Method for accurately inhibiting flying dust on hard road surface
Through drone spraying and image recognition technology, targeted spraying of dust inhibitors solves the problem of dust inhibitors being crushed and damaged when the road traffic is high, improving dust suppression efficiency and effect, and reducing costs.
Patent Information
- Application Number
- CN202410905352.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-08
- Publication Date
- 2024-11-19
AI Technical Summary
In the prior art, chemical dust inhibitors are easily crushed and damaged when the traffic flow on the road surface is large, resulting in a greatly reduced dust suppression effect and duration, and cannot effectively solve the problem of dust on hard road surfaces.
The first dust suppressor spraying and image recognition are used to evaluate the damage level of the area based on the damage of the road surface dust bonding layer, determine the spraying amount of the second dust suppressor, and targeted spraying of the drone to suppress dust by re-spraying To improve the effectiveness of dust-repressing operations.
By accurately identifying and re-spraying dust suppression agents, the efficiency of dust suppression operations is significantly improved, labor, time and cost are reduced, dust suppression effect is extended, and dust suppression effect is improved on hard road surfaces.
Smart Images

Figure CN118979462A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of road dust suppression, and in particular to a method for accurately suppressing dust on a hard road surface. Background Art
[0002] Road dust in construction areas is an important source of dust in the air. To solve the problem of road dust, the commonly used dust suppression methods are artificial watering and chemical dust suppressants. Among them, chemical dust suppressants have gradually been widely studied and applied in recent years due to their high dust suppression efficiency and long duration.
[0003] In the prior art, dust suppression is usually carried out by spraying dust suppressants on the road surface. However, when the traffic volume on the road is large, the dust suppressants are crushed and destroyed by vehicles, which greatly reduces the effect and action time of such dust suppressants. Summary of the invention
[0004] The purpose of the present invention is to solve at least one of the technical problems existing in the prior art. To this end, the present invention proposes a method for accurately suppressing dust on a hard road surface, which can identify the area where road dust occurs in advance to improve the efficiency of road dust suppression.
[0005] According to some embodiments of the present invention, a method for accurately suppressing dust on a hard road surface includes:
[0006] S1: Use drones to spray the first dust suppressant according to the amount of dust on the road;
[0007] S2: After spraying, use drones to take images of the road surface to identify the damage to the dust bonding layer after being rolled over by vehicles, and assess the damage levels of different areas of the road surface based on the damage.
[0008] S3: Determine the spraying amount of the second dust suppressant based on the damage level of the dust bonding layer in different areas of the road surface;
[0009] S4: spray the second dust suppressant on the damaged area of the dust bonding layer;
[0010] S5: Repeat S2 to S4 until the construction project is completed.
[0011] The method for precise dust suppression on hard pavement according to an embodiment of the present invention has at least the following beneficial effects: after the first round of spraying of the first dust suppressant, the road surface image is taken by using a drone to identify the damage of the road surface dust bonding layer after being rolled over by vehicles, and the damage grade of different areas of the road surface is evaluated according to the damage condition. While quickly and accurately identifying the areas where dust suppressants need to be sprayed, the spraying amount of the second dust suppressant in the second round is determined to achieve targeted spraying of dust suppressants, improve the effectiveness of dust suppression operations, thereby greatly improving work efficiency and reducing manpower, time and dust suppression costs.
[0012] According to some embodiments of the present invention, in S1, the first dust suppressant includes a binder and a film-forming agent, the binder is used to increase the adhesion between dust particles, and the film-forming agent is used to protect the dust bonding layer.
[0013] According to some embodiments of the present invention, the binder includes a high-viscosity substance, a surfactant and water, the mass fraction of the high-viscosity substance is 0.2% to 0.5%, and the mass fraction of the surfactant is 0.02% to 0.05%.
[0014] According to some embodiments of the present invention, the film-forming agent includes a film-forming substance and water, and the mass fraction of the film-forming substance is 0.2% to 0.5%.
[0015] According to some embodiments of the present invention, in S1, the binder is evenly sprayed according to the amount of dust on the road surface, and after the road surface is dried, the film-forming agent is evenly sprayed.
[0016] According to some embodiments of the present invention, the calculation formula for the amount of adhesive sprayed per unit area is:
[0017]
[0018] Among them, P1 is the amount of adhesive sprayed per unit area, S is the amount of dust suppressant required per unit weight of dust, and D is the weight of dust per unit area.
