Method, device and equipment for processing periodic defects of cold rolling mill and medium
By conducting offline grinding detection and fault type judgment on the cold rolling mill, the cause of defects is quickly determined and dealt with, and the radical problem of periodic defects in rolling mills in cold rolling production is solved, and the accuracy and production efficiency of defect treatment are improved.
Patent Information
- Application Number
- CN202411260759.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-10
- Publication Date
- 2024-11-19
AI Technical Summary
The radical problem of periodic defects of rolling mills in cold rolling production has caused serious impact on product quality and production efficiency, and the cause of defects cannot be found clearly during the defect treatment process, the processing time is long, and the cost of replacing rolls is wasted.
By conducting offline grinding and testing of the strip steel, determine the location and type of defects, determine whether it is a raw material defect, determine the working roller to be replaced if it is not a raw material defect, and if it is a raw material defect, it is picked up to achieve rapid and accurate treatment of periodic defects. .
It improves the accuracy of defect handling, reduces the occurrence of repetitive defect batch accidents, reduces the processing time and the cost of replacing rolls, and improves production efficiency.
Smart Images

Figure CN118976787A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of cold rolling control technology, and in particular to a method, device, equipment and medium for processing periodic defects of a cold rolling mill. Background Art
[0002] In the cold rolling production process, the incidence of rolling mill periodic defects is very high, and such defects seriously affect product quality and production efficiency. The treatment of defects mainly involves two aspects: root cause treatment and troubleshooting. In the cold rolling industry at home and abroad, the root cause treatment of rolling mill periodic defects has always been an industry problem, and no good method has been found so far. Therefore, reducing the impact of rolling mill periodic defects on product quality and production efficiency mainly relies on clear troubleshooting methods.
[0003] Rolling mill defect inspection is an important part of the production of cold rolling and acid rolling production lines. During the processing, the root causes of defects are often not found clearly, resulting in the recurrence of defects after the resumption of production. Secondly, during the processing, there are often multiple causes of defects that cannot be clearly identified, which can easily mislead on-site operators, ultimately leading to long processing time and waste of costs such as replacing rolls. Summary of the invention
[0004] The embodiments of the present application provide a method, device, equipment and medium for handling periodic defects of a cold rolling mill, which can perform different defect handling according to the type of defect, quickly determine the cause of the defect, solve the occurrence of batch accidents of repetitive defects during production line defect detection, and help improve the accuracy of defect handling.
[0005] In a first aspect, the present invention provides the following technical solution through an embodiment of the present invention:
[0006] A method for processing periodic defects of a cold rolling mill, comprising:
[0007] After offline grinding of the strip steel, detect whether there are defects on the surface of the strip steel after grinding; if there are defects on the surface of the strip steel, perform the following defect processing steps: determine the location of the defect according to the defect, and judge whether the defect is a raw material defect according to the defect; if it is judged that the defect is not a raw material defect, determine the working roll to be replaced based on the location of the defect, wherein the working roll to be replaced is the working roll corresponding to the faulty frame; if it is judged that the defect is a raw material defect, treat the raw material defect by pickling.
[0008] Preferably, determining the location of the defect based on the defect includes: obtaining the defect length based on the defect; determining the exit thickness of the faulty frame based on the defect length, the working roll diameter of the rolling mill and the set exit thickness of the defective coil; and determining the location of the defect based on the exit thickness of the faulty frame.
[0009] Preferably, before the offline grinding of the strip, it also includes: detecting whether there are visible defects on the upper surface of the strip; if there are visible defects on the upper surface of the strip, determining the location of the defects and judging whether the defects are raw material defects; if the defects are judged to be raw material defects, determining the working roll to be replaced based on the location of the defects.
[0010] Preferably, if it is determined that the defect is not a raw material defect, the upper surface defect rolling mill troubleshooting step is executed to determine the roll to be replaced; the upper surface defect rolling mill troubleshooting step includes: detecting whether there are defects on the roll surface of each roll in the target roll, wherein the target roll includes the working roll of the faulty frame, the intermediate roll of the faulty frame, the working roll of the front frame of the faulty frame, and the intermediate roll of the front frame of the faulty frame; if any roll surface has defects, the working rolls of the faulty frame and the front frame are controlled to press down a roll gap of a preset length; detecting whether there are defects on the roll surface of the support roll of the faulty frame and the roll surface of the support roll of the front frame; if it is detected that there are defects on the roll surface of the support roll of the faulty frame, it is determined that the support roll of the faulty frame is the roll to be replaced, and if it is detected that there are defects on the roll surface of the support roll of the front frame, it is determined that the support roll of the front frame is the roll to be replaced; if it is detected that the roll surfaces of all support rolls are free of defects, it is determined that the working roll of the faulty frame and the intermediate roll of the faulty frame are the rolls to be replaced.
[0011] Preferably, controlling the working rolls of the faulty frame and the front frame to press down a roll gap of a preset length includes: judging whether the size of the defect is larger than a preset defect size; if the size of the defect is larger than the preset defect size, controlling the working rolls of the faulty frame and the front frame to press down a roll gap of a preset length.
