Display panel and preparation method thereof

By setting up an isolation structure of conductive material in the display panel, cathode control is realized, which solves the problem of high power consumption of the display panel and improves energy efficiency and display effect.

CN118946201APending Publication Date: 2024-11-12KUNSHAN GO VISIONOX OPTO ELECTRONICS CO LTD
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202310531360.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-11
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The existing display panels consume high power, resulting in poor energy efficiency.

Method used

By providing an isolation structure in the display panel, it includes a first isolation portion and a second isolation portion, the first isolation portion is a conductive material, and the second isolation portion is in the positive projection of the substrate, and the first electrode is electrically connected to the first isolation portion, Achieve cathode control and reduce power consumption.

Benefits of technology

It effectively reduces the power consumption of the display panel, improves energy efficiency, and avoids crosstalk between sub-pixels through the isolation structure, improving the display effect and product yield.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118946201A_ABST
    Figure CN118946201A_ABST
Patent Text Reader

Abstract

The invention discloses a display panel and a preparation method of the display panel. The display panel comprises a substrate, an isolation structure, a light emitting structure and a first electrode. The isolation structure comprises a first isolation part and a second isolation part which are sequentially arranged in the direction away from the substrate, the first isolation part comprises a conductive material, and the orthographic projection of the second isolation part on the substrate is located in the orthographic projection of the first isolation part on the substrate; the adjacent light-emitting structures are separated by the isolation structures; the first electrode is arranged on the side, away from the substrate, of the light-emitting structure and electrically connected with the first isolation part, and power consumption is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application belongs to the field of display technology, and in particular, relates to a display panel and a method for preparing the display panel. Background Art

[0002] Flat display panels such as Liquid Crystal Display (LCD) panels, Organic Light Emitting Display (OLED) panels and display panels using Light Emitting Diode (LED) devices are widely used in various consumer electronic products such as mobile phones, televisions, personal digital assistants, digital cameras, laptops, desktop computers, etc. due to their advantages such as high image quality, power saving, thin body and wide application range, becoming the mainstream in display devices.

[0003] Currently, display panels have the problem of high power consumption. Summary of the invention

[0004] The purpose of the present application is to provide a display panel and a method for manufacturing the display panel, which can reduce the power consumption of the display panel.

[0005] In a first aspect, the present application provides a display panel, comprising a substrate, an isolation structure, a light-emitting structure and a first electrode. The isolation structure comprises a first isolation portion and a second isolation portion sequentially arranged on a pixel defining portion in a direction away from the substrate, the first isolation portion comprises a conductive material, and the orthographic projection of the second isolation portion on the substrate is located within the orthographic projection of the first isolation portion on the substrate; adjacent light-emitting structures are separated by means of the isolation structure; the first electrode is arranged on a side of the light-emitting structure away from the substrate, and the first electrode is electrically connected to the first isolation portion.

[0006] In some embodiments, the display panel further includes a third isolation portion, the third isolation portion is disposed on a side of the second isolation portion away from the substrate, and an orthographic projection of the second isolation portion on the substrate is located within an orthographic projection of the third isolation portion on the substrate;

[0007] Preferably, the orthographic projection of the first isolation portion on the substrate is located within the orthographic projection of the third isolation portion on the substrate;

[0008] Preferably, an orthographic projection of the first isolation portion on the substrate at least partially overlaps an orthographic projection of the first electrode on the substrate;

[0009] Preferably, an orthographic projection of the second isolation portion on the substrate does not overlap with an orthographic projection of the first electrode on the substrate.

[0010] In some embodiments, the display panel further includes a pixel definition layer disposed on the substrate, the pixel definition layer includes a pixel defining portion and a pixel opening defined by the pixel defining portion, the light emitting structure is located in the pixel opening, and the isolation structure is disposed on the pixel defining portion.

[0011] In some embodiments, the length L1 of the edge of the third isolation portion extending relative to the edge of the first isolation portion satisfies the following condition: 1 μm≤L1≤5 μm;

[0012] Preferably, L1 satisfies the following conditions: 2 μm ≤ L1 ≤ 4 μm;

[0013] Preferably, the extension length L2 of the edge of the first isolation portion relative to the edge of the second isolation portion satisfies the following condition: 0.5 μm≤L2≤4 μm;

[0014] Preferably, the material of the first isolation portion is metal;

[0015] Preferably, the material of the first isolation portion includes at least one of molybdenum, molybdenum alloy, aluminum, aluminum alloy, copper and copper alloy;

[0016] Preferably, the thickness H1 of the first isolation portion along a direction perpendicular to the substrate satisfies the following condition:

[0017]

[0018] Preferably, the thickness H1 of the first isolation portion along a direction perpendicular to the substrate satisfies the following condition:

[0019]

[0020] In some embodiments, the material of the second isolation portion is an organic insulating material;

[0021] Preferably, the side wall surface of the second isolation portion is an arc-shaped surface that is concave in a direction away from the first electrode;

[0022] Preferably, the material of the third isolation portion is an inorganic insulating material;

[0023] Preferably, the material of the second isolation portion is the same as that of the pixel definition layer;

[0024] Preferably, the material of the second isolation portion is a black light-shielding material;

[0025] Preferably, a thickness H2 of the second isolation portion along a direction perpendicular to the substrate satisfies the following condition: 0.5 μm≤H2≤3 μm.

[0026] In some embodiments, a surface of one side of the first isolation portion contacting the second isolation portion is a plane.

[0027] In some embodiments, a groove is formed on a side of the first isolation portion facing away from the substrate, and an end of the second isolation portion facing the substrate is accommodated in the groove.

