Treatment and recovery process of hot galvanizing phosphating wastewater
The existing solutions were solved by using calcium hydroxide, calcium carbonate and calcium oxide for preliminary neutralization in hot-dip galvanized phosphated wastewater treatment, combined with flocculation and adsorption treatment of PAC, PAM and composite activated carbon, and removal measures of degreasing compositions. The complex process and high cost problems have achieved efficient wastewater treatment and recycling.
Patent Information
- Application Number
- CN202411006091.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-25
- Publication Date
- 2024-11-12
AI Technical Summary
The existing hot-dip galvanized phosphating wastewater treatment process is complex, the dosage is large, and the operating cost is high, making it difficult to effectively remove contaminants such as Fe2+, SS, Cr2+, P, Zn and oil.
Calcium hydroxide, calcium carbonate and calcium oxide are used for preliminary neutralization and precipitation treatment, followed by addition of polyaluminum chloride (PAC), polyacrylamide (PAM) and composite activated carbon for flocculation and adsorption treatment, and further removal is carried out using degreasing composition. The oil and organic impurities were obtained and the supernatant was recovered.
The process flow is simplified, the dosage and operation costs are reduced, the treatment efficiency of wastewater is improved, and the heavy metals, suspended substances and organic pollutants in the phosphated wastewater can be effectively removed, so as to achieve the recycling effect of meeting the water quality standards.
Smart Images

Figure BDA0004963046580000111 
Figure BDA0004963046580000121
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of wastewater treatment, and more specifically, to a treatment and recovery process for hot-dip galvanizing and phosphating wastewater. Background Art
[0002] Hot dip galvanizing phosphating wastewater mainly includes Fe 2+ ,SS,Cr 2+ , P, Zn and grease, the pH of phosphating wastewater is 2-3. Heavy metal ions are very harmful to the environment and human health. Long-term accumulation will cause serious pollution to the environment. Therefore, this wastewater needs to be treated to meet the standards before it can be discharged and recycled.
[0003] In the prior art, wastewater treatment is carried out using a process that combines separate pretreatment and continuous treatment. The wastewater is first subjected to acidification treatment and demulsification pretreatment, then sedimentation and filtration are performed, and a mixture is obtained by mixing. The mixture is then subjected to continuous treatment. The continuous treatment process includes comprehensive aeration regulation, primary precipitation reaction, inclined plate sedimentation separation, secondary coagulation reaction, flotation separation, sand filtration and activated carbon adsorption. The final supernatant is tested to see if it meets the standards. If it does not meet the standards, continuous treatment and recycling are carried out. This treatment method has complex processes, large dosages and high operating costs. Summary of the Invention
[0004] In order to solve the problems of complex phosphating wastewater process, large dosage and high operating costs in the existing technology, the present application provides a treatment and recovery process for hot-dip galvanizing phosphating wastewater.
[0005] In the first aspect, the present application provides a process for treating and recycling hot-dip galvanizing and phosphating wastewater, which adopts the following technical solution: A process for treating and recycling hot-dip galvanizing and phosphating wastewater comprises the following steps: (1) adding calcium hydroxide, calcium carbonate and calcium oxide to the phosphating wastewater, stirring for 15-20 minutes, filtering and obtaining a mixed solution 1; (2) adding PAC, PAM and composite activated carbon to the mixed solution 1 obtained in step (1), stirring for 35-40 minutes, and filtering to obtain a mixed solution 2; (3) adding the degreasing composition to the mixed solution 2 obtained in step (2), stirring for 25-30 minutes, filtering to obtain a supernatant, and completing the treatment and recovery of the hot-dip galvanizing and phosphating wastewater; The preparation method of the composite activated carbon comprises the following steps: (1) Coconut shells, straws and bamboo stalks are crushed separately, then mixed, soaked in hydrochloric acid for 1-2 hours, washed with water, calcined at a temperature of 500-520°C for 1-1.5 hours, then heated to 1300-1350°C and calcined for 3-4 hours, washed and dried to obtain a carbonized product; (2) Dispersing the modified sepiolite fiber in deionized water, adding the carbonized product obtained in step (1), acetic acid, chitosan and metal organic framework material, stirring for 1-2 hours, and drying to obtain composite activated carbon.
[0006] By adopting the above technical solution, the phosphating wastewater includes Fe 2+ ,SS,Cr 2+ , P, Zn and grease, the pH of the phosphating wastewater is 2-3, calcium hydroxide, calcium carbonate and calcium oxide are first added, which not only adjusts the pH of the phosphating wastewater, but also produces ferrous hydroxide precipitation and chromium hydroxide precipitation, which plays a role in neutralizing and coagulating metal ions. Calcium oxide is used as a coagulant to make the ferrous hydroxide precipitation and chromium hydroxide precipitation form ferrous hydroxide flocs and chromium hydroxide flocs, which are removed by filtration; Zn in the phosphating wastewater reacts with hydroxide to generate zinc hydroxide, which is then formed into zinc hydroxide flocs by a silicon oxide coagulant, and finally separated and removed by precipitation; calcium hydroxide can react with grease to neutralize it and play a dissolving role. It is hydrolyzed into fatty acids and glycerol under alkaline conditions, and the hydroxide further reacts with fatty acids to produce salts, thereby removing grease; SS is further removed by filtration, and the resulting mixed solution is further treated.
[0007] PAC (polyaluminum chloride) is used as a flocculant to further promote the formation of flocs from suspended particles and colloidal substances in the mixed solution 1, which is convenient for sedimentation and filtration. It can also inhibit the reproduction of bacteria and microorganisms in the water and reduce water pollution. PAM (polyacrylamide) is used as a flocculant and precipitant to effectively remove suspended particles, colloidal substances and organic matter in the phosphating wastewater and improve water quality. Composite activated carbon has high activity, strong adaptability and sufficient adsorption effect, and can adsorb P, organic matter and heavy metals. PAC, PAM and composite activated carbon cooperate to adsorb and remove suspended matter and other impurities in the phosphating wastewater to obtain mixed solution 2, and then a degreasing composition is added to further remove organic impurities such as oil and fat in the mixed solution 2, purify the water quality, and the obtained supernatant is recovered.
