Membrane electrode and preparation process thereof

By adopting a three-layer frame structure and cold pressing process, the stress concentration problem caused by different thermal expansion coefficients of the frame and the proton exchange membrane is solved, the performance and preparation efficiency of the membrane electrode are improved, and the bonding strength of GDL is enhanced. Reduces costs and risks of membrane air leakage failure.

CN118970123APending Publication Date: 2024-11-15DALIAN UNIV OF TECH

Patent Information

Application Number
CN202411004578.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-25
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

During the preparation process, the existing membrane electrodes are stress-concentrated due to different thermal expansion coefficients of the frame and the proton exchange membrane, resulting in failure of the membrane electrode; the hot pressing process consumes time and effort, and the GDL bonding speed is slow and easy to fall off; the sealing frame is used to proton exchange membrane Causes shear stress, causing membrane air leakage and failure.

Method used

Adopt a three-layer frame structure, the first double-sided frame is composed of adhesive frame and second frame. The cold pressing process is combined to ensure the asymmetric arrangement of the proton exchange membrane, reduce the number of frames, and prepare the whole process using the cold pressing process to avoid thermal expansion stress and increase GDL bonding strength.

Benefits of technology

The cost of membrane electrode is reduced, the performance and service life of membrane electrodes is improved, the problems of stress concentration and low preparation efficiency are solved, the bonding firmness of GDL is enhanced, and the membrane air leakage failure is avoided.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118970123A_ABST
    Figure CN118970123A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of fuel cells, and discloses a membrane electrode and a preparation process thereof. The membrane electrode is mainly composed of a first double-faced adhesive face frame, a second frame, a GDL and a CCM, the first double-faced adhesive face frame is mainly composed of an upper side adhesive layer, a frame base body and a lower side adhesive layer, the second frame is mainly composed of an anode second frame and a cathode second frame, the GDL is mainly composed of an anode GDL and a cathode GDL, and the CCM is mainly composed of a cathode GDL and an anode GDL. The CCM4 is mainly composed of an anode catalyst layer, a proton exchange membrane and a cathode catalyst layer. The preparation process of the membrane electrode completely adopts a cold pressing process, so that the problem of long time consumption in a heating process and a cooling process in the preparation process of the membrane electrode is solved, and the preparation efficiency of the membrane electrode is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of proton exchange membrane fuel cells, and mainly relates to a membrane electrode and a preparation process thereof. Background Art

[0002] Proton exchange membrane fuel cells are currently the most promising new generation of green energy power systems, which can help solve energy crises and environmental pollution. As the core component of proton exchange membrane fuel cells, membrane electrodes are composed of proton exchange membranes, anode and cathode catalyst layers (Catalyst Coated Membrane, CCM), gas diffusion layers (Gas Diffusion Layer, GDL) and sealing frames on both sides. Structurally, the CCM is in the middle, the sealing frames clamp them, and finally the gas diffusion layers are arranged on both sides. Most of the sealing frames are single-sided double-layer, that is, the membrane electrode has a four-layer frame structure, and the frame surface is coated with hot melt adhesive. The hot melt adhesive of the sealing frame is activated by hot pressing, and it is prepared as a whole with the gas diffusion layer and CCM, thus forming a complete membrane electrode assembly.

[0003] The patent with publication number CN116799267A discloses a membrane electrode preparation process and a membrane electrode. Although it solves the problem of glue overflow during frame membrane packaging, the membrane electrode of this patent is a four-layer frame structure with complex structure and high cost. The inner double-layer frame adopts a hot pressing process, and the outer double-layer adopts a cold pressing process.

[0004] The patent with publication number CN219892211U discloses a fuel cell membrane electrode preparation structure. The membrane electrode obtained in this patent has a double-layer frame structure and adopts a T-shaped gas diffusion layer. It does not need to be pressed together by a dispensing process, which reduces the difficulty of alignment and is conducive to improving the fitting accuracy. However, the T-shaped gas diffusion layer is difficult to process, and it will cause stress concentration on the proton exchange membrane during hot pressing or stacking, thereby damaging the proton exchange membrane.

