Method for laser cutting large-size glass plate and implementation device thereof

By using low-pressure polyethylene materials as substrate and pulsed laser cutting technology, the problems of low cutting accuracy, slow speed and poor safety of large-sized glass plates are solved, and high-precision and high-speed laser cutting is achieved, avoiding toxic gases and debris The multi-layer and suspended glass plate were successfully cut.

CN118984753APending Publication Date: 2024-11-19OBSHCHESTVO S OGRANICHENNOJ OTVETSTVENNOSTJU NAUCHNO TEKHNICHESKOE OB EDINENIE IRE POLUS (OOO NTO IRE POLUS)

Patent Information

Application Number
CN202380027011.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-09-01
Filing Date
2023-05-31
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

The prior art has problems such as low accuracy, slow speed, poor safety, and toxic gases and glass debris when cutting large-sized glass plates, and it is especially difficult to cut multi-layer glass and suspended glass plates.

Method used

Low-pressure polyethylene material is used as the table substrate, combined with pulsed laser cutting technology, cutting by creating fracture stress edges inside the glass and cutting in the suspended state of the glass, reducing the impact of laser radiation on the substrate.

Benefits of technology

It improves the accuracy and speed of the cutting line, ensures the safety of the cutting process, avoids the generation of toxic gases and glass debris, and can cut multi-layer glass and suspended glass plates, reducing the impact of laser radiation on the workbench.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118984753A_ABST
    Figure CN118984753A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of laser engineering and glass cutting. The glass is cut using obliquely focused radiation of the pulsed laser. The multi-layer glass is cut in this manner. The glass plate is flatly placed on the workbench base plate or suspended on the air cushion above the workbench base plate, and the base plate is made of high-density polyethylene (0.94-0.96 g / cm < 3 >). The glass cutting device has the technical effects that the precision of a cutting line is improved, the cutting speed is increased, toxic gas and glass dust are avoided, multiple layers of glass can be cut, and the service life of a substrate is prolonged under the condition that a plate is suspended.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of laser engineering, in particular to a method and an apparatus for cutting glass sheets by means of pulsed laser. Background Art

[0002] It is necessary to clarify some concepts within the scope of this invention description.

[0003] Concept of "thick glass sheet". It is obvious that a glass sheet has the length, width and thickness of the sheet. The thickness of a glass sheet is usually much smaller than the length and width of a Jumbo type sheet (6000×3210 mm), and this thickness can be compared to the depth of the defect produced by a single pass of the laser beam along the cutting line. For example, if the depth of the defect produced by a single pass of the laser is 10 mm, then glass with a thickness between 11 and 20 mm can be considered as a "thick glass sheet". Therefore, in the original claim 1 and the specification, the glass thickness is compared with this depth value. If the thickness of the glass exceeds the depth of the defect produced by a single pass of the laser along the cutting line, the glass is defined as a "thick glass sheet" in the specification, and multiple laser treatments along the cutting line are required during the cutting process to gradually increase the defect depth from bottom to top. First, the laser treatment is performed at the bottom of the glass along the cutting line, and then the laser beam is raised to produce new defects on the cutting line again, and the process is repeated until the entire thickness of the glass is filled from bottom to top along the cutting line. The concept of "thick glass sheet" applies only within the framework of this specification and cannot be extended to other everyday situations. Its purpose is to point out the conditions under which cutting of such glass requires multiple laser treatments along the cutting line: each laser treatment is performed on top of the previous defect in order to gradually fill the defect area up to the top of the glass.

[0004] The concept of "multi-layered glass". The National Standard (GOST) R 51136-2008 "Multi-layered protective glass. General specifications". It implies that multi-layered glass means that the glass sheet can be regarded as consisting of multiple uniform layers in thickness. The multi-layer structure can be achieved by, for example, sintering two or more sheets of glass or bonding them with polymer glue or film. This is the manufacturing method of so-called laminated automotive glass (two layers of glass and a polymer film layer sandwiched between them). Interlayer ( https: / / ru.wikipedia.org / wiki / Τриплекс ) (derived from the Latin triplex, meaning "triple") is a type of multi-layer glass (two or more layers of organic or silicate glass bonded together by a special polymer film or light curing agent that can hold glass fragments when hit). Usually, this type of glass is manufactured by heating and pressing. Fire-resistant glass and tempered glass also belong to the category of multi-layer glass.

