Electricity storage device

By using the spacer and sealing member of a high-flow resin material in the power storage device, the problem of insufficient sealing is solved, the sealing property and the stability of the current collector spacing are improved, short circuits and electrocorrosion are prevented, and the battery is ensured. layer integrity and performance.

CN118985066APending Publication Date: 2024-11-19TOYOTA INDUSTRIES CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380031503.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-04-01
Filing Date
2023-03-06
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

In the conventional bipolar battery, when a resin material with a small melt mass flow rate is used as the sealing member, it is possible to prevent short circuits caused by contact of the current collector, but the sealing property may be insufficient, resulting in insufficient sealing property of the battery layer.

Method used

Use resin material with a large melt mass flow rate as the spacer to form a more stable sealing structure by welding with the sealing member, enhancing sealing properties, and suppressing the expansion of resin material on the surface of the current collector to ensure the thickness of the sealing member. The direction dimensions are stable.

Benefits of technology

It effectively improves the sealing of the power storage device and the stability of the current collector spacing, prevents short circuits and electrocorrosion, and ensures the integrity and performance of the battery layer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118985066A_ABST
    Figure CN118985066A_ABST
Patent Text Reader

Abstract

In a power storage device (1), a sealing body (3) has a plurality of frame-shaped sealing members (32) welded to respective edge portions (21c) of current collectors (21), and a plurality of frame-shaped spacers (31) disposed between adjacent sealing members (32, 32) in a stacking direction (D). An outer edge portion (31a) of each spacer (31), which protrudes outward from an edge portion (21c) of the current collector (21), and an outer edge portion (32a) of each sealing member (32) adjacent to each spacer (31) in the stacking direction (D), which protrudes outward from the edge portion (21c) of the current collector (21), are welded to each other, thereby forming an outer surface of the closed body (3). The melt mass flow rate of the resin material constituting the spacer (31) is greater than the melt mass flow rate of the resin material constituting the sealing member (32).
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to a power storage device. Background Art

[0002] As a conventional power storage device, there is a bipolar battery described in Patent Document 1, for example. This conventional bipolar battery has a plurality of bipolar electrodes in which a positive electrode active material layer is formed on one surface of a current collector and a negative electrode active material layer is formed on the other surface of the current collector. These bipolar electrodes are stacked with a gel electrolyte layer interposed therebetween to form a bipolar battery.

[0003] In this existing bipolar battery, a sealing member is arranged between the collectors adjacent to each other in the stacking direction so as to surround the single cell layer composed of a positive electrode active material layer, a gel electrolyte layer, and a negative electrode active material layer. The sealing member extends to the outside of the collector and is heat-fused to each other on the outside. The sealing member is formed of an insulating heat-melting resin such as polyethylene or polypropylene, and is heat-fused to the collector or the end collector before the bipolar electrodes are stacked. Through such a sealing member, each single cell layer is sealed, and leakage from the single cell layer and short circuit caused by contact between the collectors are prevented.

[0004] Prior art literature

[0005] Patent Literature

[0006] Patent Document 1: Japanese Patent Application Publication No. 2004-319210 Summary of the invention

[0007] Problem that the invention aims to solve

[0008] In the above-mentioned conventional bipolar battery, the portion of the sealing member heat-fused to the current collector is sandwiched between the current collectors to prevent short circuits caused by contact between the current collectors. In addition, the portions of the sealing member heat-fused to each other outside the current collectors seal the single cell layers.

[0009] In such a configuration, when a material with a low melt mass flow rate is used as the resin material constituting the sealing member, the shape in the thickness direction of the portion heat-fused to the collector is easily stabilized when heat-fused to the collector, and a short circuit caused by contact between the collectors can be appropriately prevented. On the other hand, when a material with a low melt mass flow rate is used as the resin material constituting the sealing member, at the portion heat-fused to each other outside the collector, the fluidity of both adjacent sealing members in the stacking direction is low, and therefore, the sealing of each single cell layer by the sealing member may become insufficient.

[0010] The present disclosure has been made to solve the above-mentioned problems, and an object of the present disclosure is to provide a power storage device that can maintain the intervals between current collectors more appropriately and further improve the sealing performance of the sealing body.