[0005] In the prior art, most membrane electrode structures are single-sided double-layer, i.e., the membrane electrode has a four-layer frame structure, and each layer of the frame surface is coated with hot melt adhesive, and the hot melt adhesive is solidified by hot pressing or partial hot pressing. The hot melt adhesive itself is solid, which is convenient for packaging and storage. It also has the advantages of simple production process, high added value, high bonding strength, and fast speed. However, most membrane electrodes using hot melt adhesive to seal the frame are symmetrical structures, and there are still the following disadvantages in the preparation process, as follows:

[0006] (1) Since the thickness of the single-sided double-layer or four-layer membrane electrode frame is relatively large, a single hot pressing preparation process or multiple hot pressing preparation processes are used. Due to the different thermal expansion coefficients of the sealing frame and the proton exchange membrane, the single-sided double-layer or four-layer membrane electrode frame will cause the proton exchange membrane to deform during the hot pressing process or cooling process, thereby generating greater stress on the proton exchange membrane of the membrane electrode assembly until the membrane electrode fails.

[0007] (2) In the prior art, the membrane electrode preparation process adopts hot pressing or partial hot pressing technology. During the preparation process, the membrane electrode needs to be heated up, kept warm for a certain period of time after reaching the specified temperature, and then the membrane electrode product is cooled down. This is time-consuming, labor-intensive and inefficient.

[0008] (3) In the prior art, the sealing frame and the GDL are symmetrical structures relative to the CCM. During the hot pressing process of the hollow frame and the anode and cathode GDL, the sealing frame will concentrate the shear stress on the proton exchange membrane at the overlapping boundary of the hollow frame and the proton exchange membrane, eventually causing the membrane to leak and fail.

[0009] (4) The cathode and anode GDLs are bonded to the sealing frame by dispensing or transfer printing, which is slow and easy to fall off. Summary of the invention

[0010] Based on the above background technology, the purpose of the present invention is to provide a membrane electrode and a preparation method thereof in view of the deficiencies in the above-mentioned prior art.

[0011] The technical solution of the present invention:

[0012] 1. A membrane electrode, characterized in that the membrane electrode is mainly composed of a first double-sided adhesive frame 1, a second frame 2, GDL3, and CCM4; the first double-sided adhesive frame 1 is mainly composed of an upper adhesive layer 11, a frame matrix 12, and a lower adhesive layer 13 arranged in sequence from top to bottom; the second frame 2 is mainly composed of an anode second frame 21 and a cathode second frame 22, the outer surfaces of the upper adhesive layer 11 and the lower adhesive layer 13 located at the outer end are respectively covered with the anode second frame 21 and the cathode second frame 22, and the outer surfaces of the upper adhesive layer 11 and the lower adhesive layer 13 located at the inner end are exposed; the first double-sided adhesive frame 1, the anode second frame 21, and the cathode second frame 22 work together to form a three-layer frame electrode structure skeleton; GDL3 is mainly composed of an anode GDL31 and a cathode GDL32, and an installation space is left between the two; the inner ends of the two first double-sided adhesive frames 1 are symmetrically connected from the anode GDL31 and the cathode GDL32. The two ends of DL32 are inserted to ensure that there is a gap between the outer end face of GDL3 and the inner end face of the second frame 2; CCM4 is mainly composed of an anode catalyst layer 41, a proton exchange membrane 42 and a cathode catalyst layer 43 arranged in sequence from top to bottom, the anode catalyst layer 41 and the cathode catalyst layer 43 cover the middle area of ​​the proton exchange membrane 42, and the two ends of the proton exchange membrane 42 are exposed to ensure that the anode catalyst layer 41 is arranged upward; CCM4 is installed in the installation space between the anode GDL31 and the cathode GDL32, and the two ends of the proton exchange membrane 42 are respectively installed on the upper side glue layer 11 of the first double-sided glue frame 1 at both ends to ensure that there is a gap between the cathode catalyst layer 43 and the cathode GDL32, the ends of the anode catalyst layer 41 and the cathode catalyst layer 43 are spaced from the end of the first double-sided glue frame 1, and the ends of the proton exchange membrane 42 are spaced from the ends of the anode GDL31 and the cathode GDL32.

