Preparation method of octenyl succinic acid high-branch cyclodextrine ester and application of octenyl succinic acid high-branch cyclodextrine ester in preparation of Pickering emulsion
By modifying highly branched cyclic dextrins with octenyl succinic anhydride esterification, the problems of low substitution degree and emulsification stability of octenyl succinic anhydride starch esters were solved. The prepared octenyl succinic acid highly branched cyclic dextrin esters exhibited excellent emulsification performance and stability of bioactive substances in functional emulsions, thus expanding their application fields.
Patent Information
- Application Number
- CN202410899656.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-05
- Publication Date
- 2024-11-12
AI Technical Summary
In the existing technology, octenyl succinic anhydride starch ester has a low degree of substitution, and its emulsification stability and thermal stability are not ideal. Highly branched cyclodextrins do not have the ability to encapsulate milk droplets, which limits their application in functional food processing.
Highly branched cyclic dextrin esters of octenyl succinic anhydride were prepared by esterification modification of starch with branching enzymes to generate highly branched cyclic dextrins. Glycerol was used as a solvent and N-carbonyldiimidazole as a catalyst in a falling film reactor for esterification reaction. Extraction and separation were performed using pyridinium trifluoromethanesulfonate ammonium ionic liquid.
It improves the emulsifying properties of octenyl succinic acid highly branched cyclic dextrin ester, enhances the stability and bioavailability of bioactive substances, and broadens its application range in the production of functional emulsions, special foods, and pharmaceuticals.
Smart Images

Figure CN118930669A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of emulsion preparation, and particularly relates to a preparation method of octenylsuccinic acid highly branched cyclodextrin ester and application of the same in the preparation of Pickering emulsion. Background Art
[0002] Octenyl succinic anhydride starch ester is a type of highly safe food emulsifier thickener obtained by esterifying starch with octenyl succinic anhydride. my country's national food safety standards stipulate that the amount of octenyl succinic anhydride added to octenyl succinic anhydride starch ester shall not exceed 3%. However, starch usually exists in the form of particles. When 3% octenyl succinic anhydride is added, the degree of substitution on the starch molecules is not uniform and the degree of substitution is low, usually not exceeding 0.02. In addition, octenyl succinic anhydride starch ester has a high degree of crystallinity and is prone to aging, which limits its widespread use in practical applications.
[0003] Highly branched cyclodextrin is a new type of dextrin composed of a ring structure and many short linear chains. It has many excellent properties such as high embedding rate, good hydrophilicity, easy gelatinization, delayed aging, fast gastric emptying, etc. It can be used as a special functional raw material in the fields of food, medicine and biomaterials. However, highly branched cyclodextrin does not have the unique cavity structure similar to cyclodextrin, so it does not have good encapsulation performance for emulsion droplets, which makes it impossible to be used as an emulsifier in the processing of functional foods.
[0004] The present invention successfully prepares a novel octenyl succinic acid highly branched cyclodextrin ester by esterification modification of highly branched cyclodextrin with octenyl succinic anhydride. Highly branched cyclodextrin makes up for the defects of starch such as large relative molecular weight, high viscosity, and complex crystal structure, and solves the problems existing in the field of octenyl succinic anhydride modified starch, such as difficulty in increasing degree of substitution, low reaction efficiency, unsatisfactory emulsification stability, and thermal stability. The octenyl succinic acid highly branched cyclodextrin ester prepared by the present invention is used to load biologically active substances, which can effectively improve the stability, solubility, and bioavailability of the biologically active substances. The present invention opens up a new way for the production of functional emulsions and the production of foods and medicines with unique physiological functions. Summary of the invention
[0005] The purpose of the present invention is to provide a method for preparing highly branched cyclodextrin octenylsuccinate and its application in the preparation of Pickering emulsion. The highly branched cyclodextrin octenylsuccinate obtained by the preparation method has greatly improved emulsification performance, and the bioavailability and stability of the loaded bioactive substances are improved.
[0006] The present invention is achieved through the following technical solutions: A method for preparing octenylsuccinic acid highly branched cyclodextrin ester comprises the following steps: S1. Preparation of highly branched cyclodextrin: weigh a certain amount of pregelatinized waxy corn starch, add Tris-HCl buffer with a pH of 7.0, add a certain amount of enzyme to modify the pregelatinized waxy corn starch, after the reaction is terminated, cool the reaction solution to room temperature and centrifuge, filter the supernatant through a filter membrane, add anhydrous ethanol to the filtered solution to precipitate highly branched cyclodextrin, centrifuge until no sugar is detected in the supernatant by phenol-sulfuric acid method, dry the precipitate, and obtain highly branched cyclodextrin; S2. Preparation of octenyl succinic anhydride-glycerol solution: Weigh a certain amount of glycerol, add it to 3% (based on the dry basis weight of highly branched cyclodextrin) of octenyl succinic anhydride, heat until completely dissolved, and slowly add the mixture into ice water under the action of a high-speed shear disperser to obtain an octenyl succinic anhydride-glycerol solution; S3, esterification reaction: accurately weigh a certain amount of highly branched cyclodextrin and disperse it in deionized water to obtain a highly branched cyclodextrin emulsion (35%, w / v), and place the highly branched cyclodextrin emulsion (35%, w / v), octenyl succinic anhydride-glycerol solution, esterification catalyst (4%, w / v), and 0.5 mol / L NaOH solution in a falling film reactor for esterification reaction; S4, vacuum concentration: adjust the pH of the solution to 7.0-7.5 with 1M HCl solution, send the solution to a vacuum drying oven, and vacuum concentrate at 80-100°C to concentrate the moisture content of the material to less than 10% (w / v); S5, spray drying: the material is fed into the spray dryer at a rate of 90L / h, the inlet and outlet temperatures are 130-150℃ and 80-100℃ respectively, and the solid particles are collected; S6, purification: the solid particles obtained in step S5 are extracted and separated with ionic liquid. After the extraction is completed, centrifuge at 10000r / min for 10-15min, and the precipitate is placed in a 60°C oven to dry to obtain a sample of octenylsuccinic acid highly branched cyclodextrin ester. The ionic liquid after the reaction is recovered for next use.
