Preparation method of semiconductor structure

By forming a spaced-arranged mandrel structure and side wall in the semiconductor structure, and using the side wall as a mask to etch the layer to be etched, the problem of poor uniformity of the capacitance hole size is solved, and the yield of the capacitance structure is improved.

CN118946137AInactive Publication Date: 2024-11-12CHANGXIN MEMORY TECH INC
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
CN202310500543.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-04
Publication Date
2024-11-12
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

In the production of existing semiconductor structures, the uniformity of the size of the capacitance holes is poor, resulting in a decrease in the yield of the capacitance structure.

Method used

By forming a plurality of spaced aligned mandrel structures on the layer to be etched, and forming a side wall on its side, filling the side wall area to form a sacrificial layer, removing the mandrel structure and sacrificial layer, retaining the side wall, and using the side wall as The mask etches the layer to be etched to form a capacitance hole.

Benefits of technology

The uniformity of the size of the capacitor hole is improved, the yield of the capacitor structure is enhanced, and the position consistency and size uniformity of the capacitor hole are ensured.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118946137A_ABST
    Figure CN118946137A_ABST
Patent Text Reader

Abstract

The invention provides a preparation method of a semiconductor structure, relates to the technical field of semiconductors, and is used for improving the size uniformity of capacitance holes. The preparation method comprises the steps that a patterned first mask layer is formed on a to-be-etched layer, the first mask layer comprises a plurality of first core shaft structures which are arranged at intervals in the first direction, each first core shaft structure extends in the second direction, and the second direction intersects with the first direction; forming a first side wall and a first sacrificial layer; removing the first sacrificial layer and the first mandrel structure; a second mask layer is formed, and the second mask layer fills the area defined by the first side walls and is located on the top faces of the first side walls; patterning the second mask layer to form a plurality of second core shaft structures which are arranged at intervals along a second direction; forming a second side wall and a second sacrificial layer; removing the second sacrificial layer and the second mandrel structure; and etching the to-be-etched layer by taking the first side wall and the second side wall as masks to form a capacitor hole. The method is used for improving the size uniformity of the capacitor holes.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The embodiments of the present disclosure relate to the field of semiconductor technology, and in particular, to a method for preparing a semiconductor structure. Background Art

[0002] In the process of manufacturing a semiconductor structure, it is usually necessary to form a target pattern in a layer to be etched, for example, to form a capacitor hole in a stacked layer to be etched, so as to form a capacitor structure in the capacitor hole.

[0003] In the related art, it is usually necessary to form a hard mask layer on the stack to be etched, and use a multi-patterning process to pattern the hard mask layer to form a mask pattern in the hard mask layer; wherein the multi-patterning process may include but is not limited to a self-aligned double patterning (Self-Aligned Double Patterning, referred to as SADP) process or a self-aligned quadruple patterning (Self-Aligned Quadruple Patterning, referred to as SAQP); thereafter, the hard mask layer having the mask pattern is used as a mask to etch the stack to be etched to form a capacitor hole in the stack to be etched.

[0004] However, the size uniformity of the capacitor holes formed by the above-mentioned preparation method is poor, thereby reducing the yield of the capacitor structure formed subsequently. Summary of the invention

[0005] In view of the above problems, an embodiment of the present disclosure provides a method for preparing a semiconductor structure, which can improve the uniformity of the size of the formed capacitor holes.

[0006] The present disclosure provides a method for preparing a semiconductor structure, comprising the following steps:

[0007] Forming a first mask layer on the layer to be etched, and patterning the first mask layer to form a plurality of first mandrel structures spaced apart along a first direction in the first mask layer, each of the first mandrel structures extending along a second direction, and the second direction intersecting the first direction;

[0008] forming a first sidewall on a side of the first mandrel structure, and forming a first sacrificial layer filling an area surrounded by the first sidewall;

[0009] removing the first sacrificial layer and the first mandrel structure, and retaining the first plurality of sidewall spacers;

[0010] forming a second mask layer, wherein the second mask layer completely fills the area surrounded by the first sidewalls and is located on the top surface of the first sidewalls;

[0011] Patterning the second mask layer to form a plurality of second mandrel structures spaced apart along the second direction in the second mask layer, each of the second mandrel structures extending along the first direction;

[0012] forming a second sidewall on a side of the second mandrel structure, and forming a second sacrificial layer filling an area surrounded by the second sidewall;

[0013] removing the second sacrificial layer and the second mandrel structure, and retaining a plurality of the second sidewalls;

[0014] The layer to be etched is etched using the first sidewall and the second sidewall as masks to form a capacitor hole in the layer to be etched.

[0015] In some embodiments, under the same etching conditions, the etching rate of the first sacrificial layer is substantially the same as the etching rate of the first mandrel structure;

[0016] Under the same etching conditions, the etching rate of the second sacrificial layer is substantially the same as the etching rate of the second mandrel structure.

[0017] In some embodiments, adjacent first sidewalls form first grooves, and the depths of the first grooves are the same;

[0018] Adjacent second sidewalls form second grooves, and a plurality of second grooves have the same depth.

[0019] In some embodiments, the first core shaft structure includes a first hard mask layer and a second hard mask layer, the second hard mask layer is arranged on the first hard mask layer, the thickness of the second hard mask layer is less than or equal to 1 / 4 of the thickness of the first hard mask layer, the material of the first sacrificial layer is the same as the material of the first hard mask layer, and the top surface of the first sacrificial layer is flush with the top surface of the first hard mask layer.

[0020] In some embodiments, the step of removing the first sacrificial layer and the first mandrel structure comprises:

[0021] removing the second hard mask layer and a portion of the thickness of the first sacrificial layer, wherein a top surface of the remaining first sacrificial layer is lower than a top surface of the first hard mask layer;

[0022] The first hard mask layer and remaining first sacrificial layer are removed.