[0028] In some embodiments, the light emitting structure includes a hole injection layer and an organic functional layer sequentially disposed in a direction away from the substrate;

[0029] Preferably, the orthographic projection of the hole injection layer on the substrate is located within the orthographic projection of the organic functional layer on the substrate, and the orthographic projection of the organic functional layer on the substrate is located within the orthographic projection of the first electrode on the substrate;

[0030] Preferably, the organic functional layer comprises a hole transport layer, an organic light emitting layer, an electron transport layer and an electron injection layer which are sequentially stacked in a direction away from the substrate;

[0031] Preferably, the orthographic projections of the hole transport layer, the organic light emitting layer, the electron transport layer and the electron injection layer on the substrate overlap with each other.

[0032] In some embodiments, the display panel further includes an encapsulation layer, which is disposed on a side of the first electrode facing away from the substrate;

[0033] Preferably, the encapsulation layer comprises a first inorganic encapsulation sublayer and an organic encapsulation sublayer stacked in sequence, and the first inorganic encapsulation sublayer is arranged on a side of the first electrode away from the substrate;

[0034] Preferably, the material of the third isolation portion is the same as the material of the first inorganic encapsulation sublayer;

[0035] Preferably, the first inorganic encapsulation sublayer and the organic encapsulation sublayer are embedded in the isolation structure;

[0036] Preferably, the encapsulation layer further comprises a second inorganic encapsulation sublayer arranged on a side of the organic encapsulation sublayer facing away from the substrate, and the second inorganic encapsulation sublayer covers the third isolation portion.

[0037] In a second aspect, an embodiment of the present application provides a method for preparing a display panel, comprising the following steps:

[0038] Forming a pixel definition layer on one side of the substrate, the pixel definition layer comprising a pixel definition portion and a pixel opening surrounded by the pixel definition portion;

[0039] An isolation structure is formed by a photolithography process on a side of the pixel definition layer away from the substrate, wherein the isolation structure comprises a first isolation portion and a second isolation portion sequentially arranged on the pixel definition portion in a direction away from the substrate, the first isolation portion comprises a conductive material, and an orthographic projection of the second isolation portion on the substrate is located within an orthographic projection of the first isolation portion on the substrate;

[0040] Forming a light-emitting structure by evaporation in the pixel opening;

[0041] A first electrode is formed on a side of the light emitting structure facing away from the substrate, and the first electrode is electrically connected to the first isolation portion.

[0042] The embodiments of the present application provide a display panel, a display device, and a method for manufacturing a display panel. By setting the isolation structure such that the orthographic projection of the second isolation portion on the substrate is located within the orthographic projection of the first isolation portion on the substrate, that is, the width of the first isolation portion parallel to the substrate is greater than the width of the second isolation portion parallel to the substrate, and the first isolation portion includes a conductive material, and the first isolation portion is electrically connected to the first electrode, cathode control can be achieved, thereby reducing power consumption. BRIEF DESCRIPTION OF THE DRAWINGS

[0043] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the drawings required for use in the embodiments of the present application will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0044] Figure 1 A schematic cross-sectional view of a display panel provided in some embodiments of the present application;

[0045] Figure 2 for Figure 1 A partial schematic diagram of

[0046] Figure 3 A schematic cross-sectional view of an isolation structure provided in some embodiments of the present application;

[0047] Figure 4 A schematic cross-sectional view of a display panel provided in some other embodiments of the present application;

[0048] Figure 5 A schematic cross-sectional view of a display panel provided in some other embodiments of the present application;

[0049] Figure 6 A flow chart of a method for preparing a display panel provided in some embodiments of the present application;

[0050] Figures 7 to 10 is a schematic diagram of the process structure of a method for preparing a display panel provided in some embodiments of the present application;

[0051] Fig.11 It is a schematic diagram of the process structure of a method for preparing a display panel provided in some other embodiments of the present application.

[0052] The figures are as follows:

[0053] Display panel 100; substrate 10; pixel definition layer 20; pixel defining portion 21; pixel opening 22; isolation structure 30; first isolation portion 31; groove 31a; second isolation portion 32; side wall surface 32a; third isolation portion 33; light-emitting structure 40; hole injection layer 41; organic functional layer 42; hole transport layer 421; organic light-emitting layer 422; electron transport layer 423; electron injection layer 424; first electrode E1; second electrode E2; encapsulation layer 50; first inorganic encapsulation sublayer 51; organic encapsulation sublayer 52; second inorganic encapsulation sublayer 53. DETAILED DESCRIPTION

[0054] The following detailed description and drawings of the embodiments of the present application are used to illustrate the principles of the present application, but cannot be used to limit the scope of the present application, that is, the present application is not limited to the described embodiments.

[0055] In the description of the present application, it should be noted that, unless otherwise specified, "multiple" means more than two; the terms "upper", "lower", "left", "right", "inside", "outside", etc., indicating the orientation or positional relationship, are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present application. In addition, the terms "first", "second", "third", etc. are only used for descriptive purposes and cannot be understood as indicating or implying relative importance. "Vertical" is not strictly vertical, but is within the allowable error range. "Parallel" is not strictly parallel, but is within the allowable error range.

[0056] Reference to "embodiments" in this application means that a particular feature, structure, or characteristic described in conjunction with the embodiments may be included in at least one embodiment of the present application. The appearance of the phrase in various locations in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It is explicitly and implicitly understood by those skilled in the art that the embodiments described in this application may be combined with other embodiments.

[0057] The directional words appearing in the following description are all directions shown in the figures, and do not limit the specific structure of this application. In the description of this application, it should also be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be directly connected or indirectly connected through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to the specific circumstances.

[0058] An embodiment of the present application provides a display panel, which may be an organic light emitting diode (OLED) display panel, or other types of display panels, such as a micro light emitting diode (Micro Light Emitting Diode, Micro-LED) or a quantum dot light emitting diode (Quantum Light Emitting Diode, QLED) display panel.

[0059] For the above questions, please refer to Figure 1 and Figure 2 In a first aspect, the present application provides a display panel 100 , including a substrate 10 , a pixel definition layer 20 , an isolation structure 30 , a light emitting structure 40 , and a first electrode E1 .

