Multi-mobility stamping tool

By designing a stamping tool with a movable transverse part and a wedge-shaped center part, the problem of difficult to manufacture narrowed flange edge parts in the prior art is solved, and precise molding and thickness control of composite blanks are achieved, which is suitable for the aviation field. Massive parts manufacturing.

CN118984766APending Publication Date: 2024-11-19DAHER AEROSPACE
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202380033189.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-04-11
Filing Date
2023-04-11
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

The prior art is difficult to manufacture composite blank parts with narrowed flange edges, and precise adjustment and compaction control of the hedge and mold are not possible, especially in the manufacturing of airplane ribs.

Method used

A stamping tool with a movable transverse part is designed, and the lateral expansion and narrowing of the punch is achieved through the sliding connection between the wedge-shaped central part and the movable transverse part, and the precise matching and adjustment is carried out in conjunction with the spring device to ensure the thickness of the part. and uniform compaction of flange edges.

Benefits of technology

Achieve high-quality molding of composite blanks, especially when manufacturing parts with narrowed flange edges, the thickness and compaction can be precisely controlled, reducing manufacturing costs and weight, and is suitable for manufacturing aircraft wing ribs with high structural performance. etc.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118984766A_ABST
    Figure CN118984766A_ABST
Patent Text Reader

Abstract

The present invention relates to a tool for stamping a composite blank containing a thermoplastic matrix and a continuous fiber reinforcement, and a stamping method using such a tool, the tool comprising: a forming die comprising a pressure cavity (110) having a bottom (111) and a side wall (112); and a punch (120), the external shape of which is matched to the pressure cavity, and which has a central portion (123) and at least two movable transverse portions (121, 122) slidably connected to the central portion (123), the at least two movable transverse portions being secured in translation in the punching direction (190), the further movement of the central portion (123) in the same direction causing the two movable transverse portions to move perpendicular to the punching direction (190).
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention is in the field of tools, and more particularly, in the field of stamping tools for forming thermoplastic matrix composite materials.

[0002] More specifically, the present invention relates to a stamping tool having mobility, in particular multi-mobility. Background Art

[0003] Stamping is a forming process that consists in deforming a blank into a three-dimensional shape between a punch and a die of complementary shapes separated by a spatial gap corresponding to the thickness of the part thus produced.

[0004] This forming is achieved by the relative translational movement of the punch, which approaches the die and passes through the inside of the die, so that the blank is initially close to the entrance plane of the die pressure cavity, and is then held in the spatial gap between the die and the punch to produce deformation, thereby reproducing the shape of the punch and the die during the process of the punch passing through the die.

[0005] Typically, the tool is set on a press, the die is fixed, and the punch is connected to the punch seat of the press and strikes by vertical translation.

[0006] A tool is said to have mobility when it has components that are configured to move during the punching process in a manner other than the punching motion. These components can be located on the punch or on the die, but are generally located on the punch.

[0007] According to non-limiting examples of such mobility, the components move during the punching process in a direction including a direction perpendicular to the punching direction component, or move in the punching direction but at a speed different from or even opposite to the impact speed.

[0008] These mobilities can be controlled by electric, pneumatic or hydraulic actuators or can be generated by appropriate mechanical connections driven by the striking movement itself.

[0009] Document EP 2 243 617 discloses an example of such a tool having such mobility, suitable for punching blanks made of composite material with a thermoplastic matrix, having a part movable in a direction perpendicular to the punching direction and suitable for performing a bending operation.

[0010] The mobile tool is particularly suitable for producing parts with flange edges from composite blanks which consist of continuous fiber reinforcement made of non-plastic or slightly plastic fibers such as carbon fibers or glass fibers.

[0011] In fact, the deformation of this blank occurs through interlaminar and interfiber sliding, i.e. by locally varying the distance between the fibers within acceptable limits.

[0012] Therefore, for shaping, the blank should reach a sufficiently high temperature, generally equal to or above the melting temperature of the polymer constituting the matrix of the composite material, so that this polymer does not hinder the inter-layer and inter-fiber sliding of the reinforcing fibers.

