Transfer and enrichment device and determination method for heavy metals in battery wastewater
By using the device of filling different resins with exchange columns in the battery wastewater with different resins, the efficient enrichment and accurate determination of heavy metals in the battery wastewater is achieved, the complexity and error problems of existing detection methods are solved, and the detection is improved Accuracy and security.
Patent Information
- Application Number
- CN202411033982.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-30
- Publication Date
- 2024-11-15
AI Technical Summary
The existing heavy metal detection methods in battery wastewater are complex, easy to damage the instrument, dangerous operation, and large test errors, making it difficult to accurately determine the content.
Design a transfer and enrichment device for heavy metals in battery wastewater, using sections A and B of exchange columns, respectively, and fill them with adsorption resin and gel-type ion exchange resin, so as to achieve transfer and enrichment of heavy metals through multiple circulations, and The heavy metal content was calculated by analyzing the fluorescence intensity by X-ray fluorescence spectrometer.
It realizes efficient enrichment and accurate measurement of heavy metals in battery wastewater, reduces test errors, simplifies the detection process, and improves the accuracy and safety of detection.
Smart Images

Figure CN118961775A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of heavy metal detection in battery waste water, and particularly relates to a device for transferring and enriching heavy metals in battery waste water and a method for determining the heavy metals. Background Art
[0002] With the rapid development of electronic communications and energy automobile industries, the demand for batteries has increased. The production and improper scrapping of calomel batteries, lead-acid batteries, nickel-cadmium batteries and zinc-carbon batteries produce wastewater containing heavy metals such as mercury, lead, nickel, cadmium and zinc that are difficult to degrade and highly toxic, posing a serious threat to the ecological environment and human health.
[0003] Efficient and accurate determination of heavy metal content is crucial and is the data basis for the rational design of water treatment processes.
[0004] Commonly used detection methods include atomic absorption spectroscopy (AAS) and inductively coupled plasma mass spectrometry (ICP). The instruments are precise and expensive, highly sensitive, and suitable for low / small content detection. However, the composition of battery wastewater is complex and diverse, which can easily interfere with the test results and damage instrument components; the content range of each heavy metal is different and the span is wide, so it is necessary to draw working curves separately, dilute the water samples to be tested by different multiples, and measure them, which can easily amplify the test error; the solid content is high, and there are heavy metals in the solids. If separated and filtered, only the soluble heavy metal content can be measured. If acidified and digested, the heavy metal content can be measured, but the process is complicated and has certain operational risks. Summary of the invention
[0005] In order to overcome the shortcomings of the above-mentioned prior art, the purpose of the present invention is to provide a device for transferring and enriching heavy metals in battery wastewater and a determination method. The determination method is simple and efficient, and the test results are stable and reliable, which can solve the complex technical problems of the existing determination methods.
[0006] In order to achieve the above object, the present invention adopts the following technical solutions:
[0007] The present invention provides a device for transferring and enriching heavy metals in battery wastewater, comprising an exchange column section A, wherein the lower portion of the exchange column section A is connected to an exchange column section B via a connector, and the exchange column section A and the exchange column section B are detachable; the outlet of the exchange column section B is connected to an inlet of a storage tank, and the outlet of the storage tank is connected to the inlet of the exchange column section A, and a pump is provided on a connecting pipe between the outlet of the storage tank and the inlet of the exchange column section A;
[0008] The interior of the exchange column section A is filled with an adsorption resin; the interior of the exchange column section B is filled with a gel-type ion exchange resin.
[0009] In a specific implementation process, the exchange column section A includes a detachable part and an exchange column section A shell; the detachable part is movably connected to the top of the exchange column section A shell.
[0010] In a specific implementation process, a first gasket is arranged on the top of the connecting member, a first filter baffle is built into the top of the connecting member, and a second gasket is arranged on the bottom of the connecting member.
[0011] In a specific implementation process, the exchange column section B includes an exchange column section B shell and a second filter partition; the second filter partition is arranged inside the exchange column section B shell.
[0012] In the specific implementation process, the adsorption resin is a macroporous adsorption resin; the gel-type ion exchange resin is one or more of a resin containing a methyl mercaptan functional group, a resin containing an iminodiacetic acid functional group, and a resin containing a type I quaternary amine functional group.
[0013] The present invention also provides a method for determining heavy metals in battery wastewater, comprising the following steps:
[0014] S1: Take adsorption type resin and fill it in section A of exchange column, and take gel type ion exchange resin and fill it in section B of exchange column;
[0015] S2: Take the battery wastewater and adjust the pH value with acid solution, then transfer the battery wastewater through the exchange column section A and the exchange column section B in sequence at a set flow rate, and circulate for multiple times for enrichment to obtain the adsorption resin to be tested and the gel-type ion exchange resin to be tested;
[0016] S3: After mixing the adsorption resin to be tested and the gel ion exchange resin to be tested, removing water, pressing the mixture into tablets, and obtaining mixed resin tablets;
[0017] S4: Select a mixed standard solution of metals corresponding to each heavy metal in the battery wastewater, repeat S1 to S3, prepare a standard pressed tablet, analyze the standard pressed tablet, and draw a standard working curve according to the operation method of the X-ray fluorescence spectrometer;
[0018] S5: Under the same conditions as the standard pellet analysis in S4, the fluorescence intensity of the mixed resin pellet is measured, and the content of each heavy metal in the battery wastewater is calculated in combination with the standard working curve.