[0060] Among them, the substrate 10 includes a substrate and an array layer arranged on the substrate. The substrate can be a hard substrate made of materials such as glass or plastic, or a flexible substrate made of materials such as polyethersulfone (PES), polyacrylate (PAR), polyetherimide (PEI), polyethylene naphthalate (PEN), polyethylene terephthalate (PET), polyphenylene sulfide (PPS), polyarylate, polyimide (PI), polycarbonate (PC) or cellulose acetate propionate (CAP). A driving circuit for controlling the light-emitting structure 40 to emit light is arranged in the array layer. The array layer is generally composed of inorganic film layers such as a metal layer, a semiconductor layer (active layer), and an insulating layer. By patterning these inorganic film layers, a driving circuit for controlling the light-emitting structure 40 to emit light can be formed. There are many implementation methods for its specific circuit structure, which will not be repeated here.

[0061] The light emitting structure 40 may be formed by stacking a plurality of film layer structures. For example, the light emitting structure 40 may include a stacked hole injection layer 41 (Hole Inject Layer, HIL), a hole transport layer 421 (Hole Transport Layer, HTL), a light emitting layer, an electron injection layer 424 (Electron Inject Layer, EIL) and an electron transport layer 423 (Electron Transport Layer, ETL). Figure 1 The light emitting structure 40 in FIG. 1 only illustrates the light emitting layer.

[0062] The isolation structure 30 includes a first isolation portion 31 and a second isolation portion 32 sequentially arranged in a direction away from the substrate 10 . The first isolation portion 31 includes a conductive material. The first electrode E1 is arranged on a side of the light emitting structure 40 away from the substrate 10 . The first electrode E1 is electrically connected to the first isolation portion 31 .

[0063] The display panel 100 may further include a second electrode E2, the second electrode E2, the light emitting structure 40 and the first electrode E1 are sequentially arranged in a direction away from the substrate 10, and the second electrode E2, the light emitting structure 40 and the first electrode E1 are sequentially stacked to form a sub-pixel. After the first electrode E1 and the second electrode E2 are energized, the second electrode E2 serves as an anode and the first electrode E1 serves as a cathode. The first electrode E1 is located on a side of the light emitting structure 40 away from the substrate 10, and the first electrode E1 and the second electrode E2 jointly drive the light emitting structure 40 to emit light.

[0064] The orthographic projection of the second isolation portion 32 on the substrate 10 is located within the orthographic projection of the first isolation portion 31 on the substrate 10. That is to say, the width of the first isolation portion 31 parallel to the substrate 10 is greater than the width of the second isolation portion 32 parallel to the substrate 10, and the edge of the first isolation portion 31 is protruding and extending relative to the edge of the second isolation portion 32, so that the first isolation portion 31 and the first electrode E1 are more easily overlapped, so that during the preparation process of the display panel 100, the evaporation of the first electrode E1 does not need to be restricted by the limitation of the evaporation angle. Moreover, even when preparing sub-pixels of different colors, since the light-emitting structure 40 needs to be etched multiple times, causing part of the second isolation portion 32 to be etched, it will not affect the electrical connection between the first isolation portion 31 and the first electrode E1, thereby improving the performance and product yield of the display panel 100.

[0065] Among them, the second isolation portion 32 can be a structure that is wide at the top and narrow at the bottom, or a structure that has side walls that are concave inward, so that when the light-emitting structure 40 and the first electrode E1 are evaporated, the material of the light-emitting structure 40 and the first electrode E1 will not be deposited on the side wall surface of the second isolation portion 32, thereby isolating adjacent sub-pixels.

[0066] Adjacent light-emitting structures 40 are separated by means of the isolation structure 30. The existence of the isolation structure 30 can separate different light-emitting structures 40 during the preparation process of the display panel 100. Specifically, during the preparation process of the display panel 100, the isolation structure 30 is usually formed first, and then the light-emitting structure 40 is directly evaporated without the help of a mask plate. In this process, due to the existence of the isolation structure 30, part of the light-emitting material will be evaporated in the pixel opening 22, and part of the light-emitting material will be evaporated on the side of the isolation structure 30 away from the substrate 10, so that the light-emitting materials on different sides of the isolation structure 30 in the direction parallel to the plane of the substrate 10 are discontinuous, and the light-emitting structures 40 are separated from each other without the need for an evaporation mask plate. Since the evaporation of the light-emitting structure 40 does not require a precision mask plate, the cost is reduced, and the shadow effect of the light-emitting layer evaporated by the precision mask plate is avoided, and the spacing between sub-pixels can be reduced, thereby improving the brightness of the display panel 100. Furthermore, since the electron transport layer 423 , the electron injection layer 424 , the hole transport layer 421 , the hole injection layer 41 , etc. of the light emitting structure 40 are isolated by the isolation structure 30 , crosstalk between sub-pixels can be prevented, thereby improving the display effect of the display panel 100 .

[0067] It should be noted that, for the first electrode E1, part of the first electrode E1 is located in the pixel opening 22, and part of it is located on the side of the pixel defining portion 21 away from the substrate 10 and can overlap with the first isolation portion 31, so adjacent first electrodes E1 can be electrically connected to each other with the help of the first isolation portion 31.

[0068] To sum up, the adjacent first electrode E1 is isolated by the second isolation portion 32 of the isolation structure 30, and the width of the first isolation portion 31 parallel to the substrate 10 is greater than the width of the second isolation portion 32 parallel to the substrate 10, and the first isolation portion 31 includes a conductive material. The first electrode E1 can be connected to the Vss power line through the first isolation portion 31 to maintain the potential of the first electrode E1, thereby realizing cathode control and reducing power consumption.

[0069] In some embodiments, the display panel 100 further includes a pixel definition layer 20 disposed on the substrate 10, the pixel definition layer 20 includes a pixel defining portion 21 and a pixel opening 22 formed by the pixel defining portion 21, the light emitting structure 40 is located in the pixel opening 22, and the isolation structure 30 is disposed on the pixel defining portion 21. The plurality of light emitting structures 40 are disposed in one-to-one correspondence with the plurality of pixel openings 22, and the light emitting structure 40 is located in the pixel opening 22, so that interference between adjacent sub-pixels can be avoided.

