80-year-life K3 type instrument cable and manufacturing method thereof

By using composite multi-strand dust-free rock wool rope to fill, low-smoke, halogen-free flame retardant materials and tin-plated copper conductors in instrument cables for nuclear power plants, a partial and total shielding structure is formed, which solves the difficulty of existing cables to meet the service life of 80 years and The problem of radiation resistance has achieved the improvement of high anti-interference and flame retardant performance.

CN118942793APending Publication Date: 2024-11-12CHINA NUCLEAR POWER ENGINEERING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411274912.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-11
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The instrument cables for existing nuclear power plants are difficult to meet the requirements of more than 80 years of service life, and there are shortcomings in narrow space laying, radiation resistance, and anti-interference performance.

Method used

An instrument cable including a cable core, a first winding cladding, a lining layer, a first metal shielding layer and a sheath layer are designed, and are filled with composite multi-strand dust-free rock wool rope, low smoke, halogen-free flame retardant material and Tin-plated copper conductors form part and total shielding structures, and their durability is verified by accelerated thermal aging and irradiation tests.

Benefits of technology

It realizes the high anti-interference ability, long life and radiation resistance of instrument cables, meets the requirements of the 80-year service life of nuclear power plants, and improves the flame retardant performance and processing performance of cables.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118942793A_ABST
    Figure CN118942793A_ABST
Patent Text Reader

Abstract

The invention discloses a K3 type instrument cable with the service life of 80 years and a manufacturing method thereof. A first wrapping layer, a lining layer, a first metal shielding layer and a sheath layer are sequentially arranged on the outer side of a cable core from inside to outside; the cable core is formed by twisting more than two twisted-pair groups and a filling material together. The twisted pair group is formed by sequentially wrapping a second wrapping layer, a second metal shielding layer and a third wrapping layer on the outer side of more than two wire cores which are twisted together; each wire core is composed of a conductor and an insulating layer on the outer side of the conductor, and the insulating layer is formed by extruding an inner insulating material and an outer insulating material; the first wrapping layer is formed by wrapping a flame-retardant belt, the lining layer comprises an oxygen barrier layer material, the first metal shielding layer and the second metal shielding layer are both formed by weaving tinned metal wires, and the sheath layer is formed by extruding a thermosetting sheath material. The K3 type instrument cable has the advantages that the service life is 80 years at the cable core temperature of 90 DEG C, the radiation resistance is good, the flame retardant property is excellent, and the electrical property is good.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a cable for a nuclear power plant, in particular to a K3 type instrument cable with a service life of 80 years and a manufacturing method thereof. Background Art

[0002] At present, the design life of the third-generation nuclear power plant is 60 years. Many countries are carrying out the life extension of nuclear power plants. Subsequent domestic nuclear power technology is planned to adopt an 80-year life span, which is higher than the life span of ordinary residential buildings. In order to meet the life extension needs of nuclear power plants, it is necessary to design K3 instrument cables with an 80-year life span.

[0003] In order to solve the problem of laying in narrow space, the instrument cable needs to have a compact structure, and the outer diameter and weight can be controlled within a reasonable range. The minimum bending radius can reach 8 times the cable radius to enhance the mobile laying capability. In order for the cable to work normally under the nuclear radiation in a mild environment, the insulation layer and the sheath layer need to have radiation resistance; to prevent the spread of fire and smoke, the cable structure needs to have low smoke and halogen-free flame retardant properties; to avoid frequent replacement of cables, the service life of the cable needs to be improved. In order to transmit signals stably, the anti-interference performance of the cable needs to be improved. In order to avoid waste of resources, it is necessary to design a simple cable structure and a simple process.

[0004] Prior art CN105609180A discloses an ultra-low temperature instrument control cable, comprising 2 to 12 pairs of twisted wire core groups, a gap filling layer and an outer layer; the twisted wire core group comprises a conductor, an insulating layer and a polyimide film layer from the inside to the outside; the gap filling layer is aramid fiber; the outer layer comprises a first polyimide film tape, a first braided layer, a second polyimide film tape, a high-voltage insulating layer, a third polyimide film tape, a second braided layer and a cross-linked polyethylene sheath from the inside to the outside.

[0005] Prior art CN109192368A discloses a low-voltage instrument cable for a nuclear power plant BOP system and a production method, comprising a plurality of cable cores, and a tape layer, a first shielding layer and a protective layer sequentially sleeved on the outside of the cable core from the inside to the outside, the cable core comprising a plurality of twisted wire groups, each twisted wire group comprising at least two twisted insulated wire cores, each insulated wire core comprising a conductor, a fire-resistant layer and a double-layer co-extruded heterogeneous insulation layer extruded outside the fire-resistant layer, a polyester tape and a second shielding layer are wrapped around the outside of the twisted insulated wire core, and a drainage wire is arranged in the second shielding layer.

[0006] The above instrument cables are difficult to achieve the requirement of more than 80 years of service life in nuclear power plants in terms of material selection, structural design and production and manufacturing processes.

[0007] In view of the above technical problems, the present invention is specially introduced. Summary of the invention

[0008] The main purpose of the present invention is to provide a K3 type instrument cable with an 80-year service life for a nuclear power plant and a manufacturing method thereof.

[0009] In order to achieve the above-mentioned purpose, according to one aspect of the present invention, an instrument cable is proposed, comprising a cable core, on the outside of which a first wrapping layer, an inner lining layer, a first metal shielding layer and a sheath layer are sequentially arranged from the inside to the outside; the cable core is formed by twisting two or more twisted pairs together with a filling material; the twisted pair group is formed by wrapping a second wrapping layer, a second metal shielding layer and a third wrapping layer in sequence on the outside of two or more twisted cores; the core is formed by a conductor and an insulating layer on its outside, and the insulating layer is extruded from an inner insulating material and an outer insulating material; the first wrapping layer is wrapped with a flame retardant tape, the inner lining layer includes an oxygen barrier material, the first metal shielding layer and the second metal shielding layer are both woven from tinned metal wires, and the sheath layer is extruded from a thermosetting sheath material.