[0012] Preferably, before the offline grinding of the strip, it also includes: detecting whether there are visible defects on the lower surface of the strip; if there are visible defects on the lower surface of the strip, determining the location of the defect and judging whether the defect is a raw material defect; if it is judged that the defect is a raw material defect, determining the roller to be replaced based on the location of the defect.
[0013] Preferably, if it is determined that the defect is not a raw material defect, the lower surface defect mill troubleshooting step is performed to determine the roll to be replaced; the lower surface defect mill troubleshooting step includes: detecting whether there are defects on the roll surface of each roll in the target roll, wherein the target roll includes the working roll of the faulty stand, the intermediate roll of the faulty stand, the working roll of the front stand of the faulty stand, and the intermediate roll of the front stand of the faulty stand; if there are defects on the roll surface of the intermediate roll of the faulty stand, it is determined whether the size of the defect is greater than the preset defect size; if the size of the defect is greater than the preset defect size, If the roller surface of the support roller of the faulty frame and the roller surface of the support roller of the front frame are defective, it is detected whether there are defects; if the roller surface of the support roller of the faulty frame has defects, it is determined that the support roller of the faulty frame is the roller to be replaced, and if the roller surface of the support roller of the front frame has defects, it is determined that the support roller of the front frame is the roller to be replaced; if the roller surfaces of all support rollers do not have defects, or the size of the defect is less than or equal to the preset defect size, it is determined that the working roller of the faulty frame and the intermediate roller of the faulty frame are the rollers to be replaced.
[0014] In a second aspect, the present invention provides the following technical solution through an embodiment of the present invention:
[0015] A cold rolling mill periodic defect processing device, comprising:
[0016] A defect detection module is used to detect whether there are defects on the surface of the strip after offline grinding of the strip;
[0017] The defect processing module is used to perform the following defect processing steps if there are defects on the strip surface:
[0018] The location of the defect is determined according to the defect, and whether the defect is a raw material defect is judged; if it is judged that the defect is not a raw material defect, the working roll to be replaced is determined based on the location of the defect; if it is judged that the defect is a raw material defect, the raw material defect is treated by pickling.
[0019] In a third aspect, the present invention provides the following technical solution through an embodiment of the present invention:
[0020] An electronic device comprises: a memory, a processor and a computer program stored in the memory and executable on the processor, wherein when the processor executes the program, the steps of any one of the methods described in the first aspect are implemented.
[0021] In a fourth aspect, the present invention provides the following technical solution through an embodiment of the present invention:
[0022] A computer-readable storage medium stores a computer program, which, when executed by a processor, implements the steps of any one of the methods described in the first aspect.
[0023] One or more technical solutions provided in the embodiments of the present application have at least the following technical effects or advantages:
[0024] The method for processing periodic defects of a cold rolling mill provided in an embodiment of the present invention first performs offline grinding on the strip, and can detect a variety of subtle defects on the surface of the strip. After determining that there are defects, the location of the defects and whether the defects are raw material defects are further determined. In the case of raw material defects, the working rolls to be replaced can be determined based on the location of the defects, that is, the working rolls corresponding to the faulty frame, so that the periodic defects that are not easily detected can be quickly processed. This method associates the morphology of the periodic defects of the rolling mill with the causes, can perform different defect processing according to the type of defects, and can quickly determine the causes of the defects, solve the occurrence of batch accidents of repetitive defects during the defect inspection of the production line, and provides a high accuracy rate for the periodic defect inspection of the rolling mill, which is conducive to improving the accuracy of defect processing. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0026] Figure 1 It is a flow chart of a method for processing periodic defects of a cold rolling mill in an embodiment of the present invention;
[0027] Figure 2 It is a schematic diagram of the process of polishing visible periodic defects in an embodiment of the present invention;
[0028] Figure 3 It is a schematic diagram of the process of processing visible periodic defects on the upper surface in an embodiment of the present invention;
[0029] Figure 4 It is a schematic diagram of the process of processing visible periodic defects on the lower surface in an embodiment of the present invention;
[0030] Figure 5 It is a structural schematic diagram of a periodic defect processing device for a cold rolling mill in an embodiment of the present invention;
[0031] Figure 6 A schematic structural diagram of an electronic device in an embodiment of the present invention. DETAILED DESCRIPTION
[0032] The embodiments of the present application provide a method, device, equipment and medium for handling periodic defects of a cold rolling mill, which can perform different defect handling according to the type of defect, quickly determine the cause of the defect, solve the occurrence of batch accidents of repetitive defects during production line defect detection, and help improve the accuracy of defect handling.
[0033] The technical solution of the embodiment of the present application is to solve the above technical problems, and the overall idea is as follows:
[0034] A method for processing periodic defects of a cold rolling mill comprises: after offline grinding of a steel strip, detecting whether there are defects on the surface of the steel strip after grinding; if there are defects on the surface of the steel strip, executing the following defect processing steps: determining the location of the defect according to the defect, and judging whether the defect is a raw material defect according to the defect; if it is judged that the defect is not a raw material defect, determining a working roll to be replaced based on the location of the defect, the working roll to be replaced is a working roll corresponding to a faulty frame; if it is judged that the defect is a raw material defect, treating the raw material defect by pickling.
