Pellicle frame, pellicle, exposure original plate, exposure device, and method for manufacturing pellicle
Through the combined structure of hard and soft frame members, combined with alternating stacking design and ventilation channels, the exposure area reduction and original pattern offset caused by deformation of protective film tension and support frame are solved, and effective suppression and exposure of strain are achieved. Improvement of quality.
Patent Information
- Application Number
- CN202380027548.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-03-22
- Filing Date
- 2023-03-03
- Publication Date
- 2024-11-15
AI Technical Summary
In the semiconductor exposure process, the tension of the protective film and deformation of the support frame lead to a reduction in the exposure area and the position of the original pattern shift, which is difficult for the prior art to effectively suppress these problems.
Adopting a combined structure of hard frame members and soft frame members, the Young's modulus of hard frame members is higher than that of soft frame members, and is designed by alternately stacked adhesive layers and substrate layers. With a modulus of 25 GPa or above, the soft frame member includes ventilation channels and ventilation filters to reduce recovery force and deformation of the protective membrane assembly frame.
It effectively suppresses strain caused by tension of the protective film and deformation of the protective film assembly frame, prevents strain of the original, and improves exposure quality and pattern accuracy.
Smart Images

Figure CN118974649A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a pellicle assembly frame, a pellicle assembly, an exposure original plate, an exposure device, and a method for manufacturing the pellicle assembly. Background Art
[0002] As the performance of semiconductor exposure processes has become more advanced, the pattern width of semiconductor integrated circuits has been miniaturized. On the other hand, during the exposure process, if foreign matter such as dust adheres to the original plate, poor exposure may occur, resulting in a decrease in the yield of semiconductor integrated circuits. In order to prevent foreign matter such as dust from adhering to the surface of the original plate, a protective film assembly is installed on the original plate as an original plate cover. The protective film assembly includes a support frame, a protective film supported by one end face of the support frame, and an adhesive layer provided on the other end face of the support frame (hereinafter referred to as the "original plate side end face") (for example, Patent Document 1).
[0003] Hereinafter, the support frame and the adhesive layer provided on the other end surface of the support frame may be collectively referred to as a “pellicle frame”.
[0004] Patent Document 1: Japanese Patent Application Publication No. 2014-081454 Summary of the invention
[0005] Problems to be solved by the invention
[0006] When the pellicle is laid on the pellicle assembly frame, a force toward the inside of the pellicle assembly frame is sometimes generated due to the tension of the pellicle. If the support frame is soft, the tension of the pellicle sometimes causes the support frame to be strained toward the inside of the support frame. If the support frame is strained toward the inside, the available exposure area will be reduced accordingly. Therefore, a pellicle assembly frame is required that can minimize the amount of strain toward the inside of the support frame.
[0007] On the other hand, in recent years, the exposure wavelength has been shortened and the pattern width has been miniaturized. If the support frame is hard, when the protective film assembly is attached to the original plate using the adhesive layer, the original plate may be strained due to the deformation of the support frame. As a result, the position of the circuit pattern of the original plate may be shifted.
[0008] In detail, the support frame sometimes has strain in the thickness direction orthogonal to the surface direction of the protective film in a standalone state. When the protective film assembly is attached to the original, the support frame is pressed against the flat part of the original. As a result, the support frame is attached to the original in a state corrected to be flat. In the state where the support frame is corrected to be flat, the support frame has a restoring force that wants to return to the original shape with strain. When the amount of strain in the direction orthogonal to the surface direction of the protective film remains constant, the harder the support frame (that is, the higher the bending rigidity of the support frame), the greater the restoring force. If the restoring force is large, the original may be strained due to the deformation of the support frame. Therefore, a protective film assembly frame with reduced bending rigidity is required.
[0009] The present disclosure has been completed in view of the above circumstances.
[0010] An embodiment of the present disclosure aims to provide a pellicle assembly frame, a pellicle assembly, and a method for manufacturing a pellicle assembly that can suppress strain caused by tension of the pellicle and suppress strain of an original plate caused by deformation of the pellicle assembly frame.
[0011] Solutions to Solve Problems
[0012] Means for solving the above-mentioned problems include the following embodiments.
[0013] <1> A pellicle assembly frame, comprising:
[0014] A rigid frame member for supporting the protective film, and
[0015] A soft frame member connected to the aforementioned hard frame member and used to connect to the original plate with a pattern,
[0016] The soft frame member is formed by alternately stacking a base material layer and an adhesive layer in a thickness direction perpendicular to the surface direction of the protective film, with the adhesive layer arranged at both ends.
[0017] The Young's modulus of the aforementioned hard frame member is higher than the apparent Young's modulus of the aforementioned soft frame member.
[0018] The Young's modulus of the rigid frame member is 25 GPa or more.
[0019] <2> The pellicle assembly frame according to <1> above, wherein the rigid frame member is made of a single material.
[0020] <3> In the pellicle assembly frame according to <1> or <2>, the hard frame member has a Young's modulus of 90 GPa or more.
[0021] <4> The pellicle assembly frame according to any one of <1> to <3>, wherein the ratio of the height of the rigid frame member to the height of the pellicle assembly frame is 15% to 65%.
[0022] <5> The pellicle frame according to any one of <1> to <4>, wherein the total number of the base material layer and the number of the adhesive layer is 5 or more.
[0023] <6> The pellicle frame according to any one of <1> to <5>, wherein the thickness of each of the adhesive layers is 0.01 mm to 0.5 mm.
[0024] <7> The pellicle frame according to any one of <1> to <6>, wherein the total thickness of the adhesive layers included in the soft frame member is 0.2 to 4 times the total thickness of the base material layers included in the soft frame member.
[0025] <8> In the pellicle frame according to any one of <1> to <7>, the Young's modulus of the base layer is not less than 10,000 times and not more than 9,000,000 times the Young's modulus of the adhesive layer.
[0026] <9> The pellicle frame according to any one of <1> to <8>, wherein the thickness of each of the base material layers is 2.5 mm or less.
[0027] <10> The pellicle frame according to any one of <1> to <9>, wherein a surface of the adhesive layer satisfies any one of the following (A) to (C).
[0028] (A) an inorganic layer is formed on at least the inner wall surface of the adhesive layer;
[0029] (B) at least the inner wall surface of the adhesive layer satisfies the following formula (1);
[0030] (C) At least the inner wall surface of the adhesive layer satisfies the following formula (2):
[0031] Formula (1): ([CNO - 2s ] / [CNO - 50s ])≥2.00
[0032] (In the above formula (1),
[0033] [CNO - 2s ] indicates the use of time-of-flight secondary ion mass spectrometry and the use of an ion source of Bi3 ++The CNO obtained by analyzing the first deep portion at a first depth from the surface of the adhesive layer using a primary ion gun with an irradiation area of 100 μm×100 μm - The standardized intensity of
[0034] The first depth is formed by irradiating a 600 μm square area of the surface with a sputtering ion gun using an argon cluster ion beam with a beam voltage of 20 kV and a beam current of 20 nA for a cumulative period of 2 seconds.
[0035] [CNO - 50s ] represents CNO obtained by analyzing the second deep part of the second depth using time-of-flight secondary ion mass spectrometry. - The standardized intensity of
[0036] The second depth is formed by irradiating the region with the sputtering ion gun for a cumulative 50 seconds.
[0037] Formula (2):
[0038] (In the above formula (2),
[0039] C3 is obtained by analyzing the first deep part using time-of-flight secondary ion mass spectrometry. - The standardized intensity of
[0040] C3 is obtained by analyzing the second deep part using time-of-flight secondary ion mass spectrometry. - The normalized intensity of .
[0041] <11> In the pellicle assembly frame according to any one of <1> to <10>, the soft frame member includes a ventilation passage penetrating the soft frame member, or includes the ventilation passage and a ventilation filter disposed in the ventilation passage.
[0042] <12> A pellicle assembly comprising:
[0043] The pellicle assembly frame as described in any one of <1> to <11> above, and
[0044] A protective membrane supported by the aforementioned rigid frame member.
[0045] <13> An exposure original plate, comprising:
[0046] Original with pattern, and
[0047] The pellicle assembly described in <12> above is attached to the surface of the original plate having the pattern.
[0048] <14> An exposure device comprising:
[0049] a light source for emitting exposure light,
[0050] The exposure original plate described in <13>, and
[0051] an optical system for guiding the exposure light emitted by the light source to the exposure original plate;
[0052] The exposure original plate is arranged so that the exposure light emitted from the light source is transmitted through the protective film and irradiated onto the original plate.
[0053] <15> A method for manufacturing a pellicle assembly, which is the method for manufacturing a pellicle assembly described in <12> above, comprising:
[0054] The process of preparing the aforementioned hard frame member;
[0055] A lamination step of alternately laminating at least one substrate layer sheet and a plurality of adhesive layers in the thickness direction to form a laminate;
[0056] a punching step of punching the laminated body so as to form exposure through holes along the thickness direction to form the soft frame member; and
[0057] A connecting step of connecting the hard frame member and the soft frame member.
[0058] <16> The method for manufacturing a protective film assembly as described in <15> above, which includes at least one of the following steps: a step of coating an inorganic layer on at least the inner wall surface of the aforementioned adhesive layer; a step of performing plasma nitridation treatment on at least the inner wall surface of the aforementioned adhesive layer; and a step of performing extreme ultraviolet irradiation treatment on at least the inner wall surface of the aforementioned adhesive layer.
[0059] <17> The method for manufacturing a protective membrane assembly as described in <15> or <16> above, wherein the soft frame member includes a ventilation channel penetrating the soft frame member,
[0060] The aforementioned adhesive layer is an adhesive layer sheet,
[0061] The manufacturing method includes a ventilation channel processing step, in which at least one unprocessed sheet for a substrate layer and a plurality of unprocessed sheets for adhesive layers are processed in a manner to form the ventilation channel, thereby forming the at least one substrate layer sheet and the plurality of adhesive layer sheets.
[0062] The ventilation channel processing step is performed before the lamination step.
[0063] <18> The method for manufacturing a pellicle assembly as described in <17> above, wherein the soft frame member includes the ventilation channel and a ventilation filter disposed in the ventilation channel,
[0064] The manufacturing method includes a filter fixing step, in which the ventilation filter is arranged on a part of the at least one substrate layer sheet or the plurality of adhesive layer sheets in such a manner that the ventilation filter is arranged in the ventilation passage.
[0065] The filter fixing step is performed after the ventilation duct processing step and before the laminating step.
[0066] Effects of the Invention
[0067] According to the present disclosure, a pellicle assembly frame, a pellicle assembly, an exposure original plate, an exposure device, and a method for manufacturing a pellicle assembly are provided, which can suppress strain caused by tension of the pellicle and can suppress strain of the original plate caused by deformation of the pellicle assembly frame. BRIEF DESCRIPTION OF THE DRAWINGS
[0068] Figure 1 This is a cross-sectional view of a laminate having a three-layer structure for explaining a method for calculating the apparent Young's modulus (E) of a laminate stacked horizontally.
[0069] Figure 2 This is a cross-sectional view of a laminate having a three-layer structure for explaining a method for calculating the apparent Young's modulus (E) of a laminate stacked horizontally.
[0070] Figure 3 This is a cross-sectional view of a calculation model having the same stacked structure as the pellicle frame of the first embodiment of the present disclosure.
[0071] Figure 4 is a cross-sectional view of a pellicle assembly according to a second embodiment of the present disclosure.
[0072] Figure 5 is a cross-sectional view of a pellicle assembly according to a third embodiment of the present disclosure.
[0073] Figure 6 is a cross-sectional view of a pellicle assembly according to a fourth embodiment of the present disclosure.
[0074] Figure 7 is a cross-sectional view of a pellicle assembly according to a fifth embodiment of the present disclosure.
[0075] Figure 8 This is a cross-sectional view of the pellicle assembly of Reference Example 1. DETAILED DESCRIPTION
[0076] In the present disclosure, a numerical range expressed using "to" means a range including the numerical values described before and after "to" as the minimum value and the maximum value, respectively.
[0077] In the numerical ranges recorded in stages in this disclosure, the upper limit or lower limit recorded in one numerical range can be replaced by the upper limit or lower limit of the numerical range recorded in other stages. In the numerical ranges recorded in this disclosure, the upper limit or lower limit recorded in one numerical range can be replaced by the value shown in the embodiments.
[0078] In the present disclosure, a combination of two or more preferred embodiments is a more preferred embodiment.
[0079] In the present disclosure, when there are a plurality of substances corresponding to each component, the amount of each component means the total amount of the plurality of substances unless otherwise specified.
[0080] In the present disclosure, the term "process" includes not only an independent process but also a process that cannot be clearly distinguished from other processes as long as the intended purpose of the process can be achieved.
[0081] (1) Protective film assembly frame
[0082] The protective film assembly frame disclosed in the present invention has a hard frame member for supporting the protective film and a soft frame member for attaching to an original plate having a pattern. The soft frame member is connected to the aforementioned hard frame member. The aforementioned soft frame member is formed by alternately stacking a base material layer and an adhesive layer in a thickness direction orthogonal to the surface direction of the aforementioned protective film in such a manner that the aforementioned adhesive layer is arranged at both ends. The Young's modulus of the aforementioned hard frame member is higher than the apparent Young's modulus of the aforementioned soft frame member. The Young's modulus of the aforementioned hard frame member is greater than 25 GPa.