[0008] In the composite activated carbon, coconut shells, straws and bamboo poles are crushed and soaked in hydrochloric acid to remove organic impurities in the coconut shells, straws and bamboo poles, and then calcined in steps to obtain loose and porous carbonized materials. The carbonized materials prepared using coconut shells have the advantages of high strength, good wear resistance and high chemical stability. The carbonized materials prepared using straws have a microporous structure and can adsorb harmful gases, odors, heavy metals and other substances to achieve the effect of purifying water quality. The carbonized materials prepared using bamboo poles have the advantages of strong toughness, strong durability and strong adsorption. The carbonized materials prepared using coconut shells, straws and bamboo poles cooperate with each other to jointly improve the strength, adsorption and durability of the carbonized materials.
[0009] The modified sepiolite fiber has a porous structure, strong acid resistance and excellent heat resistance. The modified sepiolite fiber can be loaded on the surface and pores of the carbonized material, thereby increasing the specific surface area of the carbonized material. The metal organic framework material has the advantages of large specific surface area, strong thermal stability, high adsorption and high strength. The metal organic framework material can be loaded on the surface and pores of the carbonized material, thereby enhancing the mechanical strength of the carbonized material. The modified sepiolite fiber, carbonized material and metal organic framework material cooperate with each other to jointly improve the mechanical strength, adsorption and specific surface area of the carbonized material, which is helpful for the adsorption work of the subsequently prepared composite activated carbon. Chitosan has a certain viscosity and coats the carbonized material to a certain extent, so that the modified sepiolite fiber, carbonized material and metal organic framework material are tightly connected, further increasing the stability of the carbonized material loading components and increasing the stability of the carbonized material performance, which is helpful for the subsequent composite biochar treatment of phosphating wastewater and improves the treatment efficiency of phosphating wastewater.
[0010] Optionally, the mass ratio of the coconut shell, straw and bamboo pole is 1:0.5-0.7:2-6.
[0011] By adopting the above technical scheme, the mass ratio of coconut shells, straws and bamboo poles is further limited within a certain range, and the obtained carbonized product has good comprehensive performance. The carbonized product of coconut shells has high strength, good wear resistance and high chemical stability. The carbonized product of straws has the advantages of large specific surface area, moderate pore size, uniform distribution and fast adsorption speed. The carbonized product of bamboo poles has the advantages of strong toughness, strong durability and strong adsorption. The coconut shells, straws and bamboo poles cooperate with each other to make up for the shortcomings and jointly improve the strength, wear resistance and adsorption of the carbonized product. The composite activated carbon prepared subsequently has better comprehensive performance and is used in phosphating wastewater treatment. It has good adsorption and purifies water quality.
[0012] Optionally, the mass ratio of the modified sepiolite fiber, the carbonized material, the chitosan and the metal organic framework material is 0.6-0.9:1:0.2-0.4:0.3-0.5.
[0013] By adopting the above technical scheme, the mass ratio of modified sepiolite fiber, carbonization, chitosan and metal organic framework material is further limited within a certain range, and the corresponding performance of the carbonization is improved. The modified sepiolite fiber has good toughness, large specific surface area, softness and elasticity, and can be adsorbed on the surface of the carbonization. The metal organic framework material has the advantages of high strength and high porosity, and can be loaded on the surface and pores of the carbonization. Chitosan has a certain viscosity and can increase the adhesion between the modified sepiolite fiber, carbonization and metal organic framework material, so that the structure and performance of the modified carbonization are stable. The modified sepiolite fiber, carbonization, chitosan and metal organic framework material have a synergistic effect, so that the prepared composite biochar has good mechanical strength and adsorption, and is used to subsequently treat phosphating wastewater, thereby improving the treatment efficiency of phosphating wastewater.
[0014] Optionally, the method for preparing the modified sepiolite fiber comprises the following steps: (1) dispersing the sepiolite fiber in hydrochloric acid, soaking for 10-15 minutes, washing with water, and then dispersing it in an aqueous solution of a silane coupling agent, stirring for 30-35 minutes, and filtering to obtain pretreated sepiolite fiber; (2) The pretreated sepiolite fibers obtained in step (1) are dispersed in deionized water, carbon nanotubes, hydroxymethyl cellulose and β-cyclodextrin are added and mixed, stirred for 30-35 minutes, and dried to obtain modified sepiolite fibers.
[0015] By adopting the above technical solution, hydrochloric acid removes organic impurities in the sepiolite fiber, increases the specific surface area of the sepiolite fiber, increases the porosity of the sepiolite fiber, and the silane coupling agent undergoes an etherification reaction with the -OH group on the surface of the sepiolite fiber, thereby introducing organic silane into the sepiolite surface, increasing the dispersibility and hydrophilicity of the sepiolite fiber, and allowing the sepiolite fiber to be evenly dispersed in water.
[0016] Carbon nanotubes have a high specific surface area and strong adsorption capacity, and can also adsorb heavy metal ions and organic pollutants. Carbon nanotubes can be loaded on the surface and pores of sepiolite fibers. Hydroxymethyl cellulose has a certain viscosity, which allows the carbon nanotubes to be tightly loaded on the surface of the sepiolite fibers. β-cyclodextrin can enhance the stability and viscosity of hydroxymethyl cellulose and improve the bonding stability between carbon fibers and sepiolite fibers. Hydroxymethyl cellulose is also nonionic and hydrophilic, β-cyclodextrin has good adsorption performance and renewability, and the carboxyl group of carboxymethyl cellulose and the cyclic structure of β-cyclodextrin provide a large adsorption surface area, which can form an envelope and coordination reaction with organic matter and metal ions in wastewater, thereby improving the wastewater treatment effect. The modified sepiolite fibers have good mechanical strength and adsorption, thereby effectively improving the performance of the composite activated carbon, and subsequently effectively removing pollutants in phosphating wastewater.
[0017] Optionally, the mass ratio of the sepiolite fiber, carbon nanotube, hydroxymethyl cellulose and β-cyclodextrin is 1:0.4-0.6:0.07-0.09:0.1-0.2.
