Bearing insulating coating mechanical property detection method

By conducting impact resistance tests on bearings, using bearing suspension angle and drop to calculate impact work, detecting the mechanical properties of bearing insulating coatings, the problem of insufficient detection of coating mechanical properties in the existing technology is solved, and the application of different bearings is achieved Sex and accuracy.

CN118937115APending Publication Date: 2024-11-12CSR ZHUZHOU ELECTRIC CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410879343.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-02
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The prior art is difficult to effectively detect the mechanical properties of bearing insulating coatings, especially in high-frequency converter applications, where increased coating thickness leads to reduced mechanical properties, resulting in problems of coating breakage and shedding.

Method used

By changing the angle of bearing suspension, the insulating coating with the outer diameter, end surface and chamfer of the bearing are subjected to impact resistance test, suspended with thin ropes and allowed the bearing to fall freely, calculate the impact work and observe the appearance and resistance of the insulating coating. Change, judge the mechanical strength.

Benefits of technology

The mechanical properties of bearing insulating coatings with different diameters and weights are realized, which is suitable for evaluating the impact resistance of the coating and improving the practicality and accuracy of the detection.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118937115A_ABST
    Figure CN118937115A_ABST
Patent Text Reader

Abstract

According to the bearing insulation coating mechanical property detection method, the quality and the insulation resistance of the detected bearing are measured firstly, then the detected bearing is suspended on the supporting rod through the thin rope, the height of the circle center of the detected bearing is measured, then the thin rope is cut off to enable the detected bearing to freely fall off, and the mechanical property of the bearing is detected. The impact energy of the measured bearing on the platform is calculated by using the mass of the measured bearing and the height of the circle center of the measured bearing, the appearance of the insulating coating of the measured bearing is checked after falling, and the insulation resistance of the measured bearing is measured again. And judging whether the mechanical strength of the tested bearing is greater than the calculated impact energy or not according to the appearance and insulation resistance change of the insulating coating of the tested bearing after falling, and performing an impact resistance test on the tested bearing to realize the detection of the mechanical property of the tested bearing. The mechanical performance of the insulating coating on the outer diameter surface, the end surface and the chamfer of the bearing can be detected by changing the suspension angle of the bearing, and the device is suitable for detecting the mechanical performance of the insulating coating of bearings with different diameters and weights, and is high in practicability.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for detecting the mechanical properties of a bearing insulation coating, which is used for detecting the mechanical properties of a bearing insulation coating. Background Art

[0002] Bearings are key components of motors, and their performance directly affects the normal operation of motors. With the widespread use of motor drive controls such as PWM (pulse width modulation) technology and IGBT (insulated gate bipolar transistor), the shaft current generated inside the bearing is getting larger and larger, which leads to more prominent problems of electrical corrosion damage to the bearing. Using bearings with insulating coatings is one of the common and effective measures to solve bearing electrical corrosion failures. The performance of the bearing insulating coating determines the bearing's ability to resist electrical corrosion. With the application of higher frequency converters, the thickness of the bearing insulating coating needs to be further increased to inhibit bearing electrical corrosion. However, the increase in coating thickness will lead to a decrease in the mechanical properties of the insulating coating, making the bearing prone to coating breakage and shedding during use. The existing coating evaluation method currently requires coating sample preparation, bonding, and stretching on a dedicated metal block to obtain the tensile bonding strength between the coating and the metal. Some existing bearing insulation coating performance detection devices and detection methods mainly solve the clamping problem during the electrical performance detection of insulating bearings. For example, "CN 209894882 U Insulated Bearing Resistance Detection Device" designs an insulating bearing detection device, including a base plate, a slide groove and a support frame, which can conveniently clamp bearings of various sizes for resistance detection. "CN 113759173 A Bearing Insulation Resistance Detection Device" mainly designs the bearing clamping device into two halves, and a conductive medium is provided on the inner side of the device to transitionally match with the outer surface of the bearing; "CN 114739807 A Insulated Bearing Power Frequency Withstand Voltage Characteristics Detection Tool" has a mounting seat that is interference-fitted with the outer diameter of the bearing and a clamping claw that is clamped with the inner diameter of the bearing, which can realize the testing of bearings with different inner diameters; "CN 205720448 U Insulated Bearing Insulation Resistance Detection Tool and Detection Device" includes an open elastic annular conductive sleeve and a zipper mechanism with locking and unlocking functions at the fracture ends of the two ends, which can conveniently and quickly clamp the bearing. The existing bearing insulation coating performance testing mainly focuses on the electrical performance testing of the coating and the tensile strength test of the coating on the standard sample, but lacks the mechanical performance testing and evaluation of the impact resistance of the bearing insulation coating. Summary of the invention

[0003] The method for detecting the mechanical properties of the insulating coating of a bearing provided by the present invention performs an impact resistance test on the tested bearing to realize the detection of the mechanical properties of the tested bearing. The mechanical properties of the insulating coating on the outer diameter surface, end surface and chamfer of the bearing can be detected by changing the angle of the bearing suspension. The method is suitable for detecting the mechanical properties of the insulating coating of bearings with different diameters and weights and has high practicality.