[0010] Furthermore, the instrument cable uses an accelerated thermal aging test method based on the Arrhenius model to verify that the thermal life of the instrument cable is not less than 80 years at a core temperature of 90°C.

[0011] Furthermore, the filling material includes a plurality of dust-free rock wool ropes made of non-hygroscopic rock wool material, and the plurality of dust-free rock wool ropes are filled into the side gaps and / or the center gap of the cable core.

[0012] Furthermore, each twisted pair group includes 2 to 4 wire cores, and the pitch diameter ratio of more than two twisted pairs and multiple dust-free rock wool ropes is not greater than 20 times, and the twisting direction is left-handed.

[0013] Furthermore, the first wrapping layer is formed by wrapping the flame retardant tape in the right direction, the nominal thickness of the flame retardant tape is 0.2 mm, the width ranges from 10 mm to 30 mm, and the wrapping overlap rate is not less than 20%.

[0014] Furthermore, the first metal shielding layer is formed by cross-weaving first tinned copper wires, the weaving density is not less than 80%, and the wire diameter range of the first tinned copper wires is 0.15-0.3 mm.

[0015] Furthermore, the second metal shielding layer is formed by cross-weaving second tinned copper wires, the weaving density is not less than 80%, and the wire diameter range of the second tinned copper wires is 0.15-0.2 mm.

[0016] Furthermore, the cross-sectional area of ​​the conductor ranges from 0.5 mm 2 ~2.5mm 2The conductor is composed of an aramid wire and multiple tinned copper monofilaments twisted together. The diameter of the tinned copper monofilament ranges from 0.32 to 0.68 mm, the diameter of the conductor ranges from 0.9 to 2.0 mm, the pitch diameter ratio of the innermost layer of the tinned copper monofilament of the conductor ranges from 20 to 40, and the pitch diameter ratio of the outermost layer of the tinned copper monofilament of the conductor ranges from 12 to 18. The twisting direction is left, and the twisting directions of adjacent layers of tinned copper monofilaments are opposite.

[0017] Furthermore, the second wrapping layer is composed of right-handed wrapping of polyester tape, and the third wrapping layer is composed of left-handed wrapping of polyester tape. The nominal thickness of the polyester tape is 0.04 mm, the width ranges from 10 mm to 30 mm, and the wrapping overlap rate is not less than 20%.

[0018] Furthermore, the outer diameter range of the instrument cable is 10 to 48 mm, the nominal thickness of the insulation layer is 0.6 mm, the pitch of the core twist is not greater than 100 mm, the nominal thickness of the lining layer is 1.0 to 1.4 mm, and the thickness of the thinnest part of the lining layer is not less than 80% of the nominal value minus 0.2 mm; the nominal thickness of the sheath layer is 1.8 to 2.5 mm, and the thickness of the thinnest part of the sheath layer is not less than 80% of the nominal value minus 0.2 mm.

[0019] The application of the instrument cable technical solution of the present invention achieves at least the following beneficial effects:

[0020] 1. The instrument cable of the present invention has a braided shielding layer structure in the twisted pair group and outside the cable core by arranging the first metal shielding layer and the second metal shielding layer, thereby forming a two-layer shielding structure of a sub-shield and a total shield in the instrument cable, which can more effectively isolate the electric field or conduct leakage current, shield external electric field interference, thereby improving the anti-interference ability during signal transmission, and also can improve the service life of the cable.

[0021] 2. The instrument cable of the present invention improves the roundness of the cable and the flame retardant performance of the cable by arranging a composite multi-strand dust-free rock wool rope to fill the center and side gaps of the cable core. The first winding layer and the sheath layer are made of low-smoke halogen-free flame retardant materials, thereby achieving the performance requirements of low-smoke halogen-free flame retardant.

[0022] 3. The instrument cable of the present invention uses radiation-resistant and long-life materials in the insulation layer and the sheath layer on the basis of designing a new cable structure shape. The structural parameter design and manufacturing method of the insulation layer and the sheath layer are combined to improve the service life and radiation resistance of the cable. The structure of the instrument cable is reasonable and compact, and the processing performance is good.

[0023] 4. The instrument cable of the present invention designs an inner lining structure outside the cable core, so that the overall structure of the cable is more compact and further isolated from contact with oxygen to enhance the flame retardant performance of the cable; the tinned copper conductor after twisting is used to improve the conductivity of the conductor, making the conductor more corrosion-resistant and reducing the oxidation of the conductor to generate CuO and Cu2O.

[0024] In order to achieve the above-mentioned purpose, according to another aspect of the present invention, a method for manufacturing an instrument cable is proposed, which is used to manufacture the instrument cable according to the above-mentioned method, and comprises the following steps: a conductor manufacturing step, a core manufacturing step, a core radiation cross-linking step, a twisted group manufacturing step, a cable core manufacturing step, a cable core outer wrapping step, an inner lining extrusion step, a general shielding braiding step, and a sheath extrusion step; in the core manufacturing step, a double-layer co-extrusion method is adopted to extrude a double-layer material with a halogen-free polyolefin as a base material to form an insulating layer; in the inner lining extrusion step, an oxygen-isolating layer material is wrapped on the outer side of the third wrapping layer by an extrusion method to form an inner lining layer; in the sheath extrusion step, an extrusion method is adopted to uniformly extrude a thermosetting sheath material on the outer side of the first metal shielding layer.

[0025] Furthermore, the manufacturing method also includes a test and inspection step. After the sheath layer extrusion step, the test and inspection step includes conducting an accelerated thermal aging test equivalent to 80 years of operation, winding the instrument cable sample into multiple test coils, and placing the multiple test coils in a circulating air aging oven for accelerated thermal aging. Based on the Arrhenius model, the accelerated thermal aging temperature is selected to be above 155°C, and the accelerated aging time is selected to be above 1313h. After the accelerated thermal aging, the test coil is subjected to an appearance inspection, a withstand voltage test, an insulation resistance measurement, and a flame retardant test.

