Optical fiber manufacturing method and optical fiber drawing device

By covering the optical fiber outlet with an atmosphere with a dew point temperature below 10°C and utilizing inert gas regeneration and control of the glass fiber outlet temperature, the problem of reduced optical fiber strength was solved, and efficient optical fiber manufacturing was achieved.

CN118973970APending Publication Date: 2024-11-15SUMITOMO ELECTRIC INDUSTRIES LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202380031257.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-03-30
Filing Date
2023-03-29
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

During the optical fiber manufacturing process, moisture from the atmosphere adheres to the glass fiber as it exits the fiber outlet of the drawing furnace, resulting in a decrease in the strength of the optical fiber.

Method used

By covering the fiber optic outlet with an atmosphere with a dew point temperature below 10°C and utilizing the regeneration and reuse of inert gases such as helium, combined with the supply of inert gases, the adhesion of atmospheric moisture to the glass fiber is suppressed. At the same time, the outlet temperature of the glass fiber is controlled between 1300°C and 1700°C to prevent rapid cooling and dust collision.

Benefits of technology

It effectively inhibits the adhesion of moisture to the surface of glass fiber, reduces the decrease in optical fiber strength and the frequency of wire breakage, and improves the quality and production efficiency of optical fiber.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118973970A_ABST
    Figure CN118973970A_ABST
Patent Text Reader

Abstract

A method for manufacturing an optical fiber forms a glass fiber by heating and melting a base material for an optical fiber in a fiber drawing furnace and drawing the base material. The fiber drawing furnace is provided with: a heating furnace for heating and melting an optical fiber base material; and a lower extension tube which is provided at the lower end of the heating furnace and through which the glass fiber passes. And the lower extension tube is provided with an optical fiber leading-out port for leading out the glass fiber. And drawing while covering the optical fiber export with an atmosphere having a dew point temperature of 10 DEG C or less.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for manufacturing an optical fiber and an optical fiber drawing device.

[0002] This application claims the benefit of priority based on Japanese Application No. 2022-055713 filed on March 30, 2022, and all the contents described in the aforementioned Japanese Application are incorporated herein by reference. Background Art

[0003] Patent document 1 discloses an optical fiber drawing furnace in which a lower extension tube is provided below a furnace core tube into which an optical fiber glass matrix is ​​inserted. In the drawing furnace, a portion of the first inert gas introduced into the furnace core tube and flowing into the lower extension tube is recovered in the lower extension tube. In addition, a gas screen is provided below the lower extension tube. In order to prevent the atmosphere from being mixed into the lower extension tube due to the recovery of a portion of the first inert gas, a second inert gas is supplied to the inside of the gas screen.

[0004] Patent Document 1: U.S. Patent Application Publication No. 2017-101336 Summary of the invention

[0005] A method for producing an optical fiber according to one embodiment of the present invention heats and melts an optical fiber base material in a drawing furnace to draw a glass fiber.

[0006] The wire drawing furnace has:

[0007] a heating furnace for heating and melting the optical fiber base material; and

[0008] A lower extension tube is disposed at the lower end of the heating furnace and is used for the glass fiber to pass through.

[0009] The lower extension tube has an optical fiber outlet for allowing the glass fiber to be led out.

[0010] The optical fiber lead-out port is covered with an atmosphere having a dew point temperature of 10° C. or less while the optical fiber is drawn.

[0011] Another aspect of the present invention relates to an optical fiber drawing device that heats and melts an optical fiber base material to draw a fiber to form a glass fiber. The optical fiber drawing device includes:

[0012] A heating furnace for heating and melting the optical fiber base material;

[0013] A lower extension tube, which is disposed at the lower end of the heating furnace, allows the glass fiber to pass through the interior and allows the glass fiber to exit from the optical fiber outlet;

[0014] a chamber surrounding the optical fiber outlet and having a supply port for supplying an inert gas to the interior; and

[0015] An inert gas generating device generates the inert gas and supplies the generated inert gas to the supply port.

[0016] Effects of the Invention

[0017] According to the configuration of the present invention, it is possible to suppress the adhesion of moisture contained in the atmosphere to the glass fiber exiting from the optical fiber outlet of the drawing furnace, thereby suppressing a decrease in the strength of the obtained optical fiber. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 It is a schematic structural diagram of an optical fiber manufacturing apparatus according to one embodiment of the present invention.

[0019] Figure 2 Yes means Figure 1 A close-up view of a portion of the lower extension tube is shown.

[0020] Figure 3 It is a partially enlarged view showing a modified example of the optical fiber manufacturing apparatus.