[0035] In order to better understand the above technical solution, the above technical solution will be described in detail below in conjunction with the accompanying drawings and specific implementation methods.
[0036] In a first aspect, an embodiment of the present invention provides a method for processing periodic defects of a cold rolling mill. Specifically, Figure 1 As shown, the method includes the following steps S101 to S105:
[0037] Step S101, after offline grinding of the steel strip, detect whether there are defects on the surface of the grinded steel strip.
[0038] In the cold rolling production process, a strip steel coil is taken out as the strip steel to be tested, the strip steel coil is unrolled, and the unrolled strip steel is subjected to offline grinding treatment, wherein the grinding process can be performed by grinding the upper and lower surfaces of the strip steel by an upper surface grinding robot and a lower surface grinding robot, and a camera device is used to collect in real time whether there are defects on the upper and lower surfaces of the strip steel after grinding. Alternatively, the surface of the strip steel after grinding is manually checked for defects.
[0039] Step S102: If there are defects on the surface of the steel strip, the following defect processing steps are performed:
[0040] Step S103, determining the location of the defect according to the defect, and judging whether the defect is a raw material defect according to the defect;
[0041] In order to reduce damage to the strip, if defects are detected on the surface of the strip, the rolling mill will be controlled to stop first. After the rolling mill is stopped, the main operator of the rolling mill will display the defect information and execute the defect processing steps: determine the location of the defect based on the defect, and determine whether the defect is a raw material defect based on the defect.
[0042] In a specific embodiment, determining the location of a defect based on the defect may include: obtaining a defect length based on the defect; determining an exit thickness of a faulty frame based on the defect length, a working roll diameter of the rolling mill, and a set exit thickness of the defective coil; and determining the location of the defect based on the exit thickness of the faulty frame.
[0043] Optionally, the main operator of the rolling mill is connected to a camera device, and the camera device detects a defect image, and the main operator of the rolling mill can calculate the defect length based on the defect image.
[0044] According to the defect length, the working roll diameter of the rolling mill and the set exit thickness of the defective coil, the exit thickness of the faulty stand is determined, which may include: substituting the defect length, the working roll diameter of the rolling mill and the set exit thickness of the defective coil into the formula H=(L×h) / (3.14×R) to calculate the exit thickness of the faulty stand, where H=exit thickness of the faulty stand, L=defect length, h=set exit thickness of the defective coil, is a set value, and R is the working roll diameter of the rolling mill. The set exit thickness of the defective coil is the set exit thickness corresponding to the strip coil, and the faulty stand refers to the stand where the rubbing occurs.
[0045] The calculated outlet thickness of the faulty frame is compared with the set outlet thicknesses of multiple frames in the rolling mill to determine the frame corresponding to the outlet thickness of the faulty frame.
[0046] In a specific embodiment, after detecting the presence of defects on the strip surface, it is also determined whether the defects are raw material defects based on the defects. Specifically, the surface of the strip is quickly scanned by a pickling reverse lookup table inspection device (e.g., a high-speed camera), and whether the detected defects are raw material defects is found from a preset database pre-stored in the main operation of the rolling mill, wherein the preset database includes a correspondence between multiple raw material defect images and defect types.
[0047] Step S104, if it is determined that the defect is not a raw material defect, then based on the location where the defect occurs, determining the working roll to be replaced, the working roll to be replaced is the working roll corresponding to the faulty frame;
[0048] Step S105: if it is determined that the defect is a raw material defect, the raw material defect is treated by pickling.
[0049] In a specific embodiment, if it is determined that the defect is not a raw material defect, it can be determined that the defect is a periodic defect, and according to the location of the defect, the working roll of the frame corresponding to the thickness of the faulty frame outlet can be determined as the working roll to be replaced. If the defect is determined to be a raw material defect, the raw material defect is treated by pickling.
[0050] In order to ensure that the cause of the defect has been effectively solved, after the roll to be replaced is replaced, the method further includes: controlling the rolling mill to restart, and re-detecting the surface defects of the strip after the strip has rolled a preset distance; if defects are detected on the surface of the strip again, continuing to perform the defect treatment step. Optionally, the preset distance can be between 20 and 25 meters.
[0051] In a specific embodiment, Figure 2 As shown, after detecting the presence of defects on the strip surface, the process may further include: controlling the rolling mill to run at a low speed. Specifically, before determining that the defects have been eliminated, in order to avoid quality loss, the rolling mill runs at a low speed; the offline quality inspection station rechecks whether the defects have been eliminated; after the defects are eliminated, the production line resumes normal production. If the defects are not eliminated, the defect handling step is continued. Optionally, the rolling mill may run at a low speed of 60 m / min.
[0052] Furthermore, in order to achieve rapid processing of visible defects on the strip surface, such as Figure 3 As shown, before offline grinding of the strip, the following may also be included: step S201, scanning the upper surface of the strip for defects to determine whether there are visible defects on the upper surface of the strip; step S202, if there are visible defects on the upper surface of the strip, determining the location of the defects and judging whether the defects are raw material defects; step S203, if it is judged that the defects are raw material defects, determining the working roll to be replaced based on the location of the defects.
