Broadband heat-conducting wave-absorbing material and preparation method thereof
By using silicone matrix, modified composite powder, molybdenum peroxidizing and hollow glass microbeads in absorbing materials, combined with electrostatic adsorption and silicone oil layer coating technology, the existing absorbing materials are limited in applications in high-frequency bands. and thickness sensitivity issues, efficient electromagnetic wave absorption in wide bands is achieved.
Patent Information
- Application Number
- CN202411045740.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-31
- Publication Date
- 2024-11-12
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing absorbent materials are limited in applications in higher frequency bands such as Ku, K, and Ka bands, and are sensitive to thickness changes, resulting in increased material complexity and application difficulty.
Using broadband thermally conductive wave absorbing materials including silicone matrix, modified composite powder, molybdenum peroxidizing, silicon carbide and hollow glass microbeads, the impedance matching and loss efficiency of electromagnetic waves are improved through electrostatic adsorption and silicone oil layer coating, and the thickness is reduced. rely.
The frequency band coverage of wave absorbing materials is broadened, the sensitivity to thickness changes is reduced, the loss efficiency of electromagnetic waves is improved, and it is suitable for Ku, K, and Ka bands.
Smart Images

Figure CN118931195A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of absorbing materials, and in particular to a broadband thermal conductive absorbing material and a preparation method thereof. Background Art
[0002] Absorbing materials refer to a type of material that can absorb or significantly reduce the electromagnetic wave energy received on its surface, thereby reducing the interference of electromagnetic waves. Common absorbing materials on the market include ferrites, carbon-based materials, and conductive polymers.
[0003] However, the effective (<-10db) absorbing frequency band of existing absorbing materials is generally 5-8GHz, and it is impossible to apply them in higher frequency bands such as Ku band (12-18GHz), K band (18-27GHz) and Ka band (26.5-40GHz); in addition, they are extremely sensitive to thickness changes, and the effective absorbing frequency band will change with the thickness. In order to meet the thickness requirements of different devices, different formulations need to be used to ensure specific absorbing performance, which increases the complexity of the material and the difficulty of application. Summary of the invention
[0004] In view of the above-mentioned problems, the present application is proposed to provide a broadband heat-conducting and wave-absorbing material and a preparation method thereof that overcomes the problems or at least partially solves the problems, including:
[0005] A broadband heat-conducting wave-absorbing material comprises, by mass, 600-800 parts of an organic silicon matrix, 7000-9000 parts of a modified composite powder, 400-600 parts of molybdenum permalloy, 400-600 parts of silicon carbide and 300-500 parts of hollow glass microspheres; wherein the modified composite powder comprises carbonyl iron powder, tetrapod zinc oxide electrostatically adsorbed on the surface of the carbonyl iron powder, and a silicone oil layer coated on the surface of the carbonyl iron powder and the tetrapod zinc oxide.
[0006] Preferably, the organic silicon matrix comprises vinyl silicone oil and hydrogen-containing silicone oil.
[0007] Preferably, the silicone oil layer includes a first silicone oil layer and a second silicone oil layer from the inside to the outside; the first silicone oil layer is octadecyltrimethoxysilane; and the second silicone oil layer is polydimethylsilicone.
[0008] Preferably, the particle size of the carbonyl iron powder is 8-12 μm; the particle size of the four-needle zinc oxide is 0.1-0.5 μm; the particle size of the molybdenum permalloy is 1-5 μm; the particle size of the silicon carbide is 38-42 μm; and the particle size of the hollow glass microspheres is 3-7 μm.
[0009] Preferably, the molybdenum permalloy is Fe3Ni3Mo4.
[0010] Preferably, the silicon carbide is β-type silicon carbide.
[0011] Preferably, it also includes: an inhibitor and a catalyst.
[0012] Preferably, the inhibitor is acetylene cyclohexanol.
[0013] Preferably, the catalyst is a platinum catalyst.
[0014] A method for preparing a broadband heat-conducting and wave-absorbing material as described in any one of the above items, comprising:
[0015] The electrostatically charged four-needle zinc oxide and carbonyl iron powder are stirred and mixed to obtain a composite powder;
[0016] The composite powder is mixed with a silicone oil solution by stirring, and then dried to obtain a modified composite powder;
[0017] The modified composite powder, molybdenum permalloy, silicon carbide, hollow glass microspheres, an organic silicon matrix, an inhibitor and a catalyst are stirred and mixed to obtain a prefabricated broadband thermal conductive wave absorbing material;
[0018] The prefabricated broadband heat-conducting and wave-absorbing material is cured to obtain the broadband heat-conducting and wave-absorbing material.