[0007] Furthermore, the enzyme in step S1 is a branching enzyme.
[0008] The specific operation of step S1 is as follows: weigh a certain amount of pregelatinized waxy corn starch, add Tris-HCl buffer (pH 7.0), adjusted to a 10% (w / v) suspension; added a certain amount of branching enzyme (0.1U / mL reactant), placed in a 60°C water bath, mechanically stirred at 150-200r / min, reacted for 2h, hydrolyzed the ɑ-1,4 glycosidic bond of the reactant, generated the ɑ-1,6 glycosidic bond, promoted the cyclization reaction, and generated short branched chains; the reactant solution was incubated at 121°C for 10min to terminate the branching enzyme reaction; the post-reaction solution was cooled to room temperature, centrifuged at 10000r / min for 10-15min, and the supernatant was filtered through a 0.22μm filter membrane to remove insoluble precipitates; an equal volume of anhydrous ethanol was added to the filtered solution to precipitate highly branched cyclodextrin, and centrifuged at 10000r / min for 10-15min until no sugar was detected in the supernatant by the phenol-sulfuric acid method, and the precipitate was placed in a 60°C oven to dry to obtain highly branched cyclodextrin.
[0009] Furthermore, the esterification catalyst is N-carbonyldiimidazole.
[0010] Furthermore, the specific operation of step S3 is as follows: a highly branched cyclodextrin emulsion (35%, w / v) prepared by highly branched cyclodextrin, an octenylsuccinic anhydride-glycerol solution, N-carbonyldiimidazole (4%, w / v), and a 0.5 mol / L NaOH solution are added to a falling film reactor through a feed port, the temperature is raised to 40-60°C, and the temperature is kept for 5-10 minutes, and the material is transferred to the falling film reactor through a feed pump, and the feed speed is controlled at 4.0-5.0 m / s. 3 / h, ensure that the liquid forms a uniform film on the inner wall of the reactor, the temperature is controlled at 40-60°C, the relative vacuum degree of the reaction is controlled at -98kPa to -78kPa, and a cyclic esterification reaction is carried out. During the esterification reaction, the pH is controlled at 8.0-8.5, the esterification time is 1-2h, and after the reaction is completed, the product is collected from the outlet of the reactor into a product collection tank.
[0011] Furthermore, in step S6, the ionic liquid is 20%-40% (w / v) pyridinium ammonium trifluoromethanesulfonate.
[0012] The present invention also provides a method for preparing a Pickering emulsion loaded with biologically active substances using the highly branched octenyl succinic acid cyclodextrin ester, comprising the following steps: accurately weighing a certain amount of the highly branched octenyl succinic acid cyclodextrin ester and dispersing it in deionized water, magnetically stirring at 75°C for 30 minutes, and then cooling to room temperature to obtain a suspension of the highly branched octenyl succinic acid cyclodextrin ester for standby use, adding an appropriate amount of soybean oil containing 0.01% (w / v) biologically active substances to the suspension to obtain a final mixture containing 30% (w / v) highly branched octenyl succinic acid cyclodextrin ester and 20% (v / v) oil; using a high-pressure homogenizer at 25000r / min for homogenization for 3 minutes; wrapping the entire device and the flask with aluminum foil to obtain a Pickering emulsion of the highly branched octenyl succinic acid cyclodextrin ester loaded with biologically active substances.
[0013] Furthermore, the bioactive substance is one of α-tocopherol, β-carotene and curcumin.
[0014] The beneficial effects of the present invention are embodied in: (1) The present invention uses branching enzymes to modify pregelatinized waxy corn starch to produce highly branched cyclodextrins, and the process is green and safe. Branching enzymes can catalyze the hydrolysis of starch ɑ-1,4 glycosidic bonds and the generation of ɑ-1,6 glycosidic bonds, promote the generation of branches, and act on the b chains in starch to degrade starch through cyclization reactions to produce highly branched cyclodextrins with a certain molecular weight. The highly branched cyclodextrins produced by enzyme modification have a low average molecular weight and a narrow distribution, low viscosity, and a high branch content. They have the advantages of easy gelatinization, delayed aging and regeneration, and not easy to crystallize during processing. The highly branched cyclodextrins produced by the present invention are used as raw materials to carry out octenyl succinic anhydride esterification reaction, which solves the problem that octenyl succinic anhydride starch esters have high crystallinity and are prone to aging, broadens the application of highly branched cyclodextrins, improves the emulsification properties of highly branched cyclodextrins, and provides new ideas for the production of functional emulsions.