[0053] In a specific embodiment, the upper surface of the strip is quickly scanned by a camera device at the offline quality inspection station to determine whether there are visible defects on the upper surface of the strip. If visible defects are collected, a stop signal is sent to the main operator of the rolling mill to control the rolling mill to stop. The main operator of the rolling mill calculates the thickness of the faulty stand outlet according to the formula H = (L×h) / (3.14×R) to determine the location of the defect.
[0054] Optionally, after the rolling mill is shut down, the main operator of the rolling mill displays the defect information and issues a shutdown alarm so as to promptly notify maintenance personnel.
[0055] If the defect is determined to be a raw material defect, based on the location of the defect, the working roll of the stand corresponding to the thickness at the exit of the faulty stand can be determined as the working roll to be replaced, and the working roll to be replaced is replaced. After determining the preset rolling distance after the roll replacement is completed, a review is performed, which may include scanning and detecting the surface defects of the strip through a camera device. If the quality is normal (no defects), normal production is resumed. If there are still defects on the surface of the strip, the machine is stopped for inspection according to steps S202 to S203.
[0056] If it is determined that the defect is not a raw material defect, the upper surface defect mill troubleshooting step is performed to determine the roll to be replaced. Specifically, the upper surface defect mill troubleshooting step includes: performing offline detection on multiple target rolls to determine whether the roll surface of each roll has defects, wherein the multiple target rolls include the working rolls of the faulty frame, the intermediate rolls of the faulty frame, the working rolls of the front frame of the faulty frame, and the intermediate rolls of the front frame of the faulty frame; if any roll surface has defects, the working rolls of the faulty frame and the front frame are controlled to press down a preset length of roll gap; detect whether the roll surface of the support rolls of the faulty frame and the front frame has defects; if the roll surface of the support roll of the faulty frame is detected to have defects, the support roll of the faulty frame is determined to be the roll to be replaced, and if the roll surface of the support roll of the front frame is detected to have defects, the support roll of the front frame is determined to be the roll to be replaced; if the roll surfaces of all support rolls are detected to have no defects, the working rolls of the faulty frame and the intermediate rolls of the faulty frame are determined to be the rolls to be replaced.
[0057] It should be noted that the purpose of inspecting the roller surface of the front frame working roller of the faulty frame and the front frame middle roller of the faulty frame is to confirm that the front roller is not damaged and to prevent small pieces of tissue from peeling off and damaging the roller, resulting in misjudgment.
[0058] In a specific embodiment, multiple target rolls are taken out and offline inspection is performed on the multiple target rolls. Specifically, in order to quickly check the cause of the defect, controlling the working rolls of the faulty frame and the front frame to press down the roll gap of a preset length may include: judging whether the size of the defect is greater than the preset defect size; if the size of the defect is greater than the preset defect size, inserting multiple target rolls, and controlling the working rolls of the faulty frame and the front frame to press down the roll gap of the preset length.
[0059] Optionally, the preset defect size may be 3 mm. The preset length of the roll gap may be a 16 mm roll gap. By judging the defect size, it is used to distinguish the inspection direction according to the defect size. When periodic defects are visible on the upper surface of the strip and the defect length is detected to be greater than 3 mm, the roll surface of the upper support roll is rotated for inspection to achieve a comprehensive inspection and avoid inspection blind spots.
[0060] Specifically, take out the working rolls of the faulty frame, the middle rolls of the faulty frame, the working rolls of the front frame, and the middle rolls of the front frame, and inspect the inside of the frame and the rolls. If there are defects on any roll surface, determine whether the defect is greater than 3mm. If so, continue to check the roll surface of the support roll and mark it after checking a single side.
[0061] Specifically, checking the roll surface of the support roller includes: inserting the working rolls of the faulty frame, the middle rolls of the faulty frame and the working rolls of the front frame, and pressing down the roll gap of 16mm on the working rolls of the faulty frame and the front frame, and rotating and re-inspecting after loading the roll gap of 16mm, to ensure that the support rollers of the two frames are checked once, and if the roll surface of the support roller of a certain frame is detected to be defective, the support roller of the corresponding frame is replaced; when the roll surfaces of all support rollers are free of defects, the working rolls and middle rolls of the faulty frame are replaced.
[0062] If the size of the defect is determined to be less than or equal to the preset defect size, the working roll and the intermediate roll of the faulty frame are determined to be the rolls to be replaced. Specifically, if the size of the defect is determined to be less than or equal to 3 mm, a prompt to replace the roll is issued, and the working roll and the intermediate roll of the faulty frame are directly replaced.
[0063] Furthermore, after replacing the corresponding rollers through the above steps, a re-inspection is carried out after starting the vehicle and rolling for a preset distance. The re-inspection may include scanning and detecting surface defects of the strip through a camera device. If the quality is normal, normal production is resumed. If defects still exist on the surface of the strip, the machine is stopped for inspection according to steps S202 to S203.