[0019] This application has the following advantages:
[0020] In the embodiments of the present application, with respect to the problems that the existing absorbing materials have a limited effective absorbing frequency band and are extremely sensitive to thickness changes, the present application provides a solution using hollow glass beads, modified composite powders and broadband absorbing powders, specifically: "A broadband thermal conductive absorbing material, comprising, by mass: 600-800 parts of an organic silicon matrix, 7000-9000 parts of a modified composite powder, 400-600 parts of molybdenum permalloy, 400-600 parts of silicon carbide and 300-500 parts of hollow glass beads; wherein the modified composite powder comprises carbonyl iron powder, tetra-needle zinc oxide electrostatically adsorbed on the surface of the carbonyl iron powder, and a silicone oil layer coated on the surface of the carbonyl iron powder and the tetra-needle zinc oxide". By adding hollow glass microbeads, the impedance matching of the absorbing material can be improved, allowing electromagnetic waves to enter the interior of the absorbing material more easily; by using modified composite powders, electromagnetic waves can be reflected and scattered multiple times inside, thereby improving the loss efficiency of electromagnetic waves and reducing dependence on material thickness; by using broadband absorbing powders such as carbonyl iron powder, molybdenum permalloy and silicon carbide, it can match electromagnetic waves in a wider frequency band, thereby effectively broadening the absorbing frequency band of the absorbing material. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] In order to more clearly illustrate the technical solution of the present application, the drawings required for use in the description of the present application will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0022] Figure 1 1 is a flow chart of the steps of a method for preparing a broadband heat-conducting and wave-absorbing material provided in one embodiment of the present application. DETAILED DESCRIPTION
[0023] In order to make the objects, features and advantages of the present application more obvious and understandable, the present application is further described in detail below in conjunction with the accompanying drawings and specific implementation methods. Obviously, the described embodiments are part of the embodiments of the present application, rather than all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in the field without creative work are within the scope of protection of the present application.
[0024] The inventors have found through analysis of the prior art that the absorbing material exhibits a good absorbing effect in a specific frequency band because its electromagnetic properties match the electromagnetic waves well in this frequency band. However, many absorbing materials can only effectively match electromagnetic waves in a specific frequency band (such as 5-8GHz), so they cannot be widely used in higher frequency bands (such as Ku band, K band and Ka band). In addition, the absorbing mechanism of the absorbing material is to convert the incident electromagnetic wave energy into heat energy or other forms of energy through dielectric loss, magnetic loss and the like. This requires the material to have appropriate dielectric and magnetic permeability properties and to be able to guide the electromagnetic waves into the material for loss in structure. However, the existing absorbing materials have insufficient control over the reflection and scattering of electromagnetic waves, and cannot effectively lose more electromagnetic wave energy, and thus cannot fully absorb electromagnetic waves, resulting in the absorbing performance being dependent on a specific thickness.
[0025] In one embodiment of the present application, a broadband thermal conductive wave absorbing material is provided, which comprises, by mass, 600-800 parts of an organic silicon matrix, 7000-9000 parts of a modified composite powder, 400-600 parts of molybdenum permalloy, 400-600 parts of silicon carbide, and 300-500 parts of hollow glass microspheres; wherein the modified composite powder comprises carbonyl iron powder, tetrapod zinc oxide electrostatically adsorbed on the surface of the carbonyl iron powder, and a silicone oil layer coated on the surface of the carbonyl iron powder and the tetrapod zinc oxide.
[0026] By adding hollow glass microbeads, the impedance matching of the absorbing material can be improved, allowing electromagnetic waves to enter the interior of the absorbing material more easily; by using modified composite powders, electromagnetic waves can be reflected and scattered multiple times inside, thereby improving the loss efficiency of electromagnetic waves and reducing dependence on material thickness; by using broadband absorbing powders such as carbonyl iron powder, molybdenum permalloy and silicon carbide, it can match electromagnetic waves in a wider frequency band, thereby effectively broadening the absorbing frequency band of the absorbing material.
[0027] Next, a broadband heat-conducting and wave-absorbing material in this exemplary embodiment will be further described.