[0005] The concept of polyethylene is defined as follows:

[0006] National Standard (GOST) 16337-2022 "High-Pressure Polyethylene" P.4.1. Polyethylene and its compositions are classified as low-hazard substances according to the degree of impact on the human body (according to the National Standard (GOST) 12.1.007, they belong to the 4th category of hazard).

[0007] National Standard (GOST) 16338-85 "Low-pressure polyethylene. Specifications".

[0008] 3.2. Polyethylene of basic grade and composition will not release toxic substances into the environment at room temperature and will not have any effect on the human body when in direct contact with it. No special protective measures are required when using it.

[0009] The concept of penolon (polyethylene foam)

[0010] National Standard (GOST) R 58955-2020 "Factory-made polyethylene foam products for buildings and structures. General specifications".

[0011] Polyethylene Foam (PEF): Semi-rigid or flexible thermal insulation material based on ethylene-derived polymers or ethylene and / or propylene-derived polymers.

[0012] [National Standard (GOST) 56729-2015*, Article 3.1.1]

[0013] 3.1.1.1 Non-cross-linked polyethylene foam (NPE): Polyethylene foam manufactured using gas foaming technology (using various hydrocarbons, carbon dioxide, nitrogen), and then replacing the gas produced during the foaming process with air.

[0014] 3.1.1.2 Physically cross-linked polyethylene foam (IXPE): Polyethylene foam with a cross-linked molecular structure formed by the physical action of electrons and foamed using a special foaming agent.

[0015] 3.1.1.3 Chemically cross-linked polyethylene foam (XPE): Polyethylene foam with a cross-linked molecular structure formed by chemical means and foamed using a special foaming agent.

[0016] Existing methods for cutting brittle transparent materials, in particular industrial glass, are based on laser-induced breakdown and the formation of defect tracks in the material when it is subjected to focused laser radiation. In this process, special attention should be paid not only to the breakdown effect, but also to the fact that the substrate material on which the transparent material is located (because it is exposed to the laser radiation in one way or another) should not interfere with the main process. The structure used as a workbench usually uses metal brushes or metal plates to support the material to be cut, or a soft porous substrate that can strongly scatter the laser radiation. However, the metal substrate under the glass not only damages the glass surface by staining it with metal melting products, but also pollutes the atmosphere due to the combustion products released (including nitrogen compounds), not to mention the difficulty of leveling such substrates. The soft substrate will deform and may not be able to withstand the impact of laser radiation, while the volatile fractions formed by laser radiation will be deposited on the lower surface of the glass, which is unacceptable in the manufacturing process.

[0017] The known patent RU 2720791 C1 proposes a method for cutting brittle materials (e.g. glass sheets that are transparent to laser radiation and have low absorption), by which the cutting of the glass sheet is achieved by means of an almost continuous stress edge formed on the cross section of the glass sheet by the laser-induced breakdown of the material ( Figure 1 , an overall view of the laser head 100). The stress edge 1 for cutting is formed by a material transparent to laser radiation, such as a glass plate 2, and during the process of oblique scanning by the laser beam 3, when the cross section of the material is irradiated with a focused laser beam of a fixed focal length while moving longitudinally along the glass surface, the cross section of the material is locally induced to form a cavity track by the laser beam. Wherein:

[0018] - a single laser beam 3 is scanned through the material to form a substantially linear and narrowly spaced oblique chain 4, from one side of the plate to the other, with each pulse forming at least one cavity; and

[0019] - The next chain of cavities with a narrower spacing is formed during another scanning pass of the beam as a result of the relative longitudinal movement of the laser beam and the glass sheet.