[0013] In short, stamping a composite blank consisting of a thermoplastic matrix reinforced with continuous fibers means maintaining the blank in a state of loose internal cohesion by heating. At the end of the stamping operation, the cohesion is restored by compacting the material between the punch wall and the die wall, whereby mobility is required to simultaneously achieve the forming of the blank and the subsequent compaction of the flange edges when the final part contains at least two flange edges.

[0014] Controlling the compaction phase at the end of the punching operation is critical, as it should simultaneously eliminate air gaps between layers while avoiding inter-fiber squeezing, as too severe a compaction tends to squeeze polymer out from between the fibers. Therefore, the ability to control thickness is critical in a tool with mobility.

[0015] Document EP1543942 discloses another example of a tool with mobility for punching a composite blank with a thermoplastic matrix and a continuous fiber reinforcement, in particular for producing a part with a flange edge in the shape of a half box.

[0016] The device of the prior art includes a punch having a movable lateral part connected to the punch by an elastic connection, the lateral part being arranged to be offset from a central part of the punch, the central part including a wedge-shaped part connected to the punch and movable vertically relative to the lateral part; during the punching operation, when the punch reaches the bottom of the die, the relative movement of the wedge-shaped part causes the lateral parts to be spaced apart from each other, thereby achieving compaction of the flange edge of the semi-box-shaped part.

[0017] The mobility mechanism of this device of the prior art enables the transverse part to move based on a rotational movement under the action of the movement of the wedge-shaped part. This rotation takes place at a point close to the bottom of the die, and on the one hand, the compaction pressure is not uniform in the depth direction of the flange edge, and on the other hand, the mobility mechanism of the device does not allow the manufacture of parts with narrowing flange edges (i.e. when the distance between the two flange edges decreases from the bottom of the die to the die inlet plane).

[0018] However, parts with this half-box shape and extruded flange edges are common in the aerospace field, such as wing ribs.

[0019] Furthermore, such mobility mechanisms of the prior art do not allow for precise adjustment of the degree of compaction achieved by these mobility and the pairing of the punch and die.

[0020] Document FR 2 717 735 discloses a tool with a transverse extrusion device for curing half-box-shaped parts. This tool is not suitable for stamping and curing composite thermoplastic blanks.

[0021] Likewise, document DE741682 discloses a tool for forming, the technical solution of which is not suitable for punching solidified composite blanks. Summary of the invention

[0022] The tool and method described below are intended to solve the above-mentioned drawbacks. To this end, the tool and method relate to a punching tool, comprising:

[0023] A press comprising a fixed platen, a movable platen and a device for moving the movable platen toward the fixed platen in a punching direction;

[0024] a forming die configured to be attached to the stationary platen of the press and having a pressure cavity having a bottom, side walls, and an entrance width measured between the side walls;

[0025] a punch configured to be mounted on the movable platen of the press, having an outer shape matching the pressing cavity and having a central portion and at least two movable transverse portions slidably connected to the central portion, wherein the central portion includes an end portion located between the at least two movable transverse portions and a wedge-shaped portion located between the at least two movable transverse portions;

[0026] pressing means acting on said at least two movable transverse portions so as to press them against the central portion so that the width of said punch is smaller than the width of said inlet;

[0027] The at least two movable lateral parts are stopped by translation in the stamping direction and abut against the bottom of the pressure chamber, and the central part continues to move in the stamping direction relative to the at least two movable lateral parts, causing the two movable lateral parts to move relative to each other in a direction perpendicular to the stamping direction toward the side wall of the pressure chamber, thereby realizing the first lateral expansion of the punch in the expansion direction toward the side wall of the pressure chamber, and the expanded width of the punch is equal to or greater than the entrance width.

[0028] Thus, the lateral expansion of the punch is achieved by the translational movement of the transverse parts, which on the one hand can evenly compact the flange edges of the parts between these transverse parts and the side walls of the mold pressure cavity, and on the other hand enables the punch to punch out parts with strongly narrowed flange edges.