[0019] In a specific implementation process, in S1, the adsorption resin and the gel-type ion exchange resin are used in excess relative to the battery wastewater;
[0020] No less than 30 g of adsorption resin is used for every 1 L of battery waste water, and no less than 90 g of gel ion exchange resin is used for every 1 L of battery waste water.
[0021] In a specific implementation process, in S2, the pH value ranges from 2 to 4, the set flow rate is 1 to 3 mL / min, and the number of cycles is not less than two times;
[0022] In S3, the process of removing water from the mixed resin is as follows:
[0023] The mixture was centrifuged at a speed of 1800-2200 r / min for 5 min, and then dried at a temperature of 100-105° C. for 3 h.
[0024] In the specific implementation process, in S4, the metal corresponding to each heavy metal in the battery wastewater is one or more of mercury, platinum, palladium, nickel, cobalt, lead, and arsenic; the concentration of the mixed standard solution is 0 mg / L~10.00 mg / L; the ordinate of the standard working curve is the fluorescence intensity, and the abscissa of the standard working curve is the content of each heavy metal element.
[0025] In the specific implementation process, in S5, the formula used to calculate the content of each heavy metal in the battery wastewater is as follows:
[0026]
[0027] Among them, Q i is the content of each heavy metal i in battery wastewater, in mg / L; q i is the content of each heavy metal i in the mixed resin tablet measured by X-ray fluorescence spectrometer, in ppm; m1 is the mass of adsorption resin, in g; m2 is the mass of gel ion exchange resin, in g; m3 is the mass of mixed resin for tableting, in g; V is the volume of battery wastewater, in L.
[0028] Compared with the prior art, the present invention has the following beneficial effects:
[0029] On the one hand, the present invention provides a device for transferring and enriching heavy metals in battery wastewater, which couples a variety of functional materials, respectively adsorbs insoluble heavy metals in battery wastewater with the help of adsorption resin, and selectively exchanges soluble heavy metals in battery wastewater with the help of gel resin, so as to achieve complete transfer of non-ionic heavy metals and ionic heavy metals. The transfer and enrichment of heavy metals in battery wastewater are carried out through multiple cycles of two-stage exchange column section A and exchange column section B, and different types of resins are filled in the two-stage exchange column section A and the exchange column section B, respectively. The battery wastewater first flows through the adsorption section and then flows through the exchange section, ensuring that the exchange process is not blocked by macromolecules and large particles, thereby increasing the exchange capacity; the gel-type ion exchange resin in the exchange section can selectively exchange soluble heavy metal ions in the wastewater, and the resin has a high exchange capacity and selectivity, and can efficiently enrich the heavy metal ions in the wastewater. In addition, the two-stage design of the exchange column section A and the exchange column section B makes the device more flexible and easy to operate. The two-stage exchange column can be disassembled separately, which is convenient for filling, taking materials and cleaning operations, reducing maintenance costs and time. The connector realizes the stable connection between the A section and the B section of the exchange column, ensuring the smooth flow of wastewater between the two sections of the exchange column. The storage tank is used to store the treated wastewater, while the pump provides power to enable the wastewater to circulate inside the device. The storage tank and the pump together constitute a circulation system, which realizes the efficient enrichment of heavy metals in the wastewater through multiple cycles.
[0030] Furthermore, the adsorption resin is a macroporous adsorption resin, which has a large pore size and specific surface area, so that it has a three-dimensional spatial pore structure inside, which helps to increase the contact area between the resin and the substance in the solution, and improve the adsorption efficiency and adsorption capacity. Due to the advantages of macroporous structure and specific surface area, macroporous adsorption resin can adsorb more target substances and has a higher selectivity for specific substances.
[0031] Further, gel-type ion exchange resins contain specific functional groups that can exchange or adsorb with specific ions or molecules to achieve selective separation and enrichment. Among them, the methyl mercaptan functional group has a high degree of selective reaction ability with heavy metal ions such as mercury, platinum, and palladium. For example, the methyl mercaptan functional group reacts with mercury ions to form a stable complex, thereby achieving the removal of mercury ions. The iminodiacetic acid functional group has a strong adsorption capacity for heavy metal ions such as nickel, cobalt, and lead. For example, the iminodiacetic acid functional group reacts with nickel ions to form a stable chelate, thereby achieving the removal of nickel ions. The I-type quaternary amine functional group has a strong affinity for monovalent anions such as arsenate, arsenite, etc. For example, the I-type quaternary amine functional group reacts with arsenate to adsorb arsenate on the resin to achieve the removal of arsenic.