[0083] In the present disclosure, the so-called "orthogonal" is not limited to the case where the intersection is 90°, but also includes the case where the intersection is within the angle range of 90±5°.
[0084] In the present disclosure, "Young's modulus of a rigid frame member" refers to the Young's modulus of the material of a rigid frame member of a single-layer structure or the Young's modulus of the material of a rigid frame member of a multi-layer structure. In the case where the rigid frame member is a multi-layer structure, it is the Young's modulus when the multiple materials of the rigid frame member of the multi-layer structure are regarded as one material, and represents the value calculated based on the calculation method of the apparent Young's modulus (E) of the horizontally stacked laminate.
[0085] In the present disclosure, the so-called "apparent Young's modulus of the soft frame member" is the Young's modulus when the multiple materials of the soft frame member as a multi-layer structure are regarded as one material, and represents the value calculated based on the calculation method of the apparent Young's modulus (E) of the horizontally stacked laminate. The details of the calculation method of the apparent Young's modulus will be described later.
[0086] Since the pellicle assembly frame of the present disclosure has the above-described structure, it is possible to suppress strain caused by tension of the pellicle and suppress strain of the original plate caused by deformation of the pellicle assembly frame.
[0087] It is speculated that this is mainly based on the following reasons.
[0088] When the protective film is laid on the protective film assembly frame, sometimes a force toward the inside of the protective film assembly frame is generated due to the tension of the protective film. In the protective film assembly frame disclosed in the present invention, the protective film is supported by a hard frame member that is harder than the soft frame member. Furthermore, the Young's modulus of the hard frame member is greater than 25 GPa. Therefore, the protective film assembly frame disclosed in the present invention is not easy to generate strain toward the inside of the protective film assembly frame due to the tension of the protective film. As a result, the protective film assembly frame disclosed in the present invention can suppress the strain caused by the tension of the protective film. Therefore, it is speculated that the protective film assembly frame disclosed in the present invention can prevent the reduction of the exposure area.
[0089] When the protective film assembly (hereinafter sometimes referred to as "protective film assembly") of the present invention is attached to the original plate, the protective film assembly frame is pressed against the flat portion of the original plate. Thus, the protective film assembly frame is attached to the original plate in a state corrected to be flat. In the state in which the protective film assembly frame is corrected to be flat, the protective film assembly frame has a restoring force that wants to return to the original shape with strain. In the protective film assembly frame of the present invention, a soft frame member that is softer than a hard frame member is directly attached to the flat portion of the original plate. Therefore, compared with the case where the soft frame member and the hard frame member have the same hardness, the restoring force can be alleviated. It is speculated that as a result, the protective film assembly frame of the present invention can reduce the restoring force generated by being attached to the original plate. Therefore, the protective film assembly frame of the present invention can suppress the strain of the original plate caused by the deformation of the protective film assembly frame attached to the original plate.
[0090] The pellicle assembly frame is a rectangular cylindrical object. The pellicle assembly frame has an exposure through hole. The exposure through hole is formed by the hollow part of the pellicle assembly frame, and represents the space through which the light passing through the pellicle passes to reach the original plate.
[0091] The shape of the pellicle assembly frame when viewed from the thickness direction is rectangular. The rectangular shape may be a square or a rectangular. "Rectangle" means a right-angled quadrilateral. "Square" means a shape in which the lengths of the four sides constituting the rectangle are equal. Rectangle means a shape other than a square in a rectangle.
[0092] The rectangular shape of the pellicle frame when viewed from the thickness direction is composed of four sides.
[0093] The length of one side in the long side direction (hereinafter referred to as "the length of one side") is preferably 200 mm or less. The dimensions of the pellicle assembly frame and the like can be standardized according to the type of exposure apparatus. When the length of one side of the pellicle assembly frame is 200 mm or less, it satisfies the dimensions standardized for exposure using extreme ultraviolet (EUV: Extreme Ultra Violet) light (wavelength: 3 nm to 30 nm) (hereinafter referred to as "EUV exposure").
[0094] The length of one side in the short-side direction (hereinafter referred to as "the width of one side") may be, for example, 5 mm to 180 mm, preferably 80 mm to 170 mm, and more preferably 100 mm to 160 mm.
[0095] The height of the pellicle assembly frame (i.e., the length of the pellicle assembly frame in the thickness direction) is preferably 2.5 mm or less, and more preferably 2.4 mm or less. Thus, the pellicle assembly frame meets the dimensions standardized for EUV exposure. The height of the pellicle assembly frame standardized for EUV exposure is, for example, 2.375 mm.
[0096] The mass of the pellicle frame is preferably 15 g or less. Therefore, the pellicle frame is suitable for EUV exposure applications.
[0097] The pellicle assembly frame of the present disclosure includes a hard frame member and a soft frame member. The hard frame member and the soft frame member are stacked in the thickness direction.
[0098] (1.1) Rigid frame components
[0099] The rigid frame member is used to support the protective film assembly frame.
[0100] The “hard” in the hard frame member means that it has a harder property in relative comparison with the soft frame member.
[0101] The material and shape of the hard frame member are not particularly limited as long as they can support the protective film. The hard frame member is preferably composed of a single material. Thus, a hard frame member connected to a protective film can be prepared with high productivity. For example, a portion of the hard frame member can be prepared as a supporting substrate, and after forming a protective film on the supporting substrate, a portion of the supporting substrate is removed by etching, thereby preparing a supporting substrate connected to the protective film.
[0102] The Young's modulus of the rigid frame member is 25 GPa or more. Thus, the rigid frame member has sufficient hardness. Therefore, even if the pellicle membrane is laid on the rigid frame member, the pellicle assembly frame is unlikely to be strained by the tension of the pellicle membrane.
[0103] The Young's modulus of the rigid frame member is more preferably 50 GPa or more. The Young's modulus of the rigid frame member is 50 GPa or more, so that even if the protective film is laid on the rigid frame member, the protective film assembly frame is not easy to be strained inwardly due to the tension of the protective film. The Young's modulus of the rigid frame member is further preferably 90 GPa or more. The Young's modulus of the rigid frame member is 90 GPa or more, so that even if the protective film is laid on the rigid frame member, the protective film assembly frame is not easy to be strained inwardly due to the tension of the protective film.
[0104] The Young's modulus of the rigid frame member is more preferably 90 GPa to 300 GPa, and further preferably 150 GPa to 300 GPa.
[0105] Examples of materials having a Young's modulus of 25 GPa or more include glass, aluminum, titanium, titanium alloy, silicon, stainless steel, polyethylene, acrylic resin, vinyl chloride resin, polystyrene resin, and the like.
[0106] Examples of materials having a Young's modulus of 50 GPa or more include glass, aluminum, titanium, titanium alloy, silicon, and stainless steel.
[0107] Examples of materials having a Young's modulus of 90 GPa or more include titanium, titanium alloys, silicon, and stainless steel.
[0108] Examples of materials having a Young's modulus of 150 GPa or more include silicon and stainless steel.
[0109] The Young's modulus of the rigid frame member is determined by a tensile test (JIS G0567J). If the rigid frame member is made of resin, the Young's modulus is determined by a three-point bending test (JIS K7171). Whether the rigid frame member is made of resin is determined by whether the rigid frame member undergoes thermal decomposition at 550°C.
[0110] Examples of materials for the rigid frame member include metal materials (e.g., aluminum, titanium, stainless steel, etc.), ceramic materials (e.g., silicon, glass, etc.), and resins (e.g., polyethylene resins, acrylic resins, vinyl chloride resins, polystyrene resins, etc.).
[0111] Among them, from the viewpoint of not having a large amount of water content and being able to suppress the amount of outgassing, the material of the hard frame member preferably includes aluminum, titanium, stainless steel, silicon, or glass, and more preferably includes aluminum, titanium, or silicon.
[0112] From the perspective of reducing the water content and suppressing the amount of outgassing, the surface of the hard frame member can be subjected to a known surface treatment to make the surface of the hard frame member hydrophobic, or it can be coated with a material with a low water content (for example, an inorganic material, a ceramic material, etc.).
[0113] The height of the hard frame member (i.e., the length of the hard frame member in the thickness direction) is not particularly limited. From the perspective of suppressing the strain of the original plate caused by the deformation of the protective film assembly frame and suppressing the strain caused by the tension of the protective film, it is preferably 0.3 mm to 1.5 mm, and more preferably 0.5 mm to 1.0 mm.
[0114] The ratio of the height of the hard frame member to the height of the protective film assembly frame (hereinafter referred to as "the height ratio of the hard frame member") is not particularly limited. From the viewpoint of suppressing the strain of the original plate caused by the deformation of the protective film assembly frame, it is preferably 65% or less, more preferably 60% or less, further preferably 50% or less, and particularly preferably 45% or less.
[0115] From the viewpoint of suppressing strain caused by tension of the pellicle membrane, the height ratio of the rigid frame member is preferably 15% or more, more preferably 20% or more, and even more preferably 25% or more.
[0116] From these viewpoints, the height ratio of the rigid frame member is preferably 15% to 65%, more preferably 20% to 65%, further preferably 25% to 65%, particularly preferably 25% to 50%, and even more preferably 28% to 45%.
[0117] (1.2) Soft frame components
[0118] The soft frame member is used to attach the protective film assembly to the original plate with a pattern. The soft frame member is connected to the hard frame member. The original plate will be described later.
[0119] The “soft” in the soft frame member means that it has a relatively soft property in comparison with the hard frame member.
[0120] The soft frame member is formed by alternately laminating base material layers and adhesive layers in a thickness direction perpendicular to the surface direction of the pellicle so that the adhesive layers are arranged at both ends.
[0121] The material and shape of the soft frame member are not particularly limited as long as they can support the pellicle membrane.
[0122] The apparent Young's modulus of the soft frame member is less than 25 GPa. Therefore, the soft frame member is sufficiently soft. Therefore, even if the pellicle assembly is attached to the original plate, the restoring force will be further reduced.
[0123] The apparent Young's modulus of the soft frame member is more preferably 1 GPa to 15 GPa, and further preferably 3 GPa to 10 GPa.
[0124] (1.2.1) Calculation method of apparent Young's modulus of pellicle assembly frame
[0125] The apparent Young's modulus of the protective film assembly frame is calculated based on the calculation method of the apparent Young's modulus (E) of the horizontally stacked stack. In detail, first, a calculation model having the same stacking structure as the protective film assembly frame is imported. Then, based on the calculation method of the apparent Young's modulus (E) of the horizontally stacked stack, the apparent Young's modulus of the calculation model is calculated. The calculated apparent Young's modulus of the calculation model is regarded as the apparent Young's modulus of the protective film assembly frame of the present disclosure. The calculated apparent Young's modulus of the soft frame member of the calculation model is regarded as the apparent Young's modulus of the soft frame member in the present disclosure.
[0126] Hereinafter, a method for calculating the apparent Young's modulus (E) of a horizontally stacked laminate and a method for calculating the apparent Young's modulus of a calculation model will be described in order.
[0127] (1.2.1.1) Calculation method of apparent Young's modulus of horizontally stacked laminate
[0128] Reference Figure 1 and Figure 2 , a method for calculating the apparent Young's modulus (E) of a horizontally stacked laminate is described. Figure 1 and Figure 2 This is a cross-sectional view of a laminate having a three-layer structure for explaining a method for calculating the apparent Young's modulus (E) of a laminate stacked horizontally. Figure 2 express Figure 1 Strain distribution in the stack shown.
[0129] The bending rigidity (EI) of the laminate can be calculated by taking the bending rigidity (EI) of each sawn board. i I i ) is calculated by the sum of .
[0130] In order to calculate the section moment of inertia (I i ), determine the neutral axis position (λ) of the stack. Figure 1 and Figure 2 The basic assumption of mid-beam bending is that within the elastic limit, equation (i) holds true.
[0131] [Number 1]
[0132]
[0133] In formula (i), “ρ” represents the radius of curvature caused by the bending moment (refer to Figure 2 ), "λ" represents the distance from the upper edge of the laminate to the neutral axis (refer to Figure 1 ), "y" represents the coordinate from the top edge of the stack downward (refer to Figure 1 ), “ε y ” represents the vertical strain in y, “σ y ” represents the vertical stress in y, and “E” represents the apparent Young’s modulus of the laminate.
[0134] Figure 1 and Figure 2 In a laminate having a three-layer structure, in any cross section, formula (ii) holds true. Therefore, the following formula (iii) holds true.
[0135] [Number 2]
[0136]
[0137] In formula (ii), “E x " represents the Young's modulus of each layer (the Xth layer from one end surface of the laminate), "h x " represents the length between one end face of the stack and the surface on the other end face side of the stack counted from the one end face of the stack (refer to Figure 1 ), "b" represents the width of the laminate (refer to Figure 1 ). X represents an integer of 1 to 3.
[0138] [Number 3]
[0139]
[0140] In formula (iii), "h" represents the length from one end face to the other end face of the laminate (see Figure 1 ).