[0070] In some embodiments, the display panel 100 further includes a third isolating portion 33, which is disposed on a side of the second isolating portion 32 away from the substrate, and an orthographic projection of the second isolating portion 32 on the substrate 10 is located within an orthographic projection of the third isolating portion 33 on the substrate. In other words, the width of the third isolating portion 33 along the direction parallel to the substrate 10 is greater than the width of the second isolating portion 32 along the direction parallel to the substrate 10. The third isolating portion 33 can serve as a mask for evaporating the light-emitting structure 40 and the first electrode E1, and can further isolate the light-emitting structure 40 of adjacent sub-pixels and the first electrode E1 of adjacent sub-pixels.

[0071] Preferably, the orthographic projection of the first isolating portion 31 on the substrate 10 is located within the orthographic projection of the third isolating portion 33 on the substrate 10. That is, the width of the third isolating portion 33 along the direction parallel to the substrate 10 is greater than the width of the first isolating portion 31 along the direction parallel to the substrate 10, and the edge of the third isolating portion 33 is arranged to protrude and extend relative to the edge of the first isolating portion 31, which can reduce the spacing between the light-emitting structures 40 and improve the pixel density.

[0072] In some embodiments, the orthographic projection of the first isolation portion 31 on the substrate 10 at least partially overlaps with the orthographic projection of the first electrode E1 on the substrate 10. That is, the edge of the first electrode E1 covers the edge of the first isolation portion 31, thereby increasing the overlap area between the first electrode E1 and the first isolation portion 31. Even when preparing sub-pixels of different colors, the light-emitting structure 40 needs to be etched multiple times, resulting in partial etching of the first electrode E1, which does not affect the electrical connection between the first isolation portion 31 and the first electrode E1, thereby improving the performance and product yield of the display panel 100.

[0073] In some embodiments, the orthographic projection of the second isolation portion 32 on the substrate 10 does not overlap with the orthographic projection of the first electrode E1 on the substrate 10. That is, there is a gap between the second isolation portion 32 and the first electrode E1, and the two are not overlapped, which can prevent crosstalk between sub-pixels.

[0074] In some embodiments, the length L1 of the edge of the third isolation portion 33 extending relative to the edge of the first isolation portion 31 satisfies the following condition: 1 μm≤L1≤5 μm.

[0075] If the length L1 of the edge of the third isolation portion 33 extending relative to the edge of the first isolation portion 31 is too short, the isolation effect between the sub-pixels cannot be guaranteed; if the length L1 of the edge of the third isolation portion 33 extending relative to the edge of the first isolation portion 31 is too long, the overlap between the first electrode E1 and the first isolation portion 31 cannot be guaranteed. The value range of L1 in this embodiment is reasonable, which can isolate the sub-pixels and achieve the overlap between the first electrode E1 and the first isolation portion 31.

[0076] Preferably, L1 satisfies the following condition: 2 μm≤L1≤4 μm, which can better isolate each sub-pixel and further improve the overlapping effect between the first electrode E1 and the first isolation portion 31 .

[0077] In some embodiments, the protruding length L2 of the edge of the first isolation portion 31 relative to the edge of the second isolation portion 32 satisfies the following condition: 0.5 μm≤L2≤4 μm.

[0078] If the length L2 of the edge of the first isolation portion 31 extending relative to the edge of the second isolation portion 32 is too short, the overlap between the first electrode E1 and the first isolation portion 31 cannot be ensured; if the length L2 of the edge of the first isolation portion 31 extending relative to the edge of the second isolation portion 32 is too long, the light emitting structure 40 may be covered, affecting the setting of the light emitting structure 40. The value range of this embodiment is reasonable, which can ensure the overlap effect between the first electrode E1 and the first isolation portion 31 without affecting the setting of the light emitting structure 40.

[0079] In some embodiments, the first isolation portion 31 is made of metal, which can ensure the conduction between the first isolation portion 31 and the first electrode E1 and connect the first electrode E1 to an external circuit. Moreover, the first isolation portion 31 is made of metal, which facilitates wet etching to form the first isolation portion 31 .

[0080] In some embodiments, the material of the first isolation portion 31 includes at least one of molybdenum, molybdenum alloy, aluminum, aluminum alloy, copper and copper alloy. The above metal materials are easy to etch and resistant to oxidation, are convenient for process preparation, and can improve the performance and product yield of the display panel 100.

[0081] Preferably, the material of the first isolation portion 31 is aluminum. First, aluminum has a lower density than other metal materials. Therefore, the use of aluminum to prepare the first isolation portion 31 can reduce the weight of the display panel 100 and facilitate transportation and installation. Secondly, aluminum has excellent corrosion resistance and is not easily oxidized or corroded. Therefore, the first isolation portion 31 can maintain stable performance even in harsh environments. Aluminum is also an excellent conductive material. The use of aluminum to prepare the first isolation portion 31 can play a good role in transmitting electrical energy and reducing power consumption. Furthermore, aluminum is easy to etch and process, and is a recyclable material that can be recycled to reduce production costs and environmental pollution.

[0082] In some embodiments, the thickness H1 of the first isolation portion 31 along a direction perpendicular to the substrate 10 satisfies the following conditions:

[0083] If the thickness H1 of the first isolation portion 31 along the direction perpendicular to the substrate 10 is too small, when preparing sub-pixels of different colors, the light-emitting structure 40 needs to be etched multiple times, which may cause part of the first isolation portion 31 to be etched, and the overlap effect between the first isolation portion 31 and the first electrode E1 cannot be guaranteed; if the thickness H1 of the first isolation portion 31 along the direction perpendicular to the substrate 10 is too large, the thickness of the isolation structure 30 is increased, resulting in a smaller light output angle of the light-emitting structure 40. The thickness H1 of the first isolation portion 31 along the direction perpendicular to the substrate 10 of this embodiment has a reasonable value range, which can ensure the overlap effect between the first electrode E1 and the first isolation portion 31, and does not affect the light output angle of the light-emitting structure 40.