[0011] Solutions for solving problems

[0012] An aspect of the present disclosure relates to a storage device comprising: an electrode stack formed by stacking a plurality of bipolar electrodes including a pair of electrodes consisting of a collector and an active material layer arranged on a first surface and a second surface of the collector; and a sealing body that seals the side surfaces of the electrode stack extending in the stacking direction of the bipolar electrodes, the sealing body having: a plurality of frame-shaped sealing members fused to the edges of the respective collectors; and a plurality of frame-shaped spacers arranged between the sealing members adjacent to each other in the stacking direction, an outer edge portion of each spacer extending outwardly from the edge of the collector and an outer edge portion of each sealing member adjacent to each spacer in the stacking direction extending outwardly from the edge of the collector are fused to each other, thereby forming an outer surface of the sealing body, and a melt mass flow rate of a resin material constituting the spacer is greater than a melt mass flow rate of a resin material constituting the sealing member.

[0013] The melt mass flow rate is a measure of the fluidity of a resin material when it is melted. In the power storage device, the melt mass flow rate of the resin material constituting the spacer is greater than the melt mass flow rate of the resin material constituting the sealing member. By increasing the melt mass flow rate of the resin material constituting the spacer, the fluidity of each spacer when the outer edge of each spacer is welded to the outer edge of each sealing member can be improved. Therefore, the mutual solubility between the spacer and the sealing member can be improved, and the airtightness of the closed body can be further improved. On the other hand, in the power storage device, since the melt mass flow rate of the sealing member welded to the collector is suppressed, it is possible to suppress the resin material from spreading to the active material layer side on the surface of the collector when the sealing member is welded to the collector. Therefore, in the power storage device, the dimension of the sealing member in the thickness direction after welding can be stabilized, and the spacing between the collectors in the stacking direction can be more appropriately maintained.

[0014] Alternatively, the thickness of the spacer is greater than the thickness of the sealing member. By making the thickness of the spacer having a melt mass flow rate greater than that of the sealing member greater than the thickness of the sealing member, the mutual solubility of the sealing member and the spacer can be further fully ensured. Thus, the welding of the outer edge of each spacer with the outer edge of each sealing member becomes easy, and the airtightness of the sealing body can be further improved.

[0015] Alternatively, the sealing member is welded to each of the first and second faces of the current collector. In this case, the electrolyte can be prevented from spreading to other faces of the current collector, and the occurrence of electrical corrosion can be suppressed. Even in the case where the sealing member is placed on each of the first and second faces of the current collector and then pressurized and heated from both sides of the first and second faces for welding, since the melt mass flow rate of the sealing member welded to the current collector is smaller than the melt mass flow rate of the resin material constituting the spacer, the expansion of the resin material when the sealing member is welded to the current collector can be fully suppressed. Therefore, the dimensional stability of the sealing member in the thickness direction after welding can be more appropriately maintained.

[0016] Effects of the Invention

[0017] According to the present disclosure, the intervals between the current collectors can be more appropriately maintained and the airtightness of the sealing body can be further improved. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 This is a schematic cross-sectional view showing a power storage device according to one embodiment of the present disclosure.

[0019] Figure 2 yes Figure 1 The illustrated diagram is an enlarged cross-sectional view of a schematic main portion of a power storage device.

[0020] Figure 3 (a) is a schematic cross-sectional view showing a state of welding of a sealing member to a current collector, (b) shows a state in a comparative example, and (c) shows a state in an example.

[0021] Figure 4 It is a schematic cross-sectional view showing a state of welding of a sealing member and a spacer. DETAILED DESCRIPTION

[0022] Hereinafter, preferred embodiments of a power storage device according to one aspect of the present disclosure will be described in detail with reference to the drawings.

[0023] Figure 1 This is a schematic cross-sectional view showing a power storage device according to one embodiment of the present disclosure. Figure 1 The power storage device 1 shown is a device used in batteries of various vehicles such as forklifts, hybrid vehicles, and electric vehicles. The power storage device 1 is a secondary battery such as a nickel-hydrogen secondary battery and a lithium-ion secondary battery. The power storage device 1 may also be a double-layer capacitor or an all-solid-state battery. In this embodiment, the case where the power storage device 1 is a lithium-ion secondary battery is exemplified.

[0024] The power storage device 1 is composed of an electrode stack 2 formed by stacking a plurality of bipolar electrodes 14, and a sealing body 3 that seals a side surface 2a of the electrode stack 2 extending in a stacking direction D of the bipolar electrodes 14. Figure 1 As shown, the electrode stack 2 includes a plurality of cells 4. Each cell 4 includes a positive electrode 11, a negative electrode 12, and a separator 13.

