Radiation-proof glass

By optimizing the composition of radiation-proof glass, especially the ratio of components such as SiO2, PbO, TiO2, etc., the problem of the reduction in the transmittance of existing radiation-proof glasses in the radiation environment is solved, and the radiation resistance and service life are significantly improved.

CN118954945APending Publication Date: 2024-11-15CDGM GLASS LLC
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202410577419.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2021-09-23
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

The transmittance of existing radiation-proof glass decreases after use in a radiation environment, and its radiation resistance is poor, which affects the product's service effect and life.

Method used

Using the reasonable ratio of components such as SiO2, PbO, TiO2, R2O, Ln2O3, Al2O3, MO and Sb2O3, control the ratio of PbO/SiO2, R2O/TiO2, Al2O3/TiO2 and Ln2O3/(Al2O3+TiO2) to optimize the glass to improve its radiation resistance.

Benefits of technology

After use in a radiant environment, the light transmittance changes slightly, which significantly improves the radiation resistance of the radiation-proof glass and extends the service life of the product.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004832830730000071
    Figure BDA0004832830730000071
  • Figure BDA0004832830730000081
    Figure BDA0004832830730000081
  • Figure BDA0004832830730000082
    Figure BDA0004832830730000082
Patent Text Reader

Abstract

The invention provides radiation-proof glass, which comprises the following components in percentage by weight: 10 to 30 percent of SiO2; pbO: 66.5% to 80%; 0.5 to 5 percent of TiO2; 1 to 5 percent of R2O; r2O is one or a plurality of materials selected from Li2O, Na2O and K2O, and Ln2O3 is one or a plurality of materials selected from La2O3, Gd2O3 and Y2O3. Through reasonable component design, the obtained anti-radiation glass is excellent in radiation resistance, and the light transmittance change is small after the anti-radiation glass is used in a radiation environment for a certain time.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application is a divisional application for the invention patent application with application number 202111112602.2, application date September 23, 2021, and name “Radiation Protection Glass”. Technical Field

[0002] The invention relates to glass, in particular to radiation-proof glass. Background Art

[0003] As a basic structural material, radiation-proof glass is often used in radioactive waste solidification treatment, nuclear medical equipment, ray detection and other devices. In space, nuclear power plants and other scientific application fields, radiation-proof glass mainly has a large absorption capacity for gamma rays, X-rays, etc. When gamma rays or X-rays enter the radiation-proof glass, due to the photoelectric effect inside the glass, positive and negative electron pairs are generated, and excited and free electrons are generated at the same time, which reduces the energy of the incident gamma rays or X-rays, reduces the penetration, and plays a protective role. However, photons and particle radiation in the irradiation environment will cause glass ionization, thereby changing the transmittance of the glass. It is generally believed that radiation resistance represents the most prominent requirement for glass materials in extreme environments such as space and nuclear radiation. The radiation resistance of radiation-proof glass in the prior art is poor. After being used in a radiation environment for a certain period of time, the transmittance decreases significantly, affecting the product's use effect and service life. Summary of the invention

[0004] The technical problem to be solved by the present invention is to provide a radiation-proof glass with excellent radiation resistance.

[0005] The technical solution adopted by the present invention to solve the technical problem is:

[0006] The invention discloses radiation-proof glass. The components of the glass are expressed in weight percentage and contain: SiO2: 10-30%; PbO: 66.5-80%; TiO2: 0.5-5%; R2O: 1-5%; Ln2O3: 0.1-10%, wherein R2O is one or more of Li2O, Na2O and K2O, and Ln2O3 is one or more of La2O3, Gd2O3 and Y2O3.

[0007] Furthermore, its components, expressed in weight percentage, also contain: Al2O3: 0-3%; MO: 0-10%; Sb2O3: 0-2%, wherein MO is one or more of BaO, SrO, CaO, and MgO.

[0008] The invention discloses radiation-proof glass. The components of the glass are expressed by weight percentage and consist of SiO2: 10-30%, PbO: 66.5-80%, TiO2: 0.5-5%, R2O: 1-5%, Ln2O3: 0.1-10%, Al2O3: 0-3%, MO: 0-10%, and Sb2O3: 0-2%. The R2O is one or more of Li2O, Na2O, and K2O, the Ln2O3 is one or more of La2O3, Gd2O3, and Y2O3, and the MO is one or more of BaO, SrO, CaO, and MgO.