[0084] Preferably, the first isolation portion 31 satisfies the following conditions along a thickness H1 perpendicular to the substrate 10: The overlapping effect between the first isolation portion 31 and the first electrode E1 can be further improved, thereby increasing the light emission viewing angle of the light emitting structure 40 .

[0085] In some embodiments, the material of the second isolation portion 32 is an organic insulating material, which can easily form a thicker second isolation portion 32 and facilitate the isolation of sub-pixels.

[0086] In some embodiments, the side wall surface 32a of the second isolation portion 32 is an arc surface that is concave in a direction away from the first electrode E1, so that the material of the continuous light-emitting structure 40 and the first electrode E1 will not be deposited on the side wall surface 32a of the second isolation portion 32, and the adjacent light-emitting structures 40 and the adjacent first electrodes E1 can be separated. Exemplarily, the material of the second isolation portion 32 is an organic insulating material, and the second isolation portion 32 can be formed by a dry etching process. The organic insulating layer is etched and shrinks, so the inner side wall of the second isolation portion 32 is concave inward to form an arc surface.

[0087] In some embodiments, the material of the third isolation portion 33 is an inorganic insulating material, and the third isolation portion 33 is formed by the inorganic insulating material, and the third isolation portion 33 can be used as a mask for evaporating the first electrode E1. When preparing the isolation structure 30, a metal layer, an organic insulating layer, and an inorganic insulating layer can be deposited in sequence on the side of the pixel defining portion 21 away from the substrate 10, and then after exposure and development, dry etching is performed first, and the inorganic insulating layer and the organic insulating layer are etched. Since the organic insulating layer is etched and shrinks, the inner side wall of the second isolation portion 32 is concave inward to form an arc surface. Finally, wet etching is used, and the metal layer is etched to obtain the first isolation portion 31, and the inorganic insulating layer is etched to obtain the third isolation portion 33.

[0088] In some embodiments, the material of the second isolation portion 32 is the same as that of the pixel definition layer 20. Exemplarily, the material of the second isolation portion 32 and the pixel definition layer 20 are both formed of photosensitive polyimide (PSPI), which is a type of organic material that has both imide rings and photosensitive genes on the polymer chain, and has excellent thermal stability, good mechanical properties, chemical and photosensitive properties. In this embodiment, the same organic insulating material is used to prepare the pixel definition layer 20 and the second isolation portion 32, which can facilitate process preparation, reduce costs, and improve production efficiency.

[0089] Preferably, the material of the second isolation portion 32 is a black light-shielding material, such as a black resin material such as polyurethane, epoxy resin, etc., which can prevent interference from external ambient light and reduce optical crosstalk between adjacent sub-pixels. In addition, the use of a black light-shielding material to prepare the second isolation portion 32 can also improve the contrast of the display panel 100.

[0090] Preferably, the thickness H2 of the second isolation portion 32 along the direction perpendicular to the substrate 10 satisfies the following condition: 0.5μm≤H2≤3μm. Since the second isolation portion 32 is formed of an organic insulating material, the thickness of the second isolation portion 32 is the largest in the isolation structure 30. If the thickness H2 of the second isolation portion 32 along the direction perpendicular to the substrate 10 is too small, the height of the isolation structure 30 cannot be guaranteed, and thus the first electrode E1 and the light-emitting structure 40 cannot be well isolated; if the thickness H2 of the second isolation portion 32 along the direction perpendicular to the substrate 10 is too large, the thickness of the isolation structure 30 is increased, resulting in a smaller light-emitting viewing angle of the light-emitting structure 40. The thickness H2 of the second isolation portion 32 along the direction perpendicular to the substrate 10 of this embodiment has a reasonable value range, which can ensure the effect of the isolation structure 30 isolating the first electrode E1 and the light-emitting structure 40, and does not affect the light-emitting viewing angle of the light-emitting structure 40.

[0091] In some embodiments, the surface of the first isolating portion 31 contacting the second isolating portion 32 is a plane. That is, the lower surface of the second isolating portion 32 and the upper surface of the first isolating portion 31 are both planes, and the second isolating portion 32 is formed on the upper surface of the first isolating portion 31.

[0092] like Figure 3As shown, in some embodiments, a groove 31a is formed on the side of the first isolation portion 31 facing away from the substrate 10, and the end of the second isolation portion 32 facing the substrate 10 is accommodated in the groove 31a. When preparing the isolation structure 30, after depositing the metal layer, the metal layer can be firstly wet-etched, or exposed and developed with a half-tone mask, to form a first isolation portion 31 with a groove 31a, and the groove 31a does not penetrate the first isolation portion 31, and then an organic insulating layer and an inorganic insulating layer are deposited, and the second isolation portion 32 and the third isolation portion 33 are obtained by dry etching. In this embodiment, since the end of the second isolation portion 32 is inserted into the groove 31a of the first isolation portion 31, the adhesion between the second isolation portion 32 and the third isolation portion 33 is enhanced, thereby improving the performance and product yield of the display panel 100.

[0093] like Figure 4 As shown, in some embodiments, the light emitting structure 40 includes a hole injection layer 41 and an organic functional layer 42 which are sequentially arranged in a direction away from the substrate 10; the hole injection layer 41 is arranged on the side of the second electrode E2 away from the substrate 10, and the organic functional layer 42 is arranged on the side of the hole injection layer 41 away from the substrate 10. Since the organic functional layer 42 needs holes and electrons to meet in order to emit light, the hole injection layer 41 can promote the injection of positive holes on the anode into the organic functional layer 42, and improve the contact between the anode and the organic functional layer 42, thereby reducing the contact resistance and improving the injection efficiency.