[0029] The tool can be implemented according to the embodiments and variations described below, which can be applied individually or in combination according to any technical operations.

[0030] Advantageously, the central portion of the punch has a shoulder which forms an abutment at the end between the at least two movable transverse portions which are translationally stopped relative to the central portion in the punching direction and which are pressed against the shoulder by at least one spring which acts on the at least two movable transverse portions in the punching direction between the at least two movable transverse portions and the movable pressure plate to form an abutment. This arrangement makes it possible to retract the expansion of the punch after punching and to pull it back even if the part comprises strongly narrowed flange edges.

[0031] According to one embodiment, the punch may include two additional movable transverse parts, which are slidably connected to the wedge-shaped part of the central part between the two additional movable transverse parts, so as to realize a second transverse expansion of the punch in an expansion direction perpendicular to the first expansion direction. This embodiment is suitable for manufacturing a half-box-shaped part with four flange edges by stamping.

[0032] Advantageously, the wedge-shaped central portion of the punch may consist of two parts, between which there is a device for adjusting the width of said central portion according to the expansion direction. This embodiment enables a precise matching of the punch and the mobile part relative to the die cavity, as well as a precise adjustment of the thickness of the part obtained by punching with such a tool.

[0033] The tool may be used in a method for manufacturing a part comprising a web having a web thickness and at least two flange edges, each of the flange edges having a flange edge thickness, at least one of the at least two flange edges having an angle of less than 90° relative to the web, the method comprising the following steps:

[0034] an adjusting step, wherein the punch is matched with the pressing cavity by the device, so as to adjust the width of the central portion according to the thickness of the web and the thickness of the flange edge;

[0035] A blank obtaining step, obtaining a composite blank containing a thermoplastic polymer matrix and a continuous fiber reinforcement, wherein the width of the composite blank is greater than the inlet width;

[0036] a heating step of heating the composite blank at a temperature equal to or greater than the melting temperature of the polymer matrix;

[0037] a punching step, placing the composite blank above the pressing cavity, and punching the composite blank with a punching stroke between the punch and the pressing cavity until the tip of the punch reaches a predetermined distance from the bottom of the pressing cavity, the distance being equal to the thickness of the web;

[0038] a compacting step, continuing the stamping stroke of the movable pressing plate to move the movable transverse portion of the punch to a distance from the side wall of the pressing chamber equal to the flange edge thickness, and making the width of the punch after expansion greater than or equal to the inlet width, thereby compacting the portion;

[0039] a consolidation step of cooling the part pressed between the punch and the pressing cavity to a temperature lower than the melting temperature of the polymer matrix to consolidate the part; and

[0040] The demoulding step is to move the movable platen in the opposite direction and demould the part.

[0041] This method enables the economical serial production of high-quality and high-structural composite structural components, in particular aircraft wing ribs, which have narrowed flange edges. BRIEF DESCRIPTION OF THE DRAWINGS

[0042] The present invention can refer to Figure 1-6 As shown, it is implemented according to the following non-limiting preferred embodiments, wherein:

[0043] Figure 1 A schematic embodiment of the tool at the beginning of a punch stroke is shown in simplified cross-sectional view;

[0044] Figure 2 Through Figure 1 The same cross-section showing the tool at the end of the punch stroke;

[0045] Figure 3 is a perspective view of an exemplary embodiment of a punch including a transverse portion movable in two mutually intersecting directions;

[0046] Figure 4 Shown in a partial perspective exploded view Figure 3 Punch;

[0047] Figure 5 schematically represents a cross section of an aircraft wing according to the sections defined on the figure;

[0048] Figure 6 A flow chart showing an exemplary embodiment of a method of using the tool is shown. DETAILED DESCRIPTION

[0049] Throughout the text, the term "blank" refers to a rigid flat blank that is cut into appropriate contours for shape changes to obtain a three-dimensional part.

[0050] Figure 1-Figure 4 The tool is shown, not the part to be manufactured.

