Semiconductor device and manufacturing method thereof

By growing a tungsten carbon nitride layer on the side walls of the interconnect jack of the semiconductor device and selectively protect it, the RC delay problem caused by metal oxide residue is solved, and the performance of the device and the stability of the dielectric layer are maintained.

CN118969723APending Publication Date: 2024-11-15GTA SEMICON CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411037474.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-30
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

In the prior art, metal oxide residues occur during the production process due to the chemical reaction between the etchant and the metal layer, resulting in an increase in the dielectric constant of the interlayer dielectric layer, increasing the RC delay, and affecting device performance.

Method used

The tungsten carbon nitride layer is selectively grown on the side walls of the interconnection socket, and this layer is used as a protective layer to reduce and remove the metal oxides to avoid chemical reactions between the dielectric layers and keep the dielectric constant unchanged.

Benefits of technology

It effectively avoids the increase in RC delay, maintains the performance of semiconductor devices, and prevents impurities from entering through the isolation protection of the tungsten carbonitride layer, ensuring the stability of the dielectric layer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118969723A_ABST
    Figure CN118969723A_ABST
Patent Text Reader

Abstract

According to the semiconductor device and the manufacturing method thereof provided by the invention, before the metal oxide is removed, the tungsten carbonitride is grown on the surface of the side wall of the interconnection jack, and the tungsten carbonitride layer has a selective growth characteristic, that is, the higher the conductivity is, the more difficult the tungsten carbonitride layer grows, so that the tungsten carbonitride layer can effectively grow on the side wall of the interconnection jack; and the surface of the metal layer does not grow or grows a relatively thin thickness. When the metal oxide is reduced and removed, the tungsten carbonitride layer plays a role in isolating and protecting the side wall of the interconnection jack, so that the situation that the k value is increased due to chemical reaction caused by invasion of corresponding impurities into the second interlayer dielectric layer is avoided, finally, the effective k value of the second interlayer dielectric layer is effectively kept, RC delay is prevented from being increased, and the performance of the semiconductor device is effectively kept.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a semiconductor device and a manufacturing method thereof. Background Art

[0002] With the continuous development of the integrated circuit industry, the size of semiconductor devices is getting smaller and smaller, which will also produce resistance / capacitance delay (RC delay), which will affect the performance of the device.

[0003] In one application scenario, a dielectric material with a low dielectric constant K or ultra-low K is used to reduce RC delay. The low-k or ultra-low-k dielectric material is often used for an interlayer dielectric layer in the interconnect layer manufacturing process.

[0004] For example, when making an interconnection layer in an interlayer dielectric layer above the current layer, a plug hole is first formed in the interlayer dielectric layer to expose the metal layer in the current layer, and then the interconnection layer is filled in the plug hole. However, in the process of making the plug hole, the through hole is made by etching. When etching to the metal layer, the etchant reacts chemically with the metal layer to produce metal oxides. These metal oxides remain on the surface of the metal layer and affect the performance of electrical signal transmission in subsequent devices.

[0005] Therefore, in the related art, it is necessary to remove the residual metal oxides before filling the interconnect layer. However, in the process of removing the residual metal oxides, a chemical reaction occurs on the surface of the interlayer dielectric layer, resulting in an increase in the k value of the interlayer dielectric layer and an increase in RC delay.

[0006] Therefore, how to solve the problem of RC delay growth is a topic that the industry generally considers.

[0007] It should be noted that the information disclosed in the above background technology section is only used to enhance the understanding of the background of the present invention, and therefore may include information that does not constitute the prior art known to ordinary technicians in the field. Summary of the invention

[0008] In view of the problems in the prior art, the purpose of the present invention is to provide a semiconductor device and a manufacturing method thereof, which overcomes the technical problem of RC delay of semiconductor devices in the prior art.