[0018] By adopting the above technical solution, the mass ratio of sepiolite fiber, carbon nanotubes, hydroxymethyl cellulose and β-cyclodextrin is further limited within a certain range, thereby improving the mechanical strength and adsorption of sepiolite fiber. Carbon nanotubes have a high specific surface area and strong adsorption, and can be loaded on the surface and pores of sepiolite fiber, thereby increasing the adsorption and strength of sepiolite fiber. Hydroxymethyl cellulose has a certain viscosity, so that the carbon nanotubes are tightly loaded on the surface of sepiolite fiber. β-cyclodextrin can enhance the stability and viscosity of hydroxymethyl cellulose and improve the bonding stability between carbon fiber and sepiolite fiber. The sepiolite fiber, carbon nanotubes, hydroxymethyl cellulose and β-cyclodextrin have a synergistic effect, thereby improving the adsorption of sepiolite fiber, which is helpful for the subsequent treatment of phosphating wastewater.
[0019] Optionally, the degreasing composition comprises the following raw materials: sodium carbonate, sodium dodecylbenzenesulfonate, sodium sulfate, N-benzyldiethanolamine, modified diatomaceous earth, sodium gluconate, ethanol, sodium ligninsulfonate, and the balance water.
[0020] By adopting the above technical solution, sodium carbonate reacts with fatty acids in oils and fats to generate a surfactant with cleaning ability, which can remove dirt and grease from metal surfaces. Sodium dodecylbenzenesulfonate has good surface activity and strong hydrophilicity, effectively reducing the tension at the oil-water interface to achieve emulsification, and can effectively remove pollutants such as oil and suspended matter in phosphating wastewater. Sodium sulfate has good flocculation, precipitation and adsorption properties, and can effectively remove pollutants such as suspended matter and turbidity in phosphating wastewater, thereby improving water quality.
[0021] N-benzyldiethanolamine has a good denitrification and dephosphorization effect, which adsorbs ammonia nitrogen or phosphate ions in the water to form a stable complex, thereby achieving the effect of denitrification and dephosphorization. Modified diatomaceous earth removes harmful substances in phosphate wastewater through adsorption, ion exchange, catalytic oxidation, and biological adsorption. Modified diatomaceous earth can adsorb phosphorus and ammonium ions, and remove phosphorus, nitrogen and other ionic substances in water through effective ion exchange sites on the surface, which can not only remove pollutants but also maintain the pH value of water stable; it also has catalytic oxidation effect, which can effectively oxidize and reduce heavy metal ions and organic pollutants, and remove organic matter and heavy metal ions in phosphate wastewater.
[0022] Sodium gluconate has good adsorption and degumming properties, which can destroy the colloidal substances in the phosphating wastewater, making the colloidal substances unstable and dispersed in the water. It also promotes the rapid aggregation of suspended matter in the phosphating wastewater into clumps and floating to the liquid surface, which is helpful for subsequent treatment; sodium lignin sulfonate can precipitate heavy metal ions and other pollutants, removing organic pollutants and heavy metals in the phosphating wastewater; various components in the degreasing composition cooperate with each other to remove organic pollutants such as oil, heavy metals, etc. in the phosphating wastewater, and jointly improve the water quality of the phosphating wastewater.
[0023] Optionally, the degreasing composition comprises, by weight, 30-50 parts of sodium carbonate, 10-14 parts of sodium dodecylbenzenesulfonate, 15-18 parts of sodium sulfate, 6-9 parts of N-benzyldiethanolamine, 12-15 parts of modified diatomaceous earth, 5-8 parts of sodium gluconate, 20-25 parts of ethanol, 4-7 parts of sodium ligninsulfonate, and the balance water.
[0024] By adopting the above technical solution and further limiting the amount of each component, the obtained degreasing composition has a relatively good effect of removing organic pollutants such as grease and heavy metals from phosphating wastewater. The sodium sulfate has excellent flocculation, precipitation and adsorption properties, and can effectively remove suspended matter, turbidity and other pollutants in the phosphating wastewater. The sodium sulfate can be loaded in the pores of the modified diatomaceous earth, thereby increasing the specific surface area of the modified diatomaceous earth, thereby increasing the adsorption capacity of the modified diatomaceous earth, and helping to remove organic matter and heavy metal ions in the phosphating wastewater. The various components cooperate with each other to remove organic pollutants such as grease and heavy metals from the phosphating wastewater, and jointly improve the water quality of the phosphating wastewater.
[0025] Optionally, the preparation method of the modified diatomaceous earth comprises the following steps: (1) Disperse diatomaceous earth in ammonia water, stir for 2-3 minutes, wash with water, and then disperse in deionized water. Add sodium hexadecylbenzenesulfonate and talc, stir evenly, and set aside; (2) Dispersing activated carbon in deionized water, adding potassium oxalate and sodium citrate, stirring for 10-20 minutes, and filtering to obtain pretreated activated carbon; (3) adding the pretreated activated carbon obtained in step (2) to the diatomaceous earth obtained in step (1), stirring evenly, and drying to obtain modified diatomaceous earth.
[0026] By adopting the above technical solution, ammonia water removes organic impurities in diatomaceous earth and increases the specific surface area of diatomaceous earth. Sodium hexadecylbenzenesulfonate can be loaded on the surface and pores of diatomaceous earth to form a stable dispersion system. Talc powder and diatomaceous earth adsorb each other, increasing the specific surface area of diatomaceous earth, thereby enhancing the adsorption effect of diatomaceous earth and improving the efficiency of diatomaceous earth in removing organic pollutants such as oil, heavy metals, etc. in phosphating wastewater.
[0027] The pore structure of activated carbon provides a large amount of adsorption surface, which can effectively adsorb organic matter and remove organic matter, pigments, heavy metal ions, oils, etc. from phosphating wastewater. It can adsorb organic matter from phosphating wastewater to its surface and effectively remove it; potassium oxalate can be used as a chelating agent to combine with heavy metals in phosphating wastewater to remove heavy metals. Sodium citrate has a flocculation effect, which changes the surface charge of particles and suspended matter in phosphating wastewater, making them more likely to attract each other and agglomerate together to form clumps; potassium oxalate and sodium citrate can be loaded on the surface and pores of activated carbon, which helps the subsequent potassium oxalate and sodium citrate to exert their purification effect.