[0015] The present invention selects emulsifier glycerol to replace the organic solvent anhydrous ethanol to treat octenyl succinic anhydride. Glycerol, as a polyhydroxy alcohol, has the dual characteristics of hydrophilicity and lipophilicity like anhydrous ethanol. During the dissolution process of octenyl succinic anhydride, the hydroxyl group in glycerol forms a hydrogen bond with the carboxyl group in octenyl succinic anhydride, and the strong interaction between molecules promotes the octenyl succinic anhydride to be better dispersed and dissolved in the system. The present invention reduces the use frequency of anhydrous ethanol in the production process of octenyl succinic acid high-branched cyclodextrin ester, and provides a new idea for the application of emulsifiers in the modification of octenyl succinic anhydride.
[0016] (3) The preparation of the present invention uses N-carbonyldiimidazole (CDI) as an esterification catalyst. N-carbonyldiimidazole can react with octenylsuccinic anhydride to generate an unstable intermediate, and this intermediate can react with highly branched cyclodextrin to generate the corresponding ester. Compared with the case without adding N-carbonyldiimidazole, the esterification reaction efficiency is significantly improved. The present invention solves the problem of low reaction efficiency in the esterification process of octenylsuccinic acid.
[0017] (4) The present invention adopts a falling film reactor for esterification reaction. The falling film reactor is a new type of reaction device. The reactants slide down along the reactor wall and fully contact the wall surface to form a thin film layer. The reactants contact the reactants on the wall surface through this thin film to react. During the reaction, the reactants enter the reactor from the top, react on the wall surface, and the waste liquid is discharged from the bottom. At present, the production of octenyl succinic anhydride starch ester generally adopts a kettle reactor, which has the disadvantages of high energy consumption, long time, and relatively low reaction efficiency. The film layer of the falling film reactor is very thin, so the material transfer speed is very fast, and the reaction is more complete, which can obtain a higher reaction rate and yield than the kettle reactor. The present invention solves the problems of low esterification efficiency and low degree of substitution in the field of octenyl succinic anhydride starch ester.
[0018] (5) The present invention uses pyridinium ammonium trifluoromethanesulfonate ionic liquid for extraction and separation. The cation (Py + ) can form ion pairs with anions in the crude product, and can effectively dissolve octenyl succinic anhydride and chloride ions, thereby realizing the extraction and separation of octenyl succinic acid high-branched cyclodextrin esters. At present, the separation and purification of octenyl succinic anhydride starch esters generally adopts the alcohol washing method. Compared with ethanol, ionic liquids, as a new type of green solvent, have the advantages of low volatility, high thermal stability, good chemical stability, and are easy to recycle. In addition, ionic liquids can also adjust their physical and chemical properties according to the extraction requirements, showing greater flexibility.
[0019] (6) The present invention uses octenyl succinic anhydride to esterify the highly branched cyclodextrin, and introduces ester groups to give the highly branched cyclodextrin lipophilicity, thereby solving the problem of poor hydrophobicity of the highly branched cyclodextrin, so that it can be used as an emulsifier for the production of functional emulsion foods. In addition, the highly branched cyclodextrin octenyl succinic acid ester is closely arranged in the emulsion to form a dense oil-water interface film, which reduces the impact of the external adverse environment on the bioactive substances, improves the stability and bioavailability of the bioactive substances, and can be used as a transfer medium for the production of special foods and medicines. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 It is a schematic diagram of the molecular weight of highly branched cyclodextrin.
[0021] Figure 2 It is the Fourier infrared spectrum of highly branched cyclodextrin and highly branched cyclodextrin octenylsuccinate.
[0022] Figure 3 This is a microscopic morphology of the Pickering emulsion based on octenyl succinic acid highly branched cyclodextrin ester.
[0023] Figure 4 Schematic diagram of the centrifugal stability of octenylsuccinic acid highly branched cyclodextrin ester-based Pickering emulsion. DETAILED DESCRIPTION
[0024] The technical solution of the present invention is described in detail below in conjunction with specific embodiments to facilitate understanding of the present invention, but is not intended to limit the present invention.
[0025] Example 1: Construction of Pickering emulsion based on highly branched cyclodextrin octenylsuccinate (1) Preparation of highly branched cyclodextrin: Weigh a certain amount of pregelatinized waxy corn starch and add Tris-HCl buffer (pH 7.0), adjusted to a 10% (w / v) suspension; added a certain amount of branching enzyme (0.1U / mL reactant), placed in a 60°C water bath, mechanically stirred at 150-200r / min, reacted for 2h, hydrolyzed the ɑ-1,4 glycosidic bonds of the reactants, generated ɑ-1,6 glycosidic bonds, promoted cyclization reactions, and generated short branches; the reactant solution was incubated at 121°C for 10min to terminate the branching enzyme reaction; the post-reaction solution was cooled to room temperature, centrifuged at 10000r / min for 10-15min, and the supernatant was filtered through a 0.22μm filter membrane to remove insoluble precipitates; an equal volume of anhydrous ethanol was added to the filtered solution to precipitate highly branched cyclodextrins, and the solution was centrifuged at 10000r / min for 10-15min until no sugar was detected in the supernatant by the phenol-sulfuric acid method, and highly branched cyclodextrins were obtained.