[0009] The present disclosure provides a method for manufacturing a semiconductor device, which includes:

[0010] Providing a semiconductor substrate, on which a first interlayer dielectric layer and a metal layer formed in the first interlayer dielectric layer are formed;

[0011] forming a second interlayer dielectric layer on the first interlayer dielectric layer and the metal layer;

[0012] Etching an interconnection plug in the second interlayer dielectric layer, wherein the interconnection plug exposes the metal layer and forms residual metal oxide on the surface of the metal layer;

[0013] selectively growing a tungsten carbonitride layer on the sidewalls of the interconnection plug;

[0014] Based on the tungsten carbonitride layer as protection, the metal oxide is reduced and removed;

[0015] After the metal oxide is removed by reduction, a first interconnection layer is filled in the interconnection plug.

[0016] In some embodiments, the metal layer is a second interconnect layer or a contact plug, and the contact plug is electrically connected to an active device on the semiconductor substrate.

[0017] In some embodiments, the thickness of the tungsten carbonitride layer is not less than

[0018] In some embodiments, during the selective growth of the tungsten carbonitride layer on the sidewall of the interconnection plug, a reaction precursor containing carbon and tungsten and ammonia are used, the reaction temperature is 350-460° C., and the electric power is 400-600W.

[0019] In some embodiments, the semiconductor device manufacturing method further includes:

[0020] Before the interconnection hole is filled with the first interconnection layer, an adhesion barrier layer is formed on the sidewall and the bottom wall of the interconnection hole, and the adhesion barrier layer covers the metal layer and the tungsten carbonitride layer.

[0021] In some embodiments, the adhesion barrier layer is tantalum nitride or titanium nitride.

[0022] In some embodiments, filling the first interconnect layer in the interconnect plug includes:

[0023] growing a seed layer on a surface of the adhesion barrier layer;

[0024] A metal body layer is filled in the interconnection plug hole, the metal body layer covers the seed crystal layer and together with the seed crystal layer constitutes the first interconnection layer.

[0025] In some embodiments, the metal oxide is subjected to reduction removal, comprising:

[0026] The metal layer is bombarded with hydrogen-containing plasma to reduce and remove the metal oxide.

[0027] The present disclosure also provides a semiconductor device, comprising:

[0028] A semiconductor substrate, on which a first interlayer dielectric layer and a metal layer located in the first interlayer dielectric layer are formed;

[0029] a second interlayer dielectric layer located on the first interlayer dielectric layer and the metal layer;

[0030] An interconnection plug located in the second interlayer dielectric layer, a tungsten carbonitride layer located on the sidewall of the interconnection plug, and a first interconnection layer filled in the interconnection plug, the tungsten carbonitride layer is located between the sidewall of the interconnection plug and the first interconnection layer, and the metal layer is located below the first interconnection layer and electrically connected to the first interconnection layer.

[0031] In some embodiments, the thickness of the tungsten carbonitride layer is greater than

[0032] The semiconductor device and the manufacturing method thereof of the present invention have the following advantages:

[0033] In the embodiment of the present disclosure, before removing the metal oxide, tungsten carbonitride is first grown on the surface of the side wall of the interconnection hole. The tungsten carbonitride layer has a selective growth characteristic, that is, the stronger the conductivity, the less likely it is to grow, so it can effectively grow on the side wall of the interconnection hole, and will not grow or grow a relatively thin thickness on the surface of the metal layer. When the metal oxide is reduced and removed, the tungsten carbonitride layer plays an isolating and protective role on the side wall of the interconnection hole, preventing the second interlayer dielectric layer from being invaded by the corresponding impurities and chemically reacting, resulting in an increase in the k value, and ultimately effectively maintaining the effective k value of the second interlayer dielectric layer, avoiding an increase in RC delay, and effectively maintaining the performance of the semiconductor device. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] Other features, objectives and advantages of the present invention will become more apparent from a reading of the detailed description of non-limiting embodiments made with reference to the following accompanying drawings.

