Circuit board embedded copper block production method
By stacking the first semi-cured sheets on both sides of the copper substrate and laminated and bonding, the composite copper plate is formed, and the problem of erasing of the browned layer of the small buried copper block is solved, and the bonding strength between the buried copper block and the semi-cured sheet is improved, ensuring the buried copper block Firm bond between the block and the circuit board.
Patent Information
- Application Number
- CN202411075960.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-07
- Publication Date
- 2024-11-15
AI Technical Summary
Small buried copper blocks are prone to being wiped during processing, resulting in a decrease in bonding strength with the semi-cured sheet.
By stacking the first semi-cured sheets on both sides of the copper substrate and laminated and bonding, a composite copper plate is formed to protect the brown layer, avoid scratching, and edge-floating and acid etching are performed on the periphery of the composite copper plate to ensure bonding strength.
The bonding strength between the buried copper block and the semi-cured sheet is improved, the brown layer is prevented from being damaged, and the bonding firmness between the buried copper block and the circuit board is enhanced.
Smart Images

Figure CN118973151A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of circuit board production, and in particular to a method for producing buried copper blocks of a circuit board. Background Art
[0002] For some circuit boards with high heat dissipation requirements, buried copper blocks are usually set in the circuit boards. The buried copper block processing process is to cut the copper substrate into several buried copper blocks, then brown the surface of the buried copper blocks to form a brown layer, open buried holes on the circuit board and fill them with buried copper blocks, and then laminate the entire circuit board so that the surface of the buried copper block is combined with the second semi-cured sheet inside the circuit board. The brown layer can roughen the surface of the buried copper block, making the surface of the buried copper block more firmly bonded to the second semi-cured sheet. However, small buried copper blocks are prone to the brown layer being scratched during operation in various processes, which reduces the bonding strength between the buried copper block and the semi-cured sheet. Summary of the invention
[0003] The present invention aims to solve at least one of the technical problems existing in the prior art. To this end, the present invention provides a method for producing a buried copper block for a circuit board, which prevents the browning layer of the buried copper block body from being abraded, and the bonding strength between the buried copper block body and the prepreg is relatively high.
[0004] According to an embodiment of the present invention, a method for producing buried copper blocks for circuit boards comprises the following steps: browning a copper substrate; stacking first semi-cured sheets on both side surfaces of the copper substrate respectively, and laminating the copper substrate and the first semi-cured sheets to form a composite copper board; cutting the composite copper board into a plurality of composite buried copper blocks, wherein the composite buried copper blocks comprise a buried copper block body and the first semi-cured sheets arranged on opposite sides of the buried copper block body; obtaining a circuit board, wherein buried holes corresponding to the composite buried copper blocks are opened on the circuit board, and the composite buried copper blocks are installed into the buried holes.
[0005] The method for producing buried copper blocks for circuit boards according to an embodiment of the present invention has at least the following beneficial effects: after the larger copper substrate is browned, the first semi-cured sheet is directly stacked on the two side surfaces and laminated together, and the first semi-cured sheet can protect the browned layer on the surface of the copper substrate so that the browned layer will not be scratched, that is, after being cut to form a smaller composite buried copper block, the browned layer on the surface of the buried copper block body is still maintained by the first semi-cured sheet and will not be scratched, and the bonding strength between the buried copper block body and the first semi-cured sheet is relatively high.
[0006] According to some embodiments of the present invention, the method of stacking first semi-cured sheets on both side surfaces of the copper substrate and laminating the copper substrate and the first semi-cured sheets to form a composite copper plate includes: before laminating the copper substrate and the first semi-cured sheets, stacking copper foil on the side of the two first semi-cured sheets away from the copper substrate, and then laminating the copper substrate, the first semi-cured sheet and the copper foil.
[0007] According to some embodiments of the present invention, after laminating the copper substrate, the first prepreg and the copper foil, the method further includes: trimming the periphery of the composite copper plate to remove the adhesive flow of the first prepreg and the edge material protruding from the copper foil.
[0008] According to some embodiments of the present invention, after the periphery of the composite copper plate is trimmed, the method further includes: removing the copper foil on a side of the first prepreg away from the copper substrate.
[0009] According to some embodiments of the present invention, the method of removing the copper foil on a side of the first prepreg away from the copper substrate comprises: acid etching the side of the first prepreg away from the copper substrate.
[0010] According to some embodiments of the present invention, before the edge of the composite copper plate is trimmed, the process further includes: machining positioning holes on the composite copper plate, and positioning the composite copper plate through the positioning holes.
[0011] According to some embodiments of the present invention, the method of browning a copper substrate comprises: browning the entire copper substrate to form a browning layer.
[0012] According to some embodiments of the present invention, before browning the copper substrate, the process further includes: cutting a large copper plate into a plurality of the copper substrates.