[0009] Furthermore, its components are expressed in weight percentage, wherein: SiO2: 18-28%, preferably SiO2: 21-27%; and / or PbO: 70-80%, preferably PbO: 71-77%; and / or TiO2: 1-3%; and / or R2O: 1.5-3%; and / or Ln2O3: 0.2-6%, preferably Ln2O3: 1-4.5%; and / or Al2O3: 0.1-1%, preferably Al2O3: 0.1-0.5%; and / or MO: 0-5%, preferably MO: 0-1.5%; and / or Sb2O3: 0.02-1%, wherein R2O is one or more of Li2O, Na2O, and K2O, Ln2O3 is one or more of La2O3, Gd2O3, and Y2O3, and MO is one or more of BaO, SrO, CaO, and MgO.

[0010] Furthermore, its components are expressed in weight percentage, wherein: PbO / SiO2 is 2.3-6.0, preferably PbO / SiO2 is 2.4-5.0, more preferably PbO / SiO2 is 2.5-3.5, and further preferably PbO / SiO2 is 2.5-3.

[0011] Furthermore, its components are expressed in weight percentage, wherein: R2O / TiO2 is 0.5-6.0, preferably R2O / TiO2 is 1.0-5.0, more preferably R2O / TiO2 is 1.0-3.0, and further preferably R2O / TiO2 is 1.7-2.6.

[0012] Furthermore, its components are expressed in weight percentage, wherein: Al2O3 / TiO2 is less than 0.8, preferably Al2O3 / TiO2 is less than 0.5, and more preferably Al2O3 / TiO2 is 0.01-0.3.

[0013] Furthermore, its components are expressed in weight percentage, wherein: Ln2O3 / (Al2O3+TiO2) is 0.05~8.0, preferably Ln2O3 / (Al2O3+TiO2) is 0.1~5.0, more preferably Ln2O3 / (Al2O3+TiO2) is 0.7~3.0, further preferably Ln2O3 / (Al2O3+TiO2) is 1.455~3.0, and further preferably Ln2O3 / (Al2O3+TiO2) is 2.222~3.0.

[0014] Furthermore, the refractive index n of the radiation-proof glass is d It is 1.75-1.85, preferably 1.78-1.82; and / or the irradiation stability ΔT is less than 45%, preferably less than 40%, more preferably less than 38%; and / or the white light absorption coefficient is less than 1.2%, preferably less than 1.1%, more preferably less than 1.0%; and / or the lead equivalent is 0.40-0.50 mmPb / mm, preferably 0.41-0.46 mmPb / mm, more preferably 0.42-0.45 mmPb / mm.

[0015] The invention discloses a device comprising the radiation-proof glass.

[0016] Compared with the prior art, the embodiments of the present invention have at least the following advantages: through reasonable component design, the radiation-proof glass obtained by the present invention has excellent radiation resistance, and the light transmittance changes little after being used in a radiation environment for a certain period of time.

[0017] Other features and advantages of the present invention will be described in the following description, and partly become obvious from the description, or be understood by practicing the present invention. The purpose and other advantages of the present invention can be realized and obtained by the structure pointed out in the description. DETAILED DESCRIPTION

[0018] The embodiments of the radiation-proof glass of the present invention are described in detail below, but the present invention is not limited to the embodiments described below, and can be implemented with appropriate changes within the scope of the purpose of the present invention. In addition, although there are cases where the repeated description is appropriately omitted, the main purpose of the invention is not limited thereto. In the following content, the radiation-proof glass of the present invention is sometimes referred to as glass.

[0019] [Radiation-proof glass]

[0020] The following is an explanation of the range of each component of the radiation-proof glass of the present invention. In this specification, unless otherwise specified, the content of each component and the total content are all expressed in weight percentage (wt%) relative to the total amount of glass material converted into oxide composition. Here, the "composition converted into oxide" means that when the oxides, complex salts and hydroxides used as raw materials for the radiation-proof glass components (components) of the present invention are decomposed and converted into oxides during melting, the total weight of the oxide material is taken as 100%.

[0021] Unless otherwise indicated in specific circumstances, the numerical ranges listed herein include upper and lower limits, and "above" and "below" include endpoint values, as well as all integers and fractions within the range, without being limited to the specific values ​​listed when the range is defined. "And / or" as used herein is inclusive, for example, "A and / or B" means only A, or only B, or both A and B.

