Manufacturing method of high-fidelity signal flexible circuit board
By using single-sided copper clad plate and bonding lamination technology in the production of flexible circuit boards, direct signal transmission of heterotopic gold fingers is achieved, which solves the problems of complex processing and signal distortion in the existing technology, and improves signal protection True and reduce costs.
Patent Information
- Application Number
- CN202411026218.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-30
- Publication Date
- 2024-11-15
AI Technical Summary
The existing flexible circuit boards are complex and costly, and are prone to reflection and scattering when signal transmission is easily generated, laser ablation efficiency is low and a lot of toner is generated.
The opening window is made of single-sided copper clad plate, and the external heretic gold fingers are formed through bonding and layering to reduce the production of through holes. The single-sided copper clad plate is used as the grounding copper layer, and signal transmission is achieved through electroplating and covering film to avoid laser light Ablation.
The processing process is simplified, the cost is reduced, the reflection and scattering problems of signal transmission are reduced, the toner problem after laser ablation is avoided, and the signal fidelity is improved.
Smart Images

Figure CN118973147A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of flexible circuit board manufacturing, and in particular to a method for manufacturing a high-fidelity signal flexible circuit board. Background Art
[0002] At present, as the functions of products such as low-altitude aircraft and digital AI video become more and more powerful, the performance requirements for flexible circuit boards such as signal fidelity and reliability are also becoming higher and higher, resulting in the emergence of flexible circuit board designs that require high-fidelity electrical signal transmission.
[0003] For some electronic modules whose electrical signal input end and receiving end are not on the same side, the plug circuit (gold finger) of the flexible circuit board is required to be on the different end and on the different side.
[0004] In the prior art, it is common to use double-sided copper clad laminates to make circuit structures with mutual conduction on both sides. Through two layers of copper layers, conductive holes are made to achieve the effect of non-plane conduction, and a covering film with different coverage areas is attached to the heterodyne to achieve the processing effect of heterodyne gold fingers.
[0005] In addition, it is generally necessary to add an independent grounding copper layer to form an overall three-layer flexible circuit board structure to achieve stable and effective transmission of electrical signals.
[0006] The manufacturing method of the above-mentioned three-layer flexible circuit board is to take a double-sided copper clad laminate, make two-sided copper layer circuits, make conductive holes to make the two-sided circuit layers conductive to form a double-sided board, then take a single-sided copper clad laminate, etch the copper layer, and attach it to the double-sided board, and make ground conductive holes, use laser ablation method to remove the PI layer of the single-sided copper clad laminate covering the gold finger, and finally attach a covering film and perform electrometallurgical processing to form a three-layer flexible circuit board with heterogeneous gold fingers.
[0007] The design and production methods of the prior art mainly have the following problems: (1) A three-layer structure design is adopted, including two conductive layers and one ground layer. It is necessary not only to make a conductive hole between the conductive layer and the ground layer, but also to make a conductive hole between the two conductive layers. The conductive holes of two depths and functions make the processing technology complicated, difficult and costly.
[0008] (2) The double-sided circuit layers rely on the conduction holes to conduct with each other, and the loop signal transmission will inevitably take a detour, which can easily cause problems such as reflection and scattering of signal transmission, resulting in signal disturbance and distortion.
[0009] (3) The laser ablation method is used to remove a large area of the PI layer, which is prone to produce a lot of carbon powder after ablation, which is difficult to remove. In addition, the laser ablation process is inefficient and costly.
[0010] Therefore, in order to solve the problems raised by the above background technology, it is necessary to provide a method for manufacturing a high-fidelity signal flexible circuit board. Summary of the invention
[0011] The present invention aims to solve the problem that the flexible circuit board in the prior art requires comprehensive performance such as high-fidelity signal and convenient processing, and proposes a method for manufacturing a high-fidelity signal flexible circuit board, which comprises the following steps: S10: taking a single-sided copper-clad laminate, making a first circuit pattern, and opening a first through window to form an open window core board, wherein the open window core board includes a first copper layer and a PI layer; S20: taking a copper layer, and laminating the copper layer and the PI layer through an adhesive layer, wherein a region of the copper layer corresponding to the first through window includes a first gold finger pattern; S30: pasting a carrying protective film to the first through window to form a carrying film graphic board; S40: drilling, whole-board electroplating, and manufacturing a second circuit pattern on the carrier film pattern board in sequence to form a via board, wherein the second circuit pattern includes a second gold finger pattern, and the first gold finger pattern and the second gold finger pattern are respectively located at different ends of different surfaces of the copper layer; S50: attaching cover films to both sides of the via plate, tearing off the carrying protective film, and forming a cover film pattern plate; the cover films attached to both sides are provided with second through windows, and the second through windows correspond to the first gold finger pattern and the second gold finger pattern respectively; S60: electrometallizing the cover film graphic board, and performing molding and post-processing to form the high-fidelity signal flexible circuit board.
