Steel ladle capable of tapping steel from upper part and pouring method adopting steel ladle
By setting up a flow-block crown and an integrally formed water outlet brick above the ladle, combined with inclined casting and oxygen blowing pipe cleaning technology, the traditional ladle outlet alignment problem and the secondary oxidation problem of liquid steel is solved, and the casting quality is significantly improved and Productivity.
Patent Information
- Application Number
- CN202411113902.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-14
- Publication Date
- 2024-11-22
AI Technical Summary
In traditional mold casting and continuous casting production, the bottom steel outlet of the ladle is difficult to align with the casting mold injection port, and it is easy to mix steel slag and secondary oxidation of liquid steel, resulting in poor quality and low pass rate of castings.
Design a steel ladle with steel outflow, and a flow-blocking crown with slag and liquid-blocking function is provided on the upper part of the steel outflow side of the steel outflow side. The steel outlet of the ladle is located at the lower part of the flow-blocking crown or the upper part of the steel outflow side of the steel outflow side. The integrated molded water outlet brick is used, combining inclined pouring and oxygen blowing tube cleaning technology.
It effectively inhibits the entry of slag and inclusions into the casting mold, significantly reduces the inclusion content, improves the mechanical properties and corrosion resistance of the steel, and improves the quality of casting products.
Smart Images

Figure CN118989303A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of iron and steel metallurgy, and in particular relates to a ladle for tapping steel from above and a casting method using the ladle. Background Art
[0002] In traditional mold casting and continuous casting production, due to the large pouring volume and high steel quality requirements, the ladle is usually poured from the bottom steel outlet, and the ladle uses a reverse taper ladle with a larger upper diameter and a smaller bottom diameter to receive the molten steel. However, when pouring steel castings, the steel outlet of this ladle and the steel pouring method using it are not easy to align the casting nozzle with the casting mold, and the steel outlet slide is easy to stick to the steel when changing castings, resulting in high pouring costs; on the other hand, directly using an inclined ladle to pour steel from the upper edge of the front side of the ladle is prone to serious mixing of steel slag and serious secondary oxidation of molten steel, resulting in poor casting quality and low pass rate. Summary of the invention
[0003] In order to solve the problems existing in the prior art, the main purpose of the present invention is to provide a ladle for tapping steel from above and a casting method using the ladle.
[0004] To solve the above technical problems, according to one aspect of the present invention, the present invention provides the following technical solutions:
[0005] A ladle for tapping steel from above has a baffle crown with slag and steel liquid blocking functions arranged on the upper part of the ladle tapping side; the ladle tapping port is located at the lower part of the baffle crown or the upper part of the ladle wall on the ladle tapping side.
[0006] As a preferred embodiment of a ladle for tapping steel from above described in the present invention, the baffle crown is higher than the upper edge of the ladle wall as a whole and presents an arc-shaped structure inclined toward the ladle body, the lower side of the baffle crown is connected to the upper edge of the ladle wall on the ladle tapping side; the angle between the inner side surface of the baffle crown and the plane of the upper edge of the ladle wall is 20-60°.
[0007] As a preferred embodiment of a ladle for tapping steel from above described in the present invention, the length from the upper edge to the lower edge of the baffle crown is 100-600 mm, its material and structure are the same as the ladle wall of the ladle, the outer side of the baffle crown is made of steel material and the inner side is made of refractory material; when the ladle is tilted for pouring, it plays a role in preventing the slag and molten steel in the ladle from flowing out of the ladle.
[0008] As a preferred solution of a ladle with top tapping described in the present invention, the ladle tapping port adopts an integrally formed nozzle seat brick, the inner diameter of the tapping hole in the nozzle seat brick is 50-80mm, the length from the inlet side to the outlet side of the tapping hole of the nozzle seat brick is greater than the thickness of the ladle wall, the inlet side of the tapping hole of the nozzle seat brick is flush with the inner side of the ladle wall, and the outlet side extends out of the outer side of the ladle wall by 100-200mm; the nozzle seat brick is made of refractory materials such as magnesium carbon, high aluminum, and corundum.