[0035] Figure 1 A flow chart showing a method for manufacturing a semiconductor device according to an embodiment of the present disclosure.

[0036] Figure 2-Figure 8 Demonstrate an implementation method using Figure 1 The semiconductor device manufacturing method shown is a structural diagram of each stage when manufacturing a semiconductor device. DETAILED DESCRIPTION

[0037] Example embodiments will now be described more fully with reference to the accompanying drawings. However, example embodiments can be implemented in many forms and should not be construed as limited to the examples set forth herein; rather, these embodiments are provided so that the present invention will be more comprehensive and complete and fully convey the concepts of the example embodiments to those skilled in the art. The described features, structures, or characteristics may be combined in any suitable manner in one or more embodiments.

[0038] In addition, the accompanying drawings are only schematic illustrations of the present invention and are not necessarily drawn to scale. The same reference numerals in the figures represent the same or similar parts, and their repeated description will be omitted. Some of the block diagrams shown in the accompanying drawings are functional entities and do not necessarily correspond to physically or logically independent entities. These functional entities can be implemented in software form, or implemented in one or more hardware modules or integrated circuits, or implemented in different networks and / or processor devices and / or microcontroller devices.

[0039] The flowcharts shown in the accompanying drawings are only exemplary and do not necessarily include all the steps. For example, some steps may be decomposed, while some steps may be combined or partially combined. Therefore, the actual execution order may be changed according to the actual situation.

[0040] Figure 1 The semiconductor device manufacturing method of the present disclosure is shown as follows: Figure 1 As shown, the semiconductor device manufacturing method includes but is not limited to the following steps:

[0041] Step 110: providing a semiconductor substrate, on which a first interlayer dielectric layer and a metal layer formed in the first interlayer dielectric layer are formed;

[0042] Step 120: forming a second interlayer dielectric layer on the first interlayer dielectric layer;

[0043] Step 130: etching interconnection plugs in the second interlayer dielectric layer, wherein the interconnection plugs expose the metal layer, and residual metal oxide is formed on the surface of the metal layer;

[0044] Step 140: selectively growing a tungsten carbonitride layer on the sidewall of the interconnection plug;

[0045] Step 150: Based on the tungsten carbonitride layer as protection, the metal oxide is reduced and removed;

[0046] Step 160: After the metal oxide is removed by reduction, a first interconnection layer is filled in the interconnection hole.

[0047] In the embodiment of the present disclosure, before removing the metal oxide, a tungsten carbonitride (WCN) layer is first grown on the surface of the side wall of the interconnection hole. The tungsten carbonitride layer has a selective growth characteristic, that is, the stronger the conductivity, the less likely it is to grow, so it can effectively grow on the side wall of the interconnection hole, and will not grow or grow a relatively thin thickness on the surface of the metal layer. When the metal oxide is reduced and removed, the tungsten carbonitride layer plays an isolating and protective role on the side wall of the interconnection hole, preventing the second interlayer dielectric layer from being invaded by the corresponding impurities and chemically reacting, resulting in an increase in the k value, and ultimately effectively maintaining the effective k value of the second interlayer dielectric layer, avoiding an increase in RC delay, and effectively maintaining the performance of the semiconductor device.

[0048] Below, the method for manufacturing a semiconductor device provided by the embodiment of the present disclosure is described in detail in conjunction with the structure of the semiconductor device at each stage during the manufacturing process.

[0049] like Figure 2 As shown, a semiconductor substrate 1 is provided, on which a first interlayer dielectric layer 21 and a metal layer 3 formed in the first interlayer dielectric layer 21 are formed.

[0050] In the embodiment of the present disclosure, the semiconductor substrate 1 provides a process operation basis for subsequent processes.

