Steam purification process for lead paste production of lead-acid battery
Through the design of the modified filter cloth material, the combination of modified silicon-based mesoporous material and polytetrafluoroethylene film is used to solve the problem of low steam purification efficiency in the production of lead-acid battery lead paste, and efficient removal of lead dust and SO2 and NOX, simplifying the process flow and improving purification efficiency.
Patent Information
- Application Number
- CN202411257545.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-09
- Publication Date
- 2024-11-22
AI Technical Summary
The prior art methods for treating steam for the production of lead-acid battery lead paste are too complex, the operation period is long, and the removal efficiency of bag dust removal is limited, so it is unable to effectively remove pollutants such as lead dust, SO2 and NOX.
Using modified filter cloth material, by combining 1.5-2D aromatic sulfone fiber with glass fiber base cloth to form a knitted felt and covering its surface with polytetrafluoroethylene film, a modified filter cloth material with high efficiency adsorption capacity is prepared. Functional groups in the modified silicon-based meporous material adsorbs lead steam and SO2, and electrostatically attracts NOX.
It realizes efficient filtration of lead dust, SO2 and NOX, simplifies the production process, and improves purification efficiency. The lead dust purification rate reaches 98.7%-99.3%, the SO2 purification rate reaches 96.2%-97.2%, and the NOX purification rate reaches 94.9%. -95.8%.
Abstract
Description
Technical Field
[0001] The invention belongs to the field of environmental protection, and in particular relates to a steam purification process for producing lead paste of lead-acid batteries. Background Art
[0002] The production of lead paste for lead-acid batteries is an important link in the manufacturing process of lead-acid batteries. During the production of lead paste for lead-acid batteries, the raw materials need to be placed in a stirring chamber for stirring. Waste gas will be generated during the stirring process. The waste gas contains volatile lead dust, SO2, nitrogen oxides and other atmospheric pollutants, which will cause harm to the environment if directly discharged into the air.
[0003] At present, the treatment methods of lead paste waste gas can be mainly divided into two categories: dry method and wet method. The main methods of dry treatment include bag dust removal and electrostatic precipitator. Bag dust removal is widely used to treat lead paste waste gas due to its high dust removal efficiency, simple structure, convenient operation and maintenance, strong adaptability, etc. However, the removal efficiency of bag dust removal is limited. The waste gas after dust removal may still contain a certain amount of lead dust and atmospheric pollutants such as SO2 and nitrogen oxides.
[0004] The patent document with patent announcement number CN 103239979 B uses the fact that the amount of CO2 dissolved and adsorbed in slightly acidic aqueous solution is significantly lower than that of lead dust, SO2, and SO3. First, slightly acidic water is used to absorb lead dust, SO2, and SO3 to achieve separation from CO2, and then lead dust is removed by precipitation and centrifugation, and finally lime is added for solid sulfur desulfurization. However, the patent and the prior art method for treating steam used in lead paste production are too complicated and have a long operation cycle. Summary of the invention
[0005] In order to solve the problem that the prior art method for treating steam for lead-acid battery lead paste production is too complicated, the present invention provides a steam purification process for lead-acid battery lead paste production.
[0006] The purpose of the present invention can be achieved through the following technical solutions:
[0007] A steam purification process for lead paste production of lead-acid batteries comprises the following steps:
[0008] The exhaust gas is collected by the suction of the air collecting hood fan, transported into the bag dust collector through the pipeline, and after purification, it is sent into the exhaust pipe through the suction of the fan for discharge. The bag dust collector uses modified filter cloth material.
[0009] Furthermore, the preparation process of the modified filter cloth material is:
[0010] A1: Mix 1.5-2D aramid fiber and 2.0-2.8D aramid fiber in a mass ratio of 1:1 and loosen them evenly. Then, form a fiber web by carding and cross-laying. Then, stack them on the upper and lower surfaces of the glass fiber base cloth respectively, pre-needle punch them for preliminary forming, and main needle punch them for reinforcement to form a knitted felt.