[0026] (2) Preparation of octenyl succinic anhydride-glycerol solution: Weigh a certain amount of glycerol, add it to 3% (based on the dry basis weight of highly branched cyclodextrin) of octenyl succinic anhydride, heat until it is completely dissolved, and slowly add the mixture into ice water under the action of a high-speed shear disperser to obtain an octenyl succinic anhydride-glycerol solution.
[0027] (3) Esterification reaction: accurately weigh a certain amount of highly branched cyclodextrin and disperse it in deionized water to obtain a highly branched cyclodextrin emulsion (35%, w / v). Add the highly branched cyclodextrin emulsion (35%, w / v), octenylsuccinic anhydride-glycerol, N-carbonyldiimidazole (4%, w / v), and 0.5 mol / L NaOH solution into the falling film reactor through the feed port. Raise the temperature to 40-60°C and keep it warm for 5-10 min. Transfer the material to the falling film reactor through the feed pump and control the feed speed to 4.0-5.0 m / s. 3 / h, ensure that the liquid forms a uniform film on the inner wall of the reactor, the temperature is controlled at 40-60°C, the relative vacuum degree of the reaction is controlled at -98kPa to -78kPa, and a cyclic esterification reaction is carried out. During the esterification reaction, the pH is controlled at 8.0-8.5, the esterification time is 1-2h, and after the reaction is completed, the product is collected from the outlet of the reactor into a product collection tank.
[0028] (4) Vacuum concentration: The pH of the reactant is adjusted to 7.0-7.5 with 1M HCl solution, and the solution is sent to a vacuum drying oven for vacuum concentration at 80-100°C to concentrate the water content of the material to less than 10% (w / v).
[0029] (5) Spray drying: The material is fed into a spray dryer at a rate of 90 L / h, with inlet and outlet temperatures of 130-150 °C and 80-100 °C, respectively, and solid particles are collected.
[0030] (6) Purification: The collected solid particles are extracted and separated with an equal volume of 20%-40% (w / v) pyridinium ammonium trifluoromethanesulfonate ionic liquid. After the extraction is completed, centrifuge at 10,000 r / min for 10-15 min, and the precipitate is placed in a 60°C oven to dry to obtain an octenylsuccinic acid highly branched cyclodextrin ester sample. The ionic liquid after the reaction is recovered for easy use next time.
[0031] (7) Construction of Pickering emulsion based on highly branched cyclodextrin octenyl succinate: Accurately weigh a certain amount of highly branched cyclodextrin octenyl succinate and disperse it in deionized water to obtain a highly branched cyclodextrin octenyl succinate suspension. Add reagent grade soybean oil to the suspension to obtain a final mixture containing 30% (w / v) highly branched cyclodextrin octenyl succinate and 20% (v / v) oil. Use a high-pressure homogenizer at 25,000 r / min for homogenization for 3 min to obtain a Pickering emulsion based on highly branched cyclodextrin octenyl succinate.
[0032] Example 2: Construction of Pickering emulsion of octenylsuccinic acid highly branched cyclodextrin ester loaded with α-tocopherol (1) Preparation of highly branched cyclodextrin: Weigh a certain amount of pregelatinized waxy corn starch and add Tris-HCl buffer (pH 7.0), adjusted to a 10% (w / v) suspension; added a certain amount of branching enzyme (0.1U / mL reactant), placed in a 60°C water bath, mechanically stirred at 150-200r / min, reacted for 2h, hydrolyzed the ɑ-1,4 glycosidic bonds of the reactants, generated ɑ-1,6 glycosidic bonds, promoted cyclization reactions, and generated short branches; the reactant solution was incubated at 121°C for 10min to terminate the branching enzyme reaction; the post-reaction solution was cooled to room temperature, centrifuged at 10000r / min for 10-15min, and the supernatant was filtered through a 0.22μm filter membrane to remove insoluble precipitates; an equal volume of anhydrous ethanol was added to the filtered solution to precipitate highly branched cyclodextrins, and the solution was centrifuged at 10000r / min for 10-15min until no sugar was detected in the supernatant by the phenol-sulfuric acid method, and highly branched cyclodextrins were obtained.
[0033] (2) Preparation of octenyl succinic anhydride-glycerol solution: Weigh a certain amount of glycerol, add it to 3% (based on the dry basis weight of highly branched cyclodextrin) of octenyl succinic anhydride, heat until it is completely dissolved, and slowly add the mixture into ice water under the action of a high-speed shear disperser to obtain an octenyl succinic anhydride-glycerol solution.