[0022] PbO is an important component of the radiation-proof glass of the present invention, which can improve the radiation-proof ability of the glass, reduce the melting and clarification temperature of the glass, and increase the refractive index and density of the glass; but if the content is too much, the glass-forming ability is reduced, the glass is easy to phase separate, and the optical properties are affected. Therefore, the content of PbO is 66.5-85%, preferably 70-80%.

[0023] SiO2 is the skeleton of glass, which can increase the viscosity of glass, reduce its tendency to crystallize, and improve the chemical stability, thermal stability, mechanical strength and transparency of glass. However, if its content is too much, it will increase the difficulty of melting glass and reduce the density and radiation shielding ability of glass. Therefore, the content of SiO2 is 10-30%, preferably 18-28%.

[0024] In some embodiments, by controlling the ratio of the content of PbO to the content of SiO2, PbO / SiO2, within the range of 2.3 to 6.0, the glass can have good radiation protection, a lower melting temperature and excellent thermal stability. Therefore, preferably PbO / SiO2 is 2.3 to 6.0, more preferably PbO / SiO2 is 2.4 to 5.0, and further preferably PbO / SiO2 is 2.5 to 3.5.

[0025] TiO2 can increase the refractive index of glass and has a high mass absorption coefficient. A proper amount of it can improve the ability of glass to shield radiation. n+ Existing in variable valence states, they can capture holes (h + ) and electron (e -) undergoes redox reaction, thereby avoiding the formation of color centers. However, if its content is too high, the glass is prone to crystallization and devitrification, resulting in reduced transmittance and chemical stability. Therefore, the content of TiO2 is 0.5-5%, preferably 1-3%.

[0026] R2O (R2O is one or more of Li2O, Na2O, K2O) can reduce the viscosity of glass, make glass easier to melt, reduce the tendency of glass to crystallize, increase the transparency and gloss of glass, provide free oxygen for TiO2, Ln2O3, Al2O3, etc., and improve the radiation resistance of glass. However, if its content is too much, the radiation resistance and refractive index of glass will be significantly reduced. Therefore, the content of R2O is 1-5%, preferably 1.5-3%.

[0027] In some embodiments, by controlling the ratio of the content of R2O to the content of TiO2, R2O / TiO2, in the range of 0.5 to 6.0, the glass can have good radiation resistance, and can also improve the melting performance and anti-crystallization performance of the glass. Therefore, preferably R2O / TiO2 is 0.5 to 6.0, more preferably R2O / TiO2 is 1.0 to 5.0, and further preferably R2O / TiO2 is 1.0 to 3.0.

[0028] Al2O3, as a network intermediate component, can increase the stability of the glass network and inhibit glass crystallization. Al2O3 can absorb non-bridging oxygen formed by irradiation, allowing more Al to enter the silicon oxygen network in the form of tetrahedrons, thereby improving the radiation resistance of the glass. However, if its content is too much, it will increase the difficulty of melting the glass, and will also reduce Ti, darken the glass color, and affect the transmittance. Therefore, the content of Al2O3 is 0-3%, preferably 0.1-1%, and more preferably 0.1-0.5%.

[0029] In some embodiments, by controlling the ratio of the content of Al2O3 to the content of TiO2, Al2O3 / TiO2, to be below 0.8, the glass not only has good radiation resistance, but also has a high visible light transmittance. Therefore, preferably Al2O3 / TiO2 is below 0.8, more preferably Al2O3 / TiO2 is below 0.5, and further preferably Al2O3 / TiO2 is 0.01 to 0.3.

[0030] MO (MO is one or more of BaO, SrO, CaO, and MgO) can reduce the viscosity of glass, increase the density and radiation protection of glass, and also improve the radiation resistance of glass. However, if its content is too high, the stability of glass will be reduced. Therefore, the content of MO is 0 to 10%, preferably 0 to 5%.

[0031] Ln2O3 (Ln2O3 is one or more of La2O3, Gd2O3, and Y2O3) can effectively improve the chemical stability and hardness of glass, and can also improve the radiation protection and radiation resistance of glass, but if its content is too much, the stability of glass will be reduced. Therefore, the content of Ln2O3 is 0.1-10%, preferably 0.2-6%.