[0012] Optionally, the first through window is produced by punching.
[0013] Optionally, the first through window is manufactured by manufacturing the first copper layer with a first window pattern, and manufacturing a PI window pattern on the PI layer within the region of the first window pattern to form the first through window.
[0014] Optionally, one side of the first windowing pattern is larger than the PI windowing pattern.
[0015] Optionally, the bonding layer is a solid acrylic adhesive layer or a solid epoxy resin adhesive layer, and a bonding layer through window is opened toward the bonding layer corresponding to the first through window.
[0016] The bonding layer is prepared by taking liquid acrylic glue or liquid epoxy resin glue, screen printing or coating the liquid acrylic glue or liquid epoxy resin glue on the PI layer, and baking and curing.
[0017] Optionally, the load-bearing protective film is a micro-adhesive film.
[0018] Optionally, the micromucosa extends 0.5 mm to 2.0 mm outside the area of the opening window.
[0019] Optionally, the method of pasting the bearing protection film to the first through window further includes: screen printing or coating a photosensitive wet film from an edge area of the bearing protection film to an edge area adjacent to the first copper layer, and curing the film.
[0020] Optionally, after the cover films are attached to both sides of the via plate, the edge area of the first via window is ablated by laser.
[0021] The technical solution of the present invention provides a method for manufacturing a high-fidelity signal flexible circuit board, which uses a single-sided copper layer to replace the double-sided copper-clad laminate of the prior art to manufacture a second circuit pattern, so that the heterogeneous gold fingers on different sides are directly located on the same circuit copper layer, and the signal transmission does not need to pass through the conductive hole, avoiding the manufacture of the conductive hole (drilling, electroplating), thereby effectively reducing the reflection and scattering of the signal transmission, and the disturbance and distortion of the signal; the single-sided copper-clad laminate is made into an opening window, and the grounding copper layer is made, and then bonded with the single-layer copper layer, and there is no need to use a laser ablation method to remove the PI layer, thereby avoiding the problem of excessive carbon powder after ablation and difficulty in removal. Before electroplating, a bearing protective film is affixed to the window pattern to protect the copper layer in the area from being electroplated and increase the support of the flexible circuit board. After electroplating, a covering film is applied for electroplating, and the covering film needs to open a window to expose the first gold finger pattern and the second gold finger pattern to be electroplated. The above technical solution reduces one copper layer, so it is only necessary to make a conductive hole between the single-sided copper layer circuit and the grounding circuit, thereby reducing the processing flow and the processing difficulty. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the structures shown in these drawings without paying creative work.
[0023] Figure 1 It is a schematic diagram of the cross-sectional structure of a high-fidelity signal flexible circuit board in the prior art; Figure 2 A schematic diagram of the process flow of a method for manufacturing a high-fidelity signal flexible circuit board according to the present invention; Figure 3 It is a schematic diagram of the cross-sectional structure of a single-sided copper clad laminate; Figure 4 A schematic diagram of a cross-sectional structure for forming a first window; Figure 5 A schematic diagram of a cross-sectional structure of a first window for making another structure; Figure 6 It is a schematic diagram of the cross-sectional structure of the copper layer and the single-sided copper-clad laminate laminated by the adhesive layer; Figure 7 It is a schematic diagram of the cross-sectional structure of the carrier film graphic board; Figure 8 A schematic diagram of the cross-sectional structure of a covering method of a carrier protective film combined with a photosensitive liquid film; Fig. 9 Schematic diagram of the cross-sectional structure of the via plate; Fig.10 It is a schematic diagram of the cross-sectional structure of a cover film graphic board; Fig.11 This is a schematic diagram of the cross-sectional structure of a high-fidelity signal flexible circuit board.