[0023] In some embodiments, the step of forming the first sidewall spacer includes:

[0024] forming a first spacer material layer, wherein the first spacer material layer covers the side surfaces and the top surface of the first mandrel structure, and covers the top surface of the first mask layer exposed between adjacent first mandrel structures;

[0025] The first sidewall material layer located on the top surface of the first core shaft structure and the top surface of the first mask layer exposed between adjacent first core shaft structures is removed, and the first sidewall material layer retained on the side surface of the first core shaft structure constitutes the first sidewall; the first groove is surrounded by adjacent first sidewalls.

[0026] In some embodiments, the step of forming the first sacrificial layer filling the area surrounded by the first sidewall spacer includes:

[0027] forming a first sacrificial material layer, wherein the first sacrificial material layer completely fills the first trench and covers the top surface of the first mandrel structure and the first sidewall;

[0028] A portion of the first sacrificial material layer is removed, and the first sacrificial material layer retained in the first groove forms a first sacrificial layer; the top surface of the first sacrificial layer is flush with the top surface of the first sidewall.

[0029] In some embodiments, the steps of forming a first mask layer on the layer to be etched and patterning the first mask layer include:

[0030] forming a third hard mask layer, a fourth hard mask layer, a first hard mask material layer and a second hard mask material layer which are sequentially stacked on the layer to be etched;

[0031] The second hard mask material layer and the first hard mask material layer are patterned to form a plurality of first core shaft structures; each of the first core shaft structures comprises a first hard mask layer and a second hard mask layer stacked together; wherein the retained first hard mask material layer constitutes a first hard mask layer, and the retained second hard mask material layer constitutes a second hard mask layer.

[0032] In some embodiments, the step of forming a plurality of the first mandrel structures comprises:

[0033] forming a first anti-reflection layer and a first photoresist layer stacked in sequence on the second hard mask material layer;

[0034] Patterning the first photoresist layer to form a plurality of first openings spaced apart along the first direction, each of the first openings extending along the second direction;

[0035] Using the patterned first photoresist layer as a mask, removing the first anti-reflection layer, the second hard mask material layer, and the first hard mask material layer exposed in the first opening;

[0036] The first photoresist layer and the remaining first anti-reflection layer are removed.

[0037] In some embodiments, the step of forming the second mask layer includes:

[0038] forming a fifth hard mask layer, wherein the fifth hard mask layer completely fills the area surrounded by the first sidewall spacer;

[0039] A sixth hard mask layer, a seventh hard mask material layer and an eighth hard mask material layer are sequentially stacked on the fifth hard mask layer; the fifth hard mask layer, the sixth hard mask layer, the seventh hard mask material layer and the eighth hard mask material layer constitute the second mask layer.

[0040] In some embodiments, the step of patterning the second mask layer to form the second mandrel structure includes:

[0041] forming a second anti-reflection layer and a second photoresist layer stacked in sequence on the eighth hard mask material layer;

[0042] Patterning the second photoresist layer to form a plurality of second openings spaced apart along the second direction, each of the second openings extending along the first direction;

[0043] Using the patterned second photoresist layer as a mask, removing the second anti-reflective layer, the eighth hard mask material layer and the seventh hard mask material layer exposed in the second opening, the remaining seventh hard mask material layer constitutes a seventh hard mask layer, the remaining eighth hard mask material layer constitutes an eighth hard mask layer, and the seventh hard mask layer and the eighth hard mask layer constitute the second mandrel structure;

[0044] The second photoresist layer and the remaining second anti-reflection layer are removed.

[0045] In some embodiments, the step of forming the second sidewall spacer includes:

[0046] forming a second spacer material layer, wherein the second spacer material layer covers the side surfaces and the top surface of the second mandrel structure, and covers the top surface of the second mask layer exposed between adjacent second mandrel structures;

[0047] The second sidewall material layer located on the top surface of the second mandrel structure and the top surface of the second mask layer exposed between adjacent second mandrel structures is removed, and the second sidewall material layer retained on the side of the second mandrel structure constitutes a second sidewall; and a second groove is formed between adjacent second sidewalls.

[0048] In some embodiments, the step of forming the second sacrificial layer includes:

[0049] forming a second sacrificial material layer, wherein the second sacrificial material layer completely fills the second trench and covers the top surface of the second mandrel structure and the second sidewall;

[0050] A portion of the thickness of the second sacrificial material layer is removed, and the second sacrificial material layer remaining in the second groove constitutes a second sacrificial layer; the top surface of the second sacrificial layer is flush with the top surface of the second sidewall.

[0051] In the method for preparing the semiconductor structure provided by the embodiment of the present disclosure, a first sacrificial layer is formed in the area enclosed by the first side wall to protect the first mask layer exposed between the first side walls. In this way, when the first mandrel structure is removed, the first sacrificial layer is removed simultaneously to prevent the first mask layer exposed between the first side walls from being etched, so that the height of the retained first side wall is consistent. Accordingly, a second sacrificial layer is formed in the area enclosed by the second side wall to ensure that the height of the retained second side wall is consistent. Finally, using the first side wall and the second side wall as masks, when etching the layer to be etched, it can be ensured that the size of the capacitor hole formed is uniform, thereby improving the yield of the formed capacitor structure.

[0052] In addition to the technical problems solved by the embodiments of the present disclosure, the technical features that constitute the technical solutions, and the beneficial effects brought about by the technical features of the technical solutions described above, other technical problems that can be solved by the method for preparing the semiconductor structure provided by the embodiments of the present disclosure, other technical features included in the technical solutions, and the beneficial effects brought about by these technical features will be further described in detail in the specific implementation methods. BRIEF DESCRIPTION OF THE DRAWINGS

[0053] In order to more clearly illustrate the embodiments of the present disclosure or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present disclosure. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.

