Method for manufacturing metal oxide semiconductor field effect transistor and metal oxide semiconductor field effect transistor
By forming a layered dielectric structure on the contact trench of the MOSFET and using isotropic etching technology to control the taper ratio of the contact trench, the problems of contact stability and reliability in small-sized semiconductor devices are solved, and the MOSFET is improved Stability and stress resistance.
Patent Information
- Application Number
- CN202411063944.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2017-09-11
- Filing Date
- 2018-09-11
- Publication Date
- 2024-11-15
AI Technical Summary
When manufacturing metal oxide semiconductor field effect transistors (MOSFETs), especially vertical power MOSFETs, pose challenges in forming stable contacts and improving reliability in small-sized semiconductor devices, especially due to the taper ratio of the contact trench It is difficult to control, resulting in cracks or cracks in the device during stress test, affecting its function.
By forming a layered dielectric structure on the side walls and bottom walls of the contact trench, and ions are implanted into the semiconductor body using isotropic etching technology to form a contact trench, thereby controlling the taper ratio of the contact trench to be within 2.5. , ensure ohmic contact with the source region and reduce the risk of cracks during the manufacturing process.
The contact structure is more reliably formed in a small-sized semiconductor device, which improves the stability and reliability of the MOSFET, reduces the risk of functional deterioration caused by ion diffusion, and enhances the stress resistance of the device.
Smart Images

Figure CN118969846A_ABST
Abstract
Description
[0001] This application is a divisional application. The name of the invention of the parent application is “Method for manufacturing metal oxide semiconductor field effect transistor and metal oxide semiconductor field effect transistor”. The application date is September 11, 2018, and the application number is 201811056173.X. Technical Field
[0002] Embodiments of the present invention relate to semiconductor MOSFET (Metal Oxide Semiconductor Field Effect Transistor), and more particularly, to vertical power MOSFET and a method for manufacturing the same. Background Art
[0003] Semiconductor transistors, particularly field effect controlled switching devices such as metal oxide semiconductor field effect transistors (MOSFETs) or insulated gate bipolar transistors (IGBTs), have been used in a variety of applications, including but not limited to use as switches in power supplies and power converters, electric vehicles, air conditioners, and even stereo systems. In particular, with respect to power devices capable of switching large currents and / or operating at higher voltages, it is generally desirable to have a low on-state resistance Ron and a high breakdown voltage U bd .
[0004] In order to achieve low on-state resistance Ron and high breakdown voltage U bd , developed a charge compensation semiconductor device. The compensation principle is based on the mutual compensation of charges in the n-doped region and the p-doped region (which are also often referred to as n-doped column region and p-doped column region) in the drift region of the vertical MOSFET.
[0005] There is a continuous progress to reduce the dimension(s) on semiconductor devices, not just for cost reasons. However, the requirements for reliably producing devices tend to increase with shrinking values of, for example, the lateral width and pitch of MOSFET cell, respectively. For example, forming contacts between the source metallization of a MOSFET and the source and body regions of the MOSFET cell may pose challenges.
[0006] Therefore, there exists a need for improved MOSFETs and the fabrication of MOSFETs. Summary of the invention
[0007] According to an embodiment of a method for forming a MOSFET, the method includes providing a wafer, the wafer including: a semiconductor body including a first side, a first semiconductor region adjacent to the first side, a second semiconductor region adjacent to the first side and forming a first pn junction with the first semiconductor region, and a third semiconductor region adjacent to the first side and forming a second pn junction with the second semiconductor region; a first dielectric layer arranged on the first side; a gate electrode embedded in the first dielectric layer; and a second dielectric layer arranged on the first dielectric layer. A trench is formed through the first dielectric layer and the second dielectric layer beside the gate electrode. A dielectric spacer is formed at the sidewall of the trench. The trench is extended into the semiconductor body to form a contact trench.
[0008] According to an embodiment of a method for forming a MOSFET, the method includes providing a wafer, the wafer including: a semiconductor body including a first side, a first semiconductor region adjacent to the first side, a second semiconductor region adjacent to the first side and forming a first pn junction with the first semiconductor region, and a third semiconductor region adjacent to the first side and forming a second pn junction with the second semiconductor region; a dielectric structure arranged on the first side and extending to the upper side; a gate electrode embedded in the dielectric structure; a contact trench extending through the dielectric structure into the third semiconductor region and including a bottom wall and a sidewall arranged at the dielectric structure; and a layered dielectric structure covering the bottom wall and the sidewall and having a first layer thickness at the sidewall and a second layer thickness at the bottom wall that is lower than the first layer thickness. Ions are implanted into the semiconductor body through the layered dielectric structure at the bottom wall of the contact trench. At least the upper layer in the layered dielectric structure is removed to expose the bottom wall. This includes performing isotropic etching.
[0009] According to an embodiment of the MOSFET, the MOSFET comprises a semiconductor body, the semiconductor body comprising a first side, a drift region adjacent to the first side, a body region adjacent to the first side and forming a first pn junction with the drift region, and a source region adjacent to the first side and forming a second pn junction with the body region. In a vertical cross section perpendicular to the first side, the MOSFET further comprises: a dielectric structure arranged on the first side and having an upper side; a first gate electrode embedded in the dielectric structure; a second gate electrode embedded in the dielectric structure; and a contact trench arranged between the first gate electrode and the second gate electrode, extending through the dielectric structure and extending at least to the source region. In a horizontal direction, the width of the contact trench has a first value in a first plane defined by the first side, and has a second value of at most about 2.5 times the first value in a second plane defined by the upper side. The first contact structure is arranged on the dielectric structure. The first contact structure comprises an access contact portion arranged in the contact trench and in ohmic contact with the source region.
[0010] Those skilled in the art will recognize additional features and advantages upon reading the following detailed description, and upon viewing the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] The components in the figures are not necessarily to scale, instead emphasis is placed on illustrating the principles of the present invention. In addition, in the various figures, the same reference numerals designate corresponding components. In the drawings: Figure 1 illustrates a vertical cross section through a semiconductor body of a semiconductor device according to an embodiment; Figure 2 illustrates a vertical cross section through a semiconductor body of a semiconductor device according to an embodiment; Figure 3 illustrates a vertical cross section through a semiconductor body of a semiconductor device according to an embodiment; Figure 4 illustrates a vertical cross section through a semiconductor body of a semiconductor device according to an embodiment; Figure 5 illustrates a vertical cross section through a semiconductor body of a semiconductor device according to an embodiment; Figure 6 illustrates a vertical cross section through a semiconductor body of a semiconductor device; and Figures 7 to 15 The diagram shows a vertical cross section through a semiconductor body during a method step of a method according to an embodiment. DETAILED DESCRIPTION
[0012] In the detailed description below, reference is made to the accompanying drawings, which form a part hereof, and in which specific embodiments of the present invention are shown by way of illustration in which they can be put into practice. In this regard, directional terms such as "top", "bottom", "front", "rear", "head", "tail" etc. are used with reference to the orientation of the (multiple) figures being described. Since the components of the embodiments can be positioned in many different orientations, directional terms are used for illustrative purposes and are by no means limiting. It is to be understood that other embodiments may be utilized and structural or logical changes may be made without departing from the scope of the present invention. Therefore, the following detailed description is not obtained in a limiting sense, and the scope of the present invention is limited by the appended claims.