[0028] In this embodiment, the organic silicon matrix includes vinyl silicone oil and hydrogen-containing silicone oil. As an example, the organic silicon matrix includes, by mass, 150-250 parts of the first vinyl silicone oil, 350-450 parts of the second vinyl silicone oil and 50-150 parts of the hydrogen-containing silicone oil; the viscosity of the first vinyl silicone oil is 2000mPa·s, and the vinyl content is 0.8%; the viscosity of the second vinyl silicone oil is 500mPa·s, and the vinyl content is 1.5%; the viscosity of the hydrogen-containing silicone oil is 50mPa·s, and the hydrogen content is 0.36%. Through the cross-linking reaction of vinyl and hydrogen groups, a stable three-dimensional network structure can be formed, which improves the strength and thermal stability of the material; through the combination of silicone oils of different viscosities, the material has appropriate adhesion and fluidity during the application process, which is convenient for construction and application.
[0029] In this embodiment, the silicone oil layer includes a first silicone oil layer and a second silicone oil layer from the inside to the outside; the first silicone oil layer is octadecyltrimethoxysilane; the second silicone oil layer is polydimethylsilicone. As an example, the viscosity of the octadecyltrimethoxysilane is 2-5mPa·s; the viscosity of the polydimethylsilicone is 20mPa·s. The octadecyltrimethoxysilane is coated on the surface of the tetrapin zinc oxide-carbonyl iron powder (ZnO-Fe) particles, which can prevent zinc oxide from falling off during subsequent processing or application, improve the stability of the ZnO-Fe particles, and improve the dispersibility of the ZnO-Fe particles in the silicone matrix, thereby improving the filling rate of the ZnO-Fe particles and ensuring the comprehensive performance of the material: the polydimethylsilicone is further coated on the surface of the ZnO-Fe particles, which can enhance the aging resistance and storage stability of the ZnO-Fe particles, making the material more stable during processing or application.
[0030] In this embodiment, the particle size of the carbonyl iron powder is 8-12μm; the particle size of the four-needle zinc oxide is 0.1-0.5μm; the particle size of the molybdenum permalloy is 1-5μm; the particle size of the silicon carbide is 38-42μm; and the particle size of the hollow glass microspheres is 3-7μm. The particle size of the four-needle zinc oxide is extremely small, which is conducive to electrostatic adsorption on the surface of the carbonyl iron powder to form a uniform adsorption layer and enhance the composite effect of the material. The small particle size of the molybdenum permalloy and the hollow glass microspheres helps to disperse evenly in the absorbing material, ensuring the uniformity and consistency of the absorbing effect. The large particle size of the silicon carbide helps to produce multiple scattering and reflection effects, extend the path of the electromagnetic wave in the material, and improve the absorbing efficiency.
[0031] In this embodiment, the four-needle zinc oxide is pre-treated at high temperature to grow the core crystal and shrink the length of the four needles to half of the original length. The high temperature treatment makes the zinc oxide core crystal grow, which improves the quality and stability of the crystal; the shrinkage of the length of the four needles to half of the original length can form a more compact and stable structure, and improve the dispersibility and filling rate of ZnO-Fe particles in the organic silicon matrix.
[0032] In this embodiment, the molybdenum permalloy is Fe3Ni3Mo4.
[0033] In this embodiment, the silicon carbide is β-type silicon carbide.
[0034] In this embodiment, it also includes: an inhibitor and a catalyst. As an example, the broadband thermal conductive wave absorbing material also includes: 18-22 parts of a catalyst and 1-3 parts of an inhibitor by weight. The catalyst can accelerate the cross-linking reaction and improve production efficiency; the inhibitor can prevent the reaction from being too fast, ensure uniformity, prevent side reactions from occurring, and improve durability.
[0035] In this embodiment, the inhibitor is acetylene cyclohexanol.
[0036] In this embodiment, the catalyst is a platinum catalyst.
[0037] In this embodiment, the thickness of the broadband heat-conducting and wave-absorbing material is 0.5-1.5 mm.
[0038] Reference Figure 1 In one embodiment of the present application, a method for preparing a broadband heat-conducting and wave-absorbing material as described in any of the above embodiments is provided, comprising:
[0039] S110, stirring and mixing the electrostatically charged four-needle zinc oxide and the carbonyl iron powder to obtain a composite powder;
[0040] S120, stirring and mixing the composite powder and the silicone oil solution, and drying the mixture to obtain a modified composite powder;
[0041] S130, stirring and mixing the modified composite powder, molybdenum permalloy, silicon carbide, hollow glass microspheres, organosilicon matrix, inhibitor and catalyst to obtain a prefabricated broadband thermal conductive wave absorbing material;
[0042] S140, curing the prefabricated broadband heat-conducting and wave-absorbing material to obtain the broadband heat-conducting and wave-absorbing material.