[0024] Description of Figure Numbers: Label name Label name 10X Prior art flexible circuit board 330 First Gold Finger Graphics 100X Prior art double-sided copper clad laminate 40 Carrier film graphic board 110X Prior art vias 410 Carrying protective film 200X Prior art single-sided copper clad laminate 420 Photosensitive wet film 210X Prior art ground vias 50 Via Plate 300X Prior art covering film 510 Via holes 10 Single-sided copper clad laminate 520 Second Gold Finger Graphic 20 Open window core board 60 Cover Film Graphic Board 200 First window 610 First covering film layer 210 First copper layer 610A Second window A 220 PI layer 620 Second covering film layer 200A Through-the-window 620B Second window B 200B Step-through window 70 High fidelity signal flexible circuit board 30 First window laminate 710 First Gold Finger 310 Copper Layer 720 Second Gold Finger 320 Adhesive layer / / The realization of the purpose, functional features and advantages of the present invention will be further explained in conjunction with embodiments and with reference to the accompanying drawings. DETAILED DESCRIPTION
[0025] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0026] It should be noted that all directional indications in the embodiments of the present invention (such as up, down, left, right, front, back, inside, outside...) are only used to explain the relative position relationship, movement status, etc. between the components in a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication will also change accordingly.
[0027] In addition, in the present invention, descriptions such as "first", "second", etc. are only used for descriptive purposes and cannot be understood as indicating or implying their relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" or "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.
[0028] In addition, the technical solutions between the various embodiments of the present invention can be combined with each other, but it must be based on the fact that ordinary technicians in the field can implement it. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such combination of technical solutions does not exist and is not within the scope of protection required by the present invention.
[0029] See also Figure 1 , Figure 1 The figure is a schematic diagram of the cross-sectional structure of a high-fidelity signal flexible circuit board in the prior art.
[0030] In the prior art, a double-sided copper-clad laminate 100X is used to make a circuit structure with mutual conduction on both sides. Two layers of copper are used to make the prior art via 110X to achieve the effect of non-plane conduction, and a covering film with different covering areas is attached to the heterodyne to achieve the processing effect of the heterodyne gold finger. It is necessary to add an independent grounding copper layer and make the prior art grounding via 210X to form an overall three-layer prior art flexible circuit board 10X to achieve stable and effective transmission of electrical signals.
[0031] The manufacturing method of the prior art flexible circuit board 10X is to take the prior art double-sided copper clad laminate 100X, make two-sided copper layer circuits, make the prior art conductive via 110X, make the two-sided circuit layers conductive, and form a double-sided board, then take the prior art single-sided copper clad laminate 200X, etch the copper layer, and attach it to the double-sided board, and make the prior art grounding conductive via 210X, use the laser ablation method to remove the PI layer of the single-sided copper clad laminate 10 covering the gold finger, and finally attach the prior art covering film 300X, perform electrometallurgical processing, and form the prior art flexible circuit board 10X with a three-layer structure having heterogeneous gold fingers.
[0032] See also Figure 2 , Figure 2 The present invention is a process flow diagram of a method for manufacturing a high-fidelity signal flexible circuit board.
[0033] The manufacturing process of the embodiment of the present invention uses Figure 1 The following will implement the various steps in the process Figure 1 Each step in the process is further explained step by step.
[0034] The production method comprises the following steps: See also Figure 3 and Figure 4 , Figure 3 This is a schematic diagram of the cross-sectional structure of a single-sided copper clad laminate. Figure 4 A schematic diagram of the cross-sectional structure for forming the first window.
[0035] Step S10: A single-sided copper clad laminate 10 is taken, and a first through window 200 is opened to form an open window core board 20 . The open window core board 20 includes a first copper layer 210 and a PI layer 220 .
[0036] Optionally, the first through window 200 is manufactured by punching to form a through through window 200A, and the PI layer 220 and the copper layer 210 of the single-sided copper clad laminate 10 are punched at the same time, which makes the processing more convenient.
[0037] See also Figure 5 , Figure 5 A schematic diagram of the cross-sectional structure of a first window for making another structure.