[0051] like Figure 1 As shown, according to some embodiments, the tool of the present invention includes a press (not fully shown), which includes a fixed platen 101 and a movable platen 102. The movable platen can be moved toward the fixed platen along a punching direction 190 by a device such as a hydraulic cylinder to perform a punching operation.

[0052] According to this exemplary embodiment, a forming die 110 having a pressure cavity 115 is attached to the fixed platen 101 by suitable means. The pressure cavity 115 is bounded by a bottom 111 and a side wall 112. According to this embodiment, the side wall 112 of the pressure cavity presents a narrowing according to an angle 192 measured relative to the punching direction 190, so that the width of the pressure cavity at the bottom 111 is greater than its width at the pressure cavity entrance on the top surface of the forming die.

[0053] The punch 120 is attached to and moves with the moving platen 102. The punch has a wedge-shaped central portion 123 inserted between movable transverse portions 121,122.

[0054] According to this embodiment, between the movable transverse portions 121 , 122 , the central portion 125 has a shoulder 125 at its end that forms an abutment.

[0055] The two movable transverse parts 121 , 122 are connected slidingly on a wedge-shaped central part 123 and are pressed against a shoulder 125 , the abutment being formed by a compression spring 130 acting between said movable transverse parts 121 , 122 and the fixed platen 102 of the press.

[0056] The position at which the shoulder forms an abutment may be adjusted by suitable means, such as a peelable wedge 126 .

[0057] According to this embodiment, the tension spring 135 tends to bring the movable lateral portions 121 , 122 into pressing contact with the wedge-shaped central portion 123 .

[0058] The shapes of the punch 120 and the pressure cavity 115 match each other so that when the punch is inserted into the pressure cavity, a space gap corresponding to the thickness of the part to be manufactured (not shown) is left between the punch and the pressure cavity.

[0059] like Figure 2As shown, when the punch 120 descends into the pressure chamber 115, the ends of the movable transverse parts 121, 122 contact the bottom 111 of the pressure chamber 115 (in this figure, they are in direct contact, but in fact, they contact the bottom of the part to be manufactured, which is located between the bottom of the pressure chamber and the end of the punch), if the punching 190 is continued, the central part 120 of the punch is located between the movable transverse parts 121, 122 in the punching direction 190 and moves relative to the movable transverse parts 121, 122. Considering the wedge shape of the sliding connection between the movable transverse parts 121, 122 and the central part 123 of the punch, this relative movement causes the punch to expand, and the movable transverse parts move in directions 291, 292 perpendicular to the punching direction 190 and approach the side wall 112 of the pressure chamber, while causing the compression spring 130 acting on the movable transverse parts in the punching direction to be compressed.

[0060] Thus, the tool is used to compress the material thickness between the punch and the cavity, more specifically between the movable lateral portion and the side walls of the cavity, including the connecting area between the side walls 112 and the bottom 111 of the cavity. This lateral compression capability of the tool makes it possible to punch and then solidify the composite blank containing a thermoplastic matrix and continuous fiber reinforcements, before which its temperature is raised to a temperature close to the melting temperature of the polymer constituting its matrix.

[0061] Back to Figure 1 In this figure, the movable lateral parts 121, 122 of the punch are closer together, so that the width 100 of the punch is smaller than the entrance width 116 at the opening of the pressure chamber. Even if the side wall of the pressure chamber is narrowed, the punch can penetrate into the interior of the pressure chamber.

[0062] like Figure 2 As shown, the penetration of the central portion 123 of the punch between its movable transverse portions 121, 122 causes the width of the punch to expand, so that, due to this expansion, the width 200 of the punch may become greater than the entrance width of the pressing chamber.

[0063] Therefore, the tool is suitable for punching parts with flange edges, whose high angle 192 is at most 30°.

[0064] At the end of the punching operation, the movable platen 102 moves upward and away from the fixed platen 101. The compression spring 130 continues to press the movable transverse parts 121, 122 of the punch toward the pressing cavity, while the tension spring 135 presses the movable transverse part against the central part 123 of the punch, so that the relative movement of the wedge-shaped central part 123 causes the movable transverse part to tighten and the punch to shrink, so that it can be removed from the pressing cavity.

