Semiconductor structure and preparation method thereof, and SiC MOSFET device
By increasing the thickness of the gate oxygen layer above the JFET region in the semiconductor structure of the SiC MOSFET device, the problem of avalanche failure during high-speed switching is solved, and the device's avalanche resistance and reliability are improved.
Patent Information
- Application Number
- CN202410930979.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-11
- Publication Date
- 2024-11-12
AI Technical Summary
SiC MOSFET devices are prone to avalanche failure under high-speed switching conditions, resulting in an instant increase in the junction temperature, affecting the reliability of the device.
In the semiconductor structure of the SiC MOSFET device, the thickness of the gate oxygen layer above the JFET region is set to an avalanche-resistant thickness that exceeds the standard thickness, thereby improving the quality of the gate oxygen layer and avalanche-resistant ability.
It effectively improves the avalanche resistance of SiC MOSFET devices, ensuring the stability and reliability of the device under high-intensity electric field conditions.
Smart Images

Figure CN118943187A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of semiconductor technology, and in particular to a semiconductor structure and a preparation method thereof, and a SiC MOSFET device. Background Art
[0002] With the development of science and technology and society, the progress of modern industry increasingly requires the support of high-temperature, high-frequency, and high-power devices. The third-generation semiconductor material SiC has the characteristics of wide bandgap, high critical breakdown electric field, and high saturation drift rate. It can work well in such extreme scenarios, and thus can bring significant performance improvements to various applications and systems. Among SIC power devices, SiC MOSFET (Metal Oxide Semiconductor Field Effect Transistor) devices are unipolar devices with an insulated gate structure. SiC MOSFET devices have the advantages of high input impedance, high switching speed stability, and low on-resistance. They are the most concerned SiC switching devices and can be used in extreme working conditions such as high temperature, high voltage, and high frequency. They are widely used in aerospace, industrial control, new energy vehicles and other fields. However, in related technologies, under high-speed switching conditions, SiC MOSFET devices are prone to avalanche failure, causing the junction temperature of SiC MOSFET devices to rise instantly, thereby affecting the reliability of SiC MOSFET devices. Summary of the invention
[0003] Based on this, it is necessary to provide a semiconductor structure and a preparation method thereof and a SiC MOSFET device that can improve the avalanche resistance of SiC MOSFET devices in order to address the above technical problems.
[0004] In a first aspect, the present application provides a semiconductor structure, comprising:
[0005] A substrate, comprising a drift region; the drift region comprising a well region and a JFET region, the well region surrounding the JFET region; the well region comprising a first doping region and a second doping region, the first doping region being located between the JFET region and the second doping region;
[0006] A gate oxide layer, located on a side of the drift region away from the substrate and covering a portion of the drift region;
[0007] A gate electrode is located on a side of the gate oxide layer away from the drift region and covers the gate oxide layer; wherein, along a direction perpendicular to the substrate, the thickness of the gate oxide layer covered by the portion of the gate electrode vertically projected within the JFET is an avalanche-resistant thickness, and the thickness of all other gate oxide layers is a standard thickness, wherein the avalanche-resistant thickness is greater than the standard thickness.
[0008] In this embodiment, the standard thickness is the thickness of the gate oxide layer required by the basic electrical characteristics of the semiconductor structure, and the basic electrical characteristics are, for example, the threshold voltage, on-resistance, switching characteristics, etc. of the semiconductor structure. Setting the standard thickness can ensure that the basic electrical characteristics of the semiconductor structure are good. On the basis of ensuring that the basic electrical characteristics of the semiconductor structure are good, by setting the avalanche resistance thickness, that is, by improving the thickness of the gate oxide layer above the JFET region, the quality of the gate oxide layer is improved, thereby improving the avalanche resistance of the semiconductor structure. The semiconductor structure provided in the embodiment of the present application is applied to a SiC MOSFET device, and the avalanche resistance of the SiC MOSFET device can be improved.
[0009] In one embodiment, the gate oxide layer covered by the portion of the gate electrode whose vertical projection is located within the JFET has a vertical projection toward the substrate as a first vertical projection, and the first vertical projection is located within the JFET region;
[0010] The vertical projections of all the remaining gate oxide layers toward the substrate are second vertical projections, and the second vertical projections are located in the JFET region, the drift region between the JFET region and the first doping region, and the first doping region.
[0011] In one embodiment, the thickness of the portion of the gate electrode whose vertical projection is located within the JFET is greater than the thickness of the gate electrode covering all the remaining gate oxide layers.