[0013] Reference will now be made in detail to various embodiments, one or more examples of which are illustrated in the various figures. Each example is provided by way of explanation and is not meant to limit the present invention. For example, features illustrated or described as parts of one embodiment may be used in other embodiments or used in combination with other embodiments to produce further embodiments. It is intended that the present invention includes such modifications and variations. Specific language is used to describe each example, which specific language should not be interpreted as limiting the scope of the appended claims. The accompanying drawings are not to scale and are for illustrative purposes only. For clarity, if not otherwise stated, otherwise the same elements or manufacturing steps have been indicated by the same reference numerals in different drawings.
[0014] The term "horizontal" as used in this specification intends to describe an orientation substantially parallel to a first or main horizontal side (typically a corresponding substantially flat surface) of a semiconductor substrate or body. This may be, for example, the surface of a wafer or die.
[0015] The term "vertical" as used in this specification is intended to describe an orientation that is substantially arranged perpendicular to the first surface (i.e., parallel to the normal direction of the first surface of the semiconductor substrate or body). Similarly, the term "horizontal" as used in this specification is intended to describe an orientation that is substantially arranged parallel to the first surface.
[0016] In this specification, the second surface of the semiconductor substrate of the semiconductor body is considered to be formed by the lower surface or backside surface, while the first surface is considered to be formed by the upper surface, front surface or main surface of the semiconductor substrate. Therefore, the terms "above" and "below" as used in this specification describe the relative position of one structural feature to another structural feature taking into account this orientation.
[0017] In this specification, n-doping is referred to as the first conductivity type and p-doping is referred to as the second conductivity type. Alternatively, a semiconductor device can be formed with the opposite doping relationship, so that the first conductivity type can be p-doped and the second conductivity type can be n-doped. Further, some figures illustrate relative doping concentrations by indicating "-" or "+" next to the doping type. For example, "n - ” means a doping concentration that is less than the doping concentration of an “n” doping region, while “n + The "n" doping region has a greater doping concentration than the "n" doping region. However, unless otherwise stated, indicating a relative doping concentration does not mean that doping regions of the same relative doping concentration must have the same absolute doping concentration. For example, two different n + The doping regions can have different absolute doping concentrations. This also applies to, for example, n + Doped regions and p + Doped region.
[0018] The specific embodiments described in this specification relate to but are not limited to the following: field effect semiconductor devices (particularly MOSFETs) and methods for manufacturing the same. In this specification, the terms "semiconductor device" and "semiconductor component" are used synonymously. The field effect semiconductor device is typically a vertical semiconductor device (such as a vertical MOSFET) having a drain metallization arranged on a second surface and a source metallization and an insulated gate electrode arranged on a first surface arranged relative to the second surface. Typically, a MOSFET is a power semiconductor device having an active area with a plurality of MOSFET cells for carrying and / or controlling a load current. Further, a power semiconductor device typically has a peripheral area having at least one edge termination structure at least partially surrounding the active area when viewed from above. However, the field effect semiconductor device may also be an IGBT, particularly a vertical power IGBT.
[0019] The term "power semiconductor device" as used in this specification is intended to describe a semiconductor device on a single chip having high voltage and / or high current switching capabilities. In other words, the power semiconductor device is intended for high currents, typically in the ampere range, and / or voltages of more than about 10 V or even more than about 100 V or about 500 V or about 1000 V or about 3000 V. In this specification, the terms "power semiconductor device" and "power semiconductor component" are used synonymously.
[0020] The term "edge termination structure" as used in this specification is intended to describe a structure that is configured to provide a transition region in a blocking mode in which a high electrical voltage (i.e., a voltage of high absolute value compared to ground, such as a drain voltage around an active region of a semiconductor device) gradually changes to a potential at or near the edge of the device and / or to a reference potential such as ground, a source potential, or a gate potential. The edge termination structure can reduce the field strength around the termination region of a rectifying junction, for example, by extending the electric field lines across the termination region.
[0021] The term "field effect" as used in this specification is intended to describe the formation of a conductive "channel" of the first conductivity type using an electric field as a medium and / or the control of the conductivity and / or shape of the channel in a semiconductor region of the second conductivity type (typically a body region of the second conductivity type) using an electric field as a medium. Due to the field effect, a unipolar current path through the channel region is formed between a source region of the first conductivity type and a drift region of the first conductivity type and / or the unipolar current path through the channel region is controlled. The drift region may be in contact with the drain region. The drift region and the drain region are typically in low-ohmic connection with the drain electrode (drain metallization). The source region is typically in low-ohmic connection with the source electrode (source metallization).
[0022] In the context of this specification, the term "in ohmic connection" is intended to describe that when no voltage or only a small probe voltage is applied to and / or across the semiconductor device, an ohmic current path (e.g., a low-ohmic current path) exists between corresponding elements or parts of a semiconductor device. The terms "in ohmic connection", "in resistive electrical connection", "electrically coupled", and "in resistive electrical connection" are used synonymously in this specification. In the context of this specification, the term "in ohmic contact" is intended to describe that two elements or parts of a semiconductor device are in direct mechanical (physically tight) contact and in ohmic connection.
[0023] The terms "electrically connect" and "electrically connected" describe an ohmic connection between two features.
[0024] In the context of this specification, the term "MOS" (metal oxide semiconductor) should be understood to include the more general term "MIS" (metal insulator semiconductor). For example, the term MOSFET (metal oxide semiconductor field effect transistor) should be understood to include FETs with gate insulators that are not oxides, i.e. the term MOSFET is used in the more general sense of the terms IGFET (insulated gate field effect transistor) and MISFET (metal insulator semiconductor field effect transistor), respectively. The term "metal" for the gate material of a MOSFET should be understood to include or include conductive materials such as, for example, metals, alloys, doped polycrystalline semiconductors and metal semiconductor compounds (such as metal silicides).