[0065] like Figure 2As shown, the wedge-shaped central portion has a symmetrically shaped bevel, so that for a given relative movement of the central portion 123 in the punching direction 190, the movable transverse portions 121, 122 move laterally along the same movement directions 291, 292. It is understood by those skilled in the art that the central portion 123 can have an asymmetrical bevel, so that a given relative movement of the central portion 123 in the punching direction 190 can result in different movement directions 291, 292 of the right movable transverse portion 122 and the left movable transverse portion 121 in the figure, so as to manufacture a part with a specific geometry, which has different flange edges on both sides.

[0066] Back to Figure 1 The central portion 123 preferably consists of two parts 123 1 , 123 2 and a device 127, such as a peelable gasket, can be arranged between the two parts to adjust the width of the central part 123, so as to accurately define the spatial gap between the movable lateral part and the side wall of the pressure chamber at the end of the punching stroke, and the matching between the punch and the pressure chamber.

[0067] like Figure 3 As shown, according to an exemplary embodiment, the punch 320 may include movable lateral portions 321, 322, 323, 324 that can expand according to the intersecting planes. Figure 3 With reference to the markings x, y, z in the drawing, when the punch is lowered, two movable transverse parts 321, 322 expand the punch in the y direction in the plane zy, and the other two movable transverse parts 323, 324 expand the punch in the x direction in the plane xz.

[0068] All the technical features and embodiments described above are applicable to both the movable transverse parts 321 , 322 in one plane and the movable transverse parts 323 , 324 in another plane.

[0069] Those skilled in the art understand that, on the one hand, the cutting planes for achieving different expansions are not necessarily perpendicular to each other, and on the other hand, this embodiment is not limited to the combination of expansions on only two intersecting planes, but can achieve mobility in multiple intersecting planes.

[0070] like Figure 4 As shown, the central portion 423 of the tool may include an assembly having several parts, and a device 427 between these parts. 1 ,427 2 , used to accurately adjust the space gap between the punch and the side wall of the pressure chamber.

[0071] According to this exemplary embodiment, the central part 423 and the movable transverse parts 321, 322, 323, 324 are connected by means of a groove 425 formed in the central part 423, which cooperates with a tenon 426 on the inner surface of the movable transverse part. These components ensure the translation stop of the movable transverse parts perpendicular to their respective expansion directions, while also ensuring the function of the shoulder 125 forming the abutment.

[0072] The choice of materials for making the various parts of the mold depends on the properties of the materials constituting the forming blank, especially the stamping temperature and thermal expansion characteristics of these materials.

[0073] As non-limiting examples, various components are made of carbon tool steel containing magnesium, chromium, and molybdenum, or of Made of steel.

[0074] The ability of the tool to produce composite parts with thermoplastic matrix extruded flange edges by stamping advantageously enables the integration of functional parts on certain parts, thereby realizing these functions in a single piece, which according to the prior art requires the assembly of multiple parts. By reducing the number of parts and components, the manufacturing cost and the weight of the structural component can be reduced.

[0075] As a non-limiting example, Figure 5 Wing 510 of aircraft 500 is shown having a plurality of ribs 550 extending between inner camber 520 and outer camber 530 .

[0076] These ribs are formed as parts with flanged edges, comprising a web 551 and bottom plates 552, 553, the bottom plates being in fact flanged edges relative to the web, which ensure that the ribs engage with the wing skin at the inner and outer cambers.

[0077] Since a portion of the wing narrows towards its tip and widens towards its connection with the fuselage, in order to be connected to the skin, some of the ribs must have angled flange edges, that is, at least one of the angles 591, 592 between the web 551 and the flange 552 of the rib is less than 90°.

[0078] According to the prior art, these ribs are produced by assembling specific parts instead of at least one flange edge.

[0079] Using the tool according to the invention, these parts can be produced directly by stamping, ie without adding any parts.