[0011] The weight of the fiber mesh on the upper surface of the glass fiber base fabric and the fiber mesh on the lower surface of the glass fiber base fabric are both 300 gsm, and the weight of the glass fiber base fabric is 400 gsm.
[0012] A2: The knitted felt obtained in step A1 is heat-set and then subjected to singeing and pressing treatment, then cooled to 25-35° C., immersed in a modified polytetrafluoroethylene emulsion for 2-3 hours, taken out, pre-baked, and baked to obtain an impregnated knitted felt;
[0013] Among them, the temperature of knitted felt heat setting is 220-240℃, the speed is 4-10m / min, and the time is 3-5min; during the singeing and pressing treatment, the upper and lower hot rollers are pressed, the temperature of the two hot rollers is 200℃, the pressure between the two hot rollers is 5KPa, the singeing and pressing unit is an integrated unit, and the processing speed is 4m / min; the pre-baking temperature is 200-230℃, the time is 4-6min; the baking temperature is 180-250℃, and the time is 5-10min;
[0014] A3: A polytetrafluoroethylene membrane with a pore size of 0.2 μm is laminated on the surface of the impregnated knitted felt to form a thin film to obtain a modified filter cloth material;
[0015] Among them, the laminating temperature is 300-340°C, the pressure is 0.2-1.5MPa, and the laminating unit speed is 1-2m / min.
[0016] Furthermore, the preparation process of the modified polytetrafluoroethylene emulsion is:
[0017] The modified silicon-based mesoporous material is added to anhydrous ethanol, and stirred for 20-30 minutes to prepare a modified silicon-based mesoporous material dispersion, and the modified silicon-based mesoporous material dispersion, silicone oil and polytetrafluoroethylene emulsion are mixed, stirred and ultrasonically vibrated for 15-30 minutes to obtain a modified polytetrafluoroethylene emulsion;
[0018] The dosage ratio of modified silicon-based mesoporous material and anhydrous ethanol is 15-20 g:1.5 L; the volume ratio of modified silicon-based mesoporous material dispersion: silicone oil: polytetrafluoroethylene emulsion is 1-1.5:0.05-0.1:3.
[0019] Furthermore, the preparation process of the modified silicon-based mesoporous material is as follows:
[0020] Tannic acid is added to 0.05 mol / L, pH 8.5 Tris-HCl buffer to obtain a tannic acid solution, and then APTS [(3-aminopropyl) triethoxysilane] is dissolved in anhydrous ethanol to obtain an APTS solution; the tannic acid solution and the APTS solution are mixed, and then MCM-41 is added, ultrasonicated for 10 minutes, and then co-precipitated at 200 r / min at room temperature for 18 hours; after the reaction is completed, the obtained solid material is washed alternately with deionized water and anhydrous ethanol for 3 times, and placed in a vacuum drying oven at 60° C. for drying, and the obtained material is a modified silicon-based mesoporous material;
[0021] The dosage ratio of tannic acid to Tris-HCl buffer is 2 g:1 L; the dosage ratio of APTS to anhydrous ethanol is 10 g:1 L; the dosage ratio of tannic acid solution, APTS solution, and MCM-41 is 1 L:500 mL:30 g.
[0022] Beneficial effects of the present invention:
[0023] 1. The present invention adds modified silicon-based mesoporous material to polytetrafluoroethylene emulsion to prepare modified polytetrafluoroethylene emulsion, and then can prepare modified filter cloth material. The surface of the modified silicon-based mesoporous material contains a large number of amino groups and phenolic hydroxyl groups. These functional groups can strongly adsorb lead ions in lead vapor, thereby removing them from the gas phase; the water vapor generated in the preparation process of lead paste can react with SO2 to form sulfurous acid smoke. This intermediate product has the characteristic of being highly reactive with amino groups, thereby enabling the modified filter cloth material to better absorb SO2 generated in the production process of lead paste; the oxygen atom in the phenolic hydroxyl group has a strong electronegativity. When the phenolic hydroxyl group reacts with NO X When they approach each other, the negatively charged oxygen atom in the phenolic hydroxyl group attracts NO X The part with partial positive charge thus reacts with NO X Electrostatic interaction occurs, allowing the modified filter cloth material to better absorb NO generated during the lead paste production process X .