[0034] (3) Esterification reaction: accurately weigh a certain amount of highly branched cyclodextrin and disperse it in deionized water to obtain a highly branched cyclodextrin emulsion (35%, w / v). Add the highly branched cyclodextrin emulsion (35%, w / v), octenylsuccinic anhydride-glycerol, N-carbonyldiimidazole (4%, w / v), and 0.5 mol / L NaOH solution into the falling film reactor through the feed port. Raise the temperature to 40-60°C and keep it warm for 5-10 min. Transfer the material to the falling film reactor through the feed pump and control the feed speed to 4.0-5.0 m / s. 3 / h, ensure that the liquid forms a uniform film on the inner wall of the reactor, the temperature is controlled at 40-60°C, the relative vacuum degree of the reaction is controlled at -98kPa to -78kPa, and a cyclic esterification reaction is carried out. During the esterification reaction, the pH is controlled at 8.0-8.5, the esterification time is 1-2h, and after the reaction is completed, the product is collected from the outlet of the reactor into a product collection tank.
[0035] (4) Vacuum concentration: The pH of the reactant is adjusted to 7.0-7.5 with 1M HCl solution, and the solution is sent to a vacuum drying oven for vacuum concentration at 80-100°C to concentrate the water content of the material to less than 10% (w / v).
[0036] (5) Spray drying: The material is fed into a spray dryer at a rate of 90 L / h, with inlet and outlet temperatures of 130-150 °C and 80-100 °C, respectively, and solid particles are collected.
[0037] (6) Purification: The collected solid particles are extracted and separated with an equal volume of 20%-40% (w / v) pyridinium ammonium trifluoromethanesulfonate ionic liquid. After the extraction is completed, centrifuge at 10,000 r / min for 10-15 min to obtain a highly branched cyclodextrin octenylsuccinate ester sample. The ionic liquid after the reaction is recovered for next use.
[0038] (7) Construction of Pickering emulsion of octenyl succinate highly branched cyclodextrin ester loaded with α-tocopherol: A certain amount of octenyl succinate highly branched cyclodextrin ester was suspended in deionized water, magnetically stirred at 75°C for 30 min, cooled to room temperature and set aside; an appropriate amount of soybean oil containing 1% (w / v) α-tocopherol was added to the octenyl succinate highly branched cyclodextrin ester solution to obtain a final mixture containing 30% (w / v) octenyl succinate highly branched cyclodextrin ester and 20% (v / v) oil, and homogenized for 3 min using a high-pressure homogenizer at 25,000 r / min. The entire apparatus and flask were wrapped with aluminum foil to avoid exposure during the preparation process, thereby obtaining a Pickering emulsion of octenyl succinate highly branched cyclodextrin ester loaded with α-tocopherol.
[0039] Example 3: Construction of Pickering emulsion of octenylsuccinic acid highly branched cyclodextrin ester loaded with β-carotene (1) Preparation of highly branched cyclodextrin: Weigh a certain amount of pregelatinized waxy corn starch and add Tris-HCl buffer (pH 7.0), adjusted to a 10% (w / v) suspension; added a certain amount of branching enzyme (0.1U / mL reactant), placed in a 60°C water bath, mechanically stirred at 150-200r / min, reacted for 2h, hydrolyzed the ɑ-1,4 glycosidic bonds of the reactants, generated ɑ-1,6 glycosidic bonds, promoted cyclization reactions, and generated short branches; the reactant solution was incubated at 121°C for 10min to terminate the branching enzyme reaction; the post-reaction solution was cooled to room temperature, centrifuged at 10000r / min for 10-15min, and the supernatant was filtered through a 0.22μm filter membrane to remove insoluble precipitates; an equal volume of anhydrous ethanol was added to the filtered solution to precipitate highly branched cyclodextrins, and the solution was centrifuged at 10000r / min for 10-15min until no sugar was detected in the supernatant by the phenol-sulfuric acid method, and highly branched cyclodextrins were obtained.
[0040] (2) Preparation of octenyl succinic anhydride-glycerol solution: Weigh a certain amount of glycerol, add it to 3% (based on the dry basis weight of highly branched cyclodextrin) of octenyl succinic anhydride, heat until it is completely dissolved, and slowly add the mixture into ice water under the action of a high-speed shear disperser to obtain an octenyl succinic anhydride-glycerol solution.
[0041] (3) Esterification reaction: accurately weigh a certain amount of highly branched cyclodextrin and disperse it in deionized water to obtain a highly branched cyclodextrin emulsion (35%, w / v). Add the highly branched cyclodextrin emulsion (35%, w / v), octenylsuccinic anhydride-glycerol, N-carbonyldiimidazole (4%, w / v), and 0.5 mol / L NaOH solution into the falling film reactor through the feed port. Raise the temperature to 40-60°C and keep it warm for 5-10 min. Transfer the material to the falling film reactor through the feed pump and control the feed speed to 4.0-5.0 m / s. 3 / h, ensure that the liquid forms a uniform film on the inner wall of the reactor, the temperature is controlled at 40-60°C, the relative vacuum degree of the reaction is controlled at -98kPa to -78kPa, and a cyclic esterification reaction is carried out. During the esterification reaction, the pH is controlled at 8.0-8.5, the esterification time is 1-2h, and after the reaction is completed, the product is collected from the outlet of the reactor into a product collection tank.