[0032] On the other hand, the present invention provides a method for determining heavy metals in battery wastewater. First, a combination of an adsorption resin and a gel-type ion exchange resin is used, which are respectively filled in different sections of an exchange column, and can effectively adsorb and enrich heavy metals in wastewater, including non-ionic and ionic states. The method of sequentially passing through the adsorption resin and the gel-type ion exchange resin can provide effective adsorption and exchange for different types of heavy metals, thereby improving the adaptability of detection. The enriched resin is converted into a tablet form that is easy to analyze through steps such as mixing, removing moisture, and tableting. Subsequently, by comparing and analyzing the mixed standard solutions corresponding to each heavy metal, a standard working curve is drawn according to the operation method of an X-ray fluorescence spectrometer, thereby realizing accurate calculation of the heavy metal content in battery wastewater. This method can detect multiple heavy metal elements (such as mercury, platinum, palladium, nickel, cobalt, lead, arsenic, etc.) in battery wastewater at one time through the preparation of a mixed standard solution and the drawing of a standard working curve, without the need to draw working curves separately and dilute them in different multiples, thereby improving detection efficiency, reducing experimental errors, and improving detection accuracy. In addition, the content of each heavy metal in the battery wastewater can be accurately calculated by combining the measured content of heavy metals in the pressed tablets, as well as parameters such as the mass of the resin and the volume of the battery wastewater.
[0033] Furthermore, adjusting the pH value of battery wastewater through acid can not only create a reaction environment for the exchange section composed of gel-type ion exchange resin, but also ionize heavy metals, which is convenient for adsorption by the adsorption section composed of adsorption resin. The wastewater passes through the exchange column at a set flow rate and is enriched multiple times to ensure that the heavy metals are fully captured. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] Figure 1 It is a schematic diagram of the device for transferring and enriching heavy metals in battery wastewater of the present invention;
[0035] Figure 2 It is a schematic diagram of the structure of the exchange column section A and the exchange column section B in the transfer and enrichment device of heavy metals in battery waste water of the present invention;
[0036] Figure 3 The present invention is a flow chart of the method for determining heavy metals in battery wastewater.
[0037] Wherein: 1-exchange column section A; 2-exchange column section B; 3-connecting piece; 4-pump; 5-storage tank; 6-first gasket; 7-second gasket; 8-first filter baffle; 9-second filter baffle; 10-detachable part; 11-exchange column section A shell; 12-exchange column section B shell. DETAILED DESCRIPTION
[0038] In the following, only some exemplary embodiments are briefly described. As those skilled in the art will appreciate, the described embodiments may be modified in various ways without departing from the spirit or scope of the present invention. Therefore, the drawings and descriptions are considered to be exemplary and non-restrictive in nature.
[0039] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.
[0040] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0041] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, an electrical connection, or a communication; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0042] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is lower in level than the second feature.
[0043] It should be understood that when used in this specification and the appended claims, the terms "include" and "comprises" indicate the presence of described features, integers, steps, operations, elements and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components and / or combinations thereof.
[0044] It should also be understood that the terms used in the present specification are only for the purpose of describing specific embodiments and are not intended to limit the present invention. As used in the present specification and the appended claims, unless the context clearly indicates otherwise, the singular forms "a", "an" and "the" are intended to include plural forms.
[0045] It should be further understood that the term "and / or" used in the present description and the appended claims refers to and includes any and all possible combinations of one or more of the associated listed items.
[0046] Various structural schematic diagrams of the embodiments disclosed in the present invention are shown in the accompanying drawings. These figures are not drawn to scale, and some details are magnified and some details may be omitted for the purpose of clear expression. The shapes of various regions and layers shown in the figures and the relative sizes and positional relationships therebetween are only exemplary, and may deviate in practice due to manufacturing tolerances or technical limitations, and those skilled in the art may additionally design regions / layers with different shapes, sizes, and relative positions according to actual needs.
[0047] The embodiments of the present invention are described in detail below with reference to the accompanying drawings.
[0048] like Figure 1 As shown, the present invention provides a device for transferring and enriching heavy metals in battery wastewater. The core of the device is composed of two exchange columns with different functions arranged in sequence, one is an adsorption section (exchange column A section 1), and the other is an ion exchange section (exchange column B section 2). In the adsorption section, it is filled with adsorption resin. The main task of the adsorption resin is to adsorb large particles, macromolecules and other solids in the battery wastewater to achieve the transfer of insoluble heavy metals. In the ion exchange section, it is filled with gel-type ion exchange resin. The gel-type ion exchange resin has a high selectivity and can specifically perform ion exchange for soluble heavy metals in battery wastewater. The exchange column A section 1 and the exchange column B section 2 can be disassembled. The exchange column A section 1 and the exchange column B section 2 are closely connected by a connector 3. After the battery wastewater is initially purified by the adsorption section, it enters the ion exchange section for exchange to enrich and separate heavy metals. Finally, the treated battery wastewater enters the storage tank 5, and enters the adsorption section and ion exchange section again through the action of the pump 4, forming a cyclic treatment process to achieve efficient transfer and enrichment of heavy metals in the battery wastewater.
[0049] Specifically, the heavy metal transfer and enrichment device in the battery wastewater comprises an exchange column A section 1, an exchange column B section 2, a connector 3, a pump 4 and a storage tank 5, an adsorption resin and a gel-type ion exchange resin.
[0050] The lower part of the exchange column A section 1 is connected to the exchange column B section 2 through a connector 3, the outlet of the exchange column B section 2 is connected to the inlet of the storage tank 5, and the outlet of the storage tank 5 is connected to the inlet of the exchange column A section 1. In addition, a pump 4 is provided on the connecting pipe between the outlet of the storage tank 5 and the inlet of the exchange column A section 1. The adsorption type resin is filled in the exchange column A section 1, and the gel type ion exchange resin is filled in the exchange column B section 2.