[0019] According to some embodiments of the present invention, in S2, identifying the damage condition of the dust bonding layer of the road surface after being crushed by a vehicle includes: collecting dust suppression road surface pictures by image acquisition equipment, enhancing and segmenting the dust suppression road surface pictures, judging the damage rate of the road surface dust bonding layer according to the segmented images, and dividing the images into four levels: level I damage, level II damage, level III damage, and level IV damage.
[0020] According to some embodiments of the present invention, in S2, evaluating the damage level of different areas of the road surface according to the damage conditions includes: using a convolutional neural network to train 4 levels of images, using the trained convolutional neural network to recognize the images transmitted back by the drone, judging and obtaining the local damage level of the dust bonding layer of the photographed road surface, and transmitting the judgment result to the control end.
[0021] According to some embodiments of the present invention, the number of images in the four levels is equal.
[0022] According to some embodiments of the present invention, the convolutional neural network parameters include a medium convolution kernel, a convolution layer, a pooling layer, a Dropout layer and a fully connected layer. The size of the medium convolution kernel is 3×3, the convolution layer is provided with 3 layers, the pooling layer is provided with 1 layer, the Dropout layer is provided with 1 layer, the fully connected layer is provided with 1 layer, and the final output is the prediction result of the local damage level of the dust bonding layer.
[0023] According to some embodiments of the present invention, the second dust suppressant includes a high-viscosity substance, a surfactant and water, the mass fraction of the high-viscosity substance is 0.2% to 0.5%, and the mass fraction of the surfactant is 0.02% to 0.05%.
[0024] According to some embodiments of the present invention, in S4, the spraying amount per unit area of the second dust suppressant is determined by the following formula:
[0025] P2 = A × P1;
[0026] Among them, P2 is the spraying amount of the second dust suppressant per unit area, A is the damaged area rate corresponding to the damage grade, and P1 is the spraying amount of the adhesive per unit area.
[0027] Additional aspects and advantages of the present invention will be given in part in the following description and in part will be obvious from the following description, or will be learned through practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] The present invention is further described below in conjunction with the accompanying drawings and embodiments:
[0029] Figure 1 It is a schematic diagram of a process of a method for accurately suppressing dust on a hard road surface according to an embodiment of the present invention;
[0030] Figure 2 It is a flowchart for identifying the damage of the dust bonding layer of the road surface after being rolled over by vehicles and evaluating the damage level of different areas of the road surface. DETAILED DESCRIPTION
[0031] This section will describe in detail the specific embodiments of the present invention. The preferred embodiments of the present invention are shown in the accompanying drawings. The purpose of the accompanying drawings is to supplement the description of the text part of the specification with graphics, so that people can intuitively and vividly understand each technical feature and the overall technical solution of the present invention, but it cannot be understood as a limitation on the scope of protection of the present invention.
[0032] In the description of the present invention, it should be understood that descriptions involving orientations, such as up, down, front, back, left, right, etc., and orientations or positional relationships indicated are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.
[0033] In the description of the present invention, "several" means one or more, "more" means more than two, "greater than", "less than", "exceed" etc. are understood as not including the number itself, and "above", "below", "within" etc. are understood as including the number itself. If there is a description of "first" or "second", it is only used for the purpose of distinguishing the technical features, and cannot be understood as indicating or implying the relative importance or implicitly indicating the number of the indicated technical features or implicitly indicating the order of the indicated technical features.
[0034] In the description of the present invention, unless otherwise clearly defined, terms such as setting, installing, connecting, etc. should be understood in a broad sense, and technicians in the relevant technical field can reasonably determine the specific meanings of the above terms in the present invention in combination with the specific content of the technical solution.
[0035] refer to Figure 1 to Figure 2 A method for accurately suppressing dust on a hard road surface according to an embodiment of the present invention is described.
[0036] like Figure 1 As shown, the method for accurately suppressing dust on a hard road according to an embodiment of the present invention includes:
[0037] S1: According to the amount of dust on the road surface, the first dust suppressant is sprayed by using a drone. First, the binder is evenly sprayed, and then the film-forming agent is evenly sprayed after the road surface is dry.