[0020] At the end of this progressive longitudinal movement and oblique periodic scanning in the same plane as the beam, a substantially continuous optically induced cavity in the form of an internal bubble stress edge 1 is obtained, along which the glass sheet is cut without chipping defects at the end of the process of longitudinal movement of the beam along its surface. The device for forming the stress edge on a given plane of the body of transparent material for subsequent cutting according to the above method is of vital importance and comprises a pulsed laser radiation source 5, which can be a solid-state laser or a fiber laser, equipped with a collimator 6, after which the beam impinges on a deflection system 7. This ensures a periodic scanning of the beam from one glass surface to the other opposite glass surface (the direction does not matter - either forward or reverse). The focusing of the beam is achieved by an optical focusing system 8, the focus setting remaining unchanged throughout the entire process. At the same time, the laser beam impinges on the surface at an acute angle. When forming the stress edge, the angle of incidence of the beam relative to the surface normal can be less than 60 degrees in an orthogonal plane (for forming a straight cut) or at a maximum angle of 45 degrees to the normal on any inclined plane (for forming an oblique cut, i.e. a bevel cut, with increased reflection losses at larger angles), i.e. the angle of the inclined plane, i.e. the angle of the cutting plane, is between 45 and 90 degrees relative to the glass surface and is set by a system capable of adjusting the direction of the beam relative to the glass surface in the coordinate space (along the three spatial axes 9, i.e. the X-axis, the Y-axis and the Z-axis). The gradual longitudinal movement of the laser beam 3 along the glass surface is ensured by a drive device 10, which ensures its progressive unidirectional movement along the X-axis and is carried out on a fixed glass plate in front of the area where the stress edge is formed. Although it is claimed that the method is insensitive to the direction in which the beam moves from the upper or lower surface of the glass, this is not the case in reality. When the beam moves from the upper side of the glass to the lower side, during the formation of the defect on the lower side, a partial radiation scattering is observed at the upper defect. In addition, when breakdown occurs on the underside, it is unclear how the table substrate affects the glass surface, since decomposition products and combustion products may be deposited on the glass surface. Therefore, this method still has shortcomings when used for industrial large-size glass plate cutting.

[0021] Utility model RU 130308U1 for industrial cutting of glass: A workbench for processing transparent non-metallic materials by laser radiation, comprising a work surface, on which at least one coating for positioning the material to be processed is arranged, wherein the at least one coating is made of a material transparent to laser radiation in the wavelength range of 300 to 3000 nanometers, and the material is an elastic flexible foam material with a closed-cell structure and a density of 20 to 200 kg / m3; the material is a Penolon material with a thickness of 1 to 50 mm. The at least one coating material is transparent to pulsed laser radiation in the wavelength range of 1030 to 1120 nanometers (preferably 1070 nanometers), wherein the elastic flexible foam material is made by physical or chemical crosslinking, and the at least one coating material is transparent to pulsed laser radiation in the wavelength range of 1030 to 1120 nanometers (preferably 1070 nanometers). However, the disadvantage of the method and device for cutting using Penolon material is that the material will deform when bearing the weight of a large piece of glass, resulting in deviations. More importantly, the material cannot withstand the pulse radiation of a picosecond laser with a central wavelength of 1.03 to 1.06 microns, a power of 50 to 200 watts, and a pulse energy range of 40 to 200 microjoules. Since the workbench made of the Penolon material is provided with holes for forming an air cushion when moving the glass, the deformation and wear of the Penolon material will change the pressure distribution of the air cushion under the glass, which makes the operation of the workbench using this coating more complicated. The above disadvantages are eliminated in the method and device for industrial laser cutting of Jumbo type industrial glass plates (the word Jumbo comes from the English word "huge", and the internationally recognized glass plate size is 6000x3210 mm) and other size workpieces (up to 12000x3210 mm) proposed in this application. Summary of the invention

[0022] The purpose of the present invention is to develop a method for laser cutting of large-sized industrial glass sheets and an apparatus for its implementation. Its technical effects include improving the accuracy of the cutting line, improving the speed and safety of the cutting process, avoiding the generation of toxic gases due to glass dust and substrate decomposition, being able to cut multiple layers of glass (including laminated glass), and reducing the impact of laser radiation on the workbench substrate when the glass sheet is suspended during the cutting process. If the substrate in the form of polyethylene evaporates accidentally, the hazard is comparable to burning a paraffin candle, no toxic emissions are generated and no nitrogen compounds are formed. Compared with mechanical cutting, the laser cutting process does not produce glass debris and dust, which often occur during mechanical cutting and are highly dangerous.

[0023] Demonstration of technical effect

[0024] 1. Improve the accuracy of cutting line.

[0025] Conventionally, large-size Jumbo-type glass sheets are cut on a table by double-sided scoring. First (and only along a straight line) a score is made on one side with a diamond or carbide cutting tool, then it is turned over and the scoring process is repeated with an attempt to align the back side. In the best case, the accuracy of this alignment is 1 to 2 mm and requires additional machining of the end faces after mechanically splitting the glass along the score line, which is far inferior to the technology for laser cutting of Jumbo-type glass sheets (especially multi-layer glass) that we have proposed and realized for the first time. This technology uses focused laser radiation to cut along a line with an accuracy of about 50 microns, which is determined by the size of the focused beam, as is known.

[0026] 2. Increase cutting speed.

[0027] Laser cutting of Jumbo-type glass sheets is an order of magnitude faster than cutting with conventional techniques and does not require the sheet to be flipped over or re-scored to align with the cut line on the other side.