[0054] Figure 1 It is a schematic diagram after forming a first sidewall in the related art;

[0055] Figure 2 A distribution diagram of capacitor holes provided in the related art;

[0056] Figure 3 A process flow chart of a method for preparing a semiconductor structure provided by an embodiment of the present disclosure;

[0057] Figure 4 A schematic diagram of a semiconductor structure after a first photoresist layer is formed in the method for preparing the semiconductor structure according to an embodiment of the present disclosure;

[0058] Figure 5 A schematic diagram of a semiconductor structure after a first mandrel structure is formed in the method for preparing the semiconductor structure provided by an embodiment of the present disclosure;

[0059] Figure 6 A schematic diagram of a method for preparing a semiconductor structure provided in an embodiment of the present disclosure after forming a first spacer material layer;

[0060] Figure 7 A schematic diagram of a method for preparing a semiconductor structure provided in an embodiment of the present disclosure after forming a first sidewall spacer;

[0061] Figure 8 A schematic diagram of a method for preparing a semiconductor structure provided in an embodiment of the present disclosure after a first sacrificial material layer is formed;

[0062] Fig. 9 A schematic diagram of a method for preparing a semiconductor structure provided in an embodiment of the present disclosure after a first sacrificial layer is formed;

[0063] Fig.10 A schematic diagram of the semiconductor structure manufacturing method provided by the embodiment of the present disclosure after the second hard mask layer is removed;

[0064] Fig.11 A schematic diagram of the method for preparing a semiconductor structure provided by an embodiment of the present disclosure after removing the first hard mask layer and the first sacrificial layer;

[0065] Fig.12 A schematic diagram of a semiconductor structure after a fifth hard mask material layer is formed in the method for preparing the semiconductor structure according to an embodiment of the present disclosure;

[0066] Fig.13 A schematic diagram of a semiconductor structure after a fifth hard mask layer is formed in the method for preparing the semiconductor structure according to an embodiment of the present disclosure;

[0067] Fig.14 A schematic diagram of a semiconductor structure after a second photoresist layer is formed in the method for preparing the semiconductor structure according to an embodiment of the present disclosure;

[0068] Fig.15 A schematic diagram of forming a second mandrel structure in a method for preparing a semiconductor structure provided by an embodiment of the present disclosure;

[0069] Fig.16 A schematic diagram of a semiconductor structure manufacturing method according to an embodiment of the present disclosure after a second spacer material layer is formed;

[0070] Fig.17 A schematic diagram of a semiconductor structure after a second sidewall spacer is formed in the method for preparing the semiconductor structure according to an embodiment of the present disclosure;

[0071] Fig.18 A schematic diagram of a semiconductor structure after forming a second sacrificial material layer in the method for preparing the semiconductor structure provided by an embodiment of the present disclosure;

[0072] Fig.19 A schematic diagram of a method for preparing a semiconductor structure provided in an embodiment of the present disclosure after a second sacrificial layer is formed;

[0073] Fig. 20 A schematic diagram of a method for preparing a semiconductor structure provided by an embodiment of the present disclosure after removing the eighth hard mask layer;

[0074] Fig.21 A schematic diagram of the method for preparing a semiconductor structure provided by an embodiment of the present disclosure after removing the seventh hard mask layer and the second sacrificial layer;

[0075] Fig. 22 A distribution diagram of the first spacer and the second spacer in the method for preparing the semiconductor structure provided by an embodiment of the present disclosure;

[0076] Fig.23 A schematic diagram of forming a capacitor hole in a method for preparing a semiconductor structure provided by an embodiment of the present disclosure;

[0077] Fig.24 A distribution diagram of capacitor holes formed in a method for preparing a semiconductor structure provided in an embodiment of the present disclosure.

[0078] Reference numerals:

[0079] 1: layer to be etched; 2: first mask layer; 3: first sidewall; 4: capacitor hole;

[0080] 10: layer to be etched; 11: support layer; 12: third sacrificial layer; 13: capacitor hole;

[0081] 20: base;

[0082] 30: first mask layer; 31: first hard mask material layer; 32: second hard mask material layer; 33: third hard mask layer; 34: fourth hard mask layer; 35: first mandrel structure; 351: first hard mask layer; 352: second hard mask layer;

[0083] 40: first anti-reflection layer;

[0084] 50: first photoresist layer; 51: first opening;

[0085] 60: dielectric layer; 61: first dielectric layer; 62: second dielectric layer;

[0086] 70: first spacer; 71: first spacer material layer; 72: first groove;

[0087] 80: first sacrificial layer; 81: first sacrificial material layer;

[0088] 90: second mask layer; 91: fifth hard mask layer; 92: sixth hard mask layer; 93: seventh hard mask material layer; 94: eighth hard mask material layer; 95: fifth hard mask material layer; 96: second mandrel structure; 961: seventh hard mask layer; 962: eighth hard mask layer;

[0089] 100: second anti-reflection layer;

[0090] 110: second photoresist layer; 111: second opening;

[0091] 120: second spacer; 121: second spacer material layer; 122: second groove;

[0092] 130 : a second sacrificial layer; 131 : a second sacrificial material layer. DETAILED DESCRIPTION

[0093] When the SADP process or SAQP process is used to pattern the layer to be etched, the target pattern formed is prone to uneven size. The following will take the target pattern as a capacitor hole as an example for detailed description. Figure 1 , a first mask layer 2 is formed on the layer to be etched 1, and the first mask layer 2 is patterned to form a plurality of first mandrel structures arranged at intervals; then, a first sidewall 3 covering the side of each first mandrel structure is formed; then, the first mandrel structure is removed, and a plurality of first sidewalls 3 are retained. However, in the process of etching the first mandrel structure, the first mask layer 2 partially exposed between adjacent first sidewalls is also etched synchronously, resulting in a height difference in the depth of the region between adjacent first sidewalls 3.

[0094] Afterwards, a second mask layer is formed to cover the first sidewalls and fill the area between the adjacent first sidewalls, and the second sidewalls are formed by the above process. Accordingly, there is a height difference in the depth of the area between the adjacent second sidewalls. When the first sidewalls and the second sidewalls are used to etch the etched layer 1, the capacitor holes 4 formed have defects of position offset and uneven size (please refer to the attached Figure 2 ), thereby reducing the yield of the capacitor structure formed subsequently.