[0024] 2. In the production process of lead paste, the present invention not only successfully realizes the efficient filtration of lead dust, but also simultaneously removes other waste gas components, thereby simplifying the production process and improving the purification efficiency. DETAILED DESCRIPTION
[0025] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0026] The polytetrafluoroethylene emulsion and silicone oil involved in this application are commercially available products: the polytetrafluoroethylene emulsion is purchased from Guangzhou Songbai Chemical, with a solid content of 60%, and the silicone oil CAS number is 63148-62-9.
[0027] Example 1
[0028] The modified silicon-based mesoporous material of this embodiment is prepared by the following steps:
[0029] 2 g of tannic acid was added to 1 L of 0.05 mol / L, pH 8.5 Tris-HCl buffer to obtain a tannic acid solution, and then 10 g of APTS was dissolved in 1 L of anhydrous ethanol to obtain an APTS solution; 1 L of tannic acid solution and 500 mL of APTS solution were mixed, and then 30 g of MCM-41 was added, ultrasonicated for 10 min, and then co-precipitated at 200 r / min at room temperature for 18 h; after the reaction was completed, the obtained solid material was washed alternately with deionized water and anhydrous ethanol for 3 times, and placed in a vacuum drying oven at 60°C for drying, and the obtained material was a modified silicon-based mesoporous material.
[0030] Comparative Example 1
[0031] The modified silicon-based mesoporous material of this comparative example is prepared by the following steps:
[0032] 10g APTS was dissolved in 1L anhydrous ethanol to obtain an APTS solution, 30g MCM-41 was added to 500mL APTS solution, ultrasonicated for 10min, and then deposited at 200r / min at room temperature for 18h; after the reaction, the obtained solid material was washed alternately with deionized water and anhydrous ethanol for 3 times, and placed in a vacuum drying oven at 60°C for drying, and the obtained material was a modified silicon-based mesoporous material.
[0033] Example 2
[0034] The modified polytetrafluoroethylene emulsion of the present embodiment is prepared by the following steps:
[0035] 15 g of modified silicon-based mesoporous material was added to 1.5 L of anhydrous ethanol and stirred for 20 min to prepare a modified silicon-based mesoporous material dispersion. 1 L of modified silicon-based mesoporous material dispersion, 0.05 L of silicone oil and 3 L of polytetrafluoroethylene emulsion were mixed, stirred and ultrasonically vibrated for 15 min to obtain a modified polytetrafluoroethylene emulsion.
[0036] The preparation process of the modified silicon-based mesoporous material is the same as that of Example 1.
[0037] Example 3
[0038] The modified polytetrafluoroethylene emulsion of the present embodiment is prepared by the following steps:
[0039] 18 g of modified silicon-based mesoporous material was added to 1.5 L of anhydrous ethanol and stirred for 25 min to prepare a modified silicon-based mesoporous material dispersion. 1.2 L of modified silicon-based mesoporous material dispersion, 0.07 L of silicone oil and 3 L of polytetrafluoroethylene emulsion were mixed, stirred and ultrasonically vibrated for 20 min to obtain a modified polytetrafluoroethylene emulsion.
[0040] The preparation process of the modified silicon-based mesoporous material is the same as that of Example 1.
[0041] Example 4
[0042] The modified polytetrafluoroethylene emulsion of the present embodiment is prepared by the following steps:
[0043] 20 g of modified silicon-based mesoporous material was added to 1.5 L of anhydrous ethanol, and stirred for 30 min to prepare a modified silicon-based mesoporous material dispersion. 1.5 L of modified silicon-based mesoporous material dispersion, 0.1 L of silicone oil and 3 L of polytetrafluoroethylene emulsion were mixed, stirred and ultrasonically vibrated for 30 min to obtain a modified polytetrafluoroethylene emulsion.
