High-modulus, low-stress-relaxation and easy-to-process polyurethane as well as preparation method and application thereof

By designing a full hard segment using a specific ratio of histamine-type chain extender, small molecule diol chain extender, and diisocyanate, polyurethane materials were prepared. This solved the processing difficulty and stress relaxation problems of invisible orthodontic appliance materials, achieving high modulus, low stress relaxation, and easy processing, making it suitable for invisible orthodontic appliances.

CN118930810AActive Publication Date: 2024-11-12SICHUAN UNIV
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202411403962.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-09
Publication Date
2024-11-12
Estimated Expiration
2044-10-09

AI Technical Summary

Technical Problem

Existing invisible orthodontic appliance materials suffer from problems such as high modulus material processing difficulty, unsatisfactory stress relaxation speed, and thickness affecting aesthetics and comfort, making it difficult to simultaneously possess high modulus, low stress relaxation, and easy processing characteristics.

Method used

Polyurethane materials were prepared by using a specific ratio of histamine-type chain extender, small molecule diol chain extender, diisocyanate and crosslinking agent, through full hard segment design, introducing dynamic bonds and appropriate crosslinking structures. The molar ratio of crosslinking agent to histamine-type chain extender was 1:(4~12), the molar ratio of diisocyanate to small molecule diol was (0.98~1.16):1, and the mass fraction of crosslinking agent was less than 1%.

Benefits of technology

It achieves high modulus, low stress relaxation and easy processing characteristics of polyurethane materials, significantly reduces processing temperature, and improves modulus and stress retention capabilities, making it suitable for invisible orthodontic appliance materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118930810A_ABST
    Figure CN118930810A_ABST
Patent Text Reader

Abstract

The invention provides high-modulus, low-stress relaxation and easy-to-process polyurethane as well as a preparation method and application thereof, and belongs to the field of biomedical materials. The polyurethane is prepared from the following raw materials: a histamine type chain extender, a small molecular dihydric alcohol chain extender, diisocyanate and a cross-linking agent; the molar ratio of the cross-linking agent to the histamine chain extender is 1: (4-12), the molar ratio of the diisocyanate to the micromolecular dihydric alcohol is (0.98-1.16): 1, and the mass fraction of the cross-linking agent in the raw materials is lower than 1%. The processing temperature of the polyurethane disclosed by the invention is obviously lower than that of a commercially available Isoplast-2530 product, the modulus and the stress retention capability are obviously improved, and the polyurethane has the potential of being used as an invisible tooth appliance material.
Need to check novelty before this filing date? Find Prior Art

Citation Information

Patent Citations

  • Environmentally friendly fluorescent water-based polyurethane and preparation method thereof

    CN106349449A

  • High-elasticity smooth and bright mirror-surface polyurethane resin and preparation method thereof

    CN106349454A

  • Method for recycling thermosetting polyurethane resin

    CN116375964A

  • Polyurea coating compositions

    US20030105220A1

  • Bone / Polyurethane Composites and Methods Thereof

    US20100112032A1