[0012] In one embodiment, it also includes:
[0013] The dielectric layer is located on a side of the gate electrode away from the gate oxide layer and covers the gate electrode and a portion of the first doped region.
[0014] In one embodiment, the dielectric layer and the gate oxide layer are made of the same material.
[0015] In one embodiment, the second doping region has a doping type opposite to that of the first doping region.
[0016] In one embodiment, it also includes:
[0017] A source electrode, located on a side of the dielectric layer away from the gate electrode, and covering the dielectric layer, a portion of the first doped region, and the second doped region;
[0018] The drain electrode is located on a side of the substrate away from the drift region and covers the substrate.
[0019] In a second aspect, the present application further provides a SiC MOSFET device, which includes a semiconductor structure as described in any of the above embodiments.
[0020] In a third aspect, the present application also provides a method for preparing a semiconductor structure, comprising:
[0021] Providing a substrate, the substrate comprising a drift region, the drift region comprising a well region and a JFET region, the well region surrounding the JFET region; the well region comprising a first doping region and a second doping region, the first doping region being located between the JFET region and the second doping region;
[0022] forming a gate oxide layer, which is located on a side of the drift region away from the substrate and covers a portion of the drift region;
[0023] A gate electrode is formed, which is located on a side of the gate oxide layer away from the drift region and covers the gate oxide layer; wherein, along a direction perpendicular to the substrate, the thickness of the gate oxide layer covered by the portion of the gate electrode vertically projected within the JFET is an avalanche-resistant thickness, and the thickness of all other gate oxide layers is a standard thickness, wherein the avalanche-resistant thickness is greater than the standard thickness.
[0024] In one embodiment, forming a gate oxide layer comprises:
[0025] forming an intermediate layer, which is located on a side of the drift region away from the substrate and covers a portion of the drift region;
[0026] The intermediate layer is etched so that the thickness of the gate oxide layer covered by the portion of the gate electrode vertically projected within the JFET along a direction perpendicular to the substrate is avalanche-resistant thickness, and the thickness of all other gate oxide layers is standard thickness.
[0027] The semiconductor structure and its preparation method and SiC MOSFET device, wherein the semiconductor structure includes a substrate, a gate oxide layer and a gate electrode. A drift region is formed in the substrate. A well region and a JFET region are formed in the drift region, and the well region surrounds the JFET region. A first doped region and a second doped region are formed in the well region, and the first doped region is located between the JFET region and the second doped region.
[0028] The gate oxide layer is located on the side of the drift region away from the substrate and covers part of the drift region. The gate electrode is located on the side of the gate oxide layer away from the drift region and covers the gate oxide layer; wherein, along the direction perpendicular to the substrate, the thickness of the gate oxide layer covered by the part of the gate electrode vertically projected within the JFET is the avalanche resistance thickness, and the thickness of all other gate oxide layers is the standard thickness, wherein the standard thickness is the thickness of the gate oxide layer required by the basic electrical characteristics of the semiconductor structure, and the avalanche resistance thickness is greater than the standard thickness; in this way, the embodiment of the present application improves the thickness of the gate oxide layer above the JFET region on the basis of ensuring the good basic electrical characteristics of the semiconductor structure, that is, sets the thickness of the gate oxide layer above the JFET region to the avalanche resistance thickness, and the avalanche resistance thickness is greater than the standard thickness, thereby improving the avalanche resistance capability of the semiconductor structure, and applying the semiconductor structure provided by the embodiment of the present application to the SiC MOSFET device can improve the avalanche resistance capability of the SiC MOSFET device. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] In order to more clearly illustrate the technical solutions in the embodiments of the present application or related technologies, the drawings required for use in the embodiments of the present application or related technical descriptions will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without paying creative work.
[0030] Figure 1 is one of the cross-sectional schematic diagrams of a semiconductor structure in one embodiment;
[0031] Figure 2 is a second cross-sectional schematic diagram of a semiconductor structure in one embodiment;
[0032] Figure 3 The third cross-sectional schematic diagram of a semiconductor structure in one embodiment;
[0033] Figure 4 It is one of the structural schematic diagrams involved in the method for preparing a semiconductor structure in one embodiment;
[0034] Figure 5 This is the second structural schematic diagram involved in the method for preparing a semiconductor structure in an embodiment. DETAILED DESCRIPTION
[0035] In order to make the purpose, technical solution and advantages of the present application more clearly understood, the present application is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application.
