efficiency of the light emitting device.

[0085] In one embodiment, a non-porous layer 600 is further included, and the non-porous layer 600 is located between the gallium nitride pillar 500 and the first doped semiconductor layer 700. The material of the non-porous layer 600 includes gallium nitride. The non-porous layer 600 is used to provide a smooth surface for the light emitting layer 800 to grow.

[0086] In one embodiment, a stress regulating layer 200 is further included, and the stress regulating layer 200 is located between the substrate and the buffer layer 300. The material of the stress regulating layer 200 includes gallium nitride, and the thickness of the stress regulating layer 200 is less than that of the buffer layer 300. The stress regulating layer 200 is used to regulate the lattice mismatch stress and thermal stress caused by the difference in thermal expansion coefficient generated in the subsequent preparation and growth process of the light-emitting device structure layer; the stress regulating layer 200 is used to regulate the large thermal stress generated by the large difference in thermal expansion coefficient between the silicon substrate and the gallium nitride material during the large temperature reduction process after the material preparation and growth are completed.

[0087] In the above description, the technical details of the patterning and etching of each layer are not described in detail. However, those skilled in the art should understand that various technical means can be used to form layers, regions, etc. of desired shapes. In addition, in order to form the same structure, those skilled in the art can also design methods that are not completely the same as the methods described above. In addition, although the various embodiments are described above separately, this does not mean that the measures in the various embodiments cannot be used in combination to advantage.

[0088] In the description of this specification, the description with reference to the terms "this embodiment", "one embodiment", "some embodiments", "example", "specific example", or "some examples" means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, unless they are contradictory.

[0089] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.

[0090] In the description of the present invention, it is to be understood that the terms “center”, “longitudinal”, “lateral”, “length”, “width”, “thickness”, “up”, “down”, “front”, “back”, “left”, “right”, “vertical”, “horizontal”, “top”, “bottom”, “inside”, “outside”, “clockwise”, “counterclockwise”, “axial”, “radial”, “circumferential”, etc., indicating orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.

[0091] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0092] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and simple improvements made to the essential contents of the present invention should be included in the protection scope of the present invention.

Claims

1. A light emitting device, It is characterized in that include: A substrate layer (100); A buffer layer (300), the buffer layer (300) being located on a surface of one side of the substrate layer (100), and having one or more target areas on the buffer layer (300); A porous structure, wherein the porous structure is embedded in the target area, the porous structure comprises gallium nitride columns (500) arranged in an array, and the gallium nitride columns (500) have nanopores (501); A light-emitting structure layer, wherein the light-emitting structure layer is located on a side surface of the gallium nitride column (500) away from the substrate layer (100), and the light-emitting structure layer comprises a first doped semiconductor layer (700), a light-emitting layer (800) and a second doped semiconductor layer (900), wherein the first doped semiconductor layer (700) is located on a side surface of the gallium nitride column (500) away from the substrate layer (100), the light-emitting layer (800) is located on a side surface of the first doped semiconductor away from the gallium nitride column (500), and the second doped semiconductor layer (900) is located on a side surface of the light-emitting layer (800) away from the first doped semiconductor layer (700), and the conductivity type of the first doped semiconductor layer (700) is opposite to the conductivity type of the second doped semiconductor layer (900).

2. The light emitting device according to claim 1, It is characterized in that The depth of the gallium nitride column (500) in the buffer layer (300) is 0.1 μm-0.8 μm, the maximum width of the gallium nitride column (500) is 5 μm-100 μm, and the distance between two adjacent gallium nitride columns (500) is 1 μm-100 μm.

3. The light emitting device according to claim 1 or 2, It is characterized in that The material of the light emitting layer (800) includes a mixture of gallium nitride, aluminum and indium.

4. The light emitting device according to claim 1 or 2, It is characterized in that The light emitting structure layer is smaller than or equal to the area of ​​the target region.