[0094] In some embodiments, the orthographic projection of the hole injection layer 41 on the substrate 10 is located within the orthographic projection of the organic functional layer 42 on the substrate 10, and the orthographic projection of the organic functional layer 42 on the substrate 10 is located within the orthographic projection of the first electrode E1 on the substrate 10. In other words, the orthographic projection areas of the hole injection layer 41, the organic functional layer 42 and the first electrode E1 on the substrate 10 are respectively gradually increasing, the edge of the organic functional layer 42 exceeds the edge of the hole injection layer 41, and the edge of the first electrode E1 exceeds the edge of the organic functional layer 42, which can prevent the first electrode E1 from having crosstalk with the hole transport layer 421.

[0095] like Figure 5As shown, in some embodiments, the organic functional layer 42 includes a hole transport layer 421, an organic light-emitting layer 422, an electron transport layer 423 and an electron injection layer 424 which are stacked in sequence in a direction away from the substrate 10. Among them, the hole transport layer 421 is usually composed of a specific organic molecular material, which has high hole mobility and high transparency. The hole transport layer 421 can promote the transport and injection of holes into the organic light-emitting layer 422, thereby emitting light. The electron injection layer 424 has good conductivity and electron injection ability, can promote the injection of negative electrons from the cathode into the electron transport layer 423, and improve the contact between the cathode and the electron transport layer 423, thereby reducing the contact resistance and improving the injection efficiency. The electron transport layer 423 has high electron mobility and high transparency, can promote the transport and injection of electrons into the organic light-emitting layer 422, thereby emitting light.

[0096] Optionally, the orthographic projections of the hole transport layer 421, the organic light emitting layer 422, the electron transport layer 423 and the electron injection layer 424 on the substrate 10 overlap each other. The hole transport layer 421, the organic light emitting layer 422, the electron transport layer 423 and the electron injection layer 424 can be respectively evaporated at the same evaporation angle, so the hole transport layer 421, the organic light emitting layer 422, the electron transport layer 423 and the electron injection layer 424 have the same width to simplify the process.

[0097] In some embodiments, the display panel 100 further includes an encapsulation layer 50, which is disposed on a side of the first electrode E1 away from the substrate 10. The encapsulation layer 50 is disposed on a side of the first electrode E1 away from the substrate 10. The encapsulation layer 50 can protect the sub-pixels from the external environment (such as air and water), prevent air and moisture from penetrating into the display panel 100, and extend the service life and stability of the quantum dots. The encapsulation layer 50 can also prevent impurities and harmful substances from entering the display panel 100, thereby ensuring the performance and quality of the display panel 100.

[0098] Optionally, at least part of the encapsulation layer 50 covers the third isolation portion 33. Part of the encapsulation layer 50 can be filled between the isolation structures 30, and another part covers the third isolation portion 33, which can not only protect each sub-pixel, but also protect the isolation structure 30. In addition, part of the encapsulation is arranged on the side of the isolation structure 30 away from the substrate 10, which can reduce the height of the isolation structure 30, thereby increasing the light output viewing angle of the light-emitting structure 40.

[0099] Preferably, the surface of the encapsulation layer 50 facing away from the substrate 10 is parallel to the plane where the substrate 10 is located, that is, the surface of the encapsulation layer 50 facing away from the substrate 10 is a flat surface, which is beneficial to the process preparation of subsequent film layers.

[0100] In some embodiments, at least a portion of the encapsulation layer 50 overlaps the sidewall surface 32 a of the second isolation portion 32 , which can better protect the isolation structure 30 and reduce the etching loss rate of the isolation structure 30 when evaporating other color sub-pixels.

[0101] In some embodiments, at least a portion of the encapsulation layer 50 is filled between the first electrode E1 and the second isolation portion 32. Since there is a certain gap between the first electrode E1 and the second isolation portion 32, the portion of the encapsulation layer 50 in this embodiment is filled in the gap, which can better protect the first electrode E1 and the second isolation portion 32 at the same time.

[0102] In some embodiments, the encapsulation layer 50 includes a first inorganic encapsulation sublayer 51 and an organic encapsulation sublayer 52 stacked in sequence, and the first inorganic encapsulation sublayer 51 is disposed on a side of the first electrode E1 facing away from the substrate 10 .

[0103] The first inorganic encapsulation sublayer 51 can be made of materials such as silicon oxide, silicon nitride or silicon oxynitride, and can provide good mechanical support and encapsulation protection to prevent the display panel 100 from being affected by the environment. At the same time, the first inorganic encapsulation sublayer 51 can also effectively isolate harmful substances such as moisture and oxygen from the outside from entering the interior of the display panel 100, thereby improving the service life and stability of the display panel 100. The organic encapsulation sublayer 52 can be made of organic materials such as polymers. The thickness of the organic encapsulation sublayer 52 is greater than that of the first inorganic encapsulation sublayer 51, and it is more flexible, so it can better adapt to the bending and curvature of the display panel 100. The organic encapsulation sublayer 52 can prevent harmful substances inside the display panel 100 from overflowing, and can also play a role in isolating external moisture, oxygen, etc. from entering the interior of the display panel 100.

[0104] In some embodiments, the material of the third isolation portion 33 is the same as that of the first inorganic encapsulation sublayer 51. Exemplarily, the material of the third isolation portion 33 and the first inorganic encapsulation sublayer 51 are both formed of silicon nitride, silicon oxide, or silicon oxynitride. In this embodiment, the third isolation portion 33 and the first inorganic encapsulation sublayer 51 are prepared respectively using the same inorganic insulating material, which can facilitate process preparation, reduce costs, and improve production efficiency.

[0105] Preferably, the first inorganic encapsulation sublayer 51 and the organic encapsulation sublayer 52 are embedded in the isolation structure 30. The stacked first inorganic encapsulation sublayer 51 and the organic encapsulation sublayer 52 are arranged inside the isolation structure 30 to better encapsulate and protect each sub-pixel.

