Flexible circuit board based on photosensitive PI and manufacturing method thereof

Through photosensitive PI, blind holes and windows are formed on the flexible circuit board, and metal seed layer electroplating is used to solve the problems of low efficiency and accuracy in traditional methods, and efficient internal and external layer conduction and welding functions are achieved, and the process flow is simplified. Improved product quality.

CN118921885APending Publication Date: 2024-11-08MFLEX YANCHENG CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411002876.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-25
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

In the field of flexible circuit boards, the traditional laser blind hole combination electroplating method is inefficient and has high operating risk. The process is complicated when using the combination of PI layer and glue layer as the protective film, and the production accuracy is low.

Method used

Blind holes and windows are formed on the line substrate using photosensitive PI, and outer lines are formed by electroplating of metal seed layer, and the photosensitive characteristics of photosensitive PI are used to remove unnecessary connection lines and protect unexposed areas to achieve the target circuit board Welding function and protection effect.

Benefits of technology

It improves the electrical conductivity of multi-layer flexible circuit boards, simplifies the process flow, reduces operating risks, and improves production accuracy and product yield.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118921885A_ABST
    Figure CN118921885A_ABST
Patent Text Reader

Abstract

The invention discloses a flexible circuit board based on photosensitive PI and a manufacturing method thereof. The method comprises the following steps: providing a circuit substrate after circuit manufacturing; respectively forming a blind hole for conduction and a window for welding on the circuit substrate by utilizing photosensitive PI (Polyimide) to obtain an inner-layer circuit board; manufacturing a metal seed layer on the inner-layer circuit board, and electroplating the inner-layer circuit board based on the metal seed layer, the blind hole and the window to form an outer-layer circuit to obtain a first semi-finished circuit board; removing the metal seed layer on the first semi-finished circuit board to obtain a second semi-finished circuit board; and exposing the window on the second semi-finished circuit board by using the photosensitive PI to obtain a target circuit board. According to the invention, by utilizing the photosensitive characteristic of the photosensitive PI and the insulation characteristic of the protective film, excellent electric conduction between layers of the multilayer flexible circuit board is realized, the manufacturing process is simple, the production efficiency is high, the operation risk is small, the manufacturing precision is high, and the product yield is high.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of flexible circuit board manufacturing, and in particular to a flexible circuit board based on photosensitive PI and a manufacturing method thereof. Background Art

[0002] Polyimide (PI) is one of the organic polymer materials with the best comprehensive performance. Due to its excellent electrical and thermodynamic properties, it has become the most widely used insulating material in modern high-tech products. In the field of flexible circuit boards, PI is mostly used as the insulating layer substrate. With the rapid development of science and technology, functionalized polyimide materials have also emerged. Liquid photosensitive polyimide (also known as photosensitive PI, hereinafter referred to as PSPI) is one of the materials with graphic properties. Due to its unique physical and chemical properties, it is often used as an insulating layer for semiconductor RDL packaging, but it has not been used in the field of flexible circuit boards.

[0003] In the field of flexible circuit boards, traditional multi-layer flexible circuit boards usually use laser blind holes combined with electroplating to achieve conduction between layers. The laser process is not only inefficient but also has high operating risks. It is also easy to cause problems such as unclean cleaning and damage to the bottom copper layer. In addition, the protective film of traditional flexible circuit boards is usually a combination of PI layer and glue layer. The pads that need to be welded in the later process (PAD for short) need to be punched out in advance to expose them. Ink printing, exposure and development and other processes are required to make the PAD meet the accuracy requirements. The process is complicated and the production accuracy is low. It is easy to fail to meet the accuracy requirements. Summary of the invention

[0004] In view of this, the present invention provides a flexible circuit board based on photosensitive PI and a method for manufacturing the same, so as to solve the problems of low efficiency, high operating risk, unclean cleaning, easy damage to the bottom copper layer, and complex process and low manufacturing precision when using a combination of PI layer and glue layer as a protective film in the prior art method of laser blind hole combined with electroplating.

[0005] The present invention provides a method for manufacturing a flexible circuit board based on photosensitive PI, comprising:

[0006] Providing a circuit substrate after circuit fabrication;

[0007] Using photosensitive PI, blind holes for conduction and windows for welding are formed on the circuit substrate to obtain an inner circuit board;

[0008] Making a metal seed layer on the inner circuit board, and electroplating the inner circuit board based on the metal seed layer, the blind holes and the openings to form an outer circuit to obtain a first semi-finished circuit board;

[0009] removing the metal seed layer on the first semi-finished circuit board to obtain a second semi-finished circuit board;

[0010] The photosensitive PI is used to expose the opening on the second semi-finished circuit board to obtain a target circuit board.