[0025] The positive electrode 11 and the negative electrode 12 are, for example, rectangular in shape when viewed from the stacking direction. The positive electrode 11 and the negative electrode 12 are arranged to face each other with the separator 13 in between. The relative direction of the positive electrode 11 and the negative electrode 12 is consistent with the stacking direction D of the bipolar electrode 14. The positive electrode 11 is composed of a current collector 21 and a positive electrode active material layer 23 provided on the first surface 21a side of the current collector 21. The negative electrode 12 is composed of a current collector 21 and a negative electrode active material layer 24 provided on the second surface 21b side of the current collector 21. Here, the first surface 21a of the current collector 21 is a surface facing the negative terminal electrode described later, and the second surface 21b of the current collector 21 is a surface facing the positive terminal electrode described later (see Figure 1 ).

[0026] The current collector 21 is a chemically inert electrical conductor used to allow current to continue to flow through the positive electrode active material layer 23 and the negative electrode active material layer 24 during the discharge or charge of the lithium ion secondary battery. In the present embodiment, the current collector 21 forms a double-layer structure in which the first current collector 21A for the positive electrode 11 and the second current collector 21B for the negative electrode 12 overlap each other. The first face 21Aa of the first current collector 21A is equivalent to the face of the first face 21a of the current collector 21 formed by combining the first current collector 21A and the second current collector 21B. The first face 21Ba of the second current collector 21B is equivalent to the face of the second face 21b of the current collector 21 formed by combining the first current collector 21A and the second current collector 21B.

[0027] In the present embodiment, a plurality of monomers 4 are stacked in such a manner that the first current collector 21A of one monomer 4 and the second current collector 21B of another monomer 4 are in contact with each other. Thus, the plurality of monomers 4 are electrically connected in series to form the above-mentioned electrode stack 2. In the monomers 4, 4 adjacent to each other in the stacking direction D, a bipolar electrode 14 is formed in which the first current collector 21A and the second current collector 21B in contact with each other are used as one current collector 21. That is, the electrode stack 2 has a plurality of bipolar electrodes 14 stacked in the stacking direction D. A terminal electrode (positive terminal electrode) including the first current collector 21A is configured at one end of the electrode stack 2 in the stacking direction D. A terminal electrode (negative terminal electrode) including the second current collector 21B is configured at the other end of the electrode stack 2 in the stacking direction D.

[0028] As materials constituting the first current collector 21A and the second current collector 21B, for example, metal materials, conductive resin materials, conductive inorganic materials, etc. can be cited. As conductive resin materials, for example, conductive polymer materials or resins in which conductive fillers are added to non-conductive polymer materials can be cited. The first current collector 21A and the second current collector 21B can have a plurality of layers including one or more layers containing the above-mentioned metal materials or conductive resin materials. A coating layer can also be formed on the surface of the first current collector 21A and the second current collector 21B by a known method such as plating treatment and spraying.

[0029] The first current collector 21A and the second current collector 21B can be formed into a plate, foil, sheet, film, mesh or other form, for example. When the first current collector 21A and the second current collector 21B are metal foils, for example, aluminum foil, copper foil, nickel foil, titanium foil or stainless steel foil is used. The first current collector 21A and the second current collector 21B can also be alloy foils or clad foils of the above metals. When the first current collector 21A and the second current collector 21B are foil-shaped, the first current collector 21A and the second current collector 21B can each be within a range of 1 μm or more and 100 μm or less.

[0030] In the present embodiment, the first current collector 21A is an aluminum foil, and the second current collector 21B is a copper foil. The current collector 21 may be, for example, a laminated foil in which a copper-plated layer as the second current collector 21B is formed on one side of the aluminum foil as the first current collector 21A. The current collector 21 may be, for example, a laminated foil in which the aluminum foil as the first current collector 21A and the copper foil as the second current collector 21B are laminated to form an integral body.

[0031] The positive electrode active material layer 23 is arranged in a rectangular shape in a first surface 21Aa of the rectangular first current collector 21A with a size smaller than the first surface 21Aa. The negative electrode active material layer 24 is arranged in a rectangular shape in a first surface 21Ba of the rectangular second current collector 21B with a size one size smaller than the first surface 21Ba. In other words, at the edge 21c of the current collector 21, an area where the positive electrode active material layer 23 is not arranged is formed on the side of the first surface 21Aa, and an area where the negative electrode active material layer 24 is not arranged is formed on the side of the first surface 21Ba. The negative electrode active material layer 24 is formed to be one size larger than the positive electrode active material layer 23. When viewed from the stacking direction D, the entire formation area of ​​the positive electrode active material layer 23 is located in the formation area of ​​the negative electrode active material layer 24.