[0106] Optionally, the surface of the organic encapsulation sublayer 52 facing away from the substrate 10 is flush with the surface of the isolation structure 30 facing away from the substrate 10 , that is, the organic encapsulation sublayer 52 is reused as a planarization layer, which can facilitate the preparation of the upper film layer.

[0107] Furthermore, the encapsulation layer 50 also includes a second inorganic encapsulation sublayer 53 disposed on the side of the organic encapsulation sublayer 52 away from the substrate 10, and the second inorganic encapsulation sublayer 53 covers the third isolation portion 33. Similarly, the second inorganic encapsulation sublayer 53 can be made of materials such as silicon oxide, silicon nitride or silicon oxynitride, which can provide good mechanical support and encapsulation protection to prevent the display panel 100 from being subjected to mechanical impact and environmental influences. At the same time, the second inorganic encapsulation sublayer 53 can also effectively isolate harmful substances such as moisture and oxygen from the outside from entering the interior of the display panel 100, thereby enhancing the stability of the isolation structure 30, thereby improving the service life and stability of the display panel 100.

[0108] The second aspect of the present application provides a display device, including the display panel 100 of any of the above embodiments. Since the display device adopts all the technical solutions of all the above embodiments, it has at least all the beneficial effects brought by the technical solutions of the above embodiments, which will not be described one by one here.

[0109] The display device may be any device with a display function, for example, a mobile phone, a tablet computer, a laptop computer, a PDA, an in-vehicle electronic device, a wearable device, an ultra-mobile personal computer (UMPC), a netbook, or a personal digital assistant (PDA), etc. It may also be a non-mobile device such as a personal computer (PC), a television (TV), a teller machine, or an automated machine.

[0110] Please refer to Figure 6 to Figure 10 In a third aspect, an embodiment of the present application provides a method for preparing a display panel 100, comprising the following steps:

[0111] S10, forming a pixel definition layer on one side of the substrate.

[0112] like Figure 7 As shown, the pixel definition layer 20 includes a pixel defining portion 21 and a pixel opening 22 formed by the pixel defining portion 21. The present embodiment of the application does not limit the preparation order of the pixel definition layer 20 and the isolation structure 30. For example, the pixel definition material layer can be formed first, and then the pixel opening 22 can be etched to form the pixel definition layer 20, and then the isolation structure 30 can be formed. Alternatively, the pixel definition material layer and the isolation structure 30 material layer can be formed first, and then the isolation structure 30 can be etched to form the pixel definition layer 20, and then the pixel opening 22 can be etched to form the pixel definition layer 20.

[0113] S20, forming an isolation structure on a side of the pixel definition layer away from the substrate through a photolithography process.

[0114] The isolation structure 30 includes a first isolation portion 31 and a second isolation portion 32 sequentially disposed on the pixel defining portion 21 in a direction away from the substrate 10. The first isolation portion 31 includes a conductive material. The orthographic projection of the second isolation portion 32 on the substrate 10 is located within the orthographic projection of the first isolation portion 31 on the substrate 10.

[0115] S30, forming a light-emitting structure by evaporation in the pixel opening.

[0116] like Fig. 9 As shown, due to the existence of the isolation structure 30, the evaporation of the light-emitting structure 40 does not require a precision mask plate, thereby reducing costs and avoiding the shadow effect of the light-emitting layer evaporated by the precision mask plate, which can reduce the spacing between sub-pixels, thereby improving the brightness of the display panel 100100.

[0117] S40, forming a first electrode on a side of the light emitting structure facing away from the substrate.

[0118] like Fig.10 As shown, the first electrode E1 is electrically connected to the first isolation portion 31, and adjacent first electrodes E1 are isolated by the isolation structure 30. Adjacent first electrodes E1 can be electrically connected to each other with the help of the isolation structure 30. Of course, the first electrode E1 can also be connected to the Vss power line through the isolation structure 30 to maintain the potential of the first electrode E1, so that cathode control can be achieved, thereby reducing power consumption.

[0119] In some embodiments, step S20 specifically includes: depositing a metal layer, an organic insulating layer and an inorganic insulating layer on a side of the pixel definition layer 20 facing away from the substrate 10 , respectively, and forming the isolation structure 30 by dry etching and wet etching.

[0120] like Fig.11 As shown, the isolation structure 30 includes a first isolation portion 31, a second isolation portion 32 and a third isolation portion 33 sequentially arranged in a direction away from the substrate 10, and a side wall surface 32a of the second isolation portion 32 is an arc surface concave in a direction away from the first electrode E1.

[0121] First, after depositing a metal layer, an organic insulating layer and an inorganic insulating layer on the pixel definition layer 20, a photoresist is applied on the inorganic insulating layer, and after exposure and development, the part to be etched is exposed, and then dry etching is performed. The inorganic insulating layer is dry-etched to form a third isolation portion 33, and the organic insulating layer is dry-etched to form a second isolation portion 32. Finally, the metal layer is wet-etched to form a first isolation portion 31, and the isolation structure 30 can be prepared.

[0122] Alternatively, a metal layer may be deposited first, and then the metal layer may be wet-etched, or exposed and developed with a half-tone mask to form a first isolation portion 31 having a groove 31a, wherein the groove 31a does not pass through the first isolation portion 31, and then an organic insulating layer and an inorganic insulating layer may be deposited, and then a second isolation portion 32 and a third isolation portion 33 may be obtained by dry etching, thereby preparing an isolation structure 30.

[0123] Although the embodiments disclosed in this application are as above, the contents described are only embodiments adopted for facilitating the understanding of this application and are not intended to limit the present invention. Any technician in the technical field to which this application belongs can make any modifications and changes in the form and details of implementation without departing from the spirit and scope disclosed in this application, but the scope of protection of this application shall still be subject to the scope defined in the attached claims.