[0051] Optionally, the semiconductor substrate 1 may be a third generation wide bandgap semiconductor material such as silicon carbide or gallium nitride. In other embodiments, the material of the semiconductor substrate 1 may also be other materials such as silicon, germanium, silicon germanium, gallium arsenide or indium gallium, and the semiconductor substrate 1 may also be other types of substrates such as a silicon substrate on an insulator or a germanium substrate on an insulator. The material of the semiconductor substrate 1 may be a material suitable for process requirements or easy to integrate.

[0052] In an optional manner, the metal layer 3 may be a second interconnection layer, which may be a bottom interconnection layer or any non-top interconnection layer above the bottom interconnection layer. If it is a bottom interconnection layer, it is used to connect the contact hole plug below, and the contact hole plug is used to make contact and electrical connection with the active device on the semiconductor substrate. If the metal layer 3 is any non-top interconnection layer above the bottom interconnection layer, it may be a wiring layer or an interconnection plug below the wiring layer.

[0053] In another optional manner, the metal layer 3 may also be a contact hole plug, which is used to electrically connect to an active device (not shown in the figure) on the semiconductor substrate 1. An active device is a functional structure, for example, active devices such as MOS field effect transistors and diodes can be made in the semiconductor substrate 1, and active devices such as resistor structures can also be formed, which are not limited here.

[0054] In the embodiment of the present disclosure, the first interlayer dielectric layer 21 plays an insulating and isolating role, so that the metal layers 3 are insulated and isolated from each other.

[0055] In one embodiment, the first interlayer dielectric layer 21 is made of low-K dielectric material or ultra-low-k dielectric material to reduce the parasitic capacitance between subsequent conductive plugs, thereby reducing RC delay. In an alternative embodiment, the first interlayer dielectric layer 21 may also be made of silicon oxide.

[0056] Taking low-k dielectric materials as an example, SiOH, SiOCH, fluorine-doped silicon dioxide (FSG), boron-doped silicon dioxide (BSG), phosphorus-doped silicon dioxide (PSG), boron-phosphorus-doped silicon dioxide (BPSG), hydrogenated silsesquioxane (HSQ, (HSiO1.5)n) or methyl silsesquioxane (MSQ, (CH3SiO1.5)n) can be selected.

[0057] Taking ultra-low-k dielectric materials as an example, SiOCH containing holes can be selected.

[0058] like Figure 3 As shown, a second interlayer dielectric layer 22 is formed on the first interlayer dielectric layer 21 .

[0059] In an alternative embodiment, the material of the second interlayer dielectric layer 22 may refer to the material of the first interlayer dielectric layer 21 . Figure 3 In the example shown, the second interlayer dielectric layer 22 includes a low-k or ultra-low-k dielectric layer 221, a silicon oxide (SiO2) layer 222 and a titanium nitride (TiN) layer 223 distributed from bottom to top. The titanium nitride layer 223 and the silicon oxide layer 222 can improve the dielectric constant.

[0060] In an alternative manner, the second interlayer dielectric layer 22 may be formed by using a process such as chemical vapor deposition.

[0061] like Figure 4 As shown, an interconnection plug 22 a is etched in the second interlayer dielectric layer 22 , the interconnection plug 22 a exposes the metal layer 3 , and residual metal oxide 31 is formed on the surface of the metal layer 3 .

[0062] In an optional manner, the following specific steps are used to etch the interconnection plug hole 22a in the second interlayer dielectric layer 22:

[0063] A patterned mask layer is formed on the second interlayer dielectric layer 22, wherein the window of the patterned mask layer exposes the position of the interconnection plug hole 22a to be formed;

[0064] The second interlayer dielectric layer 22 is etched based on the patterned mask layer until the metal layer 3 is exposed.

[0065] In this process, when approaching the metal layer 3 , a chemical reaction occurs between the etchant and the metal layer 3 to generate metal oxide 31 , and the metal oxide 31 remains on the surface of the metal layer 3 .

