Luminescent compound as well as preparation method and application thereof

By introducing indolenocarbazole groups and aromatic ring structures into OLED materials, the high-energy excited state of anthracene derivatives is regulated, and the thermal exciton mechanism is adopted to solve the problem of low efficiency of blue light materials, achieving high efficiency and low cost Organic electroluminescent devices.

CN118955536AActive Publication Date: 2024-11-15SOUTH CHINA UNIV OF TECH
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202411022643.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-29
Publication Date
2024-11-15
Estimated Expiration
2044-07-29

AI Technical Summary

Technical Problem

Research on blue/deep blue light materials in existing OLED technology is lagging behind, and high-performance blue light materials design is difficult to achieve high efficiency and high color gamut at the same time. The efficiency of traditional devices is limited by the non-luminescent triplet excitons, resulting in low exciton utilization. .

Method used

Anthracene or its derivatives are used as the nuclear structure, and indolenocarbazole groups and aromatic ring conjugated structures are introduced, and the properties of high-energy excitons are regulated through the thermal exciton mechanism to achieve 100% utilization of excitons and improve device efficiency.

Benefits of technology

It achieves efficient exciton utilization, improves the luminous efficiency, brightness and life of organic electroluminescent devices, and reduces manufacturing costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118955536A_ABST
    Figure CN118955536A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of organic photoelectric materials, and discloses a luminescent compound and a preparation method and application thereof. According to the luminescent compound, anthracene or an anthracene derivative is used as a core structure, an indolocarbazole group and a group containing an aromatic ring structure are introduced for structural modification, and after structural modification, steric hindrance and charge transfer degree of molecules can be adjusted, so that emission spectrum, molecular aggregation form and the like can be adjusted; and the purpose of improving the reverse intersystem crossing from the triplet exciton to the singlet is achieved. The compound is a blue fluorescent compound and has high luminous efficiency, and the high luminous efficiency shows that the compound can be used as a luminescent material or a luminescent main body material, particularly can be used as a fluorescent main body material, and shows high efficiency, high brightness, long service life and better charge transfer capability when being used in an organic electroluminescent device; the organic light-emitting device has the advantage of low manufacturing cost, the service life of the organic light-emitting device is prolonged, and the manufacturing cost of the organic light-emitting device is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of organic photoelectric materials, and particularly relates to a luminescent compound and a preparation method and application thereof. Background Art

[0002] Organic light-emitting diodes (OLEDs) have the advantages of active light emission, low driving voltage, fast response speed, and flexible display. After more than 30 years of development, they have been widely used worldwide. Among them, luminescent materials are the core of OLED display technology and have high technical barriers. At present, the research on red and green light materials has become mature, while the research on blue / deep blue light materials is relatively lagging behind. High-performance blue light, especially deep blue light materials, are not only conducive to achieving a wider color gamut, but also can effectively reduce the power consumption of display and lighting equipment, and are key materials in this field. However, due to the wide band gap, the design and development of high-efficiency blue light materials are restricted by unbalanced carrier injection and transmission, and the difficulty in obtaining light color and high device efficiency at the same time. These problems have become a difficulty in the development of the OLED field.

[0003] The core of the breakthrough in OLED material efficiency lies in the utilization of triplet excitons. Limited by spin statistics, 75% of the excited states in traditional OLEDs are non-luminous triplet states. Devices that only use singlet excitons have low efficiency and EQE is limited to 5%. Phosphorescent materials use the spin-orbit coupling effect of precious metals to convert non-luminous triplet states into luminous excited states, and have become the main material system used in current OLED production lines. Following phosphorescent materials, in order to reduce costs, the international community has successively proposed the idea of ​​using pure organic fluorescent molecules to improve the utilization rate of excitons and obtain cheap and efficient materials. For example, triplet-triplet annihilation (TTA), thermally activated delayed fluorescence (TADF) and hot exciton principle. Because the hot exciton mechanism emphasizes the distribution of high-energy exciton conversion channels in the molecular excited state, and proposes to use the weak binding energy of high-energy CT state excitons to realize the RISC process, while the low-energy localized state (Locally excited, LE) radiation transition is not affected, thereby realizing the separation of exciton radiation and exciton conversion. This design avoids the red shift of light color caused by the formation of strong intramolecular charge transfer states (CT), and therefore has a natural advantage in the chromaticity control of blue light molecules. On the other hand, the fast reverse intersystem crossing velocity of high-energy triplet excitons can also avoid the efficiency roll-off caused by accumulation at high current density. At the same time, this design strategy enables non-doped devices to achieve high electroluminescent efficiency and can also simplify the device manufacturing process to reduce costs. Summary of the invention