[0025] In the context of this specification, the term “gate electrode” intends to describe an electrode which is positioned beside and insulated from the body region and is configured to form and / or control a channel region through the body region.
[0026] The term “pn junction” as used in this specification intends to describe a boundary surface between (directly) adjacent semiconductor regions or semiconductor portions of different conductivity types.
[0027] In the following, embodiments of semiconductor devices and manufacturing methods for forming semiconductor devices are explained mainly with reference to silicon (Si) semiconductor devices. Therefore, a single crystal semiconductor region or layer is typically a single crystal Si region or Si layer. However, it should be understood that the semiconductor body can be made of any semiconductor material suitable for manufacturing semiconductor devices. Examples of such materials include but are not limited to: elemental semiconductor materials such as silicon (Si) or germanium (Ge); IV compound semiconductor materials such as silicon carbide (SiC) or silicon germanium (SiGe); binary, ternary or quaternary III-V semiconductor materials, such as gallium nitride (GaN). For power semiconductor applications, Si, SiC, GaAs and GaN materials are currently mainly used. If the semiconductor body includes a high bandgap material, i.e., a semiconductor material with a bandgap higher than 1eV, such as SiC or GaN having a high breakdown field strength and a high critical avalanche field strength, respectively, the doping of the corresponding semiconductor region can be selected to be higher, which reduces the on-state resistance Ron (also referred to as the on-resistance Ron) in the following text.
[0028] Reference Figure 1 , explaining a first embodiment of a semiconductor device 100. Figure 1 The semiconductor body 40 is shown in a vertical cross section through a semiconductor device 100 which is typically implemented as a MOSFET. The semiconductor body 40 has a first side, a typically flat first surface 101 facing the vertical direction z, and a typically flat second surface (back surface, rear surface) arranged opposite to the first side (first surface) 101. Figure 1 Extends between the second sides of the housing (not shown).
[0029] In a horizontal direction x substantially parallel to the first surface 101, the semiconductor body 40 is bounded by an edge or a cut (e.g. a sawing edge, which is typically at least substantially orthogonal to the first side or the first surface 101). In the following, the edge is also referred to as a lateral edge. However, typically a portion of the active area of the semiconductor device 100 and a portion of the semiconductor body 40 are illustrated separately. Figure 1 The edges are not shown.
[0030] Apart from the contact openings, the dielectric structure 13 may substantially or even completely cover the first side 101 .
[0031] Typically, the active region of the semiconductor device 100 includes a plurality of MOSFET cells, each of which has a gate electrode 12. Figure 1 The segments shown in may correspond to adjacent portions of two MOSFET cells.
[0032] Typically, each of the MOSFET cells typically comprises, at the first side 101 , a gate electrode 12 embedded in a dielectric structure 13 formed on the first side 101 .
[0033] In an exemplary embodiment, each gate electrode 12 is arranged on a corresponding gate dielectric portion 13a of the dielectric structure 13. The gate dielectric portion 13a is arranged between the corresponding gate electrode 12 and the first side 101.
[0034] In embodiments involving n-channel MOSFETs, the semiconductor body typically comprises an n-type drift region 1, a p-type body region 2 forming a first pn junction 14 with the drift region 1, and a source region 3 forming a second pn junction 15 with the body region 2. In embodiments involving p-channel MOSFETs, the doping relationship is reversed.
[0035] In the illustrated embodiment of a vertically diffused MOSFET (VDMOS), the planar gate electrode(s) 12 typically overlap the first and second pn junctions 14 and 15 when viewed from above and in plan view, respectively.
[0036] Further, the drift region 1 , the body region 2 and / or the source region 3 may adjoin (extend to) the first side 101 (in the active region).
[0037] like Figure 1 As shown in FIG. 1 , the contact trench 50 is typically arranged between two gate electrodes 12, also referred to below as first gate electrode 12 and second gate electrode 12, respectively. The contact trench 50 extends through the dielectric structure 13 and to, more typically into, the source region 3 .
[0038] According to an embodiment, the width w of the contact trench 50 in the horizontal direction x has a first value w1 in a first plane defined by the first side 101 and / or the second side (back side of the semiconductor body), and has a second value w2 in a second plane defined by the upper side 103 of the dielectric structure 13, which second value w2 is at most about 2.5 times the first value w1. In the following, the ratio w2 / w1 is also referred to as the taper ratio of the contact trench 50 in the dielectric structure 13 and the widening ratio of the contact trench 50 in the dielectric structure 13, respectively.
[0039] Further, a continuous conductive first contact structure 10 (e.g., a metal contact structure 10) is typically arranged on the dielectric structure 13. The first contact structure 10 may include: an access contact portion 10", which is arranged in the contact trench 50 and is in ohmic contact with the source region 3; and a covering portion 10', which is arranged above the contact trench 50. In the following, the access contact portion 10" is also referred to as a access contact.
[0040] Covering portion 10' may form a source terminal of MOSFET 100. Further, covering portion 10' may at least substantially cover an active area of MOSFET 100. As shown in FIG.
[0041] Furthermore, the second contact structure ( Figure 1 The first contact structure (not shown) can be arranged on the dielectric structure 13, and the second contact structure typically forms a gate terminal and a gate pad that are ohmically connected to the gate electrode, respectively. In the following, the first contact structure and the second contact structure are also referred to as the source contact structure 10 and the gate contact structure, respectively.
[0042] The source contact structure 10 may comprise a metal. Likewise, the gate contact structure may comprise a metal. The source terminal 10′ and the gate terminal may even be patterned portions of the same conductive material or conductive material layer. The gate terminal and the source terminal 10′ may be separate portions of a common metal wiring layer or stack of layers, for example due to lithographic patterning.
[0043] As follows about Figure 6 As explained in further detail, using a taper ratio w2 / w1 of the contact trench 50 of 2.5 or less (typically in the range from about 0.8 to 2.5, more typically in the range from about 1 to 1.8) at least substantially reduces the risk of forming a crack line 18 or a fissure 18 in the first contact structure 10 during manufacturing or in subsequent stress tests such as HTGS (high temperature gate stress) and UHAST (unbiased high acceleration stress test). As a result, the MOSFET 100 is more reliably sealed against mobile ions from the outside. Note that mobile ions diffused from the outside into the semiconductor body 40 and / or the dielectric 13 may degrade the function of the MOSFET (e.g., the threshold voltage of the MOSFET).
[0044] Typically, MOSFET 100 has a plurality of contact trenches 50 in dielectric structure 13, each contact trench 50 having a taper ratio of at most 2.5. More typically, no contact trench 50 in dielectric structure 13 has a taper ratio of more than 2.5.
