By etching P-type deep trenches on the silicon carbide epitaxial layer and forming PN junctions, and filling high-breakdown field strength media, the problem of ignition phenomenon of high-voltage silicon carbide diodes in tests of 1700V and above is solved, and a higher level is achieved pressure resistance and cost reduction effect.
Patent Information
- Application Number
- CN202411042917.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-31
- Publication Date
- 2024-11-15
AI Technical Summary
Silicon carbide high-voltage diodes of 1700V and above are prone to ignition during chip testing, resulting in damage to the chip and test equipment. Existing methods such as using probes to blow N2 to reduce the air pressure cannot effectively avoid this problem.
The P-type deep trench was etched on the silicon carbide epitaxial layer and formed a PN junction by inclination angle injection, filled with silicon dioxide and silicon nitride to improve breakdown field strength, and designed Schottky contact metal and passivation layer to optimize The device structure transfers high electric field to the interior of the epitaxial layer to reduce the risk of ignition.
It effectively avoids the occurrence of ignition of silicon carbide high-voltage diodes during CP testing, reduces product loss costs, and improves the voltage resistance and reliability of the device.
Smart Images

Figure CN118969611A_ABST
Abstract
Description
[0001] The present invention relates to the field of semiconductor technology, and in particular to a silicon carbide high voltage diode and a preparation method thereof. Background Art
[0002] As the third generation wide bandgap semiconductor, silicon carbide has a bandgap width of 3.26ev, which is three times that of traditional silicon-based materials. Silicon carbide devices made of this material have advantages over traditional silicon devices such as high temperature stability, high power density, high efficiency and high frequency resistance. These advantages make silicon carbide devices in many fields such as electric vehicles, renewable energy, power transmission, smart grids, industrial appliances, rail transportation, aerospace, etc. And with the continuous advancement of design structure technology and the continuous reduction of raw material costs, the cost gap between silicon carbide devices and silicon-based devices is getting smaller and smaller, and the application prospects of SiC devices will be broader.
[0003] As a wide bandgap semiconductor, silicon carbide is particularly suitable for high-voltage devices. Currently, 650V, 1200V, and 1700V silicon carbide devices have been used in large quantities in the market, and the share of products with 2000V and above is also increasing. However, such ultra-high voltage products have brought certain difficulties to chip testing. Wafer factory chip testing is also called wafer CP (Chip Probing) testing, which is an electrical test of each chip on the silicon carbide wafer. When the wafer CP test is performed, its reverse voltage will reach the avalanche voltage of the device (generally 1.5 times the designed withstand voltage value of the device). Since the chip edge and the back electrode are equipotential and the silicon carbide diode terminal size is small, the breakdown field strength of the air is also small, about 30KV / CM, and ionization occurs above the diode terminal, and then sparking occurs, damaging the wafer and test equipment. Especially for products with 1700V and above, the JTE (junction terminal extension) terminal structure is generally used to ensure that the terminal size is smaller, which is more prone to sparking, causing chip damage.
[0004] To address this difficulty, the industry generally uses a probe card to blow N2 on the chip surface to reduce the surface pressure of the chip, thereby increasing the air breakdown voltage to avoid sparking. However, this method has basically no effect on silicon carbide high-voltage diodes of 1700V and above. Summary of the invention
[0005] In view of the above problems, the present invention provides a silicon carbide high-voltage diode and a preparation method thereof for avoiding the sparking phenomenon of silicon carbide high-voltage diodes of 1700V and above.
[0006] The technical solution of the present invention is: A method for preparing a silicon carbide high voltage diode comprises the following steps: Step S100, growing a silicon carbide epitaxial layer on a silicon carbide substrate; Step S200, etching a P-type deep trench near the edge of the silicon carbide epitaxial layer through an etching process; Step S300, using an ion implantation process on the top surface of the silicon carbide epitaxial layer, sequentially preparing a P-type doping region 1, a P-type doping region 2, a P-type doping region 3 and a P-type doping region 4 extending downwards respectively; Step S400, forming field oxygen on the top surface of the silicon carbide epitaxial layer by chemical vapor deposition, the field oxygen sequentially passes through the second P-type doping region, the third P-type doping region and the fourth P-type doping region, and then extends to the edge of the device; Step S500, sputtering a layer of metal on the top surface of the silicon carbide epitaxial layer, which passes through the P-type doping region 1 and the P-type doping region 2 in sequence and extends to the top surface of the field oxide, and forming a Schottky contact metal after annealing; Step S600, sputtering a layer of aluminum metal on the Schottky contact metal as an anode lead to form a front thickened metal; Step S700, forming a passivation layer at the device terminal position; Step S800, manufacturing a back ohmic contact electrode on the back side of the silicon carbide substrate, and depositing a thickened metal on the ohmic contact electrode to form a cathode, thereby completing device manufacturing.