[0038] Optionally, the first through window 200 is manufactured as follows: a first window pattern is manufactured on the first copper layer 210, and a PI window pattern is manufactured on the PI layer 220 within the area of the first window pattern to form the first through window 200, wherein one side of the first window pattern is larger than the PI window pattern, generally larger than 20 μm to 50 μm; the pattern of the first window 200 and the pattern of the PI window form a stepped through window 200B, which can prevent glue overflow at the stepped position and facilitate the subsequent attachment of the surface covering film to completely cover the surface copper layer, thereby forming a buffer section of the gold finger.
[0039] The first through window 200 is opened in the single-sided copper clad laminate 10, and there is no need to use a laser ablation method to remove the PI layer 220, thereby avoiding the problem of excessive carbon powder after ablation and difficulty in removal.
[0040] The first copper layer 210 is a grounding copper layer, the first through window 200 is an exposed area formed by post-processing and bonding with the copper layer 310, and the open window core board 20 is a grounding and supporting layer of the double-sided flexible circuit board formed by subsequent processing in this embodiment.
[0041] See also Figure 6 , Figure 6 It is a schematic diagram of the cross-sectional structure of the copper layer 310 and the single-sided copper clad laminate 10 being overlapped by the adhesive layer 320 .
[0042] Step S20: Take a copper layer 310 which is a single layer of pure copper foil, and overlap the copper layer 310 with the PI layer 220 of the single-sided copper clad laminate 10 through an adhesive layer 320 to form a first through-window laminate 30 . The area of the copper layer 310 corresponding to the first through-window 200 includes a first gold finger pattern 330 .
[0043] Optionally, the adhesive layer 320 is a solid acrylic adhesive layer or a solid epoxy resin adhesive layer, and an adhesive layer through-window is opened toward the adhesive layer 320 corresponding to the first through-window 200; the position patterns of the adhesive layer through-window and the first through-window 200 correspond to each other, and the adhesive layer 320 with the opened window is placed between the single-sided copper clad laminate 10 with the pattern already made and the copper layer 310, and the three layers are stacked and hot-pressed into a board.
[0044] Optionally, the bonding layer 320 may also be made of liquid glue, and the single-sided copper clad laminate 10 and the copper layer 310 are overlapped and bonded. The bonding layer 320 is made by taking liquid acrylic glue or liquid epoxy resin glue, screen printing or coating the liquid acrylic glue or liquid epoxy resin glue on the PI layer 220, and baking and curing.
[0045] The thickness of the bonding layer 320 is 10 μm to 25 μm. Since the PI material is highly inert, it is difficult to directly bond with the copper layer 310 during hot pressing. Therefore, the bonding layer 320 is used to achieve good interlayer bonding. Before bonding, the PI layer 220 is plasma treated to form a surface with a certain roughness and activity to facilitate bonding of the bonding layer 320.
[0046] Since the first through window 200 is made on the single-sided copper clad laminate 10, and the adhesive layer 320 is also opened (corresponding to the first through window 200), after hot pressing into a board, the position of the copper layer 310 corresponding to the first through window 200 is exposed, and the exposed area is the first gold finger pattern 330 area.
[0047] See also Figure 7 , Figure 7 It is a schematic diagram of the cross-sectional structure of the carrier film graphic board.
[0048] Step S30: A carrying protective film 410 is attached to the first through window 200 to form a carrying film graphic plate 40 .
[0049] That is, a load-bearing protective film is attached to the surface of the copper layer 310 corresponding to the first through window 200; since the position of the first through window 200 is the gold finger pattern area, electroplating processing is not required. The load-bearing protective film is attached to this area, which can increase the hardness of the copper layer 310 in the subsequent electroplating, and is used to provide a load-bearing effect, and prevent the exposed copper in the open window area from chemical reactions, cracks, wrinkles, etc. due to the impact of chemicals.
[0050] Preferably, the load-bearing protective film 410 is a micro-mucous film, which may be a PET micro-mucous film, a PTFE micro-mucous film, etc., and the micro-mucous film extends 0.5 mm to 2.0 mm outside the area of the opening window; the micro-mucous film is attached to a single side larger than the area of the first through window 200 to prevent the edge formed between the first through window 200 and the copper layer 310 from leaking medicine, causing problems such as stratification, and can further increase the load-bearing and protective effects of the load-bearing protective film 410.
[0051] See also Figure 8 , Figure 8 A schematic diagram of the cross-sectional structure of a covering method of a carrier protective film combined with a photosensitive liquid film.