[0141] If the formula (iii) is generalized, when n layers of sawn boards are stacked, the neutral axis position (λ) can be expressed by the formula (iv), where n represents a natural number.
[0142] [Number 4]
[0143]
[0144] In formula (iv), t i Indicates (h i -h i-1 ), h0(h i-1 (in the case where i=1) is 0.
[0145] The bending rigidity (EI) of the laminate is the bending rigidity of each saw blade related to the determined neutral axis position, E i I iThe sum of is expressed by the following formula (v).
[0146] [Number 5]
[0147]
[0148] The apparent Young's modulus (E) of the laminate is obtained by dividing the formula (v) by the section moment of inertia (bh 3 / 12) is calculated and represented by the following formula (vi).
[0149] [Number 6]
[0150]
[0151] Using the parameters of the soft frame member, the bending rigidity of the soft frame member can be calculated by equation (v).
[0152] Using the parameters of the soft frame member, the apparent Young's modulus of the soft frame member can be calculated by formula (vi). Using the parameters of the hard frame member and the soft frame member, the bending rigidity of the protective membrane assembly frame can be calculated by formula (v). Using the parameters of the hard frame member and the soft frame member, the apparent Young's modulus of the protective membrane assembly frame can be calculated by formula (vi).
[0153] (1.2.2) Calculation method of apparent Young's modulus and bending rigidity of pellicle assembly frame
[0154] Specifically, refer to Figure 3 , a method for calculating the apparent Young's modulus of the pellicle assembly frame and the bending rigidity of the pellicle assembly frame is described. Figure 3 This is a cross-sectional view of a calculation model having the same stacked structure as the pellicle frame of the first embodiment of the present disclosure.
[0155] The protective membrane assembly frame of the first embodiment is a rectangular cylindrical object. The protective membrane assembly frame of the first embodiment is an assembly, which includes a soft frame member 11X and a hard frame member 12A. The soft frame member 11X and the hard frame member 12A are stacked in the thickness direction of the protective membrane assembly frame of the first embodiment. The Young's modulus of the hard frame member 12A is higher than the apparent Young's modulus of the soft frame member 11X. The Young's modulus of the hard frame member 12A is greater than 25 GPa.
[0156] The soft frame member 11X is formed by alternately stacking (m+1) adhesive layers 111 and m base layers 112 in the thickness direction of the protective film assembly frame of the first embodiment, with the adhesive layers 111 arranged at both ends. m represents a natural number. The total number of base layers 112 and adhesive layers 111 is (2m+1).
[0157] The number of layers constituting the rigid frame member 12A is one.
[0158] That is, the number of layers constituting the pellicle of the first embodiment is (2m+2).
[0159] like Figure 3 As shown, the calculation model 10X is Figure 1 The stacked structure of the calculation model 10X is the same as the stacked structure of the pellicle frame of the first embodiment.
[0160] Figure 3 In the figure, the symbol "h1" indicates the length of the thickness of the first layer (i.e., the thickness of one adhesive layer 111) counted from the surface S13 on the opposite side of the contact surface S12 where the hard frame member 12A contacts the soft frame member 11X in the thickness direction of the calculation model 10X. The symbol "t1" indicates the length of the symbol "h1".
[0161] Symbol "h2" indicates the length from the surface S13 opposite to the contact surface S12 to the thickness of the second layer (ie, the total thickness of one adhesive layer 111 and one base layer 112). Symbol "t2" indicates the length obtained by subtracting h1 from h2.
[0162] Symbol "h 2m "" represents the length of the thickness from the surface S13 on the opposite side of the contact surface S12 to the (2m)th layer (that is, the total thickness of the m adhesive layers 111 and the thickness of the m base material layers 112).
[0163] Symbol "h 2m+1 " represents the length of the thickness from the surface S13 on the opposite side of the contact surface S12 to the (2m+1)th layer (that is, the thickness of the soft frame member 11X). The symbol "t 2m+1 " indicates that from h 2m+1 Subtract h 2m After the length.
[0164] The number of layers n of the pellicle frame (ie, calculation model 10X) of the first embodiment is the sum of the number of layers of the hard frame member 12A and the number of layers of the soft frame member 11X. n represents a natural number.
[0165] When the number of layers of the rigid frame member 12A is p layers, the number of layers of the soft frame member 11X, i.e., 2m+1 plus p (2m+1+p), becomes the number of layers of the protective membrane assembly frame (i.e., the calculation model 10X) of the first embodiment. p represents a natural number. When the number of layers of the rigid frame member 12A is 1 layer, the number of layers of the soft frame member 11X, i.e., 2m+1 plus 1 (2m+2), becomes the number of layers of the protective membrane assembly frame (i.e., the calculation model 10X) of the first embodiment. The rigid frame member 12A may also be formed of more than 2 layers.
[0166] (1.2.2.1) Apparent Young's modulus of pellicle assembly frame
[0167] The apparent Young's modulus of the pellicle frame (ie, calculation model 10X) is calculated using the above-mentioned formula (iv) and formula (vi).
[0168] First, the neutral axis position (λ) is calculated using equation (iv).
[0169] In the first embodiment, in the formula (iv), "n" corresponds to the number of layers of the calculation model 10X. When the number of layers of the rigid frame member 12A is p, "h1 to h n ” corresponds to h1~h of the calculation model 10X 2m+1+p . "t1~t n ” corresponds to t1~t of the calculation model 10X 2m+1+p When the number of layers of the rigid frame member 12A is 1, "h1 to h n ” corresponds to h1~h of the calculation model 10X 2m+2 . "t1~t n ” corresponds to t1~t of the calculation model 10X 2m+2 .
[0170] Hereinafter, a case where the number of layers of the rigid frame member 12A is one will be described.
[0171] "Ei when i is an odd number" corresponds to the Young's modulus of the adhesive layer 111 of the calculation model 10X. "Ei when i is an even number" corresponds to the Young's modulus of the base material layer 112 of the calculation model 10X in principle. Among them, "Ei when i is 2m+2" corresponds to the Young's modulus of the hard frame member 12A of the calculation model 10X.
[0172] Next, using the formula (vi), the apparent Young's modulus (E) of the calculation model 10X is calculated.
[0173] In the first embodiment, in the formula (vi), "h" corresponds to h of the calculation model 10X. 2m+2 (That is, the total thickness of the soft frame member 11X and the hard frame member 12A). "n" corresponds to (2m+2) of the calculation model 10X. "E when i is an odd number i ” corresponds to the Young's modulus of the adhesive layer 111 of the calculation model 10X. “E when i is an even number i ” corresponds in principle to the Young’s modulus of the base material layer 112 of the calculation model 10X. Here, “E when i is 2m+2 i " corresponds to the Young's modulus of the rigid frame member 12A of the calculation model 10X." h1 to h n” corresponds to h1~h of the calculation model 10X 2m+2 "λ" corresponds to the neutral axis position (λ) of the calculation model 10X calculated using the formula (iv).
[0174] The calculated apparent Young's modulus (E) of the calculation model 10X is regarded as the apparent Young's modulus of the pellicle frame.
[0175] (1.2.2.2) Calculation method of bending rigidity
[0176] The bending rigidity of the pellicle assembly frame (ie, calculation model 10X) is calculated using the above-mentioned equations (iv) and (v).
[0177] First, the neutral axis position (λ) of the calculation model 10X is calculated using the formula (iv) in the same manner as the calculation method of the apparent Young's modulus of the calculation model 10X.
[0178] Next, the bending rigidity (EI) of the calculation model 10X is calculated using the formula (v).
[0179] In the first embodiment, in formula (v), "b" corresponds to the width of the calculation model 10X. The width of the calculation model 10X represents the width of one side of the protective film assembly frame of the first embodiment. In the first embodiment, the width of one side (short side) of the soft frame member 11X is the same as the width of one side (short side) of the hard frame member 12A. "n" corresponds to (2m+2) of the calculation model 10X. "E when i is an odd number i ” corresponds to the Young’s modulus of the adhesive layer 111 of the calculation model 10X. “E when i is an even number i ” corresponds in principle to the Young’s modulus of the base material layer 112 of the calculation model 10X. Here, “E when i is 2m+2 i " corresponds to the Young's modulus of the rigid frame member 12A of the calculation model 10X." h1~h n ” corresponds to h1~h of the calculation model 10X 2m+2 "λ" corresponds to the neutral axis position (λ) of the calculation model 10X calculated using the formula (iv).
[0180] The calculated bending rigidity (EI) of calculation model 10X is regarded as the bending rigidity of the pellicle frame. The closer the bending rigidity of the pellicle frame is to 0, the more the strain of the original plate caused by the deformation of the pellicle frame can be suppressed.
[0181] The apparent Young's modulus of the soft frame member 11X and the bending rigidity of the soft frame member 11X can be calculated by the same method except that the hard frame member is not considered in the calculation method of the Young's modulus of the pellicle assembly frame and the calculation method of the bending rigidity of the pellicle assembly frame (that is, the calculation model 10Y is used instead of the calculation model 10X). The calculation model 10Y has the same structure as the calculation model 10X except that it does not have the hard frame member 12A.
[0182] The Young's modulus of the hard frame member 12A and the bending rigidity of the hard frame member 12A can be calculated using the same method as described above, except that the soft frame member 11X of the calculation model 10X is not considered in the calculation method of the Young's modulus of the pellicle assembly frame and the calculation method of the bending rigidity of the pellicle assembly frame.
[0183] (1.2.3) Ventilation channels and ventilation filters
[0184] The soft frame member preferably includes a ventilation channel, or includes a ventilation channel and a ventilation filter. The ventilation channel passes through the soft frame member. The ventilation filter is arranged in the ventilation channel.
[0185] When the pellicle assembly is attached to the original plate, the ventilation channel connects the internal space of the pellicle assembly with the external space of the pellicle assembly. The "internal space of the pellicle assembly" refers to the space surrounded by the pellicle assembly and the original plate. The "external space of the pellicle assembly" refers to the space not surrounded by the pellicle assembly and the original plate.
[0186] When the pellicle assembly is attached to the original plate, a pressure difference may occur between the inner space of the pellicle assembly and the outer space of the pellicle assembly. In this case, the pellicle may relax or expand. By making the soft frame member include a ventilation channel, the pressure difference between the inner space of the pellicle assembly and the outer space of the pellicle assembly can be suppressed.
[0187] By making the soft frame member include a ventilation channel and a ventilation filter, the pressure difference between the internal space of the protective membrane assembly and the external space of the protective membrane assembly can be suppressed, and foreign matter can be suppressed from mixing from the external space of the protective membrane assembly into the internal space of the protective membrane assembly. EUV exposure is performed in a vacuum atmosphere. If the area of the ventilation filter is large enough, the time required to make the internal space of the protective membrane assembly into a vacuum can be shortened during EUV exposure.
[0188] The number of ventilation channels is not particularly limited. At least one ventilation channel may be formed on each of the four side surfaces of the pellicle frame.
[0189] A ventilation filter is a filter that allows gas to pass through but does not allow foreign matter such as dust to pass through.
[0190] As a ventilation filter, there is no limitation as long as it can prevent foreign matter from mixing into the internal space of the protective membrane component from the external space of the protective membrane component. For example, membrane ventilation filters such as HEPA ventilation filters (High Efficiency Particulate Air Filter) and ULPA ventilation filters (Ultra Low Penetration Air Filter), non-woven ventilation filters, ceramic ventilation filters, glass ventilation filters, metal sintered ventilation filters, ceramic ventilation filters, glass ventilation filters, metal sintered ventilation filters, hollow paper ventilation filters, etc. can be cited.
[0191] The ventilation filter preferably has an initial pressure loss of 100 Pa to 550 Pa and a particle capture rate of 99.7% to 100% for particles with a particle diameter of 0.15 μm to 0.3 μm.
[0192] Regarding the ventilation duct and the ventilation filter, reference can be made to the ventilation duct and the ventilation filter described in International Publication No. 2019-188445.
[0193] The method for fixing the vent filter is not particularly limited, but it is preferably fixed to the soft frame member so that the vent filter covers the ventilation passage, and examples thereof include the first to fourth fixing methods.
[0194] The first fixing method is a method of dividing one adhesive layer into two in the thickness direction of the pellicle frame and sandwiching the vent filter between the divided adjacent adhesive layers to fix the vent filter.
[0195] The second fixing method refers to a method of fixing the vent filter by bringing the vent filter into contact with at least one adhesive layer exposed in the ventilation passage.
[0196] The third fixing method is a method of fixing the vent filter by bringing the vent filter into contact with the same surface of one adhesive layer exposed in the ventilation passage.
[0197] The fourth fixing method is a method of fixing the vent filter by welding the vent filter to the same surface of one base material layer exposed in the ventilation passage.
[0198] Among them, in order to suppress the risk of the ventilation filter not being covered by the ventilation filter (i.e., the occurrence of gaps) in the ventilation passage due to the unevenness of the ventilation filter, the third and fourth fixing methods are preferred. In order to further reduce the occurrence of outgassing, the fourth fixing method is more preferred.