[0051] like Figure 2 As shown, in one embodiment, the exchange column section A 1 includes a detachable part 10 and an exchange column section A shell 11, and the exchange column section B 2 includes an exchange column section B shell 12 and a second filter baffle 9; the detachable part 10 is movably connected to the top of the exchange column section A shell 11, and the second filter baffle 9 is arranged inside the exchange column section B shell 12, and the second filter baffle 9 is located at the bottom of the exchange column section B shell 12.
[0052] In one embodiment, a first gasket 6 is disposed on the top of the connecting member 3 , a first filter baffle 8 is built into the top of the connecting member 3 , and a second gasket 7 is disposed on the bottom of the connecting member 3 .
[0053] In addition, the connector 3 is connected to the exchange column A section 1 and the exchange column B section 2 through threads. Specifically, the top of the connector 3 is provided with a first thread, which is connected to the thread at the bottom of the exchange column A section shell 11 through the first thread; the bottom of the connector 3 is provided with a second thread, which is connected to the thread at the top of the exchange column B section shell 12 through the second thread.
[0054] In one embodiment, the adsorption resin is a macroporous adsorption resin. The gel-type ion exchange resin is one or more of a resin containing a methyl mercaptan functional group, a resin containing an iminodiacetyl functional group, and a resin containing a type I quaternary amine functional group.
[0055] like Figure 3 As shown, another aspect of the present invention provides a method for determining heavy metals in battery wastewater, comprising the following steps:
[0056] S1: Take an adsorption resin and fill it in the exchange column A section 1, and take a gel-type ion exchange resin and fill it in the exchange column B section 2. The adsorption resin and the gel-type ion exchange resin are used in excess relative to the battery wastewater; no less than 30g of the adsorption resin is used for every 1L of battery wastewater, and no less than 90g of the gel-type ion exchange resin is used for every 1L of battery wastewater.
[0057] S2: Take the battery wastewater and adjust the pH value with acid solution, then transfer the battery wastewater through the exchange column A section 1 and the exchange column B section 2 at the set flow rate, and circulate for multiple times for enrichment to obtain the adsorption type resin to be tested and the gel type ion exchange resin to be tested. The pH value range is 2 to 4, the set flow rate is 1 to 3 mL / min, and the number of cycles is not less than two times.
[0058] S3: After mixing the adsorption resin to be tested and the gel ion exchange resin to be tested, remove water, press and prepare a sample, and obtain a mixed resin pressed tablet. The specific process of removing water from the mixed resin is as follows: the mixed resin is centrifuged at a speed of 1800-2200 r / min for 5 minutes, and then dried at a temperature of 100-105° C. for 3 hours.
[0059] S4: Select the metal mixed standard solution corresponding to each heavy metal in the battery wastewater, repeat S1 to S3, and prepare the standard pressed tablets according to the operation method of the X-ray fluorescence spectrometer, analyze the standard pressed tablets, and draw the standard working curve. Among them, the metal corresponding to each heavy metal in the battery wastewater is one or more of mercury, platinum, palladium, nickel, cobalt, lead, and arsenic; the concentration of the mixed standard solution is 0mg / L to 10.00mg / L; the ordinate of the standard working curve is the fluorescence intensity, and the abscissa of the standard working curve is the content of each heavy metal element.
[0060] S5: Under the same conditions as the standard pellet analysis in S4, the fluorescence intensity of the mixed resin pellet is measured, and the content of each heavy metal in the battery wastewater is calculated in combination with the standard working curve.
[0061] Among them, the formula used to calculate the content of each heavy metal in battery wastewater is as follows:
[0062]
[0063] Among them, Q i is the content of each heavy metal i in battery wastewater, in mg / L; q i is the content of each heavy metal i in the mixed resin tablet measured by X-ray fluorescence spectrometer, in ppm; m1 is the mass of adsorption resin, in g; m2 is the mass of gel ion exchange resin, in g; m3 is the mass of mixed resin for tableting, in g; V is the volume of battery wastewater, in L.
[0064] In the specific implementation process, the heavy metal transfer and enrichment device in the battery wastewater includes: exchange column A section 1, exchange column B section 2, connector 3, pump 4, storage tank 5, gasket and partition. The exchange column A section 1 and the exchange column B section 2 are connected by the connector 3, and the specific connection method is: the connector 3 and the exchange column A section 1 and the exchange column B section 2 are all built-in threaded sections, which can be manually screwed and connected, so that the exchange column A section 1 and the exchange column B section 2 are easy to disassemble.
[0065] The partition includes a first filter partition 8 and a second filter partition 9. The first filter partition 8 is arranged in the connecting member 3, which not only ensures the flow of battery waste water but also prevents the leakage of resin particles in the exchange column section A 1; the second filter partition 9 is arranged in the exchange column section B 2, which not only ensures the flow of battery waste water but also prevents the leakage of resin particles in the exchange column section B 2; the detachable member 10 on the upper part of the exchange column section A 1 can be disassembled and reassembled.
[0066] The gasket includes a first gasket 6 and a second gasket 7. The first gasket 6 is arranged on the top of the connecting member 3, and the second gasket 7 is arranged on the bottom of the connecting member 3.