[0028] 3. Ensure the safety of the cutting process without toxic gases, glass chips and dust generated by the decomposition of substrate materials.

[0029] The effects of laser radiation from a picosecond fiber laser with a central wavelength of 1.03 to 1.06 micrometers, a power of 50 to 200 watts and a pulse energy between 40 and 200 microjoules on different substrate materials were investigated.

[0030] The results of the study showed that the materials used in the conventional industry for substrates of glass panels do not meet the required safety requirements. Such materials include:

[0031] - Metal brushes (burn and spatter under laser radiation, forming nitrogen compounds similar to arc welding);

[0032] -Getinax, glass fiber, fluoroplastics, woven materials (including high temperature resistant materials), plastics, polymer materials, Penolon, polystyrene (releasing a lot of smoke, toxic components, formaldehyde, acetaldehyde, organic acids, etc. when burning). The smoke produced by incomplete combustion enhances the absorption of laser radiation, which not only accelerates the wear of the substrate, but also pollutes the surface of the board, which is unacceptable.

[0033] During the laser cutting process, no glass fragments are left on the work table and the work area is not clogged with debris.

[0034] 4. Ability to cut multiple layers of glass.

[0035] For the first time in the world, cutting of Jumbo-type glass sheets, both single-layer and multi-layer, was achieved. Multi-layer glass, such as laminated glass, fire-resistant glass and tempered glass, was cut for the first time. For the cutting of multi-layer glass, such as laminated glass, it is done in two steps along the cutting line. First, the lower glass single layer is cut using a focused laser beam while moving from the lower surface to the upper surface while gradually moving along the cutting line. Then, the process is repeated for the upper glass (laminated glass consists of two layers of glass bonded together by a polymer layer). Tempered glass and fire-resistant glass are cut in the same way.

[0036] 5. Reduce the impact of laser radiation on the workbench substrate during suspended cutting of glass plates.

[0037] There are no similar suspended glass cutting solutions. We have achieved the cutting of suspended Jumbo-type glass sheets for the first time. The closest prior art is a prototype of laser cutting glass sheets in contact with Penolon material as substrate, which has a very low thermal conductivity of 0.03 to 0.04 W / (m·Kelvin). This material tends to melt and burn, generating smoke, when in close contact with glass and exposed to laser radiation. Low-pressure high-density polyethylene, on the other hand, is able to withstand the radiation of picosecond lasers even when in contact with glass and does not release smoke, especially when the sheet is floating. This is because an air gap is formed between the glass and the substrate, the scattering of the laser radiation increases due to the low refractive index of the air and the expansion of the laser beam, which is concentrated on the glass instead of the space behind the glass, the radiation power density is reduced, and the laser thermal radiation received by the substrate surface is also reduced accordingly. At the same time, due to the presence of the air gap, the heat conduction of the glass is also eliminated. It is worth noting that compared with other types of polyethylene, low-pressure polyethylene, due to its higher density, shows the best effect in the combination of various properties.

[0038] The present invention proposes a method for laser cutting a large-size transparent glass plate, which is to create a fracture stress edge in the form of a defective structure area along the cutting line and throughout the entire thickness of the glass inside the glass, wherein the defective structure area is formed due to local laser-induced breakdown when the glass is exposed to focused pulsed laser radiation in the form of an inclined beam, and is characterized in that the defective structure is created by cutting at least once in a glass plate including at least one layer of glass in the direction from the lower surface to the upper surface and along the cutting line. In the cutting process, the glass plate can be directly placed flat on a workbench substrate, or suspended on an air cushion above the workbench substrate in a suspended state. In addition, a substrate is used, the top layer of which is made of low-pressure polyethylene, and when the defective structure area is created on the lower surface of the glass, the top layer of the substrate can resist the impact of scattered laser radiation passing through the thickness of the glass.