[0038] Specifically, the first dust suppressant includes a binder and a film-forming agent, wherein the binder includes a high-viscosity substance, a surfactant and water, the mass fraction of the high-viscosity substance is 0.2% to 0.5%, the mass fraction of the surfactant is 0.02% to 0.05%, the high-viscosity substance in the binder is used to increase the adhesion between dust particles, and the surfactant mainly plays a role in reducing the contact surface tension between the solution and the dust to promote the reaction between the two. The film-forming agent includes a film-forming substance and water, the mass fraction of the film-forming substance is 0.2% to 0.5%, and the film-forming agent mainly plays a role in forming a film to cover the adhesive layer to protect the dust adhesive layer and reduce the rain and wind erosion of the adhesive layer that is not crushed by the vehicle. Compared with traditional dust suppressants, the first dust suppressant in this specific embodiment has a simple preparation process, low cost and high efficiency, can be combined with a smaller capacity drone for fixed-point spraying, and has broad application prospects.
[0039] Specifically, in this specific embodiment, the binder is guar gum, the surfactant is sulfonated oil, and the film-forming substance is sodium alginate.
[0040] It should be noted that, specifically, when a hydrophobic surfactant is added to water, its molecules will gather on the water surface to form a monomolecular film. At this time, the hydrophobic alkane group will face the outside of the water, and the hydrophilic polar group will interact with the water molecules to reduce the surface tension. The hydrophobic group causes the molecules to produce a strong long-range attraction on the surface, partially offsetting the close-range repulsion between molecules, thereby reducing the surface tension; the principle of hydrophilic surfactants is similar, and its molecules will self-assemble into micelle structures in water, with the hydrophobic groups gathering inside the micelles and the hydrophilic groups facing the water phase. This micelle structure can wrap non-polar substances inside, thereby increasing the interfacial area between the liquid and the solid and reducing the interfacial tension.
[0041] Specifically, the calculation formula for the amount of adhesive sprayed per unit area is:
[0042]
[0043] Among them, P1 is the amount of adhesive sprayed per unit area, S is the amount of dust suppressant required per unit weight of dust, and D is the weight of dust per unit area.
[0044] S2: After spraying, use drones to take images of the road surface to identify the damage to the dust bonding layer after being rolled over by vehicles, and assess the damage levels of different areas of the road surface based on the damage.
[0045] Specifically, Figure 2 As shown, dust suppression pavement pictures are collected by image acquisition equipment, wherein the resolution of the pictures is 1 mm / pixel to 5 mm / pixel, and then the dust suppression pavement pictures are enhanced and segmented, and the size of the segmented images is 240 pixels × 240 pixels. The damage rate of the pavement dust bonding layer is judged according to the segmented images, and the images are divided into four levels, namely, level I damage, level II damage, level III damage, and level IV damage, and the number of images of the four levels is equal.
[0046] Specifically, a convolutional neural network is used to train four levels of images. The convolutional neural network parameters include a medium convolution kernel, a convolution layer, a pooling layer, a Dropout layer, and a fully connected layer. The size of the medium convolution kernel is 3×3, there are 3 convolution layers, 1 pooling layer, 1 Dropout layer, and 1 fully connected layer. The output is the prediction result of the local damage level of the dust bonding layer. Finally, the trained convolutional neural network is used to recognize the image transmitted back by the drone to judge the local damage level of the dust bonding layer of the photographed road surface, and the judgment result is transmitted to the control end.
[0047] S3: Determine the spraying amount of the second dust suppressant based on the damage level of the dust bonding layer in different areas of the road surface;
[0048] Specifically, the preparation method of the second dust suppressant is the same as that of the binder. The second dust suppressant is prepared from 0.2% to 0.5% by mass of a high-viscosity substance, 0.02% to 0.05% by mass of a surfactant, and water.
[0049] S4: spray the second dust suppressant on the damaged area of the dust bonding layer;
[0050] Specifically, the spraying amount per unit area of the second dust suppressant is determined by the following formula:
[0051] P2 = A × P1;
[0052] Among them, P2 is the spraying amount of the second dust suppressant per unit area, A is the damaged area rate corresponding to the damage grade, and P1 is the spraying amount of the adhesive per unit area.
[0053] S5: Repeat S2 to S4 until the construction project is completed and no more dust is raised.
[0054] Therefore, after the first round of spraying of the first dust suppressant, the road surface images are taken by drones to identify the damage of the road dust bonding layer after being crushed by vehicles, and the damage level of different areas of the road surface is evaluated according to the damage. While quickly and accurately identifying the areas that need to be sprayed with dust suppressants, the spraying amount of the second dust suppressant in the second round is determined to achieve targeted spraying of dust suppressants, improve the effectiveness of dust suppression operations, thereby greatly improving work efficiency and reducing manpower, time and dust suppression costs.
[0055] The following is a detailed description of the method for accurately suppressing dust on hard pavement using eight specific embodiments.