[0013] 2. The membrane electrode according to claim 1 is characterized in that the area where the proton exchange membrane 42 is located is the CCM proton exchange membrane area I, the area where the anode catalyst layer 41 and the cathode catalyst layer 43 are located is the CCM catalyst layer area II, the hollow area of ​​the first double-sided adhesive frame is the hollow area III, the area where the GDL31 and the cathode GDL32 are located is the anode and cathode GDL area IV, and the area between the inner sides of the two second frames 2 is the second frame hollow area V; the size of the CCM catalyst layer area II is smaller than the size of the hollow area III, the size of the CCM proton exchange membrane area I is smaller than the size of the anode and cathode GDL area IV, and the size of the anode and cathode GDL area IV is smaller than the size of the second frame hollow area V, wherein the CCM catalyst layer area II serves as the active area of ​​the fuel cell membrane electrode.

[0014] 3. A method for preparing a membrane electrode, characterized in that the steps are as follows:

[0015] (1) first cutting the first double-sided adhesive frame 1 to form a hollow area III;

[0016] (2) Using cold pressing, the CCM 4 is bonded to the upper adhesive layer 11 of the first double-sided adhesive frame 1, ensuring that the anode catalyst layer 41 of the CCM 4 faces upward, and the CCM catalyst layer area II and the hollow area III are centered, wherein the CCM proton exchange membrane area I and the CCM catalyst layer area II are centered;

[0017] (3) cutting the second frame hollow area V to form an anode second frame hollow area and a cathode second frame hollow area, wherein the second frame hollow area V is larger than the hollow area III;

[0018] (4) Using cold pressing, the anode second frame 21 is bonded to the upper adhesive layer 11 of the first frame 1, and the cathode second frame 22 is bonded to the lower adhesive layer 13 of the first double-sided adhesive frame 1, and the hollow area V of the second frame is centered with the hollow area III;

[0019] (5) The anode GDL31 and the cathode GDL32 are respectively placed in the second frame hollow area V on both sides of the first double-sided adhesive frame 1; the anode GDL31 and the cathode GDL32 are respectively bonded to the upper adhesive layer 11 and the lower adhesive layer 13 of the first double-sided adhesive frame 1 by cold pressing, and the anode and cathode GDL areas IV and the hollow area III are centered.

[0020] The size of CCM catalytic layer region II is less than the size of hollow region III; the size of CCM proton exchange membrane region I is less than the size of anode and cathode GDL regions IV; and the size of the second frame hollow region V is less than the size of CCM proton exchange membrane region I.

[0021] Compared with the prior art, the present invention has the following beneficial effects:

[0022] (1) The first double-sided adhesive frame is a frame substrate with adhesive on both sides, and the second frame is a non-adhesive frame structure. The second frame is not made by transfer coating or other methods. Compared with the four-layer frame, the number of adhesive layers in this structure is reduced by half, the number of frames is reduced by one, and the cost of the membrane electrode can be greatly reduced.

[0023] (2) The membrane electrode is a first double-sided adhesive frame with one side of the adhesive layer bonded to the CCM. The first double-sided adhesive frame is an asymmetric structure relative to the CCM. Compared with the traditional membrane electrode, this structure solves the problem of stress concentration of the proton exchange membrane around the hollow area of ​​the frame caused by the frame clamping the CCM.

[0024] (3) The cold pressing process is first used to compound the first double-sided adhesive frame with the CCM, then to compound the first double-sided adhesive frame with the second frame, and finally to compound the first double-sided adhesive frame with the anode and cathode GDL. The entire preparation process is carried out using the cold pressing process, which solves the problem that the sealing frame causes the proton exchange membrane to deform during the hot pressing process or the cooling process due to the different thermal expansion coefficients of the frames of the membrane electrode components and the proton exchange membrane, thereby causing large internal stress in the proton exchange membrane inside the membrane electrode. This is beneficial to improving the performance of the membrane electrode and its service life.

