High-barrier type linear easy-to-tear nylon film
By adding an antistatic layer and toughened polymer layer to the nylon film, the electrostatic problem is solved, the safety of food packaging and the wear resistance of the film are improved, and excellent oxygen barrier and linear tear-prone properties are maintained.
Patent Information
- Application Number
- CN202411033279.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-30
- Publication Date
- 2024-11-15
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing high-barrier straight-line easily tear nylon films have electrostatic problems during use, which leads to the attachment of static electricity attraction dust and impurities, affecting the shelf life and safety of food.
After extrusion and stretching of nylon films, an antistatic layer and toughened polymer layer are added to improve the antistatic properties and toughness of the films, including alumina vapor deposition layer and hydrophobic modified polyvinyl alcohol coating to enhance the films’ Hardness and barrier properties.
It effectively avoids the occurrence of static electricity, reduces food corrosion and damage, improves the use safety and wear resistance of the film, and maintains excellent oxygen barrier properties and linear tear-prone effect.
Smart Images

Figure CN118952805A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of films, and in particular relates to a high-barrier linear easy-tear nylon film. Background Art
[0002] This is especially true in the packaging field. Existing products used for packaging of food, medicine, etc. usually use materials such as PE and PP as the heat-sealing layer, and materials such as PA and PET as the outer layer. Bags with this structure have the characteristics of high sealing strength and excellent barrier properties, but they also have the problem of large tearing resistance and cannot be torn straight along the scratches when used, which causes certain troubles in people's lives. Especially for the elderly and children, due to the factors of physical strength, they prefer products that are easy to tear.
[0003] To this end, a high-barrier linear tearable nylon film with a bulletin number of "CN111497405B" is disclosed, wherein the film layer structure of the high-barrier linear tearable nylon film includes a base film, a barrier vapor-deposited layer and a surface coating; the base film is a three-layer co-extruded biaxially oriented nylon film, which is A, B and C layers from top to bottom; the A layer and the C layer are composed of 67% to 79.5% nylon 6, 20% to 30% special nylon composition and 0.5% to 3% anti-sticking nylon masterbatch; the B layer is composed of 60% to 70% nylon 6 and 30% to 40% special nylon composition; the special nylon composition contains MXD6-PA66 copolymer, long carbon chain nylon, nylon copolymer and compatibilizer. The film has excellent oxygen barrier properties and has a linear tearing effect in the MD direction. Even bags compounded with PP, PE and other films can have good linear tearing performance.
[0004] However, although the above-mentioned high-barrier linear easy-tear nylon film has excellent oxygen barrier properties and a linear easy-tear effect in the MD direction, and even the bags compounded with PP, PE and other films can have good linear tearing performance, there are still the following obvious defects during use: However, in the actual use process, since the above-mentioned nylon film is not provided with a corresponding antistatic function, the nylon film will generate static electricity during the process of packaging food, and the static electricity will attract dust, impurities or other particulate matter in the surrounding environment to adhere to the surface of the nylon film, which will cause corrosion damage to the food. Summary of the invention
[0005] The object of the present invention is to provide a high-barrier linear easy-tear nylon film to solve the problems raised in the above-mentioned background technology.
[0006] To achieve the above-mentioned purpose, the present invention provides the following technical solution: a high-barrier linear tearable nylon film, comprising a base film, and a barrier vapor-deposited layer and a surface coating layer which are mixed with the base film and extruded into a film layer, wherein the film layer is provided with a nylon resin layer which enables the film to have an oxygen barrier effect, and the surface of the nylon resin layer is provided with an antistatic layer which has an antistatic effect when the film is used, and the base film, the barrier vapor-deposited layer and the surface coating layer are mixed with a toughening polymer layer which has an energy absorption effect when the film is stretched and torn,
[0007] Preferably, the barrier deposited layer is an aluminum oxide deposited layer; the surface coating is a hydrophobically modified polyvinyl alcohol coating, the aluminum oxide deposited layer can increase the surface hardness and wear resistance of the nylon film and extend its service life, and the good barrier properties of the hydrophobically modified polyvinyl alcohol coating can extend the shelf life of food and reduce the possibility of food deterioration or oxidation.
[0008] Preferably, the base film has a thickness of 8 to 15 μm, and the base film and barrier vapor-deposited layer have a thickness of 1 to 5 μm. One side of the base film and barrier vapor-deposited layer is corona treated, so that the extruded and stretched nylon film has better hardness and oxygen barrier effect.
[0009] Preferably, the base film contains copolymer, long carbon chain nylon, nylon copolymer and compatibilizer, and the content ratio of the long carbon chain nylon, the nylon copolymer and the compatibilizer is 6-8:3-4:2-3:1-2.
[0010] Preferably, an adhesive layer is provided between the nylon resin layer and the base film, the nylon resin layer and the antistatic layer, and the nylon resin layer and the base film, the nylon resin layer and the antistatic layer are bonded together using the adhesive layer, so as to strengthen the nylon film to have good toughness and easy tearing effect during actual food use.