[0045] Reliably manufacturing (multiple) contact trenches 50 having a taper ratio (w2 / w1) of up to 2.5 in a dielectric structure has hitherto been challenging, particularly for aspect ratios of the contact trenches 50 (trench height to average trench width (e.g., (w2+w1) / 2)) of at least 1 or at least 2 and / or for small lateral dimensions, i.e., for contact trenches 50 having a second value w2 of up to about 1 μm, more typically up to about 950 nm.
[0046] The first value w1 may also be defined as the (horizontal) distance between two points in the vertical cross section where the contact trench 50 adjoins the source region 3 and the dielectric structure 13, i.e., points shared by the three regions 3, 12, 50. Further, the second value w2 may also be defined as the horizontal width of the contact trench 50 at the upper end of the contact trench 50 in the vertical cross section.
[0047] The contact groove 50 may have a circular or polygonal shape, for example, a rectangular shape when viewed from above (in a plan view).
[0048] Likewise, the access contact portion 10 ″ may have a circular or polygonal shape, for example a rectangular shape when viewed from above (in a plan view).
[0049] As in Figure 1 As shown in the figure, by means of an optional compensation region 5 arranged below, adjacent to the body region 2 and having the same conductivity type as the body region 2, the MOSFET 100 can be implemented as a compensation semiconductor device, typically as a power compensation semiconductor device having a rated breakdown voltage of at least about 100V.
[0050] In these embodiments, the total number of free electrons provided by the n-type dopant typically substantially matches the total number of free holes provided by the compensation regions 5 and the p-type dopant in the drift portion 1a between the compensation regions 5. Typically, the total number of free electrons provided by the n-type dopant varies by less than 5%, more typically by less than 1%, from the total number of free holes provided by the p-type dopant. Thus, the drift portion 1a and the compensation regions 5 may form a pn compensation structure.
[0051] Furthermore, the n-type drift region 1 may additionally include recombination centers for holes, such as platinum.
[0052] Even further, the drain region (in the exemplary embodiment, n-type) of the first conductivity type is typically Figure 1 ) is provided at the second side of the semiconductor body 40 and between the drift region 1 and the second side.
[0053] Typically, the doping concentration of the drain region is higher than the doping concentration of the drift region 1. Therefore, the switching behavior of the semiconductor device 100 may be improved.
[0054] Furthermore, the drain metallization ( Figure 1 ) is typically arranged on and / or at the second side.
[0055] In embodiments involving an IGBT, instead of a drain region, a collector region 110 of the second conductivity type may be provided.
[0056] Figure 2 The diagram is similar to the above Figure 1 A cross section of a semiconductor device 200 is shown illustrating the semiconductor device 100. The semiconductor device 200 is typically also implemented as a MOSFET.
[0057] However, the contact trench 50 and the access contact portion 10 ″ extend partially through the source region 3 into the body region 2 . Therefore, the latching behavior of the MOSFET 200 can be improved.
[0058] Further, in the transition region between the through-contact portion 10" and the covering portion 10' (e.g. source metallization or terminal) of the contact structure 10 and in the transition region between the sidewall 51 and the upper side 103 of the contact trench 50, respectively, the dielectric structure 13 is configured like a tip or nose 9 in vertical cross section. This may be attributed to the following description of Figures 7 to 15 In an exemplary embodiment, the two prong-like or nose-like structures 9 point upward and are slightly angled toward each other. The prong-like or nose-like structures 9 may have a size in the range of from about 20 nm to about 50 nm, more typically in the range of from about 30 nm to about 40 nm.
[0059] In the illustrated vertical cross section, the interface formed between the sidewall 51 of the contact trench 50 and the adjoining portion of the upper side 103 can be described substantially as a parametric plane curve having a cusp (singular point) in a mathematical sense, at least in the corresponding transition region.
[0060] like Figure 2 As shown in the figure, the vertical distance h (|x-x0|) between the first side 101 and the upper side 103 can decrease as the horizontal distance |x-x0| from the corresponding side wall 51 of the contact groove 50 and / or from the entry contact portion 10" in the adjacent part of the transition zone increases. Here, x0 represents the horizontal coordinate of the upper end of the corresponding (closest) side wall 51 in the Cartesian coordinate system xz used.
[0061] Typically, the vertical distance h(0) of the upper end of the side wall(s) 51 from the first side 101 is greater than the minimum vertical distance h(0) between the first side 101 and the upper side 103. min , typically at least about 10 nm larger.
[0062] The vertical distance h(0) of the upper end of the sidewall(s) 51 is typically at most about 100 nm greater than the smallest vertical distance between the first side 101 and the upper side 103 .
[0063] Furthermore, the vertical distance h(|x-x0|) can reach the minimum value hmin , which is typically a minimum value at a corresponding value of the horizontal distance |x1-x0| which is smaller than the maximum horizontal distance |x3-x0| of the source region 3 in the projection onto the first side 101 .
[0064] Even further, the vertical distance h(|x-x0|) typically decreases only for values of the horizontal distance |x-xo| that are less than about 70 nm, more typically less than 20 nm.
[0065] The illustrated structure may be substantially mirror-symmetric about at least a central vertical axis running through the contact trench 50 .
[0066] Figure 3 A cross-section of a semiconductor device 300 is shown, which is similar to the semiconductor device 300 described above with respect to FIG. Figure 2 The semiconductor device 200 is explained. The semiconductor device 300 is also typically implemented as a MOSFET.
[0067] However, a higher (p-doped) body contact region 4 is arranged between the body region 2 and the access contact 10 ″. Thus, a better ohmic connection can be formed with the access contact 10 ″ and with the body region 2 .
[0068] like Figure 3 As shown in FIG. 5 , a corresponding sidewall dielectric 13s may be arranged at the sidewall 51 of the contact trench 50. This may also be attributed to the manufacturing ensuring a low taper ratio of the contact trench 50.
[0069] The sidewall dielectric 13s may have a layer thickness of at most approximately 10 nm or even at most approximately 5 nm or 2 nm.
[0070] Typically, the sidewall dielectric 13s is made of tetraethyl orthosilicate (TEOS), more typically annealed TEOS.
[0071] Figure 4 The diagram is similar to the above Figure 3 A cross section of a semiconductor device 400 is shown illustrating the semiconductor device 300. The semiconductor device 400 is typically also implemented as a MOSFET.
[0072] However, the source contact structure 10 of the semiconductor device 400 is composed of three conductive layers 10 a , 10 b , and 10 c .
[0073] According to an embodiment, the lower conductive layer 10a arranged at the dielectric structure 13 is a titanium layer, more typically a stacked titanium / titanium nitride (Ti / TiN) layer. An intermediate conductive layer (typically an intermediate tungsten layer 10b) is arranged thereon. The upper conductive layer 10c arranged on the intermediate layer 10b may be made of a metal or an alloy including aluminum, copper and / or silicon.