[0043] As described in step S110, the electrostatically charged four-needle zinc oxide and the carbonyl iron powder are stirred and mixed to obtain a composite powder.
[0044] The nanometer-scale four-needle zinc oxide is treated in a high-temperature furnace at 800°C for 4 hours, so that the inner core crystal grows and the length of the four needles shrinks to half of the original length, thereby obtaining pretreated four-needle zinc oxide; the pretreated four-needle zinc oxide is subjected to electrostatic treatment by an electrostatic adsorption device, so that the four-needle zinc oxide is charged with static electricity, thereby obtaining electrostatically charged four-needle zinc oxide; the electrostatically charged four-needle zinc oxide is stirred and mixed with carbonyl iron powder by a high-speed stirrer, so that the four-needle zinc oxide is uniformly adsorbed on the surface of the carbon-based iron powder, thereby obtaining a composite powder (i.e., ZnO-Fe particles), which is chestnut-shaped spherical particles under an electron microscope.
[0045] As described in step S120, the composite powder is stirred and mixed with the silicone oil solution, and dried to obtain a modified composite powder.
[0046] The composite powder is mixed with octadecyltrimethoxysilane so that the octadecyltrimethoxysilane is coated on the surface of the composite powder to form a first silicone oil layer; excess octadecyltrimethoxysilane is removed and dried to obtain a preliminarily coated composite powder; the preliminarily coated composite powder is mixed with polydimethylsilicone oil so that the polydimethylsilicone oil is coated on the surface of the preliminarily coated composite powder to form a second silicone oil layer; excess polydimethylsilicone oil is removed and dried to obtain a modified composite powder.
[0047] As described in step S130, the modified composite powder, molybdenum permalloy, silicon carbide, hollow glass microspheres, organic silicon matrix, inhibitor and catalyst are stirred and mixed to obtain a prefabricated broadband thermal conductive wave absorbing material.
[0048] The modified composite powder, molybdenum permalloy, silicon carbide, hollow glass microspheres, organosilicon matrix, inhibitor and catalyst are weighed according to the proportion, and the above components are stirred and mixed by a planetary power mixer to obtain a prefabricated broadband thermal conductive wave absorbing material.
[0049] As described in step S140, the prefabricated broadband heat-conducting and wave-absorbing material is cured to obtain the broadband heat-conducting and wave-absorbing material.
[0050] The prefabricated broadband heat-conducting and wave-absorbing material is placed in a tunnel furnace for high-temperature curing treatment, so that the prefabricated broadband heat-conducting and wave-absorbing material is vulcanized and formed to obtain the broadband heat-conducting and wave-absorbing material.
[0051] Embodiment 1:
[0052] A broadband heat-conducting wave-absorbing material, comprising, by mass, 200 parts of vinyl silicone oil with a viscosity of 2000 mPa·s, 400 parts of vinyl silicone oil with a viscosity of 500 mPa·s, 100 parts of hydrogenated silicone oil with a viscosity of 50 mPa·s, 8000 parts of modified composite powder, 4500 parts of Fe3Ni3Mo, 500 parts of β-type silicon carbide, 400 parts of hollow glass microspheres, 20 parts of catalyst and 2 parts of inhibitor; wherein the modified composite powder It includes carbonyl iron powder, four-needle zinc oxide electrostatically adsorbed on the surface of the carbonyl iron powder, and a silicone oil layer coated on the surface of the carbonyl iron powder and the four-needle zinc oxide; the particle size of the carbonyl iron powder is 10μm; the particle size of the four-needle zinc oxide is 0.3μm; the particle size of the Fe3Ni3Mo4 is 3μm; the particle size of the β-type silicon carbide is 40μm; the particle size of the hollow glass microspheres is 5μm; the thickness of the broadband thermal conductive wave absorbing material is 1.5mm.