[0011] Optionally, the method of using photosensitive PI to form blind holes for conduction and windows for welding on the circuit substrate to obtain an inner circuit board includes:

[0012] Coating the photosensitive PI on the circuit substrate after circuit fabrication;

[0013] According to the preset circuit design, the circuit substrate coated with the photosensitive PI is processed by adopting the process of exposure, development and curing, and the blind holes and the openings are respectively formed on the circuit substrate to obtain the inner layer circuit board.

[0014] Optionally, the metal seed layer is at least one of a chromium metal layer, a titanium metal layer, an aluminum metal layer, a copper metal layer, a chromium-copper alloy layer, a copper-aluminum alloy layer, and a titanium-copper alloy layer.

[0015] Optionally, the thickness of the metal seed layer is in the range of 0.1 to 1 μm.

[0016] Optionally, the step of making a metal seed layer on the inner circuit board includes:

[0017] The metal seed layer is formed on the outer surface of the inner layer circuit board by using a vacuum sputtering process.

[0018] Optionally, electroplating the inner circuit board to form an outer circuit based on the metal seed layer, the blind hole and the window includes:

[0019] Pasting a dry film on the inner layer circuit board after vacuum sputtering, and covering the opening on the inner layer circuit board under the dry film;

[0020] Using an exposure and development process to process the inner layer circuit board after the dry film is applied;

[0021] The inner layer circuit board after exposure and development is processed by using a copper electroplating process, so that the blind holes on the inner layer circuit board are plated with a copper electroplating layer, and an outer layer circuit is formed on the outer surface of the inner layer circuit board.

[0022] Optionally, before removing the metal seed layer on the first semi-finished circuit board, the method further includes:

[0023] The inner layer circuit board after copper electroplating is subjected to dry film removal.

[0024] Optionally, the metal seed layer on the first semi-finished circuit board is removed to obtain a second semi-finished circuit board;

[0025] Provide etching solution of hydrogen peroxide-sulfuric acid system;

[0026] The first semi-finished circuit board is etched using the etching solution of the hydrogen peroxide-sulfuric acid system, so that the metal seed layer is etched away to obtain the second semi-finished circuit board.

[0027] Optionally, the step of using the photosensitive PI to expose the opening on the second semi-finished circuit board to obtain a target circuit board includes:

[0028] Applying the photosensitive PI on the outer surface of the second semi-finished circuit board;

[0029] The second semi-finished circuit board coated with the photosensitive PI is processed by using an exposure, development and curing process, so that the opening on the second semi-finished circuit board is exposed to obtain the target circuit board.

[0030] In addition, the present invention also provides a flexible circuit board based on photosensitive PI, which is manufactured using the aforementioned manufacturing method.

[0031] The beneficial effects of the present invention are as follows: the photosensitive PI has a photosensitive property and can be patterned. The photosensitive PI can be used to pattern the circuit substrate after the circuit is manufactured, so as to realize the formation of blind holes and windows. The blind holes are used for conduction between the inner and outer layer circuits, and the windows are used as pads for welding other components. Therefore, the photosensitive PI can be used to realize the manufacture of a complete inner layer circuit, and obtain an inner layer circuit board that meets the design requirements and has functionality; then, by manufacturing a metal seed layer on the inner layer circuit board, it is convenient to serve as a base for subsequent electroplating, so as to form an outer layer circuit on the inner layer circuit board, and realize the connection between layers of the multi-layer flexible circuit board. Conducting; then removing the metal seed layer, the unnecessary connection circuits on the first semi-finished circuit board can be removed, and a second semi-finished circuit board that meets the circuit design requirements can be obtained; finally, the photosensitive characteristics of the photosensitive PI are used again to process the second semi-finished circuit board, so that the area on the second semi-finished circuit board can be selectively exposed, thereby facilitating the exposure of the openings that need to be exposed on the second semi-finished circuit board, ensuring the welding function of the openings, and the photosensitive PI also has the protective characteristics of a protective film, based on which the photosensitive PI can protect the entire second semi-finished circuit board, ensuring the quality of the final target circuit board;