[0080] Therefore, if Figure 6 As shown, according to some embodiments, a method uses the tool to stamp a composite blank composed of a thermoplastic polymer matrix and a continuous fiber reinforcement material.

[0081] The finished part to be obtained is, for example, a rib comprising a web and at least two flange edges forming base plates, at least one of said base plates being formed to extend at an angle of less than 90° relative to the web.

[0082] According to an adjustment step 610, the punch may be adjusted, in particular by means of a peelable shim between two parts of the central portion, so that the spatial gap between the cavity and the parts of the punch at the end of the punching stroke is adapted to the target thickness of the part.

[0083] According to the blank obtaining step 620, the composite blank 601 formed by the method is obtained by means of technical means known in the prior art. The composite blank contains a thermoplastic polymer matrix, characterized in particular by its melting temperature and, if relevant, by its crystallization temperature or glass transition temperature, depending on the characteristics of the polymer. As non-exhaustive examples, in aerospace applications, the polymer is polyetheretherketone (PEEK), polyetherketone (PEKK), polyetherimide (PEI) or phenylene polysulfide (PPS).

[0084] The blank is reinforced with continuous reinforcing fibers 611, ie extending continuously between the two edges of the blank 601, made of glass, carbon or aramid, alone or in combination, but these examples are not exhaustive. These fibers have the property of not showing plasticity at the temperatures at which the part is used and at which the method is carried out.

[0085] The blanks are obtained by techniques known in the art, for example by high-pressure water jet cutting on pre-consolidated composite panels, or by the method described in document EP 3 096 940.

[0086] The blank thus obtained is flat and hard.

[0087] In a heating step 630, the blank is heated to a temperature equal to or greater than the melting temperature of the polymer matrix. To this end, according to an exemplary embodiment, the blank is conveyed on a polyimide sheet under an infrared radiation plate 621 or in a tool as described in document EP 3 065 931 and heated to this temperature in an open air environment.

[0088] In the punching step 640 , the hot blank 601 is placed on the forming die while the punch is away from the forming die.

[0089] The width of the blanks 616, 617 is greater than the width of the opening 116 of the pressure cavity in all directions, so the blank 601 rests on the edge of the forming die and can only conform to the shape of the pressure cavity when it is pushed into the pressure cavity and deformed by the punch.

[0090] The blank is then deformed by moving the punch toward the forming die. This deformation is possible because the composite material is heated to a temperature where the continuous fibers do not substantially resist relative movement in the polymer matrix, the blank is already deconsolidated during the heating stage and is also decompacted during the first punching stage.

[0091] In the compaction phase 645, which is continuous with the punching phase, a web is formed between the end of the punch and the bottom of the cavity when the punch stroke wedges into the bottom of the part under a certain pressure, which is determined by the compression spring 130 ( Figure 1 ) characteristics; the stroke of the moving platen in the press continues, resulting in lateral expansion of the punch, which has the effect of compacting the flange edge between the side wall of the pressure chamber and the movable lateral portion of the punch.

[0092] This compaction eliminates the voids between the fibers and ensures that the fibers and matrix are evenly distributed throughout the thickness of the part.

[0093] In a consolidation step 650, the part is cooled while maintaining the mold pressure, i.e. without moving the mobile platen of the press in contrast to the previous step, until the part reaches a temperature suitable for its demolding. To this end, according to an embodiment not shown, the mold can include heating and cooling means for better temperature control at the different stages.

[0094] During a demolding step 660 , the platen is moved away from the forming die and the part is demolded.

[0095] The parts are then trimmed by water jetting or milling to remove uncompacted edges.

[0096] The above description and examples show that the invention achieves the intended purpose and enables the manufacture of parts with narrowed flange edges by stamping composite blanks, in particular composite blanks with continuous fiber reinforcement, while providing precise control of the web and flange edge thickness. Of course, the described tool and method are also suitable for manufacturing parts with non-narrowed flange edges, and even with flared flange edges. In the latter case, the mobility provides enhanced control of the web and flange edge thickness, thereby improving the quality of the part in terms of material integrity.