[0066] like Figure 4 In the example shown, the cross section of the interconnection jack 22a is stepped, including a through hole 22a1 at the bottom and a wire groove 22a2 located above the through hole 22a1, and the inner wall of the through hole 22a1 extends upward to the bottom surface of the wire groove 22a2. In one application, one or more through holes 22a1 can be formed under each wire groove 22a2.

[0067] The through hole 22a1 is used to form a plug to connect with the metal layer 3 below, and the wire groove 22a2 is used to form a wiring structure later, and the wiring structure electrically connects multiple plugs below.

[0068] In this case, etching the interconnection plug hole 22a in the second interlayer dielectric layer 22 specifically includes the following steps:

[0069] First, a first patterned mask layer is formed on the second interlayer dielectric layer 22, and a pattern window of the first patterned mask layer defines the position of the through hole 22a1. The second interlayer dielectric layer 22 is etched based on the first patterned mask layer to form a slot;

[0070] removing the first patterned mask layer;

[0071] Next, a second patterned mask layer is formed on the second interlayer dielectric layer 22, and a pattern window of the second patterned mask layer defines a line groove 22a2 to expose the above-mentioned slot, and the line width of the pattern window of the second patterned mask layer is greater than the line width of the pattern window of the first patterned mask layer. The second interlayer dielectric layer 22 is etched based on the second patterned mask layer. In this process, the etchant etches the second interlayer dielectric layer 22 from top to bottom, and also etches the sidewalls and bottom walls of the above-mentioned slot until the slot penetrates downward through the second interlayer dielectric layer 22 to form a through hole 22a1;

[0072] Finally, the second patterned mask layer is removed.

[0073] In this process, since the line width of the pattern window of the second patterned mask layer is greater than the line width of the pattern window of the first patterned mask layer, when the through hole 22a1 is completed, a line groove 22a2 with a larger line width opening is also formed above.

[0074] In an optional manner, the patterned mask layer, the first patterned mask layer and the second patterned mask layer are made of photoresist or hard mask material. Taking photoresist as an example, the patterned mask layer is formed by exposure and development processes.

[0075] Optionally, the hard mask is an inorganic thin film material generated by chemical vapor deposition CVD (Chemical Vapor Deposition) or physical vapor deposition PVD (Physical Vapor Deposition), and its main components can be selected from titanium nitride (TiN), silicon nitride (SiN), silicon oxide (SiO2), etc., which are not limited here.

[0076] like Figure 5 As shown, a tungsten carbonitride layer 4 is selectively grown on the sidewall of the interconnection plug 22a.

[0077] As mentioned above, the growth selectivity of the tungsten carbonitride layer 4 is related to the conductivity of the substrate. The stronger the conductivity, the less likely it is to grow the tungsten carbonitride layer 4. The metal layer 3 has a relatively stronger conductivity than the second interlayer dielectric layer 22, so the tungsten carbonitride layer 4 will basically not grow on the metal layer 3. Even if the tungsten carbonitride layer 4 is grown, its thickness is extremely thin and will not affect the subsequent removal of the metal layer 3.

[0078] Thus, the tungsten carbonitride layer 4 is effectively grown on the sidewalls of the interconnection plug 22a.

[0079] In one embodiment, if the second interlayer dielectric layer 22 has a top TiN layer 223, the conductivity of the TiN layer 223 is weaker than that of the metal layer 3, but has a stronger conductivity than the underlying low-k dielectric layer or ultra-low-k dielectric layer 221, so tungsten carbonitride may also be grown thereon (not shown in the figure).

[0080] In one embodiment, the thickness of the tungsten carbonitride layer 4 is not less than In this way, in the subsequent process of removing the metal oxide 31, the tungsten carbonitride layer 4 can provide sufficient isolation protection to prevent the corresponding impurities from invading the second interlayer dielectric layer 22. The upper limit of the thickness of the tungsten carbonitride layer 4 can be selected according to actual conditions and is not limited here.