[0021] Figure 4 It is a partially enlarged view showing another modified example of the optical fiber manufacturing apparatus.

[0022] Figure 5 yes Figure 4 A schematic perspective view of a chamber according to a modified example is shown. DETAILED DESCRIPTION

[0023] [Problems to be Solved by the Invention]

[0024] In an optical fiber drawing furnace, if moisture contained in the atmosphere adheres to glass fibers exiting from an optical fiber lead-out port of the drawing furnace, the strength of the obtained optical fiber may be reduced.

[0025] An object of the present invention is to suppress the adhesion of moisture contained in the atmosphere to glass fibers exiting from an optical fiber outlet of a drawing furnace, thereby suppressing a decrease in the strength of the obtained optical fiber.

[0026] [Description of Embodiments of the Invention]

[0027] First, embodiments of the present invention will be described by way of examples.

[0028] (1) A method for producing an optical fiber according to one embodiment of the present invention comprises heating and melting an optical fiber base material in a drawing furnace to draw a glass fiber.

[0029] The wire drawing furnace has:

[0030] a heating furnace for heating and melting the optical fiber base material; and

[0031] A lower extension tube is disposed at the lower end of the heating furnace and is used for the glass fiber to pass through.

[0032] The lower extension tube has an optical fiber outlet for the glass fiber to be led out.

[0033] The optical fiber lead-out port is covered with an atmosphere having a dew point temperature of 10° C. or less while the optical fiber is drawn.

[0034] According to this method, it is possible to suppress the adhesion of moisture contained in the atmosphere to the glass fiber exiting from the optical fiber outlet of the drawing furnace, thereby suppressing a decrease in the strength of the obtained optical fiber.

[0035] (2) In the above (1), the heating furnace may include a gas inlet for introducing a gas containing helium into the heating furnace.

[0036] The lower extension tube has a gas suction port, which sucks the gas containing helium inside and discharges it to the outside of the lower extension tube.

[0037] Wire drawing is performed while regenerating and reusing the gas including the helium gas exhausted from the gas suction port.

[0038] If helium is sucked from the lower extension tube, the amount of helium flowing out of the optical fiber outlet together with the glass fiber is reduced, and the glass fiber exiting from the optical fiber outlet is easily exposed to the atmosphere. According to the above method, the optical fiber outlet is covered with an atmosphere with a dew point temperature of 10°C or less, so it is possible to suppress the adhesion of moisture in the atmosphere to the glass fiber. Therefore, expensive helium can be reused, and the strength reduction of the optical fiber can also be suppressed.

[0039] (3) In the above (1) or (2), the temperature of the glass fiber output from the optical fiber output port may be 1300° C. or higher and 1700° C. or lower.

[0040] The higher the temperature of the glass fiber exiting from the optical fiber outlet of the lower extension tube, the more the reaction between the moisture in the atmosphere and the surface of the glass fiber is promoted, and the easier it is to form scratches on the surface of the glass fiber. According to the above method, even if the glass fiber exits from the optical fiber outlet at a high temperature of more than 1300°C, since the optical fiber outlet is covered by an atmosphere with a dew point temperature of less than 10°C, it is possible to suppress the moisture in the atmosphere from adhering to the glass fiber. Thus, the strength reduction of the optical fiber can be suppressed. In addition, by setting the outlet temperature of the glass fiber to more than 1300°C, it is possible to suppress the situation in which the outer diameter of the glass fiber is changed by being rapidly cooled until it exits from the optical fiber outlet of the lower extension tube. On the other hand, by setting the outlet temperature of the glass fiber to less than 1700°C, it is possible to suppress the generation of defects on the surface of the glass fiber due to the collision of dust in the atmosphere. As a result, the strength reduction of the optical fiber can be further suppressed.

[0041] (4) In any one of the above (1) to (3), an inert gas may be supplied to the vicinity of the optical fiber lead-out port.

[0042] According to this method, the optical fiber outlet of the lower extension tube can be efficiently covered with an atmosphere having a dew point temperature of 10° C. or less. In addition, by using an inert gas, mixing of the atmosphere into the lower extension tube can be suppressed. As a result, the strength reduction of the optical fiber can be further suppressed.

[0043] (5) In any one of the above (1) to (4), an inert gas may be supplied into a chamber surrounding the optical fiber lead-out port.

[0044] According to this method, the optical fiber lead-out port of the lower extension tube can be more effectively covered with the atmosphere having a dew point temperature of 10° C. or less.

[0045] (6) In the above (5), the chamber may have a first side surface and a second side surface opposite to the first side surface,

[0046] The inert gas is supplied from the first side and exhausted from the second side.