[0056] The eight specific embodiments were all carried out on the same hard road surface of the construction land, where the hard road surface area was 100m 2 The distance between the areas is 20m, and they do not interfere with each other. The dust volume in each hard road area is controlled at 200g / m 2 On the left and right, the flow of construction vehicles passing through is exactly the same.
[0057] Embodiment 1:
[0058] The components of the binder are 0.1% guar gum, 0.01% sulfonated oil and water;
[0059] The components of the film former are 0.1% sodium alginate and water.
[0060] Prepare two containers with 400L of water, stir the water surface with a stirrer to form a vortex at a stirring rate of 150r / min. According to the mass ratio, slowly add the raw materials of the binder and film-forming agent into the vortexes of the two containers respectively. After complete addition, stir the stirrer deep into the container for 10 minutes at a stirring rate of 50r / min to ensure that the raw materials are completely dissolved, thereby completing the preparation of the binder and film-forming agent.
[0061] In the first stage of the spraying operation, the prepared adhesive is added to the medicine bin of the drone, and the drone is used to evenly spray the adhesive onto the road surface to be constructed at a height of 1m. The spraying amount is calculated by the following formula:
[0062]
[0063] Among them, P1 is the amount of adhesive sprayed per unit area, S is the amount of dust suppressant required per unit weight of dust, and D is the weight of dust per unit area.
[0064] In this embodiment, the spraying amount of the adhesive is 400 ml / m 2 After waiting for 2 hours, the dust on the road surface has been basically bonded. Add the prepared film-forming agent into the drug bin of the drone, and use the drone to spray the film-forming agent evenly on the road surface with the bonding layer at a height of 1m. The spraying amount is 400ml / m 2 After drying, the film-forming agent forms a white film, which can prevent wind and water, prolong the bonding effect, and make it easier to identify the degree of damage to the bonding layer after being run over by a vehicle.
[0065] In the second stage of the spraying operation, when the spraying area had been run over by vehicles for about 300 times, that is, 5 days later, the dust suppression pavement image was collected by image acquisition equipment with a resolution of 3 mm / pixel. The image was then enhanced and segmented. The size of the segmented image was 240 pixels × 240 pixels. According to the damage rate of the pavement dust bonding layer, the image was divided into four levels: level I damage, level II damage, level III damage, and level IV damage. The number of images of the four levels was equal.
[0066] The convolutional neural network is used to train 4 levels of images. The convolutional neural network parameters include a convolution kernel size of 3×3, 3 convolution layers, 1 pooling layer, 1 dropout layer, and a fully connected layer. Finally, the prediction results are output. The trained convolutional neural network is used to identify the images transmitted back by the drone, determine and obtain the damage level of the dust bonding layer of the road surface, and transmit the judgment results to the control end to control the drone to spray the second dust suppressant on the damaged area.
[0067] Specifically, the calculation formula for the spraying amount of the second dust suppressant is:
[0068] P2 = A × P1;
[0069] Among them, P2 is the spraying volume per unit area of the supplementary spraying adhesive, A is the damaged area rate corresponding to the damage grade, and P1 is the spraying volume per unit area of the first spraying adhesive.
[0070] It should be noted that the damage level is defined according to the damaged area of the dust bonding layer in the image, and the corresponding spraying beam of the second dust suppressant is determined. Specifically, the spraying amount corresponding to different damage levels is shown in the following table.
[0071] Damage level Damaged area rate <![CDATA[Spraying volume (ml / m 2 )]]> Level I ≈0% 0 Level II ≈25% 100 Grade III ≈50% 200 Level IV ≈75% 300
[0072] Embodiment 2:
[0073] The components of the binder are 0.2% guar gum, 0.02% sulfonated oil and water;
[0074] The components of the film former are 0.1% sodium alginate and water.
[0075] Prepare two containers with 400L of water, stir the water surface with a stirrer to form a vortex at a stirring rate of 150r / min. According to the mass ratio, slowly add the raw materials of the binder and film-forming agent into the vortexes of the two containers respectively. After complete addition, stir the stirrer deep into the container for 10 minutes at a stirring rate of 50r / min to ensure that the raw materials are completely dissolved, thereby completing the preparation of the binder and film-forming agent.
[0076] In the first stage of the spraying operation, the prepared adhesive is added to the medicine chamber of the drone, and the drone is used to spray the adhesive evenly onto the road surface to be constructed at a height of 1m. The spraying amount of the adhesive is 400ml / m 2 After waiting for 2 hours, the dust on the road surface has been basically bonded. Add the prepared film-forming agent into the drug bin of the drone, and use the drone to spray the film-forming agent evenly on the road surface with the bonding layer at a height of 1m. The spraying amount is 400ml / m 2 .