[0095] In view of this, the embodiment of the present disclosure provides a method for preparing a semiconductor structure, by forming a first sacrificial layer in the area surrounded by the first side wall, protecting the first mask layer exposed between the first side walls, so that when the first mandrel structure is removed, the first sacrificial layer will be removed simultaneously to prevent the first mask layer exposed between the first side walls from being etched, so that the height of the retained first side wall is consistent. Accordingly, a second sacrificial layer is formed in the area surrounded by the second side wall, which can ensure that the height of the retained second side wall is consistent. Finally, using the first side wall and the second side wall as masks, when etching the layer to be etched, it can be ensured that the size of the capacitor hole formed is uniform, thereby improving the yield of the formed capacitor structure.

[0096] In order to make the above-mentioned purposes, features and advantages of the embodiments of the present disclosure more obvious and understandable, the technical solutions in the embodiments of the present disclosure will be clearly and completely described below in conjunction with the drawings in the embodiments of the present disclosure. Obviously, the described embodiments are only part of the embodiments of the present disclosure, not all of the embodiments. Based on the embodiments in the present disclosure, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present disclosure.

[0097] The present embodiment does not limit the semiconductor structure. The semiconductor structure will be described below by taking a dynamic random access memory (DRAM) as an example, but the present embodiment is not limited thereto. The semiconductor structure in the present embodiment may also be other structures.

[0098] Please refer to the attached Figure 3 , a method for preparing a semiconductor structure provided by an embodiment of the present disclosure includes the following steps:

[0099] Step S100: forming a first mask layer on the layer to be etched, and patterning the first mask layer to form a plurality of first mandrel structures spaced apart along a first direction in the first mask layer, each of the first mandrel structures extending along a second direction intersecting the first direction.

[0100] In this embodiment, the layer to be etched 10 can be a substrate or other structures (for example, a stacked structure). In one example, the layer to be etched 10 is a substrate, and the method for preparing a semiconductor structure provided by the embodiment of the present disclosure can form a plurality of active columns arranged at intervals in the substrate, and shallow trenches are formed between adjacent active columns to facilitate the formation of a shallow trench isolation structure (STI) in the shallow trench. In another example, the layer to be etched 10 can also be a supporting layer for supporting a capacitor structure. It should be understood that when the layer to be etched 10 is a supporting layer, the layer to be etched 10 needs to be formed on a substrate 20, and the substrate 20 is used to provide support for the layer to be etched 10. Among them, the substrate 20 can be a silicon (Si) substrate, a germanium (Ge) substrate, a silicon germanium (GeSi) substrate, a silicon carbide (SiC) substrate, a silicon on insulator (SOI) substrate, or a germanium on insulator (GOI) substrate.

[0101] The following will take the layer 10 to be etched as a supporting layer as an example to describe in detail the various steps of the method for preparing the semiconductor structure provided by the embodiment of the present disclosure.

[0102] Please refer to the attached Figure 4 , the layer to be etched 10 may include at least two supporting layers 11 and a third sacrificial layer 12 located between adjacent supporting layers 11. Among them, the material of the supporting layer 11 may include silicon nitride, but is not limited to this. The material of the third sacrificial layer 12 may include silicon oxide, but is not limited to this. As an example, the number of layers of the supporting layer 11 may be three layers, and the three supporting layers 11 are arranged at intervals in a direction perpendicular to the substrate 20, and the third sacrificial layer 12 is arranged between adjacent supporting layers 11. In this embodiment, by setting three supporting layers 11, the supporting capacity of the layer to be etched 10 can be enhanced, the collapse of the capacitor structure formed subsequently can be prevented, and the yield of the capacitor structure is improved.

[0103] A first mask layer 30 is formed on the side of the layer to be etched 10 away from the substrate 20 by a deposition process. The deposition process includes chemical vapor deposition (CVD), physical vapor deposition (PVD), or atomic layer deposition (ALD).

[0104] In this embodiment, the first mask layer 30 may include multiple layers to ensure accuracy during the pattern transfer process. Figure 5, patterning the first mask layer 30, that is, removing part of the first mask layer 30 to form a plurality of first mandrel structures 35 in the first mask layer 30, wherein the plurality of first mandrel structures 35 are arranged at intervals along the first direction, and each first mandrel structure 35 extends along the second direction. The first direction intersects the second direction. The first direction may be an attached Figure 5 The middle M direction, the second direction can be the Figure 5 Middle N direction.

[0105] For example, please refer to the attached Figure 4 The third hard mask layer 33, the fourth hard mask layer 34, the first hard mask material layer 31 and the second hard mask material layer 32 are sequentially stacked on the layer to be etched 10 by a deposition process. The third hard mask layer 33 is disposed on the surface of the layer to be etched 10 away from the substrate 20.

[0106] The material of the third hard mask layer 33 may include amorphous carbon (ACL), which has a relatively high hardness, and is beneficial for ensuring the accuracy of pattern transfer during etching of the third hard mask layer 33, thereby improving the yield of the formed semiconductor structure.

[0107] The fourth hard mask material layer 34 and the second hard mask material layer 32 are made of the same material, for example, both include silicon oxynitride. The first hard mask material layer 31 includes a spin on hard mask (Spin On Hardmask, SOH for short) material.

[0108] Afterwards, the second hard mask material layer 32 and the first hard mask material layer 31 are patterned to form a plurality of first mandrel structures 35. The plurality of first mandrel structures 35 are arranged along the first direction M at intervals.

[0109] Each first mandrel structure 35 includes a first hard mask layer 351 and a second hard mask layer 352 which are stacked; the first hard mask layer 351 is disposed on the fourth hard mask layer 34. The retained first hard mask material layer 31 constitutes the first hard mask layer 351, and the retained second hard mask material layer 32 constitutes the second hard mask layer 352.

[0110] In this embodiment, the process steps of patterning the second hard mask material layer 32 and the first hard mask material layer 31 may include the following steps:

[0111] Exemplarily, a first anti-reflection layer 40 and a first photoresist layer 50 are stacked and formed on the first hard mask material layer 31. The first anti-reflection layer 40 can be formed on the first hard mask material layer 31 by a deposition process. The first photoresist layer 50 can be formed on the surface of the first anti-reflection layer 40 away from the first mask layer 30 by coating.