[0081] In an optional manner, during the selective growth of the tungsten carbonitride layer 4 on the sidewall of the interconnection plug 22a, a reaction precursor containing carbon and tungsten and ammonia are used, the reaction temperature is 350-460°C, and the electric power is 400-600 W. In this process, the reaction precursor and ammonia are ionized to form plasma (or plasma), and the plasma undergoes a chemical reaction on the sidewall of the interconnection plug 22a to obtain the tungsten carbonitride layer 4.

[0082] A good growth rate can be obtained within the above reaction temperature range, and the above electric power can achieve a faster ionization reaction, thereby obtaining a faster growth rate.

[0083] Combination Figure 5 and Figure 6, based on the tungsten carbonitride layer 4 as protection, the metal oxide 31 is reduced and removed.

[0084] In this process, a reduction method is used to remove the metal oxide. Specifically, the metal layer 3 is bombarded with hydrogen-containing plasma to reduce and remove the metal oxide 31. In this process, the hydrogen-containing plasma reduces the metal oxide 31 to precipitate the metal.

[0085] In this process, the tungsten carbonitride layer 4 isolates and protects the side wall of the interconnection plug 22a, prevents hydrogen-containing plasma from invading the second interlayer dielectric layer 22, prevents H from chemically reacting with carbon (C) in the second interlayer dielectric layer 22, effectively maintains the K value of the second interlayer dielectric layer 22, and avoids the increase of RC delay.

[0086] The gas source used in the process includes hydrogen and some active groups to enhance the reduction reaction of the metal oxide 31.

[0087] like Figure 7 As shown, exemplarily, an adhesion barrier layer 5 is formed on the side wall and the bottom wall of the interconnection plug hole 22a, and the adhesion barrier layer 5 covers the metal layer 3 and the tungsten carbonitride layer 4. The adhesion barrier layer 5 is used to prevent the subsequent first interconnection layer from diffusing into the second interlayer dielectric layer 22 to cause contamination, improve the performance of the interconnection structure, and at the same time provide a good interface state for the formation of the first interconnection layer, so that the first interconnection layer and the adhesion barrier layer 5 have high adhesion.

[0088] In an optional manner, TiN (titanium nitride) or TaN (tantalum nitride) may be selected for the adhesion barrier layer 5. The adhesion barrier layer 5 may be a single-layer structure or a multi-layer structure.

[0089] In an optional manner, the adhesion barrier layer 5 may be formed by using processes such as chemical vapor deposition, physical vapor deposition or atomic layer deposition. In this way, the adhesion barrier layer 5 may cover the surface of the tungsten carbonitride layer 4 in the interconnection plug hole 22a. In another embodiment, the surface of the second interlayer dielectric layer 22 may also be covered, and may be retained or removed.

[0090] like Figure 8 As shown, in the interconnection jack 22a ( Figure 7 As shown in the figure, the first interconnection layer 6 is filled in the interior, so that the first interconnection layer 6 is in contact with the adhesion barrier layer 5.

[0091] In an optional manner, in the interconnection jack 22a ( Figure 7 The first interconnection layer 6 is filled in the interior of the device, and specifically comprises the following steps:

[0092] Growing a seed layer 61 on the surface of the adhesion barrier layer 5;

[0093] A metal body layer 62 is filled in the interconnection plug hole 22 a . The metal body layer 62 covers the seed crystal layer 61 and together with the seed crystal layer 61 , constitutes the first interconnection layer 6 .

[0094] In this embodiment, the seed layer 61 serves as a cathode in the electroplating process for the subsequent formation of the metal body layer 62, and prepares for the subsequent formation of the metal body layer 62. The seed layer 61 can also provide a good interface state for the subsequent formation of the metal body layer 62, which helps to form the metal body layer 62 that is tightly bonded to the seed layer 61, and improves the electromigration of the first interconnect layer 6.