[0039] A device for implementing the above method is also proposed, which is used for laser cutting a large transparent glass plate parked on a workbench or located above the workbench in a suspended air cushion. The device comprises:

[0040] - a pulsed laser having a control unit and a laser head;

[0041] - an optical scanning device comprising at least one electrically deflectable mirror element in the form of a mirror or a rotatable mirror polyhedron;

[0042] - an optical focusing system at the output of the optical scanning device in the form of an objective lens with a fixed focal length and a focal plane tilted relative to the plane of the plate;

[0043] - a gantry equipped with a coordinate reference system with at least three degrees of freedom in the X, Y and Z axes relative to the glass surface for moving the laser head of the laser;

[0044] - a horizontal table with a base plate and a programmable coordinate drive on a gantry above the table for progressive movement of the laser head within the table and in the vertical direction, the top layer of the table base plate being made of low-pressure polyethylene capable of resisting the impact of scattered laser radiation, while the focused laser radiation penetrates the glass, being deflected from the lower surface to the upper surface of said glass within the aperture of the inclined focal plane of the optical focusing system, the beam creating a fracture stress edge in said glass in a single pass along the cutting line over the thickness of said glass or part of its thickness as a result of the deflection of the beam by said scanning device;

[0045] - Pneumatic air system for creating an air cushion under the suspended glass sheets during loading and unloading, during cutting and moving;

[0046] - a basic support fixture for fixing the position of the glass sheet suspended above the workbench and a vertically retractable support friction mechanism having a workbench sensor for moving the glass sheet during loading and unloading in automatic mode.

[0047] Other advantages and salient features of the present invention will become apparent from the following description of preferred embodiments thereof, which are given with reference to the accompanying drawings, as illustrated below and their brief description. BRIEF DESCRIPTION OF THE DRAWINGS

[0049] Figure 1 It is an overall view of the laser head for cutting glass (closest prior art RU 2720791 C1).

[0050] Figure 2It is an overall view of the cutting process when the glass sheet is suspended above the workbench surface and the glass sheet is loaded or removed using the vertically movable supporting retractable friction mechanism 205.

[0051] Figure 3 It is an overall view of the device used for the suspended glass sheet cutting process. DETAILED DESCRIPTION

[0052] Figure 2 A view of a process 200 of cutting a glass plate 2 suspended on a substrate 202 is shown above a table 201. The plate lies flat (floating) on ​​an air cushion 203, which is ensured by compressed air ejected from holes 204 in the substrate. Glass cutting can be performed when the glass plate lies flat on the substrate or in a suspended state. In the suspended state, the unevenness of the table surface and deformations caused by external climatic conditions have less influence on the cutting, and in some cases, suspension is more ideal than mechanical contact with the substrate. One of the reasons is that when the focused pulsed laser radiation forms a defect area of ​​laser-induced breakdown at the bottom of the glass, the laser radiation effect on the substrate material is reduced due to additional scattering at the glass-air-substrate boundary. Under this action of the laser on the glass, the beam moves upward along the inclined trajectory of the linear defect chain 4, forms a pulse local breakdown when it approaches the upper boundary of the glass, and then along the cutting line, that is, along the displacement of the X axis, the pulse is restored again, starting from the lower boundary of the glass and moving upward without generating radiation scattering on the previous laser breakdown path, because the previous path is located below it.

[0053] It is essential in this method that when cutting thick glass sheets, the fracture stress edge 1 is formed vertically through the entire glass thickness during two or more passes of the laser along the cutting line, compared to the depth of the defect zone formed by the laser moving along the cutting line of the glass. Each time it moves along the cutting line, a new vertical defect layer is created from the lower boundary to the upper boundary of the glass, thus avoiding scattering of the laser radiation on structural defects of the previous layer created by the laser.

[0054] This approach is also important when cutting multiple layer glass panels, especially laminated glass. The fracture stress edge is formed vertically through the entire glass thickness by scanning along the cutting line at least twice, once for each layer of glass, and each time along the cutting line a new vertical defect layer is created from the lower to the upper edge of the glass, thus avoiding scattering of the laser radiation on structural defects of the previous layer created by the laser.

[0055] It is worth noting that in this method, a pulsed picosecond fiber laser is used, which transmits radiation through an optical cable 211 with a maximum length of 25 meters, with a central wavelength of 1.03 to 1.06 microns, a power of 50 to 200 watts, and a pulse energy in the range of 40 to 200 microjoules, wherein the top layer of the substrate is a high-density (0.94 to 0.96 g / cm 3 ) low-pressure polyethylene material.

[0056] In this method, the use of pulsed nanosecond, picosecond or femtosecond solid-state lasers, including disk or fiber lasers, is crucial. The use of gas lasers is not recommended due to their suboptimal technical and economic performance.