[0199] (1.2.4) Height of soft frame components
[0200] The height of the soft frame member (that is, the length of the soft frame member in the thickness direction) is not particularly limited.
[0201] From the viewpoint of suppressing strain caused by tension of the pellicle membrane and suppressing strain of the original plate caused by deformation of the pellicle assembly frame, the height of the soft frame member is preferably 0.9 mm to 2.0 mm, more preferably 1.4 mm to 1.9 mm.
[0202] The ratio of the height of the soft frame member to the height of the pellicle assembly frame (hereinafter referred to as "height ratio of the soft frame member") is not particularly limited.
[0203] From the viewpoint of suppressing strain caused by tension of the pellicle membrane and suppressing strain of the original plate caused by deformation of the pellicle assembly frame, the height ratio of the soft frame member is preferably 40% to 90%, more preferably 60% to 80%.
[0204] (1.2.5) Number of layers constituting the soft frame member
[0205] The total number of base layers and adhesive layers contained in the soft frame component (hereinafter referred to as the "total number of layers") is not particularly limited as long as it is 3 or more layers, and can be appropriately selected based on the thickness of the base layer, the thickness of the adhesive layer, and the required dimensions of the protective film assembly frame.
[0206] In the case where there is a deviation in the flatness of the substrate layer and the adhesive layer respectively, by laminating these substrate layers and the adhesive layer, the deviation in the flatness of the substrate layer and the adhesive layer respectively can be eliminated. Thus, the flatness of the soft frame member improves. By not making the adhesive layer too thick, the deviation in the flatness of the adhesive layer can be reduced. From these viewpoints, the total number of layers is preferably more than 5 layers, more preferably more than 10 layers.
[0207] The total number of layers is not particularly limited, and may be 40 or less. From the viewpoint of simplifying the production process, the total number of layers is more preferably 30 or less, and even more preferably 20 or less.
[0208] From these viewpoints, the number of layers stacked is preferably 3 to 40, more preferably 5 to 30, and even more preferably 10 to 20.
[0209] From the viewpoint of providing a ventilation passage in the region of the soft member, the number of layers is more preferably 7 or more, and the number of layers is further preferably 9 or more.
[0210] From these viewpoints, the number of layers is preferably 7 to 40, more preferably 7 to 30, and even more preferably 9 to 20.
[0211] The total thickness of the adhesive layer contained in the soft frame member is preferably 0.2 times or more and 4 times or less of the total thickness of the base material layer contained in the soft frame member. Thus, the restoring force generated by attaching to the original plate can be further reduced. That is, the strain of the original plate caused by the deformation of the protective film assembly frame can be further suppressed.
[0212] Hereinafter, the ratio of the total thickness of the adhesive layer included in the soft frame member to the total thickness of the base material layer included in the soft frame member is referred to as “total thickness ratio of the adhesive layer”.
[0213] From the viewpoint of facilitating handling such as transporting the pellicle assembly, the total thickness of the adhesive layer is preferably 4 times or less, more preferably 3 times or less, and even more preferably 2 times or less relative to the total thickness of the base layer contained in the soft frame member.
[0214] From the perspective of reducing the rigidity of the protective film assembly frame to suppress the strain of the original plate, the total thickness ratio of the adhesive layer to the total thickness of the base material layer contained in the soft frame member is preferably 0.2 times or more, more preferably 0.6 times or more, further preferably 0.8 times or more, and particularly preferably 1.0 times or more.
[0215] From these viewpoints, the total thickness ratio of the adhesive layer to the total thickness of the base material layer included in the soft frame member is preferably 0.2 to 3 times, more preferably 0.6 to 3 times, and even more preferably 0.8 to 2 times.
[0216] (1.2.6) Adhesive layer
[0217] The adhesive layer has the following functions (a) to (c).
[0218] (a) an adhesive layer disposed between two adjacent substrate layers in the thickness direction to connect the substrate layers to each other;
[0219] (b) one of the adhesive layers disposed at both ends in the thickness direction connects the soft frame member to the hard frame member;
[0220] (c) The other of the adhesive layers disposed at both ends in the thickness direction connects the pellicle frame to the original plate.
[0221] (1.2.6.1) Thickness of adhesive layer
[0222] The thickness of each adhesive layer (hereinafter referred to as "single layer thickness of the adhesive layer") is preferably not less than 0.01 mm and not more than 0.5 mm. Thus, in the punching process of the manufacturing method of the protective film assembly of the present disclosure described later, the deformation of the adhesive layer can be further reduced, and the rigidity of the adhesive layer can be further reduced to further suppress the strain of the original plate caused by the deformation of the protective film assembly frame.
[0223] From the viewpoint of further reducing deformation of the adhesive layer in the punching step of the pellicle manufacturing method described below, the single-layer thickness of the adhesive layer is preferably 0.5 mm or less, more preferably 0.25 mm or less, and even more preferably 0.2 mm or less.
[0224] From the viewpoint of further reducing the rigidity of the adhesive layer and further suppressing the restoring force generated by sticking to the original plate, the thickness of the adhesive layer is preferably 0.01 mm or more, more preferably 0.03 mm or more, and even more preferably 0.05 mm or more.
[0225] (1.2.6.2) Adhesive layer material
[0226] The Young's modulus of the adhesive layer is preferably 0.01 MPa to 1.0 MPa. This can further reduce the rigidity of the adhesive layer and further suppress the strain of the original plate caused by the deformation of the pellicle frame.
[0227] From the viewpoint of further reducing the rigidity of the adhesive layer and further suppressing the restoring force generated by sticking to the original plate, the Young's modulus of the adhesive layer is more preferably 0.8 MPa or less, and even more preferably 0.6 MPa or less.
[0228] The Young's modulus of the adhesive layer is not particularly limited, but is more preferably 0.02 MPa or more, and further preferably 0.04 MPa or more.
[0229] Examples of the material having a Young's modulus of 1.0 MPa or less include acrylic resin, silicone resin, and styrene butadiene resin.
[0230] Examples of the material having a Young's modulus of 0.8 MPa or less include acrylic resin, silicone resin, and styrene butadiene resin.
[0231] Examples of the material having a Young's modulus of 0.6 MPa or less include acrylic resin, silicone resin, and styrene butadiene resin.
[0232] The Young's modulus of the adhesive layer is measured by a three-point bending test (JIS K7171).
[0233] The material of the adhesive layer is not particularly limited, and examples thereof include acrylic resins, silicone resins, styrene butadiene resins, urethane resins, olefin resins, epoxy resins, polyimide resins, and hydrogenated styrene resins.
[0234] Among them, from the viewpoint of further reducing the rigidity of the soft frame member, the material of the adhesive layer preferably includes an acrylic resin or a silicone resin, and from the viewpoint of further suppressing the amount of outgassing, it is preferably an acrylic resin.
[0235] (1.2.6.3) Surface of adhesive layer
[0236] The surface of the adhesive layer preferably satisfies any one of the following (A) to (C).
[0237] (A) an inorganic layer is formed on at least the inner wall surface of the adhesive layer;
[0238] (B) at least the inner wall surface of the adhesive layer satisfies the following formula (1);
[0239] (C) At least the inner wall surface of the adhesive layer satisfies the following formula (2).
[0240] Formula (1): ([CNO - 2s ] / [CNO - 50s ])≥2.00
[0241] In the above formula (1),
[0242] [CNO - 2s ] indicates that the time-of-flight secondary ion mass spectrometry (TOF-SIMS) method (hereinafter referred to as "TOF-SIMS") is used and the ion source is Bi3 ++ ions and a primary ion gun with an irradiation area of 100 μm×100 μm, and a first deep portion with a depth of a first depth from the surface of the adhesive layer is analyzed to obtain CNO - The standardized intensity.
[0243] The first depth is formed by irradiating a 600 μm square area of the surface with an argon cluster ion beam (Ar-GCIB: Gas Cluster Ion Beam) for a cumulative 2 seconds using a sputtering ion gun with a beam voltage of 20 kV and a beam current of 20 nA.
[0244] Hereinafter, a sputtering ion gun which is an argon cluster ion beam with a beam voltage of 20 kV and a beam current of 20 nA will be simply referred to as a "sputtering ion gun (Ar-GCIB)".
[0245] [CNO - 50s ] indicates: CNO obtained by analyzing the second deep part of the second depth by TOF-SIMS - The standardized intensity of
[0246] The second depth is formed by irradiating the region with the sputtering ion gun for a cumulative total of 50 seconds.
[0247] The normalized intensity is a ratio of the peak intensity of the corresponding component to the total intensity value of the peaks with intensity peak positions in the range of 45 (m / z) to 2000 (m / z) detected by TOF-SIMS.
[0248] Formula (2):
[0249] In formula (2),
[0250] Indicates: C3 obtained by TOF-SIMS analysis of the first deep part - The standardized intensity of
[0251] Indicates: C3 obtained by TOF-SIMS analysis of the second deep part - The standardized intensity.
[0252] In the present disclosure, “the surface of the adhesive layer” includes the inner wall surface of the adhesive layer and the outer wall surface of the adhesive layer.
[0253] TOF-SIMS is a method in which a solid sample is irradiated with an ion gun (primary ions) and ions (secondary ions) released from the surface of the solid sample due to a collision cascade are mass separated using the flight time difference of the ions.
[0254] In TOF-SIMS, a sputtering gun (Ar-GCIB) is irradiated on a solid sample to etch the surface of the solid sample, and by analyzing the obtained surface, secondary ions can be generated and analyzed at the desired part in the depth direction of the solid sample. Therefore, if TOF-SIMS is used, changes in functional groups and the like in the depth direction of the solid sample can be quantitatively evaluated.
[0255] TOF-SIMS has high mass resolution. For example, C3H3O + and C4H7 + Separate and analyze.
[0256] The adhesive layer satisfies any one of (A) to (C), so that the protective membrane assembly of the present disclosure described below is less likely to produce outgassing. The outgassing includes gas derived from water and gas derived from components contained in the adhesive layer. The outgassing includes volatile hydrocarbons (molecular weight: 45 to 100) and non-volatile hydrocarbons (molecular weight: 101 to 200).
[0257] It is speculated that this is mainly based on the following reasons.
[0258] Outgassing occurs, for example, when the adhesive layer is damaged when EUV light is directly irradiated on it. During EUV exposure, EUV light may be scattered on the surface of the original plate.
[0259] Under condition (A), the scattered EUV light directly irradiates the inorganic layer but not the inner wall surface of the adhesive layer. It is speculated that the protective film assembly of the present disclosure can further suppress the generation of outgassing compared with the case where no inorganic layer is formed on the inner wall surface of the adhesive layer.
[0260] In the case of condition (B), satisfying formula (1) indicates that the surface layer of the adhesive layer is surface-modified by a compound derived from a nitrogen functional group. The compound derived from a nitrogen functional group contributes to the fixation (high boiling point) of hydrocarbons, or becomes a gas barrier film that hinders the permeation of gas from the inside of the adhesive layer. Therefore, it is presumed that the generation of outgassing can be suppressed.
[0261] The inventors of the present invention used TOF-SIMS to analyze the surface of the surface-treated adhesive layer in depth. As a result, the inventors of the present invention confirmed through experiments that the standardized intensity of secondary ions changed significantly up to a depth of about 80 nm from the surface of the adhesive layer, and the standardized intensity of secondary ions did not change significantly at a depth deeper than about 80 nm from the surface of the adhesive layer. The depth of about 80 nm from the surface of the adhesive layer is formed, for example, by cumulatively irradiating the surface of the adhesive layer with a sputtering gun (Ar-GCIB) for 10 seconds.
[0262] If the surface of the adhesive layer is irradiated with a sputtering gun (Ar-GCIB) for a cumulative 2 seconds, the surface of the adhesive layer is etched, and the depth of the first deep portion becomes about 16nm from the surface of the adhesive layer. The first deep portion is analyzed by TOF-SIMS, so that the secondary ions (noise) generated by foreign matter attached to the surface of the adhesive layer can be suppressed while the secondary ions generated by the functional groups affected by the surface treatment can be detected. In other words, by analyzing the first deep portion by TOF-SIMS, the functional groups on the surface of the adhesive layer that has been surface treated can be quantitatively and accurately grasped.
[0263] If the surface of the adhesive layer is irradiated with a sputtering gun (Ar-GCIB) for a cumulative total of 50 seconds, the surface of the adhesive layer is etched, and the depth of the second deep portion becomes about 400nm from the surface of the adhesive layer. The second deep portion is analyzed using TOF-SIMS, so that secondary ions generated by functional groups that are almost unaffected by the surface treatment can be detected. In other words, the analysis results of the second deep portion can be regarded as quantitatively representing the functional groups on the surface of the adhesive layer before the surface treatment is implemented.
[0264] ([CNO - 2s ] / [CNO -50s ]) can be regarded as CNO caused by surface treatment - Therefore, satisfying equation (1) indicates that the inner wall surface of the adhesive layer is modified.
[0265] Under condition (C), satisfying formula (2) indicates that the surface layer of the inner wall surface of the adhesive layer is carbonized. The carbonized surface layer of the inner wall surface of the adhesive layer becomes a gas barrier film that blocks the gas from passing through the inside of the adhesive layer. Therefore, it is presumed that the generation of outgassing can be suppressed.