[0032] The positive electrode active material layer 23 includes a positive electrode active material that can absorb and release charge carriers such as lithium ions. Examples of the positive electrode active material include composite oxides, metallic lithium, and sulfur. The composition of the composite oxide includes, for example, at least one of iron, manganese, titanium, nickel, cobalt, and aluminum, and lithium. Examples of the composite oxide include olivine-type lithium iron phosphate (LiFePO4), LiCoO2, and LiNiMnCoO2.

[0033] The negative electrode active material layer 24 contains a negative electrode active material that can absorb and release charge carriers such as lithium ions. Examples of the negative electrode active material include graphite, artificial graphite, highly oriented graphite (graphite), mesocarbon microbeads, hard carbon, soft carbon and other carbons, metal compounds, elements or compounds thereof that can alloy with lithium, and carbon with added boron. Examples of elements that can alloy with lithium include silicon and tin.

[0034] In addition to the active material, the positive electrode active material layer 23 and the negative electrode active material layer 24 may also contain a binder and a conductive aid. The binder serves to bind the active material or the conductive aid to each other and maintain the conductive network in the electrode. As a binder, fluorine-containing resins such as polyvinylidene fluoride, polytetrafluoroethylene, fluorine rubber, thermoplastic resins such as polypropylene and polyethylene, imide resins such as polyimide and polyamide-imide, resins containing alkoxysilyl groups, acrylic resins such as polyacrylic acid or polymethacrylic acid, styrene-butadiene rubber, carboxymethyl cellulose, sodium alginate, alginate such as ammonium alginate, water-soluble cellulose ester crosslinked products, starch-acrylic acid graft polymers can be exemplified. These binders can be used alone or in combination. Conductive aids are conductive materials such as acetylene black, carbon black, and graphite, which can improve electrical conductivity. Viscosity regulating solvents such as N-methyl-2-pyrrolidone can be used.

[0035] In order to form the positive electrode active material layer 23 and the negative electrode active material layer 24 on the collector 21, for example, a roll coating method, a die coating method, a dip coating method, a doctor blade method, a spray coating method, a curtain coating method, etc. are used. Specifically, the active material, the solvent, and the binder and the conductive aid as needed are mixed to produce a slurry-like active material layer forming composition, and the active material layer forming composition is applied to the collector 21 and then dried. The solvent can use, for example, N-methyl-2-pyrrolidone, methanol, methyl isobutyl ketone, water, etc. In order to increase the electrode density, the dried active material layer forming composition can also be compressed.

[0036] The separator 13 is arranged between the positive electrode 11 and the negative electrode 12 in the stacking direction D. The separator 13 is a member that prevents electrical short circuit caused by contact between the two electrodes and allows charge carriers such as lithium ions to pass by isolating the adjacent positive electrode 11 and negative electrode in the electrode stack 2. The separator 13 is arranged between the positive electrode active material layer 23 and the negative electrode active material layer 24 that are opposite to each other in the stacking direction D.

[0037] The separator 13 is rectangular in shape, one circle larger than the positive electrode active material layer 23 and the negative electrode active material layer 24 and one circle smaller than the current collector 21, when viewed from the stacking direction D. The end 13a of the separator 13 is located outside the positive electrode active material layer 23 and the negative electrode active material layer 24, when viewed from the stacking direction D, and is welded to a sealing member 32, which will be described later, on the first surface 21a side of the current collector 21.

[0038] The separator 13 is formed in a sheet shape, for example. The separator 13 is composed of, for example, a porous sheet or non-woven fabric containing a polymer that absorbs and retains the electrolyte. Examples of the material constituting the separator 13 include polypropylene, polyethylene, polyolefin, polyester, and the like. The separator 13 may be a single-layer structure or a multi-layer structure. In the case of a multi-layer structure, the separator 13 may include, for example, a substrate layer and a pair of adhesive layers, and may be bonded and fixed to the positive electrode active material layer 23 and the negative electrode active material layer 24 by a pair of adhesive layers. The separator 13 may also include a ceramic layer that serves as a heat-resistant layer. The separator 13 may also be reinforced with a vinylidene fluoride resin compound.