[0009] To solve the above technical problem, according to another aspect of the present invention, the present invention provides the following technical solution:
[0010] A method for ladle pouring using the above-mentioned top-discharging method comprises the following steps:
[0011] S1, transporting the ladle filled with molten steel to the pouring position, adjusting the position of the ladle, aligning the steel outlet with the pouring gate of the casting mold, and tilting the ladle to make the molten steel in the ladle flow out from the ladle outlet;
[0012] S2. During the pouring process, the ladle inclination angle is continuously adjusted to ensure that the molten steel in the ladle can be quickly and accurately injected into the mold; after the mold is filled with molten steel, the ladle is adjusted and the pouring is stopped.
[0013] As a preferred embodiment of the method of pouring with the ladle for tapping steel from above described in the present invention, wherein: in the step S1, when the molten steel is tapped after smelting, the ladle for tapping steel from above is used to receive the molten steel.
[0014] As a preferred embodiment of the ladle pouring method using the above-mentioned top-discharging method described in the present invention, in the step S1, the ladle is tilted so that the tapping port is 50-400 mm lower than the slag interface in the ladle.
[0015] As a preferred embodiment of the ladle pouring method using the above-mentioned top-discharging method described in the present invention, in which: in the step S1, a steel cup is used to collect the steel slag mixture flowing out of the steel outlet when the pouring starts, and when the ladle has a large inclination angle and the steel outlet is completely buried in the molten steel in the ladle, the steel cup is removed and the steel flow flowing out of the ladle outlet is injected into the pouring gate of the casting mold for pouring.
[0016] As a preferred embodiment of the ladle pouring method using the above-mentioned upper steel discharge method described in the present invention, wherein: in the step S2, after stopping the pouring, the ladle is transferred to the next pouring position for the next pouring task.
[0017] As a preferred embodiment of the method for ladle pouring with top tapping described in the present invention, wherein: in the step S2, after stopping the pouring, an oxygen blowing pipe is used to blow oxygen to clean the residual steel and slag adhering to the ladle outlet, and then the ladle is hoisted to the slag tapping position, the ladle is reversed, and the remaining slag in the ladle is poured out from the other side of the ladle.
[0018] As a preferred embodiment of the ladle pouring method using the above-mentioned top steel tapping described in the present invention, wherein: in the step S2, when it is difficult to ensure that the steel tapping port is 100 mm lower than the slag interface in the ladle, the ladle is hoisted to the slag tapping position, the ladle is reversed, and the remaining slag in the ladle is poured out from the other side of the ladle.
[0019] The beneficial effects of the present invention are as follows:
[0020] The present invention proposes a ladle for tapping steel from above and a method for casting using the same. By modifying a conventional ladle, a baffle crown with the function of blocking slag and molten steel is arranged on the upper part of the ladle tapping side, and the ladle tapping port is located at the lower part of the baffle crown or the upper part of the ladle wall on the ladle tapping side. The molten steel inside the ladle can be poured into the casting mold through the tapping port first, and the slag and molten steel on the upper surface of the ladle are inhibited from flowing into the casting mold. It not only controls the slag from pouring into the casting mold through the tapping port, but also inhibits the molten steel with more inclusions on the upper layer of the ladle from pouring into the casting mold. During the casting operation, compared with the traditional ladle tapping from above, the exposure of molten steel during the casting process and the large particle inclusions generated by secondary oxidation are greatly reduced, thereby significantly reducing the inclusion content. The reduction of inclusions helps to improve the mechanical properties and corrosion resistance of steel, etc., has a significant effect on improving the quality of casting products, and is conducive to large-scale industrial production and popularization. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the structures shown in these drawings without paying creative work.
[0022] Figure 1 It is a cross-sectional view of a ladle for tapping steel from above according to the present invention.
[0023] Figure 2 It is a schematic cross-sectional view of a ladle for tapping steel from above according to the present invention.
[0024] Figure 3 It is a schematic cross-sectional view of a nozzle seat brick of a ladle for tapping steel from above according to the present invention.
[0025] Wherein: 1- ladle, 2- baffle crown, 3- nozzle seat brick, 4- tapping port, 5- outside of ladle wall, 6- inside of ladle wall, 7- slag, 8- angle between the inside surface of baffle crown and the upper plane of ladle wall, 9- upper plane of ladle wall.