[0074] For example, the upper conductive layer 10c may be made of aluminum (Al), copper (Cu), or an alloy of aluminum or copper (eg, AlSi, AlCu, or AlSiCu).
[0075] The lower conductive layer 10a may form a barrier layer against aluminum.
[0076] Furthermore, the lower conductive layer 10 a may be relatively thin, and, for example, may have a layer thickness in the range from about 10 nm to about 70 nm.
[0077] The layer thickness of the intermediate layer 10 b is typically greater, for example having a layer thickness in the range from approximately 100 nm to approximately 300 nm.
[0078] With the void 16 formed in the lower portion of the contact trench 50 , the intermediate layer 10 b carries a major portion of the source-drain current passing through the contact trench 50 .
[0079] The layer thickness of the upper layer 10 b (outside the contact trench 50 ) is typically even greater, typically in the range from about 3 micrometers to about 5 micrometers.
[0080] like Figure 4 As shown in the figure, the dielectric structure 13 may also include a lower dielectric layer 13b and gate dielectric portions 13a arranged at the gate electrode(s) 12, in addition to a gate dielectric portion 13a typically made of thermal silicon oxide, silicon nitride or silicon oxynitride. Typically, the lower dielectric layer 13b is made of a dielectric material such as undoped silicate glass (USG).
[0081] Furthermore, the upper dielectric layer 13c may be disposed on the lower dielectric layer 13b. Typically, the upper dielectric layer 13c is made of borophosphosilicate glass (BPSG). Therefore, the manufacturing cost may be reduced compared to a semiconductor device having an upper dielectric layer 13c made of USG.
[0082] For clarity, the optional sidewall dielectric (13s) is typically made of the same material as the lower dielectric layer 13b. Figure 4 Not shown.
[0083] This material combination allows efficient fabrication of reliable semiconductor devices having a desired taper ratio of the contact trench(es) 50 .
[0084] The thickness of the lower dielectric layer 13 b above the gate electrode(s) 12 may be in the range from about 250 nm to about 350 nm.
[0085] The thickness of the upper dielectric layer 13 c over the gate electrode(s) 12 may be in a range from about 1 micron to about 1.5 microns.
[0086] Figure 5 The diagram is similar to the above Figure 4 The semiconductor device 400 is a vertical cross-section of the semiconductor device 401 of the semiconductor device 400 explained in detail. The semiconductor device 401 is typically also implemented as a MOSFET and is as described below with respect to Figures 7 to 15 Explained as made. Figure 5 From a closer inspection, which corresponds to a line drawing in the form of a cross-sectional view obtained using an electron beam microscope, the taper ratio (w2 / w1) of the contact trench 50 in the dielectric structure 13 is about 1.8 and is therefore within the desired range for ensuring that the cover portion 10′ forms a uniform sealing layer over the semiconductor body 40 and the dielectric structure 13. Thus, the semiconductor device 401 is safely protected from the diffusion of ions.
[0087] In contrast, Figure 6 The corresponding cross section of a semiconductor device 600 is shown, obtained similarly to the semiconductor device 401 (however, without protecting the sidewalls of the contact trench 50 with a sidewall dielectric (13s) during fabrication). This results in a greater taper ratio (w2 / w1) of about 3:1 and ultimately in a crack 18 that goes completely through the first contact structure 10 and even slightly into the semiconductor body 40. As a result, the semiconductor device 600 has a high risk of changing its characteristics or even failing during device operation due to the in-diffusion of ions.
[0088] In the following, the above description of the Figures 1 to 4 The method steps of the method for producing semiconductor components 100 to 401 are explained.
[0089] In a first process, a wafer formed of a semiconductor body 40 may be provided, the wafer having a first side 101 and a dielectric structure 13 arranged on the first side 101 and comprising in a vertical cross section two gate electrodes 12 separated from the semiconductor body 40. The semiconductor body 40 may be, for example, a silicon semiconductor body.
[0090] like Figure 7As shown in the figure, the semiconductor body 40 typically includes a first semiconductor region 1 adjacent to the first side 101, a second semiconductor region 2 adjacent to the first side 101 and forming a first pn junction 14 with the first semiconductor region 1, and a third semiconductor region 3 adjacent to the first side 101 and forming a second pn junction 15 with the second semiconductor region 2.
[0091] In embodiments relating to the fabrication of a MOSFET, the first semiconductor region 1 , the second semiconductor region 2 , and the third semiconductor region 3 may form a drift region 1 , a body region 2 , and a source region 3 , respectively.
[0092] Typically, Figure 7 It corresponds only to a small section of a wafer, more typically to a small section of an active area of one semiconductor device 500 among many semiconductor devices to be fabricated in parallel on the wafer level.
[0093] In other words, the provided wafer typically includes a plurality of device regions, wherein each device region includes a plurality of transistor structures (more typically vertical power FET structures, in particular MOSFET structures such as a plurality of VDMOS structures formed in the semiconductor body 40).
[0094] Furthermore, at least the provided active region(s) of the semiconductor body 40 may comprise the active regions as described above with respect to Figure 1 Explain the compensation structure.
[0095] Charge compensation semiconductor devices can be produced using the so-called "multi-epitaxial" process. In this case, an n-doped epitaxial layer is first grown on a highly n-doped substrate, which can be several μm thick and is generally referred to as "buffer epitaxy". In addition to the doping level introduced in the epitaxy step, implantation is used to introduce doping ions into the buffer epitaxy through a mask, where the doping ions are in the first charged position (for example, boron for phosphorus doping). Implantation (either through a mask or on the entire surface) can also be used to apply anti-doping. However, it is also possible to separate the individual epitaxial layers with the required doping. Thereafter, the entire process is repeated as many times as required until an n (multi-epitaxial) layer with sufficient thickness and equipped with charge centers is created. The charge centers are mutually adjusted to each other and are stacked vertically one on top of another. These centers are then mixed with outward thermal diffusion in a fluctuating vertical column to form adjacent p-type charge compensation regions (compensation regions) and n-type charge compensation regions (drift portions). The actual device manufacturing can then be performed at this point.
[0096] Another technique for producing charge-compensated semiconductor devices involves trench etching and compensation with trench filling. The volume for absorbing the voltage is deposited in a single epitaxial step (n-doped epitaxy) on a highly n-doped substrate, so that the thickness corresponds to the total thickness of the multilayer epitaxial structure. Thereafter, deep trenches are etched, which determine the shape of the p-columns (compensation zones). The deep trenches are then filled with p-doped epitaxy that is at least substantially free of crystal defects.