[0004] In order to overcome the shortcomings and deficiencies of the above-mentioned prior art, the primary purpose of the present invention is to provide a luminescent compound. The luminescent compound uses anthracene or anthracene derivatives as the core structure, introduces an indole carbazole group and a group containing an aromatic ring conjugated structure for structural modification, regulates the properties of the high-energy excited state, realizes the exciton utilization mode dominated by the thermal exciton mechanism, and thus obtains a high efficiency of exciton utilization.

[0005] Another object of the present invention is to provide a method for preparing the above-mentioned luminescent compound.

[0006] Another object of the present invention is to provide application of the above-mentioned luminescent compound in light-emitting diode devices and / or organic electroluminescent devices.

[0007] Another object of the present invention is to provide an organic electroluminescent device.

[0008] The purpose of the present invention is achieved through the following solutions:

[0009] A luminescent compound uses anthracene or anthracene derivatives as the core structure, and introduces indolecarbazole groups and groups containing aromatic ring structures for structural modification.

[0010] As a further preferred solution, in the embodiment of the present application, the luminescent compound has one of the following structural formula (I) or a derivative of the following structural formula (I):

[0011]

[0012] Where Ar is C6-C 60 An aromatic ring group or an aromatic ring derivative group, wherein C6-C 60 The aromatic ring derivative group is C6-C 60 Halogenated aromatic ring groups, C6-C 60 Alkyl substitution of aromatic ring groups, C6-C 60 Alkoxy substitution of aromatic ring groups, C6-C 60 One of the cyano substituents of the aromatic ring group.

[0013] As a further preferred embodiment, in the present application, Ar is one of the following structural formulas or derivatives with substituents on the benzene ring of the following structural formulas:

[0014]

[0015] The substituents on the benzene ring of the structural formula of the derivative are halogen or C1-C 20 The alkyl group, the halogen group includes Cl, Br, the C1-C 20The alkyl group includes a straight chain alkyl group or a branched chain alkyl group; preferably, the alkyl group is a C1-C8 straight chain alkyl group. The substituent group may be any position on the phenyl ring that can be substituted, and may be one substitution or multiple substitutions, and each substituent group is independent of each other.

[0016] As a further preferred solution, the chemical structural formula of the luminescent compound is one of the following structural formulas:

[0017]

[0018] A method for preparing the above-mentioned luminescent compound comprises the following steps:

[0019] (1) reacting Ar-Br with pinacol diborate to generate compound I;

[0020] (2) adding n-butyl lithium to 2-bromoindole[3,2,1-JK]carbazole and 2,6-dibromoanthraquinone in a solvent for reaction, and then adding stannous chloride dihydrate to react to obtain compound II;

[0021] (3) reacting compound I with compound II to obtain a luminescent compound represented by formula (I);

[0022] The specific reaction route is as follows:

[0023]

[0024] The reaction in step (1) is preferably carried out in a solvent in the presence of a catalyst and a base, wherein the solvent is preferably 1,4-dioxane, the catalyst is preferably [1,1'-bis(diphenylphosphino)ferrocene]palladium dichloride, and the base is preferably potassium acetate; the reaction is carried out at 60-110° C. for 8-12 hours;

[0025] The step (2) of adding n-butyl lithium to react means adding n-butyl lithium at -78°C and stirring for 8-12 hours; the step (2) of adding stannous chloride dihydrate to react means reacting at -78-0°C for 8-12 hours;

[0026] The reaction in step (3) refers to a reaction in a solvent in the presence of a catalyst and a base, wherein the solvent is preferably toluene, the catalyst is preferably tetrakis(triphenylphosphine)palladium and tetrabutylammonium bromide, and the base is preferably potassium carbonate; the reaction is preferably carried out at 90-110° C. for 8-12 hours.