[0004] In order to achieve the above object, the technical solution adopted by the present invention is: The method for detecting the mechanical properties of the bearing insulation coating is characterized by comprising the following steps: S1: Weigh the mass M (kg) of the bearing under test and measure the insulation resistance R of the bearing under test; S2: Fix the 7-shaped support rod vertically on the platform; S3: Use a thin rope to suspend the bearing under test on the support rod and measure the height L1 (cm) of the center of the bearing under test; S4: Cut the string with scissors, and the bearing under test falls onto the platform; S5: Calculate the impact energy W (J) of the insulating coating of the tested bearing on the platform, W = M × L1 ÷ 10.2; S6: Observe the appearance of the insulating coating of the tested bearing, and measure the insulation resistance R1 of the tested bearing again. If the insulating coating is not damaged and 0.95≤R1 / R≤1, the mechanical strength of the insulating coating of the tested bearing is greater than W, otherwise it is less than W. S7: If the mechanical strength of the insulating coating of the measured bearing is greater than W, replace the measured bearing and increase the suspension height of the measured bearing, and repeat S1 to S6 until the maximum mechanical strength of the insulating coating of the measured bearing is obtained. If the mechanical strength of the insulating coating of the measured bearing is less than W, replace the measured bearing and lower the suspension height of the measured bearing, and repeat S1 to S6 until the maximum mechanical strength of the insulating coating of the measured bearing is obtained.

[0005] Preferably, when the measured bearing is suspended on the support rod in step S3, if the center axis of the measured bearing is parallel to the horizontal direction, the "mechanical strength of the insulating coating of the measured bearing" in step S6 refers to the mechanical strength of the outer diameter surface of the insulating coating of the measured bearing.

[0006] Preferably, when the measured bearing is suspended on the support rod in step S3, if the center axis of the measured bearing is perpendicular to the horizontal direction, the "mechanical strength of the insulating coating of the measured bearing" in step S6 refers to the mechanical strength of the end face of the insulating coating of the measured bearing.

[0007] Preferably, when the measured bearing is suspended on the support rod in step S3, if the central axis of the measured bearing is at an angle of 45 degrees to the horizontal direction, the "mechanical strength of the insulating coating of the measured bearing" in step S6 refers to the mechanical strength of the chamfered position of the insulating coating of the measured bearing.

[0008] Preferably, a connection hole for connecting with a thin rope is provided at the upper end of the support rod.

[0009] Preferably, a height measuring scale is provided on the vertical side surface of the support rod.

[0010] Preferably, the diameter of the bearing to be measured is set to D, L1>D / 2 and 10cm <L1<150cm。

[0011] The beneficial effects of the invention are: The method for detecting the mechanical properties of the insulating coating of a bearing of the present invention firstly measures the mass and the insulating resistance of the bearing to be tested, then suspends the bearing to be tested on a support rod with a thin rope, measures the height of the center of the bearing to be tested, and then cuts the thin rope to allow the bearing to be tested to fall freely, calculates the impact work of the bearing to be tested on a platform using the mass of the bearing to be tested and the height of the center of the bearing to be tested, checks the appearance of the insulating coating of the bearing to be tested after the fall, and measures the insulating resistance of the bearing to be tested again, determines whether the mechanical strength of the bearing to be tested is greater than the calculated impact work based on the changes in the appearance and the insulating resistance of the insulating coating of the bearing to be tested after the fall, performs an impact resistance test on the bearing to be tested, and detects the mechanical properties of the bearing to be tested. The mechanical properties of the insulating coating on the outer diameter surface, end surface, and chamfer of the bearing can be detected by changing the angle at which the bearing is suspended, and is suitable for detecting the mechanical properties of the insulating coating of bearings with different diameters and weights, and has high practicality. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 Schematic diagram of the bearing under test suspended on the support rod.

[0013] Figure 2 It is a schematic diagram of the suspension when the center axis of the measured bearing is parallel to the horizontal direction.