[0036] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which this application belongs. The terms used herein in the specification of this application are only for the purpose of describing specific embodiments and are not intended to limit this application.
[0037] It is understood that the terms "first", "second", etc. used in this application may be used herein to describe various elements, but these elements are not limited by these terms. These terms are only used to distinguish a first element from another element. For example, without departing from the scope of this application, a first resistor may be referred to as a second resistor, and similarly, a second resistor may be referred to as a first resistor. Both the first resistor and the second resistor are resistors, but they are not the same resistor.
[0038] It can be understood that the “connection” in the following embodiments should be understood as “electrical connection”, “communication connection”, etc. if the connected circuits, modules, units, etc. have electrical signals or data transmission between each other.
[0039] It can be understood that “at least one” means one or more, “plurality” means two or more, and “at least a portion of an element” means a part or all of an element.
[0040] When used herein, the singular forms "a", "an", and "said / the" may also include plural forms, unless the context clearly indicates otherwise. It should also be understood that the terms "include / comprise" or "have" and the like specify the presence of stated features, wholes, steps, operations, components, parts, or combinations thereof, but do not exclude the possibility of the presence or addition of one or more other features, wholes, steps, operations, components, parts, or combinations thereof. At the same time, the term "and / or" used in this specification includes any and all combinations of the relevant listed items.
[0041] The semiconductor structure provided in the embodiments of the present application can be applied to SiC MOSFET devices.
[0042] In an exemplary embodiment, Figure 1 As shown, a semiconductor structure is provided. The semiconductor structure includes a substrate 110 , a gate oxide layer 150 and a gate electrode 170 .
[0043] The substrate 110 includes a drift region 120, that is, the drift region 120 is formed in the substrate 110. Exemplarily, the substrate 110 is an N-type SiC substrate, and the drift region 120 is an N-type drift region. The thickness of the substrate 110 is generally several hundred microns; the doping of the substrate 110 is generally heavily doped, and the doping concentration of the substrate 110 is generally 3x10 19 cm -1The resistivity of the substrate 110 is very low, which is convenient for realizing ohmic contact. The thickness and doping concentration of the drift region 120 determine the withstand voltage of the semiconductor structure. The greater the thickness, the stronger the withstand voltage, but the corresponding on-resistance will also increase. The smaller the doping concentration, the stronger the withstand voltage. The thickness of the drift region 120 is generally several to tens of microns. The doping concentration of the drift region 120 is generally 10 14 cm -1 ~10 16 cm -1 between.
[0044] The drift region 120 includes a well region 130 and a JFET region 140, that is, the well region 130 and the JFET region 140 are formed in the drift region 120. Exemplarily, the well region 130 is a P-type well region (i.e., a Pwell region); the Pwell region can be formed by implanting P-type ions in the drift region 120. When a forward bias is applied, the Pwell channel region will be inverted to make the semiconductor structure conductive; the doping concentration of the Pwell region is generally 10 16 cm -1 ~10 18 cm -1 The well region 130 surrounds the JFET region 140, wherein the well region 130 includes a first doping region 131 and a second doping region 132, that is, the first doping region 131 and the second doping region 132 are formed in the well region 130, the first doping region 131 is located between the JFET region 140 and the second doping region 132, and the ion doping types of the first doping region 131 and the second doping region 132 are different. Exemplarily, the first doping region 131 is an N+ region; the N+ region can be formed by ion implantation in the Pwell region, and the doping concentration of the N+ region is relatively high, and the doping concentration of the N+ region is generally 10 19 cm -1 The second doping region 132 is a P+ region; the P+ region can be formed by ion implantation in the Pwell region, and the P+ region can be used to connect the N+ region and the Pwell region to avoid the adverse effects of parasitic transistors. The doping concentration of the P+ region is several orders of magnitude higher than that of the Pwell region. The doping concentration of the P+ region is generally 10 19 cm -1 The doping concentration of the JFET region 140 is generally equal to the doping concentration of the drift region 120 .
[0045] The gate oxide layer 150 is located on the side of the drift region 120 away from the substrate 110 and covers a portion of the drift region 120. The quality of the gate oxide layer 150 will affect the mobility of the channel. 2 .
[0046] The gate electrode 170 is located on a side of the gate oxide layer 150 away from the drift region 120 and covers the gate oxide layer 150; wherein, along a direction perpendicular to the substrate 110, the thickness of the gate oxide layer 150 covered by the portion of the gate electrode 170 vertically projected within the JFET region 140 is the avalanche resistance thickness, and the thickness of all other gate oxide layers 150 is the standard thickness, wherein the avalanche resistance thickness is greater than the standard thickness. Exemplarily, the material of the gate electrode 170 is polysilicon material.