[0064] If the equipment is found to have damaged rollers, proceed to the next step: If the equipment is damaged, issue a maintenance reminder so that the equipment maintenance personnel can be contacted immediately to the site to find the cause of the equipment damage and deal with the root cause of the defect. Start the machine and roll for 20 meters for re-inspection. If the quality is normal, resume production. If there are still defects after the re-inspection, continue to stop and inspect according to steps S202~S203; if there are no abnormalities after the re-inspection, replace the corresponding frame rollers, and start the machine and roll for 20 meters for re-inspection. If the quality is normal, resume production. If there are still defects after the re-inspection, continue to stop and inspect according to steps S202~S203.
[0065] Furthermore, in order to achieve rapid processing of visible defects on the strip surface, such as Figure 4 As shown, before offline grinding of the strip, the following may also be included: step S301, scanning the lower surface of the strip for defects to determine whether there are visible defects on the lower surface of the strip; step S302, if there are visible defects on the lower surface of the strip, determining the location of the defects and judging whether the defects are raw material defects; step S303, if it is judged that the defects are raw material defects, determining the roller to be replaced based on the location of the defects.
[0066] In a specific embodiment, the lower surface of the strip is quickly scanned by a camera device at the offline quality inspection station to determine whether there are visible defects on the lower surface of the strip. If visible defects are collected, a stop signal is sent to the main operator of the rolling mill to control the rolling mill to stop. The main operator of the rolling mill calculates the thickness of the faulty stand outlet according to the formula H=L*h / 3.14*R to determine the location of the defect.
[0067] Optionally, after the rolling mill is shut down, the main operator of the rolling mill will display the defect information and issue a shutdown alarm so as to promptly notify maintenance personnel.
[0068] If the defect is found to be a raw material defect through pickling reverse table inspection, based on the location of the defect, it can be determined that the working roll of the frame corresponding to the thickness of the faulty frame outlet is the working roll to be replaced, and the working roll to be replaced is replaced. After determining the preset distance of the starting rolling after the roll replacement is completed, a review is conducted, which may include scanning and detecting the surface defects of the strip through a camera device. If the quality is normal, production is resumed. If there are still defects on the surface of the strip, the shutdown inspection is continued according to steps S302 to S303. Among them, the preset distance can be between 20 and 25 meters.
[0069] If the defect is not a raw material defect detected by the pickling reverse table inspection, the lower surface defect mill troubleshooting step is executed to determine the roll to be replaced, and the lower surface defect mill troubleshooting step includes: performing offline inspection on multiple target rolls to determine whether there are defects on the roll surface of each roll, wherein the multiple target rolls include the working rolls of the faulty stand, the intermediate rolls of the faulty stand, the working rolls of the front stand of the faulty stand, and the intermediate rolls of the front stand of the faulty stand; if there are defects on the roll surface of the intermediate rolls of the faulty stand, it is determined whether the size of the defect is greater than the preset defect size; if the size of the defect is greater than the preset If the defect size is set, the support rollers of the faulty frame and the front frame are tested offline to determine whether there are defects on the roller surfaces of the support rollers of the faulty frame and the front frame; if there are defects on the roller surfaces of the support rollers of the faulty frame, the support rollers of the faulty frame are determined to be the rollers to be replaced; if there are defects on the roller surfaces of the support rollers of the front frame, the support rollers of the front frame are determined to be the rollers to be replaced; if there are no defects on the roller surfaces of all support rollers, or the size of the defects is less than or equal to the preset defect size, the working rollers of the faulty frame and the intermediate rollers of the faulty frame are determined to be the rollers to be replaced.
[0070] Specifically, the working rolls of the faulty frame, the intermediate rolls of the faulty frame, the working rolls of the front frame, and the intermediate rolls of the front frame are taken out for inspection inside the frame and the rolls. If defects are detected on the surface of the intermediate rolls of the faulty frame, it is determined whether the defect size is greater than 3 mm. If so, the roll surface of the lower support rolls of the faulty frame and the front frame is tested offline. If defects are detected on the surface of the working rolls of the faulty frame, the working rolls of the faulty frame are replaced.
[0071] Specifically, checking the roller surface of the lower support roller includes: if the roller surface of the lower support roller of a certain frame is detected to be defective, replacing the lower support roller of the corresponding frame; when the roller surfaces of all lower support rollers are free of defects, replacing the working rollers and intermediate rollers of the faulty frame.
[0072] If the size of the defect is determined to be less than or equal to the preset defect size, the working roll and the intermediate roll of the faulty frame are determined to be the rolls to be replaced. Specifically, if the size of the defect is determined to be less than or equal to 3 mm, a prompt to replace the roll is issued, and the working roll and the intermediate roll of the faulty frame are directly replaced.
[0073] Furthermore, in order to ensure that the causes of the defects have been effectively resolved, after replacing the corresponding rollers through the above steps, a review is carried out after starting the vehicle and rolling a preset distance. The review may include scanning and detecting surface defects of the strip through a camera device. If the quality is normal, normal production is resumed. If defects still exist on the surface of the strip, the machine is stopped for inspection according to steps S302 to S303.