[0026] Furthermore, the test and inspection steps also include radiation aging test. After the accelerated thermal aging test, the cable samples after accelerated thermal aging are placed in the air for cobalt 60 source gamma irradiation, with a cumulative dose of not less than 36.9 Mrad and a dose rate of ≤1 Mrad / h. After the irradiation, appearance inspection and voltage withstand test are carried out.

[0027] Furthermore, in the wire core manufacturing step, the inner insulating material is cross-linked polyethylene material, and the outer insulating material is cross-linked polyolefin insulating material; for the inner insulating material: from the feed to the discharge direction, the body temperature zone of the extruder is: zone one 60-70°C, zone two 120-140°C, zone three 150-160°C, zone four 160-170°C; for the outer insulating material: from the feed to the discharge direction, the body temperature zone of the extruder is: zone one 40-60°C, zone two 130-150°C, zone three 160-170°C, zone four 170-180°C; zone one of the extruder is the feed section, zones two and three are the plasticizing sections, and zone four is the homogenizing section; from the feed to the discharge direction, the head temperature zone of the extruder is: zone one 160-170°C, zone two 170-180°C; among them, zone one is the head section and zone two is the neck section.

[0028] Furthermore, in the wire core manufacturing step, for the inner insulating material: the temperature zone of the extruder body is: 65°C in zone 1, 120°C in zone 2, 150°C in zone 3, and 160°C in zone 4; for the outer insulating material: the temperature zone of the extruder body is: 50°C in zone 1, 130°C in zone 2, 160°C in zone 3, and 180°C in zone 4; the temperature zone of the extruder head is: 170°C in zone 1, and 175°C in zone 2.

[0029] Furthermore, in the wire core radiation cross-linking step, the cross-linking speed is 150-200 m / min, the radiation energy is 1.2 MeV, the beam current is 32 mA, the threading passes are 25, and the elongation of the insulation under thermal extension load after cross-linking is ≤175%, and the permanent elongation after cooling is ≤15%.

[0030] Furthermore, in the step of extruding the sheath layer, a sheath mold sleeve is provided on the head of the extruder; the aperture of the sheath mold sleeve is larger than the outer diameter of the cable core; from the feed to the discharge direction, the temperature distribution of each zone of the extruder body is as follows: zone one 130-140°C, zone two 140-145°C, zone three 145-150°C, zone four 150-160°C, wherein zone one is the feed section, zones two and three are the plasticizing sections, and zone four is the homogenizing section; from the feed to the discharge direction, the temperature zones of the head of the extruder are as follows: zone one 160-165°C, zone two 160-165°C; wherein zone one is the head section and zone two is the neck section; the sheath pulling speed is 20m / min, and the eccentricity is not greater than 20%.

[0031] The application of the manufacturing method and technical solution of the present invention achieves at least the following beneficial effects:

[0032] 1. The manufacturing method of the instrument cable of the present invention ensures that the instrument cable has good heat aging resistance, radiation resistance and long life performance by designing the manufacturing process of the insulation layer and the sheath layer, and designs the test and inspection steps, so as to meet the service life requirement of more than 80 years in a nuclear power plant.

[0033] 2. The manufacturing method of the instrument cable of the present invention can reduce the production difficulty, improve the production efficiency, and make it relatively easy to control the size by designing the inner lining layer to adopt the tube extrusion production method.

[0034] 3. The manufacturing method of the instrument cable of the present invention can make the cable structure more compact by designing the sheath layer to adopt an extrusion production method, which can reduce the gap caused by the uneven cable core, improve the flame retardant performance of the cable, and improve the economic benefits. BRIEF DESCRIPTION OF THE DRAWINGS

[0035] The accompanying drawings constituting a part of the present invention are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the accompanying drawings:

[0036] Figure 1 A schematic cross-sectional view of the instrument cable of the present invention is shown.

[0037] The above drawings include the following reference numerals:

[0038] 1. Conductor; 2. Insulation layer; 3. First wrapping layer; 4. Lining layer; 5. Dust-free rock wool rope; 6. First metal shielding layer; 7. Sheath layer; 8. Twisted pair group; 9. Core; 10. Second wrapping layer; 11. Second metal shielding layer; 12. Third wrapping layer. DETAILED DESCRIPTION

[0039] It should be noted that, in the absence of conflict, the embodiments of the present invention and the features in the embodiments can be combined with each other. The present invention will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.

[0040] The present invention is further described in detail below in conjunction with specific embodiments, and these embodiments cannot be understood as limiting the scope of protection claimed by the present invention. The term "including" when used indicates the existence of a feature, but does not exclude the existence or addition of one or more other features; the orientation or position relationship indicated by the terms "lateral", "upper", "lower", "front", "rear", "left", "right", "top", "bottom", "inside", "outside", etc. is based on the orientation or position relationship shown in the drawings, which is only for the convenience of description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention; in addition, the terms "first" and "second" are only used for descriptive purposes, and cannot be understood as indicating or implying relative importance.

[0041] In the description, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be directly connected, or indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances. In addition, in the description of the present invention, unless otherwise specified, "plurality" means two or more.

[0042] Embodiment 1:

[0043] The present invention provides an instrument cable, such as Figure 1 As shown, it includes a cable core, and a first wrapping layer 3, an inner lining layer 4, a first metal shielding layer 6 and a sheath layer 7 are sequentially arranged on the outside of the cable core from the inside to the outside. The cable core is formed by twisting two or more twisted pairs 8 together with a filling material. The twisted pair 8 is composed of two or more twisted cores 9 wrapped with a second wrapping layer 10, a second metal shielding layer 11 and a third wrapping layer 12 in sequence on the outside. The instrument cable uses an accelerated thermal aging test method based on the Arrhenius model to verify that the thermal life of the cable is not less than 80 years at a core temperature of 90°C.

[0044] The wire core 9 is composed of an insulating layer 2 extruded on the outside of the conductor 1, and the insulating layer 2 is extruded from a double-layer insulating material. The first wrapping layer 3 is wrapped with a low-smoke halogen-free high flame retardant tape, the inner lining layer 4 includes a low-smoke halogen-free oxygen barrier material, the first metal shielding layer 6 and the second metal shielding layer 11 are both braided from tinned metal wires, and the sheath layer 7 is extruded from a thermosetting low-smoke halogen-free flame retardant sheath material.