[0095] The seed layer 61 can be a single layer structure or a multi-layer structure consisting of a small grain layer and a large grain layer with different grain diameters. When the multi-layer structure is selected, the small grain layer is below the large grain layer, which can improve the adhesion between the seed layer 61 and the adhesion barrier layer 5.

[0096] Optionally, the seed layer 61 is formed by physical vapor deposition or chemical vapor deposition.

[0097] In this embodiment, the adhesion barrier layer 5 can prevent the Cu in the seed layer 61 and the metal body layer 62 from diffusing into the second interlayer dielectric layer 22 to cause contamination, thereby improving the performance of the interconnect structure. At the same time, the adhesion barrier layer 5 can provide a good interface state for the formation of the seed layer 61, so that the formed seed layer 61 and the adhesion barrier layer 5 have high adhesion.

[0098] In one embodiment, the material of the metal layer 62 is Cu, and the metal layer 62 is formed by physical vapor deposition or electroplating.

[0099] In an optional manner, the method for manufacturing the first interconnection layer 6 may include:

[0100] A seed layer 61 and a metal material layer are sequentially deposited, wherein the seed layer 61 is attached to the surface of the adhesion barrier layer 5 to form the inner wall of the interconnection plug hole 22a and may also cover the second interlayer dielectric layer 22, and the metal material layer fills the interconnection plug hole 22a and is higher than the second interlayer dielectric layer 22;

[0101] The metal material layer is planarized until the metal material layer in the interconnection hole 22 a is flush with the second interlayer dielectric layer 22 . Finally, the remaining metal material layer in the interconnection hole 22 a is used as the metal body layer 62 .

[0102] In one embodiment, the adhesion barrier layer 5, the seed layer 61 and the metal body layer 62 can be manufactured in the same process, and deposited and finally planarized in sequence, so as to improve the process efficiency.

[0103] In one embodiment, chemical-mechanical polishing (CMP) is used for planarization. In actual process operation, the chemical-mechanical polishing process includes multiple chemical-mechanical polishing operation steps.

[0104] In the embodiment of the present disclosure, the first interconnection layer 6 may be a top interconnection layer, a bottom interconnection layer, or any interconnection layer between the top interconnection layer and the bottom interconnection layer, which is not limited herein.

[0105] The present disclosure also provides a semiconductor device, which can be a semiconductor device using Figure 1 The method shown in the figure Figure 8 The semiconductor device shown specifically comprises:

[0106] A semiconductor substrate 1, on which a first interlayer dielectric layer 21 and a metal layer 3 located in the first interlayer dielectric layer 21 are formed;

[0107] A second interlayer dielectric layer 22 located on the first interlayer dielectric layer 21 and the metal layer 3;

[0108] The interconnection plug hole 22a (eg, Figure 7 As shown in the figure), a tungsten carbonitride layer 4 located on the side wall of the interconnection hole 22a and a first interconnection layer 6 filled in the interconnection hole 22a, the tungsten carbonitride layer 4 is located between the side wall of the interconnection hole 22a and the first interconnection layer 6, and the metal layer 3 is located below the first interconnection layer 6 and is electrically connected to the first interconnection layer 6.

[0109] In the embodiment of the present disclosure, the tungsten carbonitride layer 4 only covers the sidewall of the interconnection plug 22a, and provides isolation protection for the second interlayer dielectric layer 22. Referring to the semiconductor device manufacturing method of the above embodiment, the tungsten carbonitride layer 4 is manufactured before the first interconnection layer 6, which can prevent the corresponding substances from invading the second interlayer dielectric layer 22 during the process of removing the metal oxide on the metal layer 3, effectively maintain the k value of the second interlayer dielectric layer 22, avoid the final increase of RC delay, and maintain the device performance.

[0110] In the embodiment of the present disclosure, the thickness of the tungsten carbonitride layer 4 is greater than

[0111] In the embodiment of the present disclosure, an adhesion barrier layer 5 is further formed in the interconnection plug hole 22 a , and the adhesion barrier layer 5 is in contact with the tungsten carbonitride layer 4 and the metal layer 3 .