[0028] Activated carbon can be loaded on the surface and pores of diatomaceous earth, so that activated carbon, potassium oxalate and sodium citrate can be stably loaded on the surface of diatomaceous earth. Combined with sodium hexadecylbenzenesulfonate and talc, the adsorption performance of diatomaceous earth is significantly improved. The various components cooperate with each other to remove organic pollutants such as oil, heavy metals, etc. in phosphating wastewater, thereby improving water quality.
[0029] Optionally, the mass ratio of the diatomaceous earth, sodium hexadecylbenzenesulfonate and talc is 1:0.1-0.3:0.2-0.4.
[0030] By adopting the above technical solution, the mass ratio of diatomaceous earth, sodium hexadecylbenzenesulfonate and talc is further limited within a certain range, thereby improving the adsorption performance of the diatomaceous earth. The sodium hexadecylbenzenesulfonate can be loaded on the surface and pores of the diatomaceous earth to form a stable dispersion system. The talc and diatomaceous earth adsorb each other, increasing the specific surface area of the diatomaceous earth. The sodium hexadecylbenzenesulfonate can also be loaded on the surface and pores of the talc. The diatomaceous earth, sodium hexadecylbenzenesulfonate and talc cooperate with each other, thereby enhancing the adsorption effect of the diatomaceous earth and improving the efficiency of the diatomaceous earth in removing organic pollutants such as oil, grease and heavy metals in phosphating wastewater.
[0031] Preferably, the mass ratio of the diatomaceous earth, potassium oxalate and sodium citrate is 1:0.3-0.6:0.2-0.5.
[0032] By adopting the above technical solution, the mass ratio of diatomaceous earth, potassium oxalate and sodium citrate is further limited within a certain range, thereby improving the corresponding performance of the diatomaceous earth. Potassium oxalate and sodium citrate can be loaded on the surface and pores of the diatomaceous earth, thereby increasing the specific surface area of the diatomaceous earth. Potassium oxalate is used as a chelating agent to combine with heavy metals in the phosphation wastewater to remove heavy metals. Sodium citrate has a flocculation effect, which changes the surface charge of particles and suspended matter in the phosphation wastewater, making them more likely to attract each other and agglomerate together to form clumps. Potassium oxalate and sodium citrate can be loaded on the surface and pores of activated carbon, which helps potassium oxalate and sodium citrate to subsequently exert the effect of purifying the phosphation wastewater.
[0033] In summary, this application has the following beneficial effects: 1. The phosphating wastewater in this application includes Fe 2+ ,SS,Cr 2+ , P, Zn and grease, the pH of phosphating wastewater is 2-3, first add calcium hydroxide, calcium carbonate and calcium oxide, which not only adjust the pH of phosphating wastewater, but also produce ferrous hydroxide precipitation and chromium hydroxide precipitation, which play a role in neutralizing and coagulating metal ions. Calcium oxide is used as a coagulant to make ferrous hydroxide precipitation and chromium hydroxide precipitation form ferrous hydroxide flocs and chromium hydroxide flocs, which are removed by filtration; Zn in phosphating wastewater reacts with hydroxide to generate zinc hydroxide, which is then passed through a silicon oxide coagulant to form zinc hydroxide flocs, and finally separated and removed by precipitation.
[0034] 2. In the present application, PAC further promotes the formation of flocs of suspended particles and colloidal substances in the mixed solution 1, which is convenient for precipitation and filtration, and can also inhibit the reproduction of bacteria and microorganisms in the water, reducing the pollution of water sources; PAM can effectively remove suspended particles, colloidal substances and organic matter in phosphating wastewater, and improve water quality; composite activated carbon has high activity, strong adaptability, and sufficient adsorption effect, and can adsorb P, organic matter, and heavy metals. PAC, PAM and composite activated carbon cooperate to adsorb and remove suspended matter and other impurities in the phosphating wastewater to obtain mixed solution 2, and then the degreasing composition is added to further remove organic impurities such as grease in the mixed solution 2, purify the water quality, and the obtained supernatant is recovered.
[0035] 3. The modified sepiolite fiber in this application has good toughness, large specific surface area, softness and elasticity, and can be adsorbed on the surface of the carbonized material. The metal organic framework material has the advantages of high strength and high porosity, and can be loaded on the surface and pores of the carbonized material. Chitosan has a certain viscosity, which can increase the adhesion between the modified sepiolite fiber, carbonized material and the metal organic framework material, so that the structure and performance of the modified carbonized material are stable. The modified sepiolite fiber, carbonized material, chitosan and metal organic framework material have a synergistic effect, so that the prepared composite biochar has good mechanical strength and adsorption, and the subsequent treatment of phosphating wastewater improves the treatment efficiency of phosphating wastewater. DETAILED DESCRIPTION
[0036] Preparation example of modified sepiolite fiber Preparation Example 1-1 The preparation method of modified sepiolite fiber comprises the following steps: (1) 1 kg of sepiolite fiber was dispersed in 2 L of 12% hydrochloric acid, soaked for 12 min, washed with water, and then dispersed in 1.5 L of 0.3% silane coupling agent aqueous solution, stirred for 35 min, and filtered to obtain pretreated sepiolite fiber; (2) The pretreated sepiolite fibers obtained in step (1) were dispersed in 2 L of deionized water, carbon nanotubes, hydroxymethyl cellulose and β-cyclodextrin were added and mixed, stirred for 35 min, and dried to obtain modified sepiolite fibers.
[0037] The mass ratio of sepiolite fiber, carbon nanotubes, hydroxymethyl cellulose and β-cyclodextrin is 1:0.6:0.07:0.1.
[0038] Preparation Example 1-2 The difference from Preparation Example 1-1 is that step (1) is not performed.
[0039] Preparation Examples 1-3 The difference from Preparation Example 1-1 is that no carbon nanotubes are added.
[0040] Preparation Examples 1-4 The difference from Preparation Example 1-1 is that hydroxymethyl cellulose is not added.