[0026] The realization of the effects, functional features and advantages of the present invention will be further explained in conjunction with embodiments and with reference to the accompanying drawings. DETAILED DESCRIPTION
[0027] The following will be described clearly and completely in conjunction with the technical solutions in the embodiments. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0028] The present invention provides a ladle for tapping steel from above and a casting method using the same. A conventional ladle is modified, and a baffle crown with slag and steel liquid blocking functions is arranged on the upper part of the ladle's tapping side. The ladle tapping port is located at the lower part of the baffle crown or the upper part of the ladle wall on the ladle's tapping side.
[0029] like Figure 1-3 As shown, a ladle for tapping steel from above is provided with a baffle crown 2 having the functions of blocking slag and molten steel at the upper part of the tapping side of the ladle 1; the tapping port 4 of the ladle 1 is located at the lower part of the baffle crown 2 or the upper part of the ladle wall on the tapping side of the ladle 1.
[0030] In one embodiment of the present invention, the baffle crown 2 is higher than the upper edge of the ladle wall as a whole, and is in an arc-shaped structure inclined toward the body of the ladle 1, and the lower side of the baffle crown 2 is connected to the upper edge of the ladle wall on the steel-outlet side of the ladle; the angle 8 between the inner side surface of the baffle crown 2 and the upper edge plane 9 of the ladle wall is 20-60°.
[0031] In one embodiment of the present invention, the length from the upper edge to the lower edge of the baffle crown 2 is 100-600mm, and its material and structure are the same as the outer side 5 and the inner side 6 of the ladle wall of the ladle 1. The outer side of the baffle crown 2 is made of steel material and the inner side is made of refractory material; when the ladle is tilted for pouring, it plays a role in preventing the slag 7 and molten steel in the ladle from flowing out of the ladle.
[0032] In one embodiment of the present invention, the steel outlet 4 of the ladle 1 adopts an integrally formed nozzle seat brick 3, the inner diameter of the steel outlet hole of the nozzle seat brick 3 is 50-80mm, the length from the inlet side to the outlet side of the steel outlet hole of the nozzle seat brick 3 is greater than the thickness of the ladle wall, the inlet side of the steel outlet hole of the nozzle seat brick 3 is flush with the inner side of the ladle wall, and the outlet side extends out of the outer side of the ladle wall by 100-200mm; the nozzle seat brick 3 is made of refractory materials such as magnesium carbon, high aluminum, and corundum.
[0033] The technical solution of the present invention is further described below in conjunction with specific embodiments.
[0034] Example 1
[0035] A certain factory uses a 3-ton induction furnace for smelting and pouring steel castings with a casting weight of 0.5 tons. The ladle used for top tapping is equipped with a baffle crown with the function of blocking slag and molten steel on the upper part of the ladle tapping side; the ladle tapping port is located on the ladle tapping side of the ladle, close to the upper edge of the ladle. The baffle crown is higher than the upper edge of the ladle wall as a whole, and is an arc-shaped structure inclined toward the ladle body. The lower side of the baffle crown is connected to the upper edge of the ladle wall on the ladle tapping side; the angle between the inner side of the baffle crown and the upper edge plane of the ladle wall is 60°. The length from the upper edge to the lower edge of the baffle crown is 400mm, the arc length of the upper edge is 200mm, and the arc length of the lower edge is 1500mm. Its material and structure are the same as the ladle wall of the ladle. The outer side of the baffle crown is made of steel material and the inner side is made of refractory material; when the ladle is tilted for pouring, it plays a role in preventing the slag and molten steel in the ladle from flowing out of the ladle. The ladle tapping port adopts an integrally formed nozzle seat brick. The inner diameter of the tapping hole in the nozzle seat brick is 60mm. The length from the inlet side to the outlet side of the tapping hole of the nozzle seat brick is greater than the thickness of the ladle wall. The inlet side of the tapping hole of the nozzle seat brick is flush with the inner side of the ladle wall, and the outlet side extends out of the outer side of the ladle wall by 120mm. The nozzle seat brick is made of high-aluminum refractory material.