[0027] The present application also discloses an anthracene-based blue fluorescent compound. The anthracene-based blue fluorescent small molecule is a small molecule having the above-mentioned luminescent compound structure or a small molecule containing a structural fragment of the luminescent compound.

[0028] The anthracene-based blue fluorescent small molecule described in the present application is applied to light-emitting diode devices and / or organic electroluminescent devices, and is used to manufacture light-emitting devices or light-emitting layers.

[0029] An organic electroluminescent device comprises, from bottom to top, an anode, a hole injection layer, a hole transport layer, an organic light-emitting layer, an electron transport layer, an electron injection layer, and a cathode; wherein the organic light-emitting layer is the above-mentioned anthracene-based blue fluorescent small molecule or contains the above-mentioned anthracene-based blue fluorescent small molecule.

[0030] As a further preferred solution, in the embodiment of the present application, the organic light-emitting layer is a pure film of blue fluorescent molecules or a composite film doped with a guest, wherein the guest is preferably 4,4'-bis[4-(di-p-tolylamino)phenylvinyl]biphenyl (DPAVBi), with a mass fraction of 1%-20%.

[0031] Compared with the prior art, the present invention has the following advantages and beneficial effects:

[0032] 1. The luminescent compound described in the present application uses an anthracene nucleus as a building unit, and its structure is modified by introducing an indolecarbazole group and an aromatic ring structure group to regulate its high-energy excited state properties, thereby opening a high-energy reverse intersystem crossing channel for excitons, realizing a "hot exciton" mechanism, and achieving 100% utilization of excitons.

[0033] 2. The present application provides an anthracene-containing compound, a preparation method and an application thereof. The anthracene-containing compound has a high luminescence efficiency. The high luminescence efficiency indicates that the compound can be used as a luminescent material or a luminescent host material, especially as a fluorescent host material, and can be used in an organic electroluminescent device to exhibit high efficiency, high brightness, long life and better charge transfer capability, and has the advantage of low manufacturing cost, and prolongs the life of the organic electroluminescent device, thereby reducing the manufacturing cost of the organic electroluminescent device.

[0034] 3. The luminescent compounds described in the present application adjust the steric hindrance and charge transfer degree of the molecule by selecting the Ar group and using heterocyclic compounds with aromatic rings or aromatic groups, thereby adjusting the emission spectrum and the molecular aggregation form to enhance the antisystem crossing of triplet excitons to singlet states. BRIEF DESCRIPTION OF THE DRAWINGS

[0035] Figure 1 It is the ultraviolet-visible light absorption spectrum of the luminescent compounds M1-M4 in toluene solution.

[0036] Figure 2 It is the fluorescence emission spectrum of the luminescent compounds M1-M4 in toluene solution.

[0037] Figure 3 Thermogravimetric analysis diagram of luminescent compounds M1-M4.

[0038] Figure 4 The electroluminescence spectrum of the non-doped organic electroluminescent device prepared based on the luminescent compounds M1-M4. DETAILED DESCRIPTION

[0039] The present invention is further described in detail below in conjunction with the examples and drawings, but the embodiments of the present invention are not limited thereto. If specific conditions are not specified in the examples, they are carried out according to conventional conditions or conditions recommended by the manufacturer. If the manufacturer of the reagents or instruments used is not specified, they are all conventional products that can be purchased commercially.

[0040] The term "comprising" and other equivalent descriptions involved in the specification and claims of this application are intended to cover non-exclusive inclusions, including both the contents clearly described in the specification and claims, and the steps or units that are not described in the specification and claims but are inherent in the product, method or structure.

[0041] The embodiment of the present application discloses a luminescent compound, which uses an anthracene derivative as the core structure, introduces indole and carbazole and a group containing an aromatic ring conjugated structure for structural modification, regulates the properties of the high-energy excited state, and realizes an exciton utilization method dominated by a thermal exciton mechanism, thereby obtaining an improvement in the exciton utilization rate. In the scheme of this embodiment, the modification is carried out using a group with an aromatic ring structure, which can adjust the steric hindrance and charge transfer degree of the molecule, and then adjust the emission spectrum, the molecular aggregation form, etc., to achieve the purpose of improving the antisystem crossing of triplet excitons to singlet states.