[0045] Preferably, the filling material is a plurality of dust-free rock wool ropes 5 made of non-hygroscopic rock wool material, and the plurality of dust-free rock wool ropes 5 are filled into the side gaps and / or the center gaps of the cable core. Figure 1 When there are two twisted pairs 8 shown, multiple dust-free rock wool ropes 5 are filled into the side gaps of the cable core. When the cable core has more than three twisted pairs 8, multiple dust-free rock wool ropes 5 are filled into the central gap and the side gaps of the cable core.

[0046] Further preferably, each twisted pair group 8 includes 2 to 4 cores 9, and the pitch diameter ratio of more than two twisted pairs 8 and multiple dust-free rock wool ropes 5 is not more than 20 times, and the twisting direction is left-handed. The pitch of the core 9 is not more than 100mm. By arranging a composite multi-strand dust-free rock wool rope to fill the center and side gaps of the cable core, the roundness of the cable is improved, and the flame retardant performance of the cable is improved. The first winding layer and the sheath layer are made of low-smoke halogen-free flame retardant materials, thereby achieving the performance requirements of low-smoke halogen-free flame retardant.

[0047] Preferably, the first wrapping layer 3 is formed by right-hand wrapping of low-smoke halogen-free high flame retardant tape, the nominal thickness of the flame retardant tape is 0.2 mm, the width range is 10 mm to 30 mm, and the wrapping overlap rate is not less than 20%. The selection specifications and overlap rate design of the flame retardant tape can effectively ensure the tightness of the first wrapping layer, while reducing material waste and improving production efficiency.

[0048] Preferably, the first metal shielding layer 6 is formed by cross-weaving first tinned copper wires, the weaving density is not less than 80%, and the wire diameter range of the first tinned copper wires is 0.15-0.3 mm. The second metal shielding layer 11 is formed by cross-weaving second tinned copper wires, the weaving density is not less than 80%, and the wire diameter range of the second tinned copper wires is 0.15-0.2 mm. The first tinned copper wires and the second tinned copper wires are woven into metal meshes respectively, and the metal mesh material requirements are: high conductivity, corrosion resistance, high mechanical strength and tensile strength.

[0049] By arranging the first metal shielding layer and the second metal shielding layer, a braided shielding layer structure is provided in the twisted pair group and outside the cable core, thereby forming a two-layer shielding structure of sub-shield and total shield in the instrument cable, which can more effectively isolate the electric field or conduct leakage current, shield external electric field interference, thereby improving the anti-interference ability during signal transmission, and also can improve the service life of the cable.

[0050] The cross-sectional area of ​​conductor 1 is 0.5 mm 2 ~2.5mm 2 The conductor 1 is composed of an aramid fiber and a plurality of tinned copper monofilaments twisted together. The diameter of the tinned copper monofilaments ranges from 0.32 to 0.68 mm, the diameter of the conductor 1 ranges from 0.9 to 2.0 mm, the pitch-diameter ratio of the innermost layer of the tinned copper monofilaments of the conductor 1 ranges from 20 to 40, the pitch-diameter ratio of the outermost layer of the tinned copper monofilaments of the conductor 1 ranges from 12 to 18, the twisting direction is left-handed, and the twisting directions of the adjacent layers of tinned copper monofilaments are opposite. The tinned copper conductor after twisting can improve the conductivity of the conductor, make the conductor more corrosion-resistant, and reduce the oxidation of the conductor to generate CuO and Cu2O.

[0051] The second wrapping layer 10 is composed of polyester tape wrapped in right direction, and the third wrapping layer 12 is composed of polyester tape wrapped in left direction. The nominal thickness of the polyester tape is 0.04 mm, the width range is 10 mm to 30 mm, and the wrapping overlap rate is not less than 20%. The material requirements of the polyester tape are: it has certain insulation performance, high temperature resistance, low temperature resistance, excellent mechanical properties, etc., and can effectively protect the insulation from being damaged by the metal shielding layer.

[0052] The outer diameter of the instrument cable ranges from 10 to 48 mm, the nominal thickness of the insulation layer 2 is 0.6 mm, and the inner and outer insulation materials are tightly extruded on the surface of the conductor 1. The inner insulation material is cross-linked polyethylene material, and the outer insulation material is cross-linked polyolefin insulation material, both of which have an 80-year life, nuclear radiation resistance, low smoke, halogen-free, non-toxic, flame retardant and thermosetting properties. The core 9 needs to be irradiated and cross-linked, and the elongation of the insulation under heat extension load after cross-linking is ≤175%, and the permanent elongation after cooling is ≤15%.

[0053] The nominal thickness of the inner lining layer 4 is 1.0-1.4 mm, and the thickness of the thinnest part of the inner lining layer 4 is not less than 80% of the nominal value minus 0.2 mm; by designing the structure of the inner lining layer outside the cable core, the overall structure of the cable is made tighter and further isolated from contact with oxygen to enhance the flame retardant performance of the cable.

[0054] The nominal thickness of the sheath layer 7 is 1.8-2.5 mm, and the thickness of the thinnest part of the sheath layer 7 is not less than 80% of the nominal value minus 0.2 mm. The sheath layer 7 is evenly and tightly extruded outside the metal shielding layer, and the sheath material requirements of the sheath layer 7 are: nuclear radiation resistance, low smoke, halogen-free, non-toxic, oil-resistant, flame-retardant and thermosetting. The sheath layer 7 can further block the transmission of harsh environments such as high temperature, high pressure, high dose of γ, β rays to the insulation.

[0055] Based on the design of a new cable structure shape, radiation-resistant and long-life materials are used in the insulation layer and sheath layer. The structural parameter design and manufacturing method of the insulation layer and sheath layer are combined to improve the service life and radiation resistance of the cable. The structure of the instrument cable is reasonable and compact, and the processing performance is good.