[0067] The installation and use order of the heavy metal transfer and enrichment device in the above-mentioned battery wastewater is as follows: a perforated partition, namely the second filter partition 9, is built into the bottom of the exchange column section B shell 12, and a gel-type ion exchange resin is filled; the top of the exchange column section B shell 12 is threadedly connected to the connecting piece 3 and a second gasket 7 is set; a perforated partition, namely the first filter partition 8, is built into the connecting piece 3, the exchange column section A shell 11 is connected to the connecting piece 3 and a first gasket 6 is set; after filling with the adsorption resin, a detachable part 10 is installed on the top of the exchange column section A shell 11.
[0068] In the specific implementation process, the method for determining heavy metals in battery wastewater includes the following steps:
[0069] Step 1: weigh a quantitative adsorption resin, m1g, to be filled in section A 1 of the exchange column, and weigh a quantitative gel ion exchange resin, m2g, to be filled in section B 2 of the exchange column; respectively adsorb insoluble heavy metals in the battery wastewater with the help of the macroporous adsorption resin, and selectively exchange soluble heavy metals in the battery wastewater with the help of the gel ion exchange resin, so as to achieve complete transfer of non-ionic heavy metals and ionic heavy metals;
[0070] The second step is to install a device for transferring and enriching heavy metals in battery wastewater;
[0071] Step 3: Take a certain amount of battery wastewater, VL, adjust the pH to 2-4 with nitric acid, and pass it through the exchange column A section 1 and the exchange column B section 2 at a flow rate of 1-3 mL / min. The effluent of the exchange column B section 2 flows back to the exchange column A section 1, and the cycle is repeated for multiple times;
[0072] Step 4: Split the exchange column A section 1 and the exchange column B section 2, remove the adsorption resin and gel ion exchange resin filled in the exchange column A section 1 and the exchange column B section 2, obtain the adsorption resin to be tested and the gel ion exchange resin to be tested. Mix them evenly to obtain a mixed resin, and remove water;
[0073] Step 5: Weigh an appropriate amount of the mixed resin in step 4, m3 g, add boric acid to the bottom, and use a tablet press to obtain a mixed resin tablet to be tested;
[0074] Step 6: Select one or more standard solutions of mercury, platinum, palladium, nickel, cobalt, lead, and arsenic, and prepare a series of mixed standard solutions with concentrations of 0 mg / L, 0.10 mg / L, 0.50 mg / L, 1.00 mg / L, 2.00 mg / L, 5.00 mg / L, and 10.00 mg / L. Repeat the first to fifth steps to obtain a series of standard pressed tablets. According to the operation method of the X-ray fluorescence spectrometer, adjust the working parameters, analyze the standard pressed tablets, and draw a standard working curve with fluorescence intensity as the ordinate and the content of each heavy metal element as the abscissa; use X-ray fluorescence spectroscopy to achieve simultaneous, qualitative, and quantitative analysis of multiple heavy metal elements.
[0075] Step 7: Under the same conditions and parameters as in step 6, the fluorescence intensity of the mixed resin pellets in step 5 is measured by X-ray fluorescence spectrometer, and the content of each heavy metal in the mixed resin pellets is calculated according to the standard working curve, q i Combined with formula (1), the content of heavy metals in battery wastewater is calculated as Q i .
[0076] Furthermore, in the first step, the adsorption resin is a macroporous adsorption resin. The gel-type ion exchange resin is a mixed gel-type ion exchange resin containing a methyl mercaptan functional group (reacting with mercury, platinum, and palladium), an iminodiacetic acid functional group (reacting with nickel, cobalt, and lead), and a type I quaternary amine functional group (reacting with arsenic). The adsorption resin and the gel-type ion exchange resin need to be in excess relative to the battery wastewater.
[0077] Preferably, the mass ratio of the resin containing methyl mercaptan functional group, the resin containing iminodiacetyl functional group and the resin containing type I quaternary amine functional group in the gel-type ion exchange resin is not greater than 1:1:1. The dosage ratio of the adsorption-type resin to the battery wastewater is not less than 30g:1L, and the dosage ratio of the gel-type ion exchange resin to the battery wastewater is not less than 90g:1L, so as to ensure that the resin is excessive and sufficient to adsorb and exchange heavy metals in the wastewater.
[0078] Furthermore, the fourth step of removing water includes removing external free water and removing internal equilibrium water, and the removal method is: transfer the resin (adsorption resin and gel ion exchange resin) in the exchange column to the filter tube, put it into the centrifuge, rotate it at 1800-2200r / min for 5 minutes; transfer it to the evaporating dish, and dry it at 100-105°C for 3 hours. By centrifugation and drying, the free water outside the resin and the internal equilibrium water are removed to avoid the problems of loose tablets prepared from wet raw materials, easy to fall off, and contamination of the instrument cavity.
[0079] Furthermore, in the sixth step, the working conditions of mercury, platinum, palladium, nickel, cobalt, lead and arsenic at least include: spectroscopic crystal LiF200, detector SC, pulse height PHA 60%-140%.
[0080] The determination method provided by the present invention can accurately test the total content of non-ionic and ionic states of various heavy metals in battery wastewater. The method has good reproducibility and is easy to implement and promote.
[0081] Example 1
[0082] Step 1: Use an electronic balance to weigh 30.5034 g of D101 styrene macroporous adsorption resin to be filled in section A 1 of the exchange column; weigh 30.2189 g of methyl mercaptan ion exchange resin (exchange reaction with mercury, platinum, and palladium) and 31.5579 g of iminodiacetic acid ion exchange resin (exchange reaction with nickel, cobalt, and lead) and 31.7088 g of type I quaternary ammonium ion exchange resin (react with arsenic), mix them evenly, and fill them in section B 2 of the exchange column.