[0036] The above-mentioned ladle for tapping steel from above is used to receive molten steel from the induction furnace, and the molten steel is deoxidized and alloyed, and a total of 3.4 tons of molten steel is received; the ladle for tapping steel from above receiving the molten steel is transferred to the pouring position, the position is adjusted, the ladle tapping port is aligned with the pouring port of the casting mold, and the ladle is tilted so that the molten steel in the ladle flows out from the ladle tapping port; a steel cup is used to receive the steel slag mixture flowing out of the tapping port at the beginning of pouring, and when the ladle has a large inclination angle and the tapping port is completely buried in the molten steel in the ladle, the steel cup is removed to receive the molten steel flowing out of the ladle tapping port Inject into the pouring mouth of the casting mold for pouring; during the pouring process, continuously adjust the inclination angle of the ladle to ensure that the inlet of the ladle outlet is 200mm lower than the interface between the slag and the molten steel on the surface of the ladle; after the casting mold is filled with molten steel, adjust the ladle and stop pouring; lift the ladle to the next pouring position to pour the next casting for pouring; after pouring 6 castings, use an oxygen blowing pipe to blow oxygen to clean the ladle outlet, and clean the residual steel and slag adhered to the outlet; lift the ladle to the slag discharge position, reverse the ladle, and pour out the remaining slag in the ladle from the other side of the ladle.
[0037] Example 2
[0038] A certain factory uses a 5-ton induction furnace for smelting and pouring steel castings with a casting weight of 1.0 ton. The ladle used for top tapping is equipped with a baffle crown with the function of blocking slag and molten steel on the upper part of the ladle tapping side; the ladle tapping port is located on the ladle tapping side of the ladle, close to the upper edge of the ladle. The baffle crown is higher than the upper edge of the ladle wall as a whole, and is an arc-shaped structure inclined toward the ladle body. The lower side of the baffle crown is connected to the upper edge of the ladle wall on the ladle tapping side; the angle between the inner side of the baffle crown and the upper edge plane of the ladle wall is 55°. The length from the upper edge to the lower edge of the baffle crown is 500mm, the arc length of the upper edge is 200mm, and the arc length of the lower edge is 1700mm. Its material and structure are the same as the ladle wall of the ladle. The outer side of the baffle crown is made of steel material and the inner side is made of refractory material; when the ladle is tilted for pouring, it plays a role in preventing the slag and molten steel in the ladle from flowing out of the ladle. The ladle tapping port adopts an integrally formed nozzle seat brick. The inner diameter of the tapping hole in the nozzle seat brick is 68mm. The length from the inlet side to the outlet side of the tapping hole of the nozzle seat brick is greater than the thickness of the ladle wall. The inlet side of the tapping hole of the nozzle seat brick is flush with the inner side of the ladle wall, and the outlet side extends out of the outer side of the ladle wall by 180mm. The nozzle seat brick is made of high-aluminum refractory material.
[0039] The above-mentioned ladle for tapping steel from above is used to receive molten steel from the induction furnace, and the molten steel is deoxidized and alloyed, and a total of 5.5 tons of molten steel is received; the ladle for tapping steel from above receiving the molten steel is transferred to the pouring position, the position is adjusted, the ladle tapping port is aligned with the pouring port of the casting mold, and the ladle is tilted so that the molten steel in the ladle flows out from the ladle tapping port; a steel cup is used to receive the steel slag mixture flowing out of the tapping port at the beginning of pouring, and when the ladle has a large inclination angle and the tapping port is completely buried in the molten steel in the ladle, the steel cup is removed to receive the molten steel flowing out of the ladle tapping port Pour into the pouring mouth of the casting mold for pouring; during the pouring process, continuously adjust the inclination angle of the ladle to ensure that the inlet of the ladle outlet is 200mm lower than the interface between the slag and the molten steel on the surface of the ladle; after the casting mold is filled with molten steel, adjust the ladle and stop pouring; lift the ladle to the next pouring position to pour the next casting for pouring; after pouring 5 castings, use an oxygen blowing pipe to blow oxygen to clean the ladle outlet, and clean the residual steel and slag adhered to the outlet; lift the ladle to the slag discharge position, reverse the ladle, and pour out the remaining slag in the ladle from the other side of the ladle.