[0014] Figure 3 It is a schematic diagram of the suspension when the center axis of the measured bearing is perpendicular to the horizontal direction.

[0015] Figure 4 It is a schematic diagram of the suspension when the center axis of the measured bearing is at an angle of 45 degrees to the horizontal direction. DETAILED DESCRIPTION

[0016] Combine the following Figures 1 to 4 The embodiments of the present invention are described in detail.

[0017] The method for detecting the mechanical properties of the bearing insulation coating is characterized by comprising the following steps: S1: weigh the mass M (kg) of the bearing 3 to be tested, and measure the insulation resistance R of the bearing 3 to be tested; S2: Fix the 7-shaped support rod 1 vertically on the platform 2; S3: Use a thin rope 4 to suspend the measured bearing 3 on the support rod 1, and measure the height L1 (cm) of the center of the measured bearing 3; S4: Cut the string with scissors, and the bearing 3 to be tested falls onto the platform 1; S5: Calculate the impact energy W (J) of the insulating coating of the tested bearing on the platform, W = M × L1 ÷ 10.2; S6: Observe the appearance of the insulating coating of the tested bearing, and measure the insulation resistance R1 of the tested bearing again. If the insulating coating is not damaged and 0.95≤R1 / R≤1, the mechanical strength of the insulating coating of the tested bearing is greater than W, otherwise it is less than W. S7: If the mechanical strength of the insulating coating of the measured bearing 3 is greater than W, replace the measured bearing 3 and increase the suspension height of the measured bearing 3, repeat S1 to S6 until the maximum mechanical strength of the insulating coating of the measured bearing is obtained; if the mechanical strength of the insulating coating of the measured bearing 3 is less than W, replace the measured bearing 3 and lower the suspension height of the measured bearing 3, repeat S1 to S6 until the maximum mechanical strength of the insulating coating of the measured bearing is obtained.

[0018] The above-mentioned method for detecting the mechanical properties of the insulating coating of the bearing first measures the mass and insulation resistance of the measured bearing 3, then suspends the measured bearing 3 on the support rod 1 with a thin rope 4, and measures the height of the center of the measured bearing, then cuts the thin rope 4 to allow the measured bearing 2 to fall freely, and calculates the impact work of the measured bearing on the platform using the mass of the measured bearing and the height of the center of the measured bearing. After the fall, the appearance of the insulating coating of the measured bearing is checked and the insulation resistance of the measured bearing is measured again. According to the changes in the appearance and insulation resistance of the insulating coating of the measured bearing after the fall, it is judged whether the mechanical strength of the measured bearing is greater than the calculated impact work, and the impact resistance test is performed on the measured bearing to realize the detection of the mechanical properties of the measured bearing. The mechanical properties of the insulating coating on the outer diameter surface, end face, and chamfer of the bearing can be detected by changing the angle of the bearing suspension. It is suitable for the mechanical property detection of the insulating coating of bearings of different diameters and weights, and has high practicality. The formula W=M×L1÷10.2 is obtained by converting the impact energy calculation formula of free fall. The impact energy calculation formula of free fall is W=MHg, where W is the impact energy of free fall, in J, M is the mass of free fall, in kg, and h is the initial height of free fall, in m. After unit conversion, the formula for the impact energy of the tested bearing insulation coating on the platform is derived as W=M×L1÷10.2.

[0019] Among them, when the measured bearing 3 is suspended on the support rod 1 in step S3, if the central axis of the measured bearing 3 is parallel to the horizontal direction, then the "mechanical strength of the measured bearing insulation coating" in step S6 refers to the mechanical strength of the outer diameter surface of the measured bearing insulation coating. Figure 2 As shown, when the measured bearing 3 is suspended on the support rod 1, its axis is set horizontally, and its outer diameter surface contacts the platform first after falling, so the mechanical strength of the outer diameter surface of the insulating coating of the measured bearing can be tested.

[0020] Wherein, when the measured bearing 3 is suspended on the support rod 1 in step S3, if the central axis of the measured bearing 3 is perpendicular to the horizontal direction, the "mechanical strength of the measured bearing insulation coating" in step S6 refers to the mechanical strength of the end face of the measured bearing insulation coating. Figure 3 As shown, when the bearing 3 to be measured is suspended on the support rod 1, its central axis is arranged vertically and the end face is downward. After falling, its end face contacts the platform first. Therefore, the mechanical strength of the end face of the insulating coating of the bearing to be measured can be detected.