[0266] (1.2.6.3.1) Condition (A)
[0267] The inorganic layer may be formed on the inner wall surface of the adhesive layer, or on both the inner wall surface and the outer wall surface of the adhesive layer.
[0268] The material of the inorganic layer is not limited as long as it can suppress outgassing, and for example, it may be a material with low transmittance of EUV light (metal, ceramic, etc.).
[0269] As the metal that can be used as the inorganic layer, it is preferably any metal selected from the group consisting of aluminum, titanium, vanadium, chromium, manganese, iron, cobalt, nickel, copper, zinc, gallium, germanium, rubidium, strontium, yttrium, zirconium, niobium, molybdenum, ruthenium, rhodium, palladium, silver, hafnium, tantalum, tungsten, platinum and gold. The inorganic layer may be an alloy using two or more elements selected from these, or may be an oxide.
[0270] (1.2.6.3.2) Condition (B)
[0271] The adhesive layer only needs to have an inner wall surface satisfying the formula (1). Alternatively, both the inner wall surface and the outer wall surface of the adhesive layer may satisfy the formula (1).
[0272] CNO of the adhesive layer analyzed by TOF-SIMS - The standardized strength depends on the material of the adhesive layer, whether plasma nitridation treatment is performed, etc.
[0273] Speculation CNO - The main sources are amide bonds or urethane bonds contained in the adhesive layer and nitrogen functional groups introduced into the adhesive layer by plasma nitridation.
[0274] From the viewpoint of suppressing the cost increase of plasma nitridation treatment, ([CNO - 2s ] / [CNO - 50s ]) For example, it can be 500 or less, preferably 300 or less, more preferably 100 or less, and further preferably 10 or less.
[0275] From the viewpoint that the surface of the adhesive layer is modified with a compound derived from a nitrogen functional group to further suppress the generation of outgassing, ([CNO - 2s ] / [CNO - 50s ]) may be, for example, 2.00 or more, preferably 3.00 or more, more preferably 10.0 or more, and further preferably 100 or more.
[0276] From the viewpoint that the surface layer of the adhesive layer is modified with a compound derived from a nitrogen functional group to suppress the generation of outgassing, [CNO - 2s ] The content ratio is preferably 0.001% or more, more preferably 0.010% or more, further preferably 0.100% or more, particularly preferably 1.000% or more.
[0277] From the viewpoint of suppressing the cost increase of plasma nitridation treatment, [CNO - 2s ] The content ratio is preferably 5.000% or less, more preferably 1.000% or less, further preferably 0.100% or less, particularly preferably 0.010% or less.
[0278] From the viewpoint of suppressing outgassing by modifying the surface of the adhesive layer with a compound derived from a nitrogen functional group, [CNO - 2s ] is preferably greater than 0.01, more preferably greater than 0.03, further preferably greater than 0.10, and particularly preferably greater than 1.00.
[0279] From the viewpoint of suppressing the cost increase of plasma nitridation treatment, [CNO - 2s ] is preferably less than 3.00, more preferably less than 1.00, further preferably less than 0.30, and particularly preferably less than 0.03.
[0280] As a method for making the inner wall surface of the adhesive layer etc. satisfy the formula (1), for example, there is a method of subjecting the inner wall surface of the adhesive layer etc. to plasma nitriding treatment.
[0281] In particular, when the adhesive layer does not contain nitrogen atoms, if the inner wall surface of the adhesive layer is subjected to plasma nitridation treatment, ([CNO - 2s ] / [CNO - 50s ]) will increase dramatically. For example, ([CNO - 2s ] / [CNO- 50s ]) becomes 10 or more. It is presumed that the reason is that nitrogen atoms are introduced into the first deep part by plasma nitridation, while nitrogen atoms are not easily introduced into the second deep part, as ([CNO - 2s ] / [CNO - 50s ]) of the denominator [CNO - 50s ]Keep it low.
[0282] (1.2.6.3.3) Condition (C)
[0283] As for the adhesive layer, it is sufficient that the inner wall surface of the adhesive layer satisfies the formula (2), and both the inner wall surface and the outer wall surface of the adhesive layer may satisfy the formula (2).
[0284] C3 of the adhesive layer analyzed by TOF-SIMS - The standardized intensity depends on the material of the adhesive layer, whether EUV irradiation treatment is implemented, etc.
[0285] Speculation C3 - The main cause is carbonization of the inner wall surface of the adhesive layer caused by the surface treatment. The surface treatment includes plasma nitridation treatment or extreme ultraviolet irradiation treatment (hereinafter referred to as "EUV irradiation treatment").
[0286] When the inner wall surface of the adhesive layer satisfies the formula (2), the surface layer of the adhesive layer is carbonized, the generation of outgassing is suppressed, and the gas permeation from the inside of the adhesive layer can be suppressed.
[0287] From the perspective of suppressing the increase in cost of EUV irradiation treatment, For example, it may be 10.0 or less, preferably 5.0 or less, more preferably 3.0 or less, and further preferably 2.0 or less.
[0288] From the viewpoint of suppressing outgassing by carbonizing and modifying the surface of the adhesive layer, For example, it may be 1.10 or more, preferably 1.20 or more, more preferably 1.40 or more, and further preferably 2.00 or more.
[0289] As a method for making the inner wall surface of the adhesive layer etc. satisfy the formula (2), for example, there is a method of subjecting the inner wall surface of the adhesive layer etc. to EUV irradiation treatment.
[0290] When the inner wall surface of the adhesive layer is subjected to EUV irradiation treatment, the surface of the inner wall surface absorbs EUV and becomes high temperature. As a result, the surface of the inner wall surface subjected to EUV irradiation treatment is easily carbonized.
[0291] (1.2.7) Base material layer
[0292] Even if the base material layer is not thickly coated with adhesive to form a thick adhesive layer, a soft frame member can be formed. The soft frame member includes at least one base material layer, so the thickness of the adhesive layer contained in the soft frame member is thinner than the thick adhesive layer formed by thickly coating the adhesive. Therefore, the adhesive layer contained in the soft frame member can be formed by drying in a shorter time. Furthermore, since the large deformation of the protective film assembly frame can be suppressed, it can be easily transported as a protective film assembly. The upper limit of the thickness of each commercially available optical adhesive sheet (OCA: Optical Clear Adhesive) is about 250μm. Therefore, the base material layer can make the thickness of the adhesive layer contained in the soft frame member a thickness that meets market demand.
[0293] (1.2.7.1) Thickness of the substrate layer
[0294] The thickness of each substrate layer (hereinafter referred to as "single-layer thickness of the substrate layer") is preferably 2.5 mm or less. This facilitates the punching step of the method for manufacturing the pellicle assembly described later and facilitates the lamination step of the method for manufacturing the pellicle assembly described later.
[0295] From the viewpoint of facilitating the punching step in the pellicle manufacturing method described below, the single-layer thickness of the substrate layer is preferably 2.5 mm or less, more preferably 2.0 mm or less, further preferably 1.0 mm or less, and particularly preferably 0.5 mm or less.
[0296] From the viewpoint of facilitating the lamination step in the pellicle manufacturing method described below, the single-layer thickness of the substrate layer is preferably 0.01 mm or more, more preferably 0.05 mm or more, and even more preferably 0.10 mm or more.
[0297] (1.2.7.2) Material of the base material
[0298] The Young's modulus of the substrate layer is preferably 2 GPa to 200 GPa. This facilitates the punching step of the pellicle manufacturing method and suppresses large deformation of the pellicle frame, thereby facilitating handling such as transporting the pellicle.
[0299] From the viewpoint of suppressing strain of the original plate due to deformation of the pellicle frame, the Young's modulus of the base layer is preferably 200 GPa or less, more preferably 110 GPa or less, further preferably 50 GPa or less, and particularly preferably 10 GPa or less.
[0300] From the viewpoint of facilitating the punching process of the manufacturing method of the protective membrane assembly and suppressing large deformation of the protective membrane assembly frame so as to facilitate operations such as transporting the protective membrane assembly, the Young's modulus of the substrate layer is preferably greater than 0.1 GPa, more preferably greater than 0.5 GPa, and even more preferably greater than 1 GPa.
[0301] From these viewpoints, the Young's modulus of the substrate layer is preferably 0.1 GPa to 110 GPa, more preferably 0.5 GPa to 50 GPa, and particularly preferably 1 GPa to 10 GPa.
[0302] Examples of materials having a Young's modulus of 110 GPa or less include glass, stainless steel, aluminum, titanium, titanium alloy, silicon, polyethylene terephthalate resin, polyethylene resin, polypropylene resin, polyimide resin, polyethylene naphthalate resin, polycarbonate resin, polyphenylene sulfide resin, fluororesin, polyetheretherketone resin, and polyethersulfone resin.
[0303] Examples of materials having a Young's modulus of 50 GPa or less include polyethylene terephthalate resin, polyethylene resin, polypropylene resin, polyimide resin, polyethylene naphthalate resin, polycarbonate resin, polyphenylene sulfide resin, fluororesin, polyetheretherketone resin, and polyethersulfone resin.
[0304] Examples of materials having a Young's modulus of 10 GPa or less include polyethylene terephthalate resin, polyethylene resin, polypropylene resin, polyimide resin, polyethylene naphthalate resin, polycarbonate resin, polyphenylene sulfide resin, fluororesin, polyetheretherketone resin, polyethersulfone resin, and aramid resin.
[0305] The Young's modulus of the substrate layer is determined by a tensile test (JIS G0567J). When the substrate layer is made of resin, the value is determined by a three-point bending test (JIS K7171). Whether the substrate layer is made of resin is determined by whether the material of the hard frame member undergoes thermal decomposition at 550°C. When evaluating a stacked frame, analysis can be performed after peeling off the stacked state.
[0306] The Young's modulus of the substrate layer is preferably 10,000 to 9,000,000 times that of the adhesive layer. This can further reduce the restoring force caused by attachment to the original plate. That is, the strain of the original plate caused by the deformation of the pellicle assembly frame can be further suppressed.
[0307] Hereinafter, the ratio of the Young's modulus of the base material layer to the Young's modulus of the adhesive layer is referred to as "Young's modulus ratio of the base material layer".
[0308] From the viewpoint of further reducing the restoring force generated by adhering to the original plate, the Young's modulus ratio of the substrate layer is more preferably 3 million times or less (for example, when the material of the substrate layer is titanium), further preferably 1 million times or less, and particularly preferably 200,000 times or less (for example, when the material of the substrate layer is polyethylene terephthalate resin).
[0309] From the viewpoint of facilitating the lamination step in the pellicle manufacturing method described below, the Young's modulus ratio of the substrate layer is more preferably 50,000 times or more, and even more preferably 300,000 times or more.
[0310] From the viewpoint of further reducing the restoring force caused by sticking to the original plate and facilitating the lamination step in the pellicle manufacturing method, the ratio is preferably 50,000 to 3,000,000 times, and more preferably 50,000 to 200,000 times.
[0311] When there are plural base layers having different Young's moduli among the plurality of base layers included in the soft frame member, the Young's modulus of the base layer having the smallest Young's modulus among the plurality of base layers having different Young's moduli is defined as “Young's modulus of the base layer”.
[0312] When there are plural adhesive layers having different Young's moduli among the adhesive layers included in the soft frame member, the Young's modulus of the adhesive layer having the largest Young's modulus among the adhesive layers having different Young's moduli is defined as “Young's modulus of the adhesive layer”.
[0313] The material of the base material layer is not particularly limited, and examples thereof include metals, ceramics, and resins.
[0314] Examples of the metal that can be used for the base material layer include aluminum, titanium, and stainless steel.
[0315] Examples of ceramics that can be used for the base layer include silicon and glass.
[0316] Examples of the resin that can be used for the substrate layer include polyethylene resin, polypropylene resin, polyethylene terephthalate resin, polyimide resin, polyethylene naphthalate resin, polystyrene resin, acrylic resin, polycarbonate resin, polyimide resin, polyphenylene sulfide resin, fluororesin, polyetheretherketone resin, polyethersulfone resin, and aramid resin.
[0317] From the viewpoint of forming the soft frame member in a good shape, the material of the base material layer is preferably a material that can be slit coated or spin coated, and examples of such materials are preferably acrylic resins, silicone resins, and styrene butadiene resins.
[0318] From the viewpoint of making the shape of the soft frame member easy to process, the material of the substrate layer is preferably resin. If the material of the substrate layer is resin, the cutout and opening can be formed by punching. Among them, the material of the substrate layer preferably includes polyethylene terephthalate resin, polyethylene naphthalate resin or polyimide resin.
[0319] (2) Protective film assembly
[0320] The pellicle assembly of the present disclosure includes the pellicle assembly frame of the present disclosure and a pellicle supported by a hard frame member.
[0321] The protective film assembly of the present disclosure is suitable for EUV exposure.
[0322] (2.1) Protective film
[0323] The pellicle prevents foreign matter from adhering to the surface of the original plate and allows exposure light to pass through during exposure. Foreign matter includes dust. Examples of exposure light include deep ultraviolet (DUV: Deep UltraViolet) light and EUV.