[0053] The preparation method of the broadband thermal conductive wave absorbing material comprises: treating the four-needle zinc oxide in a high-temperature furnace at 800°C for 4 hours, so that the inner core crystal grows and the length of the four needles shrinks to half of the original length, thereby obtaining pre-treated four-needle zinc oxide; electrostatically treating the pre-treated four-needle zinc oxide by an electrostatic adsorption device, so that the four-needle zinc oxide is electrostatically charged, thereby obtaining electrostatically charged four-needle zinc oxide; stirring and mixing the electrostatically charged four-needle zinc oxide with carbonyl iron powder by a high-speed mixer, so that the four-needle zinc oxide is uniformly adsorbed on the surface of the carbon-based iron powder, thereby obtaining a composite powder. The composite powder is mixed with silicone oil, so that the silicone oil is coated on the surface of the composite powder to form a silicone oil layer; the excess silicone oil is removed and dried to obtain a modified composite powder. The modified composite powder, molybdenum permalloy, silicon carbide, hollow glass microspheres, organosilicon matrix, inhibitor and catalyst are weighed according to the ratio, and the above components are stirred and mixed by a planetary power mixer to obtain a prefabricated broadband thermal conductive wave absorbing material. The prefabricated broadband heat-conducting and wave-absorbing material is placed in a tunnel furnace for high-temperature curing treatment, so that the prefabricated broadband heat-conducting and wave-absorbing material is vulcanized and formed to obtain the broadband heat-conducting and wave-absorbing material.
[0054] Embodiment 2:
[0055] A broadband heat-conducting wave-absorbing material, comprising, by mass: 200 parts of vinyl silicone oil with a viscosity of 2000 mPa·s, 400 parts of vinyl silicone oil with a viscosity of 500 mPa·s, 100 parts of hydrogenated silicone oil with a viscosity of 50 mPa·s, 8000 parts of modified composite powder, 4500 parts of Fe3Ni3Mo, 500 parts of β-type silicon carbide, 400 parts of hollow glass microspheres, 20 parts of catalyst and 2 parts of inhibitor; wherein the modified composite powder The body includes carbonyl iron powder, four-needle zinc oxide electrostatically adsorbed on the surface of the carbonyl iron powder, and a silicone oil layer coated on the surface of the carbonyl iron powder and the four-needle zinc oxide; the particle size of the carbonyl iron powder is 10μm; the particle size of the four-needle zinc oxide is 0.3μm; the particle size of the Fe3Ni3Mo4 is 3μm; the particle size of the β-type silicon carbide is 40μm; the particle size of the hollow glass microspheres is 5μm; the thickness of the broadband thermal conductive wave absorbing material is 1mm.
[0056] The preparation method of the broadband thermal conductive wave absorbing material is the same as that of Example 1.
[0057] Embodiment 3:
[0058] A broadband heat-conducting wave-absorbing material, comprising, by mass, 200 parts of vinyl silicone oil with a viscosity of 2000 mPa·s, 400 parts of vinyl silicone oil with a viscosity of 500 mPa·s, 100 parts of hydrogenated silicone oil with a viscosity of 50 mPa·s, 8000 parts of modified composite powder, 4500 parts of Fe3Ni3Mo, 500 parts of β-type silicon carbide, 400 parts of hollow glass microspheres, 20 parts of catalyst and 2 parts of inhibitor; wherein the modified composite powder It includes carbonyl iron powder, four-needle zinc oxide electrostatically adsorbed on the surface of the carbonyl iron powder, and a silicone oil layer coated on the surface of the carbonyl iron powder and the four-needle zinc oxide; the particle size of the carbonyl iron powder is 10μm; the particle size of the four-needle zinc oxide is 0.3μm; the particle size of the Fe3Ni3Mo4 is 3μm; the particle size of the β-type silicon carbide is 40μm; the particle size of the hollow glass microspheres is 5μm; the thickness of the broadband thermal conductive wave absorbing material is 0.5mm.
[0059] The preparation method of the broadband thermal conductive wave absorbing material is the same as that of Example 1.
[0060] The broadband heat-conducting and wave-absorbing materials of Examples 1-3 were tested for electromagnetic wave reflection loss, and the results are shown in the following table:
[0061] Group thickness Peak absorption <-10db band Effective absorption bandwidth Example 1 1.5mm 24.8GHz@-32db 16.7GHz-34.4GHz 17.7GHz Example 2 1mm 26.5GHz@-36db 18.4GHz-36.9GHz 18.5GHz Example 3 0.5mm 28.7GHz@-33db 20.5GHz-37.7GHz 17.2GHz
[0062] Table 1 Electromagnetic wave reflection loss test results of Examples 1-3
[0063] It can be seen from Table 1 that the broadband thermal conductive absorbing material provided by the present application has a small change in the absorption peak with thickness, is less sensitive to thickness, and has an effective absorbing frequency band within the Ku, K, and Ka bands, having a relatively wide absorbing frequency band.