[0039] As the electrolyte impregnated into the separator 13, for example, a liquid electrolyte (electrolyte) containing a non-aqueous solvent and an electrolyte salt dissolved in the non-aqueous solvent, a polymer gel electrolyte containing an electrolyte retained in a polymer matrix, etc. can be cited. In the case where the electrolyte is impregnated into the separator 13, as its electrolyte salt, well-known lithium salts such as LiClO4, LiAsF6, LiPF6, LiBF4, LiCF3SO3, LiN(FSO2)2, and LiN(CF3SO2)2 can be used. As the non-aqueous solvent, well-known solvents such as cyclic carbonates, cyclic esters, chain carbonates, chain esters, and ethers can be used. These well-known solvent materials can also be used in combination of two or more.

[0040] The sealing body 3 is a member that seals the side surface 2a extending in the stacking direction D of the bipolar electrode 14 in the electrode stack 2. The sealing body 3 seals the space S between the current collectors 21, 21 adjacent to each other in the stacking direction D. The space S is defined by the current collectors 21, 21 adjacent to each other in the stacking direction D and the sealing body 3. The electrolyte is stored in the space S.

[0041] The sealing body 3 is composed of a plurality of frame-shaped spacers 31 and a plurality of frame-shaped sealing members 32. The spacers 31 are arranged between the current collectors 21, 21 adjacent to each other in the stacking direction D. In addition, the spacers 31 are arranged between the sealing members 32, 32 adjacent to each other in the stacking direction D. The sealing members 32 are welded to the edges 21c of the current collectors 21. In this embodiment, as shown in FIG. Figure 2 As shown, the sealing member 32 is arranged in a manner covering the edge 21c of the collector 21, that is, the sealing member 32 is located on both sides of the first surface 21a side and the second surface 21b side in the edge 21c of the collector 21, and is further located on the side end surface 21d of the collector 21 in a manner connecting them.

[0042] The sealing member 32 is fused to the first surface 21a over the entirety of the overlapping portion with the first surface 21a, and is fused to the second surface 21b over the entirety of the overlapping portion with the second surface 21b. The sealing member 32 may be fused to the entirety of the side end surface 21d of the collector 21, or may be fused to only a portion thereof. The sealing member 32 may not necessarily be fused to the side end surface 21d. In this case, the sealing member 32 may be in contact with the side end surface 21d, or may be slightly separated from the side end surface 21d.

[0043] The spacer 31 is a portion that also functions as a member for maintaining a gap between the current collectors 21, 21 adjacent in the stacking direction D. The spacer 31 is disposed between the sealing members 32, 32 that cover the edge portions 21c of the current collectors 21, 21 adjacent in the stacking direction D. The thickness T2 of the spacer 31 is greater than the thickness T1 of the sealing member 32.

[0044] In the present embodiment, the sealing member 32 is provided in a manner covering the edge 21c of the current collector 21, but the thickness T1 of the sealing member 32 is determined by the thickness of the portion located on the first surface 21a of the current collector 21 (or the thickness of the portion located on the second surface 21b of the current collector 21). The thickness T2 of the spacer 31 is determined by the thickness of the portion located between the sealing members 32, 32 adjacent to each other in the stacking direction D. The ratio of the thickness T1 of the sealing member 32 to the thickness T2 of the spacer 31 is, for example, 1:2 to 1:4.

[0045] The outer edge 32a of the sealing member 32 and the outer edge 31a of the spacer 31 both extend slightly outward from the edge 21c of the current collector 21 when viewed from the stacking direction D. When viewed from the stacking direction D, the outer edge 31a of each spacer 31 extending outward from the edge 21c of the current collector 21 and the outer edge 32a of each sealing member 32 adjacent to each spacer 31 in the stacking direction D extending outward from the edge 21c of the current collector 21 are welded to each other to form a welded portion W, and the outer surface 3a of the sealing body 3 is formed by the welded portion W. In more detail, the portion including the end face of the outer edge 31a of each spacer 31 and the portion including the end face of the outer edge 32a of each sealing member 32 are integrated by welding, thereby forming a welded portion W extending in the stacking direction D. The outer edge 31a of the spacer 31 and the outer edge 32a of the sealing member 32 can be welded by methods such as infrared welding, hot plate welding, etc. In the welded portion W, the resin material constituting the sealing member 32 and the resin material constituting the spacer 31 are fused to ensure the sealing of the space S between the adjacent collectors 21, 21 in the stacking direction D.