[0044] The preparation process of the modified silicon-based mesoporous material is the same as that of Example 1.
[0045] Comparative Example 2
[0046] The modified polytetrafluoroethylene emulsion of this comparative example is compared with Example 2, except that the modified silicon-based mesoporous material in Example 2 is replaced by the product prepared in Comparative Example 1, and the remaining raw materials and preparation process are the same as in Example 2.
[0047] Comparative Example 3
[0048] The modified polytetrafluoroethylene emulsion of this comparative example is prepared by the following steps:
[0049] 0.07 L of silicone oil was mixed with 3 L of polytetrafluoroethylene emulsion, stirred and ultrasonically vibrated for 15 min to obtain a modified polytetrafluoroethylene emulsion.
[0050] Example 5
[0051] This embodiment describes a steam purification process for lead paste production of lead-acid batteries, comprising the following steps:
[0052] The exhaust gas is collected by the suction of the air collecting hood fan, transported to the bag filter through the pipeline, purified, and then sent to the exhaust pipe through the suction of the fan for discharge. The bag filter uses modified filter cloth material.
[0053] The preparation process of the modified filter cloth material is as follows:
[0054] A1: 1.5D aramid fiber and 2.0D aramid fiber were mixed and loosened in a mass ratio of 1:1, and then formed into a fiber web by carding and cross-laying, and then stacked on the upper and lower surfaces of a 400gsm glass fiber base cloth, respectively. The weight of the fiber web on the upper surface of the glass fiber base cloth and the fiber web on the lower surface of the glass fiber base cloth were both 300gsm, pre-needled and initially formed, and then reinforced by main needle punching to form a knitted felt;
[0055] A2: The knitted felt obtained in step A1 is subjected to a singeing and pressing treatment after being heat-set at 220°C and 4m / min for 3min. During the singeing and pressing treatment, the upper and lower hot rolling rollers are used for pressing. The temperature of the two hot rolling rollers is 200°C, and the pressure between the two hot rolling rollers is 5KPa. The singeing and pressing unit is an integrated unit. The processing speed is 4m / min. After the treatment, it is cooled to 25°C, immersed in a modified polytetrafluoroethylene emulsion for 2h, taken out, pre-baked at 200°C for 4min, and baked at 180°C for 5min to obtain an impregnated knitted felt;
[0056] A3: A polytetrafluoroethylene membrane with a pore size of 0.2 μm is laminated on the surface of the impregnated knitted felt at 300° C., 0.2 MPa, and a laminating unit speed of 1 m / min to form a thin film to obtain a modified filter cloth material.
[0057] The preparation process of the modified polytetrafluoroethylene emulsion is the same as that of Example 2.
[0058] The exhaust gas removal effect of this embodiment is as follows: the lead dust purification rate reaches 98.7%, the SO2 purification rate reaches 96.2%, and the NO X The purification rate reached 94.9%.
[0059] Example 6
[0060] This embodiment describes a steam purification process for lead paste production of lead-acid batteries, comprising the following steps:
[0061] The exhaust gas is collected by the suction of the air collecting hood fan, transported to the bag filter through the pipeline, purified, and then sent to the exhaust pipe through the suction of the fan for discharge. The bag filter uses modified filter cloth material.