[0007] Specifically, in step 300, the P-type doping region 4 is implanted at an inclined angle with an angle range of 4-10 degrees to form a PN junction structure on both sides of the P-type deep trench.
[0008] Specifically, in step S400, the material of the field oxygen is silicon dioxide.
[0009] Specifically, the thickness of the Schottky contact metal in step S500 is in the range of 500 Å to 1500 Å.
[0010] Specifically, the thickness of the front thickened metal in step S600 is 2um-6um.
[0011] Specifically, the passivation layer includes an inorganic passivation layer and an organic passivation layer which are sequentially arranged from bottom to top.
[0012] A silicon carbide high-voltage diode comprises, from bottom to top, a back thickened metal, a back ohmic contact metal, a silicon carbide substrate and a silicon carbide epitaxial layer; The top surface of the silicon carbide epitaxial layer is provided with: A plurality of P-type doped regions 1 are provided, each extending downward from the top surface of the silicon carbide epitaxial layer and arranged at intervals; A second P-type doped region extending downward from the top surface of the silicon carbide epitaxial layer; A third P-type doped region extending downward from the top surface of the silicon carbide epitaxial layer and connected to a side portion of the second P-type doped region; A P-type doped region four extends downward from the top surface of the silicon carbide epitaxial layer, has a U-shaped cross-section, and is spaced apart from the P-type doped region three; Field oxygen is arranged on the top surface of the silicon carbide epitaxial layer, passes through the second P-type doping region, the third P-type doping region and the fourth P-type doping region in sequence, and then extends to the edge of the device; A Schottky contact metal is disposed on the top surface of the silicon carbide epitaxial layer, passes through the P-type doping region 1 and the P-type doping region 2 in sequence, and then climbs to the top surface of the field oxide; A front thickened metal extending upward from a top surface of the Schottky contact metal; The passivation layer extends from the top surface of the field oxide toward the front thickened metal and climbs to the top surface of the front thickened metal.
[0013] Specifically, the passivation layer includes an inorganic passivation layer and an organic passivation layer.
[0014] The present invention forms a P-type deep trench by etching on the silicon carbide epitaxial layer, and forms a PN junction on both sides of the trench by inclined ion implantation. When the device is subjected to reverse high-voltage test, the presence of the deep trench PN junction causes the high electric field to be transferred from the surface of the silicon carbide device to the inside of the silicon carbide epitaxial material. In addition, since the breakdown field strength of silicon dioxide and silicon nitride (3-20MV / cm) is much greater than that of air (about 0.033MV / cm), filling silicon dioxide and silicon nitride in the silicon carbide trench can also increase the anti-sparking ability of the diode. The structural optimization design of the present invention can better avoid the occurrence of sparking during the CP test of the silicon carbide high-voltage diode, and reduce the loss cost of the product. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 is a structural schematic diagram of step S100 of the present invention; Figure 2 is a structural schematic diagram of step S200 of the present invention; Figure 3 is a schematic structural diagram of step S300 of the present invention; Figure 4 is a structural schematic diagram of step S400 of the present invention; Figure 5 is a schematic structural diagram of step S500 of the present invention; Figure 6 is a schematic structural diagram of step S600 of the present invention; Figure 7 is a schematic diagram of the cross-sectional structure after the inorganic passivation layer is prepared; Figure 8 is a schematic diagram of the cross-sectional structure after the organic passivation layer is prepared; Fig. 9 is a schematic diagram of the cross-sectional structure of the back ohmic contact electrode; Fig.10 This is a schematic diagram of the cross-sectional structure after the back side is thickened with metal; In the figure, 1 is a silicon carbide substrate, 2 is a silicon carbide epitaxial layer, 3 is a P-type deep trench region, 4 is a P-type doping region one, 5 is a P-type doping region two, 6 is a P-type doping region three, 7 is a P-type doping region four, 8 is a field oxygen, 9 is a Schottky contact metal, 10 is a front thickened metal, 11 is an inorganic passivation layer, 12 is an organic passivation layer, 13 is a back ohmic contact electrode, and 14 is a back thickened metal. DETAILED DESCRIPTION
[0016] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.