[0052] Optionally, different from the above-mentioned supporting protective film 410 which adopts the covering method of attaching all solid films, the supporting protective film 410 can also be covered in combination with the photosensitive wet film 420. Specifically, the manufacturing method of pasting the supporting protective film 410410 to the first through window 200 also includes: silk-screening or coating the photosensitive wet film 420 from the edge area of the supporting protective film 410 to the edge area of the adjacent first copper layer 210, and curing.
[0053] That is, the carrying protective film 410 is only attached within the range of the first through window 200. At the same time, a photosensitive wet film 420 is made in the edge area formed between the first through window 200 and the copper layer 310. The pattern formed by the photosensitive wet film 420 covers the edge steps (or the gaps at the edges) to prevent the edges from seeping into the medicine. The wet film has high processing precision and can flow into the gaps to form a better bonding effect. The width covered by the silk-screen or coated photosensitive wet film 420 is 0.5mm to 2.0mm.
[0054] See also Fig. 9 , Fig. 9 Schematic diagram of the cross-sectional structure of the via plate.
[0055] Step S40: The carrier film graphic board 40 is drilled, electroplated, and processed to produce the second circuit pattern in sequence to form a via plate 50, including the formed via 510, and the second circuit pattern includes a second gold finger pattern 520, and the first gold finger pattern 330 and the second gold finger pattern 520 are respectively located at different ends of the copper layer 310.
[0056] The carrier film graphic board 40 is drilled and the whole board is electroplated in sequence. The drilling position is to connect the second circuit pattern of the copper layer 310 that needs to be grounded with the corresponding first circuit pattern of the ground layer to form a grounding effect. It can be seen that the present embodiment only uses one drilling, and only needs to make a conductive hole 510 between the single-sided copper layer circuit and the grounding circuit, which reduces the processing flow and reduces the processing difficulty. The electroplating here generally adopts pulse electroplating, and the hole wall copper can be plated preferentially.
[0057] With the support of the opening window core board 20 and the carrying protective film 410, a second circuit pattern is made on the copper layer 310 to avoid the problem of circuit hashing in the single-layer copper layer 310; here, after the copper layer 310 located in the first through window 200 area is made into the second circuit pattern, a first gold finger pattern 330 is formed, and the second circuit pattern formed at the other end of the same copper layer is a second gold finger pattern 520. Since the covering film is not attached at this time, the first gold finger pattern 330 and the second gold finger pattern 520 are the second circuit patterns of the same layer.
[0058] It can be seen that in this embodiment, a single-sided copper layer 310 is used to replace the double-sided copper clad laminate 100X in the prior art to produce a second circuit pattern, so that the different-sided and different-end gold fingers are directly located on the same circuit copper layer, and the signal transmission does not need to pass through the prior art conductive hole 110X, thereby avoiding the process of producing the prior art conductive hole 110X, and effectively reducing the reflection and scattering of signal transmission, and the generation of signal disturbance and distortion problems.
[0059] See also Fig.10 , Fig.10Schematic diagram of the cross-sectional structure of the cover film graphic board.
[0060] Step S50: Cover films are attached to both sides of the via plate 50, and the carrying protective film 410 is torn off to form a cover film pattern plate 60. The cover films attached to both sides are provided with second through windows, which correspond to the first gold finger pattern 330 and the second gold finger pattern 520 respectively.
[0061] The surface of the flexible circuit board generally needs to be attached with a covering film layer. In this embodiment, after the second circuit pattern is produced, a covering film needs to be attached to cover the area that does not require further processing. Therefore, two covering film layers are taken, namely the first covering film layer 610 and the second covering film layer 620, and the second through window A (610A) and the second through window B (620B) are opened respectively. The second through window A (610A) corresponds to the first gold finger pattern 330, and the second through window B (620B) corresponds to the second gold finger pattern 520.
[0062] Preferably, after the cover films are attached to both sides of the via plate 50, the edge area of the first through window 200 is ablated by laser; the laser ablation of the cover film exposes the first gold finger pattern 330 and the second gold finger pattern 520 for subsequent electroplating process.