[0021] Among them, when the bearing 3 to be measured is suspended on the support rod 1 in step S3, if the central axis of the bearing to be measured forms a 45-degree angle with the horizontal direction, the "mechanical strength of the insulating coating of the bearing to be measured" in step S6 refers to the mechanical strength at the chamfer position of the insulating coating of the bearing to be measured. As Figure 4 As shown, when the bearing 3 to be measured is suspended on the support rod 1, its central axis forms a 45-degree angle with the horizontal direction. After falling, the chamfer position at its edge contacts the platform first. Therefore, the mechanical strength at the chamfer position of the insulating coating of the bearing to be measured can be detected.

[0022] Among them, a connection hole 11 for connecting with the thin string is opened at the upper end of the support rod 1. It is convenient to connect the thin string with the support rod 1.

[0023] Among them, a height measurement scale 12 is arranged on the vertical side surface of the support rod 1. After the bearing 3 to be measured is suspended, the center of the bearing to be measured is determined, and the height of the center of the bearing to be measured is measured through the height measurement scale 12. The height measurement scale 12 facilitates the measurement of the height of the center of the bearing 3 to be measured.

[0024] Among them, the diameter of the bearing to be measured is set as D, L1 > D / 2 and 10 cm < L1 < 150 cm. Ensure that the suspension height of the bearing to be measured meets the detection requirements.

[0025] The technical solutions of the embodiments of the present invention are completely described above in combination with the accompanying drawings. It should be noted that the described embodiments are only a part of the embodiments of the present invention. All other embodiments obtained by those of ordinary skill in the art based on the embodiments of the present invention without creative efforts belong to the scope of protection of the present invention.

Claims

1. A method for detecting mechanical properties of a bearing insulation coating, characterized in that: The following steps are involved: S1: Weigh the mass M (kg) of the bearing under test and measure the insulation resistance R of the bearing under test; S2: Fix the 7-shaped support rod vertically on the platform; S3: Use a thin rope to suspend the bearing under test on the support rod and measure the height L1 (cm) of the center of the bearing under test; S4: Cut the string with scissors, and the bearing under test falls onto the platform; S5: Calculate the impact energy W (J) of the insulating coating of the tested bearing on the platform, W = M × L1 ÷ 10.2; S6: Observe the appearance of the insulating coating of the tested bearing, and measure the insulation resistance R1 of the tested bearing again. If the insulating coating is not damaged and 0.95≤R1 / R≤1, the mechanical strength of the insulating coating of the tested bearing is greater than W, otherwise it is less than W. S7: If the mechanical strength of the insulating coating of the measured bearing is greater than W, replace the measured bearing and increase the suspension height of the measured bearing, and repeat S1 to S6 until the maximum mechanical strength of the insulating coating of the measured bearing is obtained. If the mechanical strength of the insulating coating of the measured bearing is less than W, replace the measured bearing and lower the suspension height of the measured bearing, and repeat S1 to S6 until the maximum mechanical strength of the insulating coating of the measured bearing is obtained.

2. The method for detecting mechanical properties of a bearing insulation coating according to claim 1, characterized in that: When the measured bearing is suspended on the support rod in step S3, if the central axis of the measured bearing is parallel to the horizontal direction, the "mechanical strength of the measured bearing insulation coating" in step S6 refers to the mechanical strength of the outer diameter surface of the measured bearing insulation coating.

3. The method for detecting mechanical properties of bearing insulation coating according to claim 1, characterized in that: When the measured bearing is suspended on the support rod in step S3, if the central axis of the measured bearing is perpendicular to the horizontal direction, the "mechanical strength of the measured bearing insulation coating" in step S6 refers to the mechanical strength of the end face of the measured bearing insulation coating.

4. The method for detecting mechanical properties of a bearing insulation coating according to claim 1, characterized in that: When the measured bearing is suspended on the support rod in step S3, if the central axis of the measured bearing is at an angle of 45 degrees to the horizontal direction, the "mechanical strength of the measured bearing insulation coating" in step S6 refers to the mechanical strength of the chamfered position of the measured bearing insulation coating.

5. The method for detecting mechanical properties of bearing insulation coating according to claim 1, characterized in that: A connection hole connected with the thin rope is arranged at the upper end of the support rod.

6. The method for detecting mechanical properties of a bearing insulation coating according to claim 1, characterized in that: A height measuring scale is provided on the vertical side of the support rod.

7. The method for detecting mechanical properties of a bearing insulation coating according to claim 1, characterized in that: The diameter of the bearing to be measured is set to D, L1>D / 2 and 10cm <L1<150cm。