[0097] Both techniques can be used to produce Figures 1 to 5 Explanation of charge compensation semiconductor devices.
[0098] exist Figure 7 In the exemplary embodiment illustrated in , the first dielectric layers 13a, 13b are arranged on and at the first side 101, and the second dielectric layer 13c is arranged on and at the first dielectric layers 13a, 13b, wherein the gate electrode 12 is embedded in the first dielectric layers 13a, 13b.
[0099] The first dielectric layer may be made of only one material. However, the first dielectric layer may also include a lower sublayer forming the gate dielectric layer 13 a and an intermediate dielectric layer 13 b covering at least the gate electrode 12 .
[0100] Providing the wafer may include providing a semiconductor body 40 and forming a gate dielectric layer 13 a at the first side 101 of the semiconductor body 40 .
[0101] In embodiments involving the manufacture of silicon semiconductor devices, the gate dielectric layer 13 a may be formed by thermally oxidizing the semiconductor body 40 at the first side 101 .
[0102] The gate electrode layer 12 may be formed on the gate dielectric layer 13 a , for example, by depositing doped polysilicon.
[0103] Thereafter, the gate electrode layer 12 may be lithographically structured to form the gate electrode 12 .
[0104] Thereafter, USG may be deposited as a conformal layer 13b, for example, on the gate electrode 12 and the gate dielectric layer 12a. In the fabricated semiconductor device 500, the deposited layer 13b typically forms an intermediate dielectric layer 13b of the dielectric structure 13.
[0105] The intermediate dielectric layer 13 b may have a layer thickness in the range from about 250 nm to about 350 nm.
[0106] Afterwards, another dielectric material (such as BPSG) may be deposited to form an upper dielectric layer 13c. Figure 7The resulting structure is shown schematically in FIG.
[0107] The upper dielectric layer 13 c may have a layer thickness in a range from about nanometers to about micrometers, more typically in a range from about 1 micrometer to about 1.5 micrometers.
[0108] Thereafter, trenches 50 ′ may be formed through the second dielectric layer 13 c and the first dielectric layers 13 a , 13 b , for example etched to the first side 101 .
[0109] As in Figure 8 As shown in FIG. 1 , a lithographically structured mask 17 may be used to etch trenches 50 ′ through the first and second dielectric layers 13 a - 13 c .
[0110] The taper ratio of the trench 50 is typically close to 1 or, for example, in a range from about 0.8 to about 1.2, more typically in a range from about 0.9 to 1.1.
[0111] The aspect ratio (height to width) of trench 50 may be in a range from about 0.5 to about 5, more typically in a range from about 0.8 to about 2.
[0112] Thereafter, the mask 17 may be removed.
[0113] Thereafter, dielectric spacers 13 s may be formed at the sidewalls 51 of the trench 50 .
[0114] For this purpose, a material different from that of the second dielectric layer 13c, more typically TEOS, may be deposited as a conformal layer 13s, which is also referred to as dielectric protection layer 13s in the following. Fig. 9 The resulting structure 500 is illustrated in FIG.
[0115] Typically, the dielectric protection layer 13s has a layer thickness in the range from about 10 nm to about 50 nm, more typically in the range from about 20 nm to about 40 nm. For example, the layer thickness of the dielectric protection layer 13s may be about 30 nm.
[0116] Afterwards, the dielectric protection layer 13s may be anisotropically etched to remove the dielectric protection layer 13s from the upper side 103 of the second dielectric layer 13c and the bottom wall 52' of the trench 50'. Fig.10 The resulting structure 500 including the formed dielectric spacers 13s is shown in FIG.
[0117] Thus, a respective tip-like or nose-like structure 9 is formed at the upper end of each of the side walls 51 .
[0118] Thereafter, the trench 50' may be extended into the semiconductor body 40 to form a contact trench 50. This is typically achieved by etching while the sidewalls 51 of the trench 50' are protected by the protection layer 13s. Fig.11 The resulting structure 500 comprising a formed (lower) bottom wall 52 and an adjacent lower sidewall portion 51 ′ of the contact trench 50 in the semiconductor body 40 is shown in FIG.
[0119] Thus, no or at least substantially no change is made to the taper ratio of the trench 50 ′ and the contact trench 50 over the first side 101 , respectively, during the extension of the trench 50 ′.
[0120] Extending trench 50' typically includes anisotropically etching the semiconductor material.
[0121] As in Fig.11 (and Fig.13 ), etching can be performed so that the formed contact trench 50 extends through the third semiconductor region 3 and partially enters the second semiconductor region 2.
[0122] Afterwards, a contact structure 10 may be formed on the second dielectric layer 13c and in the contact trench 50. Fig.12 The resulting structure 501 is shown in FIG. Fig.15 The process for forming the contact structure 10 is explained.
[0123] Prior to forming the contact structure 10, a dielectric stray layer 13s' may typically be deposited as a conformal layer. Fig.13 The resulting structure 500 is shown in FIG.
[0124] Typically, the dielectric stray layer 13s' and the dielectric spacers 13s are made of the same material, or at least of a material that is similar with respect to the isotropic etching performed later.
[0125] The dielectric stray layer 13s′ and the (multiple) dielectric spacers 13s typically form a layered dielectric structure 13s, 13s′ having a first layer thickness L1 at the sidewall 51 above the first side 101 that is higher than a second layer thickness L2 at the bottom wall 52 and the lower sidewall portion 51′ of the contact trench 50 below the first side 101.
[0126] In an exemplary embodiment, the layered dielectric structures 13s, 13s' are respectively composed of a lower layer 13s arranged at the sidewalls 51 and forming dielectric spacers at the sidewall(s) 51, and an upper layer 13s' covering the bottom wall 52, the lower layer 13s and the dielectric structure 13.
[0127] Typically, the lower layer 13s and the upper layer 13s' are respective dielectric oxide layers. For example, the upper layer (dielectric stray layer) 13s' and the lower layer (dielectric spacer) 13s may be made of TEOS.
[0128] The layered dielectric structure 13s, 13s' can be used as a stray mask for implanted ions (eg, aluminum ions). Fig.13 This is illustrated by a dotted arrow.