[0017] The following describes an embodiment of the present invention with reference to FIGS. 1 to 10 ; A method for preparing a silicon carbide high voltage diode comprises the following steps: Step S100, growing a silicon carbide epitaxial layer 2 on a silicon carbide substrate 1, referring to Figure 1 As shown; Specifically, the thickness of the silicon carbide epitaxial layer 2 ranges from 5 to 30 um.
[0018] Step S200, etching a P-type deep trench 3 near the edge of the silicon carbide epitaxial layer 2 by dielectric film deposition, glue coating, photolithography, development, etching and other processes; Figure 2 As shown; Specifically, the cross section of the P-type deep trench 3 is a rectangular structure, with a vertical depth of 2um to 5um and a lateral width of 2um to 5um.
[0019] Step S300, using an ion implantation process on the top surface of the silicon carbide epitaxial layer 2, sequentially preparing a P-type doping region 1 4, a P-type doping region 2 5, a P-type doping region 3 6 and a P-type doping region 4 7 extending downwards respectively; Specifically, the dielectric film is deposited, coated, photolithographically, and developed to transfer the ion implantation pattern to the dielectric film, and then the P-type (aluminum ion) ion implantation area is produced through an etching process, wherein the P-type doping area 1 4 and the P-type doping area 2 5 use the same high-temperature ion implantation conditions (the implantation temperature is 450°C-550°C, and the implantation energy is 30KV-450KV). The P-type doping area 3 6 has a lower doping concentration and needs to re-produce the ion implantation window. The P-type doping area 4 7 needs to re-produce the ion implantation window and inject at a tilted angle, generally in the range of 4-10° ( Figure 3At the middle angle α), a PN junction morphology is formed on both sides of the P-type deep trench 3, referring to Figure 3 As shown; Specifically, the P-type doping region 3 6 is a device terminal JTE structure (junction terminal extension), which has the advantages of short terminal structure size and high withstand voltage efficiency, and is particularly suitable for silicon carbide high voltage diodes. Compared with the P-type doping region 1 4, the injection junction depth is deeper and the injection concentration is lower. The principle is to set a lightly doped P-type doping region 3 6 outside the main junction P-type doping region 2 5, and use the extension of the lightly doped P region to form a depletion layer with positive charge in the terminal region, thereby extending the peak electric field, alleviating the electric field concentration effect, and improving the device withstand voltage.
[0020] The doping concentration of the P-type doping region 1 4 is 1e17-1e18, and the depth is 0.6-1um. The benefit is that the device leakage current is reduced when the reverse high voltage is used. The doping concentration of the P-type doping region 2 5 and the P-type doping region 3 6 is 1e15-1e17, and the depth is 0.6-1.2um. The benefit is that a JTE structure is formed to improve the device withstand voltage. The doping concentration of the P-type doping region 4 7 is 1e17-1e18, and the depth is 0.6-1um. The benefit is that during the reverse high voltage test, the high electric field is transferred from the surface of the silicon carbide device to the inside of the silicon carbide epitaxial material to avoid sparking.
[0021] Step S400, a field oxide 8 is formed on the top surface of the silicon carbide epitaxial layer 2 by chemical vapor deposition. The field oxide 8 passes through the P-type doping region 2 5, the P-type doping region 3 6 and the P-type doping region 4 7 in sequence and then extends to the edge of the device. Figure 4 As shown; The material of the field oxygen 8 is silicon dioxide.
[0022] Step S500, a layer of metal is sputtered on the top surface of the silicon carbide epitaxial layer 2, which passes through the P-type doping region 1 4 and the P-type doping region 2 5 in sequence and extends to the top surface of the field oxide 8. After annealing, a Schottky contact metal 9 is formed. The Schottky annealing temperature is generally 400°C-500°C; the thickness of the Schottky contact metal 9 ranges from 500A to 1500A; the metal is generally titanium or molybdenum; refer to Figure 5 As shown; Step S600, sputtering a layer of aluminum metal on the Schottky contact metal 9 as an anode lead to form a front thickened metal 10 with a thickness of 2um-6um; Figure 6 As shown; Step S700, making a passivation layer at the device terminal position, referring to Figure 7 and Figure 8 As shown; The passivation layer extends from the top surface of the front thickened metal 10 to the device terminal, that is, starting from the left side of the terminal and ending at the edge of the chip, in order to protect the front contact metal and silicon carbide epitaxy when bonding the silicon carbide diode.