[0032] The flexible circuit board based on photosensitive PI of the present invention and the manufacturing method thereof utilize the photosensitivity of photosensitive PI and the insulating properties of the protective film to achieve excellent electrical conduction between layers in the multi-layer flexible circuit board, which effectively avoids the problems of low efficiency, high operating risk, unclean cleaning and easy damage to the bottom copper layer caused by the method of laser blind hole combined with electroplating, and also avoids the problems of complex process and low manufacturing precision caused by the process of punching the protective film when the combination of the traditional PI layer and the glue layer is used as a protective film. The manufacturing process is simple, the production efficiency is high, the operating risk is small, the manufacturing precision is high, and the product yield is high. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] The features and advantages of the present invention will be more clearly understood by referring to the accompanying drawings, which are schematic and should not be construed as limiting the present invention in any way. In the accompanying drawings:

[0034] Figure 1 A flow chart of a method for manufacturing a flexible circuit board based on photosensitive PI in Embodiment 1 of the present invention is shown;

[0035] Figure 2 The cross-sectional structure diagram of a single panel in the first embodiment of the present invention is shown;

[0036] Figure 3 The cross-sectional structure diagram of the circuit substrate in the first embodiment of the present invention is shown;

[0037] Figure 4 The cross-sectional structure diagram of the circuit substrate coated with photosensitive PI in the first embodiment of the present invention is shown;

[0038] Figure 5 The cross-sectional structure diagram of the inner layer circuit board obtained after exposure, development and curing in the first embodiment of the present invention is shown;

[0039] Figure 6 The cross-sectional structure diagram of the inner layer circuit board after vacuum sputtering in the first embodiment of the present invention is shown;

[0040] Figure 7 The cross-sectional structure diagram of the inner layer circuit board after dry film bonding, exposure and development in the first embodiment of the present invention is shown;

[0041] Figure 8 The cross-sectional structure diagram of the inner layer circuit board after copper electroplating in the first embodiment of the present invention is shown;

[0042] Fig. 9 The cross-sectional structure diagram of the second semi-finished circuit board obtained after etching in the first embodiment of the present invention is shown;

[0043] Fig.10 The cross-sectional structure diagram of the second semi-finished circuit board coated with photosensitive PI in the first embodiment of the present invention is shown;

[0044] Fig.11 The cross-sectional structure diagram of the target circuit board obtained in the first embodiment of the present invention is shown.

[0045] The description of each reference numeral is as follows:

[0046] 1. Substrate insulation layer, 2. Substrate copper, 3. First photosensitive PI layer, 4. Blind hole, 5. Window, 6. Metal seed layer, 7. Dry film, 8. Electroplated copper layer, 9. Second photosensitive PI layer. DETAILED DESCRIPTION

[0047] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present invention.

[0048] Embodiment 1

[0049] This embodiment provides a method for manufacturing a flexible circuit board based on photosensitive PI, such as Figure 1 As shown, including:

[0050] S1: Provide the circuit substrate after circuit manufacturing;

[0051] S2: using photosensitive PI, forming blind holes for conduction and openings for welding on the circuit substrate to obtain an inner circuit board;

[0052] S3: making a metal seed layer on the inner circuit board, and electroplating the inner circuit board based on the metal seed layer, the blind holes and the openings to form an outer circuit, thereby obtaining a first semi-finished circuit board;

[0053] S4: removing the metal seed layer on the first semi-finished circuit board to obtain a second semi-finished circuit board;

[0054] S5: using the photosensitive PI, exposing the opening on the second semi-finished circuit board to obtain a target circuit board.

[0055] Photosensitive PI has the photosensitive properties of dry film and can be patterned. Photosensitive PI can be used to pattern the circuit substrate after circuit production to achieve the formation of blind holes and windows. Blind holes are used for conduction between inner and outer layer circuits, and windows are used as pads for welding other components. Therefore, photosensitive PI can be used to achieve the production of complete inner layer circuits and obtain an inner layer circuit board that meets the design requirements and has functionality. Then, by making a metal seed layer on the inner layer circuit board, it is convenient to serve as a base for subsequent electroplating, so as to form an outer layer circuit on the inner layer circuit board and achieve conduction between layers of a multi-layer flexible circuit board. By removing the metal seed layer, unnecessary connection lines on the first semi-finished circuit board can be removed, and a second semi-finished circuit board that meets the circuit design requirements can be obtained; finally, the second semi-finished circuit board is processed by utilizing the photosensitive characteristics of the photosensitive PI again, so that areas on the second semi-finished circuit board can be selectively exposed, thereby facilitating the exposure of windows that need to be exposed on the second semi-finished circuit board, thereby ensuring the welding function of the windows. At the same time, the photosensitive PI also has the protective characteristics of a protective film. Based on the photosensitive PI, the entire second semi-finished circuit board can be protected to ensure the quality of the final target circuit board.