[0042] Example 1

[0043] This embodiment provides a luminescent compound M1, whose molecular formula is C 64 H 40 N2O2, the structural formula is:

[0044]

[0045] The synthesis route and method of the luminescent compound are as follows:

[0046]

[0047] (1) Synthesis of Compound 1

[0048] Under nitrogen atmosphere, 4-bromoanisole (30.00 mmol) and diboronic acid pinacol ester (60.00 mmol) were added to a 250 mL double-necked bottle, stirred with 100 ml of 1,4-dioxane until completely dissolved, and then [1,1'-bis(diphenylphosphino)ferrocene] palladium dichloride (2.00 mmol) and potassium acetate (90.00 mmol) were added, the temperature was raised to 90°C, and the reaction was stirred for 12 hours. Post-treatment: (1) extraction with dichloromethane and water; (2) vacuum rotary evaporation to obtain a crude product; (3) using petroleum ether and dichloromethane as eluents, the product was separated by column chromatography to obtain compound 1. 1 HNMR, 13 CNMR, MS and elemental analysis results showed that the obtained compound was the target product.

[0049] (2) Synthesis of Compound 2

[0050] Under nitrogen atmosphere, 2-bromoindole [3,2,1-JK] carbazole (70.00 mmol) and 2,6-dibromoanthraquinone (30.00 mmol) were added to a 250 mL two-necked bottle, stirred with 100 ml tetrahydrofuran until completely dissolved, cooled to -78 °C, slowly injected with n-butyl lithium (60.00 mmol), stirred for 12 hours, added stannous chloride dihydrate (60.00 mmol), stirred for another 12 hours, and then quenched with water. Post-treatment: (1) Extraction with dichloromethane; (2) Vacuum rotary evaporation to obtain a crude product; (3) Using petroleum ether and dichloromethane as eluents, column chromatography was performed to separate the product to obtain compound 2. 1 HNMR, 13 CNMR, MS and elemental analysis results showed that the obtained compound was the target product.

[0051] (3) Synthesis of Compound M1

[0052] Under nitrogen atmosphere, compound 1 (40.00 mmol), compound 2 (20.00 mmol), tetrakis(triphenylphosphine)palladium (1.00 mmol), tetrabutylammonium bromide (2.00 mmol) and potassium carbonate (50 mmol) were placed in a 250 mL round-bottom flask, and then 150 mL of toluene was added, stirred and heated, and the reaction temperature was raised to 90°C for 12 hours. When the reaction was cooled to room temperature, post-treatment was performed: (1) extraction with dichloromethane and water; (2) vacuum rotary evaporation to obtain a crude product; (3) using petroleum ether and dichloromethane as eluents, column chromatography was performed to separate the product to obtain compound M1. 1 HNMR, 13 CNMR, MS and elemental analysis results showed that the obtained compound was the target product.

[0053] Example 2

[0054] This embodiment provides a luminescent compound M2, whose molecular formula is C 86 H 50 N4, structural formula:

[0055]

[0056] The synthesis route and method of the luminescent compound are as follows:

[0057]

[0058] (1) Synthesis of Compound 3

[0059] Under nitrogen atmosphere, 9-(4-bromophenyl)carbazole (30.00mmol) and diboronic acid pinacol ester (60.00mmol) were added to a 250mL double-necked bottle, stirred with 100ml 1,4-dioxane until completely dissolved, and then [1,1'-bis(diphenylphosphino)ferrocene] palladium dichloride (2.00mmol) and potassium acetate (90.00mmol) were added, the temperature was raised to 90°C, and the reaction was stirred for 12 hours. Post-treatment: (1) extraction with dichloromethane and water; (2) vacuum rotary evaporation to obtain a crude product; (3) using petroleum ether and dichloromethane as eluents, the product was separated by column chromatography to obtain compound 3. 1 HNMR, 13 CNMR, MS and elemental analysis results showed that the obtained compound was the target product.