[0112] In the embodiment of the present disclosure, the first interconnection layer 6 includes a seed layer 61 in contact with the adhesion barrier layer 5 and a metal layer 62 filling the interconnection plug hole 22 a , wherein the seed layer 61 is located between the adhesion barrier layer 5 and the metal layer 62 .

[0113] The above contents are further detailed descriptions of the present invention in combination with specific preferred embodiments, and it cannot be determined that the specific implementation of the present invention is limited to these descriptions. For ordinary technicians in the technical field to which the present invention belongs, several simple deductions or substitutions can be made without departing from the concept of the present invention, which should be regarded as falling within the protection scope of the present invention.

Claims

1. A method for manufacturing a semiconductor device, characterized in that: include: Providing a semiconductor substrate, on which a first interlayer dielectric layer and a metal layer formed in the first interlayer dielectric layer are formed; forming a second interlayer dielectric layer on the first interlayer dielectric layer and the metal layer; Etching an interconnection plug in the second interlayer dielectric layer, wherein the interconnection plug exposes the metal layer and forms residual metal oxide on the surface of the metal layer; selectively growing a tungsten carbonitride layer on the sidewalls of the interconnection plug; Based on the tungsten carbonitride layer as protection, the metal oxide is reduced and removed; After the metal oxide is removed by reduction, a first interconnection layer is filled in the interconnection plug.

2. The method for manufacturing a semiconductor device according to claim 1, wherein: The metal layer is a second interconnect layer or a contact plug, and the contact plug is electrically connected to an active device on the semiconductor substrate.

3. The method for manufacturing a semiconductor device according to claim 1, wherein: The thickness of the tungsten carbonitride layer is not less than 4. The method for manufacturing a semiconductor device according to claim 3, wherein: In the process of selectively growing the tungsten carbonitride layer on the sidewall of the interconnection plug, a reaction precursor containing carbon and tungsten and ammonia are used, the reaction temperature is 350-460° C., and the electric power is 400-600W.

5. The method for manufacturing a semiconductor device according to claim 1, wherein: The semiconductor device manufacturing method further comprises: Before the interconnection hole is filled with the first interconnection layer, an adhesion barrier layer is formed on the sidewall and the bottom wall of the interconnection hole, and the adhesion barrier layer covers the metal layer and the tungsten carbonitride layer.

6. The method for manufacturing a semiconductor device according to claim 5, characterized in that: The adhesion barrier layer is tantalum nitride or titanium nitride.

7. The method for manufacturing a semiconductor device according to claim 5, wherein: The step of filling the first interconnection layer in the interconnection hole comprises: growing a seed layer on a surface of the adhesion barrier layer; A metal body layer is filled in the interconnection plug hole, the metal body layer covers the seed crystal layer and together with the seed crystal layer constitutes the first interconnection layer.

8. The method for manufacturing a semiconductor device according to claim 1, wherein: The metal oxide is reduced and removed, comprising: The metal layer is bombarded with hydrogen-containing plasma to reduce and remove the metal oxide.

9. A semiconductor device, characterized in that: include: A semiconductor substrate, on which a first interlayer dielectric layer and a metal layer located in the first interlayer dielectric layer are formed; a second interlayer dielectric layer located on the first interlayer dielectric layer and the metal layer; An interconnection plug located in the second interlayer dielectric layer, a tungsten carbonitride layer located on the sidewall of the interconnection plug, and a first interconnection layer filled in the interconnection plug, the tungsten carbonitride layer is located between the sidewall of the interconnection plug and the first interconnection layer, and the metal layer is located below the first interconnection layer and electrically connected to the first interconnection layer.

10. The semiconductor device according to claim 9, characterized in that The thickness of the tungsten carbonitride layer is greater than