[0040] The present invention transforms a conventional ladle, and sets a baffle crown with the function of blocking slag and molten steel on the upper part of the ladle's tapping side, and the ladle tapping port is located at the lower part of the baffle crown or the upper part of the ladle wall on the ladle tapping side. The molten steel inside the ladle can be poured into the mold through the tapping port first, and the slag and molten steel on the upper surface of the ladle can be inhibited from flowing into the mold. It not only controls the slag from pouring into the mold through the tapping port, but also inhibits the molten steel with more inclusions on the upper layer of the ladle from pouring into the mold. During the pouring operation, compared with the traditional ladle tapping and pouring, the exposure of molten steel during the pouring process and the large particle inclusions generated by secondary oxidation are greatly reduced, thereby significantly reducing the inclusion content. The reduction of inclusions helps to improve the mechanical properties and corrosion resistance of steel, etc., has a significant effect on improving the quality of casting products, and is conducive to industrial large-scale production and popularization.
[0041] The above description is only a preferred embodiment of the present invention, and does not limit the patent scope of the present invention. All equivalent structural changes made by using the contents of the present invention specification under the inventive concept of the present invention, or directly / indirectly applied in other related technical fields are included in the patent protection scope of the present invention.
Claims
1. A ladle for tapping steel from above, characterized in that: A baffle crown is arranged on the upper part of the steel tapping side of the ladle, and the steel tapping port of the ladle is located at the lower part of the baffle crown or the upper part of the ladle wall on the steel tapping side of the ladle.
2. The ladle for tapping steel from above according to claim 1, characterized in that: The baffle crown is higher than the upper edge of the ladle wall as a whole and presents an arc-shaped structure inclined toward the ladle body. The lower side of the baffle crown is connected to the upper edge of the ladle wall on the steel outlet side of the ladle; the angle between the inner side surface of the baffle crown and the plane of the upper edge of the ladle wall is 20-60°.
3. The ladle for tapping steel from above according to claim 1, characterized in that: The length from the upper edge to the lower edge of the baffle crown is 100-600mm, and its material and structure are the same as those of the ladle wall.
4. The ladle for tapping steel from above according to claim 1, characterized in that: The ladle tapping hole adopts an integrally formed nozzle seat brick. The inner diameter of the tapping hole in the nozzle seat brick is 50-80mm. The length from the inlet side to the outlet side of the tapping hole of the nozzle seat brick is greater than the thickness of the ladle wall. The inlet side of the tapping hole of the nozzle seat brick is flush with the inner side of the ladle wall, and the outlet side extends out of the outside of the ladle wall by 100-200mm.
5. A ladle pouring method using the top tapping method according to any one of claims 1 to 4, characterized in that: The steps include: S1. The ladle with molten steel flowing out of the upper portion is transported to the pouring position, the position of the ladle is adjusted, the outlet of the ladle is aligned with the pouring port of the casting mold, and the ladle is tilted so that the molten steel in the ladle flows out from the outlet of the ladle; S2. During the pouring process, the ladle inclination angle is constantly adjusted to ensure that the molten steel in the ladle can be quickly and accurately poured into the mold; After the mold is filled with molten steel, adjust the ladle and stop pouring.
6. A preferred embodiment of the method according to claim 5, wherein: In the step S1, when the molten steel is tapped after smelting, the upper tapping ladle is used to receive the molten steel.
7. A preferred embodiment of the method according to claim 5, wherein: In the step S1, the ladle is tilted so that the tapping port is 50-400 mm below the slag interface in the ladle.
8. A preferred embodiment of the method according to claim 5, wherein: In step S1, a steel cup is used to collect the steel slag mixture flowing out of the steel outlet at the beginning of pouring. After the ladle has a large inclination angle and the steel outlet is completely immersed in the molten steel in the ladle, the steel cup is removed and the steel flow flowing out of the ladle outlet is poured into the pouring port of the casting mold for pouring.
9. A preferred embodiment of the method according to claim 5, wherein: In step S2, after the pouring is stopped, the ladle is transferred to the next pouring position for the next pouring task.
10. A preferred embodiment of the method according to claim 5, wherein: In the step S2, after stopping the pouring, oxygen is blown through an oxygen lance to clean the residual steel and slag adhering to the ladle outlet, and then the ladle is hoisted to the slag discharge position, the ladle is reversed, and the remaining slag in the ladle is poured out from the other side of the ladle; or when the ladle outlet cannot be ensured to be 100 mm lower than the slag interface in the ladle, the ladle is hoisted to the slag discharge position, the ladle is reversed, and the remaining slag in the ladle is poured out from the other side of the ladle.