[0056] The method for manufacturing a flexible circuit board based on photosensitive PI in this embodiment utilizes the photosensitive properties of photosensitive PI and the insulating properties of the protective film to achieve excellent electrical conduction between layers in a multi-layer flexible circuit board, which effectively avoids the problems of low efficiency, high operating risk, unclean cleaning, and easy damage to the bottom copper layer caused by the method of laser blind hole combined with electroplating, and avoids the problems of complex process and low manufacturing precision caused by the need to perform protective film punching when the combination of traditional PI layer and glue layer is used as a protective film. The manufacturing process is simple, the production efficiency is high, the operating risk is small, the manufacturing precision is high, and the product yield is high.

[0057] The following describes in detail each step of the manufacturing method of this embodiment.

[0058] In S1, the circuit substrate is a flexible substrate that has been processed by circuit manufacturing. Circuit manufacturing generally refers to etching the flexible substrate according to the preset circuit design to form an inner layer circuit on the flexible substrate. Flexible substrates include single-sided boards, double-sided boards, and multi-layer boards, which are not limited in this embodiment. The preset circuit design depends on the specific product design, which generally includes circuit area, circuit layout, and circuit parameters. In addition to conventional circuits, these circuits also include blind holes and windows.

[0059] For the sake of convenience, the flexible substrate of this embodiment takes a single-sided board as an example, and its cross-sectional structure is as follows: Figure 2 As shown, it includes a substrate insulating layer 1 (usually a substrate PI) and a substrate copper 2. The cross-sectional structure of the circuit substrate obtained after the single-sided board is manufactured is as follows Figure 3For double-sided boards and multi-layer boards, the same method is used to make circuits on the side where the circuits need to be made, and the methods described in S2 to S5 of this embodiment are used to process the side where the circuits need to be made. The principle is the same as that of the single-sided board, and will not be repeated here.

[0060] Preferably, S2 includes:

[0061] S21: coating the photosensitive PI on the circuit substrate after circuit fabrication;

[0062] S22: According to the preset circuit design, the circuit substrate coated with the photosensitive PI is processed by adopting an exposure, development and curing process, and the blind holes and the openings are respectively formed on the circuit substrate to obtain the inner layer circuit board.

[0063] After the circuit is manufactured, photosensitive PI is coated on the circuit substrate, and the photosensitive characteristics of the photosensitive PI are utilized to perform exposure, development, and curing, so that blind holes and windows can be formed at required positions. The blind holes are used for conduction, so that conduction between the inner and outer layer circuits can be achieved. The windows are used for welding, so that welding between the entire circuit board and external electronic components can be achieved, thereby facilitating the acquisition of an inner layer circuit board that can form excellent electrical conduction with the outer layer. Among them, exposure, development, and curing according to the preset circuit design can effectively improve the manufacturing accuracy of the blind holes and windows.

[0064] The cross-sectional structure of the circuit substrate coated with photosensitive PI in this embodiment is as follows: Figure 4 As shown, the cross-sectional structure of the inner layer circuit board obtained after exposure, development and curing is as shown in Figure 5 As shown, in Figure 4 and Figure 5 In the figure, 3 is the first photosensitive PI layer, 4 is a blind hole, and 5 is an open window. Figure 5 The number of blind holes and windows is 1 each, but in actual production, the number of blind holes and windows is not limited to 1, depending on the specific product design.

[0065] Preferably, in S3, forming a metal seed layer on the inner layer circuit board includes:

[0066] S31: Using a vacuum sputtering process to form the metal seed layer on the outer surface of the inner layer circuit board.

[0067] The vacuum sputtering process can efficiently and accurately form a metal seed layer on the outer surface of the inner circuit board, providing a base for subsequent electroplating, thereby facilitating the formation of outer circuits and ensuring good electrical conductivity between the inner and outer layers of the final circuit board.