5. The light emitting device according to claim 1 or 2, It is characterized in that The invention also comprises a non-porous layer (600), wherein the non-porous layer (600) is located between the gallium nitride pillar (500) and the first doped semiconductor layer (700), and the material of the non-porous layer (600) comprises gallium nitride.

6. The light emitting device according to claim 1 or 2, It is characterized in that It also comprises a stress regulating layer (200), wherein the stress regulating layer (200) is located between the substrate and the buffer layer (300), the material of the stress regulating layer (200) comprises gallium nitride, and the thickness of the stress regulating layer (200) is less than the thickness of the buffer layer (300).

7. A method for preparing a light emitting device, It is characterized in that include: Providing a substrate layer (100); forming a buffer layer (300) on a surface of one side of the substrate layer (100), wherein the buffer layer (300) has one or more target areas; Forming a porous structure in the target area, the porous structure comprising gallium nitride columns (500) embedded in the target area in an array form, and the gallium nitride columns (500) have nanopores (501); A light-emitting structure layer is formed on a surface of the gallium nitride column (500) on a side away from the substrate layer (100), the light-emitting structure layer comprising a first doped semiconductor layer (700), a light-emitting layer (800) and a second doped semiconductor layer (900), the first doped semiconductor layer (700) being located on a surface of the gallium nitride column (500) on a side away from the substrate layer (100), the light-emitting layer (800) being located on a surface of the first doped semiconductor layer on a side away from the gallium nitride column (500), the second doped semiconductor layer (900) being located on a surface of the light-emitting layer (800) on a side away from the first doped semiconductor layer (700), and the conductivity type of the first doped semiconductor layer (700) and the conductivity type of the second doped semiconductor layer (900) being opposite.

8. The method for preparing a light emitting device according to claim 7, It is characterized in that Forming a porous structure in a target area on the buffer layer (300), comprising: A dielectric layer (400) is disposed on a surface of the buffer layer (300) facing away from the substrate layer (100), wherein the dielectric layer (400) has a preset pattern, and the preset pattern comprises a hole array composed of a plurality of through holes (401); Using the dielectric layer (400) as a mask, ions are injected into the buffer layer (300) through the through holes (401) in the hole array to form gallium nitride columns (500); Performing a porosification treatment on the gallium nitride column (500) to form a nanopore (501); The material of the buffer layer (300) includes one or more of gallium nitride, indium nitride, and gallium indium nitride, and the ions include one or more of silicon ions, germanium ions, boron ions, tellurium ions, iodine ions, carbon ions, phosphorus ions, arsenic ions, sulfur ions, antimony ions, and tin ions.

9. The method for preparing a light emitting device according to claim 8, It is characterized in that The gallium nitride column (500) is formed by a local ion implantation process, the depth of the ion implantation is 0.1 μm-0.8 μm, and the implantation ion concentration of the local ion implantation process is 10 18 Magnitude.

10. The method for preparing a light emitting device according to claim 9, It is characterized in that Using an electrochemical etching process to make the gallium nitride column (500) porous; The parameters of the electrochemical etching process include: the electrolyte used includes oxalic acid, hydrofluoric acid or nitric acid, the concentration of the electrolyte is 0.1M-0.3M, the etching voltage is 8V-15V, and the negative electrode used includes a platinum electrode or a gold electrode.

11. The method for preparing a light emitting device according to any one of claims 8 to 10, It is characterized in that Also includes: After forming the light emitting structure layer, the mask is removed to the first doped semiconductor layer (700), and an electrode is formed on the light emitting structure layer after removing part of the mask.

Citation Information

Patent Citations

  • Gallium nitride light-emitting diode structure and preparing method thereof

    CN103633211A

  • Semiconductor light-emitting element and wafer

    JP2012244154A

  • Semiconductor light emitting device and fabrication method thereof

    KR1020090030819A

  • High reflectivity MESA sidewall electrodes

    WO2022251143A1

Cited By

  • Semiconductor device and manufacturing method therefor, and electronic device

    WO2026103197A1