Biochar material rich in mineral substances and application thereof
By attaching biomass charcoal powder to a flexible mesh substrate and combining near-infrared phototherapy, the existing single and scald functions of thermal therapy and phototherapy are solved, multi-effect maintenance of joints is achieved, blood circulation and metabolism are promoted, and anti-inflammatory conditions are provided. and analgesic effects.
Patent Information
- Application Number
- CN202411090745.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-09
- Publication Date
- 2024-11-22
AI Technical Summary
Existing thermal therapy and laser therapy have single functions in joint maintenance, which can easily lead to dry skin on the surface, especially in patients with difficulty in temperature regulation, which may cause scalds, and insufficient effect and efficiency.
Using mineral-rich biochar material, the photothermal conversion is achieved by attaching biomass char powder to a flexible mesh substrate, combined with near-infrared phototherapy, providing gentle heat, avoiding scalds, and improving skin protection through minerals and Analgesic effect.
It improves the effect and efficiency of joint maintenance, promotes blood circulation and metabolism, avoids scalds, enhances skin protection, and has anti-inflammatory and analgesic effects.
Smart Images

Figure CN118987209A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of medical materials, and in particular to a biochar material rich in minerals and application thereof. Background Art
[0002] Joint problems are becoming more common as the population ages and lifestyles change. This problem can be caused by a variety of factors, including long-term wear and tear, obesity, aging, and poor exercise habits. These factors work together to cause joint inflammation, pain, and limited mobility, which seriously affects people's daily lives and work efficiency.
[0003] For joint care, especially for knees, currently non-invasive methods such as heat therapy and laser therapy are mainly used. Heat therapy increases local blood circulation, relieves pain and muscle tension, promotes the discharge of metabolic waste, improves joint nutrition supply and functional recovery; laser therapy uses light of a specific wavelength to penetrate deep into tissues, promote cell activity, accelerate the repair process, and has anti-inflammatory and analgesic effects.
[0004] However, heat therapy and laser therapy can cause dryness of the surface skin during treatment, especially in patients with reduced sensation or inability to self-regulate temperature, which can cause burns in severe cases. In addition, the functions of heat therapy and light therapy are relatively simple, and the effect and efficiency of joint care still need to be improved. Summary of the invention
[0005] In view of the deficiencies of the prior art, the purpose of the present invention is to provide a new type of joint care material to improve the care effect and efficiency.
[0006] The present invention provides a mineral-rich biochar material, comprising a flexible mesh substrate and biomass carbon powder attached to one side surface of the mesh substrate, wherein the biomass carbon powder contains Si with a mass fraction of 1% to 8%, Ca with a mass fraction of 0.3% to 2.8%, and K with a mass fraction of 0.9% to 5.5%.
[0007] The present invention fixes biomass charcoal powder with a flexible mesh base. The material as a whole has a mesh structure and can fit the joint part, so that the joint can undergo thermal therapy of biochar and phototherapy of near-infrared light at the same time. At the same time, biomass charcoal powder is rich in minerals, which can improve the effect and efficiency of joint maintenance.
[0008] Furthermore, the particle size of the biomass carbon powder is 50 to 300 μm.
[0009] Furthermore, the specific surface area of the biomass carbon powder is 200 to 550 m 2 / g.
[0010] Furthermore, the biomass charcoal powder is prepared by the following method: drying the biomass material, grinding it and pyrolyzing it in an inert gas atmosphere, the pyrolysis temperature is 650-850°C, the heating rate is 5-10°C / min, the insulation time is 0.5-5h, cooling after pyrolysis, grinding it into powder, and obtaining biomass charcoal powder.
[0011] The biomass charcoal powder provided by the present invention has the property of photothermal conversion, and can efficiently convert light energy into heat energy, providing gentle and lasting heat for the joints, thereby promoting blood circulation and metabolism, accelerating the repair process of the joints, and avoiding burns by controlling the power of light or the temperature. At the same time, the biomass charcoal powder is rich in minerals, which can protect the skin, reduce water loss, prevent dryness of the skin under phototherapy and heat therapy, and also has anti-inflammatory and analgesic effects.
[0012] Furthermore, one side surface of the mesh base is coated with an adhesive, and the biomass carbon powder is adhered to the mesh base. The biomass carbon powder is fixed by adhesion, which is easy to operate and has uniform adhesion.
[0013] Furthermore, the width of each mesh strip in the mesh base is 0.5 to 2 cm.
[0014] Furthermore, the mesh holes on the mesh substrate are polygonal in shape, and the size of the mesh holes is 0.1 to 1 cm. 2 .