[0057] Figure 3 An apparatus for implementing the method is shown: for cutting a large transparent glass plate 2 parked on a workbench 201, on a substrate 202 of the workbench or above the workbench in a suspended state on an air cushion 203, the apparatus comprising:

[0058] - a pulsed laser with a control unit 206 and a laser head 100;

[0059] - scanning optics 7, comprising at least one electrically deflectable mirror element in the form of a mirror or a rotatable mirror polyhedron;

[0060] - an optical focusing system 8 at the output of the scanning optics 7 in the form of an objective lens with fixed focal length and tilted focal plane relative to the plane of the plate;

[0061] - a gantry 210, a coordinate reference system with at least three degrees of freedom in the three axes X, Y and Z 9 relative to the glass surface, for moving the laser head of the laser;

[0062] - a horizontal table 201 with a base plate 202 and a programmable coordinate drive on a gantry 210 located above the table, the programmable coordinate drive being used for the progressive movement of the laser head 100 in the table and in the vertical direction, the top layer of the table base plate 202 being made of low-pressure polyethylene capable of resisting the impact of scattered laser radiation, while the focused laser radiation penetrates the glass and is deflected from the lower surface of the glass to the upper surface within the aperture of the inclined focal plane of the optical focusing system, and as a result of the deflection of the beam by the scanning device, the laser beam is swept along the cutting line in a single pass over the thickness of the glass or part of the thickness thereof to create a fracture stress edge 1 in the glass;

[0063] - a pneumatic air system 207 for creating an air cushion 203 under the suspended glass sheet during loading and unloading, during cutting and moving;

[0064] - Basic support fixtures 203, 209 for fixing the position of the glass sheet when it is suspended above the table, and a vertically retractable support friction mechanism 205 with table sensor for moving the sheet when loading and unloading in automatic mode.

[0065] The device is capable of not only straight vertical glass cutting, but also curved, rounded and inclined glass cutting. When performing bevel cutting, the coordinate drive has rotational freedom.

[0066] Importantly, in the device, the top layer of the substrate is formed in the form of a set of spacers, which can be in the form of squares, rectangles, diamonds or polyhedrons, with an average slope error within a base length of 6 meters, not exceeding 300 microns in the horizontal direction and 150 microns in the vertical direction at the joints of adjacent spacers. These spacers contain at least one hole for supplying compressed air from a pneumatic air system to create a suspended state of the plate under the glass by air cushion when cutting or moving the glass along the surface of the substrate during the loading / unloading phase. A high-density (0.94 to 0.96 g / cm 3 ) low-pressure polyethylene material, polyethylene can be provided in the form of film or block material.

[0067] Notably, the pulsed picosecond fiber laser used in the device delivers radiation through fiber optic cables up to 25 meters long, has a central wavelength of 1.03 to 1.06 microns, a power of 50 to 200 watts, and a pulse energy range of 40 to 200 microjoules.

[0068] Importantly, pulsed nanosecond, picosecond or femtosecond solid-state lasers, including disk or fiber lasers, are used in the device.

[0069] It is obvious to those skilled in the art that the present invention is not limited to the above-described embodiments and can be modified within the scope of the claims set forth. If necessary, the distinguishing features set forth in this specification and other distinguishing features can also be used alone.

[0070] The invention was tested when cutting large-size monolithic industrial glass (dimensions of 6000×3210 mm, thickness of 2 to 20 mm) and cutting multilayer glass with 3 to 7 layers (total workpiece thickness up to 25 mm, including laminated glass). The tests were conducted using a picosecond ytterbium fiber laser YLPP-100-10-100-R-GP (OOO "NTO IRE-Polus", https: / / www.ipgphotonics.com / ru) with a pulse duration of 10 to 20 picoseconds, a pulse energy of up to 100 microjoules, and a repetition rate of up to 4 MHz. For cutting 20 mm thick glass, a scanning system based on an IPG 2D MidPower motorized scanner, a focusing system based on a 100 mm F-theta lens, and a longitudinal movement speed of up to 160 mm / s were used.

[0071] Example Embodiments of the Invention

[0072] To test the method of cutting thin sheet glass (in the form of Jumbo glass) on a bench and when the glass is suspended above the bench, both bench and cutting techniques were tested. Low-pressure polyethylene (high density 0.94 to 0.96 g / cm 3 ) was chosen as substrate material due to its good tolerance to the chosen radiation mode, its widespread use in industry and the corresponding low cost. Other types of polyethylene show poor tolerance to laser radiation. Picosecond fiber lasers with a central wavelength of 1.03 to 1.06 μm, a power of 50 to 200 W and a pulse energy in the range of 40 to 200 μJ were used. A scanning system based on an IPG 2D MidPower motorized scanner, a focusing system based on a 100 mm F-theta lens, and a longitudinal movement speed of up to 160 mm / s (for cutting 20 mm thick glass) and 600 mm / s for 2 mm thick single-layer glass were used. Such a polyethylene substrate can last for 1 year in a mode where the sheet is flat on the substrate and is operated for 7 hours per day. The durability in the suspended mode is not yet limited, which significantly exceeds 1 year.