[0047] According to this method, a gas flow of an inert gas is formed in the chamber, so that dust, cyanide and other gases ejected from the wire drawing furnace are less likely to remain.

[0048] (7) An optical fiber drawing device according to one embodiment of the present invention heats and melts an optical fiber base material to draw a fiber to form a glass fiber, the fiber drawing device comprising:

[0049] A heating furnace for heating and melting the optical fiber base material;

[0050] A lower extension tube, which is arranged at the lower end of the heating furnace, allows the glass fiber to pass through the inside and allows the glass fiber to exit from the optical fiber outlet;

[0051] a chamber surrounding the optical fiber outlet and having a supply port for supplying an inert gas to the interior; and

[0052] An inert gas generating device generates the inert gas and supplies the generated inert gas to the supply port.

[0053] The drawing device of the present invention generates inert gas from an inert gas generating device and supplies the inert gas into a chamber from a supply port, thereby preventing moisture contained in the atmosphere from adhering to the glass fiber exiting from the optical fiber outlet, thereby preventing the strength of the obtained optical fiber from decreasing.

[0054] (8) In the above (7), a plate may be provided between the supply port and a position where the glass fiber passes through the interior of the chamber.

[0055] According to this configuration, the inert gas does not directly hit the glass fiber, and thus linear swaying of the glass fiber can be suppressed.

[0056] (9) In the above (7) or (8), an opening and closing door may be provided on the front surface of the chamber.

[0057] Since the chamber is provided with an opening and closing door, the operator can easily perform the initial operation of drawing the glass fiber from the optical fiber base material (so-called seeding operation).

[0058] [Effects of the Invention]

[0059] According to the configuration of the present invention, it is possible to suppress the adhesion of moisture contained in the atmosphere to the glass fiber exiting from the optical fiber outlet of the drawing furnace, thereby suppressing a decrease in the strength of the obtained optical fiber.

[0060] [Details of the embodiments of the present invention]

[0061] Hereinafter, an embodiment of the manufacturing device and manufacturing method of the optical fiber involved in the present invention will be described with reference to the accompanying drawings. In the following description, even if there are different drawings, the same or equivalent elements are marked with the same reference numerals or names, and repeated descriptions are appropriately omitted. In addition, the dimensions of each component shown in each drawing are set for the convenience of description, and may be different from the actual dimensions of each component.

[0062] (Optical fiber manufacturing device)

[0063] Figure 11 is a schematic diagram of a manufacturing device 1 for optical fiber according to an embodiment of the present invention. The manufacturing device 1 includes a drawing furnace 100. The drawing furnace 100 is a device for heating and melting an optical fiber base material 2 to draw a glass fiber 3. Although not shown, the manufacturing device 1 may further include a cooling device for cooling the glass fiber 3, a coating device for coating the outer periphery of the glass fiber 3 with a coating resin, a winding device for winding the glass fiber 3 coated with the coating resin, and the like. The drawing furnace 100 is an example of an optical fiber drawing device.

[0064] The drawing furnace 100 includes a heating furnace 10 and a lower extension tube 20. The heating furnace 10 heats and melts the optical fiber base material 2. The heating furnace 10 includes a frame 11, a furnace core tube 12, and a heater 13. The frame 11 is configured to surround the furnace core tube 12 and the heater 13. The heater 13 is configured to surround the furnace core tube 12. A heat insulating material (not shown) is arranged between the heater 13 and the frame 11. The optical fiber base material 2 is suspended in the furnace core tube 12 by a base material suspension mechanism (not shown). The suspended optical fiber base material 2 is drawn in such a manner that the lower portion is melted by the heat from the heater 13 and the glass fiber 3 having a predetermined outer diameter is continuously obtained.

[0065] The furnace core tube 12 has a gas inlet 16. One end of a gas pipe 14 is connected to the gas inlet 16. An inert gas supplier 15 for supplying an inert gas such as argon, helium, or nitrogen is connected to the other end of the gas pipe 14. The inert gas supplied from the inert gas supplier 15 is supplied from the gas inlet 16 into the furnace core tube 12 through the gas pipe 14. The inert gas supplied into the furnace core tube 12 flows into the lower extension pipe 20.