[0060] (2) Synthesis of Compound M2

[0061] Under nitrogen atmosphere, compound 3 (40.00 mmol), compound 2 (20.00 mmol), tetrakis(triphenylphosphine)palladium (1.00 mmol), tetrabutylammonium bromide (2.00 mmol) and potassium carbonate (50 mmol) were placed in a 250 mL round-bottom flask, and then 150 mL of toluene was added, stirred and heated, and the reaction temperature was raised to 90°C for 12 hours. When the reaction was cooled to room temperature, post-treatment was performed: (1) extraction with dichloromethane and water; (2) vacuum rotary evaporation to obtain a crude product; (3) using petroleum ether and dichloromethane as eluents, column chromatography was performed to separate the product to obtain compound M2. 1 HNMR, 13 CNMR, MS and elemental analysis results showed that the obtained compound was the target product.

[0062] Example 3

[0063] This embodiment provides a luminescent compound M3, whose molecular formula is C 62 H 34 F2N2, the structural formula is:

[0064]

[0065] The specific synthesis route and preparation method steps are as follows:

[0066]

[0067] (1) Synthesis of Compound 4

[0068] Under nitrogen atmosphere, 4-bromofluorobenzene (30.00 mmol) and biboronic acid pinacol ester (60.00 mmol) were added to a 250 mL double-necked bottle, stirred with 100 ml 1,4-dioxane until completely dissolved, and then [1,1'-bis(diphenylphosphino)ferrocene] palladium dichloride (2.00 mmol) and potassium acetate (90.00 mmol) were added, the temperature was raised to 90°C, and the reaction was stirred for 12 hours. Post-treatment: (1) extraction with dichloromethane and water; (2) vacuum rotary evaporation to obtain a crude product; (3) using petroleum ether and dichloromethane as eluents, the product was separated by column chromatography to obtain compound 4. 1 HNMR, 13 CNMR, MS and elemental analysis results showed that the obtained compound was the target product.

[0069] (2) Synthesis of Compound M3

[0070] Under nitrogen atmosphere, compound 4 (40.00 mmol), compound 2 (20.00 mmol), tetrakis(triphenylphosphine)palladium (1.00 mmol), tetrabutylammonium bromide (2.00 mmol) and potassium carbonate (50 mmol) were placed in a 250 mL round-bottom flask, and then 150 mL of toluene was added, stirred and heated, and the reaction temperature was raised to 90°C for 12 hours. When the reaction was cooled to room temperature, post-treatment was performed: (1) extraction with dichloromethane and water; (2) vacuum rotary evaporation to obtain a crude product; (3) using petroleum ether and dichloromethane as eluents, column chromatography was performed to separate the product to obtain compound M3. 1 HNMR, 13 CNMR, MS and elemental analysis results showed that the obtained compound was the target product.

[0071] Example 4

[0072] This embodiment provides a luminescent compound M4, whose molecular formula is C 70 H 52 N2, structural formula:

[0073]

[0074] The specific synthesis route and preparation method steps are as follows:

[0075]

[0076] (1) Synthesis of Compound 5

[0077] Under nitrogen atmosphere, 4-tert-butyl bromobenzene (30.00 mmol) and biboronic acid pinacol ester (60.00 mmol) were added to a 250 mL double-necked bottle, stirred with 100 ml 1,4-dioxane until completely dissolved, and then [1,1'-bis(diphenylphosphino)ferrocene] palladium dichloride (2.00 mmol) and potassium acetate (90.00 mmol) were added, the temperature was raised to 90°C, and the reaction was stirred for 12 hours. Post-treatment: (1) extraction with dichloromethane and water; (2) vacuum rotary evaporation to obtain a crude product; (3) using petroleum ether and dichloromethane as eluents, the product was separated by column chromatography to obtain compound 5. 1 HNMR, 13 CNMR, MS and elemental analysis results showed that the obtained compound was the target product.