[0032] In some embodiments, by controlling the ratio of the content of Ln2O3 to the total content of Al2O3 and TiO2 (Al2O3+TiO2) Ln2O3 / (Al2O3+TiO2) in the range of 0.05 to 8.0, the glass can have better radiation protection and radiation resistance, and also have better chemical stability and hardness. Therefore, preferably Ln2O3 / (Al2O3+TiO2) is 0.05 to 8.0, more preferably Ln2O3 / (Al2O3+TiO2) is 0.1 to 5.0, and further preferably Ln2O3 / (Al2O3+TiO2) is 0.7 to 3.0.

[0033] Sb2O3 is a good clarifier, which is beneficial to the overflow of gas in the glass, thereby increasing the bubble degree of the glass. Therefore, the content of Sb2O3 is 0-2%, preferably 0.02-1%.

[0034] The radiation-proof glass of the present invention has a high visible light transmittance. CeO2 will significantly reduce the visible light transmittance of the glass, so in some embodiments, it is preferred not to contain CeO2.

[0035] The "does not contain" and "0%" recorded in this article mean that the compound, molecule or element is not intentionally added as a raw material to the glass of the present invention; however, as raw materials and / or equipment for producing glass, there may be certain impurities or components that are not intentionally added, which may be contained in small amounts or trace amounts in the final glass. This situation is also within the scope of protection of the patent of this invention.

[0036] Next, the performance of the radiation shielding glass of the present invention will be described.

[0037] <Refractive Index>

[0038] The refractive index of glass (n d ) Tested according to the method specified in GB / T 7962.1-2010.

[0039] In some embodiments, the refractive index (n d ) is 1.75 to 1.85, preferably 1.78 to 1.82.

[0040] <Radiation stability>

[0041] The radiation stability (ΔT) of the glass is tested according to the test method for radiation-resistant glass panels for peep windows in the standard "Q\BU.J1577-1996" of the Second Research and Design Institute of Nuclear Industry.

[0042] In some embodiments, the radiation stability (ΔT) of the radiation shielding glass of the present invention is 45% or less, preferably 40% or less, and more preferably 38% or less.

[0043] <White light absorption coefficient>

[0044] The white light absorption coefficient of glass is tested according to the method specified in GB / T7962.9-2010.

[0045] In some embodiments, the white light absorption coefficient of the radiation protection glass of the present invention is 1.2% or less, preferably 1.1% or less, and more preferably 1.0% or less.

[0046] <Lead Equivalent>

[0047] The lead equivalent of glass is tested according to the method specified in GB / T7962.10-2010

[0048] In some embodiments, the lead equivalent of the radiation protection glass of the present invention is 0.40-0.50 mmPb / mm, preferably 0.41-0.46 mmPb / mm, and more preferably 0.42-0.45 mmPb / mm.

[0049] Due to the above-mentioned excellent properties, the radiation-proof glass of the present invention can be widely used in space, nuclear power plants and other scientific application fields, and can be used to manufacture radioactive waste solidification treatment equipment, nuclear medical equipment, radiation detectors and other equipment.

[0050] [Manufacturing method]

[0051] The manufacturing method of the radiation-proof glass of the present invention is as follows: weigh the raw materials (such as carbonate, nitrate, sulfate, hydroxide, oxide, etc.) in proportion according to the raw materials corresponding to the components of the glass, add them into a furnace (such as a ceramic crucible) after fully mixing, melt, clarify, homogenize and then cool at 1000-1400°C; pour the molten glass into a preheated metal mold at about 1000-1300°C; put the molten glass injected into the preheated metal mold together with the metal mold into an annealing furnace for slow cooling, and obtain the radiation-proof glass after annealing. Those skilled in the art can appropriately select raw materials, process methods and process parameters according to actual needs.

[0052] Example

[0053] In order to further clearly explain and illustrate the technical solution of the present invention, the following non-limiting examples are provided. In this example, the above-mentioned method for manufacturing radiation-proof glass is used to obtain radiation-proof glass having the composition shown in Table 1 and Table 2. In addition, the properties of each glass are measured by the test method described in the present invention, and the measurement results are shown in Table 1 and Table 2.

[0054] Table 1.

[0055]

[0056]

[0057] Table 2.