[0066] The lower extension tube 20 is provided at the lower end of the heating furnace 10. The lower extension tube 20 is provided so as to connect the inlet of the lower extension tube 20 and the outlet of the furnace core tube 12. The lower extension tube 20 is preferably provided to be in close contact with the lower part of the heating furnace 10, for example. The lower extension tube 20 may be formed integrally with the heating furnace 10, or may be provided to be removable relative to the heating furnace 10. An optical fiber outlet 21 is formed at the lower end of the lower extension tube 20. The glass fiber 3 drawn in the furnace core tube 12 continuously passes through the lower extension tube 20 and is led out from the optical fiber outlet 21. By providing the lower extension tube 20, the rapid cooling of the glass fiber 3 softened by heating can be suppressed, and the glass fiber 3 can be hardened by cooling to a certain extent, thereby suppressing the change in the outer diameter of the glass fiber 3.

[0067] The lower extension tube 20 has a gas suction port 22. The gas suction port 22 is provided to suck a mixed gas including an inert gas and other gases and discharge it to the outside of the lower extension tube 20. The inert gas is supplied into the furnace core tube 12 and flows into the lower extension tube 20. The other gases include impurities generated during the wire drawing process. Figure 1 In the example, two gas suction ports 22 are provided. One end of the gas piping 23a is connected to one gas suction port 22. One end of the gas piping 23b is connected to the other gas suction port 22. A portion of the gas piping 23b is omitted in the illustration, and a gas regeneration device 24 is connected to the other ends of the gas pipings 23a and 23b. The gas regeneration device 24 separates and purifies the inert gas (for example, helium) from the mixed gas sucked by the gas suction port 22, and regenerates it into a state in which the inert gas can be reused. It can be configured such that the gas regeneration device 24 and the inert gas supplier 15 are connected by the piping 25, and the inert gas regenerated by the gas regeneration device 24 is supplied to the inert gas supplier 15.

[0068] exist Figure 1 For example, the lower extension tube 20 has a damper mechanism 26. Figure 2 As shown in the example, the damper mechanism 26 includes an upper damper 261 and a lower damper 262. A gas recovery space 263 is formed between the upper damper 261 and the lower damper 262. The mixed gas G1 recovered to the gas recovery space 263 through the through hole 261a of the upper damper 261 is sucked from the gas recovery space 263 to the outside through the gas suction port 22 formed on the bottom surface of the lower damper 262.

[0069] The optical fiber outlet 21 formed at the center of the bottom surface of the lower damper 262 is covered by an atmosphere having a dew point temperature of 10° C. or less. Figure 2 As shown, gas G2 whose dew point temperature is controlled to be 10° C. or less is supplied to the vicinity of the optical fiber lead-out port 21 .

[0070] (Method for manufacturing optical fiber)

[0071] Next, as a method for manufacturing an optical fiber according to the present embodiment, Figure 1 A method for manufacturing an optical fiber using the manufacturing apparatus 1 shown will be described.

[0072] The manufacturing method of the optical fiber involved in this embodiment includes: a first step of heating and melting the optical fiber base material 2 in a heating furnace 10; a second step of passing the glass fiber 3 output from the heating furnace 10 through a lower extension tube 20; and a third step of allowing the glass fiber 3 to output from an optical fiber outlet 21 covered by an atmosphere with a dew point temperature below 10°C.

[0073] In the first step, the optical fiber base material 2 is suspended in the furnace core tube 12, and the lower part of the optical fiber base material 2 is heated by the heater 13 to melt the optical fiber base material 2. The molten optical fiber base material 2 becomes a glass fiber 3 of a predetermined outer diameter due to the weight and tensile force of the molten glass and is continuously drawn. In addition, in the first step, an inert gas is introduced into the furnace core tube 12 from the gas inlet 16. The above-mentioned gases can be used as the inert gas. Next, the case where helium is used as the inert gas is described.

[0074] In the furnace core tube 12, for example, silica particles granulated from silica components volatilized from the optical fiber base material 2 and carbon particles peeled from carbon components used in the heating furnace 10 are continuously generated. These impurities are transported to the lower extension tube 20 by the inert gas traction flow.

[0075] In the second step, the glass fiber 3 exiting the heating furnace 10 (furnace core tube 12) passes through the lower extension tube 20. The glass fiber 3 passes through the lower extension tube 20, thereby relieving rapid cooling, and because it is cooled and hardened to a certain extent, the change in outer diameter is suppressed. In addition, in the second step, a mixed gas G1 including helium and other gases in the lower extension tube 20 is sucked from the gas suction port 22, and the other gases contain impurities generated in the first and second steps. The sucked mixed gas is separated and purified by the gas regeneration device 24, thereby regenerating it as reusable helium.

[0076] In the third step, the glass fiber 3 that has passed through the lower extension tube 20 is led out from the optical fiber lead-out port 21 covered with an atmosphere having a dew point temperature of 10°C or less. For example, a gas G2 whose dew point temperature is controlled to be 10°C or less is supplied to the periphery of the optical fiber lead-out port 21, thereby covering the optical fiber lead-out port 21 with an atmosphere having a dew point temperature of 10°C or less. The glass fiber 3 that has been led out from the optical fiber lead-out port 21 passes through an atmosphere having a dew point temperature of 10°C or less.