[0129] According to the embodiment, the above Figures 7 to 11 and Fig.13 The explained process may also be described as providing a wafer, the wafer comprising: a semiconductor body 40, the semiconductor body 40 comprising a first side 101, a first semiconductor region 1 adjacent to the first side, a second semiconductor region 2 adjacent to the first side and forming a first pn junction 14 with the first semiconductor region 1, and a third semiconductor region 3 adjacent to the first side and forming a second pn junction 15 with the second semiconductor region 2; dielectric structures 13a, 13b, 13c, which are arranged at the first side 101 and extend to the upper side 103 of the dielectric structure; a gate electrode 1 2, which is embedded in the dielectric structure 13a, 13b, 13c; a contact trench 50, which extends through the dielectric structure 13a, 13b, 13c into the third semiconductor region 3 beside the gate electrode 12; and side walls 51, which are arranged at the dielectric structures 13a, 13b, 13c; and a bottom wall 52; and a layered structure 13s, 13s′ of a dielectric material covering the bottom wall 52 and the side walls 51 and comprising a first layer thickness at the side walls 51 and a second layer thickness at the bottom wall 52 that is lower than the first layer thickness.
[0130] After the ions are implanted into the semiconductor body 40 through the dielectric stray layer 13s' and the bottom wall 52 of the contact trench 50, a thermal annealing process may be used to activate the implanted ions in the semiconductor material.
[0131] Afterwards, the dielectric stray layer 13s′ may be removed using an isotropic etch (typically a wet chemical etch). In an exemplary embodiment, this results in the semiconductor body 40 being exposed in a bottom portion of the contact trench 50 below the first side 101. Typically, the semiconductor body 40 is exposed at a bottom wall 52 and an adjacent lower sidewall portion 51′ of the contact trench 50 below the first side 101.
[0132] The isotropic etching is typically performed so that the etching rate of the second dielectric layer 13c is at least two times higher, more typically at least five times higher, than the etching rates of the dielectric spacer(s) 13s and the dielectric stray layer 13s'.
[0133] As in Fig.14As shown in the figure, after isotropically etching the dielectric stray layer 13s', the sidewalls 51 may still be covered by a thin remaining portion of the dielectric layer 13s, for example, a remaining portion with a thickness of at most a few nanometers.
[0134] In other embodiments, the dielectric layer (dielectric spacers) 13s is at least substantially removed.
[0135] If the dielectric stray layer 13s' is removed without the sidewalls 51 being protected by the dielectric spacer(s) 13s, the taper ratio is likely to be unfavorably increased. Note that BPSG can have an approximately 10-fold higher etch rate than TEOS and USG. This may result in a susceptibility to external ions such as Figure 6 The structure shown in the figure.
[0136] Afterwards, a contact structure 10 may be formed on the second dielectric layer 13c and in the trench 50. Fig.15 The resulting structure 500 is shown in FIG.
[0137] Typically, the contact structure 10 is formed as a layered structure, as described above. Figure 4 As shown in.
[0138] After optionally cleaning the contact trenches 50 and the exposed surfaces of the dielectric structures 13a, 13b, 13c, one or more conductive layers may be deposited.
[0139] For example, a wet chemical etch such as an HF etch may be used to clean the exposed surfaces.
[0140] Afterwards, a thin titanium layer may typically be deposited as a conformal layer on and at the (cleaned) exposed surface. Due to the annealing typically used later, a titanium silicide layer may be formed between the titanium layer and the semiconductor body 40 .
[0141] Thereafter, a titanium nitride layer may typically be deposited as a conformal layer on and at the titanium nitride layer.
[0142] Thereafter, a tungsten layer may typically be deposited as a conformal layer on and at the titanium nitride layer.
[0143] Thereafter, the alloy may typically be deposited as a conformal layer on and at the tungsten layer.
[0144] The deposited alloy may include aluminum and copper. Additionally, the deposited alloy may include silicon.
[0145] Thereafter, the upper surface of the deposited alloy may be planarized, for example by chemical mechanical polishing.
[0146] Further, the formed covering portion 10 ′ of the contact structure 10 on the first side may be photolithographically structured to form a source terminal and a gate terminal.
[0147] Thereafter, a drain metallization (terminal) may be formed opposite the first contact structure 10 .
[0148] Thereafter, the semiconductor body (wafer) may be separated into individual semiconductor devices, for example by sawing along sawing lines or scribe lines, whereby each semiconductor device has a corresponding lateral edge delimiting the semiconductor device in a horizontal direction substantially parallel to the first side 101 .
[0149] According to an embodiment of a method for manufacturing a MOSFET, the method comprises providing a wafer, the wafer comprising: a semiconductor body 40, the semiconductor body 40 comprising a first side 101, a first semiconductor region 1 adjacent to the first side, a second semiconductor region 2 adjacent to the first side and forming a first pn junction 14 with the first semiconductor region 1, and a third semiconductor region 3 adjacent to the first side and forming a second pn junction 15 with the second semiconductor region 2; a dielectric structure 13a, 13b, 13c extending between the first side 101 and an upper side 103; an embedded The semiconductor body 40 is further processed from the first side 101. The further processing may include implanting ions into the semiconductor body 40 through the layered dielectric oxide 13s, 13s′ and the bottom wall 52 of the contact trench 50. An isotropic oxide etch is used to expose the bottom wall 52 so that the lower dielectric oxide layer 13s is only partially removed, or the oxide etch is stopped if the lower dielectric oxide layer 13s at the sidewall 51 is at least substantially removed.
[0150] According to an embodiment, a field effect semiconductor device includes a semiconductor body, the semiconductor body including a first side, a drift region adjacent to the first side, a body region adjacent to the first side and forming a first pn junction with the drift region, and a source region adjacent to the first side and forming a second pn junction with the body region. In a vertical cross section perpendicular to the first side, the MOSFET further includes: a dielectric structure, which is arranged on the first side and has an upper side; a first gate electrode embedded in the dielectric structure; a second gate electrode embedded in the dielectric structure; and a contact trench, which is arranged between the first gate electrode and the second gate electrode, extending through the dielectric structure and extending at least to the source region. In the vertical cross section, the taper ratio of the contact trench is at most about 2.5. The first contact structure is arranged on the dielectric structure. The first contact structure includes an access contact portion, which is arranged in the contact trench and is in ohmic contact with the source region.
[0151] According to an embodiment, a field effect semiconductor device includes a semiconductor body, the semiconductor body including a first side, a first semiconductor region adjacent to the first side, a second semiconductor region adjacent to the first side and forming a first pn junction with the first semiconductor region, and a third semiconductor region adjacent to the first side and forming a second pn junction with the second semiconductor region. In a vertical cross section perpendicular to the first side, the field effect semiconductor device further includes: a dielectric structure arranged on the first side; a first gate electrode embedded in the dielectric structure; a second gate electrode embedded in the dielectric structure; a contact trench arranged between the first gate electrode and the second gate electrode, extending through the dielectric structure and extending to the third semiconductor region; and a first contact structure arranged on the dielectric structure and / or arranged at the dielectric structure. The first contact structure includes: an access contact portion arranged in the contact trench and in ohmic contact with the third semiconductor region; and a covering portion adjacent to the access contact portion and forming an interface with the dielectric structure outside the contact trench. In a vertical cross section, at least near the sidewalls of the contact trench and the access contact portion, respectively, a vertical distance between the first side and the interface decreases with increasing horizontal distance from the sidewalls of the contact trench and / or from the access contact portion.