[0077] In the second stage of the spraying operation, when the spraying area has been rolled over by vehicles for about 300 times, that is, 5 days later, the dust suppression road surface image is collected by image acquisition equipment, and the image resolution is 3mm / pixel. Then the image is enhanced and segmented. The size of the segmented image is 240 pixels × 240 pixels. According to the damage rate of the road dust bonding layer, the image is divided into four levels: level I damage, level II damage, level III damage, and level IV damage. Among them, the number of images of the four levels is equal. The four-level images are trained using a convolutional neural network, and the trained convolutional neural network is used to identify the images transmitted back by the drone, and the damage level of the local dust bonding layer of the road surface is judged and obtained. The judgment result is transmitted to the control end, and the drone is controlled to spray the second dust suppressant on the damaged area.
[0078] Embodiment 3:
[0079] The components of the binder are 0.5% guar gum, 0.05% sulfonated oil and water.
[0080] The components of the film former are 0.1% sodium alginate and water.
[0081] Prepare two containers with 400L of water, stir the water surface with a stirrer to form a vortex at a stirring rate of 150r / min. According to the mass ratio, slowly add the raw materials of the binder and film-forming agent into the vortexes of the two containers respectively. After complete addition, stir the stirrer deep into the container for 10 minutes at a stirring rate of 50r / min to ensure that the raw materials are completely dissolved, thereby completing the preparation of the binder and film-forming agent.
[0082] In the first stage of the spraying operation, the prepared adhesive is added to the medicine chamber of the drone, and the drone is used to spray the adhesive evenly onto the road surface to be constructed at a height of 1m. The spraying amount of the adhesive is 400ml / m 2 After waiting for 2 hours, the dust on the road surface has been basically bonded. Add the prepared film-forming agent into the drug bin of the drone, and use the drone to spray the film-forming agent evenly on the road surface with the bonding layer at a height of 1m. The spraying amount is 400ml / m 2 .
[0083] In the second stage of the spraying operation, when the spraying area has been rolled over by vehicles for about 300 times, that is, 5 days later, the dust suppression road surface image is collected by image acquisition equipment, and the image resolution is 3mm / pixel. Then the image is enhanced and segmented. The size of the segmented image is 240 pixels × 240 pixels. According to the damage rate of the road dust bonding layer, the image is divided into four levels: level I damage, level II damage, level III damage, and level IV damage. Among them, the number of images of the four levels is equal. The four-level images are trained using a convolutional neural network, and the trained convolutional neural network is used to identify the images transmitted back by the drone, and the damage level of the local dust bonding layer of the road surface is judged and obtained. The judgment result is transmitted to the control end, and the drone is controlled to spray the second dust suppressant on the damaged area.
[0084] Embodiment 4:
[0085] The components of the binder are 0.5% guar gum, 0.05% sulfonated oil and water.
[0086] The components of the film former are 0.2% sodium alginate and water.
[0087] Prepare two containers with 400L of water, stir the water surface with a stirrer to form a vortex at a stirring rate of 150r / min. According to the mass ratio, slowly add the raw materials of the binder and film-forming agent into the vortexes of the two containers respectively. After complete addition, stir the stirrer deep into the container for 10 minutes at a stirring rate of 50r / min to ensure that the raw materials are completely dissolved, thereby completing the preparation of the binder and film-forming agent.
[0088] In the first stage of the spraying operation, the prepared adhesive is added to the medicine chamber of the drone, and the drone is used to spray the adhesive evenly onto the road surface to be constructed at a height of 1m. The spraying amount of the adhesive is 400ml / m 2 After waiting for 2 hours, the dust on the road surface has been basically bonded. Add the prepared film-forming agent into the drug bin of the drone, and use the drone to spray the film-forming agent evenly on the road surface with the bonding layer at a height of 1m. The spraying amount is 400ml / m 2 .
[0089] In the second stage of the spraying operation, when the spraying area has been rolled over by vehicles for about 300 times, that is, 5 days later, the dust suppression road surface image is collected by image acquisition equipment, and the image resolution is 3mm / pixel. Then the image is enhanced and segmented. The size of the segmented image is 240 pixels × 240 pixels. According to the damage rate of the road dust bonding layer, the image is divided into four levels: level I damage, level II damage, level III damage, and level IV damage. Among them, the number of images of the four levels is equal. The four-level images are trained using a convolutional neural network, and the trained convolutional neural network is used to identify the images transmitted back by the drone, and the damage level of the local dust bonding layer of the road surface is judged and obtained. The judgment result is transmitted to the control end, and the drone is controlled to spray the second dust suppressant on the damaged area.