[0068] Specifically, the metal seed layer is at least one of a chromium metal layer, a titanium metal layer, an aluminum metal layer, a copper metal layer, a chromium-copper alloy layer, a copper-aluminum alloy layer, and a titanium-copper alloy layer.

[0069] The above materials are used as metal seed layers, which have the advantages of good electrical conductivity, thermal conductivity, corrosion resistance, ductility and reliability, and can facilitate subsequent electroplating, reduce electroplating defects, and help improve the production accuracy of subsequent electroplating. At the same time, it is also convenient to use simple processes to remove unnecessary connection lines in the future.

[0070] Specifically, the thickness of the metal seed layer is in the range of 0.1 to 1 μm.

[0071] The metal seed layer within the above thickness range can not only ensure that it plays a good base role in the subsequent electroplating, but also facilitate efficient removal by a simple process after the electroplating is completed.

[0072] The cross-sectional structure of the inner layer circuit board after vacuum sputtering in this embodiment is as follows: Figure 6 As shown, in Figure 6 In the figure, 6 is a metal seed layer.

[0073] Preferably, in S3, based on the metal seed layer, the blind hole and the opening, the inner layer circuit board is electroplated to form an outer layer circuit, comprising:

[0074] S32: pasting a dry film on the inner layer circuit board after vacuum sputtering, and covering the opening on the inner layer circuit board under the dry film;

[0075] S33: using an exposure and development process to process the inner layer circuit board after the dry film is applied;

[0076] S34: using a copper electroplating process to process the inner layer circuit board after exposure and development, so that the blind holes on the inner layer circuit board are plated with a copper electroplating layer, and an outer layer circuit is formed on the outer surface of the inner layer circuit board.

[0077] A dry film is pasted on the metal seed layer so that the window is covered under the dry film, which can avoid the copper plating layer on the window and ensure the functionality of the window for welding; based on the dry film, exposure and development are carried out, and then electroplating is carried out, which can realize selective copper plating on the inner layer circuit board. Based on the selective copper plating, it can be ensured that the formed outer layer circuit meets the design requirements, and then on the basis of realizing the functionality of the entire circuit board, good electrical conductivity is achieved between the inner and outer layers of the entire circuit board, which effectively avoids the problems of low efficiency, high operation risk, unclean cleaning and easy damage to the bottom copper layer brought about by the method of laser blind hole combined with electroplating. The production process is simple, the production efficiency is high, the operation risk is small, the production precision is high, and the product yield is high.

[0078] The cross-sectional structure of the inner circuit board after dry film bonding, exposure and development in this embodiment is as follows: Figure 7 As shown, in Figure 7 In the figure, 7 is the dry film. The cross-sectional structure of the inner layer circuit board after copper electroplating is as follows: Figure 8 As shown, in Figure 8 In the figure, 8 is an electroplated copper layer.

[0079] Preferably, after S34 and before S4 in this embodiment, the method further includes:

[0080] S35: removing the dry film from the inner layer circuit board after copper electroplating.

[0081] By removing the dry film, the metal seed layer located in the inner layer of the dry film can be exposed, which makes it easier to quickly etch the metal seed layer and remove unnecessary connection lines.

[0082] The cross-sectional structure of the first semi-finished circuit board obtained after removing the dry film in this embodiment is as follows: Fig. 9 shown.

[0083] Preferably, this embodiment S4 includes:

[0084] S41: providing an etching solution of a hydrogen peroxide-sulfuric acid system;

[0085] S42: using the etching solution of the hydrogen peroxide-sulfuric acid system to etch the first semi-finished circuit board, so that the metal seed layer is etched away, thereby obtaining the second semi-finished circuit board.

[0086] The etching solution of the hydrogen peroxide-sulfuric acid system can remove the metal through a rapid redox reaction to achieve rapid etching. On the basis of quickly etching the metal seed layer, it will not affect the electroplated copper layer near the metal seed layer, so that the electroplated copper layer near the metal seed layer will not be etched along with the etching of the metal seed layer, which not only achieves the removal of the metal seed layer, but also ensures the functionality of the electroplated copper layer.

[0087] Among them, the etching solution of hydrogen peroxide-sulfuric acid system is mainly composed of the following components:

[0088] Hydrogen peroxide (H2O2): acts as an oxidant, providing the oxygen atoms required to oxidize copper.

[0089] Sulfuric acid (H2SO4): provides an acidic environment, enhances the oxidizing properties of hydrogen peroxide, and serves as one of the reactants.