[0062] The preparation process of the modified filter cloth material is as follows:
[0063] A1: 1.7D aramid fiber and 2.5D aramid fiber were mixed and loosened in a mass ratio of 1:1, and then formed into a fiber web by carding and cross-laying, and then stacked on the upper and lower surfaces of a 400gsm glass fiber base cloth, respectively. The weight of the fiber web on the upper surface of the glass fiber base cloth and the fiber web on the lower surface of the glass fiber base cloth were both 300gsm, pre-needled and initially formed, and then reinforced by main needle punching to form a knitted felt;
[0064] A2: The knitted felt obtained in step A1 is subjected to a singeing and pressing treatment after being heat-set at 230°C and 8m / min for 4min. During the singeing and pressing treatment, the upper and lower hot rolling rollers are used for pressing. The temperature of the two hot rolling rollers is 200°C, and the pressure between the two hot rolling rollers is 5KPa. The singeing and pressing unit is an integrated unit. The processing speed is 4m / min. After the treatment, it is cooled to 30°C, immersed in a modified polytetrafluoroethylene emulsion for 2.5h, taken out, pre-baked at 220°C for 5min, and baked at 200°C for 8min to obtain an impregnated knitted felt;
[0065] A3: A polytetrafluoroethylene membrane with a pore size of 0.2 μm is laminated on the surface of the impregnated knitted felt at 320° C., 0.8 MPa, and a laminating unit speed of 1.5 m / min to form a thin film to obtain a modified filter cloth material.
[0066] The preparation process of the modified polytetrafluoroethylene emulsion is the same as that of Example 3.
[0067] The exhaust gas removal effect of this embodiment is as follows: the lead dust purification rate reaches 98.9%, the SO2 purification rate reaches 96.5%, and the NO X The purification rate reached 95.2%.
[0068] Example 7
[0069] This embodiment describes a steam purification process for lead paste production of lead-acid batteries, comprising the following steps:
[0070] The exhaust gas is collected by the suction of the air collecting hood fan, transported to the bag filter through the pipeline, purified, and then sent to the exhaust pipe through the suction of the fan for discharge. The bag filter uses modified filter cloth material.
[0071] The preparation process of the modified filter cloth material is as follows:
[0072] A1: 2D aramid fiber and 2.8D aramid fiber were mixed and loosened in a mass ratio of 1:1, and then formed into a fiber web by carding and cross-laying, and then stacked on the upper and lower surfaces of a 400gsm glass fiber base cloth, respectively. The weight of the fiber web on the upper surface of the glass fiber base cloth and the fiber web on the lower surface of the glass fiber base cloth were both 300gsm, pre-needled and initially formed, and then reinforced by main needle punching to form a knitted felt;
[0073] A2: The knitted felt obtained in step A1 is subjected to a singeing and pressing treatment after being heat-set at 240°C and 10m / min for 5min. During the singeing and pressing treatment, the upper and lower hot rolling rollers are used for pressing. The temperature of the two hot rolling rollers is 200°C, and the pressure between the two hot rolling rollers is 5KPa. The singeing and pressing unit is an integrated unit. The processing speed is 4m / min. After the treatment, it is cooled to 35°C, immersed in a modified polytetrafluoroethylene emulsion for 3h, taken out, pre-baked at 250°C for 6min, and baked at 250°C for 10min to obtain an impregnated knitted felt;
[0074] A3: A polytetrafluoroethylene membrane with a pore size of 0.2 μm is laminated on the surface of the impregnated knitted felt at 340° C., 1.5 MPa, and a laminating unit speed of 2 m / min to form a thin film to obtain a modified filter cloth material.
[0075] The preparation process of the modified polytetrafluoroethylene emulsion is the same as that of Example 4.
[0076] The exhaust gas removal effect of this embodiment is as follows: the lead dust purification rate reaches 99.3%, the SO2 purification rate reaches 97.2%, and the NO X The purification rate reached 95.8%.
[0077] Comparative Example 4
[0078] The remaining raw materials, parameters and preparation process are the same as those in Example 5, except that the preparation process of the modified polytetrafluoroethylene emulsion is the same as that in Comparative Example 2.
[0079] The exhaust gas removal effect of this comparative example is as follows: the lead dust purification rate reaches 94.5%, the SO2 purification rate reaches 92.1%, and the NO X The purification rate reached 89.4%.