[0124] The above is only a specific implementation of the present application. Those skilled in the art can clearly understand that for the convenience and simplicity of description, the replacement of other connection methods described above can refer to the corresponding process in the aforementioned method embodiment, and will not be repeated here. It should be understood that the protection scope of the present application is not limited to this. Any technician familiar with the technical field can easily think of various equivalent modifications or replacements within the technical scope disclosed in this application, and these modifications or replacements should be included in the protection scope of the present application.

Claims

1. A display panel, characterized in that: include: substrate; An isolation structure, comprising a first isolation portion and a second isolation portion sequentially arranged in a direction away from the substrate, the first isolation portion comprising a conductive material, and an orthographic projection of the second isolation portion on the substrate being located within an orthographic projection of the first isolation portion on the substrate; Light-emitting structures, adjacent light-emitting structures being separated by the isolation structure; The first electrode is disposed on a side of the light emitting structure away from the substrate, and the first electrode is electrically connected to the first isolation portion.

2. The display panel according to claim 1, characterized in that: The display panel further includes a third isolation portion, the third isolation portion is arranged on a side of the second isolation portion away from the substrate, and an orthographic projection of the second isolation portion on the substrate is located within an orthographic projection of the third isolation portion on the substrate; Preferably, the orthographic projection of the first isolation portion on the substrate is located within the orthographic projection of the third isolation portion on the substrate; Preferably, the orthographic projection of the first isolation portion on the substrate at least partially overlaps with the orthographic projection of the first electrode on the substrate; Preferably, an orthographic projection of the second isolation portion on the substrate does not overlap with an orthographic projection of the first electrode on the substrate.

3. The display panel according to claim 1, characterized in that: The display panel further comprises a pixel definition layer disposed on the substrate, the pixel definition layer comprises a pixel definition portion and a pixel opening defined by the pixel definition portion, the light emitting structure is located in the pixel opening, and the isolation structure is disposed on the pixel definition portion.

4. The display panel according to claim 2, characterized in that: The length L1 of the edge of the third isolation portion extending relative to the edge of the first isolation portion satisfies the following condition: 1 μm≤L1≤5 μm; Preferably, L1 satisfies the following conditions: 2 μm≤L1≤4 μm; Preferably, the extension length L2 of the edge of the first isolation portion relative to the edge of the second isolation portion satisfies the following condition: 0.5 μm≤L2≤4 μm; Preferably, the material of the first isolation portion includes at least one of molybdenum, molybdenum alloy, aluminum, aluminum alloy, copper and copper alloy; Preferably, the thickness H1 of the first isolation portion along a direction perpendicular to the substrate satisfies the following condition: Preferably, the thickness H1 of the first isolation portion along a direction perpendicular to the substrate satisfies the following condition:

5. The display panel according to claim 2, characterized in that: The material of the second isolation part is an organic insulating material; Preferably, the side wall surface of the second isolation portion is an arc-shaped surface that is concave in a direction away from the first electrode; Preferably, the material of the third isolation portion is an inorganic insulating material; Preferably, the material of the second isolation portion is the same as that of the pixel definition layer; Preferably, the material of the second isolation portion is a black light-shielding material; Preferably, a thickness H2 of the second isolation portion along a direction perpendicular to the substrate satisfies the following condition: 0.5 μm≤H2≤3 μm.

6. The display panel according to claim 1, characterized in that: A surface of one side of the first isolating portion contacting the second isolating portion is a plane.

7. The display panel according to claim 1, characterized in that: A groove is formed on a side of the first isolating portion facing away from the substrate, and an end of the second isolating portion facing the substrate is accommodated in the groove.

8. The display panel according to claim 1, characterized in that: The light emitting structure comprises a hole injection layer and an organic functional layer arranged in sequence in a direction away from the substrate; Preferably, the orthographic projection of the hole injection layer on the substrate is located within the orthographic projection of the organic functional layer on the substrate, and the orthographic projection of the organic functional layer on the substrate is located within the orthographic projection of the first electrode on the substrate; Preferably, the organic functional layer comprises a hole transport layer, an organic light emitting layer, an electron transport layer and an electron injection layer which are sequentially stacked in a direction away from the substrate; Preferably, the hole transport layer, the organic light emitting layer, the electron transport layer and the electron injection layer overlap with each other in their orthographic projections on the substrate.

9. The display panel according to claim 1, characterized in that: The display panel further comprises an encapsulation layer, wherein the encapsulation layer is arranged on a side of the first electrode away from the substrate; Preferably, the encapsulation layer comprises a first inorganic encapsulation sublayer and an organic encapsulation sublayer stacked in sequence, and the first inorganic encapsulation sublayer is arranged on a side of the first electrode away from the substrate; Preferably, the material of the third isolation portion is the same as the material of the first inorganic encapsulation sublayer; Preferably, the first inorganic encapsulation sublayer and the organic encapsulation sublayer are embedded in the isolation structure; Preferably, the encapsulation layer further comprises a second inorganic encapsulation sublayer arranged on a side of the organic encapsulation sublayer away from the substrate, and the second inorganic encapsulation sublayer covers the third isolation portion.

10. A method for preparing a display panel, characterized in that: The following steps are involved: Forming a pixel definition layer on one side of the substrate, the pixel definition layer comprising a pixel definition portion and a pixel opening surrounded by the pixel definition portion; An isolation structure is formed by a photolithography process on a side of the pixel definition layer away from the substrate, wherein the isolation structure comprises a first isolation portion and a second isolation portion sequentially arranged on the pixel definition portion in a direction away from the substrate, the first isolation portion comprises a conductive material, and an orthographic projection of the second isolation portion on the substrate is located within an orthographic projection of the first isolation portion on the substrate; Forming a light-emitting structure by evaporation in the pixel opening; A first electrode is formed on a side of the light emitting structure away from the substrate, and the first electrode is electrically connected to the first isolation portion.

Citation Information

Cited By

  • Display panel, preparation method of display panel and display device

    CN120583867A

  • Display panel, method for manufacturing display panel, and display device

    CN120583867B