[0047] In this embodiment, the standard thickness is the thickness of the gate oxide layer required by the basic electrical characteristics of the semiconductor structure, and the basic electrical characteristics are, for example, the threshold voltage, on-resistance, switching characteristics, etc. of the semiconductor structure. Setting D1 as the standard thickness can ensure that the basic electrical characteristics of the semiconductor structure are good. On the basis of ensuring that the basic electrical characteristics of the semiconductor structure are good, by setting D2 to be greater than D1, that is, by improving the thickness of the gate oxide layer 150 above the JFET region 140, the quality of the gate oxide layer 150 is improved, thereby improving the avalanche resistance of the semiconductor structure. The semiconductor structure provided in the embodiment of the present application is applied to a SiC MOSFET device, and the avalanche resistance of the SiC MOSFET device can be improved.
[0048] In an exemplary embodiment, continue to refer to Figure 1 , the gate oxide layer 150 covered by the portion of the gate electrode 170 whose vertical projection is located within the JFET region 140, has a vertical projection toward the substrate 110 as a first vertical projection, and the first vertical projection is located within the JFET region 140; the vertical projections of all the remaining gate oxide layers 150 toward the substrate 110 are second vertical projections, and the second vertical projections are located within the JFET region 140, the drift region 120 between the JFET region 140 and the first doping region 131, and the first doping region 131.
[0049] In this embodiment, the thickness D1 of the gate oxide layer 150 with the second vertical projection is a standard thickness, that is, the thickness of the gate oxide layer 150 above the channel is kept unchanged, thereby ensuring that the basic electrical characteristics of the semiconductor structure are good. On the basis of ensuring that the basic electrical characteristics of the semiconductor structure are good, the thickness D2 of the gate oxide layer 150 with the first vertical projection is greater than D1, that is, the thickness of the gate oxide layer 150 above the JFET region 140 is increased, so that the quality of the gate oxide layer 150 is improved, and the ability of the gate oxide layer 150 to withstand high-intensity electric fields can be improved, thereby improving the avalanche resistance of the semiconductor structure. The semiconductor structure provided in the embodiment of the present application is applied to a SiC MOSFET device, and the avalanche resistance of the SiC MOSFET device can be improved.
[0050] In an exemplary embodiment, continue to refer to Figure 1The thickness of the portion of the gate electrode 170 whose vertical projection is located within the JFET region 140 is greater than the thickness of the gate electrode 170 covering all the remaining gate oxide layers 150 .
[0051] In this embodiment, the thickness of the gate oxide layer 150 above the channel is kept unchanged, thereby ensuring that the basic electrical characteristics of the semiconductor structure are good. At the same time, the thickness of the gate oxide layer 150 above the JFET region 140 is increased, thereby improving the quality of the gate oxide layer 150 and the ability of the gate oxide layer 150 to withstand high-intensity electric fields, thereby improving the avalanche resistance of the semiconductor structure.
[0052] In an exemplary embodiment, referring to Figure 2 The semiconductor structure further includes a dielectric layer 160. The dielectric layer 160 is located on a side of the gate electrode 170 away from the gate oxide layer 150 and covers the gate electrode 170 and a portion of the first doped region 131. Exemplarily, the material of the dielectric layer 160 is SiO 2 .
[0053] In an exemplary embodiment, the dielectric layer 160 and the gate oxide layer 150 are made of the same material, so that the semiconductor structure is simple and the cost is low.
[0054] In an exemplary embodiment, referring to Figure 3 The semiconductor structure further includes a source electrode 190 and a drain electrode 180. The source electrode 190 is located on a side of the dielectric layer 160 away from the gate electrode 170, and covers the dielectric layer 160, a portion of the first doping region 131, and the second doping region 132. The drain electrode 180 is located on a side of the substrate 110 away from the drift region 120, and covers the substrate 110.
[0055] Here, under high temperature conditions, the source metal and the drain metal respectively form ohmic contacts with the heavily doped SiC material, thereby forming the source electrode 190 and the drain electrode 180 .
[0056] In an exemplary embodiment, a SiC MOSFET device is provided. The SiC MOSFET device includes the semiconductor structure in any of the above embodiments.
[0057] The SiC MOSFET device provided in this embodiment belongs to the same inventive concept as the above-mentioned semiconductor structure, and can achieve the same technical effect, and the repeated contents will not be repeated here.