[0324] The pellicle covers the entire opening of the exposure through hole of the pellicle assembly frame on the hard frame member side. The pellicle can be supported directly by the pellicle assembly frame member or through an adhesive layer. The adhesive layer can be a cured product of a known adhesive.
[0325] The thickness of the pellicle membrane is preferably from 2 nm to 200 nm.
[0326] The material of the pellicle membrane is not particularly limited, and examples thereof include carbon-based materials, SiN, polycrystalline silicon, or a stacked structure in which a plurality of layers thereof are stacked.
[0327] Carbon-based materials include graphene and carbon nanotubes (hereinafter referred to as "CNTs"). Among them, the material of the pellicle membrane preferably includes CNTs. The CNTs may be single-walled CNTs or multi-walled CNTs.
[0328] When the carbon content of the pellicle membrane is 40 mass % or more, the pellicle membrane can be connected to the rigid frame member by van der Waals force without interposing the adhesive layer.
[0329] The protective film may be a non-woven fabric structure, which is formed, for example, from fiber-shaped CNTs.
[0330] (2.2) Protective film
[0331] The pellicle assembly of the present disclosure may include a protective film (gasket) as necessary.
[0332] The protective film protects at least the surface of the adhesive layer that is in contact with the original plate. The protective film can be peeled off from the adhesive layer.
[0333] The thickness of the protective film is preferably 5 μm to 500 μm, more preferably 30 μm to 200 μm. Examples of the material of the protective film include polyester and the like.
[0334] A release agent may be applied to the surface of the protective film that contacts the adhesive layer. Examples of the release agent include silicone-based release agents and fluorine-based release agents.
[0335] (2.3) Exposure of the original version
[0336] The protective film assembly disclosed in the present invention can be equipped with an exposure original plate.
[0337] The exposure original plate includes an original plate and a protective film assembly. The original plate is an original plate with a circuit pattern. The original plate has a pattern. The protective film assembly is attached to the surface of the original plate having the pattern.
[0338] For example, the original plate may not be stacked in the order of the supporting substrate, the reflective layer, and the absorber layer. The absorber layer absorbs a portion of the light (e.g., EUV), thereby forming a desired image on the sensing substrate (e.g., a semiconductor substrate with a photoresist film). As the reflective layer, a multilayer film of molybdenum (Mo) and silicon (Si) can be cited. The material of the absorber layer can be a material with high absorption such as EUV. As materials with high absorption such as EUV, chromium (Cr), tantalum nitride, etc. can be cited.
[0339] (2.4) Exposure device
[0340] The protective film assembly of the present disclosure can be equipped in an exposure device.
[0341] The exposure device includes a light source, the exposure original plate, and an optical system. The light source emits exposure light. The optical system guides the exposure light emitted by the light source to the exposure original plate. The exposure original plate is configured so that the exposure light emitted from the light source passes through the protective film and irradiates the original plate.
[0342] The exposure device can form a fine pattern (for example, a line width of 32 nm or less) using EUV or the like, and can perform pattern exposure with reduced poor resolution caused by foreign matter even when using EUV, in which poor resolution caused by foreign matter is likely to become a problem.
[0343] The exposure light is preferably EUV. EUV has a short wavelength and is easily absorbed by gases such as oxygen and nitrogen. Therefore, exposure using EUV light is performed in a vacuum environment.
[0344] (2.5) Example of a pellicle assembly
[0345] Next, refer to Figures 4 to 6 An example of the pellicle module of the present disclosure will be described. Figure 4This is a cross-sectional view of a pellicle assembly according to a second embodiment of the present disclosure.
[0346] (2.5.1) Second Implementation Method
[0347] like Figure 4 As shown, the pellicle 1 according to the second embodiment of the present disclosure is attached to the surface of the original plate for use.
[0348] The pellicle 1 according to the second embodiment of the present disclosure includes a pellicle frame 10A, a pellicle 20, and an adhesive layer 21. The pellicle 20 is supported by the pellicle frame 10A via a known adhesive layer 21.
[0349] Hereinafter, surface direction D1 of pellicle membrane 20 is referred to as “surface direction D1 ”, and direction D2 perpendicular to the surface direction of pellicle membrane 20 is referred to as “thickness direction D2 ”.
[0350] The pellicle frame 10A is a rectangular cylindrical object. The pellicle frame 10A has an exposure through hole THA. The exposure through hole THA linearly penetrates the pellicle frame 10A along the thickness direction D2 at the center of the surface direction D1 of the pellicle frame 10A.
[0351] The pellicle frame 10A is an assembled product, and includes a soft frame member 11A and a hard frame member 12A. The soft frame member 11A and the hard frame member 12A are stacked in the thickness direction D2 of the pellicle frame 10A.
[0352] The Young's modulus of the rigid frame member 12A is higher than the apparent Young's modulus of the soft frame member 11A. The Young's modulus of the rigid frame member 12A is 25 GPa or more.
[0353] The soft frame member 11A is a rectangular cylindrical object similar to the pellicle frame 10A. The soft frame member 11A has a through hole TH11. The through hole TH11 constitutes a part of the exposure through hole THA of the pellicle frame 10A.
[0354] In the second embodiment, the soft frame member 11A is formed by alternately stacking six adhesive layers 111 and five base layers 112 in the thickness direction D2 such that the adhesive layers 111 are arranged at both ends.
[0355] In the second embodiment, the soft frame member 11A includes four ventilation channels THB and four ventilation filters 113. One ventilation channel THB is formed on each of the four side surfaces of the pellicle assembly frame 10A. The ventilation channel THB penetrates from the inner wall surface S10A of the pellicle assembly frame 10A to the outer wall surface S10B in a non-linear shape in the surface direction D1. One ventilation filter 113 is arranged in one ventilation channel THB.
[0356] The ventilation filter 113 is fixed in the soft frame member 11A and covers the ventilation passage THB. Specifically, in the second embodiment, the ventilation filter 113 is fixed by contacting the ventilation filter 113 on the same surface of one adhesive layer 111 exposed in the ventilation passage THB. The ventilation filter 113 is, for example, a HEPA ventilation filter.
[0357] The rigid frame member 12A is a rectangular cylindrical member similar to the pellicle frame 10A. The rigid frame member 12A has a through hole TH12. The through hole TH12 constitutes a part of the exposure through hole THA of the pellicle frame 10A.
[0358] In the second embodiment, the thickness of the pellicle 1 is, for example, 2.375 mm. The length L10 of one side of the pellicle frame 10A is, for example, 150 mm. The width W10 of one side of the pellicle frame 10A is, for example, 4.0 mm.
[0359] The thickness of the soft frame member 11A is, for example, 1.650 mm. The single layer thickness of the adhesive layer 111 is, for example, 0.236 mm. The material of the adhesive layer 111 is, for example, acrylic resin (Young's modulus: 0.045 MPa). The single layer thickness of the base layer 112 is, for example, 0.236 mm. The material of the base layer 112 is, for example, polyethylene terephthalate resin (Young's modulus: 4 GPa).
[0360] The thickness of the rigid frame member 12A is, for example, 0.725 mm.
[0361] The pellicle 1 is suitable for EUV exposure. Since EUV light is also easily absorbed by gases such as oxygen and nitrogen, EUV exposure is performed in a vacuum atmosphere.
[0362] (2.5.2) Third Implementation Method
[0363] Reference Figure 5 A pellicle assembly frame according to a third embodiment of the present disclosure will be described. Figure 5 is a cross-sectional view of a pellicle assembly frame according to a third embodiment of the present disclosure.
[0364] A pellicle assembly frame 10B of the third embodiment of the present disclosure is the same as the pellicle assembly frame 10A of the second embodiment except that a method of fixing the vent filter 113 is different.
[0365] The pellicle assembly frame 10B is an assembled product, and includes a soft frame member 11B and a hard frame member 12A. The soft frame member 11B and the hard frame member 12A are stacked in the thickness direction D2. The Young's modulus of the hard frame member 12A is higher than the apparent Young's modulus of the soft frame member 11B. The Young's modulus of the hard frame member 12A is 25 GPa or more.
[0366] The soft frame member 11B is a rectangular cylindrical object similar to the pellicle frame 10A. In the third embodiment, the soft frame member 11B is formed by alternately stacking six adhesive layers 111 and five base layers 112 in the thickness direction D2 with the adhesive layers 111 disposed at both ends.
[0367] In the third embodiment, the soft frame member 11B includes four ventilation passages THB and four ventilation filters 113 . One ventilation filter 113 is disposed in one ventilation passage THB.
[0368] The ventilation filter 113 is fixed in the soft frame member 11B and covers the ventilation channel THB. In detail, in the third embodiment, one of the plurality of adhesive layers 111 has an adhesive portion 111a and an adhesive portion 111b that are formed by dividing one adhesive layer 111 into two in the thickness direction D2. The divided adjacent adhesive portions 111a and 111b of the ventilation filter 113 are clamped to each other, thereby fixing the ventilation filter 113. The ventilation filter 113 is, for example, a HEPA ventilation filter.
[0369] (2.5.3) Fourth Implementation Method
[0370] Reference Figure 6 A pellicle assembly frame according to a fourth embodiment of the present disclosure will be described. Figure 6 4 is a cross-sectional view of a pellicle assembly frame according to a fourth embodiment of the present disclosure.
[0371] A pellicle assembly frame 10C according to the fourth embodiment of the present disclosure is the same as the pellicle assembly frame 10A according to the second embodiment except that a method of fixing the vent filter 113 is different.
[0372] The pellicle assembly frame 10C is an assembled product, and includes a soft frame member 11C and a hard frame member 12A. The soft frame member 11C and the hard frame member 12A are stacked in the thickness direction D2. The Young's modulus of the hard frame member 12A is higher than the apparent Young's modulus of the soft frame member 11C. The Young's modulus of the hard frame member 12A is 25 GPa or more.
[0373] The soft frame member 11C is a rectangular cylindrical object similar to the pellicle frame 10A. In the fourth embodiment, the soft frame member 11C is formed by alternately stacking six adhesive layers 111 and five base layers 112 in the thickness direction D2 with the adhesive layers 111 disposed at both ends.
[0374] In the fourth embodiment, the soft frame member 11C includes four ventilation passages THB and four ventilation filters 113 . One ventilation filter 113 is disposed in one ventilation passage THB.
[0375] The ventilation filter 113 is fixed in the soft frame member 11C and covers the ventilation passage THB. Specifically, in the fourth embodiment, the ventilation filter 113 is welded to the same surface of one substrate layer 112 exposed in the ventilation passage THB, thereby fixing the ventilation filter 113. The ventilation filter 113 is, for example, a HEPA ventilation filter.
[0376] (2.5.4) Fifth Implementation
[0377] Reference Figure 7 A pellicle assembly frame according to a fifth embodiment of the present disclosure will be described. Figure 7 is a cross-sectional view of a pellicle assembly frame according to a fifth embodiment of the present disclosure.
[0378] A pellicle assembly frame 10D according to the fifth embodiment of the present disclosure is the same as the pellicle assembly frame 10A according to the second embodiment except that the configuration of the hard frame member and the soft frame member and the method of fixing the vent filter 113 are mainly different.
[0379] The pellicle assembly frame 10D is an assembled product, and includes a soft frame member 11D and a hard frame member 12D. The soft frame member 11D and the hard frame member 12D are stacked in the thickness direction D2. The Young's modulus of the hard frame member 12D is higher than the apparent Young's modulus of the soft frame member 11D. The Young's modulus of the hard frame member 12D is 25 GPa or more.
[0380] The soft frame member 11D and the hard frame member 12D are rectangular cylindrical objects like the protective membrane assembly frame 10A. In the fifth embodiment, the soft frame member 11D is formed by alternately stacking four adhesive layers 111 and three base material layers 112 in the thickness direction D2 with the adhesive layers 111 arranged at both ends. The hard frame member 12D is formed by stacking three hard layers 121 in the thickness direction D2.
[0381] In the fifth embodiment, the soft frame member 11D includes four ventilation passages THB and four ventilation filters 113 . One ventilation filter 113 is disposed in one ventilation passage THB.
[0382] The ventilation filter 113 is fixed in the soft frame member 11D and covers the ventilation passage THB. Specifically, in the fifth embodiment, the ventilation filter 113 is fixed by contacting the same surface of one adhesive layer 111 exposed in the ventilation passage THB. The ventilation filter 113 is, for example, a HEPA ventilation filter.
[0383] (3) Method for manufacturing protective membrane assembly
[0384] The manufacturing method of the protective film assembly disclosed in the present invention is the manufacturing method of the protective film assembly disclosed in the present invention, comprising: a process of preparing the aforementioned hard frame component; a stacking process of alternately stacking at least one substrate layer sheet and a plurality of adhesive layers in the aforementioned thickness direction to form a stacked body; a punching process of punching the aforementioned stacked body in a manner of forming exposure through holes along the aforementioned thickness direction to form the aforementioned soft frame component; and a connecting process of connecting the aforementioned hard frame component with the aforementioned soft frame component.