[0041] Preparation Examples 1-5 The difference from Preparation Example 1-1 is that β-cyclodextrin is not added.
[0042] Preparation Examples 1-6 The difference from Preparation Example 1-1 is that the mass ratio of sepiolite fiber, carbon nanotubes, hydroxymethyl cellulose and β-cyclodextrin is 1:0.4:0.09:0.2.
[0043] Preparation Examples 1-7 The difference from Preparation Example 1-1 is that the mass ratio of sepiolite fiber, carbon nanotubes, hydroxymethyl cellulose and β-cyclodextrin is 1:0.2:0.1:0.02.
[0044] Preparation example of modified diatomite Preparation Example 2-1 The preparation method of modified diatomaceous earth comprises the following steps: (1) Disperse 0.8 kg of diatomaceous earth in 1.5 L of 23% ammonia water, stir for 3 min, wash with water, and then disperse in 1.2 L of deionized water. Add sodium hexadecylbenzenesulfonate and talc, stir evenly, and set aside. (2) Disperse 0.3 kg of activated carbon in 1 L of deionized water, add potassium oxalate and sodium citrate, stir for 20 min, and filter to obtain pretreated activated carbon; (3) adding the pretreated activated carbon obtained in step (2) to the diatomaceous earth obtained in step (1), stirring evenly, and drying to obtain modified diatomaceous earth.
[0045] The mass ratio of diatomaceous earth, sodium hexadecylbenzenesulfonate and talc is 1:0.1:0.2.
[0046] The mass ratio of diatomaceous earth, potassium oxalate and sodium citrate is 1:0.3:0.5.
[0047] Preparation Example 2-2 The difference from Preparation Example 2-1 is that sodium hexadecylbenzenesulfonate is not added.
[0048] Preparation Example 2-3 The difference from Preparation Example 2-1 is that no talc is added.
[0049] Preparation Example 2-4 The difference from Preparation Example 2-1 is that the mass ratio of diatomaceous earth, sodium hexadecylbenzenesulfonate and talc is 1:0.3:0.4.
[0050] Preparation Example 2-5 The difference from Preparation Example 2-1 is that the mass ratio of diatomaceous earth, sodium hexadecylbenzenesulfonate and talc is 1:0.7:0.1.
[0051] Preparation Example 2-6 The difference from Preparation Example 2-1 is that potassium oxalate is not added.
[0052] Preparation Example 2-7 The difference from Preparation Example 2-1 is that sodium citrate is not added.
[0053] Preparation Example 2-8 The difference from Preparation Example 2-1 is that the mass ratio of diatomaceous earth, potassium oxalate and sodium citrate is 1:0.6:0.2.
[0054] Preparation Example 2-9 The difference from Preparation Example 2-1 is that the mass ratio of diatomaceous earth, potassium oxalate and sodium citrate is 1:0.1:0.9. Example
[0055] Example 1 A process for treating and recycling hot-dip galvanizing and phosphating wastewater comprises the following steps: (1) Add 0.4 kg of calcium hydroxide, 0.2 kg of calcium carbonate and 0.3 kg of calcium oxide to 1 ton of phosphating wastewater, stir for 20 minutes, and filter to obtain a mixed solution 1; (2) adding 2 kg of PAC, 1.5 kg of PAM and 1.8 kg of composite activated carbon to the mixed solution 1 obtained in step (1), stirring for 40 min, and filtering to obtain a mixed solution 2; (3) adding 6 kg of the degreasing composition to the mixed solution 2 obtained in step (2), stirring for 30 min, filtering to obtain a supernatant, and completing the treatment and recovery of the hot-dip galvanizing and phosphating wastewater; The preparation method of composite activated carbon comprises the following steps: (1) 1 kg of coconut shell, straw, and bamboo stalks were crushed separately, mixed, and soaked in 5 L of 12% hydrochloric acid for 2 h, washed with water, calcined at 510°C for 1.5 h, and then heated to 1300°C for 4 h. After calcination, the mixture was washed and dried to obtain a carbonized product. (2) 0.9 kg of modified sepiolite fiber was dispersed in 1.4 L of deionized water, and the carbonized product obtained in step (1), 0.4 L of acetic acid with a mass concentration of 8%, chitosan and metal organic framework material (MOF-235, purchased from Beijing Beike New Materials Technology Co., Ltd.) were added, stirred for 2 h, and dried to obtain composite activated carbon.
[0056] The mass ratio of coconut shell, straw and bamboo pole is 1:0.5:6.
[0057] The mass ratio of modified sepiolite fiber, carbonized material, chitosan and metal organic framework material is 0.6:1:0.4:0.3.
[0058] Degreasing composition, 50kg sodium carbonate, 14kg sodium dodecylbenzenesulfonate, 18kg sodium sulfate, 9kg N-benzyldiethanolamine, 15kg modified diatomaceous earth, 8kg sodium gluconate, 25kg ethanol, 7kg sodium ligninsulfonate, and 170kg water.
[0059] The modified sepiolite fiber was prepared according to Preparation Example 1-1, and the modified diatomaceous earth was prepared according to Preparation Example 2-1.
[0060] Example 2 A process for treating and recovering hot-dip galvanizing and phosphating wastewater, which differs from Example 1 in that the mass ratio of coconut shells, straws and bamboo poles is 1:0.7:2.
[0061] The mass ratio of modified sepiolite fiber, carbonized material, chitosan and metal organic framework material is 0.9:1:0.2:0.5.
[0062] Degreasing composition, 30kg sodium carbonate, 10kg sodium dodecylbenzenesulfonate, 15kg sodium sulfate, 6kg N-benzyldiethanolamine, 12kg modified diatomaceous earth, 5kg sodium gluconate, 20kg ethanol, 4kg sodium ligninsulfonate, and 180kg water.
[0063] Example 3 A process for treating and recovering hot-dip galvanizing and phosphating wastewater, which differs from Example 1 in that the mass ratio of modified sepiolite fiber, carbonized material, chitosan and metal organic framework material is 0.2:1:0.8:0.1.