[0083] Step 2: Install the second filter baffle 9 at the bottom of the exchange column section B shell 12 and fill it with gel-type ion exchange resin; rotate, tighten and connect the exchange column section B shell 12 and the connecting piece 3 along the thread direction; install the first filter baffle 8 in the connecting piece 3, rotate, tighten and connect the exchange column section A shell 11 and the connecting piece 3 along the thread direction; fill it with adsorption resin, rotate, tighten and connect the detachable part 10 on the upper part of the exchange column section A shell 11 along the thread direction, and complete the installation of the heavy metal transfer and enrichment device in battery wastewater.
[0084] Step 3: Use a glass measuring cylinder to measure 1.0L of wastewater, and use 1mol / L nitric acid to adjust the pH of the wastewater to 2-4, preferably 3.5, to ensure that adsorption and exchange can be carried out efficiently. The wastewater is circulated through the exchange column section A 1 at a flow rate of 1-3mL / min, preferably 2mL / min, so as to adsorb the insoluble heavy metals in the battery wastewater; then circulate the exchange column section B 2 at a flow rate of 1-3mL / min, preferably 2mL / min, which has specific selectivity for mercury, platinum, palladium, nickel, cobalt, lead, and arsenic, especially in an acidic environment, and has a strong binding effect on the ionic state. The effluent from the exchange column section B 2 is refluxed to the exchange column section A 1, and the cycle is repeated 3 times to extend the reaction time and improve the enrichment degree.
[0085] Step 4: Split the exchange column A section 1 and the exchange column B section 2, remove the adsorption resin and gel ion exchange resin filled in the exchange column A section 1 and the exchange column B section 2, and obtain the adsorption resin and gel ion exchange resin to be tested. Mix them evenly to obtain a mixed resin, transfer them to a centrifuge adapter filter tube, put them into the centrifuge, set the centrifugal speed to 1800-2200r / min, preferably 1800r / min, and the rotation time to 5min to remove the free water carried by the resin particles outside; transfer the centrifuged resin particles to a glass evaporating dish, set the oven temperature to 100-105°C, preferably 100°C, and the drying time to 3h.
[0086] Step 5: Use an electronic balance to weigh 3 g of the mixed resin in step 4, add boric acid to make a rimmed bottom, and use a tablet press to make a tablet to obtain a mixed resin tablet to be tested;
[0087] Step 6: Select 100.00 mg / L certified standard solutions of mercury, platinum, palladium, nickel, cobalt, lead, and arsenic. Use a pipette to transfer 0 mL, 1 mL, 2 mL, 5 mL, and 10 mL to a 100 mL volumetric flask, and adjust the volume to obtain 0 mg / L, 1.00 mg / L, 2.00 mg / L, 5.00 mg / L, and 10.00 mg / L standard solutions. Use a pipette to transfer 1 mL and 5 mL to a 1000 mL volumetric flask, adjust the volume to obtain 0.10 mg / L and 0.50 mg / L standard solutions. Use a pipette to transfer 1.00 mL of each group of standard solutions to a 100 mL volumetric flask, adjust the volume to obtain 8 mixed standard solutions with configuration concentrations of 0 mg / L, 0.10 mg / L, 0.50 mg / L, 1.00 mg / L, 2.00 mg / L, 5.00 mg / L, and 10.00 mg / L.
[0088] Repeat steps 1, 2, 3, 4 and 5 to obtain 8 standard pressed tablets. According to the X-ray fluorescence spectrometer operation method, set the spectroscopic crystal LiF200, the detector SC, and the pulse height PHA60%-140%, analyze the 8 standard pressed tablets, and draw the standard working curve with the fluorescence intensity as the ordinate and the content of each heavy metal element as the abscissa.
[0089] Step 7: According to the operation method of the X-ray fluorescence spectrometer, set the spectroscopic crystal LiF200, the detector SC, the pulse height PHA60%-140%, and measure the fluorescence intensity of the mixed resin pellets in the fifth step. According to the standard working curve, the contents of mercury, platinum, palladium, nickel, cobalt, lead and arsenic in the mixed resin pellets are 21.38ppm, 3.90ppm, 0.16ppm, 91.63ppm, 30.98ppm, 52.12ppm and 10.00ppm respectively. Combined with formula (1), the contents of mercury, platinum, palladium, nickel, cobalt, lead and arsenic in the battery wastewater are calculated to be 2.63mg / L for mercury, 0.48mg / L for platinum, 0.02mg / L for palladium, 11.27mg / L for nickel, 3.81mg / L for cobalt, 6.41mg / L for lead and 1.23mg / L for arsenic respectively.
[0090] Example 2
[0091] Step 1: Use an electronic balance to weigh 40.0679 g of DA-201 styrene macroporous adsorption resin to be filled in section A 1 of the exchange column; weigh 30.2374 g of methyl mercaptan ion exchange resin (to react with mercury, platinum, and palladium) and 40.2188 g of iminodiacetic acid ion exchange resin (to react with nickel, cobalt, and lead) and 30.4752 g of type I quaternary ammonium ion exchange resin (to react with arsenic), mix them evenly, and fill them in section B 2 of the exchange column.