[0013] According to some embodiments of the present invention, the method of cutting the composite copper plate into a plurality of composite buried copper blocks comprises: using a CNC machine tool to cut the composite copper plate to form a plurality of composite buried copper blocks.
[0014] According to some embodiments of the present invention, after installing the composite buried copper block into the buried hole, the method further includes: laminating the circuit board and the composite buried copper block so that the first semi-cured sheet of the composite buried copper block is combined with the second semi-cured sheet inside the circuit board.
[0015] Additional aspects and advantages of the present invention will be given in part in the following description and in part will be obvious from the following description, or will be learned through practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] The above and / or additional aspects and advantages of the present invention will become apparent and easily understood from the description of the embodiments in conjunction with the following drawings, in which:
[0017] Figure 1 It is a schematic diagram of the main process of the method for producing buried copper blocks of a circuit board according to an embodiment of the present invention;
[0018] Figure 2 A schematic diagram of a complete process of a method for producing buried copper blocks for circuit boards according to an embodiment of the present invention;
[0019] Figure 3 A schematic cross-sectional view of a composite copper plate covered with copper foil formed by lamination according to an embodiment of the present invention;
[0020] Figure 4 is a schematic cross-sectional view of a composite buried copper block according to an embodiment of the present invention;
[0021] Figure 5 It is a cross-sectional schematic diagram of the composite buried copper block after being placed into a circuit board according to an embodiment of the present invention.
[0022] Reference numerals:
[0023] Copper substrate 100, buried copper block body 110, browning layer 120;
[0024] A first prepreg 200;
[0025] Copper foil 300;
[0026] Circuit board 400 and second prepreg 410 . DETAILED DESCRIPTION
[0027] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.
[0028] In the description of the present invention, it should be understood that descriptions involving orientation, such as orientation or positional relationship indicated as up, down, etc., are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.
[0029] In the description of the present invention, "a plurality" means more than two. If there is a description of "first" or "second", it is only used for the purpose of distinguishing technical features, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features or implicitly indicating the order of the indicated technical features.
[0030] In the description of the present invention, unless otherwise clearly defined, terms such as setting, installing, connecting, etc. should be understood in a broad sense, and technicians in the relevant technical field can reasonably determine the specific meanings of the above terms in the present invention based on the specific content of the technical solution.
[0031] For some circuit boards 400 with higher heat dissipation requirements, buried copper blocks are usually set in the circuit board 400. The buried copper block processing process is to cut the copper substrate 100 into several buried copper blocks, then brown the surface of the buried copper blocks to form a brown layer 120, open buried holes on the circuit board 400 and fill them with buried copper blocks, and then laminate the circuit board 400 as a whole, so that the surface of the buried copper block is combined with the second semi-cured sheet 410 inside the circuit board 400. The brown layer 120 can roughen the surface of the buried copper block, so that the surface of the buried copper block is more firmly combined with the second semi-cured sheet 410. However, the small buried copper block is prone to the brown layer 120 being scratched during the operation of each process, which reduces the bonding strength between the buried copper block and the semi-cured sheet.
[0032] Reference Figures 1 to 5 , is a method for producing buried copper blocks of a circuit board 400 according to an embodiment of the present invention, comprising the following steps:
[0033] S10: browning the copper substrate 100;
[0034] S20: stacking the first prepreg 200 on both side surfaces of the copper substrate 100 respectively, and laminating the copper substrate 100 and the first prepreg 200 to form a composite copper plate;
[0035] S30: cutting the composite copper plate into a plurality of composite buried copper blocks, wherein the composite buried copper blocks include a buried copper block body 110 and first prepreg sheets 200 disposed on opposite sides of the buried copper block body 110;
[0036] S40: Obtain a circuit board 400, on which buried holes corresponding to the composite buried copper blocks are opened, and install the composite buried copper blocks into the buried holes.
[0037] After the larger copper substrate 100 is browned, the first semi-cured sheet 200 is directly stacked on the two side surfaces and laminated. The first semi-cured sheet 200 can protect the browned layer 120 on the surface of the copper substrate 100, so that the browned layer 120 will not be scratched. That is, after being cut into a smaller composite buried copper block, the browned layer 120 on the surface of the buried copper block body 110 is still under the protection of the first semi-cured sheet 200 and will not be scratched. The bonding strength between the buried copper block body 110 and the first semi-cured sheet 200 is relatively high.
[0038] Specifically, in step S20, it includes:
[0039] S21: Before laminating the copper substrate 100 and the first prepreg 200, copper foil 300 is stacked on the side of the two first prepregs 200 away from the copper substrate 100, and then the copper substrate 100, the first prepreg 200 and the copper foil 300 are laminated.