[0152] Although various exemplary embodiments of the present invention have been disclosed, it will be apparent to those skilled in the art that various changes and modifications that will achieve some of the advantages of the present invention may be made without departing from the spirit and scope of the present invention. It will be apparent to those skilled in the art that other components that perform the same function may be appropriately substituted. It should be mentioned that the features explained with reference to a particular figure may be combined with features in other figures, even in those cases where this has not yet been explicitly mentioned. Such modifications to the innovative concept are intended to be covered by the appended claims.
[0153] Spatially relative terms such as "below," "under," "below," "above," and "above" are used for ease of description to explain the positioning of one element relative to a second element. These terms are intended to cover different orientations of the device in addition to those depicted in the figures. Further, terms such as "first," and "second," etc. are also used to describe various elements, regions, sections, etc. and are not intended to be limiting. The same terms refer to the same elements throughout the description.
[0154] As used herein, the terms "having," "comprising," "including," and "comprising," etc. are open-ended terms that indicate the presence of stated elements or features but do not exclude additional elements or features. The quantifiers "a," "an," and the pronoun "the" are intended to include the plural as well as the singular, unless the context clearly indicates otherwise.
[0155] With the above range of variations and applications in mind, it should be understood that the present invention is not limited by the foregoing description, nor is it limited by the accompanying drawings. Instead, the present invention is limited only by the following claims and their legal equivalents.
Claims
1. A MOSFET (100), include: - a semiconductor body (40) comprising a first side (101), a drift region (1) adjacent to the first side, a body region (2) adjacent to the first side and forming a first pn junction (14) with the drift region (1), and a source region (3) adjacent to the first side and forming a second pn junction (15) with the body region (2); In a vertical cross section perpendicular to the first side (101), the MOSFET further comprises: - a dielectric structure (13) arranged on the first side (101) and having an upper side (103); - a first gate electrode (12) embedded in the dielectric structure (13); - a second gate electrode (12) embedded in the dielectric structure (13); a contact trench (50) arranged between the first gate electrode (12) and the second gate electrode (12), extending through the dielectric structure (13) and at least to the source region (3), the width (w) of the contact trench (50) having, in a horizontal direction (x), a first value (w1) in a first plane defined by the first side (101) and a second value (w2) in a second plane defined by the upper side (103), the second value (w2) being at most 2.5 times the first value (w1); and - a first contact structure (10) arranged on the dielectric structure (13) and comprising an access contact portion (10") arranged in the contact trench (50) and in ohmic contact with the source region (3); wherein the ratio of the second value to the first value (w2 / w1) is referred to as the taper ratio of the contact trench (50).
2. The MOSFET according to claim 1, in, The second value (w2) is at most 1 μm, wherein the vertical distance (h) between the first side (101) and the upper side (103) decreases with increasing horizontal distance (x-x0) from the side wall (51) of the contact trench (50) and / or from the through contact portion (10"), wherein the vertical distance of the upper end of the side wall (51) from the first side (101) is greater than the minimum vertical distance between the first side (101) and the upper side (103), typically greater than 10 nm, wherein the vertical distance of the side wall from the first side (101) is greater than the minimum vertical distance between the first side (101) and the upper side (103), typically greater than 10 nm, wherein the vertical distance of the upper end of the side wall (51) from the first side (101) is greater than the minimum vertical distance between the first side (101) and the upper side (103), ... The vertical distance of the upper end of (51) is at most 100nm greater than the minimum vertical distance between the first side (101) and the upper side (103), and / or wherein the vertical distance (h) has a lowest value at a value (x1-x0) of the horizontal distance (x-x0), the value (x1-x0) of the horizontal distance (x-x0) being smaller than the maximum distance (x3-x0) of the source region (3) in the projection onto the first side (101), wherein the vertical distance (h) decreases only for values of the horizontal distance (x-x0) that are smaller than 70nm.
3. MOSFET according to claim 2, wherein the second value (w2) is at most 950 nm, and wherein the vertical distance (h) decreases only for values of the horizontal distance (x-x0) that are less than 20 nm.
4. A MOSFET according to claim 1 or 2 or 3, wherein the MOSFET comprises a plurality of MOSFET cells in a vertical cross section, each MOSFET cell comprising a corresponding contact trench (50), the contact trench (50) being arranged between two adjacent gate electrodes (12) and extending through the dielectric structure (13) and at least to the corresponding source region (3), wherein the MOSFET is implemented as a power semiconductor device, and / or wherein the MOSFET is implemented as a compensation semiconductor device.
5. The MOSFET according to claim 1 or 2 or 3, in, The surface in the transition region between the side wall (51) and the upper side (103) and / or in the transition region of the contact structure (10) between the access contact portion (10") and the covering portion (10') of the first contact structure (10) can be described in a vertical cross section essentially as a parametric plane curve including a tip (9).
6. MOSFET according to claim 1 or 2 or 3, wherein the drift region (1) comprises n-type dopants and / or recombination centers for holes.
7. A MOSFET according to claim 1 or 2 or 3, wherein the dielectric structure (13) comprises in a vertical cross section at least one of the following: - a first gate dielectric portion, which is arranged between the first gate electrode (12) and the first side (101); - a second gate dielectric portion, which is arranged between the second gate electrode (12) and the first side (101); - a lower dielectric layer (13b) arranged at the first gate electrode (12) and the second gate electrode (12); - an upper dielectric layer (13c) arranged on the lower dielectric layer (13b); and A sidewall dielectric (13s), which is arranged at the sidewall (51) and has a layer thickness of at most 10 nm.
8. The MOSFET according to claim 1 , wherein the first contact structure ( 10 ) comprises at least one of the following in a vertical cross section: - a lower conductive layer (10a) which forms an interface with the dielectric structure (13) at the upper side (103); - an intermediate conductive layer (10b) arranged on the lower conductive layer (10a); and - an upper conductive layer (10c) arranged on the middle conductive layer (10b).
9. The MOSFET of claim 8, wherein the lower conductive layer (10a) comprises titanium, wherein the intermediate conductive layer (10b) comprises tungsten, and wherein the upper conductive layer (10c) comprises an alloy containing at least one of aluminum, copper and silicon.