[0023] The passivation layer includes an inorganic passivation layer 11 and an organic passivation layer 12 arranged in sequence from bottom to top, the purpose of which is to insulate and protect the terminal, isolate water vapor, reduce thermal stress, etc. Figure 7 and Figure 8 shown.
[0024] Step S800, forming a back ohmic contact electrode 13 on the back side of the silicon carbide substrate 1, referring to Fig. 9 and depositing a thickened metal 14 on the ohmic contact electrode 13 to form a cathode to complete the device manufacturing, refer to Fig.10 shown.
[0025] A silicon carbide high-voltage diode comprises, from bottom to top, a back thickened metal 14, a back ohmic contact metal 13, a silicon carbide substrate 1 and a silicon carbide epitaxial layer 2; The top surface of the silicon carbide epitaxial layer 2 is provided with: A plurality of P-type doped regions 4 are provided, extending downward from the top surface of the silicon carbide epitaxial layer 2 and arranged at intervals; The P-type doping region 2 5 extends downward from the top surface of the silicon carbide epitaxial layer 2 . The implantation conditions of the P-type doping region 2 5 and the P-type doping region 1 4 are consistent and can be implanted simultaneously.
[0026] A third P-type doping region 6 extends downward from the top surface of the silicon carbide epitaxial layer 2 and is connected to the side of the second P-type doping region 5; the vertical depth of the third P-type doping region 6 is greater than the vertical depth of the second P-type doping region 5; The silicon carbide epitaxial layer 2 is provided with a P-type doping region 1 4, a P-type doping region 2 5 and a P-type doping region 3 6 extending downward from the top surface, wherein the P-type doping region 1 4 is used to reduce the reverse leakage of the device, and the P-type doping region 2 5 and the P-type doping region 3 6 are used as device terminals and bear a larger reverse voltage value through a shorter terminal size.
[0027] The P-type doping region four 7 extends downward from the top surface of the silicon carbide epitaxial layer 2, has a U-shaped cross-section, and is spaced apart from the P-type doping region three 6; the spacing between the P-type doping region three 6 and the P-type doping region four 7 is in the range of 5-30um, which increases the distance between the internal high electric field and the front metal during the reverse cp test to avoid sparks.
[0028] The P-type deep trench 3 for setting the P-type doping region 47 is located near the edge of the silicon carbide epitaxial layer 2. The purpose of the P-type doping region 47 is to transfer the high electric field from the surface of the silicon carbide device to the inside of the silicon carbide epitaxial material during CP testing, thereby avoiding sparking.
[0029] Field oxide 8, arranged on the top surface of the silicon carbide epitaxial layer 2, sequentially passes through the P-type doping region 2 5, the P-type doping region 3 6 and the P-type doping region 4 7, and then extends to the edge of the device; The purpose of field oxygen 8 is to protect the surface of the epitaxial layer at the silicon carbide terminal during etching and to increase the reliability of the device during operation.
[0030] The Schottky contact metal 9 is arranged on the top surface of the silicon carbide epitaxial layer 2, passes through the P-type doping region 1 4 and the P-type doping region 2 5 in sequence, and then climbs to the top surface of the field oxide 8; A front thickened metal 10 extending upward from the top surface of the Schottky contact metal 9; The passivation layer extends from the top surface of the field oxide 8 toward the front thickened metal 10 , and climbs up to the top surface of the front thickened metal 10 .
[0031] The passivation layer includes an inorganic passivation layer 11 and an organic passivation layer 12 .
[0032] The preparation process of the present invention enables the chip to transfer the surface high electric field strength to a deeper epitaxial layer through the P-type deep trench 3 PN junction when performing reverse high-voltage CP testing, and the high breakdown field strength dielectric filled in the trench is designed and optimized in these two ways to never avoid the sparking phenomenon. The present invention solves the occurrence of the sparking phenomenon without increasing the chip terminal size and changing the wafer CP test machine, thereby reducing the loss cost of the product.