[0385] By alternately stacking a substrate layer sheet and a plurality of adhesive layers in the thickness direction to form a stacked body, the stacked body is punched out in a manner to form exposure through holes along the thickness direction, thereby making it possible to manufacture a protective film assembly frame with suppressed opening deviation even for multiple stacked bodies.
[0386] In the present disclosure, the “adhesive layer layer” includes an adhesive layer sheet and an adhesive layer coating layer obtained by coating an adhesive for an adhesive layer.
[0387] The pellicle manufacturing method of the present disclosure has the above-described configuration, and thus can obtain a pellicle that can suppress strain caused by tension of the pellicle and can suppress strain of the original plate caused by deformation of the pellicle frame.
[0388] The stacking step and the punching step are performed sequentially. The preparation step may be performed before the stacking step, after the stacking step and before the punching step, or after the punching step. The connection step is performed after the punching step and the preparation step.
[0389] The method for manufacturing the pellicle assembly of the present disclosure preferably further includes at least one of the surface treatment step described below and the ventilation channel processing step described below. In the case where the method for manufacturing the pellicle assembly of the present disclosure includes the ventilation channel processing step, the method for manufacturing the pellicle assembly of the present disclosure preferably further includes the filter fixing step described below.
[0390] The surface treatment process is performed after the punching process. The ventilation channel processing process is performed before the lamination process. The filter fixing process is performed after the ventilation channel processing process and before the lamination process.
[0391] Hereinafter, a pellicle manufacturing method according to an embodiment of the present disclosure will be described.
[0392] The manufacturing method of the protective membrane assembly of this embodiment includes a surface treatment process, a ventilation channel processing process and a filter fixing process in addition to a lamination process, a punching process, a preparation process and a connection process. The ventilation channel processing process, the filter fixing process, the lamination process, the punching process, the surface treatment process, the preparation process and the connection process are performed in sequence. The adhesive layer is a sheet for the adhesive layer.
[0393] (3.1) Ventilation channel processing steps
[0394] The method for manufacturing the pellicle assembly of the present embodiment includes a ventilation channel processing step, thereby obtaining a pellicle assembly in which the soft frame member includes the ventilation channel.
[0395] In the ventilation channel processing step, at least one base material unprocessed sheet and the plurality of adhesive layer unprocessed sheets are processed so as to form ventilation channels, thereby forming at least one base material layer sheet and a plurality of adhesive layer sheets. The ventilation channel processing step is performed before the lamination step.
[0396] In the present disclosure, the “unprocessed sheet for base material layer” is a material for the base material layer, and means a sheet in a full sheet form.
[0397] In the present disclosure, the "unprocessed sheet for adhesive layer" is the material of the adhesive layer, and means a sheet in a full sheet form.
[0398] In the present disclosure, the "substrate layer sheet" refers to the material of the substrate layer. The substrate layer sheet may be a sheet processed so as to form ventilation passages, or may be a sheet in a continuous form.
[0399] In the present disclosure, the term "adhesive layer sheet" refers to the material of the adhesive layer. The adhesive layer sheet may be a sheet processed so as to form ventilation passages, or may be a sheet in a continuous form.
[0400] The material of the unprocessed sheet for the base layer is the same as that of the base layer. The material of the unprocessed sheet for the adhesive layer is the same as that of the adhesive layer.
[0401] The ventilation duct is constructed by forming openings in at least one base material layer unprocessed sheet and a plurality of adhesive layer unprocessed sheets and stacking them.
[0402] The number of processed sheets of the unprocessed sheet material for the substrate layer and the unprocessed sheet material for the adhesive layer is appropriately selected according to the shape of the ventilation duct formed in the soft frame member, etc. For example, each substrate layer unprocessed sheet material and the unprocessed sheet material for the adhesive layer can be processed separately, or the unprocessed sheet material for the adhesive layer can be processed in a state where the unprocessed sheet material for the substrate layer is stacked on at least one main surface of the unprocessed sheet material for the substrate layer.
[0403] The processing method of the unprocessed sheet for the base layer and the unprocessed sheet for the adhesive layer is not particularly limited as long as it is a known method, for example, a method using a punching die, a method using laser irradiation, a method using a slitter, a method using a water jet, etc.
[0404] (3.2) Filter fixing process
[0405] The method for manufacturing the pellicle assembly of the present embodiment includes a filter fixing step, thereby obtaining a pellicle assembly in which the soft frame member includes the ventilation duct and the ventilation filter.
[0406] In the filter fixing step, the vent filter is fixed to a part of at least one substrate layer sheet or a plurality of adhesive layer sheets so that the vent filter is arranged in the vent channel. The filter fixing step is performed after the vent channel processing step and before the lamination step.
[0407] There is no particular limitation on the method for fixing the ventilation filter. For example, there can be cited: a method of welding and bonding the ventilation filter to the substrate layer sheet in a manner that the opening formed in the substrate layer sheet is covered by the ventilation filter; a method of bonding the ventilation filter to the adhesive layer in a manner that the opening formed in the adhesive layer sheet is covered by the ventilation filter; a method of maintaining the ventilation filter in a state where the ventilation filter is clamped by adjacent substrate layer sheets, etc.
[0408] (3.3) Lamination process
[0409] The method for producing a pellicle according to the present embodiment includes a lamination step, thereby obtaining a laminated body.
[0410] In the lamination step, at least one substrate layer sheet and a plurality of adhesive layer sheets are alternately laminated in the thickness direction to form a laminate.
[0411] The number of stacked base layer sheets is the same as the number of base layers included in the soft frame member. The number of stacked adhesive layer sheets is the same as the number of adhesive layers included in the soft frame member.
[0412] The stacking method of alternately stacking the substrate layer sheet and the adhesive layer sheet in the thickness direction is not particularly limited, as long as it is a known method. As a stacking method when forming a 5-layer laminate, for example, it can be cited: arranging the adhesive layer sheet on the two main surfaces of the substrate layer sheet and sandwiching it between a pair of rollers to form a 3-layer laminate, and arranging the adhesive layer sheet on one main surface of the substrate layer sheet and sandwiching it between a pair of rollers to form a 2-layer laminate, so that the 3-layer laminate and the 2-layer laminate are stacked and sandwiched between a pair of rollers to form a method; arranging the substrate layer sheet on the two main surfaces of the adhesive layer sheet and sandwiching it between a pair of rollers to form a 3-layer laminate, arranging the adhesive layer sheet on the two main surfaces of the obtained 3-layer laminate and sandwiching it between a pair of rollers to form a 5-layer laminate, etc. When the stacking is more than 5 layers, it can be formed as follows: a two-layer stack formed by arranging a base layer sheet on one main surface of an adhesive layer sheet and sandwiching the sheet between a pair of rollers is stacked to a target number of layers to obtain a stacked body, and a base layer sheet is arranged on both main surfaces of an adhesive layer sheet and sandwiched between a pair of rollers to form a three-layer stacked body, and the aforementioned stack and the three-layer stack are stacked and sandwiched between a pair of rollers.
[0413] (3.4) Punching process
[0414] The method for manufacturing the pellicle assembly of the present embodiment includes a punching step, thereby obtaining a soft frame member.
[0415] In the punching step, the laminate is punched out so as to form exposure through holes along the thickness direction, thereby forming a soft frame member.
[0416] The method for punching the laminate is not particularly limited and may be any known method, and examples thereof include a method using a punching die, a method using laser irradiation, a method using a slitter, and a method using a water jet.
[0417] (3.5) Surface treatment process
[0418] The method for producing a pellicle according to the present embodiment includes a surface treatment step, thereby obtaining a pellicle in which the surface of the adhesive layer satisfies any one of the above (A) to (C).
[0419] The surface treatment process includes at least one of the following processes: a process of coating an inorganic layer on at least the inner wall surface of the adhesive layer (hereinafter referred to as the "coating process"); a process of performing plasma nitridation treatment on at least the inner wall surface of the adhesive layer (hereinafter referred to as the "plasma nitridation treatment process"); and a process of performing extreme ultraviolet irradiation treatment on at least the inner wall surface of the adhesive layer (hereinafter referred to as the "EUV irradiation treatment process").
[0420] (3.5.1) Coating process
[0421] In the coating step, the inorganic layer may be coated on the inner wall surface of the adhesive layer, or on both the inner wall surface and the outer wall surface of the adhesive layer. In this case, the inorganic layer may be coated on the entire inner wall surface of the pellicle assembly frame, or on both the inner wall surface and the outer wall surface of the pellicle assembly frame.
[0422] The method for coating the inorganic layer on at least the inner wall surface of the adhesive layer is not particularly limited, and examples thereof include vapor deposition and sputtering.
[0423] (3.5.2) Plasma nitridation process
[0424] In the plasma nitriding process, the plasma nitriding process may be performed on the inner wall surface of the adhesive layer, or on both the inner wall surface and the outer wall surface of the adhesive layer. In this case, the plasma nitriding process may be performed on the entire inner wall surface of the pellicle assembly frame, or on both the inner wall surface and the outer wall surface of the pellicle assembly frame.
[0425] The plasma nitriding treatment is performed, for example, using a plasma processing apparatus (a research and development sputtering apparatus “CFS-4EP-LL” manufactured by Shibaura Electric Co., Ltd., type: load lock type) under the following treatment conditions.
[0426] <Treatment conditions of plasma nitridation treatment>
[0427] ·Chamber vacuum limit: pressure <1e -3 Pa
[0428] Material gas: N2 (G1 grade)
[0429] Gas flow rate: 21sccm
[0430] ·Processing pressure: 0.5Pa
[0431] RF power: 100W
[0432] Processing time: 1 second to 90 seconds
[0433] (3.5.3) EUV irradiation process
[0434] In the EUV irradiation treatment step, the EUV irradiation treatment may be performed on the inner wall surface of the adhesive layer, or on both the inner wall surface and the outer wall surface of the adhesive layer. In this case, the EUV irradiation treatment may be performed on the entire inner wall surface of the pellicle assembly frame, or on both the inner wall surface and the outer wall surface of the pellicle assembly frame.
[0435] EUV irradiation treatment is performed, for example, using an EUV irradiation device (facility name: NewSUBARU Radiation Light Facility, beamline: "BL-9C_H-ch", operated by: Hyogo Prefectural University Advanced Industrial Science and Technology Research Institute) and a quadrupole mass spectrometer: "M-200" manufactured by Canon Anelva Co., Ltd. under the following treatment conditions.
[0436] <Treatment conditions of EUV irradiation treatment>
[0437] ·Irradiation light: EUV (wavelength: 13.5nm)
[0438] Irradiation intensity: 0.3W / cm 2
[0439] Beam size: 2×0.5mm
[0440] Irradiation time: 10 minutes
[0441] (3.6) Preparation process
[0442] The method for manufacturing the pellicle assembly of the present embodiment includes a preparation step. Thus, a rigid frame member is obtained.
[0443] In the preparation step, a rigid frame member is prepared.
[0444] The rigid frame member prepared in the preparation step may or may not be provided with a protective film.
[0445] As a method for preparing a hard frame member without a protective film, for example, there can be cited: a method of obtaining a hard frame member through transfer of a commercial product; a method of obtaining a hard frame member by a cutting method, etc. In the cutting method, a raw material plate as a material of the hard frame member is cut into the hard frame member by a known method.
[0446] As a method of preparing a hard frame member on which a pellicle film is laid, for example, there is a method of obtaining it through the transfer of a commercially available product.
[0447] (3.7) Laying process
[0448] In the case where a rigid frame member without a pellicle membrane is prepared in the preparation step, the method for manufacturing a pellicle membrane assembly of the present embodiment may include a laying step, whereby the pellicle membrane is laid on the rigid frame member. In other words, the pellicle membrane is supported by the rigid frame member.
[0449] The laying step may be performed after the preparation step is performed, and may be performed before the connection step is performed or after the connection step is performed.
[0450] In the laying process, the protective film is laid on the rigid frame member.
[0451] The method of applying the pellicle to the rigid frame member is not particularly limited, and examples thereof include a method using an adhesive and a method not using an adhesive.
[0452] In the method using an adhesive, a known adhesive is applied to a rigid frame member to obtain a coating film, and the pellicle membrane is brought into contact with the obtained coating film and heated, thereby making the coating film adhere closely to the pellicle membrane and the rigid frame member, and integrating the pellicle assembly frame and the rigid frame member.
[0453] The method of applying the adhesive is not particularly limited, and examples thereof include a method using a dispenser.
[0454] In the method without using an adhesive, the protective film is brought into contact with the hard frame member and pressurized against each other. Thus, the protective film and the hard frame member are closely fitted and integrated. In order to facilitate chemical bonding between the hard frame member and the protective film, the pressurization can be performed with a coating provided between the hard frame member and the protective film.
[0455] (3.8) Connection process
[0456] The method for manufacturing the pellicle assembly of the present embodiment includes a connecting step, thereby obtaining a pellicle assembly frame in which the hard frame member and the soft frame member are integrated.
[0457] In the connecting step, the hard frame member and the soft frame member are connected.
[0458] The method of connecting the hard frame member and the soft frame member is not particularly limited, and the connection adhesive layer is heated while the hard frame member is in contact with an adhesive layer (hereinafter referred to as "connection adhesive layer") disposed at one end of the soft frame member in the thickness direction. Thus, the connection adhesive layer and the hard frame member are closely attached, and the hard frame member and the soft frame member are integrated.