[0056] The present invention further proposes a method for manufacturing an instrument cable, which is used to manufacture the instrument cable according to the above record, the maximum operating temperature of the cable conductor is 90°C, and the cable is designed to have a service life of not less than 80 years. When the cable is short-circuited (the longest duration does not exceed 5s), the maximum temperature of the conductor does not exceed 250°C. The use environment requirements are as follows: ambient temperature: (-35~60)°C; cumulative dose of gamma ray irradiation under normal working conditions: 335kGy (33.5Mrad). The minimum bending radius during cable installation should not be less than 8 times the actual outer diameter of the cable. The cable should be fixedly laid in cable brackets, cable ducts, cable trenches and cable tunnels. Specifically comprising the following steps:

[0057] Conductor manufacturing step S1, manufacturing conductor 1 by twisting. Specifically, tinned copper is selected as the conductor material, and a high-strength aramid wire and a plurality of metal monofilaments made of tinned copper are twisted to form conductor 1. Conductor 1 is divided into multiple layers from the inside to the outside, and two adjacent metal monofilaments in each layer of metal monofilaments are closely attached to each other, and the twisting direction of the outermost layer of tinned copper monofilaments is left-handed. In the adjacent two layers of metal monofilaments, the inner and outer layers of metal monofilaments are closely attached, and the twisting pitch of the metal monofilaments is not greater than 18 times the outer diameter after twisting.

[0058] In this embodiment, the radial cross-sectional area of ​​the conductor is 2.5 mm 2 Take the cable manufacturing as an example. The twisting equipment is the SJ500 high-speed stranding machine. The conductor structure is completed by 2 layers of twisting. It adopts a 1+6 structure arrangement. The outer layer is twisted in the left direction. The twisting pitch is 33±3mm, and the twisting pitch is not more than 18 times the outer diameter after twisting.

[0059] In the wire core manufacturing step S2, the inner insulating material and the outer insulating material based on halogen-free polyolefin are wrapped around the outer side of the conductor 1 by double-layer co-extrusion, and cooled to form an insulating layer 2. Specifically, in the wire core manufacturing step S2, the inner insulating material is cross-linked polyethylene material, and the outer insulating material is low-smoke halogen-free flame-retardant cross-linked polyolefin insulating material. In this embodiment, the extrusion adopts Φ65+Φ50 extrusion equipment.

[0060] For internal insulation materials: from feeding to discharging direction, the temperature zones of the extruder body are: 60-70℃ in zone 1, 120-140℃ in zone 2, 150-160℃ in zone 3, and 160-170℃ in zone 4; for external insulation materials: from feeding to discharging direction, the temperature zones of the extruder body are: 40-60℃ in zone 1, 130-150℃ in zone 2, 160-170℃ in zone 3, and 170-180℃ in zone 4; zone 1 of the extruder is the feeding section, zones 2 and 3 are the plasticizing sections, and zone 4 is the homogenizing section; from feeding to discharging direction, the temperature zones of the extruder head are: 160-170℃ in zone 1, and 170-180℃ in zone 2; among them, zone 1 is the head section and zone 2 is the neck section.

[0061] The better solution is: for internal insulation material: the temperature zones of the extruder body are: 65℃ for zone one, 120℃ for zone two, 150℃ for zone three, and 160℃ for zone four; for external insulation material: the temperature zones of the extruder body are: 50℃ for zone one, 130℃ for zone two, 160℃ for zone three, and 180℃ for zone four; the temperature zones of the extruder head are: 170℃ for zone one, and 175℃ for zone two.

[0062] In the wire core radiation cross-linking step S3, the wire core 9 is subjected to radiation cross-linking. Specifically, in the wire core radiation cross-linking step S3, the cross-linking speed is 150-200 m / min, the radiation energy is 1.2 MeV, the beam current is 32 mA, the threading passes are 25, and the elongation of the insulation under heat extension load after cross-linking is ≤175%, and the permanent elongation after cooling is ≤15%.

[0063] In the twisted pair manufacturing step S4, at least two wire cores 9 are twisted, and after twisting, a second wrapping layer 10 is overlapped and wrapped on the outside in sequence, a second metal shielding layer 11 is braided, and a third wrapping layer 12 is overlapped and wrapped again to form a twisted pair group 8.

[0064] Specifically, each twisted pair group 8 is composed of 2 to 4 wire cores 9 twisted together, the twisting direction is left-handed, and the twisting pitch is not greater than 100mm. Using a relatively large twisting pitch can relatively improve production efficiency and improve the flexibility of the cable core. After twisting, a layer of high-temperature resistant polyester tape with a thickness of 0.04mm is overlapped and wrapped, the wrapping overlap rate is not less than 20%, and the wrapping direction is right-handed. After wrapping, a metal shielding layer is woven, which is made of a second tinned copper wire cross-woven, with a weaving density of not less than 80%, and the wire diameter range of the second tinned copper wire is 0.15 to 0.2mm. A layer of high-temperature resistant polyester tape is overlapped and wrapped outside the second metal shielding layer 11, and the wrapping overlap rate is not less than 20%, and the wrapping direction is right-handed.

[0065] In the cable core manufacturing step S5, at least two twisted pairs 8 are twisted with a plurality of dust-free rock wool ropes 5 to form a cable core, the twisting direction is left-handed, and the twisting pitch ratio is not greater than 20 times. Figure 1 When there are two twisted pairs 8 shown, multiple dust-free rock wool ropes 5 are filled into the side gaps of the cable core. When the cable core has more than three twisted pairs 8, multiple dust-free rock wool ropes 5 are filled into the central gap and the side gaps of the cable core.

[0066] In the cable core outer wrapping step S6, a layer of low-smoke zero-halogen high flame retardant tape is wrapped on the outer side of the cable core to form a first wrapping layer 3. Specifically, the wrapping direction is right, the nominal thickness of the low-smoke zero-halogen high flame retardant tape is 0.2 mm, the width ranges from 10 mm to 30 mm, and the wrapping overlap rate is not less than 20%.