[0046] On the inner side of the welded portion W, the spacer 31 is not welded to any of the sealing members 32 on the first face 21a side of one collector 21 adjacent in the stacking direction D and the sealing member 32 on the second face 21b side of the other collector 21. In the unwelded portion, the spacer 31 and the sealing member 32 on the first face 21a side of the collector 21 may be in contact or slightly separated. Similarly, in the unwelded portion, the spacer 31 and the sealing member 32 on the second face 21b side of the collector 21 may be in contact or slightly separated. The spacer 31 is not welded to any of the collectors 21, 21 adjacent in the stacking direction D.

[0047] In the present embodiment, the inner edge portion 32b of the sealing member 32 extends further to the inner side (i.e., the active material layer side) of the current collector 21 than the inner edge portion 31b of the spacer 31. Here, the inner edge portion 32b of the sealing member 32 and the inner edge portion 31b of the spacer 31 are both portions overlapping with the current collector 21 when viewed from the stacking direction D. That is, the inner edge portion 31b of the spacer 31 is in a state of overlapping with the sealing member 32 on the first surface 21a side of the current collector 21 and the sealing member 32 on the second surface 21b side of the current collector 21 at the inner side of the welded portion W when viewed from the stacking direction D. On the first surface 21a side of the current collector 21, the end portion 13a of the above-mentioned separator 13 is welded to the portion of the inner edge portion 32b of the sealing member 32 extending from the inner edge portion 31b of the spacer 31. Furthermore, when viewed in the stacking direction D, the inner edge portion 31 b of the spacer 31 may protrude further to the inner side of the current collector 21 (ie, the active material layer side) than the inner edge portion 32 b of the sealing member 32 .

[0048] As the resin material constituting the sealing member 32 and the spacer 31, for example, acid-modified polyethylene (acid-modified PE), acid-modified polypropylene (acid-modified PP), polyethylene, polypropylene and other materials with electrolyte resistance can be cited. The resin material constituting the sealing member 32 and the resin material constituting the spacer 31 can be the same or different.

[0049] In the present embodiment, the resin material constituting the sealing member 32 is acid-modified polyethylene or acid-modified polypropylene, and the resin material constituting the spacer 31 is polyethylene or polypropylene. Acid-modified polyethylene and acid-modified polypropylene have the property of being easily bonded to metals compared to polyethylene and polypropylene that have not been acid-modified. In the present embodiment in which the current collector 21 includes a metal foil such as copper foil or aluminum foil, by constituting the sealing member 32 with acid-modified polyethylene or acid-modified polypropylene, the bonding strength (bonding strength) relative to the current collector 21 can be improved. In the spacer 31 that does not require bonding with the current collector 21, by using inexpensive polyethylene or polypropylene, the low cost of the power storage device 1 can be achieved.

[0050] The melt mass flow rate of the resin material constituting the spacer 31 is greater than the melt mass flow rate of the resin material constituting the sealing member 32. The melt mass flow rate (Melt Mass-Flow Rate) is a measure of the fluidity of the resin material when it is melted. In the present embodiment, the melt mass flow rate is measured at a temperature of 230°C and a load of 2.16kg in accordance with JIS K 7210 (ISO1133). As an example, the melt mass flow rate of the resin material constituting the sealing member 32 is 1g / 10min to 10g / 10min, and the melt mass flow rate of the resin material constituting the spacer 31 is 5g / 10min to 15g / 10min.

[0051] As another example, when polyethylene is used as the resin material constituting the sealing member 32 and the spacer 31, the melt mass flow rate of the resin material constituting the sealing member 32 can be set to less than 1 g / 10 min, and the melt mass flow rate of the resin material constituting the spacer 31 can be set to 1 g / 10 min to 5 g / 10 min. By setting the melt mass flow rate of the resin material such as polyethylene or polypropylene constituting the sealing member 32 to a relatively small value such as 2 g / 10 min or less or 1 g / 10 min or less among the resin materials constituting the sealing member 32, it is possible to more effectively suppress the expansion of the resin material on the surface of the collector 21 toward the active material layer side relative to the heating and pressurization in the stacking direction D performed by the heaters 41, 41 when the sealing member 32 is welded to the collector 21.

[0052] Generally, the melt mass flow rate of a resin material has an inverse relationship with the molecular weight of the resin material. The larger the molecular weight, the higher the boiling point and melting point of the resin material tend to become, and the melt mass flow rate tends to become smaller. The smaller the molecular weight, the lower the boiling point and melting point of the resin material tend to become, and the melt mass flow rate tends to become larger. Therefore, the adjustment of the melt mass flow rate of the resin material constituting the sealing member 32 and the adjustment of the melt mass flow rate of the resin material constituting the spacer 31 can be implemented, for example, by adjusting the molecular weight of the main agent of the resin material. In addition, the melt mass flow rate can also be adjusted by containing auxiliary materials such as elastomers.