[0112] After that, please refer to the attached Figure 4 , patterning the first photoresist layer 50, for example, removing part of the first photoresist layer 50 by exposure, development or etching, so as to form a plurality of first openings 51 in the first photoresist layer 50, wherein the plurality of first openings 51 are arranged at intervals along the first direction, and each first opening 51 extends along the second direction.

[0113] After that, please refer to the attached Figure 5 , using the patterned first photoresist layer 50 as a mask, the first anti-reflection layer 40 , the second hard mask material layer 32 and the first hard mask material layer 31 exposed in the first opening 51 are removed.

[0114] Please refer to the attached Figure 5 , and use etching gas or etching liquid to remove the first photoresist layer 50 and the remaining first anti-reflection layer 40 to form a plurality of first mandrel structures 35. Each first mandrel structure 35 includes a first hard mask layer 351 and a second hard mask layer 352, and the second hard mask layer 352 is disposed on the first hard mask layer 351.

[0115] The thickness of the second hard mask layer 352 is less than or equal to 1 / 4 of the thickness of the first hard mask layer 351. In this configuration, since the material of the first hard mask layer 351 is different from that of the second hard mask layer 352, by limiting the thickness ratio of the first hard mask layer 351 and the second hard mask layer 352, the etching rates of the first mandrel structure 35 and the first sacrificial layer formed subsequently are ensured to be substantially the same as much as possible, and excessive etching of the film layer below the first mandrel structure 35 and the film layer below the first sacrificial layer is avoided.

[0116] In this embodiment, the material of the first anti-reflection layer 40 may include nitride. For example, the material of the first anti-reflection layer 40 includes silicon nitride or silicon oxynitride, but is not limited thereto. The first anti-reflection layer 40 can alleviate or eliminate the standing wave effect of the first photoresist layer 50, thereby increasing the accuracy of the mask pattern transferred from the mask to the first photoresist layer 50, thereby improving the accuracy of the pattern transfer process.

[0117] It should be noted that, in the present embodiment, the first mask layer 30 can be directly deposited and formed on the layer to be etched 10. The first mask layer 30 can also be indirectly located above the layer to be etched 10. Exemplarily, a dielectric layer 60 is arranged between the first mask layer 30 and the layer to be etched 10, and the dielectric layer 60 includes a first dielectric layer 61 and a second dielectric layer 62 which are stacked in sequence, and the first dielectric layer 61 is arranged on the top surface of the layer to be etched 10 away from the substrate 20. The material of the first dielectric layer 61 is different from the material of the second dielectric layer 62. For example, the material of the first dielectric layer 61 includes polysilicon, but is not limited thereto, and the material of the second dielectric layer 62 includes silicon oxide, but is not limited thereto.

[0118] In the actual etching process, the dielectric layer 60 can be used as a mask layer, and the mask pattern can be first transferred into the dielectric layer 60 and then transferred from the dielectric layer 60 to the layer to be etched 10 to ensure the accuracy of the pattern transfer process.

[0119] Step S200: forming a first sidewall spacer on a side surface of the first mandrel structure, and forming a first sacrificial layer filling an area enclosed by the first sidewall spacer;

[0120] For example, please refer to the attached Figure 6 , the first spacer material layer 71 is formed by an atomic layer deposition process, and the first spacer material layer 71 covers the side and top surfaces of the first mandrel structure 35, and covers the top surface of the first mask layer 30 exposed between adjacent first mandrel structures 35. In other words, the first spacer material layer 71 covers the top surface of the fourth hard mask layer 34 exposed between adjacent first mandrel structures 35. In this embodiment, the first spacer material layer 71 is formed by an atomic layer deposition process, which can improve the thickness uniformity of the first spacer material layer 71.

[0121] Afterwards, please refer to the attached Figure 7 The first spacer material layer 71 located on the top surface of the first mandrel structure 35 and the top surface of the first mask layer 30 exposed between the adjacent first mandrel structures 35 is removed, and the first spacer material layer 71 remaining on the side of the first mandrel structure 35 forms a first spacer 70. The adjacent first spacers 70 form a first trench 72.

[0122] Afterwards, please refer to the attached Figure 8 A first sacrificial material layer 81 is formed by a deposition process. The first sacrificial material layer 81 fills the first trench 72 and covers the top surfaces of the first mandrel structure 35 and the first sidewall 70 .

[0123] Please refer to the attached Fig. 9, remove part of the first sacrificial material layer 81, and retain the first sacrificial material layer 81 in the first groove to form a first sacrificial layer 80; the top surface of the first sacrificial layer 80 is flush with the top surface of the first sidewall 70. In this step, the first sacrificial material layer 81 can be etched back by an etching process, or the first sacrificial material layer 81 can be removed by a chemical mechanical polishing process (CMP).

[0124] Step S300: removing the first sacrificial layer and the first mandrel structure, and retaining a plurality of first sidewalls.

[0125] In this embodiment, under the same etching conditions, the etching rate of the first sacrificial layer 80 is substantially the same as the etching rate of the first core shaft structure 35, so as to ensure that the first sacrificial layer 80 and the first core shaft structure 35 can be etched synchronously, avoid over-etching of the fourth hard mask layer 34 located below the first sacrificial layer 80 and the first core shaft structure 35, and ensure that the depth of the first groove 72 formed between adjacent first side walls 70 is the same.

[0126] It should be noted that, in this embodiment, the same etching conditions can be understood as the same etching solution (etching gas) and the same etching temperature, etc. The etching rates are substantially the same, which can be understood as: the etching rate of the first sacrificial layer 80 is strictly the same as the etching rate of the first mandrel structure 35, or the etching rate of the first sacrificial layer 80 is roughly the same as the etching rate of the first mandrel structure 35. For example, the difference between the etching rate of the first sacrificial layer 80 and the etching rate of the first mandrel structure 35 is within the process error, for example, the difference between the two is less than or equal to 5%.