[0090] Embodiment 5:
[0091] The components of the binder are 0.5% guar gum, 0.05% sulfonated oil and water.
[0092] The components of the film former are 0.5% sodium alginate and water.
[0093] Prepare two containers with 400L of water, stir the water surface with a stirrer to form a vortex at a stirring rate of 150r / min. According to the mass ratio, slowly add the raw materials of the binder and film-forming agent into the vortexes of the two containers respectively. After complete addition, stir the stirrer deep into the container for 10 minutes at a stirring rate of 50r / min to ensure that the raw materials are completely dissolved, thereby completing the preparation of the binder and film-forming agent.
[0094] In the first stage of the spraying operation, the prepared adhesive is added to the medicine chamber of the drone, and the drone is used to spray the adhesive evenly onto the road surface to be constructed at a height of 1m. The spraying amount of the adhesive is 400ml / m 2 After waiting for 2 hours, the dust on the road surface has been basically bonded. Add the prepared film-forming agent into the drug bin of the drone, and use the drone to spray the film-forming agent evenly on the road surface with the bonding layer at a height of 1m. The spraying amount is 400ml / m 2 .
[0095] In the second stage of the spraying operation, when the spraying area has been rolled over by vehicles for about 300 times, that is, 5 days later, the dust suppression road surface image is collected by image acquisition equipment, and the image resolution is 3mm / pixel. Then the image is enhanced and segmented. The size of the segmented image is 240 pixels × 240 pixels. According to the damage rate of the road dust bonding layer, the image is divided into four levels: level I damage, level II damage, level III damage, and level IV damage. Among them, the number of images of the four levels is equal. The four-level images are trained using a convolutional neural network, and the trained convolutional neural network is used to identify the images transmitted back by the drone, and the damage level of the local dust bonding layer of the road surface is judged and obtained. The judgment result is transmitted to the control end, and the drone is controlled to spray the second dust suppressant on the damaged area.
[0096] Embodiment 6:
[0097] The components of the binder are 0.5% guar gum, 0.05% sulfonated oil and water.
[0098] The components of the film former are 0.5% sodium alginate and water.
[0099] Prepare two containers with 400L of water, stir the water surface with a stirrer to form a vortex at a stirring rate of 150r / min. According to the mass ratio, slowly add the raw materials of the binder and film-forming agent into the vortexes of the two containers respectively. After complete addition, stir the stirrer deep into the container for 10 minutes at a stirring rate of 50r / min to ensure that the raw materials are completely dissolved, thereby completing the preparation of the binder and film-forming agent.
[0100] In the first stage of the spraying operation, the prepared adhesive is added to the medicine chamber of the drone, and the drone is used to spray the adhesive evenly onto the road surface to be constructed at a height of 1m. The spraying amount of the adhesive is 400ml / m 2 After waiting for 2 hours, the dust on the road surface has been basically bonded. Add the prepared film-forming agent into the drug bin of the drone, and use the drone to spray the film-forming agent evenly on the road surface with the bonding layer at a height of 1m. The spraying amount is 400ml / m 2 .
[0101] In the second stage of the spraying operation, when the spraying area has been rolled over by vehicles for about 300 times, that is, 5 days later, the dust suppression road surface image is collected by image acquisition equipment, and the image resolution is 3mm / pixel. Then the image is enhanced and segmented. The size of the segmented image is 240 pixels × 240 pixels. According to the damage rate of the road dust bonding layer, the image is divided into four levels: level I damage, level II damage, level III damage, and level IV damage. Among them, the number of images of the four levels is equal. The four-level images are trained using a convolutional neural network, and the trained convolutional neural network is used to identify the images transmitted back by the drone, and the damage level of the local dust bonding layer of the road surface is judged and obtained. The judgment result is transmitted to the control end, and the drone is controlled to spray the second dust suppressant on the damaged area.
[0102] Embodiment 7:
[0103] The components of the binder are 0.5% guar gum, 0.05% sulfonated oil and water.
[0104] The components of the film former are 0.5% sodium alginate and water.