[0053] When manufacturing the power storage device 1 as described above, a plurality of current collectors 21 provided with the positive electrode active material layer 23 and the negative electrode active material layer 24 are prepared. Next, in the edge portion 21c of each current collector 21, the sealing member 32 is welded to each of the first surface 21a and the second surface 21b. Next, the current collectors 21 to which the sealing member 32 is welded are stacked via the separator 31. Then, the outer edge portion 31a including the end face of each stacked separator 31 and the outer edge portion 32a including the end face of each sealing member 32 are welded to each other to form a welded portion W, thereby forming a closed body 3 composed of the separator 31 and the sealing member 32.

[0054] In the above process, when the sealing member 32 is fused to the current collector 21, for example, Figure 3 As shown in (a), frame-shaped sealing members 32 are respectively arranged on the first surface 21a side and the second surface 21b of the edge 21c of the collector 21, and the edge 21c of the collector 21 and the sealing members 32 on both surfaces are clamped by heaters 41, 41 to heat and pressurize.

[0055] When the sealing member 32 is welded to the current collector 21, if the melt mass flow rate of the resin material constituting the sealing member 32 is equal to or greater than the melt mass flow rate of the resin material constituting the separator 31, as shown in FIG. Figure 3 As shown in (b), since the sealing member 32 is heated and pressurized by the heaters 41, 41 in the stacking direction D (the thickness direction of the sealing member 32), it is conceivable that the resin material will expand toward the active material layer side on the surface of the collector 21. When the resin material expands toward the active material layer side, the thickness of the sealing member 32 will change according to the degree of expansion of the resin material, and the shape of the sealing member 32 in the thickness direction after welding becomes unstable. As a result, it is conceivable that a short circuit will occur due to contact between adjacent collectors 21, 21 in the stacking direction D. In addition, when the thickness of the sealing member 32 after welding becomes insufficient, it is conceivable that it will also affect the welding of the end 13a of the separator 13 relative to the sealing member 32.

[0056] In contrast, in the power storage device 1, since the melt mass flow rate of the sealing member 32 welded to the current collector 21 is suppressed, Figure 3 As shown in (c), when the sealing member 32 is welded to the collector 21, it is possible to suppress the expansion of the resin material on the surface of the collector 21 toward the active material layer side relative to the heating and pressurization in the stacking direction D by the heaters 41, 41. Therefore, in the power storage device 1, the dimension of the sealing member 32 in the thickness direction after welding can be stabilized, and the interval between the collectors 21, 21 in the stacking direction D can be properly maintained. Therefore, a short circuit caused by contact between the collectors 21, 21 can be properly prevented. In addition, since the thickness of the sealing member 32 after welding can be fully ensured, the welding of the sealing member 32 and the end 13a of the separator 13 can also be properly implemented.

[0057] In the above process, the outer edge 31a of each spacer 31 and the outer edge 32a of each sealing member 32 are welded, for example, Figure 4 Infrared heater 42 is used as shown. Figure 4 In the example, the infrared heater 42 is arranged separately from the outer edge portion 31a of each spacer 31 and the outer edge portion 32a of each sealing member 32, and heats the outer edge portion 31a including the end surface of each spacer 31 and the outer edge portion 32a including the end surface of each sealing member 32 in a non-contact manner from a direction intersecting the stacking direction D (the thickness direction of the spacer 31).

[0058] The outer edge 31a of each spacer 31 and the outer edge 32a of each sealing member 32 are heated in a state of being constrained and closely attached to each other in the stacking direction D. In the spacers 31 and sealing members 32 adjacent to each other in the stacking direction D, the outer edge 31a of each spacer 31 melted by heating and the outer edge 32a of each sealing member 32 melted by heating are welded to each other, forming a welded portion W.

[0059] When the outer edge 31a of each spacer 31 and the outer edge 32a of each sealing member 32 are welded, if the melt mass flow rate of the resin material constituting the spacer 31 is the same as or lower than the melt mass flow rate of the resin material constituting the sealing member 32, the fluidity of both the spacer 31 and the sealing member 32 adjacent to each other in the stacking direction D becomes low. As a result, it is conceivable that the mutual solubility between the spacer 31 and the sealing member 32 is insufficient, and the sealing performance of the sealing body 3 to the space S between the current collectors 21, 21 becomes insufficient.