[0042] (4) Vacuum concentration: The pH of the reactant is adjusted to 7.0-7.5 with 1M HCl solution, and the solution is sent to a vacuum drying oven for vacuum concentration at 80-100°C to concentrate the water content of the material to less than 10% (w / v).
[0043] (5) Spray drying: The material is fed into a spray dryer at a rate of 90 L / h, with inlet and outlet temperatures of 130-150 °C and 80-100 °C, respectively, and solid particles are collected.
[0044] (6) Purification: The collected solid particles are extracted and separated with an equal volume of 20%-40% (w / v) pyridinium ammonium trifluoromethanesulfonate ionic liquid. After the extraction is completed, centrifuge at 10,000 r / min for 10-15 min, and the precipitate is placed in a 60°C oven to dry to obtain an octenylsuccinic acid highly branched cyclodextrin ester sample. The ionic liquid after the reaction is recovered for easy use next time.
[0045] (7) Preparation of Pickering emulsion of octenyl succinate highly branched cyclodextrin ester loaded with β-carotene: A certain amount of octenyl succinate highly branched cyclodextrin ester was suspended in deionized water, magnetically stirred at 75°C for 30 min, cooled to room temperature and set aside; an appropriate amount of soybean oil containing 0.1% (w / v) β-carotene was added to the octenyl succinate highly branched cyclodextrin ester solution to obtain a final mixture containing 30% (w / v) octenyl succinate highly branched cyclodextrin ester and 20% (v / v) oil, and homogenized for 3 min using a high-pressure homogenizer at 25,000 r / min; the entire apparatus and flask were wrapped with aluminum foil to avoid exposure during the preparation process, and a Pickering emulsion of octenyl succinate highly branched cyclodextrin ester loaded with β-carotene was obtained.
[0046] Example 4: Construction of Pickering emulsion of octenylsuccinic acid highly branched cyclodextrin ester loaded with curcumin (1) Preparation of highly branched cyclodextrin: Weigh a certain amount of pregelatinized waxy corn starch and add Tris-HCl buffer (pH 7.0), adjusted to a 10% (w / v) suspension; added a certain amount of branching enzyme (0.1U / mL reactant), placed in a 60°C water bath, mechanically stirred at 150-200r / min, reacted for 2h, hydrolyzed the ɑ-1,4 glycosidic bonds of the reactants, generated ɑ-1,6 glycosidic bonds, promoted cyclization reactions, and generated short branches; the reactant solution was incubated at 121°C for 10min to terminate the branching enzyme reaction; the post-reaction solution was cooled to room temperature, centrifuged at 10000r / min for 10-15min, and the supernatant was filtered through a 0.22μm filter membrane to remove insoluble precipitates; an equal volume of anhydrous ethanol was added to the filtered solution to precipitate highly branched cyclodextrins, and the solution was centrifuged at 10000r / min for 10-15min until no sugar was detected in the supernatant by the phenol-sulfuric acid method, and highly branched cyclodextrins were obtained.
[0047] (2) Preparation of octenyl succinic anhydride-glycerol solution: Weigh a certain amount of glycerol, add it to 3% (based on the dry basis weight of highly branched cyclodextrin) of octenyl succinic anhydride, heat until it is completely dissolved, and slowly add the mixture into ice water under the action of a high-speed shear disperser to obtain an octenyl succinic anhydride-glycerol solution.
[0048] (3) Esterification reaction: accurately weigh a certain amount of highly branched cyclodextrin and disperse it in deionized water to obtain a highly branched cyclodextrin emulsion (35%, w / v). Add the highly branched cyclodextrin emulsion (35%, w / v), octenylsuccinic anhydride-glycerol, N-carbonyldiimidazole (4%, w / v), and 0.5 mol / L NaOH solution into the falling film reactor through the feed port. Raise the temperature to 40-60°C and keep it warm for 5-10 min. Transfer the material to the falling film reactor through the feed pump and control the feed speed to 4.0-5.0 m / s. 3 / h, ensure that the liquid forms a uniform film on the inner wall of the reactor, the temperature is controlled at 40-60°C, the relative vacuum degree of the reaction is controlled at -98kPa to -78kPa, and a cyclic esterification reaction is carried out. During the esterification reaction, the pH is controlled at 8.0-8.5, the esterification time is 1-2h, and after the reaction is completed, the product is collected from the outlet of the reactor into a product collection tank.
[0049] (4) Vacuum concentration: The pH of the reactant is adjusted to 7.0-7.5 with 1M HCl solution, and the solution is sent to a vacuum drying oven for vacuum concentration at 80-100°C to concentrate the water content of the material to less than 10% (w / v).
[0050] (5) Spray drying: The material is fed into a spray dryer at a rate of 90 L / h, with inlet and outlet temperatures of 130-150 °C and 80-100 °C, respectively, and solid particles are collected.
[0051] (6) Purification: The collected solid particles are extracted and separated with an equal volume of 20%-40% (w / v) pyridinium ammonium trifluoromethanesulfonate ionic liquid. After the extraction is completed, centrifuge at 10,000 r / min for 10-15 min, and the precipitate is placed in a 60°C oven to dry to obtain an octenylsuccinic acid highly branched cyclodextrin ester sample. The ionic liquid after the reaction is recovered for easy use next time.