[0078] (2) Synthesis of Compound M4

[0079] Under nitrogen atmosphere, compound 5 (40.00 mmol), compound 2 (20.00 mmol), tetrakis(triphenylphosphine)palladium (1.00 mmol), tetrabutylammonium bromide (2.00 mmol) and potassium carbonate (50 mmol) were placed in a 250 mL round-bottom flask, and then 150 mL of toluene was added, stirred and heated, and the reaction temperature was raised to 90°C for 12 hours. When the reaction was cooled to room temperature, post-treatment was performed: (1) extraction with dichloromethane and water; (2) vacuum rotary evaporation to obtain a crude product; (3) using petroleum ether and dichloromethane as eluents, column chromatography was performed to separate the product to obtain compound M4. 1 HNMR, 13 CNMR, MS and elemental analysis results showed that the obtained compound was the target product.

[0080] Application Example 1

[0081] The present application embodiment provides a non-doped organic light-emitting diode device, and the preparation method thereof is as follows: taking a pre-prepared indium tin oxide (ITO) glass with a sheet resistance of 15Ω, ultrasonically cleaning it with detergent, deionized water, isopropyl alcohol and detergent in sequence, and plasma treating it for 15 minutes. Then in the glove box, 30 nm polyethylene dioxythiophene doped poly (styrene sulfonate) (PEDOT:PSS) was first spin-coated on the ITO surface as a hole injection layer, and then 35 nm thick 4,4',4"-tri (carbazole-9-yl) triphenylamine (TCTA) was sequentially evaporated in an evaporator as a hole transport layer, 30 nm thick luminescent compounds M1 to M4 were used as luminescent layers, 25 nm thick 1,3,5-tri (1-phenyl-1H-benzimidazol-2-yl) benzene (TPBi) was used as an electron transport layer, 1 nm thick lithium fluoride (LiF) was used as an electron injection layer, and 100 nm thick aluminum (Al) was used as a cathode. The device structure is: ITO / PEDOT:PSS / TCTA / luminescent layer (M1-M4) / TPBi / LiF / Al.

[0082] The performance parameters of the prepared non-doped organic light-emitting device are shown in Table 1.

[0083] Table 1: Performance parameters of non-doped organic light-emitting devices

[0084] Luminescent Materials Turn-on voltage(V) <![CDATA[Maximum brightness (cd m -2 )]]> <![CDATA[Maximum current efficiency (cd A -1 )]]> Color coordinates (x, y) M1 3.0 12000 8.2 (0.15,0.08) M2 3.2 12800 8.9 (0.14,0.07) M3 3.4 11700 7.9 (0.13,0.14) M4 3.9 12550 8.7 (0.13,0.09)

[0085] The results in the table show that all devices have good color purity, and the emission spectrum peak is around 450nm, showing blue light emission. In addition, these devices have low turn-on voltage (<3.9V), high brightness (>10000cdm -2 ). This indicates that the anthracene-based blue light-emitting small molecule provided by the present invention can be used to construct a high-efficiency blue light-emitting organic light-emitting diode.

[0086] Application Example 2

[0087] This application embodiment provides a doped organic electroluminescent device, and its preparation method is as follows: take a pre-prepared indium tin oxide (ITO) glass with a square resistance of 15Ω, and use detergent, deionized water, isopropyl alcohol and detergent ultrasonic cleaning in turn, and plasma treatment for 15 minutes. Then, in a glove box, 5nm thick 2,3,5,6-tetrafluoro-7,7',8,8'-tetracyanodimethyl-p-benzoquinone (F4TCNQ) as a hole injection layer, 35nm thick 4,4',4"-tri(carbazole-9-yl)triphenylamine (TCTA) as a hole transport layer, 30nm thick luminescent small molecules M1~M4 (mass fraction 98%) and 4,4'-bis[4-(di-p-tolylamino)phenyl]biphenyl (DPA) are sequentially evaporated on the surface of ITO. VBi) (mass fraction 2%) mixed film as the light-emitting layer, 25nm thick 1,3,5-tri(1-phenyl-1H-benzimidazol-2-yl)benzene (TPBi) as the electron transport layer, 1nm thick cesium fluoride (CsF) as the electron injection layer, 100nm thick aluminum (Al) as the cathode. Device structure ITO / F4TCNQ / TCTA / light-emitting layer (M1-M4 (98%): DPAVBi (2%)) / TPBi / CsF / Al.