[0077] However, moisture contained in the atmosphere adheres to the glass fiber 3 exiting from the optical fiber outlet 21 of the lower extension tube 20, which may reduce the strength of the glass fiber 3. In particular, when the dew point temperature in the area where the optical fiber manufacturing device is installed is high, more moisture adheres to the glass fiber 3, which increases the frequency of disconnection of the resulting optical fiber.

[0078] Table 1 shows the relationship between the dew point temperature and the disconnection frequency of the region where the optical fiber manufacturing device is installed. In a state where the same device as the optical fiber manufacturing device 1 is used and the dew point temperature of the optical fiber outlet 21 is not managed, devices A to E are prepared with different outlet temperatures of the glass fiber 3 and helium recovery, and the disconnection frequency of the optical fiber is evaluated when the dew point temperature of the region is changed. The disconnection frequency shows the number of disconnections that occurred for 1000 km of optical fiber when a screening test was performed in the process after drawing.

[0079]

Table 1

[0080]

[0081] [Pieces / 1000km]

[0082] As shown in Table 1, it can be seen that when the dew point temperature of the region is low, the disconnection frequency is stable in any of the devices A to E. On the other hand, it can be seen that when the dew point temperature of the region is high, the disconnection frequency of the devices (devices C and D) with high outlet temperatures of the glass fiber 3 becomes high. In addition, it can be seen that when the outlet temperatures of the glass fiber 3 are the same (devices D and E), for the device that does not recover helium (device E), the increase in disconnection frequency when the dew point temperature increases decreases.

[0083] As described above, according to the optical fiber manufacturing method of the present invention, the optical fiber outlet 21 of the lower extension tube 20 is covered by an atmosphere having a dew point temperature of 10° C. or less while drawing. As a result, regardless of the dew point temperature of the region where the optical fiber manufacturing device 1 is installed and the outlet temperature of the glass fiber, it is possible to suppress the adhesion of moisture in the atmosphere to the glass fiber 3 that is output from the optical fiber outlet 21 of the lower extension tube 20. As a result, it is difficult to form scratches on the surface of the glass fiber 3, and it is possible to suppress the reduction in the strength of the obtained optical fiber.

[0084] In addition, when the helium gas introduced into the heating furnace 10 is recovered and reused, as shown in Table 1, the frequency of disconnection increases compared to the case where the helium gas is not recovered. The reason for this is believed to be that the amount of helium gas flowing out of the optical fiber outlet 21 is reduced, so the glass fiber 3 is easily exposed to the atmosphere. However, as described above, the optical fiber outlet 21 is covered with an atmosphere with a dew point temperature of 10° C. or less, so it is possible to suppress the adhesion of moisture in the atmosphere to the glass fiber 3. Therefore, the expensive helium gas can be reused, and the strength reduction of the optical fiber can also be suppressed.

[0085] The temperature of the glass fiber 3 exiting from the optical fiber outlet 21 is preferably above 1300° C. In addition, the temperature of the glass fiber 3 exiting from the optical fiber outlet 21 is preferably below 1700° C. The temperature of the glass fiber 3 exiting from the optical fiber outlet 21 can be controlled by, for example, changing the length of the lower extension tube 20 or changing the temperature and flow rate of the helium gas.

[0086] The higher the outlet temperature of the glass fiber 3 is, the more the reaction between the moisture in the atmosphere and the surface of the glass fiber is promoted, so as shown in Table 1, the frequency of disconnection increases. However, even when the glass fiber 3 is discharged from the optical fiber outlet 21 at a high temperature of 1300°C or more, the optical fiber outlet 21 is covered with an atmosphere with a dew point temperature of 10°C or less, so that the adhesion of moisture to the glass fiber 3 can be suppressed. In addition, by setting the outlet temperature of the glass fiber 3 to 1300°C or more, it is possible to suppress the situation in which the glass fiber 3 is rapidly cooled and the outer diameter changes until it is discharged from the optical fiber outlet 21 of the lower extension tube 20. On the other hand, by setting the outlet temperature of the glass fiber 3 to 1700°C or less, it is possible to suppress the generation of defects on the surface of the glass fiber due to collision with dust in the atmosphere.