[0074] If the equipment is found to have damaged rollers, proceed to the next step: If the equipment is damaged, issue a maintenance reminder so that the equipment maintenance personnel can be contacted immediately to the site to find the cause of the equipment damage and deal with the root cause of the defect. Start the machine and roll for 20 meters for re-inspection. If the quality is normal, resume production. If there are still defects after re-inspection, continue to stop and inspect according to steps S202~S203. If there are no abnormalities after re-inspection, replace the corresponding frame rollers, start the machine and roll for 20 meters for re-inspection. If the quality is normal, resume production. If there are still defects after re-inspection, continue to stop and inspect according to steps S202~S203.
[0075] In order to better understand the above technical solution, the above technical solution is described in detail below:
[0076] During the operation of the cold rolling mill, the strip is inspected offline. First, the upper and lower surfaces of the strip are scanned for defects to determine whether there are visible defects on the upper and lower surfaces of the strip. If there are defects on the upper surface, it is determined whether the defects are raw material defects. If not, the upper surface defect mill troubleshooting steps are performed to determine the roller to be replaced. If there are defects on the lower surface, it is determined whether the defects are raw material defects. If not, the lower surface defect mill troubleshooting steps are performed to determine the roller to be replaced. After the upper and lower surfaces are scanned for defects, the strip is ground offline to detect whether there are defects on the surface of the ground strip. If there are defects, it is determined whether the defects are raw material defects. If not, the working roller to be replaced is determined based on the location of the defect. In this way, the strip is inspected.
[0077] This application deals with defects from multiple aspects, such as defect differentiation, inspection process, and determination method. In terms of defect differentiation, defects are divided into visible marks from grinding, visible marks from the upper surface, and visible marks from the lower surface. This classification serves as the basis for the inspection process and clarifies the method for determining the location of each type of defect. This method can effectively reduce the processing time of periodic defects in the pickling process, and greatly reduce the risks of periodic defects to production.
[0078] In summary, a method for handling periodic defects of a cold rolling mill provided by an embodiment of the present invention has a process for conventional defect handling procedures, in which there is no defect inspection, and no process for increasing the degree of attention paid to the cause of the defect by comparing the defect morphology, which leads to frequent recurrence of defects, wrong roll replacement, etc., thus causing large-scale quality accidents. The method can perform different defect treatments according to the type of defect, quickly determine the cause of the defect, determine the working roll to be replaced based on the detected defect information, solve the occurrence of batch accidents of repetitive defects during the production line defect inspection process, and is conducive to improving the accuracy of defect handling.
[0079] In the second aspect, based on the same inventive concept, this embodiment provides a cold rolling mill periodic defect processing device, such as Figure 5 As shown, including:
[0080] The defect detection module 401 is used to detect whether there are defects on the surface of the strip after offline grinding of the strip;
[0081] The defect processing module 402 is used to perform the following defect processing steps if there are defects on the surface of the strip:
[0082] The location of the defect is determined according to the defect, and whether the defect is a raw material defect is judged; if it is judged that the defect is not a raw material defect, the working roll to be replaced is determined based on the location of the defect; if it is judged that the defect is a raw material defect, the raw material defect is treated by pickling.
[0083] As an optional embodiment, the defect processing module 402 is specifically used to: obtain the defect length according to the defect; determine the faulty frame exit thickness according to the defect length, the working roll diameter of the rolling mill and the set exit thickness of the defective coil; and determine the location where the defect occurs based on the faulty frame exit thickness.
[0084] As an optional embodiment, the device also includes: an upper surface defect scanning module, which is used to detect whether there are visible defects on the upper surface of the strip; if there are visible defects on the upper surface of the strip, the location of the defect is determined, and whether the defect is a raw material defect is judged; if the defect is judged to be a raw material defect, the working roll to be replaced is determined based on the location of the defect.
[0085] As an optional embodiment, the device further includes:
[0086] The first rolling mill determination module is used for executing the upper surface defect rolling mill troubleshooting step to determine the rolling mill to be replaced if it is determined that the defect is not a raw material defect; the upper surface defect rolling mill troubleshooting step includes: detecting whether the roll surface of each rolling mill in the target rolling mill has defects, wherein the target rolling mill includes the working roll of the faulty frame, the intermediate roll of the faulty frame, the working roll of the front frame of the faulty frame, and the intermediate roll of the front frame of the faulty frame; if any roll surface has defects, the working rolls of the faulty frame and the front frame are controlled to press down a roll gap of a preset length; detecting whether the roll surface of the support roll of the faulty frame and the roll surface of the support roll of the front frame have defects; if it is detected that the roll surface of the support roll of the faulty frame has defects, the support roll of the faulty frame is determined to be the rolling mill to be replaced, and if it is detected that the roll surface of the support roll of the front frame has defects, the support roll of the front frame is determined to be the rolling mill to be replaced; if it is detected that the roll surfaces of all support rolls have no defects, the working roll of the faulty frame and the intermediate roll of the faulty frame are determined to be the rolling mill to be replaced.
[0087] As an optional embodiment, the defect-generating rolling roller determination module is specifically used to: determine whether the size of the defect is greater than a preset defect size; if the size of the defect is greater than the preset defect size, control the working rolls of the faulty frame and the front frame to press down a roll gap of a preset length.