[0063] Since the window core panel 20 and the copper layer 310 are bonded by the adhesive layer 320 by hot pressing, the adhesive layer 320 may overflow under the hot pressing state, and the overflow may reach the edge of the bonding position between the first through window 200 and the copper layer 310. Therefore, before electroplating, the overflowed colloid needs to be removed. The present embodiment adopts laser micro-ablation to effectively remove the overflowed colloid. Since the ablation range is small, the generated carbon powder can be effectively removed by plasma treatment combined with sandblasting.
[0064] See also Fig.11 , Fig.11 This is a schematic diagram of the cross-sectional structure of a high-fidelity signal flexible circuit board.
[0065] Step S60: The cover film graphic board 60 is electroplated, and then molded and processed in post-processing steps to form a high-fidelity signal flexible circuit board 70.
[0066] The electroplating process is to perform electroplating on the first gold finger pattern 330 and the second gold finger pattern 520 to form the first gold finger 710 and the second gold finger 720 respectively, that is, to form heterogeneous gold fingers; the molding process is to remove the invalid board edge area.
[0067] The above description is only a preferred embodiment of the present invention, and does not limit the patent scope of the present invention. All equivalent structural changes made by using the contents of the present invention specification and drawings under the inventive concept of the present invention, or directly / indirectly applied in other related technical fields are included in the patent protection scope of the present invention.
Claims
1. A method for manufacturing a high-fidelity signal flexible circuit board, characterized in that: The production method comprises the following steps: S10: taking a single-sided copper-clad laminate, making a first circuit pattern, and opening a first through window to form an open window core board, wherein the open window core board includes a first copper layer and a PI layer; S20: taking a copper layer, and laminating the copper layer and the PI layer through an adhesive layer, wherein a region of the copper layer corresponding to the first through window includes a first gold finger pattern; S30: pasting a carrying protective film to the first through window to form a carrying film graphic board; S40: drilling, whole-board electroplating, and manufacturing a second circuit pattern on the carrier film pattern board in sequence to form a via board, wherein the second circuit pattern includes a second gold finger pattern, and the first gold finger pattern and the second gold finger pattern are respectively located at different ends of different surfaces of the copper layer; S50: attaching cover films to both sides of the via plate, tearing off the carrying protective film, and forming a cover film pattern plate; the cover films attached to both sides are provided with second through windows, and the second through windows correspond to the first gold finger pattern and the second gold finger pattern respectively; S60: electrometallizing the cover film graphic board, and performing molding and post-processing to form the high-fidelity signal flexible circuit board.
2. The method for manufacturing a high-fidelity signal flexible circuit board according to claim 1, characterized in that: The first through window is produced by punching.
3. The method for manufacturing a high-fidelity signal flexible circuit board according to claim 1, characterized in that: The first-pass window is manufactured as follows: The first copper layer is made into a first window pattern, and the PI layer within the area of the first window pattern is made into a PI window pattern to form the first through window.
4. The method for manufacturing a high-fidelity signal flexible circuit board according to claim 3, characterized in that: The first windowing pattern is larger on one side than the PI windowing pattern.
5. The method for manufacturing a high-fidelity signal flexible circuit board according to claim 1, characterized in that: The bonding layer is a solid acrylic adhesive layer or a solid epoxy resin adhesive layer, and a bonding layer through window is opened toward the bonding layer corresponding to the first through window.
6. The method for manufacturing a high-fidelity signal flexible circuit board according to claim 1, characterized in that: The bonding layer is made by: Take liquid acrylic glue or liquid epoxy resin glue, screen print or apply the liquid acrylic glue or liquid epoxy resin glue on the PI layer, and bake and cure.
7. The method for manufacturing a high-fidelity signal flexible circuit board according to claim 1, characterized in that: The load-bearing protective film is a micro-adhesive film.
8. The method for manufacturing a high-fidelity signal flexible circuit board according to claim 7, characterized in that: The micro-mucosa extends 0.5 mm to 2.0 mm outside the area of the opening window.
9. The method for manufacturing a high-fidelity signal flexible circuit board according to claim 1, characterized in that: The manufacturing method of attaching the load-bearing protective film to the first through window further includes: A photosensitive wet film is screen-printed or coated from the edge area of the carrying protection film to the edge area adjacent to the first copper layer, and then cured.
10. The method for manufacturing a high-fidelity signal flexible circuit board according to claim 1, characterized in that: After the cover films are attached to both sides of the via plate, the edge area of the first via window is ablated by laser.