[0127] For example, please refer to the attached Fig.10 , the second hard mask layer 352 and a portion of the thickness of the first sacrificial layer 80 are removed, and the top surface of the remaining first sacrificial layer 80 is lower than the top surface of the first hard mask layer 351 .

[0128] Afterwards, please refer to the attached Fig.11 , the parameters of the etching process can be readjusted, and the first hard mask layer 351 and the remaining first sacrificial layer 80 can be removed. The etching time used to finally etch the first hard mask layer 351 is substantially the same as the etching time used to etch the remaining first sacrificial layer 80, thereby ensuring that the heights of the remaining first sidewalls 70 are equal, that is, the depths of the first trenches 72 formed between adjacent first sidewalls 70 are also the same.

[0129] Step S400: forming a second mask layer, wherein the second mask layer completely fills the area enclosed by the first sidewall spacer and is located on the top surface of the first sidewall spacer.

[0130] Please refer to the attached Fig.12 and attached Fig.13, a fifth hard mask layer 91 is formed, and the fifth hard mask layer 91 fills the area surrounded by the first spacer 70 .

[0131] Exemplarily, a fifth hard mask material layer 95 is formed on the fourth hard mask layer 34, and the fifth hard mask material layer 95 fills the area surrounded by the first spacer 70, that is, the fifth hard mask material layer 95 fills the first trench and covers the top surface of the first spacer 70. In other words, the top surface of the fifth hard mask material layer 95 is higher than the top surface of the first spacer 70; then, the fifth hard mask material layer 95 is etched back, and the fifth hard mask material layer 95 located in the first trench is retained to form the fifth hard mask layer 91.

[0132] Afterwards, please refer to the attached Fig.14 , a sixth hard mask layer 92 , a seventh hard mask material layer 93 and an eighth hard mask material layer 94 which are stacked in sequence are formed on the fifth hard mask layer 91 ; the fifth hard mask layer 91 , the sixth hard mask layer 92 , the seventh hard mask material layer 93 and the eighth hard mask material layer 94 constitute a second mask layer 90 .

[0133] The fifth hard mask layer 91 and the seventh hard mask material layer 93 are made of the same material, both comprising a spin on hard mask (SOH) material. The sixth hard mask layer 92 and the eighth hard mask material layer 94 are made of the same material, both comprising silicon oxynitride.

[0134] Step S500: patterning the second mask layer to form a plurality of second mandrel structures spaced apart along a second direction in the second mask layer, wherein each second mandrel structure extends along the first direction.

[0135] For example, please refer to the attached Fig.14 A second anti-reflection layer 100 and a second photoresist layer 110 are stacked and formed on the eighth hard mask material layer 94 .

[0136] Thereafter, the second photoresist layer 110 is patterned to form a plurality of second openings 111 arranged at intervals along the second direction, and each second opening 111 extends along the first direction.

[0137] Afterwards, please refer to the attached Fig.15 , using the patterned second photoresist layer 110 as a mask, the second anti-reflective layer 100, the eighth hard mask material layer 94, and the seventh hard mask material layer 93 exposed in the second opening 111 are removed. The retained seventh hard mask material layer 93 constitutes the seventh hard mask layer 961, the retained eighth hard mask material layer 94 constitutes the eighth hard mask layer 962, the seventh hard mask layer 961 and the eighth hard mask layer 962 constitute the second mandrel structure 96; the eighth hard mask layer 962 is disposed on the seventh hard mask layer 961.

[0138] Please continue to refer to the attached Fig.15 , and use etching gas or etching liquid to remove the second photoresist layer 110 and the remaining second anti-reflection layer 100. In this embodiment, the material of the second anti-reflection layer 100 may include nitride. For example, the material of the second anti-reflection layer 100 includes silicon nitride or silicon oxynitride, but is not limited thereto. The second anti-reflection layer 100 can alleviate or eliminate the standing wave effect of the second photoresist layer 110, thereby increasing the accuracy of the mask pattern transferred from the mask to the second photoresist layer 110, thereby improving the accuracy of the pattern transfer process.

[0139] Step S600: forming a second sidewall spacer on the side of the second mandrel structure, and forming a second sacrificial layer filling the area surrounded by the second sidewall spacer;

[0140] Please refer to the attached Fig.16 A second spacer material layer 121 is formed by an atomic layer deposition process, and the second spacer material layer 121 covers the side and top surfaces of the second core shaft structure 96, and covers the top surface of the second mask layer 90 exposed between adjacent second core shaft structures 96; that is, the second spacer material layer 121 covers the top surface of the sixth hard mask layer 92 exposed between adjacent second core shaft structures 96.

[0141] Please refer to the attached Fig.17 , using etching gas or etching liquid, remove the second spacer material layer 121 located on the top surface of the second mandrel structure 96 and the top surface of the second mask layer 90 exposed between the adjacent second mandrel structures 96, and the second spacer material layer 121 remaining on the side of the second mandrel structure 96 forms the second spacer 120. Wherein, the second trench 122 is formed between the adjacent second spacers 120.

[0142] Please refer to the attached Fig.18 A second sacrificial material layer 131 is formed by a deposition process. The second sacrificial material layer 131 fills the second trench 122 and covers the top surface of the second mandrel structure 96 and the second sidewall 120 .

[0143] Please refer to the attached Fig.19 , an etching process or a chemical mechanical polishing process (CMP) is used to remove a portion of the thickness of the second sacrificial material layer 131, and the second sacrificial material layer 131 remaining in the second groove 122 constitutes a second sacrificial layer 130; the top surface of the second sacrificial layer 130 is flush with the top surface of the second sidewall 120.

[0144] Step S700: removing the second sacrificial layer and the second mandrel structure, and retaining a plurality of second sidewalls.