[0025] (4) The upper and lower adhesive layers of the first double-sided adhesive frame are directly bonded to the cathode GDL and the anode GDL, instead of the GDL point bonding and hot pressing bonding method. The GDL bonding is more firm and not easy to fall off.

[0026] (5) The membrane electrode preparation process uses the cold pressing process, which solves the problem of long heating and cooling processes in the membrane electrode preparation process and improves the efficiency of membrane electrode preparation. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1 It is a schematic diagram of the membrane electrode structure of the present invention.

[0028] Figure 2 It is a schematic diagram of the membrane electrode structure area of ​​the present invention.

[0029] Figure 3 It is a process flow chart of the membrane electrode structure preparation process of the present invention.

[0030] Figure 4 The present invention is a schematic diagram of the membrane electrode structure preparation process Figure 1 .

[0031] Figure 5 The present invention is a schematic diagram of the membrane electrode structure preparation process Figure 2 .

[0032] Figure 6 The present invention is a schematic diagram of the membrane electrode structure preparation process Figure 3 .

[0033] In the figure: 1 first double-sided adhesive frame; 2 second frame; 3 GDL; 4 CCM; 11 upper adhesive layer; 12 frame substrate; 13 lower adhesive layer; 21 anode second frame; 22 cathode second frame; 31 anode GDL; 32 cathode GDL; 41 anode catalyst layer; 42 proton exchange membrane; 43 cathode catalyst layer; Ⅰ CCM proton exchange membrane area; Ⅱ CCM catalyst layer area; Ⅲ hollow area, Ⅳ anode and cathode GDL areas; Ⅴ second frame hollow area; a1, boundary distance between CCM catalyst layer area Ⅱ and hollow area Ⅲ; a2, boundary distance between CCM proton exchange membrane area Ⅰ and hollow area Ⅲ; a3, boundary distance between CCM proton exchange membrane area Ⅰ and anode and cathode GDL area Ⅳ; a4, boundary distance between anode and cathode GDL area Ⅳ and second frame hollow area V. DETAILED DESCRIPTION

[0034] The specific implementation of the present invention is further described below in conjunction with the accompanying drawings and technical solutions.

[0035] The membrane electrode of the present invention is mainly composed of a first double-sided adhesive frame 1, a second frame 2, GDL3, and CCM4, wherein the first double-sided adhesive frame 1 is mainly composed of an upper adhesive layer 11, a frame matrix 12, and a lower adhesive layer 13, the second frame is mainly composed of an anode second frame 21 and a cathode second frame 22, GDL3 is mainly composed of an anode GDL31 and a cathode GDL32, and CCM4 is mainly composed of an anode catalyst layer 41, a proton exchange membrane 42, and a cathode catalyst layer 43.

[0036] The boundary distance a1 between the CCM catalytic layer area II and the hollow area III is limited to between 1 mm and 5 mm, which makes assembly more convenient;

[0037] The boundary distance a2 between the CCM proton exchange membrane area I and the hollow area III is limited to between 3 mm and 10 mm, so the bonding is more firm and less prone to air leakage;

[0038] The boundary distance a3 between the CCM proton exchange membrane region I and the anode and cathode GDL region VI is limited to between 3 mm and 5 mm, so that the bonding is more firm;

[0039] The boundary distance a4 between the cathode and cathode GDL regions IV and the second frame hollow region V is limited to between 0.25 mm and 1 mm;

[0040] The main frame 12 and the second frame 2 of the first double-layer adhesive frame 1 are made of PPS (polyphenylene sulfide), PEN (polyethylene naphthalate), high temperature resistant PET (polyethylene terephthalate), PI (polyimide), and the thickness is between 15um and 25um;

[0041] The adhesive layer 11 of the first double-sided adhesive frame 1 is made of pressure-sensitive adhesive, and the thickness of the adhesive layer is between 5um and 10um;