[0015] By limiting the size of the mesh bars and mesh holes, the joints can receive the effects of near-infrared light and the heat of biomass charcoal powder at the same time.
[0016] Furthermore, the mesh substrate is made of transparent material, ensuring that near-infrared light can pass through the mesh substrate to act on the biomass carbon powder, thereby ensuring the light-to-heat conversion efficiency.
[0017] Furthermore, the material of the mesh base is selected from one of polyethylene, polyvinyl chloride, polypropylene and polystyrene. The mesh base is made of a flexible film material, which can fit the joints and enhance the heat conduction efficiency.
[0018] The present invention also provides an application, using the above-mentioned mineral-rich biochar material in joint physiotherapy equipment.
[0019] In summary, the present invention has the following beneficial effects:
[0020] The present invention attaches biomass charcoal powder rich in minerals to a flexible mesh base, which can fit the joints to enhance heat conduction efficiency; the mesh structure allows a portion of light to be absorbed by the biomass charcoal powder, and the other portion directly acts on the joints, so that the joints can be simultaneously subjected to thermal and phototherapy effects; the biomass charcoal powder has photothermal conversion properties, and can efficiently convert light energy into thermal energy, providing gentle and lasting heat for the joints, thereby promoting blood circulation and metabolism, accelerating the repair process of the joints, and avoiding burns by controlling the power or temperature of the light; the biomass charcoal powder is rich in minerals that have anti-inflammatory, analgesic, skin protection and water loss reduction effects, and can improve the effect of joint care. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 It is a structural diagram of the biochar material in a specific implementation manner.
[0022] Figure 2 This is a graph showing the temperature rise of the biochar material attached to the knee under near-infrared irradiation in Example 1. DETAILED DESCRIPTION
[0023] In order to make the above-mentioned purposes, features and advantages of the present invention more obvious and easy to understand, the specific embodiments of the present invention are described in detail below. It should be noted that the following embodiments are only used to illustrate the implementation method and typical parameters of the present invention, and are not used to limit the parameter range described in the present invention. Reasonable changes derived therefrom are still within the scope of protection of the claims of the present invention.
[0024] It should be noted that the endpoints and any values of the ranges disclosed in this article are not limited to the precise ranges or values, and these ranges or values should be understood to include values close to these ranges or values. For numerical ranges, the endpoint values of each range, the endpoint values of each range and the individual point values, and the individual point values can be combined with each other to obtain one or more new numerical ranges, and these numerical ranges should be regarded as specifically disclosed in this article.
[0025] The specific embodiment of the present invention provides a mineral-rich biochar material for joint maintenance, which includes a flexible mesh substrate that can be directly attached to the joint; one side surface of the mesh substrate is attached with biomass carbon powder, which has a light-to-heat conversion property. Through the irradiation of a near-infrared lamp, part of the light is absorbed by the biomass carbon powder and converted into heat energy, and the other part directly acts on the joint, so that the joint can achieve the synergistic effect of heat therapy and phototherapy. At the same time, the temperature of the biomass carbon powder is controlled by the light power, which can avoid the risk of scalding, and the required near-infrared light power is low, and the energy consumption is low.
[0026] Preferably, the mesh substrate is a flexible transparent material, and near-infrared light can pass through the transparent mesh substrate to act on the biomass carbon powder to ensure the light-to-heat conversion efficiency. In a specific embodiment, the optional materials of the mesh substrate include polyethylene, polyvinyl chloride, polypropylene, polystyrene, etc. These flexible film materials can fit the joints to enhance the heat conduction efficiency.
[0027] Combination Figure 1 As shown, the mesh substrate is composed of a plurality of interlaced mesh strips 1, and mesh holes 2 are formed between the mesh strips 1. The mesh holes 2 shown in the figure are square. In various embodiments, the shape of the mesh holes 2 can be other polygons, such as triangles, rectangles, hexagons, etc. In a specific embodiment, the width of each mesh strip 1 is preferably 0.5 to 2 cm, and the size of the mesh holes 2 is preferably 0.1 to 1 cm. 2 The sizes of the mesh strips 1 and the mesh holes 2 can be adjusted according to the joints in different parts to ensure that the joints can receive the effects of near-infrared light and the heat of biomass charcoal powder at the same time.
[0028] Preferably, one side of the mesh substrate is coated with an adhesive, and the biomass carbon powder is adhered to the mesh substrate. The biomass carbon powder is fixed by adhesion, which is convenient to operate and has uniform adhesion. In a specific embodiment, the particle size of the biomass carbon powder is 50 to 300 μm, and the specific surface area is 200 to 550 m 2 / g, ensuring that it can be evenly adhered to the mesh substrate and has good photothermal conversion efficiency.