[0058] In an exemplary embodiment, a method for preparing a semiconductor structure is provided. The method for preparing a semiconductor structure can be used to prepare the semiconductor structure in any of the above embodiments. The method for preparing a semiconductor structure comprises the following steps:
[0059] Providing a substrate, the substrate comprising a drift region, the drift region comprising a well region and a JFET region, the well region surrounding the JFET region; the well region comprising a first doping region and a second doping region, the first doping region being located between the JFET region and the second doping region;
[0060] In which, the substrate is exemplarily an N-type SiC substrate, a drift region is formed in the substrate, and exemplarily, the drift region is an N-type drift region; the thickness of the substrate can be several hundred microns, and the doping concentration of the substrate can be 3x10 19 cm -1 The resistivity of the substrate is very low, which is convenient for realizing ohmic contact; the thickness of the drift region can be several to tens of microns, and the doping concentration of the drift region can be between 10 14 cm -1 ~10 16 cm -1 between.
[0061] A well region and a JFET region are formed in the drift region; illustratively, the well region is a P-type well region (i.e., a Pwell region), and the Pwell region can be formed by implanting P-type ions in the drift region. When a forward bias is applied, the Pwell channel region will be inverted to make the semiconductor structure conductive; the doping concentration of the Pwell region can be between 10 16 cm -1 ~10 18 cm -1 A first doping region and a second doping region are formed in the well region, and the ion doping types of the first doping region and the second doping region are different; illustratively, the first doping region is an N+ region; the N+ region can be formed by ion implantation in the Pwell region, and the doping concentration of the N+ region can be 10 19 cm -1 The second doped region is a P+ region, which can be formed by ion implantation in the Pwell region. The P+ region can be used to connect the N+ region and the Pwell region to avoid the adverse effects of parasitic transistors. The doping concentration of the P+ region is several orders of magnitude higher than that of the Pwell region. The doping concentration of the P+ region can be 10 19 cm -1 Above; the doping concentration of the JFET region is generally equal to the doping concentration of the drift region.
[0062] forming a gate oxide layer, which is located on a side of the drift region away from the substrate and covers a portion of the drift region;
[0063] Wherein, the material of the gate oxide layer is SiO 2 .
[0064] A gate electrode is formed, which is located on a side of the gate oxide layer away from the drift region and covers the gate oxide layer; wherein, along a direction perpendicular to the substrate, the thickness of the gate oxide layer covered by the portion of the gate electrode vertically projected within the JFET is the avalanche-resistant thickness, and the thickness of all other gate oxide layers is the standard thickness, wherein the avalanche-resistant thickness is greater than the standard thickness.
[0065] Exemplarily, the material of the gate electrode is polysilicon material.
[0066] In this embodiment, the standard thickness is the thickness of the gate oxide layer required by the basic electrical characteristics of the semiconductor structure, such as the threshold voltage, on-resistance, switching characteristics, etc. of the semiconductor structure. The thickness of the gate oxide layer above the channel is kept unchanged, thereby ensuring that the basic electrical characteristics of the semiconductor structure are good, while the thickness of the gate oxide layer above the JFET region is increased, thereby improving the quality of the gate oxide layer, and improving the ability of the gate oxide layer to withstand high-intensity electric fields, thereby improving the avalanche resistance of the semiconductor structure.
[0067] In an exemplary embodiment, forming a gate oxide layer includes:
[0068] refer to Figure 4 , forming an intermediate layer 150 ′, which is located on a side of the drift region 120 away from the substrate 110 and covers a portion of the drift region 120 , and the thickness of the intermediate layer 150 ′ is an avalanche resistance thickness D2;
[0069] refer to Figure 5 , the middle layer 150' is etched so that along the direction perpendicular to the substrate 110, the thickness of the gate oxide layer 150 covered by the portion of the gate electrode 170 vertically projected within the JFET region 140 is the avalanche resistance thickness D2, and the thickness of all other gate oxide layers 150 is the standard thickness D1.
[0070] In this embodiment, the standard thickness is the thickness of the gate oxide layer required by the basic electrical characteristics of the semiconductor structure, and the basic electrical characteristics are, for example, the threshold voltage, on-resistance, switching characteristics, etc. of the semiconductor structure. On the basis of keeping the thickness of the gate oxide layer 150 above the channel unchanged, that is, setting D1 to the standard thickness, thereby ensuring that the basic electrical characteristics of the semiconductor structure are good, the bottom etching of the gate electrode 170 is performed, that is, by increasing the thickness of the gate oxide layer 150 above the JFET region 140, the quality of the gate oxide layer 150 is improved, and the ability of the gate oxide layer 150 to withstand high-intensity electric fields can be improved, thereby improving the avalanche resistance of the semiconductor structure. The semiconductor structure provided in the embodiment of the present application is applied to a SiC MOSFET device, and the avalanche resistance of the SiC MOSFET device can be improved.