[0459] Example
[0460] Hereinafter, the present disclosure will be described in further detail using examples, but the present invention is not limited to these examples.
[0461] [1] Example 1
[0462] [1.1] Lamination process
[0463] As the adhesive for the adhesive layer, a styrene-butadiene adhesive was prepared.
[0464] As a sheet for a substrate layer, a polyethylene terephthalate resin sheet (thickness: 0.55 mm) was prepared.
[0465] The adhesive for the adhesive layer is applied to the two main surfaces of the substrate layer sheet by a roll coater, and the coating layer for the adhesive layer is formed on the two main surfaces of the substrate layer sheet. Thus, one substrate layer sheet and two adhesive layer layers are alternately stacked in the thickness direction to form a three-layer laminate of adhesive layer layer / substrate sheet / adhesive layer layer.
[0466] The single layer thickness of the base material layer was 0.55 mm. The single layer thickness of the adhesive layer was 0.55 mm.
[0467] [1.2] Punching process
[0468] The three-layer laminate was punched out using a punching die so as to form exposure through holes along the thickness direction, thereby forming a soft frame member having a long side length of 151 mm and a width of 4 mm and a short side length of 119 mm and a width of 4 mm.
[0469] [1.3] Preparation process
[0470] As a hard frame member, a rectangular pellicle assembly frame made of silicon (height: 0.725 mm, length of one side (long side): 151 mm, width of one side (long side): 4.0 mm, length of one side (short side): 119 mm, width of one side (short side): 4.0 mm) was prepared.
[0471] [1.4] Connection process
[0472] The hard frame member is lifted by decompression adsorption, and the outer periphery of the hard frame member is positioned in a manner consistent with the outer periphery of the soft frame member, and a load of 0.6N is pressed on the adhesive layer of the soft frame member at room temperature to integrate the hard frame member and the soft frame member. Thus, a protective film assembly frame is obtained. The height of the protective film assembly frame is 2.375mm.
[0473] For the obtained pellicle assembly, the apparent Young's modulus of the soft frame member, the apparent Young's modulus of the pellicle assembly frame, and the bending rigidity of the pellicle assembly frame were calculated from the above-mentioned formulas (iv), (v), and (vi) using the following parameters. The calculation results are shown in Table 1.
[0474] <Setting parameters>
[0475] ·Young's modulus (Ex) of rigid frame member (silicon): 185 GPa
[0476] ·Young's modulus of adhesive layer (Ex): 0.17MPa
[0477] Young's modulus of substrate layer (Ex): 3.50 GPa
[0478] b (width of one side (short side) of the pellicle assembly frame): 4 mm
[0479] Thickness of hard frame member: 0.725mm
[0480] · Single layer thickness of adhesive layer: (2.375mm-0.725mm) / total number of layers of soft frame components
[0481] ·Single layer thickness of substrate layer: (2.375mm-0.725mm) / total number of layers of soft frame components
[0482] Total number of layers of soft frame components: refer to Table 1
[0483] [2] Example 2 to Example 15
[0484] A pellicle was obtained and the Young's modulus of the rigid frame member was calculated in the same manner as in Example 1 except that the total number of layers, the single-layer thickness of the base layer, and the single-layer thickness of the adhesive layer were changed as shown in Table 1. The calculation results are shown in Table 1.
[0485] In Examples 4 to 15, a three-layer laminate of an adhesive layer / substrate sheet / adhesive layer and a two-layer laminate of an adhesive layer / substrate sheet were prepared, and the three-layer laminate and the two-layer laminate were stacked to produce a pellicle assembly frame in such a manner as to have the total number of layers shown in Table 1. For example, in Example 7, a pellicle assembly frame was produced by stacking a 2-layer laminate, a 2-layer laminate, a 2-layer laminate, a 2-layer laminate, and a 3-layer laminate in this order.
[0486] [3] Reference Example 1
[0487] like Figure 8 As shown, as the hard frame member 91, an anodized aluminum pellicle assembly frame (external dimensions: 150 mm×122 mm, height H91: 3.5 mm, width W: 2.0 mm) is prepared.
[0488] A dispenser is used to apply a prepared styrene butadiene resin adhesive to the original side end surface of the hard frame member 91. After a protective film is arranged thereon, hot pressing is performed at 100°C, and a flattening treatment is performed after heating to form a soft frame member 92 with a flat surface shape. Thus, a protective film assembly frame 90 is obtained. The thickness H92 of the soft frame member 92 is 0.5 mm.
[0489] For the obtained pellicle frame 90 , the Young's modulus and the like of the rigid frame member were calculated in the same manner as in Example 1.
[0490] The apparent Young's modulus of the pellicle assembly frame 90 of Reference Example 1 is 693 GPa (6.93×10 11 Pa). The bending rigidity of the pellicle assembly frame 90 of Reference Example 1 is 51.9×10 -2Pa·m 4 .
[0491] When pellicle 9 of Reference Example 1 was attached to an original plate, the strain amount of the original plate was not within the allowable range.
[0492] [Table 1]
[0493]
[0494] In Table 1, "total number of layers" indicates the sum of the number of substrate layers and the number of adhesive layers contained in the soft frame member. "Total thickness ratio of adhesive layers" indicates the ratio of the total thickness of adhesive layers contained in the soft frame member to the total thickness of substrate layers contained in the soft frame member. "Single layer thickness of adhesive layer" indicates the thickness of each adhesive layer contained in the soft frame member. "Single layer thickness of substrate layer" indicates the thickness of each substrate layer contained in the soft frame member. "Young's modulus ratio of substrate layer" indicates the ratio of the Young's modulus of the substrate layer contained in the soft frame member to the Young's modulus of the adhesive layer contained in the soft frame member.
[0495] The protective film assembly frame of Examples 1 to 15 includes a hard frame member and a soft frame member connected to the hard frame member. The soft frame member is formed by alternately stacking a base layer and an adhesive layer in the thickness direction with the adhesive layer arranged at both ends. The Young's modulus of the hard frame member is higher than the apparent Young's modulus of the soft frame member. The Young's modulus of the hard frame member is 185 GPa, which is greater than 25 GPa.
[0496] Therefore, the bending rigidity of the soft frame members of Examples 1 to 15 is 5.38×10 -2 Pa·m 4 The following is lower than the bending rigidity of the pellicle assembly frame of Reference Example 1 (51.9×10 -2 Pa·m 4 ) value. That is, it can be seen that the bending rigidity of the soft frame member of Examples 1 to 15 can reduce the strain of the original plate when the pellicle assembly is attached to the original plate. In other words, it can be seen that the pellicle assembly frame of the present disclosure can suppress the strain of the original plate caused by the deformation of the pellicle assembly frame.
[0497] Furthermore, the Young's modulus of the rigid frame members of Examples 1 to 15 is 185 GPa. That is, the rigid frame members of Examples 1 to 15 are sufficiently rigid. Therefore, it is known that the pellicle assembly frames of Examples 1 to 15 are not easily strained inwardly by the tension of the pellicle.
[0498] As described above, it can be seen that the pellicle assembly frames of Examples 1 to 15 can suppress strain caused by tension of the pellicle and can suppress strain of the original plate caused by deformation of the pellicle assembly frame.
[0499] The disclosed contents of Japanese Patent Application No. 2022-045814 filed on March 22, 2022 are incorporated herein by reference in their entirety.
[0500] All documents, patent applications, and technical standards described in this specification are incorporated herein by reference to the same extent as if each document, patent application, and technical standard was specifically and individually described as being incorporated by reference.
Claims
1. A protective film assembly frame, comprising: A rigid frame member for supporting the protective film, and A soft frame member connected to the hard frame member and used to connect to the original plate with a pattern, The soft frame member is formed by alternately stacking a base material layer and an adhesive layer in a thickness direction perpendicular to the surface direction of the protective film in such a manner that the adhesive layer is arranged at both ends. The Young's modulus of the hard frame member is higher than the apparent Young's modulus of the soft frame member. The Young's modulus of the rigid frame member is greater than or equal to 25 GPa. 2 . The pellicle assembly frame according to claim 1 , wherein the rigid frame member is formed of a single material. 3 . The pellicle assembly frame according to claim 1 , wherein the Young's modulus of the rigid frame member is 90 GPa or more. 4 . The pellicle assembly frame according to claim 1 , wherein a ratio of a height of the rigid frame member to a height of the pellicle assembly frame is 15% to 65%. 5 . The pellicle frame according to claim 1 , wherein the total number of the base material layer and the number of the adhesive layer is 5 or more. 6 . The pellicle assembly frame according to claim 3 , wherein the thickness of each of the adhesive layers is not less than 0.01 mm and not more than 0.5 mm. 7 . The pellicle frame according to claim 3 , wherein the total thickness of the adhesive layers included in the soft frame member is 0.2 to 4 times the total thickness of the base material layers included in the soft frame member. 8 . The pellicle frame according to claim 3 , wherein the Young's modulus of the base layer is not less than 10,000 times and not more than 9,000,000 times the Young's modulus of the adhesive layer. 9 . The pellicle frame according to claim 3 , wherein the thickness of each of the base material layers is 2.5 mm or less.
10. The protective film assembly frame according to claim 1, wherein the surface of the adhesive layer satisfies the following Any one of (A) to (C): (A) an inorganic layer is formed on at least the inner wall surface of the adhesive layer; (B) at least the inner wall surface of the adhesive layer satisfies the following formula (1); (C) At least the inner wall surface of the adhesive layer satisfies the following formula (2): Formula (1): ([CNO - 2s / [CNO - 50s ) ≥ 2.00 In the formula (1), [CNO - 2s ] indicates: using time-of-flight secondary ion mass spectrometry and using an ion source of Bi3 ++ ions and an irradiation area of 100 μm×100 μm, and a first deep portion at a first depth from the surface of the adhesive layer is analyzed to obtain CNO - The standardized intensity of The first depth is formed by irradiating a 600 μm square area of the surface with a sputtering ion gun using an argon cluster ion beam with a beam voltage of 20 kV and a beam current of 20 nA for a cumulative period of 2 seconds. [CNO - 50s ] indicates: CNO obtained by analyzing the second deep part at the second depth using time-of-flight secondary ion mass spectrometry - The standardized intensity of The second depth is formed by irradiating the region with the sputtering ion gun for a cumulative period of 50 seconds. Formula (2): In the formula (2), The C3 obtained by analyzing the first deep part by time-of-flight secondary ion mass spectrometry - The standardized intensity of The C3 obtained by analyzing the second deep part by time-of-flight secondary ion mass spectrometry - The standardized intensity. 11 . The pellicle assembly frame according to claim 1 , wherein the soft frame member includes a ventilation passage penetrating the soft frame member, or includes the ventilation passage and a ventilation filter disposed in the ventilation passage.
12. A protective membrane assembly, comprising: The pellicle assembly frame according to any one of claims 1 to 11, and A protective film is supported by the rigid frame member.
13. An exposure master comprising: Original with pattern, and The pellicle according to claim 12, which is attached to the surface of the original plate having the pattern.
14. An exposure device comprising: a light source for emitting exposure light, The exposure original plate according to claim 13, and an optical system for guiding the exposure light emitted by the light source to the exposure original plate, The exposure original plate is arranged so that the exposure light emitted from the light source is transmitted through the pellicle and irradiated onto the original plate.
15. A method for manufacturing a pellicle assembly, which is the method for manufacturing a pellicle assembly according to claim 12, comprising: A step of preparing the rigid frame member; A lamination step of alternately laminating at least one substrate layer sheet and a plurality of adhesive layers in the thickness direction to form a laminate; A punching step of punching the laminated body so as to form exposure through holes along the thickness direction, thereby forming the soft frame member; as well as A connecting step of connecting the hard frame member and the soft frame member.
16. The method for manufacturing a pellicle assembly according to claim 15, comprising at least one of the following steps: A step of coating an inorganic layer on at least the inner wall surface of the adhesive layer; A step of performing a plasma nitridation treatment on at least an inner wall surface of the adhesive layer; and A step of subjecting at least the inner wall surface of the adhesive layer to extreme ultraviolet ray irradiation.
17. The method for manufacturing a protective membrane assembly according to claim 15 or 16, wherein the soft frame member comprises a ventilation channel penetrating the soft frame member, The adhesive layer is an adhesive layer sheet. The manufacturing method includes a ventilation channel processing step, in which at least one unprocessed sheet for a substrate layer and a plurality of unprocessed sheets for adhesive layers are processed in a manner to form the ventilation channel, thereby forming the at least one substrate layer sheet and the plurality of adhesive layer sheets. The ventilation channel processing step is performed before the lamination step.
18. The method for manufacturing a pellicle assembly according to claim 17, wherein the soft frame member comprises the ventilation channel and a ventilation filter disposed in the ventilation channel, The manufacturing method includes a filter fixing step, in which the ventilation filter is arranged on a part of the at least one substrate layer sheet or the plurality of adhesive layer sheets in such a manner that the ventilation filter is arranged in the ventilation passage, The filter fixing step is performed after the ventilation duct processing step and before the laminating step.