[0029] Biomass carbon powder is also rich in Si, Ca, and K mineral elements, which can play a beneficial role in joints. Among them, Si helps to maintain the skin barrier, reduce water loss, and avoid the problem of dry and damaged skin surface caused by phototherapy and heat therapy; Ca has analgesic effects and relieves muscle pain; K is very important for maintaining normal muscle function and nerve conduction. The presence of these mineral elements can achieve multi-effect maintenance of joints. In a specific embodiment, the mass fraction of Si in the biomass carbon powder is 1% to 8%, the mass fraction of Ca is 0.3 to 2.8%, and the mass fraction of K is 0.9 to 5.5%. By controlling the content of minerals, it is ensured that the biomass carbon powder can fully play its role in joint maintenance.
[0030] The preparation method of the above-mentioned mineral-rich biochar material is as follows:
[0031] A biomass material with a high ash content is selected as a raw material. In a specific embodiment, the biomass material is a lignocellulosic biomass, preferably an agricultural waste. The biomass material is dried and then ground to less than 100 mesh. The biomass material is pyrolyzed in an inert gas atmosphere, with a typical pyrolysis temperature of 650-850°C, a heating rate of 5-10°C / min, and a holding time of 0.5-5h. After the pyrolysis is completed, the temperature is lowered to room temperature, and the carbon material obtained by the pyrolysis is ground into powder to obtain biomass carbon powder. The biomass carbon powder is then adhered to a mesh substrate to obtain a meshed mineral-rich biochar material.
[0032] By using the above-mentioned mineral-rich biochar materials in joint physiotherapy equipment, the photothermal conversion characteristics of biomass carbon powder and the beneficial effects of minerals on joints can be utilized, combined with near-infrared light irradiation, to achieve multi-effect maintenance of joints. Specifically, the mesh biochar material is applied directly to the joints as a dressing, and the minerals rich in biomass carbon powder can be used to perform preliminary maintenance and relief on the joints; through the irradiation of near-infrared lamps, biomass carbon powder can efficiently convert light energy into heat energy, providing gentle and lasting heat to the joints, thereby promoting blood circulation and metabolism, and accelerating the repair process of the joints; part of the near-infrared light directly irradiates the joints through the mesh, promoting blood circulation and cell activity, and accelerating the repair process.
[0033] In summary, the use of the biochar material of the present invention for joint therapy can effectively combine phototherapy, thermotherapy and mineral maintenance, which is beneficial to improving the overall health of the joints and enhancing the effect of joint maintenance.
[0034] The following specific embodiments are provided to further illustrate the technical solutions and effects of the present invention.
[0035] Example 1
[0036] Take 20g peach bark, dry it at 80℃ for 24h, and then grind it to 65 mesh. Pyrolyze it in a N2 atmosphere of 100mL / min, with a heating rate of 10℃ / min, and heat it to 800℃ for 1h. After the pyrolysis, the material is cooled to room temperature and ground into powder to obtain biomass carbon powder with a particle size of less than 200μm. The mass fraction of Si in the biomass carbon powder is 3.5%, the mass fraction of Ca is 1%, and the mass fraction of K is 3%.
[0037] Prepare a polyethylene mesh base with a rectangular mesh shape and a mesh size of 0.5m 2 The mesh strip width is 1 cm. One side of the mesh substrate is coated with an adhesive, and the biomass carbon powder obtained in the above step is adhered to the transparent mesh substrate to obtain a mesh biochar material.
[0038] The biochar material prepared in this example was applied to the joints and irradiated with near-infrared light of 808 nm wavelength at a power of 0.47 W. The temperature of the part covered by the biochar material was tested. The results were as follows: Figure 2 As shown, the temperature is stabilized at 42 °C, indicating that the temperature of the biochar material is controllable.
[0039] Example 2
[0040] Take 20g rice husk, dry it at 80℃ for 24h, and then grind it to 80 mesh. Pyrolyze it in a N2 atmosphere of 100mL / min, with a heating rate of 15℃ / min, and heat it to 700℃ for 2h. After the pyrolysis, the material is cooled to room temperature and ground into powder to obtain biomass carbon powder with a particle size of less than 200μm. The mass fraction of Si in the biomass carbon powder is 6.76%, the mass fraction of Ca is 1.4%, and the mass fraction of K is 1.99%.