[0042] The thickness and size of the second frame 2, cathode and anode GDL3, and CCM4 are not constrained;

[0043] The specific implementation method of the preparation process of the membrane electrode structure of the present invention is as follows:

[0044] First, cut the first double-sided adhesive frame to form the first double-sided adhesive frame hollow area III;

[0045] Secondly, the CCM4 is bonded to the upper adhesive layer 11 of the first double-sided adhesive frame 1 by cold pressing, ensuring that the anode catalyst layer 41 of the CCM4 faces upward, and the CCM catalyst layer area II and the hollow area III are centered, wherein the CCM proton exchange membrane area I and the CCM catalyst layer area II are centered;

[0046] Cut the second frame hollow area V again to form the anode second frame hollow area and the cathode second frame hollow area, and the second frame hollow area V is larger than the hollow area III;

[0047] Then, the anode second frame 21 is bonded to the upper adhesive layer 11 of the first frame 1 by cold pressing, and the cathode second frame 22 is bonded to the lower adhesive layer 13 of the first frame 1, and the hollow area V of the second frame is centered with the hollow area III;

[0048] Finally, the cathode GDL31 and the anode GDL32 are respectively placed in the second frame hollow area V on both sides of the first double-sided adhesive frame, and the cathode GDL31 and the anode GDL32 are respectively bonded to the upper adhesive layer 11 of the first frame 1 and the cathode GDL32 is bonded to the upper adhesive layer 13 of the first frame 1 by cold pressing, and the anode and cathode GDL areas IV and the hollow area III are centered.

[0049] The upper adhesive layer 11 and the lower adhesive layer 13 of the first double-sided adhesive frame 1 are not limited to pressure-sensitive adhesives, but may also be in the form of hot-melt adhesives.

[0050] The first double-sided adhesive frame in the membrane electrode structure may also be in the form of an adhesive film, which directly connects the second frame 2, CCM4, and the anode and cathode GDL3 into an integrated structure.

[0051] The present invention innovatively solves the problem that due to the different thermal expansion coefficients of the membrane electrode sub-component frame and the proton exchange membrane, the single-sided double-layer or four-layer frame of the membrane electrode will cause the proton exchange membrane to deform during the hot pressing process or cooling process, thereby generating large internal stress on the proton exchange membrane of the membrane electrode assembly. It solves the problem that in the prior art, the frame and GDL are symmetrical structures relative to the CCM, and the proton exchange membrane will experience stress concentration at the overlapping boundary of the hollow frame and the proton exchange membrane during the hot pressing preparation process of the hollow frame and the anode and cathode GDL. It solves the problem that in the prior art, the membrane electrode preparation process adopts hot pressing or partial hot pressing, and the membrane electrode needs to be heated during the preparation process, and kept warm for a certain period of time after reaching the specified temperature, and the cooling process of the membrane electrode product is completed, which is time-consuming, labor-intensive and inefficient.

[0052] In the membrane electrode preparation process of the present invention, cold pressing technology is used throughout, which can effectively reduce the damage to the CCM proton exchange membrane, has high efficiency and low cost, and is conducive to the commercial-scale quantitative preparation of the membrane electrode.