Claims

1. A stamping tool comprising: A press comprising a fixed pressing plate (101), a movable pressing plate (102) and a device for moving the movable pressing plate along a punching direction (190) toward the fixed pressing plate (101); a forming die configured to be attached to the fixed platen of the press and having a pressure cavity (110) having a bottom (111), side walls (112) and an entrance width (116) measured between the side walls; A punch (120) configured to be mounted on the movable platen of the press, having an outer shape matching the pressing chamber, and having a central portion (123) and at least two movable transverse portions (121, 122, 321, 322, 323, 324) slidably connected to the central portion (123), wherein the central portion includes an end portion located between the at least two movable transverse portions and a wedge portion located between the at least two movable transverse portions; Pressing means (130, 135) acting on the at least two movable transverse parts so as to press them against the central part (123) so that the width of the punch (100) is smaller than the inlet width (116); It is characterized in that the at least two movable lateral parts are stopped by translation in the stamping direction (190) and abut against the bottom of the pressure chamber, and the central part (123) continues to move in the stamping direction relative to the at least two movable lateral parts, causing the two movable lateral parts to move relative to each other according to a direction (291, 292) perpendicular to the stamping direction (190) toward the side wall of the pressure chamber, thereby realizing the first lateral expansion of the punch in the expansion direction toward the side wall (112) of the pressure chamber, and the expanded width (200) of the punch is equal to or greater than the entrance width (116).

2. The punching tool according to claim 1, characterized in that: in, The central portion (123) of the punch has a shoulder (125), which forms an abutment at the end between the at least two movable lateral portions (121, 122), and the movable lateral portion is stopped in translation relative to the central portion (123) in the punching direction and is pressed against the shoulder by at least one spring (130), which acts on the at least two movable lateral portions (121, 122) in the punching direction between the at least two movable lateral portions and the movable pressure plate (102) to form an abutment.

3. The punching tool according to claim 1, characterized in that: in, The punch (320) includes two additional movable lateral parts (323, 324) slidably connected to the central part, and the central part has a wedge shape between the two additional movable lateral parts, thereby realizing a second lateral expansion of the punch (320) in an expansion direction (x) perpendicular to the first expansion direction (291, 292).

4. The punching tool according to claim 1, characterized in that: in, The wedge shape of the central portion (123, 423) comprises two parts (1231, 1232) and has means (127, 4271, 4272) between the two parts for adjusting the width of the central portion according to the expansion direction.

5. A method for manufacturing a part, the part comprising a web (551) having a web thickness and at least two flange edges (552, 553), each of the flange edges having a flange edge thickness, at least one of the at least two flange edges having an angle (591, 592) with respect to the web of less than 90°, the method being implemented using a tool according to claim 4, comprising the following steps: an adjustment step (610), matching the punch with the pressing cavity by means of the device (127, 4271, 4272), thereby adjusting the width of the central portion according to the thickness of the web and the thickness of the flange edge; A blank obtaining step (620) of obtaining a composite blank (601) containing a thermoplastic polymer matrix and a continuous fiber reinforcement (611), wherein the width (616, 617) of the composite blank is greater than the inlet width (116); a heating step (630) of heating the composite blank at a temperature equal to or greater than the melting temperature of the polymer matrix; a punching step (640), placing the composite blank above the pressing cavity, and punching the composite blank (601) between the punch and the pressing cavity with a punching stroke until the tip of the punch reaches a predetermined distance from the bottom (111) of the pressing cavity, the distance being equal to the web thickness; A compacting step (645), continuing the stamping stroke of the movable platen to move the movable lateral portion of the punch to a distance from the side wall of the pressure chamber equal to the flange edge thickness, and making the width (200) of the punch after expansion greater than or equal to the inlet width (116), thereby compacting the portion; a consolidation step (650) of cooling the part pressed between the punch and the stamp to a temperature below the melting temperature of the polymer matrix to consolidate the part; as well as The demolding step (660) moves the movable platen in the opposite direction and demolds the part.

Citation Information

Cited By

  • Combined cap type thermoplastic composite material end cover hot stamping forming die