[0041] Prepare a polypropylene mesh base with a regular hexagonal mesh shape and a mesh size of 0.8m 2 The mesh strip width is 0.5 cm. One side of the mesh substrate is coated with an adhesive, and the biomass carbon powder obtained in the above step is adhered to the transparent mesh substrate to obtain a mesh biochar material.
[0042] The biochar material prepared in this example was applied to the joints and irradiated with near-infrared light of 808 nm wavelength at a power of 0.48 W. The temperature of the area covered by the biochar material was tested and found to be stable at 48° C.
[0043] Example 3
[0044] Take 20g of walnut shells, dry them at 80℃ for 24h, and then grind them to 50 mesh. Pyrolyze them in a N2 atmosphere at 100mL / min, with a heating rate of 20℃ / min, and heat them to 750℃ for 0.5h. After the pyrolysis, the material is cooled to room temperature and ground into powder to obtain biomass carbon powder with a particle size of less than 100μm. The mass fraction of Si in the biomass carbon powder is 3.07%, the mass fraction of Ca is 1.31%, and the mass fraction of K is 5.44%.
[0045] Prepare a polyethylene mesh base with a square mesh shape and a mesh size of 0.2m 2 The mesh strip width is 1.5 cm. One side of the mesh substrate is coated with an adhesive, and the biomass carbon powder obtained in the above step is adhered to the transparent mesh substrate to obtain a mesh biochar material.
[0046] The biochar material prepared in this example was applied to the joints and irradiated with near-infrared light of 808 nm wavelength at a power of 0.45 W. The temperature of the area covered by the biochar material was tested and found to be stable at 40° C.
[0047] Example 4
[0048] Take 20g rice husk, dry it at 80℃ for 24h, and then grind it to 150 mesh. Pyrolyze it in a N2 atmosphere of 100mL / min, with a heating rate of 15℃ / min, and heat it to 650℃ for 4h. After the pyrolysis, the material is cooled to room temperature and ground into powder to obtain biomass carbon powder with a particle size of less than 100μm. The mass fraction of Si in the biomass carbon powder is 7.61%, the mass fraction of Ca is 0.72%, and the mass fraction of K is 1.46%.
[0049] Prepare a polyethylene mesh base with a square mesh shape and a mesh size of 0.8m 2 The mesh strip width is 0.8 cm. One side of the mesh substrate is coated with an adhesive, and the biomass carbon powder obtained in the above step is adhered to the transparent mesh substrate to obtain a mesh biochar material.
[0050] The biochar material prepared in this example was applied to the joints and irradiated with near-infrared light of 808 nm wavelength at a power of 0.46 W. The temperature of the area covered by the biochar material was tested and found to be stable at 45° C.
[0051] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein by equivalents. However, these modifications or replacements do not make the essence of the corresponding technical solutions deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A biochar material rich in minerals, characterized in that: It comprises a flexible mesh substrate and biomass carbon powder attached to one side surface of the mesh substrate, wherein the biomass carbon powder contains Si with a mass fraction of 1% to 8%, Ca with a mass fraction of 0.3% to 2.8%, and K with a mass fraction of 0.9% to 5.5%.
2. The mineral-rich biochar material according to claim 1, characterized in that: The particle size of the biomass carbon powder is 50 to 300 μm.
3. The mineral-rich biochar material according to claim 2, characterized in that: The specific surface area of the biomass carbon powder is 200-550m 2 / g.
4. The mineral-rich biochar material according to any one of claims 1 to 3, characterized in that: The biomass carbon powder is prepared by the following method: drying the biomass material, grinding it and then pyrolyzing it in an inert gas atmosphere, the pyrolysis temperature is 650-850°C, the heating rate is 5-10°C / min, the insulation time is 0.5-5h, cooling after pyrolysis, grinding it into powder, and obtaining the biomass carbon powder.
5. The mineral-rich biochar material according to claim 1, characterized in that: One side surface of the mesh base is coated with an adhesive, and the biomass carbon powder is adhered to the mesh base.
6. The mineral-rich biochar material according to claim 1, characterized in that: The width of each mesh strip in the mesh base is 0.5 to 2 cm.
7. The mineral-rich biochar material according to claim 6, characterized in that: The mesh holes on the mesh substrate are polygonal in shape, and the size of the mesh holes is 0.1 to 1 cm 2 .
8. The mineral-rich biochar material according to claim 1, characterized in that: The mesh base is made of transparent material.
9. The mineral-rich biochar material according to claim 8, characterized in that: The material of the mesh base is selected from one of polyethylene, polyvinyl chloride, polypropylene and polystyrene.
10. An application, characterized in that: The mineral-rich biochar material described in any one of claims 1 to 9 is used in joint physiotherapy equipment.