[0088] The performance results of the prepared doped organic electroluminescent device are shown in Table 2.

[0089] Table 2: Performance parameters of doped organic light-emitting devices

[0090] Luminescent Materials Turn-on voltage(V) <![CDATA[Maximum brightness (cd m -2 )]]> Maximum external quantum efficiency (%) Color coordinates (x, y) M1:BD 4.1 16680 10.3 (0.14,0.11) M2: BD 4.0 17580 12.3 (0.15,0.10) M3:BD 3.8 18700 13.8 (0.14,0.10) M4:BD 4.2 17880 14.5 (0.15,0.09)

[0091] The above embodiments are preferred implementation modes of the present invention, but the implementation modes of the present invention are not limited to the above embodiments. Any other changes, modifications, substitutions, combinations, and simplifications that do not deviate from the spirit and principles of the present invention should be equivalent replacement methods and are included in the protection scope of the present invention.

Claims

1. A luminescent compound, Features Its structure is one of the following structural formula (I) or a derivative of the following structural formula (I): Where Ar is C 6 -C 60 An aromatic ring group or an aromatic ring derivative group, wherein C 6 -C 60 The aromatic ring derivative group is C 6 -C 60 Halogenated aromatic ring groups, C 6 -C 60 Alkyl substitution of aromatic ring groups, C 6 -C 60 Alkoxy substitution of aromatic ring groups, C 6 -C 60 One of the cyano substituents of the aromatic ring group.

2. The luminescent compound according to claim 1, Features The Ar is one of the following structural formulas or derivatives with substituents on the benzene ring of the following structural formulas: The substituents on the benzene ring of the structural formula of the derivative are halogen or C 1 -C 20 Alkyl, halogen including Cl or Br, the C 1 -C 20 The alkyl group includes a straight chain alkyl group or a branched chain alkyl group; The substituent replaces any substitutable position on the benzene ring, the number of the substituent is at least one, and each substituent is independent of each other.

3. The luminescent compound according to claim 1, Features The chemical structural formula of the luminescent compound is one of the following structural formulas:

4. An anthracene-based blue fluorescent compound, Features The anthracene-based blue fluorescent small molecule is the luminescent compound described in any one of claims 1 to 3 or a compound containing a structural fragment of the luminescent compound described in any one of claims 1 to 3.

5. A method for preparing the luminescent compound according to any one of claims 1 to 3, Features The following steps are involved: (1) reacting Ar-Br with pinacol diborate to generate compound I; (2) adding n-butyl lithium to 2-bromoindole[3,2,1-JK]carbazole and 2,6-dibromoanthraquinone in a solvent for reaction, and then adding stannous chloride dihydrate to react to obtain compound II; (3) reacting compound I with compound II to obtain a luminescent compound represented by formula (I); The specific reaction route is as follows:

6. Use of the anthracene-based blue fluorescent small molecule according to claim 4 in a light emitting diode device or an organic electroluminescent device.

7. An organic electroluminescent device, Features From bottom to top, it includes an anode, a hole injection layer, a hole transport layer, an organic light-emitting layer, an electron transport layer, an electron injection layer, and a cathode; wherein the organic light-emitting layer is the anthracene-based blue fluorescent small molecule described in claim 4 or a mixture containing the anthracene-based blue fluorescent small molecule described in claim 4.

8. The organic electroluminescent device according to claim 7, Features: The organic light-emitting layer is a pure film of the anthracene-based blue fluorescent molecule as described in claim 4 or a composite film doped with a guest.

9. The organic electroluminescent device according to claim 8, Features: The mass fraction of the guest in the guest-doped composite film is 1%-20%.

10. The organic electroluminescent device according to claim 8, Features: The guest in the guest-doped composite film is 4,4'-bis[4-(di-p-tolylamino)phenylvinyl]biphenyl.

Citation Information

Patent Citations

  • Compound, preparation method thereof and light-emitting diode

    CN111233897A

  • Organic electroluminescent element, display device, and lighting device

    JP2012191031A