[0080] Comparative Example 5
[0081] The remaining raw materials, parameters and preparation process are the same as those in Example 5, except that the preparation process of the modified polytetrafluoroethylene emulsion is the same as that in Comparative Example 3.
[0082] The exhaust gas removal effect of this comparative example is as follows: the lead dust purification rate reaches 92.5%, the SO2 purification rate reaches 87.1%, and the NO X The purification rate reached 80.4%.
[0083] Comparative Example 6
[0084] This comparative example describes a steam purification process for lead paste production of lead-acid batteries, comprising the following steps:
[0085] The exhaust gas is collected by the suction of the air collecting hood fan, transported to the bag filter through the pipeline, purified, and then sent to the exhaust pipe through the suction of the fan for discharge. The bag filter uses modified filter cloth material.
[0086] The preparation process of the modified filter cloth material is as follows:
[0087] A1: 1.5D aramid fiber and 2.0D aramid fiber were mixed and loosened in a mass ratio of 1:1, and then formed into a fiber web by carding and cross-laying, and then stacked on the upper and lower surfaces of a 400gsm glass fiber base cloth, respectively. The weight of the fiber web on the upper surface of the glass fiber base cloth and the fiber web on the lower surface of the glass fiber base cloth were both 300gsm, pre-needled and initially formed, and then reinforced by main needle punching to form a knitted felt;
[0088] A2: The knitted felt obtained in step A1 is subjected to a singeing and pressing treatment after heat setting at 220°C and 4m / min for 3min. During the singeing and pressing treatment, the upper and lower hot rolling rollers are used for pressing. The temperature of the two hot rolling rollers is 200°C, and the pressure between the two hot rolling rollers is 5KPa. The singeing and pressing unit is an integrated unit. The processing speed is 4m / min. After the treatment, it is cooled to 25°C to obtain a pretreated knitted felt.
[0089] A3: A polytetrafluoroethylene membrane with a pore size of 0.2 μm is laminated on the surface of the pretreated knitted felt at 300° C., 0.2 MPa, and a laminating unit speed of 1 m / min to form a thin film to obtain a modified filter cloth material.
[0090] The exhaust gas removal effect of this comparative example is as follows: the lead dust purification rate reaches 89.5%, the SO2 purification rate reaches 83.4%, and the NO X The purification rate reached 76.5%.
[0091] By analyzing the exhaust gas purification rate data of Examples 5 to 7 and Comparative Examples 4 to 6, it can be concluded that immersing the filter cloth material in a modified polytetrafluoroethylene emulsion can effectively improve the purification efficiency of the exhaust gas generated in the lead paste production process.
[0092] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.
[0093] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A steam purification process for lead paste production of lead-acid batteries, characterized in that: The following steps are involved: The exhaust gas is collected by the air collecting hood fan, and then transported to the bag dust collector. After purification, it is sent to the exhaust pipe through the fan for discharge. The bag dust collector uses modified filter cloth material; The preparation method of the modified filter cloth material is: The knitted felt is subjected to heat setting, singeing and pressing treatments, cooled and immersed in a modified polytetrafluoroethylene emulsion for 2-3 hours, taken out and pre-baked and baked to obtain an impregnated knitted felt; a polytetrafluoroethylene film is coated on the surface of the impregnated knitted felt to obtain a modified filter cloth material.
2. A steam purification process for lead paste production of lead-acid batteries according to claim 1, characterized in that: The preparation method of knitted felt is: After two kinds of aromatic sulfone fibers of different fineness are opened evenly, they are combed into a web and cross-laid to form a fiber web, which is stacked on the upper and lower surfaces of the glass fiber base cloth respectively, and is pre-needled and mainly needled to form a knitted felt.