[0092] Step 2: Install the second filter baffle 9 at the bottom of the exchange column section B shell 12 and fill it with gel-type ion exchange resin; rotate, tighten and connect the exchange column section B shell 12 and the connecting piece 3 along the thread direction; install the first filter baffle 8 in the connecting piece 3, rotate, tighten and connect the exchange column section A shell 11 and the connecting piece 3 along the thread direction; fill it with adsorption resin, rotate, tighten and connect the detachable part 10 on the upper part of the exchange column section A shell 11 along the thread direction, and complete the installation of the heavy metal transfer and enrichment device in battery wastewater.
[0093] Step 3: Use a glass measuring cylinder to measure 1.2L of wastewater, and use 1mol / L nitric acid to adjust the pH of the wastewater to 3.5 to ensure that adsorption and exchange can be carried out efficiently. The wastewater is circulated through the exchange column section A 1 at a flow rate of 1-3mL / min, preferably 2mL / min, to adsorb insoluble heavy metals in the battery wastewater; then circulate through the exchange column section B 2 at a flow rate of 1-3mL / min, preferably 2mL / min, which has specific selectivity for mercury, platinum, palladium, nickel, cobalt, lead, and arsenic, especially in an acidic environment, and has a strong binding effect on the ionic state. The effluent from the exchange column section B 2 is refluxed to the exchange column section A 1, and the cycle is repeated 3 times to extend the reaction time and improve the enrichment degree.
[0094] Step 4: Split the exchange column A section 1 and the exchange column B section 2, remove the adsorption resin and gel ion exchange resin filled in the exchange column A section 1 and the exchange column B section 2, and obtain the adsorption resin and gel ion exchange resin to be tested. Mix them evenly to obtain a mixed resin, transfer them to a centrifuge adapter filter tube, put them into the centrifuge, set the centrifugal speed to 1800-2200r / min, preferably 2000r / min, and the rotation time to 5min to remove the free water carried by the resin particles; transfer the centrifuged resin particles to a glass evaporating dish, set the oven temperature to 100-105°C, preferably below 100°C, and the drying time to 3h.
[0095] Step 5: Use an electronic balance to weigh 4.3965 g of the mixed resin in step 4, add boric acid to make a rimmed bottom, and use a tablet press to make a tablet to obtain a mixed resin tablet to be tested;
[0096] Step 6: Select 100.00 mg / L certified standard solutions of mercury, platinum, palladium, nickel, cobalt, lead, and arsenic. Use a pipette to transfer 0 mL, 1 mL, 2 mL, 5 mL, and 10 mL to a 100 mL volumetric flask, and adjust the volume to obtain 0 mg / L, 1.00 mg / L, 2.00 mg / L, 5.00 mg / L, and 10.00 mg / L standard solutions. Use a pipette to transfer 1 mL and 5 mL to a 1000 mL volumetric flask, adjust the volume to obtain 0.10 mg / L and 0.50 mg / L standard solutions. Use a pipette to transfer 1.00 mL of each group of standard solutions to a 100 mL volumetric flask, adjust the volume to obtain 8 mixed standard solutions with configuration concentrations of 0 mg / L, 0.10 mg / L, 0.50 mg / L, 1.00 mg / L, 2.00 mg / L, 5.00 mg / L, and 10.00 mg / L.
[0097] Repeat steps 1, 2, 3, 4 and 5 to obtain 8 standard pressed tablets. According to the X-ray fluorescence spectrometer operation method, set the spectroscopic crystal LiF200, the detector SC, and the pulse height PHA60%-140%, analyze the 8 standard pressed tablets, and draw the standard working curve with the fluorescence intensity as the ordinate and the content of each heavy metal element as the abscissa.
[0098] Step 7: According to the operation method of the X-ray fluorescence spectrometer, set the spectroscopic crystal LiF200, the detector SC, the pulse height PHA60%-140%, and measure the fluorescence intensity of the mixed resin pellets in the fifth step. According to the standard working curve, the contents of mercury, platinum, palladium, nickel, cobalt, lead and arsenic in the mixed resin pellets are 22.21ppm, 3.91ppm, 0.17ppm, 95.92ppm, 32.43ppm, 54.55ppm and 10.30ppm respectively. Combined with formula (1), the contents of mercury, platinum, palladium, nickel, cobalt, lead and arsenic in the battery wastewater are calculated to be 2.61mg / L mercury, 0.46mg / L platinum, 0.02mg / L palladium, 11.27mg / L nickel, 3.81mg / L cobalt, 6.41mg / L lead and 1.21mg / L arsenic respectively.
[0099] By comparing the test results of Example 1 and Example 2, it can be seen that the detection method provided by the present invention has high reliability and strong repeatability.
[0100] The above shows and describes the basic principles and main features of the present invention and the advantages of the present invention. It is obvious to those skilled in the art that the present invention is not limited to the details of the above exemplary embodiments, and the present invention can be implemented in other specific forms without departing from the spirit or basic features of the present invention. Therefore, no matter from which point of view, the embodiments should be regarded as exemplary and non-restrictive. The scope of the present invention is defined by the attached claims rather than the above description, and it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims are included in the present invention. Any figure mark in the claims should not be regarded as limiting the claims involved.