[0040] Lamination is a method of combining two or more layers of the same or different materials into a whole by heating and pressurizing. If the laminating device is in direct contact with the first prepreg 200, the first prepreg 200 is likely to adhere to the laminating device, affecting production. Stacking the copper foil 300 on the side of the first prepreg 200 away from the copper substrate 100 can avoid direct contact between the laminating device and the first prepreg 200 during the lamination process, thereby avoiding the first prepreg 200 from adhering to the laminating device, so that the composite substrate can be relatively easily separated from the laminating device, and the production and processing are relatively convenient.
[0041] Specifically, after step S21, the following steps are also included:
[0042] A20: The periphery of the composite copper plate is trimmed to remove the adhesive flow of the first prepreg 200 and the edge material of the copper foil 300.
[0043] Since the copper foil 300, the first prepreg 200 and the copper substrate 100 are combined by one-time lamination, there will be glue flow extrusion around the periphery of the first prepreg 200 during the lamination process, and the copper foil 300 is usually larger in area than the copper substrate 100, so there will be excess edge material extending relative to the copper substrate 100. Therefore, by removing the edge, the glue flow around the composite copper plate and the excess edge material of the copper foil 300 can be removed, making the composite copper plate more neat, facilitating the production of subsequent process flows, and reducing abnormal risks.
[0044] Specifically, after step A20, the following steps are also included:
[0045] A30: removing the copper foil 300 on the side of the first prepreg 200 away from the copper substrate 100 .
[0046] The copper foil 300 bonded to the side of the first prepreg 200 away from the copper substrate 100 will affect the bonding of the composite buried copper block and the circuit board 400 in the subsequent process. Therefore, after removing the copper foil 300 on the side of the first prepreg 200 away from the copper substrate 100, when the composite buried copper block is placed in the buried hole of the circuit board 400, the first prepreg 200 of the composite buried copper block can be bonded to the second prepreg 410 inside the circuit board 400. Furthermore, during the lamination process of the first semi-cured sheet 200, the copper substrate 100 and the copper foil 300, the copper foil 300 will be wrinkled and coarsened, making the bonding surface of the copper foil 300 and the first semi-cured sheet 200 rough. Therefore, after the copper foil 300 is removed, the surface of the first semi-cured sheet 200 away from the copper substrate 100 will remain rough, so that when the first semi-cured sheet 200 is installed in the buried hole of the circuit board 400, the first semi-cured sheet 200 of the composite buried copper block can be more tightly bonded to the second semi-cured sheet 410 of the circuit board 400, thereby improving the process reliability of the buried copper block of the circuit board 400.
[0047] Specifically, step A30 includes:
[0048] A31: Acid etching is performed on the side of the first prepreg 200 away from the copper substrate 100 .
[0049] The copper foil 300 is removed by acid etching, which can relatively completely retain the rough surface of the first prepreg 200 away from the copper substrate 100, so that the first prepreg 200 of the composite buried copper block is firmly bonded to the second prepreg 410 of the circuit board 400, and the browning layer 120 is not easily damaged. Specifically, the acid etching is to corrode and remove the copper foil 300 with a weak acid.
[0050] Specifically, before step A20, the following steps are also included:
[0051] A10: Process positioning holes on the composite copper plate and position the composite copper plate through the positioning holes.
[0052] Processing positioning holes on the composite copper plate can facilitate positioning of the composite copper plate when edge fishing, avoid the risk of shaking of the composite copper plate when edge fishing, and make the edge fishing position more accurate.
[0053] Specifically, the positioning holes may be processed on the composite copper plate by drilling; it is understandable that the positioning holes may be processed on the composite copper plate by other processing methods, and those skilled in the art may configure the positioning holes according to actual needs. The composite copper plate may be positioned by inserting the pins on the fixture into the positioning holes.
[0054] Specifically, in step S10, the following steps are included:
[0055] S11 : browning the entire copper substrate 100 to form a browning layer 120 .
[0056] By browning the entire copper substrate 100, a browning layer 120 is formed on the outer surface of the copper substrate 100, so that the browning process of the copper substrate 100 is relatively simple and the processing is relatively convenient. It is conceivable that in other embodiments, the copper substrate 100 can be browned, or both sides of the copper substrate 100 can be browned, and those skilled in the art can make specific configurations according to actual needs.
[0057] Specifically, before step S10, the following steps are also included:
[0058] S00: Cut the large copper plate into multiple copper substrates 100. Since the purchased large copper plate has a large area, it is usually necessary to cut the large copper plate into copper substrates 100 of a certain size before the copper substrates 100 can be conveniently browned. It is understandable that the number of copper substrates 100 cut from the large copper plate can be specifically configured according to actual needs, and the size of the cut copper substrates 100 can also be specifically configured according to actual needs.