[0064] Example 4 A process for treating and recovering hot-dip galvanizing and phosphating wastewater is disclosed, which differs from Example 1 in that the modified sepiolite fiber is prepared using Preparation Example 1-2.
[0065] Example 5 A process for treating and recovering hot-dip galvanizing and phosphating wastewater is disclosed, which differs from Example 1 in that the modified sepiolite fiber is prepared using Preparation Examples 1-3.
[0066] Example 6 A process for treating and recovering hot-dip galvanizing and phosphating wastewater is disclosed, which differs from Example 1 in that the modified sepiolite fiber is prepared using Preparation Examples 1-4.
[0067] Example 7 A process for treating and recovering hot-dip galvanizing and phosphating wastewater is disclosed, which differs from Example 1 in that the modified sepiolite fiber is prepared using Preparation Examples 1-5.
[0068] Example 8 A process for treating and recovering hot-dip galvanizing and phosphating wastewater is disclosed, which differs from Example 1 in that the modified sepiolite fiber is prepared using Preparation Examples 1-6.
[0069] Example 9 A process for treating and recovering hot-dip galvanizing and phosphating wastewater is disclosed, which differs from Example 1 in that the modified sepiolite fiber is prepared using Preparation Examples 1-7.
[0070] Example 10 A process for treating and recovering hot-dip galvanizing and phosphating wastewater is provided, which differs from Example 1 in that the modified diatomaceous earth is prepared using Preparation Example 2-2.
[0071] Example 11 A process for treating and recovering hot-dip galvanizing and phosphating wastewater is provided, which differs from Example 1 in that the modified diatomaceous earth is prepared using Preparation Example 2-3.
[0072] Example 12 A process for treating and recovering hot-dip galvanizing and phosphating wastewater is provided, which differs from Example 1 in that the modified diatomaceous earth is prepared using Preparation Example 2-4.
[0073] Example 13 A process for treating and recovering hot-dip galvanizing and phosphating wastewater is provided, which differs from Example 1 in that the modified diatomaceous earth is prepared using Preparation Example 2-5.
[0074] Example 14 A process for treating and recovering hot-dip galvanizing and phosphating wastewater is provided, which differs from Example 1 in that the modified diatomaceous earth is prepared using Preparation Example 2-6.
[0075] Example 15 A process for treating and recovering hot-dip galvanizing and phosphating wastewater is provided, which differs from Example 1 in that the modified diatomaceous earth is prepared using Preparation Example 2-7.
[0076] Example 16 A process for treating and recovering hot-dip galvanizing and phosphating wastewater is provided, which differs from Example 1 in that the modified diatomaceous earth is prepared using Preparation Example 2-8.
[0077] Example 17 A process for treating and recovering hot-dip galvanizing and phosphating wastewater is provided, which differs from Example 1 in that the modified diatomaceous earth is prepared using Preparation Example 2-9.
[0078] Comparative Example Comparative Example 1 A process for treating and recovering hot-dip galvanizing and phosphating wastewater, which differs from Example 1 in that no composite activated carbon is added.
[0079] Comparative Example 2 A process for treating and recovering hot-dip galvanizing and phosphating wastewater, which differs from Example 1 in that modified sepiolite fiber is not added.
[0080] Comparative Example 3 A process for treating and recovering hot-dip galvanizing and phosphating wastewater, which differs from Example 1 in that chitosan is not added.
[0081] Comparative Example 4 A process for treating and recovering hot-dip galvanizing and phosphating wastewater, which differs from Example 1 in that no metal organic framework material is added.
[0082] Comparative Example 5 A process for treating and recovering hot-dip galvanizing and phosphating wastewater, which differs from Example 1 in that no degreasing composition is added.
[0083] Performance testing The phosphating wastewater treated in Examples 1-17 and Comparative Examples 1-5 was subjected to compliance testing according to the "Iron and Steel Industry Water Pollutant Discharge Standard" GB13456-2012; The degreasing performance of the degreasing compositions prepared in Example 1, Examples 10-17 and Comparative Example 5 was tested in accordance with the JB / T4323.1-1999 standard; the test results are shown in Table 1.
[0084] Table 1 Test data of embodiments and comparative examples Combining the examples and the data in Table 1, it can be seen that the phosphating wastewater treated by Examples 1-2, 8, 12 and 16 has a better effect. In Example 1, the pH value is 7.9, Fe 2+ The content is 0.1mg / L, COD crThe content of activated carbon is 5 mg / L, there is no SS, the contents of P and Zn are both 0, the oil content is 0.2 mg / L, and the oil removal rate of the steel plate is 99.9%. This shows that the addition of the composite activated carbon and the degreasing composition, as well as the combination of other components, in the present application can treat phosphating wastewater. The combination of various components has high adsorption capacity, removes organic impurities such as oil and fat from the phosphating wastewater, purifies the water quality, and improves the treatment efficiency of the phosphating wastewater. The obtained supernatant is recovered.
[0085] Example 3 changes the mass ratio of modified sepiolite fiber, carbonized material, chitosan and metal organic framework material. As shown in Table 1, compared with Example 1, Fe 2+ The content is 0.2mg / L, COD cr The content of carbon is 7 mg / L, and the content of oil is 0.3 mg / L, indicating that the modified sepiolite fiber, carbonized material, chitosan and metal organic framework material have a synergistic effect, so that the prepared composite biochar has good mechanical strength and adsorption properties, and the subsequent treatment of phosphating wastewater improves the treatment efficiency of phosphating wastewater.
[0086] In the preparation method of modified sepiolite fiber in Example 4, no fiber pretreatment is performed. As shown in Table 1, compared with Example 1, Fe 2+ The content is 1.0mg / L, COD cr The content of O is 13 mg / L, the content of P is 0.04 mg / L, the content of Zn is 0, and the content of oil is 0.9 mg / L, indicating that hydrochloric acid removes organic impurities in the sepiolite fiber, increases the specific surface area of the sepiolite fiber, increases the porosity of the sepiolite fiber, and the silane coupling agent undergoes an etherification reaction with the -OH group on the surface of the sepiolite fiber, thereby introducing organic silane into the surface of the sepiolite, increasing the dispersibility and hydrophilicity of the sepiolite fiber, which is helpful for the subsequent loading of the sepiolite fiber with other components.