[0067] In the inner lining layer extrusion step S7, the low smoke halogen-free flame retardant oxygen-insulating layer material is wrapped on the outside of the first wrapping layer 3 by extrusion, and cooled to form the inner lining layer 4. By designing the inner lining layer to be produced by extrusion tube, the production difficulty can be reduced, the production efficiency can be improved, and the size control can be relatively easy.

[0068] In the overall shielding braiding step S8, tinned metal wires are cross-woven on the outer side of the inner lining layer 4 to form a first metal shielding layer 6. The first metal shielding layer 6 is cross-woven with first tinned copper wires, the braiding density is not less than 80%, and the diameter of the first tinned copper wires ranges from 0.15 to 0.3 mm.

[0069] In the sheath layer extrusion step S9, a thermosetting low-smoke halogen-free flame-retardant polyolefin sheath material is uniformly extruded on the outside of the first metal shielding layer 6. By designing the sheath layer to adopt an extrusion production method, the cable structure can be made tighter, the gap caused by the uneven cable core can be reduced, the flame retardant performance of the cable can be improved, and the economic benefits can be improved.

[0070] Specifically, in the sheath layer extrusion step S9, a sheath mold sleeve is provided on the extruder head; the aperture of the sheath mold sleeve is larger than the outer diameter of the cable core; from the feed to the discharge direction, the temperature distribution of each zone of the extruder body is: zone 1 130-140°C, zone 2 140-145°C, zone 3 145-150°C, zone 4 150-160°C, wherein zone 1 is the feed section, zones 2 and 3 are the plasticizing sections, and zone 4 is the homogenizing section; from the feed to the discharge direction, the temperature zone of the extruder head is: zone 1 160-165°C, zone 2 160-165°C; wherein zone 1 is the head section, and zone 2 is the neck section.

[0071] In this embodiment, preferably, the core aperture of the jacket mold is equal to the outer diameter of the cable core + 1 mm. The jacket pulling speed is 20 m / min, and the eccentricity is not greater than 20%.

[0072] Test and inspection step S10, after the sheath layer extrusion step S9, the test and inspection step S10 includes conducting an accelerated thermal aging test equivalent to 80 years of operation, winding the instrument cable sample into multiple test coils, placing the multiple test coils in a circulating air aging oven for accelerated thermal aging, and after the accelerated thermal aging, performing an appearance inspection, a withstand voltage test, an insulation resistance measurement on the test coils and passing a flame retardant test.

[0073] Specifically, the effective test length of each test coil is not less than 3.05m, and the test temperature and time of the circulating air aging oven are derived from the insulation thermal life assessment test results. Based on the Arrhenius model, the accelerated thermal aging temperature is selected and the accelerated thermal aging time is calculated. The steps are as follows:

[0074] Based on the Arrhenius equation, we can get:

[0075] In the formula, τ is the time required for a certain change of the material, in h,

[0076] Ea——Material activation energy, unit eV,

[0077] R——Boltzmann constant, 0.00008617,

[0078] H——insulation temperature, unit K,

[0079] A—Constants related to materials and diagnostic tests.

[0080] Transforming the equation yields:

[0081] Activation energy data of internal insulation: Ea = 126.8 kJ / mol = 1.314 eV,

[0082] Activation energy data of external insulation: Ea = 129.2 kJ / mol = 1.339 eV,

[0083] Activation energy data of outer sheath: Ea = 127.4 kJ / mol = 1.320 eV,

[0084] Working temperature of the material: H2 = 273.15 + 90 = 363.15K,

[0085] Accelerated aging temperature: H1 = 273.15 + 155 = 428.15K,

[0086] The life of the material to be identified: τ2 = 80 × 365 × 24 = 700800h,

[0087] Substituting the above parameters, we can get the accelerated thermal aging time τ1 = 1194h,

[0088] Adding a 10% margin gives 1313h.

[0089] In summary, based on the Arrhenius model, the accelerated thermal aging temperature is selected to be above 155°C, and a 10% margin is added, and the accelerated thermal aging time is calculated to be above 1313h.

[0090] During the appearance inspection, the cable structure is required to remain intact, without obvious deformation, cracking and other abnormal phenomena. The cable sample is bent into a coil with an inner diameter not exceeding 20 times the outer diameter of the cable and immersed in water for 1 hour, and then subjected to a withstand voltage test. An AC voltage of 3150V / mm is applied between conductors and conductors, and between conductors and water and shielding for 5 minutes, and the insulation should not be broken down. Insulation resistance measurement is performed, and the insulation resistance value must be greater than 1MΩ·km (at an ambient temperature of 20±5℃). Pass the bundled B-type flame retardant test.

[0091] The test inspection step S8 also includes performing a radiation aging test. After the accelerated thermal aging test, the cable sample after accelerated thermal aging is placed in the air for cobalt 60 source γ irradiation, with a cumulative dose of not less than 36.9 Mrad (33.5 Mrad + 10% margin), and a dose rate of ≤1 Mrad / h. After the irradiation, an appearance inspection and a withstand voltage test are performed.

[0092] During the appearance inspection, the cable structure is required to remain intact without obvious deformation, cracking and other abnormal phenomena. The cable sample is bent into a coil with an inner diameter not exceeding 20 times the outer diameter of the cable and immersed in water for 1 hour, and then subjected to a withstand voltage test. An AC voltage of 3150V / mm is applied between conductors and conductors, and between conductors and water and shielding for 5 minutes, and the insulation should not be broken down. Test test inspection step S8 ensures that the instrument cable has good heat aging resistance, radiation resistance and long life performance, and can meet the requirements of a service life of more than 80 years in a nuclear power plant.

[0093] The advantages of this instrument cable are: resistance to nuclear radiation, good flame retardancy, long service life, good flexibility, and good economy. After adopting the above scheme, the service life of this cable reaches more than 80 years, with good radiation resistance, good anti-interference performance, and good processing performance, which can effectively improve production efficiency. And at the same time, it meets the basic requirements of electrical and mechanical properties.