[0059] Specifically, in step S30, it includes:
[0060] S31: Cut the composite copper plate using a CNC machine tool to form a plurality of composite buried copper blocks. Since the composite copper plate includes a copper substrate 100 and a first prepreg 200 bonded to the two side surfaces of the copper substrate 100, when the composite copper plate is cut using a CNC machine tool, the first prepreg 200 will prevent the copper substrate 100 from generating copper wire flash during cutting, so that the formed composite buried copper block is not prone to defects such as copper wire flash, so that the forming quality of the composite buried copper block is relatively good.
[0061] It is conceivable that other types of cutting equipment may be used to cut the composite copper plate to form a plurality of composite buried copper blocks, such as saw blade machines, CNC milling machines, etc. Personnel in the art may configure the equipment according to actual needs.
[0062] Specifically, after step S40, the following steps are also included:
[0063] S50: Laminating the circuit board 400 and the composite buried copper block, so that the first prepreg 200 of the composite buried copper block is combined with the second prepreg 410 inside the circuit board 400. After the composite copper block is placed in the buried hole reserved in the circuit board 400, the circuit board 400 is laminated. Under the high temperature and pressure of the lamination, the first prepreg 200 on the buried copper block body 110 can be firmly bonded to the second prepreg 410 inside the circuit board 400, and the reliability of the manufactured circuit board 400 is good.
[0064] In the description of this specification, the description with reference to the terms "one embodiment", "some embodiments", "illustrative embodiments", "examples", "specific examples", or "some examples" means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner.
[0065] Although the embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the claims and their equivalents.
Claims
1. A method for producing buried copper blocks of circuit boards, It is characterized in that The following steps are involved: Browning the copper substrate (100); First prepregs (200) are stacked on both side surfaces of the copper substrate (100) respectively, and the copper substrate (100) and the first prepregs (200) are laminated to form a composite copper plate; The composite copper plate is cut into a plurality of composite buried copper blocks, wherein the composite buried copper blocks include a buried copper block body (110) and the first prepreg sheets (200) arranged on opposite sides of the buried copper block body (110); A circuit board (400) is obtained, wherein buried holes corresponding to the composite buried copper blocks are opened on the circuit board (400), and the composite buried copper blocks are installed in the buried holes.
2. The method for producing buried copper blocks of a circuit board according to claim 1, It is characterized in that The method of stacking first prepregs (200) on both side surfaces of the copper substrate (100) and laminating the copper substrate (100) and the first prepregs (200) to form a composite copper plate comprises: before laminating the copper substrate (100) and the first prepregs (200), stacking copper foils (300) on the sides of the two first prepregs (200) away from the copper substrate (100), and then laminating the copper substrate (100), the first prepregs (200) and the copper foils (300).
3. The method for producing buried copper blocks of a circuit board according to claim 2, It is characterized in that After laminating the copper substrate (100), the first prepreg (200) and the copper foil (300), the method further includes: trimming the periphery of the composite copper plate to remove the adhesive flow of the first prepreg (200) and the edge material protruding from the copper foil (300).
4. The method for producing buried copper blocks of a circuit board according to claim 3, It is characterized in that After the periphery of the composite copper plate is trimmed, the method further comprises: removing the copper foil (300) on the side of the first prepreg (200) away from the copper substrate (100).
5. The method for producing buried copper blocks of a circuit board according to claim 4, It is characterized in that The method for removing the copper foil (300) on the side of the first prepreg (200) away from the copper substrate (100) comprises: acid etching the side of the first prepreg (200) away from the copper substrate (100).
6. The method for producing buried copper blocks of circuit boards according to claim 3, It is characterized in that Before the periphery of the composite copper plate is trimmed, the method further includes: machining positioning holes on the composite copper plate, and positioning the composite copper plate through the positioning holes.
7. The method for producing buried copper blocks of a circuit board according to claim 1, It is characterized in that The method for browning a copper substrate (100) comprises: browning the entire copper substrate (100) to form a browning layer (120).
8. The method for producing buried copper blocks of a circuit board according to claim 1, It is characterized in that Before browning the copper substrate (100), the method further comprises: cutting a large copper plate into a plurality of the copper substrates (100).
9. The method for producing buried copper blocks of a circuit board according to claim 1, It is characterized in that The method for cutting the composite copper plate into a plurality of composite buried copper blocks comprises: using a numerically controlled machine tool to cut the composite copper plate to form a plurality of composite buried copper blocks.
10. The method for producing buried copper blocks of circuit boards according to claim 1, It is characterized in that After the composite buried copper block is installed into the buried hole, the method further includes: laminating the circuit board (400) and the composite buried copper block so that the first prepreg (200) of the composite buried copper block is combined with the second prepreg (410) inside the circuit board (400).