[0058]

[0059]

[0060] Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent substitutions for some of the technical features therein; and these modifications or substitutions do not make the essence of the corresponding technical solutions deviate from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. Radiation-proof glass, characterized in that: Its components are expressed in weight percentage and contain: SiO2: 10-30%; PbO: 66.5-80%; TiO2: 0.5-5%; R2O: 1-5%; Ln2O3: 0.1-10%, wherein R2O is one or more of Li2O, Na2O, and K2O, and Ln2O3 is one or more of La2O3, Gd2O3, and Y2O3.

2. The radiation-proof glass according to claim 1, characterized in that: The components thereof are expressed in weight percentage and further contain: Al2O3: 0-3%; MO: 0-10%; Sb2O3: 0-2%, wherein MO is one or more of BaO, SrO, CaO and MgO.

3. Radiation-proof glass, characterized in that: Its components are expressed in weight percentage, and are composed of SiO2: 10-30%; PbO: 66.5-80%; TiO2: 0.5-5%; R2O: 1-5%; Ln2O3: 0.1-10%; Al2O3: 0-3%; MO: 0-10%; Sb2O3: 0-2%, wherein R2O is one or more of Li2O, Na2O, and K2O, Ln2O3 is one or more of La2O3, Gd2O3, and Y2O3, and MO is one or more of BaO, SrO, CaO, and MgO.

4. The radiation-proof glass according to any one of claims 1 to 3, characterized in that: Its components are expressed in weight percentage, wherein: SiO2: 18-28%, preferably SiO2: 21-27%; and / or PbO: 70-80%, preferably PbO: 71-77%; and / or TiO2: 1-3%; and / or R2O: 1.5-3%; and / or Ln2O3: 0.2-6%, preferably Ln2O3: 1-4.5%; and / or Al2O3: 0.1-1%, preferably Al2O3: 0.1-0.5%; and / or MO: 0-5%, preferably MO: 0-1.5%; and / or Sb2O3: 0.02-1%, wherein R2O is one or more of Li2O, Na2O, and K2O, Ln2O3 is one or more of La2O3, Gd2O3, and Y2O3, and MO is one or more of BaO, SrO, CaO, and MgO.

5. The radiation-proof glass according to any one of claims 1 to 3, characterized in that: Its components are expressed in weight percentage, wherein: PbO / SiO2 is 2.3-6.0, preferably PbO / SiO2 is 2.4-5.0, more preferably PbO / SiO2 is 2.5-3.5, and further preferably PbO / SiO2 is 2.5-3.

6. The radiation protection glass according to any one of claims 1 to 3, characterized in that: Its components are expressed in weight percentage, wherein: R2O / TiO2 is 0.5-6.0, preferably R2O / TiO2 is 1.0-5.0, more preferably R2O / TiO2 is 1.0-3.0, and further preferably R2O / TiO2 is 1.7-2.

6.

7. The radiation-proof glass according to any one of claims 1 to 3, characterized in that: The components are expressed in weight percentage, wherein: Al2O3 / TiO2 is less than 0.8, preferably Al2O3 / TiO2 is less than 0.5, and more preferably Al2O3 / TiO2 is 0.01-0.

3.

8. The radiation-proof glass according to any one of claims 1 to 3, characterized in that: Its components are expressed in weight percentage, wherein: Ln2O3 / (Al2O3+TiO2) is 0.05~8.0, preferably Ln2O3 / (Al2O3+TiO2) is 0.1~5.0, more preferably Ln2O3 / (Al2O3+TiO2) is 0.7~3.0, further preferably Ln2O3 / (Al2O3+TiO2) is 1.455~3.0, and further preferably Ln2O3 / (Al2O3+TiO2) is 2.222~3.

0.

9. The radiation-proof glass according to any one of claims 1 to 3, characterized in that: The refractive index n of the radiation-proof glass d It is 1.75-1.85, preferably 1.78-1.82; and / or the irradiation stability ΔT is less than 45%, preferably less than 40%, more preferably less than 38%; and / or the white light absorption coefficient is less than 1.2%, preferably less than 1.1%, more preferably less than 1.0%; and / or the lead equivalent is 0.40-0.50 mmPb / mm, preferably 0.41-0.46 mmPb / mm, more preferably 0.42-0.45 mmPb / mm.

10. A device, characterized in that: A radiation-proof glass comprising any one of claims 1 to 9.

Citation Information

Patent Citations

  • Optical glass

    CN1622922A