[0105] Prepare two containers with 400L of water, stir the water surface with a stirrer to form a vortex at a stirring rate of 150r / min. According to the mass ratio, slowly add the raw materials of the binder and film-forming agent into the vortexes of the two containers respectively. After complete addition, stir the stirrer deep into the container for 10 minutes at a stirring rate of 50r / min to ensure that the raw materials are completely dissolved, thereby completing the preparation of the binder and film-forming agent.
[0106] In the first stage of the spraying operation, the prepared adhesive is added to the medicine chamber of the drone, and the drone is used to spray the adhesive evenly onto the road surface to be constructed at a height of 1m. The spraying amount of the adhesive is 400ml / m 2 After waiting for 2 hours, the dust on the road surface has been basically bonded. Add the prepared film-forming agent into the drug bin of the drone, and use the drone to spray the film-forming agent evenly on the road surface with the bonding layer at a height of 1m. The spraying amount is 400ml / m 2 .
[0107] Embodiment 8:
[0108] The components of the binder are 0.5% guar gum, 0.05% sulfonated oil and water.
[0109] Prepare two containers with 400L of water, stir the water surface with a stirrer to form a vortex at a stirring rate of 150r / min. According to the mass ratio, slowly add the raw materials of the binder and film-forming agent into the vortexes of the two containers respectively. After complete addition, stir the stirrer deep into the container for 10 minutes at a stirring rate of 50r / min to ensure that the raw materials are completely dissolved, thereby completing the preparation of the binder and film-forming agent.
[0110] In the first stage of the spraying operation, the prepared adhesive is added to the medicine chamber of the drone, and the drone is used to spray the adhesive evenly onto the road surface to be constructed at a height of 1m. The spraying amount of the adhesive is 400ml / m 2 After waiting for 2 hours, the dust on the road surface has been basically bonded. Add the prepared film-forming agent into the drug bin of the drone, and use the drone to spray the film-forming agent evenly on the road surface with the bonding layer at a height of 1m. The spraying amount is 400ml / m 2 .
[0111] Comparative Example 1:
[0112] The sprayed reagents in Examples 1 to 5 were replaced with an equal amount of water.
[0113] In the first stage of the spraying operation, water is added to the medicine tank of the drone, and the drone is used to spray the adhesive evenly on the road surface to be constructed at a height of 1m. After waiting for 2 hours, water is added to the medicine tank of the drone, and the drone is used to spray the water evenly on the road surface with the adhesive layer at a height of 1m. The spraying amount is 400ml / m 2 .
[0114] In the second stage of the spraying operation, when the spraying area has been rolled over by vehicles for about 300 times, that is, after 5 days, the dust suppression road surface image is collected by image acquisition equipment, and the image resolution is 3mm / pixel. Then the image is enhanced and segmented. The size of the segmented image is 240 pixels × 240 pixels. According to the damage rate of the road dust bonding layer, the image is divided into four levels: level I damage, level II damage, level III damage, and level IV damage. Among them, the number of images of the four levels is equal. The four-level images are trained using a convolutional neural network, and the trained convolutional neural network is used to identify the images transmitted back by the drone, judge and obtain the damage level of the local dust bonding layer of the road surface, and transmit the judgment result to the control end to control the drone to spray water on the damaged area.
[0115] Comparative Example 2:
[0116] Do not spray any material.
[0117] After the first stage of spraying operation was completed in Examples 1 to 5 and Comparative Examples 1 to 2, the dust concentration in the air at a height of 1 m from the ground was continuously tested when the same vehicle passed through different test areas. The results are shown in the following table.
[0118]
[0119] It can be seen from the data in the table that the application of the dust suppressant combination and the spraying method provided by the present invention can significantly reduce the dust concentration of the hard road surface in the construction land, and when the components of the binder are 0.5% guar gum, 0.05% sulfonated oil and water, and the components of the film-forming agent are 0.5% sodium alginate and water, the dust suppression effect is more obvious and can be maintained for more than 15 days.
[0120] After the first stage of the spraying operation in Examples 6 to 7 was completed, the dust concentration in the air at a height of 1 m from the ground was continuously tested when the same vehicle passed through different test areas.
[0121]
[0122] It can be seen from the data in the table that the road dust suppression methods of Examples 6 and 7 can reduce the dust concentration after the vehicle passes by by about 80% within the first 5 days, compared with Comparative Example 2 which does not take any measures. After 5 days, since Example 6 sprayed the damaged area of the dust bonding layer, the dust concentration from 5 to 10 days did not increase significantly, and on the 15th day, the dust concentration could still be reduced by 57%. On the 15th day, the spraying operations of Examples 7 and 8 were almost completely ineffective, while Comparative Example 1 which sprayed water at the same time almost completely failed after the first day. Therefore, the dust suppression methods in Examples 6 to 8 are significantly better than dust suppression by sprinkling water, and the dust suppression method in Example 6 has the best effect.