[0087] In the preparation methods of modified sepiolite fibers in Examples 5-7, carbon nanotubes, hydroxymethyl cellulose and β-cyclodextrin are not added. As shown in Table 1, compared with Example 1, Fe 2+ 、COD cr , P, Zn and oil contents all increased to varying degrees, indicating that carbon nanotubes have a high specific surface area and strong adsorption capacity, and can be loaded on the surface and pores of sepiolite fibers, thereby increasing the ability of sepiolite fibers to adsorb heavy metal ions and organic pollutants; hydroxymethyl cellulose has a certain viscosity, which allows carbon nanotubes to be tightly loaded on the surface of sepiolite fibers, further increasing the performance stability of modified sepiolite fibers; β-cyclodextrin can enhance the stability and viscosity of hydroxymethyl cellulose, improve the bonding stability of carbon fibers and sepiolite fibers, and also has good adsorption properties and renewability, thereby effectively improving the performance of the composite activated carbon.
[0088] Example 9 changes the mass ratio of sepiolite fiber, carbon nanotubes, hydroxymethyl cellulose and β-cyclodextrin. As shown in Table 1, compared with Example 1, Fe 2+ 、COD cr The contents of P, Zn and oil are lower than those in Examples 5-7, but higher than those in Example 1 and Example 8, indicating that the combination of sepiolite fibers, carbon nanotubes, hydroxymethyl cellulose and β-cyclodextrin has a synergistic effect, thereby improving the adsorption of sepiolite fibers, which is helpful for the subsequent treatment of phosphating wastewater.
[0089] In the preparation method of modified diatomite in Examples 10-11, sodium hexadecylbenzenesulfonate and talc were not added. As shown in Table 1, compared with Example 1, Fe 2+ 、COD cr , P, Zn and oil contents all increased to varying degrees, indicating that sodium hexadecylbenzenesulfonate can be loaded on the surface and pores of diatomaceous earth to form a stable dispersion system. Talc and diatomaceous earth adsorb each other, increasing the specific surface area of diatomaceous earth, thereby enhancing the adsorption effect of diatomaceous earth and improving the efficiency of diatomaceous earth in removing organic pollutants such as grease, heavy metals, etc. in phosphating wastewater.
[0090] Example 13 changes the mass ratio of diatomaceous earth, sodium hexadecylbenzenesulfonate and talc. As shown in Table 1, compared with Example 1, Fe 2+ 、COD cr The contents of talc, P, Zn and oil are lower than those in Examples 10-11, but higher than those in Example 1 and Example 12, indicating that talc and diatomaceous earth adsorb each other, increasing the specific surface area of diatomaceous earth, and sodium hexadecylbenzenesulfonate can also be loaded on the surface and pores of talc. Diatomaceous earth, sodium hexadecylbenzenesulfonate and talc cooperate with each other, thereby enhancing the adsorption effect of diatomaceous earth and improving the efficiency of diatomaceous earth in removing organic pollutants such as grease and heavy metals in phosphating wastewater.
[0091] In the preparation method of modified diatomite in Examples 14-15, potassium oxalate and sodium citrate were not added. As shown in Table 1, compared with Example 1, Fe 2+ 、COD cr , P, Zn and oil contents increased to varying degrees, indicating that potassium oxalate can be used as a chelating agent to combine with heavy metals in phosphating wastewater, thereby removing heavy metals. Sodium citrate has a flocculation effect, which changes the surface charge of particles and suspended matter in phosphating wastewater, making them more likely to attract each other and agglomerate together to form agglomerates.
[0092] Example 17 changes the mass ratio of diatomaceous earth, potassium oxalate and sodium citrate. As shown in Table 1, compared with Example 1, Fe 2+ 、COD crThe contents of P, Zn and oil are lower than those in Examples 14-15, but higher than those in Example 1 and Example 16, indicating that potassium oxalate and sodium citrate can be loaded on the surface and pores of activated carbon, which helps the subsequent potassium oxalate and sodium citrate to purify the phosphating wastewater.
[0093] In Comparative Example 1, no composite activated carbon was added. As shown in Table 1, compared with Example 1, Fe 2+ The content is 3.5mg / L, COD cr The content of O is 30 mg / L, the content of P is 0.3 mg / L, the content of Zn is 0.1 mg / L, and the content of oil is 2.4 mg / L, indicating that the various components in the composite activated carbon cooperate with each other to improve the strength, adsorption and durability of the carbonized product, increase the stability of the carbonized product performance, and contribute to the subsequent composite biochar treatment of phosphating wastewater, thereby improving the treatment efficiency of phosphating wastewater.
[0094] In Comparative Example 2, no modified sepiolite fiber is added. As shown in Table 1, compared with Example 1, Fe 2+ The content is 3.2mg / L, COD cr The content of carbon is 27 mg / L, the content of P is 0.2 mg / L, the content of Zn is 0.09 mg / L, and the content of oil is 2.2 mg / L, indicating that the modified sepiolite fiber has a porous structure, strong acid resistance and excellent heat resistance. The modified sepiolite fiber can be loaded on the surface and pores of the carbonized material, increasing the specific surface area of the carbonized material, improving the mechanical strength, adsorption and specific surface area of the carbonized material, and improving the treatment efficiency of the phosphating wastewater.
[0095] In Comparative Example 3, chitosan was not added. As shown in Table 1, compared with Example 1, Fe 2+ The content is 2.7mg / L, COD cr The content of chitosan is 22 mg / L, the content of P is 0.05 mg / L, the content of Zn is 0.04 mg / L, and the content of oil is 1.8 mg / L, indicating that chitosan has a certain viscosity, which can increase the adhesion between the modified sepiolite fiber, carbonized material and metal organic framework material, making the structure and performance of the modified carbonized material stable, and subsequently treating phosphating wastewater, thereby improving the treatment efficiency of phosphating wastewater.