[0011] Preferably, the toughening polymer layer comprises an elastic polymer, nano-montmorillonite and a thermoplastic polyester elastomer, and the elastic polymer, nano-montmorillonite and the thermoplastic polyester elastomer are mixed by a mixer, which can enhance the toughness and strength of the nylon film without affecting the tearing properties of the film.
[0012] Compared with the prior art, the technical effects and advantages of the present invention are as follows: the high-barrier linear easy-tear nylon film, by attaching an antistatic layer to both sides of the nylon film after the nylon film is extruded and stretched, can avoid the phenomenon of static electricity generated by friction between the nylon film and the food during the food packaging process, so that the food generates static electricity when the nylon film is used, thereby solving the problem of static electricity attracting dust, impurities or other particulate matter in the surrounding environment to adhere to the surface of the nylon film and causing corrosion damage to the food, further improving the safety of food using the high-barrier linear easy-tear nylon film, and using the toughened polymer layer to make the nylon film have better toughness during pulling use, while not affecting the high-barrier linear easy-tear effect of the nylon film in use, and having high transparency, and can still maintain excellent oxygen barrier properties after steaming and sterilization. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Figure 1 It is a structural schematic diagram of the present invention.
[0014] In the figure: 1. base film; 2. barrier evaporation layer; 3. surface coating; 4. nylon resin layer; 5. antistatic layer; 6. toughening polymer layer; 7. adhesive layer. DETAILED DESCRIPTION
[0015] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0016] See also Figure 1The present invention provides a technical solution: a high-barrier linear tearable nylon film, comprising a base film 1, a barrier vapor-deposited layer 2 and a surface coating 3 which are mixed and extruded with the base film 1 to form a film layer. The base film 1, the barrier vapor-deposited layer 2 and the surface coating 3 are mixed in proportion and dispersed evenly by a high-speed stirrer. The evenly mixed raw materials are melted and co-extruded through three extruders, and the melt is cast through a T-die to a quenched cast sheet with a surface temperature of 15 to 35°C by a chilled roller. The film layer is provided with a nylon resin layer 4 which makes the film have an oxygen barrier effect, and the polymerization monomer of nylon is a polymer containing an amide group. Common polymer monomers include: aminocaproic acid, also known as 6-aminocaproic acid, which is the main monomer for preparing nylon 6, m-phenylenediamine and p-phenylenediamine, which are used to prepare nylon 6,6, and other auxiliary monomers such as nitrosophenol, which are used to prepare different types and modifications of nylon, and have high strength, wear resistance, chemical corrosion resistance and thermal stability. The surface of the nylon resin layer 4 is provided with an antistatic layer 5 that has an antistatic effect during use. The antistatic agent 5 can form a thin film on the surface of the nylon film to reduce the generation and accumulation of static electricity. These antistatic agents can be organic surfactants or special chemical additives, such as antistatic agent polymers. The antistatic layer 5 is surfactant adsorption, ion conductivity, conductive polymer or metal conductive powder. The base film 1, the barrier evaporation layer 2 and the surface coating 3 are mixed with a toughening polymer layer 6 that absorbs energy when the film is stretched and torn. By adding a reinforcing polymer layer on the surface or inside the nylon film, its strength, toughness and wear resistance can be significantly improved. This is particularly beneficial for applications that need to withstand stretching, tearing or impact forces, and helps to reduce damage and aging of nylon films during use and extend their service life.
[0017] The barrier deposited layer 2 is an aluminum oxide deposited layer; aluminum oxide film can effectively improve the gas and water vapor barrier properties of the material, and is therefore often used in packaging materials to prevent food and other products from being affected by the external environment. The surface coating 3 is a hydrophobically modified polyvinyl alcohol coating. Polyvinyl alcohol is a polymer formed by polymerization of vinyl alcohol monomers, usually in the form of a polymer of vinyl alcohol monomers, and has good water solubility and adhesion.
[0018] The thickness of the base film 1 is 8 to 15 μm, the thickness of the base film 1 and the barrier vapor-deposited layer 2 are both 1 to 5 μm, the base film 1 and the barrier vapor-deposited layer 2 are subjected to corona treatment on one side, the film is subjected to heat setting treatment, the setting temperature is 180-215°C, and at least one layer is subjected to corona treatment, and then the base film is rolled and slit to obtain a corona value of >50dyn.
[0019] The base film 1 contains copolymer, long carbon chain nylon, nylon copolymer and compatibilizer, and the content ratio of the long carbon chain nylon, the nylon copolymer and the compatibilizer is 6-8:3-4:2-3:1-2.
[0020] An adhesive layer 7 is provided between the nylon resin layer 4 and the base film 1, the nylon resin layer 4 and the antistatic layer 5, and the nylon resin layer 4 and the base film 1, the nylon resin layer 4 and the antistatic layer 5 are bonded together by the adhesive layer 7. The toughening polymer layer 6 comprises an elastic polymer, nano-montmorillonite and a thermoplastic polyester elastomer, and the elastic polymer, nano-montmorillonite and the thermoplastic polyester elastomer are mixed together by a mixer.