3. A steam purification process for lead paste production of lead-acid batteries according to claim 1, characterized in that: The temperature of heat setting of knitted felt is 220-240℃, the speed is 4-10m / min, and the time is 3-5min; during the singeing and pressing treatment, the upper and lower hot rolling rollers are used for pressing, the temperature of the two hot rolling rollers is 200℃, the pressure between the two hot rolling rollers is 5KPa, the singeing and pressing unit is an integrated unit, and the processing speed is 4m / min; the cooling temperature is 25-35℃; the pre-baking temperature is 200-230℃, the time is 4-6min; the baking temperature is 180-250℃, and the time is 5-10min.
4. A steam purification process for lead paste production of lead-acid batteries according to claim 1, characterized in that: The laminating temperature is 300-340°C, the pressure is 0.2-1.5MPa, the laminating unit speed is 1-2m / min; the pore size of the polytetrafluoroethylene membrane is 0.2μm.
5. A steam purification process for lead paste production of lead-acid batteries according to claim 2, characterized in that: The fineness of the aramid fiber is 1.5-2D and 2.0-2.8D respectively; the mass ratio of 1.5-2D aramid fiber to 2.0-2.8D aramid fiber is 1:1; the gram weight of the fiber mesh on the upper surface of the glass fiber base cloth and the fiber mesh on the lower surface of the glass fiber base cloth are both 300gsm, and the gram weight of the glass fiber base cloth is 400gsm.
6. A steam purification process for lead paste production of lead-acid batteries according to claim 1, characterized in that: The preparation process of modified polytetrafluoroethylene emulsion is: The modified silicon-based mesoporous material is added to anhydrous ethanol, and stirred for 20-30 minutes to prepare a modified silicon-based mesoporous material dispersion. The modified silicon-based mesoporous material dispersion, silicone oil and polytetrafluoroethylene emulsion are mixed, stirred and ultrasonically vibrated for 15-30 minutes to obtain a modified polytetrafluoroethylene emulsion.
7. A steam purification process for lead paste production of lead-acid batteries according to claim 6, characterized in that: The usage ratio of modified silicon-based mesoporous material and anhydrous ethanol is 15-20 g:1.5 L; the volume ratio of modified silicon-based mesoporous material dispersion: silicone oil: polytetrafluoroethylene emulsion is 1-1.5:0.05-0.1:
3.
8. A steam purification process for lead paste production of lead-acid batteries according to claim 6, characterized in that: The preparation process of modified silicon-based mesoporous materials is as follows: Tannic acid is added to Tris-HCl buffer to obtain a tannic acid solution, and APTS is dissolved in anhydrous ethanol to obtain an APTS solution; the tannic acid solution and the APTS solution are mixed, and then MCM-41 is added, ultrasonicated for 10 minutes, and then co-precipitated at 200 r / min at room temperature for 18 hours; after the reaction, the obtained solid material is washed alternately with deionized water and anhydrous ethanol for 3 times, and placed in a vacuum drying oven at 60°C for drying, and the obtained material is a modified silicon-based mesoporous material.
9. A steam purification process for lead paste production of lead-acid batteries according to claim 8, characterized in that: The molar concentration of Tris-HCl buffer is 0.05 mol / L and the pH is 8.
5.
10. A steam purification process for lead paste production of lead-acid batteries according to claim 8, characterized in that: The usage ratio of tannic acid to Tris-HCl buffer is 2 g:1 L; the usage ratio of APTS to anhydrous ethanol is 10 g:1 L; the usage ratio of tannic acid solution, APTS solution, and MCM-41 is 1 L:500 mL:30 g.
Citation Information
Patent Citations
Economical method for desulfurizing and dedusting glue gas produced during smelting of secondary lead
CN103239979B
High-intensity low-stretchability polysulfonamide high-temperature-resisting membrane filter material and preparation method thereof
CN103170183A
Functionalized ionic liquid hybrid mesoporous molecular sieve MCM-48 composite material and preparation method and application thereof
CN103691400A
Activated carbon modification method capable of effectively removing trace acidic gas from air
CN103894148A
Waste gas treatment system for lead-acid storage batteries and application method of waste gas treatment system
CN109078443A