[0096] In Comparative Example 4, no metal organic framework material was added. As shown in Table 1, compared with Example 1, Fe 2+ The content is 2.9mg / L, COD crThe content of O is 24 mg / L, the content of P is 0.1 mg / L, the content of Zn is 0.07 mg / L, and the content of oil is 2.0 mg / L, indicating that the metal organic framework material has the advantages of high strength and high porosity, and can be loaded on the surface and pores of the carbonized material, so that the prepared composite biochar has good mechanical strength and adsorption, and the subsequent treatment of phosphating wastewater improves the treatment efficiency of phosphating wastewater.
[0097] In Comparative Example 5, no degreasing composition was added. As shown in Table 1, compared with Example 1, Fe 2+ The content is 2.2mg / L, COD cr The content of is 20 mg / L, the content of P is 0.15 mg / L and the content of Zn is 0.07 mg / L, the content of oil is 2.9 mg / L, and the deoiling rate of the steel plate is 82.1%, indicating that the addition of the degreasing composition further removes organic impurities such as oil and fat in the mixed solution 2, purifies the water quality, and the obtained supernatant is recovered.
[0098] This specific embodiment is merely an explanation of the present application and is not a limitation of the present application. After reading this specification, those skilled in the art may make non-creative modifications to the present embodiment as needed, but as long as they are within the scope of the claims of the present application, they are protected by the patent law.
Claims
1. A process for treating and recovering hot-dip galvanizing and phosphating wastewater, characterized in that: The steps include: (1) Add calcium hydroxide, calcium carbonate and calcium oxide to the phosphating wastewater, stir for 15-20 minutes, filter and obtain a mixed solution 1; (2) Add PAC, PAM and composite activated carbon to the mixed solution 1 obtained in step (1), stir for 35-40 minutes, and filter to obtain a mixed solution 2; (3) adding the degreasing composition to the mixed solution 2 obtained in step (2), stirring for 25-30 minutes, filtering to obtain a supernatant, and completing the treatment and recovery of hot-dip galvanizing and phosphating wastewater; The preparation method of the composite activated carbon comprises the following steps: (1) Coconut shells, straws and bamboo poles are crushed separately, then mixed, soaked in hydrochloric acid for 1-2 hours, washed with water, calcined at 500-520°C for 1-1.5 hours, then heated to 1300-1350°C and calcined for 3-4 hours, washed and dried after calcination to obtain a carbonized product; (2) Dispersing the modified sepiolite fiber in deionized water, adding the carbonized product obtained in step (1), acetic acid, chitosan and metal organic framework material, stirring for 1-2 hours, and drying to obtain composite activated carbon.
2. A process for treating and recycling hot-dip galvanizing and phosphating wastewater according to claim 1, characterized in that: The mass ratio of the coconut shell, the straw and the bamboo pole is 1:0.5-0.7:2-6.
3. A process for treating and recovering hot-dip galvanizing and phosphating wastewater according to claim 1, characterized in that: The mass ratio of the modified sepiolite fiber, the carbonized material, the chitosan and the metal organic framework material is 0.6-0.9:1:0.2-0.4:0.3-0.
5.
4. A process for treating and recycling hot-dip galvanizing and phosphating wastewater according to claim 1, characterized in that: The preparation method of the modified sepiolite fiber comprises the following steps: (1) Dispersing the sepiolite fiber in hydrochloric acid, soaking for 10-15 minutes, washing with water, and then dispersing it in an aqueous solution of a silane coupling agent, stirring for 30-35 minutes, and filtering to obtain pretreated sepiolite fiber; (2) The pretreated sepiolite fibers obtained in step (1) are dispersed in deionized water, and carbon nanotubes, hydroxymethyl cellulose and β-cyclodextrin are added and mixed, stirred for 30-35 minutes, and dried to obtain modified sepiolite fibers.
5. A process for treating and recovering hot-dip galvanizing and phosphating wastewater according to claim 4, characterized in that: The mass ratio of the sepiolite fiber, the carbon nanotube, the hydroxymethyl cellulose and the beta-cyclodextrin is 1:0.4-0.6:0.07-0.09:0.1-0.
2.
6. A process for treating and recycling hot-dip galvanizing and phosphating wastewater according to claim 1, characterized in that: The degreasing composition comprises the following raw materials: sodium carbonate, sodium dodecylbenzene sulfonate, sodium sulfate, N-benzyldiethanolamine, modified diatomaceous earth, sodium gluconate, ethanol, sodium lignin sulfonate and the balance of water.
7. A process for treating and recycling hot-dip galvanizing and phosphating wastewater according to claim 6, characterized in that: The degreasing composition comprises, by weight, 30-50 parts of sodium carbonate, 10-14 parts of sodium dodecylbenzene sulfonate, 15-18 parts of sodium sulfate, 6-9 parts of N-benzyldiethanolamine, 12-15 parts of modified diatomaceous earth, 5-8 parts of sodium gluconate, 20-25 parts of ethanol, 4-7 parts of sodium lignin sulfonate, and the balance of water.
8. A process for treating and recycling hot-dip galvanizing and phosphating wastewater according to claim 6, characterized in that: The preparation method of the modified diatomite comprises the following steps: (1) Disperse diatomaceous earth in ammonia water, stir for 2-3 minutes, wash with water, and then disperse in deionized water, add sodium hexadecylbenzene sulfonate and talcum powder, stir evenly, and set aside; (2) Dispersing the activated carbon in deionized water, adding potassium oxalate and sodium citrate, stirring for 10-20 minutes, and filtering to obtain pretreated activated carbon; (3) Add the pretreated activated carbon obtained in step (2) to the diatomaceous earth obtained in step (1), stir evenly, and dry to obtain modified diatomaceous earth.
9. A process for treating and recycling hot-dip galvanizing and phosphating wastewater according to claim 8, characterized in that: The mass ratio of the diatomaceous earth, sodium hexadecylbenzenesulfonate and talcum powder is 1:0.1-0.3:0.2-0.
4.
10. A process for treating and recycling hot-dip galvanizing and phosphating wastewater according to claim 8, characterized in that: The mass ratio of the diatomaceous earth, potassium oxalate and sodium citrate is 1:0.3-0.6:0.2-0.5.