[0145] In this embodiment, under the same etching conditions, the etching rate of the second sacrificial layer 130 is substantially the same as the etching rate of the second core shaft structure 96, so as to ensure that the second sacrificial layer 130 and the second core shaft structure 96 can be etched synchronously, avoiding over-etching of the sixth hard mask layer 92 located below the second sacrificial layer 130 and the second core shaft structure 96, ensuring that the depth of the second groove 122 formed between adjacent second side walls 120 is the same, avoiding the formation of height differences among multiple second side walls 120.

[0146] It should be noted that, in this embodiment, the same etching conditions can be understood as the same etching solution (etching gas) and the same etching concentration. The etching rates are substantially the same, which can be understood as: the etching rate of the second sacrificial layer 130 is strictly the same as the etching rate of the second mandrel structure 96, or the etching rate of the second sacrificial layer 130 is roughly the same as the etching rate of the second mandrel structure 96. For example, the difference between the etching rate of the second sacrificial layer 130 and the etching rate of the second mandrel structure 96 is within the process error, for example, the difference between the two is less than or equal to 5%.

[0147] For example, please refer to the attached Fig. 20 The eighth hard mask layer 962 and a portion of the second sacrificial layer 130 are removed by an etching process, so that the top surface of the remaining second sacrificial layer 130 is lower than the top surface of the seventh hard mask layer 961 .

[0148] Afterwards, please refer to the attached Fig.21 , the parameters of the etching process can be readjusted, and the seventh hard mask layer 961 and the remaining second sacrificial layer 130 can be removed. The etching time used for etching the seventh hard mask layer 961 is substantially the same as the etching time used for etching the remaining second sacrificial layer 130, thereby ensuring that the heights of the remaining second sidewalls 120 are equal, that is, the depths of the second trenches 122 formed between adjacent second sidewalls 120 are also the same, thereby avoiding the phenomenon of the second sidewalls 120 being uneven.

[0149] Please refer to the attached Fig. 22 , a plurality of first side walls 70 are arranged at intervals along a first direction M, and each first side wall 70 extends along a second direction N, wherein the first direction M and the second direction N intersect, and in one example, the angle between the first direction M and the second direction N is an acute angle. In another example, the first direction M and the second direction N are perpendicular to each other.

[0150] The plurality of second sidewalls 120 are arranged at intervals along the second direction N, and each second sidewall 120 extends along the first direction M. Two adjacent first sidewalls 70 and two adjacent second sidewalls 120 define the location of the capacitor hole 13. Figure 3 To Attachment Fig.21 Can be attached Fig. 22The cross-sectional view along the S direction in FIG. 1 , correspondingly, both the first side walls 70 arranged at intervals and the second side walls 120 arranged at intervals can be seen in the cross-sectional view.

[0151] Step S800: using the first sidewall spacer and the second sidewall spacer as masks, etching the layer to be etched to form a capacitor hole in the layer to be etched.

[0152] Please refer to the attached Fig.23 and attached Fig.24 The first sidewall 70 and the second sidewall 120 are used as masks, and an etching process, such as dry etching or wet etching, is used to etch the layer 100 to form a capacitor hole 13 in the layer 100. Fig. 22 It can be seen from the figure that the depths of the capacitor holes 13 are consistent.

[0153] From the attached Figure 2 and attached Fig.23 Compared with the shape and position of the capacitor hole 13 shown in the figure, by forming a first sacrificial layer 80 in the area surrounded by the first side wall 70, the first mask layer 30 exposed between the first side walls 70 is protected. In this way, when the first mandrel structure 35 is removed, the first sacrificial layer 80 will be removed simultaneously to prevent the first mask layer 30 exposed between the first side walls 70 from being etched, so that the height of the retained first side walls is consistent. Accordingly, forming a second sacrificial layer 130 in the area surrounded by the second side wall 120 can ensure that the height of the retained second side wall 120 is consistent. Finally, using the first side wall 70 and the second side wall 120 as masks, when etching the layer 10 to be etched, it can be ensured that the size of the capacitor holes 13 formed is uniform, and the distance between adjacent capacitor holes 13 is equal, avoiding the position displacement of the capacitor holes 13, and improving the yield of the formed capacitor structure.

[0154] The various embodiments or implementation methods in this specification are described in a progressive manner. Each embodiment focuses on the differences from other embodiments, and the same or similar parts between the various embodiments can be referenced to each other.

[0155] In the description of this specification, the description with reference to terms such as "one embodiment", "some embodiments", "illustrative embodiment", "example", "specific example", or "some examples" means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present disclosure.

[0156] In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner.

[0157] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present disclosure, rather than to limit them. Although the present disclosure has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein by equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present disclosure.

Claims

1. A method for preparing a semiconductor structure, characterized in that: The steps include: Forming a first mask layer on the layer to be etched, and patterning the first mask layer to form a plurality of first mandrel structures spaced apart along a first direction in the first mask layer, each of the first mandrel structures extending along a second direction, and the second direction intersecting the first direction; forming a first sidewall on a side of the first mandrel structure, and forming a first sacrificial layer filling an area surrounded by the first sidewall; removing the first sacrificial layer and the first mandrel structure, and retaining the first plurality of sidewall spacers; forming a second mask layer, wherein the second mask layer completely fills the area surrounded by the first sidewalls and is located on the top surface of the first sidewalls; Patterning the second mask layer to form a plurality of second mandrel structures spaced apart along the second direction in the second mask layer, each of the second mandrel structures extending along the first direction; forming a second sidewall on a side of the second mandrel structure, and forming a second sacrificial layer filling an area surrounded by the second sidewall; removing the second sacrificial layer and the second mandrel structure, and retaining a plurality of the second sidewalls; The layer to be etched is etched using the first sidewall and the second sidewall as masks to form a capacitor hole in the layer to be etched.

2. The method for preparing a semiconductor structure according to claim 1, characterized in that: Under the same etching conditions, the etching rate of the first sacrificial layer is substantially the same as the etching rate of the first mandrel structure; Under the same etching conditions, the etching rate of the second sacrificial layer is substantially the same as the etching rate of the second mandrel structure.

3. The method for preparing a semiconductor structure according to claim 1, characterized in that: Adjacent first side walls form first grooves, and the depths of the first grooves are the same; Adjacent second sidewalls form second grooves, and a plurality of second grooves have the same depth.