[0087] In addition, in this example, the gas G2 whose dew point temperature is controlled to be 10°C or less is supplied to the periphery of the optical fiber lead-out port 21. Thus, the optical fiber lead-out port 21 can be efficiently covered by an atmosphere whose dew point temperature is 10°C or less. Examples of the gas G2 include inert gases such as argon and nitrogen. When an inert gas is used, mixing of the atmosphere into the lower extension tube 20 can be suppressed.

[0088] As a structure for supplying the gas G2 around the optical fiber outlet 21, for example, Figure 3 As shown, the optical fiber manufacturing device 1 may include a gas purification tube 30. The gas purification tube 30 is disposed at the lower end of the lower extension tube 20. The gas purification tube 30 is disposed to connect the outlet of the lower extension tube 20 and the inlet of the gas purification tube 30, and is preferably disposed to be in close contact with the lower extension tube 20. The gas purification tube 30 may be formed integrally with the lower extension tube 20, or may be disposed to be removable relative to the lower extension tube 20. In the gas purification tube 30, the glass fiber 3 exiting from the optical fiber outlet 21 of the lower extension tube 20 passes continuously.

[0089] The gas purification pipe 30 has a gas introduction port 31. The gas introduction port 31 is provided to supply the gas G2 into the gas purification pipe 30. Figure 3In the example of FIG. 3 , two gas inlet ports 31 are provided. A first end portion of a gas pipe 32a is connected to one gas inlet port 31. A first end portion of a gas pipe 32b is connected to the other gas inlet port 31. A portion of the gas pipe 32b is omitted in the figure, and a gas supplier 33 is connected to second ends of the gas pipes 32a and 32b. The gas G2 supplied from the gas supplier 33 is supplied from the gas inlet port 31 into the gas purification pipe 30 through the gas pipes 32a and 32b. The gas G2 supplied into the gas purification pipe 30 is supplied to the periphery of the glass fiber 3 passing through the gas purification pipe 30.

[0090] exist Figure 3 In the example, the gas purification tube 30 has an outer wall 34 and an inner wall 35. The inner wall 35 is provided inside the outer wall 34. A double tube structure is formed by the outer wall 34 and the inner wall 35. Specifically, tubes extending along the traveling direction of the glass fiber 3 are formed by the outer wall 34 and the inner wall 35, respectively. In addition, there is a cavity between the outer wall 34 and the inner wall 35. The inner wall 35 is shorter than the outer wall 34. In addition, the gas inlet 31 is provided on the upper side of the lower end of the inner wall 35 in the outer wall 34. According to the above-mentioned structure, the inner wall 35 suppresses the gas G2 introduced from the gas inlet 31 from directly hitting the glass fiber 3. That is, the gas G2 introduced into the gas purification tube 30 collides with the inner wall 35 and diffuses into the inside of the gas purification tube 30.

[0091] A structure other than the gas purification tube 30 may be used to supply the gas G2 around the optical fiber outlet 21. As another structure for supplying the gas G2 around the optical fiber outlet 21, for example, Figure 4 As shown, the optical fiber manufacturing device 1 may include a chamber 40. The chamber 40 is disposed at the lower end of the lower extension tube 20. The chamber 40 is configured to connect the outlet of the lower extension tube 20 and the inlet of the chamber 40, and is preferably configured to be in close contact with the lower extension tube 20. The chamber 40 may be formed integrally with the lower extension tube 20, or may be configured to be removable relative to the lower extension tube 20. Figure 4 In the example, the entrance of the chamber 40 is set wider than the exit of the lower extension tube 20, and the chamber 40 surrounds the optical fiber outlet 21 of the lower extension tube 20. Inside the chamber 40, the glass fiber 3 exiting from the optical fiber outlet 21 of the lower extension tube 20 passes continuously.

[0092] exist Figure 4In the example of the present invention, the chamber 40 has a rectangular parallelepiped shape extending in the traveling direction of the glass fiber 3. The chamber 40 has a first side surface 41 and a second side surface 42. The second side surface 42 is a surface opposite to the first side surface 41. The glass fiber 3 passes between the first side surface 41 and the second side surface 42. A supply port 43 is provided on the first side surface 41. An exhaust port 44 is provided on the second side surface 42. The exhaust port 44 may be, for example, a slit whose opening size can be changed. The gas G2 is supplied from the supply port 43 and discharged from the exhaust port 44. In other words, the supply port 43 is provided for supplying the gas G2 into the chamber 40, and the exhaust port 44 is provided for exhausting the gas G2 in the chamber 40. As described above, the gas G2 is supplied in a manner of passing through the periphery of the glass fiber 3 from the supply port 43 to the exhaust port 44.