[0021] The basement membrane 1 is mainly prepared by the following operation process:
[0022] (1) The components of the base film 1, the barrier vapor-deposited layer 2 and the surface coating 3 are mixed in proportion and dispersed evenly by a high-speed stirrer.
[0023] (2) The uniformly mixed raw materials are melted and co-extruded through three extruders, and the melt is cast through a T-die onto a chilled roller with a surface temperature of 15 to 35°C to quench the cast sheet.
[0024] (3) The cast sheet is subjected to a humidity conditioning treatment in a water tank at 40 to 75° C. for about 1 to 2 minutes. The residual moisture on the surface of the cast sheet after humidity conditioning is blown dry with an air knife, and synchronous or distributed stretching is performed at a stretching temperature of 130 to 205° C. and a stretching ratio of 2.5×2.5 to 3.5×3.5.
[0025] (4) The film is subjected to heat setting treatment at a setting temperature of 180-215°C, and the film is subjected to corona treatment, and then rolled and slit to obtain the base film
[0026] (5) After the corona surface of the base film is subjected to plasma treatment, a barrier vapor-deposited layer is coated, and then the film coated with the barrier vapor-deposited layer is sent to a coating device, and a hydrophobically modified polyvinyl alcohol coating and an antistatic layer 5 are uniformly coated on the surface of the coating layer. After drying and winding, the high-barrier linear easy-to-tear nylon film is obtained.
[0027] Specifically, when in use, the nylon film adopts a nylon resin layer 4 and a base film 1, a barrier vapor-deposited layer 2 and a surface coating 3, and has excellent oxygen barrier properties. At 23°C and 50% RH, the oxygen permeability of the film is less than 0.8cc / m2·day·atm, and has a linear tearing effect in the MD direction. Even the bag compounded with films such as PP and PE can have good linear tearing performance. At the same time, it has high transparency and can maintain excellent oxygen barrier properties after steaming and sterilization. After the extrusion and stretching of the nylon film, the antistatic layer 5 is attached to both sides of the nylon film, which can prevent the nylon film from generating static electricity due to friction between the nylon film and the food during the food packaging process, so that the food generates static electricity when the nylon film is used, thereby solving the problem of static electricity attracting dust, impurities or other particulate matter in the surrounding environment to adhere to the surface of the nylon film and causing corrosion damage to the food. In addition, the toughened polymer layer can be used to make the nylon film have better toughness during pulling use, and will not affect the high barrier linear tearing effect of the nylon film during use.
[0028] Finally, it should be noted that the above is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A high-barrier linear tearable nylon film, comprising a base film (1), a barrier vapor-deposited layer (2) and a surface coating (3) which are mixed with the base film (1) and extruded to form a film layer, Features: The film layer is provided with a nylon resin layer (4) which enables the film to have an oxygen barrier effect, and the surface of the nylon resin layer (4) is provided with an antistatic layer (5) which has an antistatic effect when the film is in use. The base film (1), the barrier vapor-deposited layer (2) and the surface coating (3) are mixed with a toughening polymer layer (6) which has an energy absorption effect when the film is stretched and torn.
2. A high barrier linear easy-tear nylon film according to claim 1, Features: The barrier vapor-deposited layer (2) is an aluminum oxide vapor-deposited layer; and the surface coating (3) is a hydrophobically modified polyvinyl alcohol coating.
3. A high barrier linear easy-tear nylon film according to claim 1, Features: The base film (1) has a thickness of 8 to 15 μm, the base film (1) and the barrier vapor-deposited layer (2) have a thickness of 1 to 5 μm, and one side of the base film (1) and the barrier vapor-deposited layer (2) is subjected to corona treatment.
4. A high barrier linear easy-tear nylon film according to claim 1, Features: The base film (1) contains copolymer, long carbon chain nylon, nylon copolymer and compatibilizer, and the content ratio of the long carbon chain nylon, the nylon copolymer and the compatibilizer is 6-8:3-4:2-3:1-2.
5. The high barrier linear easy-tear nylon film according to claim 1, Features: An adhesive layer (7) is provided between the nylon resin layer (4) and the base film (1), the nylon resin layer (4), and the antistatic layer (5), and the nylon resin layer (4) and the base film (1), the nylon resin layer (4), and the antistatic layer (5) are bonded together by the adhesive layer (7).
6. A high barrier linear easy-tear nylon film according to claim 1, Features: The toughening polymer layer (6) comprises an elastic polymer, nano-montmorillonite and a thermoplastic polyester elastomer, and the elastic polymer, nano-montmorillonite and the thermoplastic polyester elastomer are mixed in a mixer.
Citation Information
Patent Citations
Easy-to-strip layer stranded high-density fiber bundle air-blowing micro-cable
CN108646369A
Linear easy-to-tear aluminized nylon film and preparation method thereof
CN111516334A
Polyamide vacuum bag composite film for wind turbine blade and production process of polyamide vacuum bag composite film
CN111892810A
Antistatic high-barrier nano-coated nylon film
CN209096184U