[0090] Stabilizer: used to improve the stability of etching solution and prevent hydrogen peroxide from decomposing too quickly in the solution. The selection and dosage of stabilizer have an important influence on the etching rate and stability of the solution.

[0091] Other additives: such as cyclic amine derivatives, aminotrimethylenephosphonic acid, organic acid salts, water-soluble lignin, phosphorus-containing additives, etc. These additives can improve the performance of etching solutions, such as increasing the amount of copper dissolved, reducing board surface oxidation, and enhancing chloride ion resistance.

[0092] The cross-sectional structure of the second semi-finished circuit board obtained after etching in this embodiment is as follows: Fig. 9 shown.

[0093] Preferably, this embodiment S5 includes:

[0094] S51: coating the photosensitive PI on the outer surface of the second semi-finished circuit board;

[0095] S52: According to the preset circuit design, the second semi-finished circuit board coated with the photosensitive PI is processed by using an exposure, development and curing process, so that the opening on the second semi-finished circuit board is exposed to obtain the target circuit board.

[0096] After the inner and outer layers are made, the outer surface of the second semi-finished circuit board is coated with photosensitive PI again. At this time, based on the photosensitive characteristics of the photosensitive PI, the inner layer of the second semi-finished circuit board is selectively exposed, where the window of the inner layer needs to be exposed for welding with external electronic components, so the exposure of the window can be selectively realized; on the other hand, based on the protective film characteristics of the photosensitive PI, the inner layer of the second semi-finished circuit board is selectively covered and protected. Without using the combination of PI and glue, these areas are protected. When the combination of the traditional PI layer and the glue layer is used as a protective film, the process is complicated and the production precision is low due to the process of punching the protective film. The production process is simple, the production efficiency is high, the operation risk is small, the production precision is high, and the product yield is high. .

[0097] The cross-sectional structure of the second semi-finished circuit board coated with photosensitive PI in this embodiment is as follows: Fig.10 As shown, in Fig.10 9 is the second photosensitive PI layer; the cross-sectional structure of the target circuit board is as follows Fig.11 shown.

[0098] In the first specific embodiment, a layer of PSPI with a thickness of 20 μm is coated on the single-sided board after circuit production, maintained at 100°C for 5 minutes, pre-cured to remove part of the solvent, exposed and developed, and opened at the position where welding is required. Finally, it is cured at 200°C in a nitrogen environment for 2 hours. The thickness of the cured PSPI (i.e., the thickness of the first photosensitive PI layer) is 15 μm; a single-layer flexible circuit board with only inner layer circuits can be obtained.

[0099] In the second specific embodiment, a layer of PSPI with a thickness of 18 μm is coated on the single-sided board after the circuit is made, maintained at 100° C. for 5 minutes, pre-cured to remove part of the solvent, exposed and developed, a window is made at the position where welding is required, and a blind hole with a diameter of 75 μm is formed at the position where the layers need to be electrically connected, and baked at 200° C. for 2 hours in a nitrogen environment for curing, and the thickness of the cured PSPI is 12 μm (i.e., the thickness of the first photosensitive PI layer); then a layer of 30 nm thick metal chromium is first vacuum sputtered on the surface (the sputtered metal chromium has better bonding with PSPI), and then a layer of 300 nm thick metal copper is vacuum sputtered, and the composite layer of metal chromium and metal copper is used as a metal seed layer, and the outer layer circuit is formed through an electroplating process to achieve conduction between the layers; finally, a layer of PSPI with a thickness of 18 μm is printed on the surface of the outer layer circuit, and a protective film with a thickness of 12 μm (i.e., the thickness of the second photosensitive PI layer) is formed through a pre-curing, exposure, development and curing process, so that a single-layer flexible circuit board containing both inner and outer layer circuits can be obtained.

[0100] Embodiment 2

[0101] This embodiment provides a flexible circuit board based on photosensitive PI, which is manufactured using the method for manufacturing a flexible circuit board based on photosensitive PI described in the first embodiment.

[0102] The flexible circuit board manufactured in this embodiment utilizes the photosensitive properties of the photosensitive PI and the insulating properties of the protective film to achieve excellent electrical conduction between the layers of the multi-layer flexible circuit board, which effectively avoids the problems of low efficiency, high operating risk, unclean cleaning and easy damage to the bottom copper layer brought about by the method of laser blind hole combined with electroplating, and also avoids the problems of complex process and low manufacturing precision brought about by the process of punching the protective film when the combination of the traditional PI layer and the glue layer is used as a protective film. The manufacturing process is simple, the production efficiency is high, the operating risk is small, the manufacturing precision is high, and the product yield is high.