[0093] exist Figure 4 In the example, a first end of the supply pipe 43a is connected to the supply port 43. A gas generating device 45 is connected to a second end of the supply pipe 43a. A first end of the exhaust pipe 44a is connected to the exhaust port 44. A second end of the exhaust pipe 44a is connected to the outside (not shown) of the wire drawing furnace 100.

[0094] The gas generating device 45 is configured to generate gas G2 and supply the generated gas G2 to the supply port 43. In this example, the gas G2 may be an inert gas managed in such a manner that the dew point temperature around the optical fiber outlet 21 is 10° C. or less. The gas G2 may be dry air managed in such a manner that the dew point temperature around the optical fiber outlet 21 is 10° C. or less. Dry air is air in which the water vapor content is reduced by adsorbing water vapor in the air by a desiccant. The desiccant includes at least any one of zeolite, silica gel, and a refrigerated desiccant.

[0095] The gas G2 generated by the gas generating device 45 is supplied from the supply port 43 of the first side 41 into the chamber 40 through the supply pipe 43a. The gas G2 supplied into the chamber 40 is supplied to the periphery of the glass fiber 3 passing through the chamber 40. The gas G2 supplied into the chamber 40 is discharged from the discharge port 44 of the second side 42 through the discharge pipe 44a to the outside of the drawing furnace 100. The gas generating device 45 is an example of an inert gas generating device.

[0096] As described above, the gas G2 is supplied into the chamber 40 covering the optical fiber lead-out port 21. Therefore, the optical fiber lead-out port 21 of the lower extension tube 20 can be more effectively covered by the atmosphere having a dew point temperature of 10°C or less. In addition, the gas G2 is supplied from the supply port 43 and discharged from the discharge port 44, so that a gas flow of the gas G2 is formed in the chamber 40 so as to pass around the glass fiber 3. Therefore, the gas such as dust and cyanide ejected in the drawing furnace 100 is not easily retained.

[0097] exist Figure 4 In the example of the present invention, a plate 46 is further provided in the chamber 40 between the supply port 43 and the position where the glass fiber 3 passes inside the chamber 40. Specifically, the plate 46 extends between the supply port 43 and the glass fiber 3 in the traveling direction of the glass fiber 3. The plate 46 may be directly or indirectly supported by the first side surface 41, or may be directly or indirectly supported by the upper surface of the chamber 40. There is a cavity between the supply port 43 and the plate 46. The length of the plate 46 in the traveling direction of the glass fiber 3 is longer than the opening length of the supply port 43 in the traveling direction of the glass fiber 3. In addition, the supply port 43 is provided on the first side surface 41 at an upper side than the lower end of the plate 46. According to the above-mentioned structure, the plate 46 suppresses the gas G2 supplied from the supply port 43 from directly hitting the glass fiber 3. That is, the gas G2 supplied into the chamber 40 collides with the plate 46 and diffuses into the inside of the chamber 40. Therefore, the linear sway of the glass fiber 3 can be suppressed.

[0098] Furthermore, the chamber 40 may be provided with an opening and closing door 48 on the front surface 47 different from the first side surface 41 and the second side surface 42 . Figure 5 40 is a schematic oblique view of the chamber 40. Figure 5 As shown, an opening and closing door 48 is provided on the front surface 47 of the chamber 40. According to the above structure, the operator can open the opening and closing door 48 to check the inside of the chamber 40, so it is easy to carry out the initial operation of drawing glass fibers from the optical fiber mother material (so-called seeding operation).

[0099] The present invention has been described in detail and with reference to specific embodiments, but it is obvious to those skilled in the art that various changes or modifications can be made without departing from the spirit and scope of the present invention. In addition, the number, position, shape, etc. of the structural components described above are not limited to the above embodiments, and can be changed to the number, position, shape, etc. suitable for implementing the present invention. In addition, the elements included in each example described above can be combined with each other.

[0100] The lower extension pipe 20 may not include the damper mechanism 26 .

[0101] The gas purification pipe 30 has a double pipe structure, but is not limited to this structure.

[0102] The gas G2 may be supplied to the periphery of the optical fiber lead-out port 21 using a structure other than the gas purification tube 30 and the chamber 40 .

[0103] The method of supplying the gas G2 around the optical fiber outlet 21 and the method of setting the chamber 40 are exemplified. However, the optical fiber outlet 21 may be covered with an atmosphere having a dew point temperature of 10° C. or less by using other methods. For example, the air conditioner in the room where the optical fiber manufacturing device 1 is installed may be managed so that the dew point temperature of the entire room is 10° C. or less.