[0088] As an optional embodiment, the device also includes: a lower surface defect scanning module, which is used to detect whether there are visible defects on the lower surface of the steel strip; if there are visible defects on the lower surface of the steel strip, the location of the defect is determined, and it is judged whether the defect is a raw material defect; if the defect is determined to be a raw material defect, the rolling mill to be replaced is determined based on the location of the defect.
[0089] As an optional embodiment, the device further includes:
[0090] The second rolling mill determination module is used for executing the lower surface defect rolling mill troubleshooting step to determine the rolling mill to be replaced if it is determined that the defect is not a raw material defect; the lower surface defect rolling mill troubleshooting step includes: detecting whether the roll surface of each rolling mill in the target rolling mill has defects, wherein the target rolling mill includes the working roll of the faulty frame, the intermediate roll of the faulty frame, the working roll of the front frame of the faulty frame, and the intermediate roll of the front frame of the faulty frame; if there is a defect on the roll surface of the intermediate roll of the faulty frame, it is determined whether the size of the defect is greater than the preset defect size; if the size of the defect is greater than the preset defect size, detecting whether the roll surface of the support roll of the faulty frame and the roll surface of the support roll of the front frame have defects; if there is a defect on the roll surface of the support roll of the faulty frame, it is determined that the support roll of the faulty frame is the rolling mill to be replaced, and if there is a defect on the roll surface of the support roll of the front frame, it is determined that the support roll of the front frame is the rolling mill to be replaced; if there is no defect on the roll surface of all the support rolls, or the size of the defect is less than or equal to the preset defect size, it is determined that the working roll of the faulty frame and the intermediate roll of the faulty frame are the rolling mill to be replaced. The above modules can be implemented by software codes, in which case, the above modules can be stored in the memory of the control device. The above modules can also be implemented by hardware such as integrated circuit chips.
[0091] An embodiment of the present invention provides a device for processing periodic defects of a cold rolling mill, and its implementation principle and technical effects are the same as those of the aforementioned method embodiment. For the sake of brief description, for matters not mentioned in the device embodiment, reference may be made to the corresponding contents in the aforementioned method embodiment.
[0092] In a third aspect, based on the same inventive concept, this embodiment provides an electronic device 500, such as Figure 6 As shown, it includes: a memory 501, a processor 502 and a computer program 503 stored in the memory and executable on the processor. When the processor 502 executes the program, the steps of the defect handling method described in the first aspect are implemented.
[0093] Since the electronic device introduced in this embodiment is an electronic device used to implement the defect handling method in the embodiment of the present application, based on the defect handling method introduced in the embodiment of the present application, a person skilled in the art can understand the specific implementation of the electronic device of the present embodiment and its various variations, so how the electronic device implements the method in the embodiment of the present application is not described in detail here. As long as a person skilled in the art implements the electronic device used in the defect handling method in the embodiment of the present application, it belongs to the scope of protection of this application.
[0094] Those skilled in the art will appreciate that embodiments of the present invention may be provided as methods, systems, or computer program products. Therefore, the present invention may take the form of a complete hardware embodiment, a complete software embodiment, or an embodiment combining software and hardware. Moreover, the present invention may take the form of a computer program product implemented on one or more computer-usable storage media (including but not limited to disk storage, CD-ROM, optical storage, etc.) containing computer-usable program code.
[0095] The present invention is described with reference to flowcharts and / or block diagrams of methods, devices (systems), and computer program products according to embodiments of the present invention. It should be understood that each process and / or block in the flowchart and / or block diagram, as well as the combination of processes and / or blocks in the flowchart and / or block diagram, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, a special-purpose computer, an embedded processor, or other programmable data processing device to produce a machine, so that the instructions executed by the processor of the computer or other programmable data processing device generate instructions for implementing the processes in the flowchart and / or block diagram. Figure 1 A process or multiple processes and / or boxes Figure 1 A module that specifies functions in one or more boxes.
[0096] These computer program instructions may also be stored in a computer-readable memory that can direct a computer or other programmable data processing device to work in a specific manner, so that the instructions stored in the computer-readable memory produce a manufactured product including an instruction module, which is implemented in the process Figure 1 A process or multiple processes and / or boxes Figure 1 A function specified in one or more boxes.
[0097] These computer program instructions can also be loaded onto a computer or other programmable data processing device so that a series of operating steps are executed on the computer or other programmable device to produce a computer-implemented process, thereby providing instructions for implementing the process. Figure 1 A process or multiple processes and / or boxes Figure 1 A step that specifies a function in one or more boxes.
[0098] Although the preferred embodiments of the present invention have been described, those skilled in the art may make other changes and modifications to these embodiments once they have learned the basic creative concept. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments and all changes and modifications that fall within the scope of the present invention.
[0099] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.
Claims
1. A method for processing periodic defects of a cold rolling mill, characterized in that: include: After the strip is offline ground, the surface of the ground strip is tested for defects; If there are defects on the strip surface, perform the following defect treatment steps: Determining the location of the defect according to the defect, and judging whether the defect is a raw material defect according to the defect; If it is determined that the defect is not a raw material defect, the working roll to be replaced is determined based on the location where the defect occurs, wherein the working roll to be replaced is the working roll corresponding to the faulty frame; If the defect is determined to be a raw material defect, the raw material defect is treated by pickling.