Claims
1. A method for preparing a silicon carbide high voltage diode, characterized in that: The following steps are involved: Step S100, growing a silicon carbide epitaxial layer (2) on a silicon carbide substrate (1); Step S200, etching a P-type deep trench (3) near the edge of the silicon carbide epitaxial layer (2) through an etching process on the silicon carbide epitaxial layer (2); Step S300, using an ion implantation process on the top surface of the silicon carbide epitaxial layer (2), sequentially preparing a P-type doping region 1 (4), a P-type doping region 2 (5), a P-type doping region 3 (6) and a P-type doping region 4 (7) extending downwards respectively; Step S400, forming a field oxygen (8) on the top surface of the silicon carbide epitaxial layer (2) by chemical vapor deposition, wherein the field oxygen (8) sequentially passes through the second P-type doping region (5), the third P-type doping region (6) and the fourth P-type doping region (7), and then extends to the edge of the device; Step S500, sputtering a layer of metal on the top surface of the silicon carbide epitaxial layer (2) that passes through the P-type doping region 1 (4) and the P-type doping region 2 (5) in sequence and then extends to the top surface of the field oxide (8), and annealing to form a Schottky contact metal (9); Step S600, sputtering a layer of aluminum metal on the Schottky contact metal (9) as an anode lead to form a front thickened metal (10); Step S700, forming a passivation layer at the device terminal position; Step S800, manufacturing a back ohmic contact electrode (13) on the back side of the silicon carbide substrate (1), and depositing a thickened metal (14) on the ohmic contact electrode (13) to form a cathode, thereby completing device manufacturing.
2. The method for preparing a silicon carbide high voltage diode according to claim 1, characterized in that: In step 300, the P-type doping region 4 (7) is implanted at an inclined angle, with the angle range being 4-10°, to form a PN junction structure on both sides of the P-type deep trench (3).
3. The method for preparing a silicon carbide high voltage diode according to claim 1, characterized in that: In step S400, the material of the field oxygen (8) is silicon dioxide.
4. The method for preparing a silicon carbide high voltage diode according to claim 1, characterized in that: The thickness of the Schottky contact metal (9) in step S500 is in the range of 500 Å to 1500 Å.
5. The method for preparing a silicon carbide high voltage diode according to claim 1, characterized in that: The thickness of the front thickened metal (10) in step S600 is 2um-6um.
6. The method for preparing a silicon carbide high voltage diode according to claim 1, characterized in that: The passivation layer comprises an inorganic passivation layer (11) and an organic passivation layer (12) which are arranged in sequence from bottom to top.
7. A silicon carbide high voltage diode, prepared by the method for preparing a silicon carbide high voltage diode according to any one of claims 1 to 6, characterized in that: The device comprises, from bottom to top, a back thickening metal (14), a back ohmic contact metal (13), a silicon carbide substrate (1) and a silicon carbide epitaxial layer (2); The top surface of the silicon carbide epitaxial layer (2) is provided with: A plurality of P-type doped regions (4) extending downward from the top surface of the silicon carbide epitaxial layer (2) and arranged at intervals; A second P-type doped region (5) extending downward from the top surface of the silicon carbide epitaxial layer (2); A third P-type doped region (6), extending downward from the top surface of the silicon carbide epitaxial layer (2) and connected to the side of the second P-type doped region (5); A P-type doped region four (7), extending downward from the top surface of the silicon carbide epitaxial layer (2), having a U-shaped cross-section, and spaced apart from the P-type doped region three (6); Field oxygen (8) is arranged on the top surface of the silicon carbide epitaxial layer (2), passes through the second P-type doping region (5), the third P-type doping region (6) and the fourth P-type doping region (7) in sequence, and then extends to the edge of the device; A Schottky contact metal (9) is arranged on the top surface of the silicon carbide epitaxial layer (2), passes through the P-type doping region 1 (4) and the P-type doping region 2 (5) in sequence, and then climbs to the top surface of the field oxide (8); A front thickened metal (10) extending upward from the top surface of the Schottky contact metal (9); The passivation layer extends from the top surface of the field oxide (8) in the direction of the front thickened metal (10), and climbs to the top surface of the front thickened metal (10).
8. The silicon carbide high voltage diode according to claim 7, characterized in that: The passivation layer comprises an inorganic passivation layer (11) and an organic passivation layer (12).