[0094] Preferably, the cable of this embodiment can also undergo the following tests: voltage test, conductor resistance measurement, insulation resistance test, working capacitance measurement, capacitance unbalance measurement, inductance-resistance ratio measurement, thermoelectromotive force and tolerance test, conductor inspection and dimension inspection, insulation mechanical properties test before and after aging, insulation thermal extension test, insulation water absorption test, insulation shrinkage test, insulation toxicity index, sheath mechanical properties test before and after aging, sheath thermal extension test, sheath water absorption test, sheath low temperature performance test, sheath anti-cracking test, sheath oil immersion test, wear resistance test, additional aging test for finished cables, single vertical burning test, bundled burning Class B test, smoke density test, pH and conductivity test, acid gas content test, finished cable bending test, printed mark abrasion resistance test, and the test results are all passed.

[0095] Embodiment 2:

[0096] The difference between the manufacturing method of Example 2 and Example 1 is that in the wire core manufacturing step S2, the insulating layer 2 of this embodiment adopts low-smoke halogen-free flame-retardant ethylene-propylene rubber insulation material, and is produced using a continuous sulfur production line. From the feeding to the discharging direction, the body temperature zone of the rubber extruder is: zone 1 60-70°C, zone 2 65-75°C, zone 3 70-80°C, zone 4 75-85°C; the head temperature zone is: zone 1 80-90°C, zone 2 75-85°C; among them, zone 1 is the head section and zone 2 is the neck section. When the insulating material is extruded, the saturated steam pressure is maintained at 1.5-1.7MPa, and the water level is controlled between 20% and 30%.

[0097] Embodiment 3:

[0098] The difference between the manufacturing method of Example 3 and Example 1 is that in the twisted pair manufacturing step S4 and the overall shielding braiding step S8, the copper metal tape is overlapped and wrapped to replace the tinned metal wire cross-braiding to form the first metal shielding layer 6 and the second metal shielding layer 11. The copper metal tape wrapping overlap rate is not less than 15%. The nominal thickness of the copper metal tape is controlled to be 0.1 mm to 0.12 mm.

[0099] By comprehensively comparing the above three embodiments, the cable yield rate of embodiment 1 is the highest, reaching 99%, embodiment 2 reaches 97.5%, and embodiment 3 reaches 98%. From this result, it can be seen that for the insulation layer, the difficulty of double-layer co-extrusion of plastic insulation materials is lower than that of rubber materials, and the double-layer co-extrusion production efficiency is higher. Embodiment 3 also adopts the insulation double-layer co-extrusion process, and its yield rate is also higher than that of embodiment 2.

[0100] From the bending performance of the cable, the structure of Example 1 is better than that of Example 3. Since the cable structure of Example 1 has two shielding structures, namely, the sub-shielding layer and the overall shielding layer, combined with a metal wire mesh of a suitable structure, its shielding performance can meet the use requirements.

[0101] In summary, from the above description, it can be seen that the above embodiments of the present invention achieve the following technical effects:

[0102] 1. The instrument cable of the present invention has a braided shielding layer structure in the twisted pair group and outside the cable core by arranging the first metal shielding layer and the second metal shielding layer, thereby forming a two-layer shielding structure of a sub-shield and a total shield in the instrument cable, which can more effectively isolate the electric field or conduct leakage current, shield external electric field interference, thereby improving the anti-interference ability during signal transmission, and also can improve the service life of the cable.

[0103] 2. The instrument cable of the present invention improves the roundness of the cable and the flame retardant performance of the cable by arranging a composite multi-strand dust-free rock wool rope to fill the center and side gaps of the cable core. The first winding layer and the sheath layer are made of low-smoke halogen-free flame retardant materials, thereby achieving the performance requirements of low-smoke halogen-free flame retardant.

[0104] 3. The instrument cable of the present invention uses radiation-resistant and long-life materials in the insulation layer and the sheath layer on the basis of designing a new cable structure shape. The structural parameter design and manufacturing method of the insulation layer and the sheath layer are combined to improve the service life and radiation resistance of the cable. The structure of the instrument cable is reasonable and compact, and the processing performance is good.

[0105] 4. The instrument cable of the present invention designs an inner lining structure outside the cable core, so that the overall structure of the cable is more compact and further isolated from contact with oxygen to enhance the flame retardant performance of the cable; the tinned copper conductor after twisting is used to improve the conductivity of the conductor, making the conductor more corrosion-resistant and reducing the oxidation of the conductor to generate CuO and Cu2O.

[0106] 5. The manufacturing method of the instrument cable of the present invention ensures that the instrument cable has good heat aging resistance, radiation resistance and long life performance by designing the manufacturing process of the insulation layer and the sheath layer, and designs the test and inspection steps, so as to meet the service life requirement of more than 80 years in a nuclear power plant.

[0107] 6. The manufacturing method of the instrument cable of the present invention can reduce the difficulty of production, improve the production efficiency, and make it relatively easy to control the size by designing the inner lining layer to adopt the tube extrusion production method.

[0108] 7. The manufacturing method of the instrument cable of the present invention can make the cable structure more compact by designing the sheath layer to adopt an extrusion production method, which can reduce the gap caused by the unevenness of the cable core, improve the flame retardant performance of the cable, and improve the economic benefits.

[0109] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. A K3 instrument cable with a service life of 80 years, comprising a cable core, It is characterized in that A first wrapping layer (3), an inner lining layer (4), a first metal shielding layer (6) and a sheath layer (7) are sequentially arranged on the outer side of the cable core from inside to outside; The cable core is formed by twisting two or more twisted pairs (8) together with a filling material; the twisted pair (8) is formed by wrapping a second wrapping layer (10), a second metal shielding layer (11) and a third wrapping layer (12) in sequence around the outer side of two or more twisted cores (9); the core (9) is formed by a conductor (1) and an insulating layer (2) outside thereof, and the insulating layer (2) is formed by extruding an inner insulating material and an outer insulating material; The first wrapping layer (3) is formed by wrapping a flame retardant tape, the inner lining layer (4) comprises an oxygen-isolating layer material, the first metal shielding layer (6) and the second metal shielding layer (11) are both formed by braiding tinned metal wires, and the sheath layer (7) is formed by extruding a thermosetting sheath material.