[0052] (7) Preparation of a Pickering emulsion of highly branched octenyl succinate cyclodextrin ester loaded with curcumin: A certain amount of highly branched octenyl succinate cyclodextrin ester was suspended in deionized water, magnetically stirred at 75°C for 30 min, and then cooled to room temperature for use; an appropriate amount of soybean oil containing 0.01% (w / v) curcumin was added to the highly branched octenyl succinate cyclodextrin ester solution to obtain a final mixture containing 30% (w / v) highly branched octenyl succinate cyclodextrin ester and 20% (v / v) oil; a high-pressure homogenizer was used at 25,000 r / min for homogenization for 3 min; the entire apparatus and flask were wrapped with aluminum foil to avoid exposure during the preparation process, and a Pickering emulsion of highly branched octenyl succinate cyclodextrin ester loaded with curcumin was obtained.
[0053] Experimental data characterization Figure 1 : is a molecular weight distribution diagram of highly branched cyclodextrin prepared by the method of the present invention. Figure 1 It can be seen that the molecular weight of highly branched cyclodextrin is about 200 KDa, and compared with starch, highly branched cyclodextrin has a smaller molecular weight and a narrower distribution range, which indicates that the highly branched cyclodextrin prepared by the method of the present invention can make up for the low degree of substitution and uneven substitution caused by the excessively large molecular weight and wide distribution range of ordinary starch during the esterification process.
[0054] Figure 2 The infrared spectra of highly branched cyclodextrin and highly branched cyclodextrin octenylsuccinate prepared by the method of the present invention are shown in FIG. Figure 2 It can be seen that the infrared spectra of octenyl succinate highly branched cyclodextrin ester and highly branched cyclodextrin are significantly different. Compared with highly branched cyclodextrin, octenyl succinate highly branched cyclodextrin ester has a higher infrared spectrum at 1723 cm −1 and 1570cm −1 A characteristic peak appeared at 1723cm −1 The peak at 1570 cm-1 is due to the carbonyl C=O stretching vibration of the ester group, while the peak at 1570 cm-1 is due to the carbonyl C=O stretching vibration of the ester group. −1 The peak at is the symmetrical stretching of carboxyl vibration, indicating that the method of the present invention is successfully used to prepare octenyl succinic acid high-branched cyclodextrin ester.
[0055] Figure 3 This is a microscope morphology of the octenyl succinic acid highly branched cyclodextrin ester-based Pickering emulsion prepared in Example 1. Figure 3 It can be seen that the particles are wrapped on the surface of the oil droplets, and some particles are dispersed in the water, which hinders the aggregation of the oil droplets and plays the role of a stabilizer. The droplet size is small, indicating that octenyl succinic acid high-branched cyclodextrin ester can be used as an emulsifier to stabilize the emulsion.
[0056] Figure 4 This is the infrared transmission spectrum of the centrifugal stability of the octenyl succinic acid highly branched cyclodextrin ester-based Pickering emulsion prepared in Example 1. Figure 4 It can be seen that when the Pickering emulsion of octenyl succinic acid highly branched cyclic dextrin ester reaches the final particle stratification position, the transmittance of the corresponding emulsion decreases and the change is more obvious, the particle migration rate decreases, and the ability to resist instability gradually increases. Its instability index is 0.088±0.022, and the instability index is low, indicating that octenyl succinic acid highly branched cyclic dextrin ester can be used as an emulsifier to stabilize the emulsion.
[0057] Table 1 shows the degree of substitution of different substrates by octenyl succinic anhydride. It can be seen from Table 1 that highly branched cyclodextrin ester of octenyl succinic acid shows a higher degree of substitution. Highly branched cyclodextrin has low viscosity, high water solubility, small molecular weight, easy gelatinization, not easy aging, and low degree of crystallization. After being treated with octenyl succinic anhydride, it shows a higher degree of substitution, which can solve the problems of low degree of substitution and uneven degree of substitution faced by current octenyl succinic anhydride.
[0058] Table 1 Degree of substitution of different substrates by octenylsuccinic anhydride
Claims
1. A method for preparing octenylsuccinic acid highly branched cyclodextrin ester, characterized in that: The steps include: S1. Preparation of highly branched cyclodextrin: weigh a certain amount of pregelatinized waxy corn starch, add Tris-HCl buffer with a pH of 7.0, add a certain amount of enzyme to modify the pregelatinized waxy corn starch, after the reaction is terminated, cool the reaction solution to room temperature and centrifuge, filter the supernatant through a filter membrane, add anhydrous ethanol to the filtered solution to precipitate highly branched cyclodextrin, centrifuge until no sugar is detected in the supernatant by phenol-sulfuric acid method, dry the precipitate, and obtain highly branched cyclodextrin; S2. Preparation of octenyl succinic anhydride-glycerol solution: Weigh a certain amount of glycerol, add it to 3% octenyl succinic anhydride, based on the dry basis mass of highly branched cyclodextrin, heat until completely dissolved, and slowly add the mixture into ice water under the action of a high-speed shear disperser to obtain an octenyl succinic anhydride-glycerol solution; S3, esterification reaction: accurately weigh a certain amount of highly branched cyclodextrin and disperse it in deionized water to obtain a highly branched cyclodextrin emulsion of 35%, w / v, and place the highly branched cyclodextrin emulsion of 35%, w / v, octenyl succinic anhydride-glycerol solution, esterification catalyst 4%, w / v, and 0.5 mol / L NaOH solution in a falling film reactor for esterification reaction; S4, vacuum concentration: adjust the pH of the reactant to 7.0-7.5 with 1M HCl solution, send the solution to a vacuum drying oven, and vacuum concentrate at 80-100°C to concentrate the moisture content of the material to less than 10% (w / v); S5, spray drying: the material is fed into the spray dryer at a rate of 90L / h, the inlet and outlet temperatures are 130-150℃ and 80-100℃ respectively, and the solid particles are collected; S6, purification: the solid particles obtained in step S5 are extracted and separated with ionic liquid. After the extraction is completed, centrifuge at 10000r / min for 10-15min, and the precipitate is placed in a 60°C oven to dry to obtain a sample of octenylsuccinic acid highly branched cyclodextrin ester. The ionic liquid after the reaction is recovered for next use.