[0101] In addition, it should be understood that although this specification is described in accordance with the implementation modes, not every implementation mode contains only one independent technical solution. This description of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment can also be appropriately combined to form other implementation modes that can be understood by those skilled in the art. The above content is only to illustrate the technical idea of the present invention, and cannot be used to limit the protection scope of the present invention. Any changes made on the basis of the technical solution according to the technical idea proposed by the present invention shall fall within the protection scope of the claims of the present invention.
Claims
1. A device for transferring and enriching heavy metals in battery wastewater, characterized in that: The invention comprises an exchange column section A (1), wherein the lower part of the exchange column section A (1) is connected to an exchange column section B (2) via a connecting piece (3), and the exchange column section A (1) and the exchange column section B (2) are detachable; the outlet of the exchange column section B (2) is connected to the inlet of a storage tank (5), and the outlet of the storage tank (5) is connected to the inlet of the exchange column section A (1), and a pump (4) is provided on the connecting pipe between the outlet of the storage tank (5) and the inlet of the exchange column section A (1); The interior of the exchange column section A (1) is filled with an adsorption resin; the interior of the exchange column section B (2) is filled with a gel-type ion exchange resin.
2. The device for transferring and enriching heavy metals in battery wastewater according to claim 1, characterized in that: The exchange column section A (1) comprises a detachable part (10) and an exchange column section A shell (11); the detachable part (10) is movably connected to the top of the exchange column section A shell (11).
3. The device for transferring and enriching heavy metals in battery wastewater according to claim 1, characterized in that: A first gasket (6) is arranged at the top of the connecting member (3), a first filter baffle (8) is built into the top of the connecting member (3), and a second gasket (7) is arranged at the bottom of the connecting member (3).
4. The device for transferring and enriching heavy metals in battery wastewater according to claim 1, characterized in that: The exchange column section B (2) comprises an exchange column section B shell (12) and a second filter baffle (9); the second filter baffle (9) is arranged inside the exchange column section B shell (12).
5. The device for transferring and enriching heavy metals in battery wastewater according to claim 1, characterized in that: The adsorption resin is a macroporous adsorption resin; the gel-type ion exchange resin is one or more of a resin containing a methyl mercaptan functional group, a resin containing an iminodiacetic acid functional group, and a resin containing a type I quaternary amine functional group.
6. A method for determining heavy metals in battery wastewater, characterized in that: The following steps are involved: S1: filling the A section (1) of the exchange column with an adsorption resin, and filling the B section (2) of the exchange column with a gel-type ion exchange resin; S2: taking battery wastewater and adjusting the pH value with acid solution, and then transferring the battery wastewater through the exchange column section A (1) and the exchange column section B (2) at a set flow rate, and circulating for multiple times for enrichment to obtain the adsorption resin to be tested and the gel-type ion exchange resin to be tested; S3: After mixing the adsorption resin to be tested and the gel ion exchange resin to be tested, removing water, pressing the mixture into tablets, and obtaining mixed resin tablets; S4: Select a metal mixed standard solution corresponding to each heavy metal in the battery wastewater, repeat S1 to S3, prepare a standard pressed tablet, analyze the standard pressed tablet, and draw a standard working curve according to the operation method of the X-ray fluorescence spectrometer; S5: Under the same conditions as the standard pellet analysis in S4, the fluorescence intensity of the mixed resin pellet is measured, and the content of each heavy metal in the battery wastewater is calculated in combination with the standard working curve.
7. The method for determining heavy metals in battery waste water according to claim 6, characterized in that: In S1, the adsorption resin and the gel ion exchange resin are used in excess relative to the battery wastewater; No less than 30 g of adsorption resin is used for every 1 L of battery waste water, and no less than 90 g of gel ion exchange resin is used for every 1 L of battery waste water.
8. The method for determining heavy metals in battery wastewater according to claim 6, characterized in that: In S2, the pH value ranges from 2 to 4, the set flow rate is 1 to 3 mL / min, and the number of cycles is not less than two times; In S3, the process of removing water is as follows: The mixture was centrifuged at a speed of 1800-2200 r / min for 5 min, and then dried at a temperature of 100-105° C. for 3 h.
9. The method for determining heavy metals in battery wastewater according to claim 6, characterized in that: In S4, the metals corresponding to the heavy metals in the battery wastewater are one or more of mercury, platinum, palladium, nickel, cobalt, lead, and arsenic; the concentration of the mixed standard solution is 0 mg / L to 10.00 mg / L; the ordinate of the standard working curve is the fluorescence intensity, and the abscissa of the standard working curve is the content of each heavy metal element.
10. The method for determining heavy metals in battery waste water according to claim 6, characterized in that: In S5, the formula used to calculate the content of each heavy metal in the battery wastewater is as follows: Among them, Q i is the content of each heavy metal i in battery wastewater, in mg / L; q i is the content of each heavy metal i in the mixed resin tablet measured by X-ray fluorescence spectrometer, in ppm; m1 is the mass of adsorption resin, in g; m2 is the mass of gel ion exchange resin, in g; m3 is the mass of mixed resin for tableting, in g; V is the volume of battery wastewater, in L.
Citation Information
Cited By
Transfer and enrichment device and determination method for heavy metals in battery wastewater
WO2026026179A1