[0123] The embodiments of the present invention are described in detail above with reference to the accompanying drawings, but the present invention is not limited to the above embodiments, and various changes can be made within the knowledge scope of ordinary technicians in the technical field without departing from the purpose of the present invention.
Claims
1. A method for accurately suppressing dust on hard roads. It is characterized in that include: S1: Use drones to spray the first dust suppressant according to the amount of dust on the road; S2: After spraying, use drones to take images of the road surface to identify the damage to the dust bonding layer after being rolled over by vehicles, and assess the damage levels of different areas of the road surface based on the damage. S3: Determine the spraying amount of the second dust suppressant based on the damage level of the dust bonding layer in different areas of the road surface; S4: spray the second dust suppressant on the damaged area of the dust bonding layer; S5: Repeat S2 to S4 until the construction project is completed.
2. The method for accurately suppressing dust on hard roads according to claim 1, It is characterized in that In S1, the first dust suppressant includes a binder and a film-forming agent, wherein the binder is used to increase the adhesion between dust particles, and the film-forming agent is used to protect the dust bonding layer.
3. The method for accurately suppressing dust on hard roads according to claim 2, It is characterized in that The binder comprises a high-viscosity substance, a surfactant and water. The mass fraction of the high-viscosity substance is 0.2% to 0.5%, and the mass fraction of the surfactant is 0.02% to 0.05%.
4. The method for accurately suppressing dust on hard road surface according to claim 2, It is characterized in that The film-forming agent comprises a film-forming substance and water, and the mass fraction of the film-forming substance is 0.2% to 0.5%.
5. The method for accurately suppressing dust on hard road surface according to claim 2, It is characterized in that In S1, the binder is evenly sprayed according to the amount of dust on the road surface, and after the road surface is dried, the film-forming agent is evenly sprayed.
6. The method for accurately suppressing dust on hard road surface according to claim 2, It is characterized in that The calculation formula for the amount of adhesive sprayed per unit area is: Among them, P 1 is the amount of adhesive sprayed per unit area, S is the amount of dust suppressant required per unit weight of dust, and D is the weight of dust per unit area.
7. The method for accurately suppressing dust on hard road surface according to claim 1, It is characterized in that In S2, the damage of the dust bonding layer of the road surface after being rolled by the vehicle is identified, including: The dust suppression pavement pictures are collected by image acquisition equipment, enhanced and segmented, and the damage rate of the pavement dust bonding layer is judged according to the segmented images. The images are divided into four levels: level I damage, level II damage, level III damage, and level IV damage.
8. The method for accurately suppressing dust on hard road surface according to claim 1, It is characterized in that In S2, the damage levels of different areas of the road surface are evaluated according to the damage conditions, including: The convolutional neural network is used to train 4 levels of images. The trained convolutional neural network is used to recognize the images transmitted back by the drone, judge and obtain the local damage level of the dust bonding layer of the photographed road surface, and transmit the judgment result to the control end.
9. The method for accurately suppressing dust on hard road surface according to claim 7, It is characterized in that The number of images in the four levels is equal.
10. The method for accurately suppressing dust on hard road surface according to claim 7, It is characterized in that The convolutional neural network parameters include medium convolution kernel, convolution layer, pooling layer, Dropout layer and fully connected layer. The size of the medium convolution kernel is 3×3, there are 3 convolution layers, 1 pooling layer, 1 Dropout layer, and 1 fully connected layer. The final output is the prediction result of the local damage level of the dust bonding layer.
11. The method for accurately suppressing dust on hard road surface according to claim 1, It is characterized in that The second dust suppressant comprises a high-viscosity substance, a surfactant and water. The mass fraction of the high-viscosity substance is 0.2% to 0.5%, and the mass fraction of the surfactant is 0.02% to 0.05%.
12. The method for accurately suppressing dust on hard road surface according to claim 1, It is characterized in that In S4, the spraying amount per unit area of the second dust suppressant is determined by the following formula: P 2 =A×P 1 ; Among them, P 2 is the spraying amount per unit area of the second dust suppressant, A is the damaged area rate corresponding to the damage grade, P 1 It is the amount of adhesive sprayed per unit area.