[0104] The optical fiber manufacturing device 1 may include a slow cooling furnace between the drawing furnace 100 and the cooling device, a coating device, and a winding device (none of which are shown in the figure), for slowly lowering the temperature of the glass fiber 3 exiting the drawing furnace 100. Inert gas or dry air may be supplied to the inside of the slow cooling furnace. The chamber 40 may be provided between the drawing furnace 100 and the slow cooling furnace, or between the slow cooling furnace and the cooling device.

[0105] Description of the label

[0106] 1: Optical fiber manufacturing device

[0107] 2: Optical fiber base material

[0108] 3: Fiberglass

[0109] 10: Heating furnace

[0110] 11: Frame

[0111] 12: Furnace core tube

[0112] 13: Heater

[0113] 14: Gas piping

[0114] 15: Inert gas supplier

[0115] 16: Gas inlet

[0116] 20: Lower extension tube

[0117] 21: Optical fiber outlet

[0118] 22: Gas suction port

[0119] 23a, 23b: Gas piping

[0120] 24: Gas regeneration device

[0121] 25: Piping

[0122] 26: Air door mechanism

[0123] 261: Upper air door

[0124] 261a: Through the hole

[0125] 262: Lower air door

[0126] 263: Gas Recovery Space

[0127] 30: Gas purification tube

[0128] 31: Gas inlet

[0129] 32a, 32b: Gas piping

[0130] 33: Gas supply

[0131] 34: Outer wall

[0132] 35: Inner wall

[0133] 40: Chamber

[0134] 41: First side

[0135] 42: Second side

[0136] 43: Supply port

[0137] 43a: Supply pipe

[0138] 44: Exhaust port

[0139] 44a: discharge pipe

[0140] 45: Gas generating device

[0141] 46: Plate

[0142] 47: Front surface

[0143] 48: Open and close doors

[0144] 100: Wire drawing furnace

[0145] G1: Mixed gas

[0146] G2: Gas

Claims

1. A method for producing an optical fiber, wherein a base material for an optical fiber is heated and melted in a drawing furnace to draw a fiber to form a glass fiber, The wire drawing furnace has: a heating furnace for heating and melting the optical fiber base material; and A lower extension tube is disposed at the lower end of the heating furnace and is used for the glass fiber to pass through. The lower extension tube has an optical fiber outlet for the glass fiber to be led out. The optical fiber lead-out port is covered with an atmosphere having a dew point temperature of 10° C. or less while the optical fiber is drawn.

2. The method for manufacturing an optical fiber according to claim 1, wherein: The heating furnace has a gas inlet for introducing a gas containing helium into the heating furnace. The lower extension tube has a gas suction port, which sucks the gas containing helium inside and discharges it to the outside of the lower extension tube. Wire drawing is performed while regenerating and reusing the gas including the helium gas exhausted from the gas suction port.

3. The method for manufacturing an optical fiber according to claim 1 or 2, wherein: The temperature of the glass fiber exiting from the optical fiber outlet is 1300° C. or higher and 1700° C. or lower.

4. The method for producing an optical fiber according to any one of claims 1 to 3, wherein: An inert gas is supplied around the optical fiber outlet.

5. The method for producing an optical fiber according to any one of claims 1 to 4, wherein: An inert gas is supplied into a chamber surrounding the optical fiber lead-out port.

6. The method for manufacturing an optical fiber according to claim 5, wherein: The chamber has a first side and a second side opposite to the first side, The inert gas is supplied from the first side surface and exhausted from the second side surface.

7. An optical fiber drawing device, which heats and melts an optical fiber base material to draw a glass fiber, The wire drawing device comprises: A heating furnace for heating and melting the optical fiber base material; A lower extension tube, which is arranged at the lower end of the heating furnace, allows the glass fiber to pass through the inside and allows the glass fiber to exit from the optical fiber outlet; a chamber, which surrounds the optical fiber outlet and has a supply port for supplying an inert gas to the interior; as well as An inert gas generating device generates the inert gas and supplies the generated inert gas to the supply port.

8. The optical fiber drawing device according to claim 7, wherein: A plate is disposed between the supply port and a location where the glass fiber passes through the interior of the chamber.

9. The optical fiber drawing device according to claim 7 or 8, wherein: An opening and closing door is provided on the front surface of the chamber.

Citation Information

Patent Citations

  • Optical fiber drawing tower provided with optical fiber drawing wire diameter sealing device

    CN105541106A

  • Low-loss large-effective-area fiber and preparation technology therefor

    CN106125192A

  • Device for surface-treating and drawing fluoride optical fiber preform and production of fluoride optical fiber

    JP1994247739A

  • Gas reclamation system for optical fiber production

    US20170101336A1

  • Optical fiber producing method

    US6928840B1