4. The method for preparing a semiconductor structure according to claim 1, characterized in that: The first core shaft structure includes a first hard mask layer and a second hard mask layer, the second hard mask layer is arranged on the first hard mask layer, the thickness of the second hard mask layer is less than or equal to 1 / 4 of the thickness of the first hard mask layer, the material of the first sacrificial layer is the same as the material of the first hard mask layer, and the top surface of the first sacrificial layer is flush with the top surface of the first hard mask layer.

5. The method for preparing a semiconductor structure according to claim 4, characterized in that: The step of removing the first sacrificial layer and the first mandrel structure comprises: removing the second hard mask layer and a portion of the thickness of the first sacrificial layer, wherein a top surface of the remaining first sacrificial layer is lower than a top surface of the first hard mask layer; The first hard mask layer and remaining first sacrificial layer are removed.

6. The method for preparing a semiconductor structure according to claim 3, characterized in that: The step of forming the first sidewall spacer comprises: forming a first spacer material layer, wherein the first spacer material layer covers the side surfaces and the top surface of the first mandrel structure, and covers the top surface of the first mask layer exposed between adjacent first mandrel structures; The first sidewall material layer located on the top surface of the first core shaft structure and the top surface of the first mask layer exposed between adjacent first core shaft structures is removed, and the first sidewall material layer retained on the side surface of the first core shaft structure constitutes the first sidewall; the first groove is surrounded by adjacent first sidewalls.

7. The method for preparing a semiconductor structure according to claim 6, characterized in that: The step of forming the first sacrificial layer filling the area surrounded by the first sidewalls comprises: forming a first sacrificial material layer, wherein the first sacrificial material layer completely fills the first trench and covers the top surface of the first mandrel structure and the first sidewall; A portion of the first sacrificial material layer is removed, and the first sacrificial material layer retained in the first groove forms a first sacrificial layer; the top surface of the first sacrificial layer is flush with the top surface of the first sidewall.

8. The method for preparing a semiconductor structure according to claim 4, characterized in that: The steps of forming a first mask layer on the layer to be etched and patterning the first mask layer include: forming a third hard mask layer, a fourth hard mask layer, a first hard mask material layer and a second hard mask material layer which are sequentially stacked on the layer to be etched; The second hard mask material layer and the first hard mask material layer are patterned to form a plurality of first core shaft structures; each of the first core shaft structures comprises a first hard mask layer and a second hard mask layer stacked together; wherein the retained first hard mask material layer constitutes a first hard mask layer, and the retained second hard mask material layer constitutes a second hard mask layer.

9. The method for preparing a semiconductor structure according to claim 8, characterized in that: The step of forming a plurality of the first mandrel structures comprises: forming a first anti-reflection layer and a first photoresist layer stacked in sequence on the second hard mask material layer; Patterning the first photoresist layer to form a plurality of first openings spaced apart along the first direction, each of the first openings extending along the second direction; Using the patterned first photoresist layer as a mask, removing the first anti-reflection layer, the second hard mask material layer, and the first hard mask material layer exposed in the first opening; The first photoresist layer and the remaining first anti-reflection layer are removed.

10. The method for preparing a semiconductor structure according to any one of claims 1 to 9, characterized in that: The step of forming the second mask layer comprises: forming a fifth hard mask layer, wherein the fifth hard mask layer completely fills the area surrounded by the first sidewall spacer; A sixth hard mask layer, a seventh hard mask material layer and an eighth hard mask material layer are sequentially stacked on the fifth hard mask layer; the fifth hard mask layer, the sixth hard mask layer, the seventh hard mask material layer and the eighth hard mask material layer constitute the second mask layer.

11. The method for preparing a semiconductor structure according to claim 10, characterized in that: The step of patterning the second mask layer to form the second mandrel structure includes: forming a second anti-reflection layer and a second photoresist layer stacked in sequence on the eighth hard mask material layer; Patterning the second photoresist layer to form a plurality of second openings spaced apart along the second direction, each of the second openings extending along the first direction; Using the patterned second photoresist layer as a mask, removing the second anti-reflective layer, the eighth hard mask material layer and the seventh hard mask material layer exposed in the second opening, the remaining seventh hard mask material layer constitutes a seventh hard mask layer, the remaining eighth hard mask material layer constitutes an eighth hard mask layer, and the seventh hard mask layer and the eighth hard mask layer constitute the second mandrel structure; The second photoresist layer and the remaining second anti-reflection layer are removed.

12. The method for preparing a semiconductor structure according to claim 11, characterized in that: The step of forming the second sidewall includes: forming a second spacer material layer, wherein the second spacer material layer covers the side surfaces and the top surface of the second mandrel structure, and covers the top surface of the second mask layer exposed between adjacent second mandrel structures; The second sidewall material layer located on the top surface of the second mandrel structure and the top surface of the second mask layer exposed between adjacent second mandrel structures is removed, and the second sidewall material layer retained on the side of the second mandrel structure constitutes a second sidewall; and a second groove is formed between adjacent second sidewalls.

13. The method for preparing a semiconductor structure according to claim 12, characterized in that: The step of forming the second sacrificial layer comprises: forming a second sacrificial material layer, wherein the second sacrificial material layer completely fills the second trench and covers the top surface of the second mandrel structure and the second sidewall; A portion of the thickness of the second sacrificial material layer is removed, and the second sacrificial material layer remaining in the second groove constitutes a second sacrificial layer; the top surface of the second sacrificial layer is flush with the top surface of the second sidewall.

Citation Information

Patent Citations

  • Multi-patterning method

    CN112017950A

  • Mask structure and forming method thereof, and memory and forming method thereof

    CN112133625A

  • Mask structure, semiconductor structure and preparation method of mask structure

    CN113097141A

  • Metal interconnection structure and preparation method thereof, peripheral circuit, memory and system thereof

    CN113838800A

  • Method for regulating hardmask over-etch for multi-patterning processes

    TW201830517A