[0060] In this regard, in the power storage device 1, the melt mass flow rate of the resin material constituting the spacer 31 is greater than the melt mass flow rate of the resin material constituting the sealing member 32. By increasing the melt mass flow rate of the resin material constituting the spacer 31, the fluidity of each spacer 31 when the outer edge portion 31a of each spacer 31 and the outer edge portion 32a of each sealing member 32 are welded can be improved. Therefore, the mutual solubility between the spacer 31 and the sealing member 32 can be fully improved, and the airtightness of the sealing body 3 can be further improved.

[0061] In this embodiment, if Figure 4 As shown, each spacer 31 is heated by the infrared heater 42 from a direction intersecting the stacking direction D (the thickness direction of the spacer 31), and only the outer edge portion 31a of the spacer 31 is melted and welded to the outer edge portion 32a of the sealing member 32. Therefore, even if the melt mass flow rate of the resin material constituting the spacer 31 is the same as or greater than the melt mass flow rate of the resin material constituting the sealing member 32, since the inner edge portion 31b of the spacer 31 between the collectors 21, 21 will not melt when being welded to the sealing member 32, it is possible to avoid affecting the thickness dimension of the spacer 31 for preventing short circuits between the adjacent collectors 21, 21 in the stacking direction D.

[0062] In the power storage device 1, the thickness T2 of the spacer 31 is greater than the thickness T1 of the sealing member 32. When the outer edge portion 31a of each spacer 31 and the outer edge portion 32a of the sealing member 32 are welded, the thickness of the spacer 31 having a melt mass flow rate greater than that of the sealing member 32 is greater than the thickness of the sealing member 32, thereby being able to further fully ensure the mutual fusibility between the sealing member 32 and the spacer 31. Therefore, the welding of the outer edge portion 31a of each spacer 31 and the outer edge portion 32a of each sealing member 32 becomes easy, and the airtightness of the sealing body 3 can be further improved.

[0063] In the power storage device 1, the sealing member 32 is welded to each of the first surface 21a and the second surface 21b of the collector 21. As a result, the electrolyte can be prevented from spreading to other surfaces of the collector 21, and the occurrence of electrolytic corrosion can be suppressed. Even in the case where the sealing member 32 is arranged on each of the first surface 21a and the second surface 21b of the collector 21 and then pressurized and heated from both sides of the first surface 21a side and the second surface 21b side for welding, since the melt mass flow rate of the sealing member 32 welded to the collector 21 is smaller than the melt mass flow rate of the resin material constituting the spacer 31, the expansion of the resin material when the sealing member 32 is welded to the collector 21 can be fully suppressed. Therefore, the dimensional stability of the sealing member 32 in the thickness direction after welding can be more appropriately maintained.

[0064] Description of Reference Numerals

[0065] 1…electricity storage device; 2…electrode stack; 3…sealing body; 3a…outer surface; 21 (21A, 21B)…current collector; 14…bipolar electrode; 21a…first surface; 21b…second surface; 23…positive electrode active material layer (active material layer); 24…negative electrode active material layer (active material layer); 31…spacer; 31a…outer edge; 31b…inner edge; 32…sealing member; 32a…outer edge; 32b…inner edge; D…stacking direction; T1…thickness of the sealing member; T2…thickness of the spacer.

Claims

1. A power storage device, characterized in that: have: An electrode stack formed by stacking a plurality of bipolar electrodes including a pair of electrodes consisting of a current collector and an active material layer provided on a first surface and a second surface of the current collector; and a sealing body that seals a side surface of the electrode stack extending in the stacking direction of the bipolar electrodes, The sealing body comprises: a plurality of frame-shaped sealing members welded to the edges of the respective current collectors; and a plurality of frame-shaped spacers arranged between the sealing members adjacent to each other in the stacking direction. The outer edge of each of the spacers extending outward from the edge of the current collector and the outer edge of each of the sealing members adjacent to each of the spacers in the stacking direction extending outward from the edge of the current collector are welded to each other, thereby forming the outer surface of the sealing body. The melt mass flow rate of the resin material constituting the spacer is greater than the melt mass flow rate of the resin material constituting the sealing member.

2. The power storage device according to claim 1, wherein The thickness of the spacer is greater than the thickness of the sealing member.

3. The power storage device according to claim 1 or 2, wherein: The sealing member is welded to each of the first surface and the second surface of the current collector.