2. The instrument cable according to claim 1, Features: The instrument cable uses an accelerated thermal aging test method based on the Arrhenius model to verify that the thermal life of the wire core (9) is not less than 80 years at a temperature of 90° C.

3. The instrument cable according to claim 1, Features: The filling material comprises a plurality of dust-free rock wool ropes (5) made of non-hygroscopic rock wool material, and the plurality of dust-free rock wool ropes (5) are filled into the side gaps and / or the center gap of the cable core.

4. The instrument cable according to claim 3, Features: Each of the twisted pairs (8) comprises 2 to 4 wire cores (9), the pitch diameter ratio of two or more of the twisted pairs (8) and a plurality of the dust-free rock wool ropes (5) twisted together is not greater than 20 times, and the twisting direction is left-handed.

5. The instrument cable according to claim 4, Features: The first wrapping layer (3) is formed by wrapping the flame retardant tape in the right direction, the flame retardant tape has a nominal thickness of 0.2 mm, a width ranging from 10 mm to 30 mm, and a wrapping overlap rate of not less than 20%.

6. The instrument cable according to claim 1, Features: The first metal shielding layer (6) is formed by cross-weaving first tinned copper wires, with a weaving density of not less than 80%, and the wire diameter of the first tinned copper wires ranges from 0.15 to 0.3 mm.

7. The instrument cable according to claim 6, Features: The second metal shielding layer (11) is formed by cross-weaving second tinned copper wires, with a weaving density of not less than 80%, and the wire diameter of the second tinned copper wires ranges from 0.15 to 0.2 mm.

8. A method for manufacturing an instrument cable, It is characterized in that The method for manufacturing the instrument cable according to any one of claims 1 to 7 comprises the following steps: Conductor manufacturing step S1, wire core manufacturing step S2, wire core radiation cross-linking step S3, twisted group manufacturing step S4, cable core manufacturing step S5, cable core outer wrapping step S6, inner lining layer extrusion step S7, overall shielding braiding step S8, sheath layer extrusion step S9; In the wire core manufacturing step S2, a double-layer material with a halogen-free polyolefin as a base material is extruded to form an insulating layer (2) by a double-layer co-extrusion method; In the inner lining layer extrusion step S7, the oxygen barrier layer material is wrapped around the outer side of the third wrapping layer (3) by extrusion to form the inner lining layer (4); In the sheath layer extrusion step S9, a thermosetting sheath material is evenly extruded on the outside of the first metal shielding layer (6) by an extrusion method.

9. The manufacturing method according to claim 8, Features: The manufacturing method also includes a test and inspection step S10. After the sheath layer extrusion step S9, the test and inspection step S10 includes performing an accelerated thermal aging test equivalent to 80 years of operation, winding the sample of the instrument cable into multiple test coils, placing the multiple test coils in a circulating air aging oven for accelerated thermal aging, selecting an accelerated thermal aging temperature of more than 155°C and an accelerated aging time of more than 1313h based on the Arrhenius model, and performing an appearance inspection, a withstand voltage test, an insulation resistance measurement, and passing a flame retardant test on the test coil after the accelerated thermal aging.

10. The manufacturing method according to claim 9, Features: The test and inspection step S8 also includes performing a radiation aging test. After the accelerated thermal aging test, the cable sample after accelerated thermal aging is placed in the air for cobalt 60 source gamma irradiation, with a cumulative dose of not less than 36.9 Mrad and a dose rate of ≤1 Mrad / h. After the irradiation, an appearance inspection and a withstand voltage test are performed.

11. The manufacturing method according to claim 8, Features: In the wire core manufacturing step S2, the inner insulating material is cross-linked polyethylene material, and the outer insulating material is cross-linked polyolefin insulating material; for the inner insulating material: from the feeding to the discharging direction, the body temperature zone of the extruder is: 60-70°C in the first zone, 120-140°C in the second zone, 150-160°C in the third zone, and 160-170°C in the fourth zone; for the outer insulating material: from the feeding to the discharging direction, the body temperature zone of the extruder is: 40-60°C in the first zone, 130-150°C in the second zone, 160-170°C in the third zone, and 170-180°C in the fourth zone; The first zone of the extruder is the feeding section, the second zone and the third zone are the plasticizing section, and the fourth zone is the homogenizing section; from the feeding to the discharging direction, the head temperature zone of the extruder is: 160-170°C in the first zone and 170-180°C in the second zone; among them, the first zone is the head section and the second zone is the neck section.

12. The manufacturing method according to claim 11, Features: In the wire core manufacturing step S2, for the inner insulating material: the temperature zone of the extruder is: 65°C in zone 1, 120°C in zone 2, 150°C in zone 3, and 160°C in zone 4; for the outer insulating material: the temperature zone of the extruder is: 50°C in zone 1, 130°C in zone 2, 160°C in zone 3, and 180°C in zone 4; The head temperature zones of the extruder are: 170°C in zone 1 and 175°C in zone 2.

13. The manufacturing method according to claim 8, Features: In the wire core radiation cross-linking step S3, the cross-linking speed is 150-200 m / min, the radiation energy is 1.2 MeV, the beam current is 32 mA, the threading passes are 25, and the elongation of the insulation under thermal extension load after cross-linking is ≤175%, and the permanent elongation after cooling is ≤15%.

14. The manufacturing method according to claim 11, Features: In the sheath layer extrusion step S9, a sheath mold sleeve is provided on the head of the extruder; the aperture of the sheath mold sleeve is larger than the outer diameter of the cable core; from the feed to the discharge direction, the temperature distribution of each zone of the body of the extruder is: zone 1 130-140°C, zone 2 140-145°C, zone 3 145-150°C, zone 4 150-160°C, wherein zone 1 is the feed section, zones 2 and 3 are the plasticizing sections, and zone 4 is the homogenizing section; from the feed to the discharge direction, the head temperature zones of the extruder are: zone 1 160-165°C, zone 2 160-165°C; wherein zone 1 is the head section, and zone 2 is the neck section; the sheath pulling speed is 20m / min, and the eccentricity is not greater than 20%.