Claims

1. A membrane electrode, It is characterized in that The membrane electrode mainly comprises a first double-sided adhesive frame (1), a second frame (2), a GDL (3), and a CCM (4); the first double-sided adhesive frame (1) mainly comprises an upper adhesive layer (11), a frame matrix (12), and a lower adhesive layer (13) arranged in sequence from top to bottom; the second frame (2) mainly comprises an anode second frame (21) and a cathode second frame (22); the outer surfaces of the upper adhesive layer (11) and the lower adhesive layer (13) at the outer ends are respectively covered with the anode second frame (21) and the cathode second frame (22); The cathode second frame (22), the upper adhesive layer (11) and the lower adhesive layer (13) are located at the inner end and the outer surface is exposed; the first double-sided adhesive frame (1), the anode second frame (21) and the cathode second frame (22) work together to form a three-layer frame electrode structure skeleton; the GDL (3) is mainly composed of the anode GDL (31) and the cathode GDL (32), and an installation space is reserved between the two; the inner ends of the two first double-sided adhesive frames (1) are symmetrically connected from both sides of the anode GDL (31) and the cathode GDL (32). The CCM (4) is inserted into the anode GDL (3) to ensure that there is a gap between the outer end surface of the GDL (3) and the inner end surface of the second frame (2); the CCM (4) is mainly composed of an anode catalyst layer (41), a proton exchange membrane (42) and a cathode catalyst layer (43) arranged in sequence from top to bottom, the anode catalyst layer (41) and the cathode catalyst layer (43) cover the middle area of ​​the proton exchange membrane (42), and the two ends of the proton exchange membrane (42) are exposed to ensure that the anode catalyst layer (41) is arranged upward; the CCM (4) is installed on the anode GDL (31) In the installation space between the cathode GDL (32), the two ends of the proton exchange membrane (42) are respectively installed on the upper adhesive layer (11) of the first double-sided adhesive frame (1) at the two ends, ensuring that there is a gap between the cathode catalyst layer (43) and the cathode GDL (32), that the ends of the anode catalyst layer (41) and the cathode catalyst layer (43) are spaced from the ends of the first double-sided adhesive frame (1), and that the ends of the proton exchange membrane (42) are spaced from the ends of the anode GDL (31) and the cathode GDL (32).

2. The membrane electrode according to claim 1, It is characterized in that The area where the proton exchange membrane (42) is located is the CCM proton exchange membrane area (I), the area where the anode catalyst layer (41) and the cathode catalyst layer (43) are located is the CCM catalyst layer area (II), the hollow area of ​​the first double-sided adhesive frame is the hollow area (III), the area where the GDL (3)1 and the cathode GDL (32) are located is the anode and cathode GDL area (IV), and the area between the inner sides of the two second frames (2) is the second frame hollow area (V); the size of the CCM catalyst layer area (II) is smaller than the size of the hollow area (III), the size of the CCM proton exchange membrane area (I) is smaller than the size of the anode and cathode GDL area (IV), and the size of the anode and cathode GDL area IV is smaller than the size of the second frame hollow area (V), wherein the CCM catalyst layer area (II) serves as the active area of ​​the fuel cell membrane electrode.

3. A method for preparing a membrane electrode, It is characterized in that Here are the steps: (1) first cutting the first double-sided adhesive frame (1) to form a hollow area (III); (2) using a cold pressing method, bonding the CCM (4) to the upper adhesive layer (11) of the first double-sided adhesive frame (1), ensuring that the anode catalyst layer (41) of the CCM (4) faces upward, and the CCM catalyst layer region (II) and the hollow region (III) are centered, wherein the CCM proton exchange membrane region (I) and the CCM catalyst layer region (II) are centered; (3) cutting the second frame hollow area (V) to form an anode second frame hollow area and a cathode second frame hollow area, wherein the second frame hollow area (V) is larger than the hollow area (III); (4) Using cold pressing, the anode second frame (21) is bonded to the upper adhesive layer (11) of the first frame 1, and the cathode second frame (22) is bonded to the lower adhesive layer (13) of the first double-sided adhesive frame (1), and the second frame hollow area (V) and the hollow area (III) are centered; (5) The anode GDL (31) and the cathode GDL (32) are respectively placed in the second frame hollow area (V) on both sides of the first double-sided adhesive frame 1; the anode GDL (31) and the cathode GDL (32) are respectively bonded to the upper adhesive layer (11) and the lower adhesive layer (13) of the first double-sided adhesive frame (1) by cold pressing, and the anode and cathode GDL areas (IV) and the hollow area (III) are centered.

Citation Information

Patent Citations

  • Membrane electrode packaging process and membrane electrode

    CN116799267A

  • Fuel cell membrane electrode packaging structure

    CN219892211U

Cited By

  • AEM water electrolysis membrane electrode failure diagnosis method

    CN120161101A