[0071] In the description of this specification, the description with reference to the terms "some embodiments", "other embodiments", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present application. In this specification, the schematic description of the above terms does not necessarily refer to the same embodiment or example.
[0072] The technical features of the above embodiments may be combined arbitrarily. To make the description concise, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this application.
[0073] The above-described embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the present application. It should be pointed out that, for a person of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the protection scope of the present application. Therefore, the protection scope of the present application shall be subject to the attached claims.
Claims
1. A semiconductor structure, It is characterized in that include: A substrate, comprising a drift region; the drift region comprising a well region and a JFET region, the well region surrounding the JFET region; the well region comprising a first doping region and a second doping region, the first doping region being located between the JFET region and the second doping region; A gate oxide layer, located on a side of the drift region away from the substrate and covering a portion of the drift region; A gate electrode is located on a side of the gate oxide layer away from the drift region and covers the gate oxide layer; wherein, along a direction perpendicular to the substrate, the thickness of the gate oxide layer covered by the portion of the gate electrode vertically projected within the JFET is an avalanche-resistant thickness, and the thickness of all other gate oxide layers is a standard thickness, wherein the avalanche-resistant thickness is greater than the standard thickness.
2. The semiconductor structure according to claim 1, It is characterized in that The gate oxide layer covered by the portion of the gate electrode whose vertical projection is located within the JFET, has a vertical projection toward the substrate as a first vertical projection, and the first vertical projection is located within the JFET region; The vertical projections of all the remaining gate oxide layers toward the substrate are second vertical projections, and the second vertical projections are located in the JFET region, the drift region between the JFET region and the first doping region, and the first doping region.
3. The semiconductor structure according to claim 2, It is characterized in that The thickness of the portion of the gate electrode whose vertical projection is located within the JFET is greater than the thickness of the gate electrode covering all the remaining gate oxide layers.
4. The semiconductor structure according to claim 2, It is characterized in that Also includes: The dielectric layer is located on a side of the gate electrode away from the gate oxide layer and covers the gate electrode and a portion of the first doped region.
5. The semiconductor structure according to claim 4, It is characterized in that The dielectric layer and the gate oxide layer are made of the same material.
6. The semiconductor structure according to claim 4, It is characterized in that Also includes: A source electrode, located on a side of the dielectric layer away from the gate electrode, and covering the dielectric layer, a portion of the first doped region, and the second doped region; The drain electrode is located on a side of the substrate away from the drift region and covers the substrate.
7. The semiconductor structure according to claim 1, It is characterized in that The second doping region has a doping type opposite to that of the first doping region.
8. A SiC MOSFET device, It is characterized in that Comprising the semiconductor structure according to any one of claims 1 to 7.
9. A method for preparing a semiconductor structure, It is characterized in that include: Providing a substrate, the substrate comprising a drift region, the drift region comprising a well region and a JFET region, the well region surrounding the JFET region; the well region comprising a first doping region and a second doping region, the first doping region being located between the JFET region and the second doping region; forming a gate oxide layer, which is located on a side of the drift region away from the substrate and covers a portion of the drift region; A gate electrode is formed, which is located on a side of the gate oxide layer away from the drift region and covers the gate oxide layer; wherein, along a direction perpendicular to the substrate, the thickness of the gate oxide layer covered by the portion of the gate electrode vertically projected within the JFET is an avalanche-resistant thickness, and the thickness of all other gate oxide layers is a standard thickness, wherein the avalanche-resistant thickness is greater than the standard thickness.
10. The method for preparing a semiconductor structure according to claim 9, It is characterized in that The forming of the gate oxide layer comprises: forming an intermediate layer, which is located on a side of the drift region away from the substrate and covers a portion of the drift region; The intermediate layer is etched so that the thickness of the gate oxide layer covered by the portion of the gate electrode vertically projected within the JFET along a direction perpendicular to the substrate is avalanche-resistant thickness, and the thickness of all other gate oxide layers is standard thickness.
Citation Information
Cited By
Metal-oxide-semiconductor field effect transistor (MOSFET) device and manufacturing method