[0073] The device for cutting glass includes:

[0074] - a pulsed laser having a control unit and a laser head;

[0075] - scanning optics comprising an electrically deflectable mirror element in the form of a mirror (the alternative embodiment of a rotatable mirror polyhedron was also tested) irradiated at the laser wavelength;

[0076] - an optical focusing system based on a 100 mm F-theta lens, located at the output of the scanning optics, in the form of an objective lens with a fixed focal length of 250 mm and an inclined focal plane relative to the plate plane;

[0077] - a gantry equipped with a coordinate reference system with three degrees of freedom in the X, Y and Z axes relative to the glass surface, used to move the laser head of the laser within the table with an accuracy of 100 to 200 microns;

[0078] - a horizontal table with a base plate and a programmable coordinate drive on a gantry located above the table, the programmable coordinate drive being used for the progressive movement of the laser head inside the table and in the vertical direction, the top layer of the table base plate being made of low-pressure polyethylene capable of resisting the impact of scattered laser radiation, while the focused laser radiation penetrates the glass, the beam being deflected from the lower surface of the glass to the upper surface within the aperture of the inclined focal plane of the optical focusing system under the deflection action of the scanning device, the laser beam being swept along the cutting line in a single pass over the thickness of the glass or part of the thickness thereof to create a fracture stress edge in the glass;

[0079] - Pneumatic air system for creating an air cushion under the suspended glass sheet during loading and unloading, during cutting and moving, with compressed air line pressure of 6 to 10 bar;

[0080] - A basic support fixture for fixing the position of the glass sheet when it is suspended above the table, and a vertically retractable support friction mechanism with table sensor for moving the sheet when loading and unloading in automatic mode.

[0081] The top layer of the substrate is in the form of a set of rectangular spacers with dimensions of 500 × 1500 mm and a thickness of 10 mm, with an average slope error within a base length of 6 meters, not exceeding 300 microns in the horizontal direction and 150 microns in the vertical direction at the joints of adjacent spacers. These spacers have at least one hole with a diameter of 5 mm for supplying compressed air from a pneumatic air system to create a suspended state of the plate due to an air cushion with a gap of 150 to 200 microns under the glass when cutting or moving the glass along the substrate surface during the loading / unloading phase. The top layer of the workbench substrate uses a high-density (0.94 to 0.96 g / cm 3 ) low-pressure polyethylene. Density is 0.95g / cm 3 The manufacturer of low-pressure polyethylene, with the trademark PE-500, is as follows: Simona, Germany, Teichweg 16, D-55606 Kirn; in Russia, the manufacturer is OOO "Firma Elmika" located in Rostov-on-Don.

[0082] Glass cutting tests were conducted with pulsed nanosecond and femtosecond solid-state lasers, however, the best results were achieved with picosecond fiber lasers with respect to a set of parameters, as mentioned above. It is noteworthy that the glass type, whether monolithic or multilayer, was cut in a single pass along the cutting line over the entire thickness. However, for multilayer glass, the best quality results were obtained when cutting each layer in a single pass. This is because there is a polymer film between the glass layers, which affects the quality of cutting in a single pass over the entire thickness, and the best results were achieved when cutting each layer one by one along the cutting line. The cutting line can be either straight or curved. We note that in the closest prior art RU 2720791 C1, monolayer glass was cut in a single pass, but for the first time we have successfully cut large-sized Jumbo-type glass, especially multilayer glass.

[0083] The table below shows the main cutting characteristics of multilayer glass (laminated). Glass grades are indicated according to international standards, national standard (GOST) 30826-2014, company standard (STO) 11765852-07-02021, glass manufacturer is OOO "AG C Flat Glass Klin", Klin, Russian Federation.

[0084] sheet

[0085]

[0086] The multi-layer Jumbo-type glass cutting technology based on the above-mentioned method and implemented in an apparatus for cutting multi-layer glass (including laminated glass, tempered glass and fire-resistant glass) has been described on our 2022 website "https: / / www.ipgphotonics.com / ru / news#fkompaniya-ipg-v-novostyakh" and was demonstrated for the first time at the GLASSTEC-22 international exhibition in Düsseldorf, Germany, from September 20 to 23, 2022.