[0064] Although the preferred embodiments of the present application have been described, those skilled in the art may make additional changes and modifications to these embodiments once they have learned the basic creative concept. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments and all changes and modifications that fall within the scope of the embodiments of the present application.
[0065] Finally, it should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or terminal device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or terminal device. In the absence of further restrictions, the elements defined by the sentence "comprise a ..." do not exclude the existence of other identical elements in the process, method, article or terminal device including the elements.
[0066] The above is a detailed introduction to a broadband thermal conductive absorbing material and a preparation method thereof provided by the present application. Specific examples are used herein to illustrate the principle and implementation method of the present application. The description of the above embodiments is only used to help understand the method and core idea of the present application. At the same time, for a person skilled in the art, according to the idea of the present application, there may be changes in the specific implementation method and application scope. In summary, the content of this specification should not be understood as limiting the present application.
Claims
1. A broadband thermal conductive wave absorbing material, It is characterized in that The composition comprises, by mass, 600-800 parts of an organosilicon matrix, 7000-9000 parts of a modified composite powder, 400-600 parts of molybdenum permalloy, 400-600 parts of silicon carbide and 300-500 parts of hollow glass microspheres; wherein the modified composite powder comprises carbonyl iron powder, tetrapod zinc oxide electrostatically adsorbed on the surface of the carbonyl iron powder, and a silicone oil layer coated on the surface of the carbonyl iron powder and the tetrapod zinc oxide.
2. The broadband heat-conducting and wave-absorbing material according to claim 1, It is characterized in that The organic silicon matrix includes vinyl silicone oil and hydrogen silicone oil.
3. The broadband heat-conducting and wave-absorbing material according to claim 1, It is characterized in that The silicone oil layer includes a first silicone oil layer and a second silicone oil layer from the inside to the outside; the first silicone oil layer is octadecyltrimethoxysilane; and the second silicone oil layer is polydimethyl silicone oil.
4. The broadband heat-conducting and wave-absorbing material according to claim 1, It is characterized in that The particle size of the carbonyl iron powder is 8-12 μm; the particle size of the four-needle zinc oxide is 0.1-0.5 μm; the particle size of the molybdenum permalloy is 1-5 μm; the particle size of the silicon carbide is 38-42 μm; and the particle size of the hollow glass microspheres is 3-7 μm.
5. The broadband heat-conducting and wave-absorbing material according to claim 1, It is characterized in that The molybdenum permalloy is Fe 3 Ni 3 Mo 4 .
6. The broadband heat-conducting and wave-absorbing material according to claim 1, It is characterized in that The silicon carbide is β-type silicon carbide.
7. The broadband heat-conducting and wave-absorbing material according to claim 1, It is characterized in that Also includes: Inhibitors and catalysts.
8. The broadband heat-conducting and wave-absorbing material according to claim 7, It is characterized in that The inhibitor is acetylene cyclohexanol.
9. The broadband heat-conducting and wave-absorbing material according to claim 7, It is characterized in that The catalyst is a platinum catalyst.
10. A method for preparing the broadband heat-conducting and wave-absorbing material according to any one of claims 1 to 9, It is characterized in that include: The electrostatically charged four-needle zinc oxide and carbonyl iron powder are stirred and mixed to obtain a composite powder; The composite powder is mixed with a silicone oil solution by stirring, and then dried to obtain a modified composite powder; The modified composite powder, molybdenum permalloy, silicon carbide, hollow glass microspheres, an organic silicon matrix, an inhibitor and a catalyst are stirred and mixed to obtain a prefabricated broadband heat-conducting and wave-absorbing material; The prefabricated broadband heat-conducting and wave-absorbing material is cured to obtain the broadband heat-conducting and wave-absorbing material.
Citation Information
Patent Citations
Silica gel / carbonyl iron powder composite broadband wave absorbing sheet and preparation method thereof
CN109880377A
Broadband heat-conducting wave-absorbing gasket and preparation method thereof
CN112143239A
High-heat-conductivity wave-absorbing silica gel gasket and preparation method thereof
CN112980398A
High-temperature-resistant heat-conducting and wave-absorbing composite material and preparation method thereof
CN114350156A
Silicon-free heat-conducting wave-absorbing sheet and preparation method thereof
CN117659958A
Cited By
Wave-absorbing material with nanoparticle core-shell structure as well as preparation method and application of wave-absorbing material
CN120795625A