2. The method for preparing octenylsuccinic acid highly branched cyclodextrin ester according to claim 1, characterized in that: The enzyme in step S1 is a branching enzyme.
3. The method for preparing octenylsuccinic acid highly branched cyclodextrin ester according to claim 2, characterized in that: The specific operation of step S1 is as follows: weigh a certain amount of pregelatinized waxy corn starch, add pH The method comprises the following steps: adjusting the suspension to 10% w / v by using 7.0 Tris-HCl buffer; adding a certain amount of branching enzyme (0.1 U / mL reactant), placing the reactant in a water bath at 60°C, mechanically stirring the reactant at a speed of 150-200 r / min, reacting the reactant for 2 hours, hydrolyzing the ɑ-1,4 glycosidic bond, generating the ɑ-1,6 glycosidic bond, promoting the cyclization reaction, and generating short branched chains; incubating the reactant solution at 121°C for 10 minutes to terminate the branching enzyme reaction; cooling the reaction solution to room temperature, centrifuging the reactant at 10000 r / min for 10-15 minutes, filtering the supernatant through a 0.22 μm filter membrane, and removing insoluble precipitates; adding an equal volume of anhydrous ethanol to the filtered solution to precipitate highly branched cyclodextrin, centrifuging the reactant at 10000 r / min for 10-15 minutes, until no sugar is detected in the supernatant by the phenol-sulfuric acid method, and drying the precipitate in a 60°C oven to obtain highly branched cyclodextrin.
4. The method for preparing octenylsuccinic acid highly branched cyclodextrin ester according to claim 1, characterized in that: The esterification catalyst is N-carbonyldiimidazole.
5. The method for preparing octenylsuccinic acid highly branched cyclodextrin ester according to claim 4, characterized in that: The specific operation of step S3 is as follows: adding a highly branched cyclodextrin emulsion (35%, w / v) prepared by highly branched cyclodextrin, an octenylsuccinic anhydride-glycerol solution, N-carbonyldiimidazole (4%, w / v), and a 0.5 mol / L NaOH solution to a falling film reactor through a feed port, raising the temperature to 40-60° C., keeping the temperature for 5-10 min, transferring the material to the falling film reactor through a feed pump, and controlling the feed speed to 4.0-5.0 m / s. 3 / h, ensure that the liquid forms a uniform film on the inner wall of the reactor, the temperature is controlled at 40-60℃, the relative vacuum degree of the reaction is controlled at -98kPa to -78kPa, and a cyclic esterification reaction is carried out. During the esterification reaction, the pH is controlled at 8.0-8.5, and the esterification time is 1-2h. After the reaction is completed, the product is collected from the outlet of the reactor into a product collection tank.
6. The method for preparing octenylsuccinic acid highly branched cyclodextrin ester according to claim 1, characterized in that: In step S6, the ionic liquid is 20%-40% (w / v) pyridinium ammonium trifluoromethanesulfonate.
7. A method for preparing a Pickering emulsion loaded with a biologically active substance using the highly branched cyclodextrin octenylsuccinate prepared by the preparation method of any one of claims 1 to 6, characterized in that: The method comprises the following steps: accurately weighing a certain amount of highly branched octenyl succinate cyclodextrin ester and dispersing it in deionized water, magnetically stirring at 75°C for 30 minutes, and then cooling to room temperature to obtain a highly branched octenyl succinate cyclodextrin ester suspension for use, adding an appropriate amount of soybean oil containing 0.01% (w / v) bioactive substances to the suspension to obtain a final mixture containing 30% (w / v) highly branched octenyl succinate cyclodextrin ester and 20% (v / v) oil; homogenizing for 3 minutes using a high-pressure homogenizer at 25000 r / min; and wrapping the entire device and the flask with aluminum foil to obtain a Pickering emulsion of highly branched octenyl succinate cyclodextrin ester loaded with bioactive substances.
8. The method for preparing a Pickering emulsion loaded with biologically active substances using highly branched cyclodextrin octenylsuccinate according to claim 7, characterized in that: The bioactive substance is one of α-tocopherol, β-carotene and curcumin.