Claims

1. A method for laser cutting of large transparent glass sheets by creating a fracture stress edge inside the glass in the form of a defective structural region along the cutting line and throughout the entire thickness of the glass, said defective structural region being formed due to localized laser induced breakdown when the glass is exposed to focused pulsed laser radiation in the form of an inclined beam, characterized in that: The invention relates to a method for creating a defect structure in a glass including at least one layer of glass by making at least one cut along the direction from the lower surface to the upper surface of the glass plate and along the cutting line, wherein during the cutting process, the glass plate is directly placed flat on a workbench substrate or is suspended on an air cushion above the workbench substrate, and wherein a substrate is used, the top layer of which is made of low-pressure polyethylene, and when the defect structure area is generated on the lower surface of the glass, the top layer of the substrate can resist the impact of scattered laser radiation passing through the thickness of the glass.

2. The method according to claim 1, wherein: A pulsed picosecond fiber laser was used, which transmitted radiation via an optical fiber as long as 25 meters. The central wavelength of the pulsed picosecond fiber laser was 1.03 to 1.06 microns, the power was 50 to 200 watts, the pulse energy range was 40 to 200 microjoules, and low-pressure polyethylene with a density of 0.94 to 0.96 g / cm3 that was resistant to scattered laser radiation impact was used as the top layer of the substrate.

3. The method according to claim 1, wherein: Pulsed nanosecond, picosecond, or femtosecond solid-state lasers, including disk or fiber lasers, are used.

4. A device for laser cutting a large transparent glass plate resting on a workbench or above the workbench in a state of suspension on an air cushion, for implementing the method as claimed in claim 1, the device comprising: - a pulsed laser having a control unit and a laser head; - scanning optics comprising at least one electrically deflectable mirror element in the form of a mirror or a rotatable mirror polyhedron; - an optical focusing system at the output of said scanning optics in the form of an objective lens with a fixed focal length and a focal plane tilted relative to the plane of the plate; - a gantry equipped with a coordinate reference system with at least three degrees of freedom in the X, Y and Z axes relative to the glass surface for moving the laser head of the laser; - a horizontal table having a base plate and a programmable coordinate drive on the gantry above the table, the programmable coordinate drive being used for the progressive movement of the laser head within the table and in the vertical direction, the top layer of the table base plate being made of low-pressure polyethylene capable of resisting the impact of scattered laser radiation, while the focused laser radiation penetrates the glass and is deflected from the lower surface to the upper surface of the glass within the aperture of the inclined focal plane of the optical focusing system, the beam creating a fracture stress edge in the glass in a single pass along the cutting line over the thickness of the glass or part of the thickness thereof as a result of the deflection of the beam by the scanning device; - a pneumatic air system for creating an air cushion under the suspended glass sheets during loading and unloading, during cutting and moving; as well as - a basic support fixture for fixing the position of the glass sheet suspended above the workbench and a vertically retractable support friction mechanism having a workbench sensor for moving the glass sheet during loading and unloading in automatic mode.

5. The device according to claim 4, wherein the top layer of the substrate is made of a group of square, rectangular, diamond or polyhedral shaped pads, the average inclination error of the pads does not exceed 300 microns over a reference length of 6 meters, and the vertical error at the joints of adjacent pads does not exceed 150 microns, and the pads include at least one hole for supplying compressed air from a pneumatic air system so that when the glass is cut or moved along the surface of the substrate during the loading / unloading stage, the glass is suspended due to the air cushion under the glass, and low-pressure polyethylene with a density of 0.94 to 0.96 g / cm3 is used as the top layer of the workbench substrate.

6. The device according to claim 5, wherein: A pulsed picosecond fiber laser was used, which transmitted radiation through an optical fiber as long as 25 meters. The pulsed picosecond fiber laser had a central wavelength of 1.03 to 1.06 microns, a power of 50 to 200 watts, and a pulse energy range of 40 to 200 microjoules.

7. The device according to claim 5, wherein: Pulsed nanosecond, picosecond, or femtosecond solid-state lasers, including disk or fiber lasers, are used.

Citation Information

Patent Citations

  • TABLE FOR PROCESSING NON-METALLIC TRANSPARENT MATERIALS WITH LASER RADIATION

    RU130308U1

  • Method of laser processing of transparent brittle material and device for its implementation

    RU2720791C1

Cited By

  • Laser system and process for machining beam-transparent material

    WO2026147737A1