[0103] The manufacturing method of the flexible circuit board based on the photosensitive PI in this embodiment is the same as the method steps described in the first embodiment. Therefore, for details not provided in this embodiment, please refer to the first embodiment and the second embodiment. Figures 1 to 11 The specific description of this embodiment will not be repeated in detail.

[0104] Although the embodiments of the present invention have been described in conjunction with the accompanying drawings, those skilled in the art may make various modifications and variations without departing from the spirit and scope of the present invention, and such modifications and variations are all within the scope defined by the appended claims.

Claims

1. A method for manufacturing a flexible circuit board based on photosensitive PI, characterized in that: The method comprises: Providing a circuit substrate after circuit fabrication; Using photosensitive PI, blind holes for conduction and windows for welding are formed on the circuit substrate to obtain an inner circuit board; Making a metal seed layer on the inner circuit board, and electroplating the inner circuit board based on the metal seed layer, the blind holes and the openings to form an outer circuit to obtain a first semi-finished circuit board; removing the metal seed layer on the first semi-finished circuit board to obtain a second semi-finished circuit board; The photosensitive PI is used to expose the opening on the second semi-finished circuit board to obtain a target circuit board.

2. The method according to claim 1, characterized in that: The method uses photosensitive PI to form blind holes for conduction and windows for welding on the circuit substrate to obtain an inner circuit board, including: Coating the photosensitive PI on the circuit substrate after circuit fabrication; According to the preset circuit design, the circuit substrate coated with the photosensitive PI is processed by adopting the process of exposure, development and curing, and the blind holes and the openings are respectively formed on the circuit substrate to obtain the inner layer circuit board.

3. The manufacturing method according to claim 1, characterized in that: The metal seed layer is specifically at least one of a chromium metal layer, a titanium metal layer, an aluminum metal layer, a copper metal layer, a chromium-copper alloy layer, a copper-aluminum alloy layer, and a titanium-copper alloy layer.

4. The method according to claim 1, characterized in that: The thickness of the metal seed layer is in the range of 0.1 to 1 μm.

5. The method according to claim 1, characterized in that: The step of manufacturing a metal seed layer on the inner circuit board comprises: The metal seed layer is formed on the outer surface of the inner layer circuit board by using a vacuum sputtering process.

6. The method according to claim 5, characterized in that: The method of electroplating the inner circuit board based on the metal seed layer, the blind hole and the opening to form an outer circuit comprises: Pasting a dry film on the inner layer circuit board after vacuum sputtering, and covering the opening on the inner layer circuit board under the dry film; Using an exposure and development process to process the inner layer circuit board after the dry film is applied; The inner layer circuit board after exposure and development is processed by using a copper electroplating process, so that the blind holes on the inner layer circuit board are plated with a copper electroplating layer, and an outer layer circuit is formed on the outer surface of the inner layer circuit board.

7. The manufacturing method according to claim 6, characterized in that: Before removing the metal seed layer on the first semi-finished circuit board, the method further includes: The inner layer circuit board after copper electroplating is subjected to dry film removal.

8. The manufacturing method according to claim 7, characterized in that: removing the metal seed layer on the first semi-finished circuit board to obtain a second semi-finished circuit board; Provide etching solution of hydrogen peroxide-sulfuric acid system; The first semi-finished circuit board is etched using the etching solution of the hydrogen peroxide-sulfuric acid system, so that the metal seed layer is etched away to obtain the second semi-finished circuit board.

9. The manufacturing method according to claim 1, characterized in that: The method of using the photosensitive PI to expose the opening on the second semi-finished circuit board to obtain a target circuit board includes: Applying the photosensitive PI on the outer surface of the second semi-finished circuit board; According to the preset circuit design, the second semi-finished circuit board coated with the photosensitive PI is processed by adopting the process of exposure, development and curing, so that the opening on the second semi-finished circuit board is exposed to obtain the target circuit board.

10. A flexible circuit board based on photosensitive PI, characterized in that: The method is manufactured by the manufacturing method according to any one of claims 1 to 9.

Citation Information

Cited By

  • Laminating method and system of multi-layer flexible circuit board

    CN120786822A