2. The method according to claim 1, characterized in that Determining the location where the defect occurs according to the defect includes: Obtaining a defect length according to the defect; Determine the exit thickness of the faulty stand according to the defect length, the working roll diameter of the rolling mill and the set exit thickness of the defective coil; Based on the faulty rack exit thickness, the location where the defect occurs is determined.
3. The method according to claim 1, characterized in that Before the strip steel is subjected to offline grinding, the process also includes: Detecting whether there are visible defects on the upper surface of the steel strip; If there are visible defects on the upper surface of the steel strip, determine the location of the defect and judge whether the defect is a raw material defect; If the defect is determined to be a raw material defect, the working roll to be replaced is determined based on the location where the defect occurs.
4. The method according to claim 3, characterized in that If it is determined that the defect is not a raw material defect, the step of checking the surface defect rolling mill is performed to determine the roll to be replaced; The upper surface defect mill troubleshooting step comprises: detecting whether the roll surface of each roll in the target roll has defects, wherein the target roll includes the working roll of the faulty stand, the middle roll of the faulty stand, the working roll of the front stand of the faulty stand, and the middle roll of the front stand of the faulty stand; If there is a defect on any roll surface, the working rolls of the faulty frame and the front frame are controlled to press down a roll gap of a preset length; Detecting whether the roller surface of the support roller of the faulty frame and the roller surface of the support roller of the front frame have defects; If it is detected that there are defects on the roller surface of the support roller of the faulty frame, the support roller of the faulty frame is determined to be the roller to be replaced; if it is detected that there are defects on the roller surface of the support roller of the front frame, the support roller of the front frame is determined to be the roller to be replaced; if it is detected that there are no defects on the roller surfaces of all support rollers, the working roller of the faulty frame and the intermediate roller of the faulty frame are determined to be the rollers to be replaced.
5. The method according to claim 4, characterized in that The method of controlling the working rolls of the faulty frame and the front frame to press down the roll gap of a preset length comprises: Determining whether the size of the defect is greater than a preset defect size; If the size of the defect is larger than a preset defect size, the working rolls of the faulty frame and the front frame are controlled to press down a roll gap of a preset length.
6. The method according to claim 1, characterized in that Before the strip steel is subjected to offline grinding, the process also includes: Detecting whether there are visible defects on the lower surface of the steel strip; If there are visible defects on the lower surface of the steel strip, the location of the defect is determined, and whether the defect is a raw material defect; If the defect is determined to be a raw material defect, the roller to be replaced is determined based on the location where the defect occurs.
7. The method according to claim 6, characterized in that If it is determined that the defect is not a raw material defect, the surface defect rolling mill troubleshooting step is performed to determine the roll to be replaced; The step of checking the lower surface defective rolling mill comprises: detecting whether the roll surface of each roll in the target roll has defects, wherein the target roll comprises the working roll of the faulty stand, the middle roll of the faulty stand, the working roll of the front stand of the faulty stand and the middle roll of the front stand of the faulty stand; If there is a defect on the roller surface of the intermediate roller of the faulty frame, determining whether the size of the defect is greater than a preset defect size; If the size of the defect is larger than the preset defect size, detecting whether the roller surface of the support roller of the faulty frame and the roller surface of the support roller of the front frame have defects; If there is a defect on the roller surface of the support roller of the faulty frame, the support roller of the faulty frame is determined to be a roller to be replaced; if there is a defect on the roller surface of the support roller of the front frame, the support roller of the front frame is determined to be a roller to be replaced; If there are no defects on the roll surfaces of all support rolls, or the size of the defect is less than or equal to the preset defect size, the working rolls of the faulty stand and the intermediate rolls of the faulty stand are determined to be the rolls to be replaced.
8. A cold rolling mill periodic defect processing device, characterized in that: include: A defect detection module is used to detect whether there are defects on the surface of the strip after offline grinding of the strip; The defect processing module is used to perform the following defect processing steps if there are defects on the strip surface: The location of the defect is determined according to the defect, and whether the defect is a raw material defect is judged; if it is judged that the defect is not a raw material defect, the working roll to be replaced is determined based on the location of the defect; if it is judged that the defect is a raw material defect, the raw material defect is treated by pickling.
9. An electronic device, characterized in that: include: A memory, a processor, and a computer program stored in the memory and executable on the processor, wherein the processor implements the steps of the method according to any one of claims 1 to 7 when executing the program.
10. A computer-readable storage medium having a computer program stored thereon, characterized in that: When the program is executed by a processor, the steps of the method described in any one of claims 1 to 7 are implemented.
Citation Information
Patent Citations
Learned model generation method, learned model, surface defect inspection method, steel manufacturing method, pass / fail determination method, grade determination method, surface defect determination program, pass / fail determination program, determination system, and steel manufacturing equipment
CN113260854A
Cold-rolled strip steel surface defect tracing method
CN113732065A
Method for repairing surface defects of hot rolled strip steel
CN113976669A
Indentation defect searching and evaluating method
CN117968614A
Method of manufacturing hot-rolled steel strip
JP2010264472A